Carbon dioxide capture device
The use of polymer compound particles with amino groups supported on carriers addresses the inefficiencies of current carbon dioxide capture technologies by enhancing absorption and release rates with reduced energy consumption, suitable for large-scale facilities and contributing to a low-carbon society.
Patent Information
- Application Number
- JP2025152063
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2014-08-15
- Filing Date
- 2025-09-12
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2035-08-14
AI Technical Summary
Current carbon dioxide capture technologies, such as chemical absorption using amine aqueous solutions, require high energy input for gas release and have limited reversible absorption capacity and rate, making them inefficient for large-scale applications.
A gas absorbing material using polymer compound particles with amino groups, supported on carriers and stabilized with a film, enhances reversible gas absorption capacity and rate, allowing for efficient absorption and release of acidic gases like carbon dioxide with reduced energy consumption.
The material achieves high-speed gas absorption and release with low heat requirements, maintaining performance stability over multiple cycles, and is suitable for large-scale facilities, contributing to a low-carbon society by improving energy efficiency in carbon dioxide recovery processes.
Smart Images

Figure 0007954477000003 
Figure 0007954477000004 
Figure 0007954477000005
Abstract
Description
[Technical Field]
[0001] The present invention relates to a gas absorbing material, a gas absorbent, and an acidic gas absorption device, an acidic gas recovery device, a water vapor absorption device, a water vapor recovery device, a heat exchanger, and a heat recovery device using the gas absorbent. [Background technology]
[0002] In recent years, global warming caused by carbon dioxide and water vapor emitted from large-scale facilities such as thermal power plants, steel mills, and cement factories, as well as environmental pollution from hydrogen sulfide and other gases, have become serious problems. To mitigate climate change and environmental pollution and realize a low-carbon society, research is underway on methods to separate and recover carbon dioxide, hydrogen sulfide and other acidic gases, and water vapor emitted from these large-scale facilities and sequester them underground or beneath the seabed (Carbon dioxide Capture and Storage; CCS). However, current technology results in very high energy costs for CCS, and a significant reduction in energy costs is required. In particular, since the carbon dioxide separation and recovery process accounts for approximately 60% of the energy costs in CCS, improving the efficiency of the carbon dioxide separation and recovery process and significantly reducing energy consumption are essential to reducing energy costs in CCS. Furthermore, in the field of energy supply, processes are being carried out to separate and recover carbon dioxide, acidic gases such as hydrogen sulfide, and water vapor from fuel gases such as natural gas with high carbon dioxide concentrations, coal gas produced in integrated gasification combined cycle (IGCC) power plants, and hydrogen used in fuel cells. Improving the efficiency and energy conservation of these carbon dioxide separation and recovery processes is also important for reducing energy costs in these fields.
[0003] One known method for separating carbon dioxide from exhaust gas is chemical absorption using an amine aqueous solution. In this method, a low-temperature absorbent (amine aqueous solution) is brought into contact with the exhaust gas in an absorption tower, selectively absorbing carbon dioxide into the absorbent. The absorbent is then transported to a desorption tower and heated to release the carbon dioxide. This chemical absorption method is actually applied to exhaust gas treatment from large-scale facilities. However, it has the problem of requiring a large amount of energy because the absorbent needs to be heated to over 130°C to release the carbon dioxide. In contrast, Patent Document 1 and Non-Patent Documents 1 and 2 propose using a temperature-responsive electrolyte whose basicity changes around the phase transition temperature for the separation and recovery of carbon dioxide. Patent Document 1 describes an example in which carbon dioxide is absorbed by a temperature-responsive electrolyte at 30°C, and then the carbon dioxide is released from the temperature-responsive electrolyte by heating it to 75°C. [Prior art documents] [Patent Documents]
[0004] [Patent Document 1] International Publication No. 2013 / 027668 [Non-patent literature]
[0005] [Non-Patent Document 1] J. Am. Chem. Soc., 134, 18177-, (2012). [Non-Patent Document 2] Angew. Chem, Intl Ed., 53, 2654-, (2014). [Overview of the Initiative] [Problems that the invention aims to solve]
[0006] As described above, the temperature-responsive electrolytes described in Patent Document 1 and Non-Patent Documents 1 and 2 can absorb carbon dioxide at 30°C and release the absorbed carbon dioxide at 75°C, thus significantly reducing the heating temperature during carbon dioxide recovery compared to conventional chemical absorption methods. However, when the inventors investigated these temperature-responsive electrolytes, they found that the reversible absorption amount of acidic gas per unit volume is small, and the absorption and release rates of acidic gas are also small, making them insufficient for use in treating exhaust gases from large-scale facilities and various fuel gases.
[0007] Therefore, in order to solve the problems of the prior art, the inventors have been conducting research with the aim of providing a gas absorbing material and a gas absorber that can realize a gas absorber that has a large reversible gas absorption capacity per unit volume, can absorb and release gas at high speed, and can further reduce the amount of heat required for gas release. Furthermore, the inventors have been conducting research with the aim of providing an acid gas absorption device and an acid gas recovery device that can efficiently absorb and / or recover acid gases by using the gas absorber, and further, a water vapor absorption device, a water vapor recovery device, a heat exchanger and a heat recovery device. [Means for solving the problem]
[0008] As a result of diligent research to solve the above problems, the present inventors have found that by using polymer compound particles having amino groups as a gas absorbing material, it is possible to realize a gas absorber that has a large reversible gas absorption capacity per unit volume, can absorb and release gas at high speed, and furthermore, can keep the amount of heat required for gas release low. In particular, we found that the absorption and release performance of the gas absorber is further improved by having the following configuration. (1) The gel particle film is supported on a carrier such as a thin plate, film, or fiber made of metal, carbon material, or polymer compound. (2) The carriers supporting the gel particle film are stacked and assembled. (3) The gel particle film is stabilized and immobilized by adding a stabilizer. (4) An absorption accelerator is added to the gel particle membrane to increase the absorption capacity and accelerate the absorption rate of acidic gas.
[0009] Specifically, the present invention has the following configurations. [1] A gas absorption material comprising polymer compound particles having an amino group. [2] The gas absorption material according to [1], wherein the polymer compound particles are hydrogel particles. [3] The gas absorption material according to [2], wherein the polymer compound particles have a water content of 0.1 mL or more per 1 g of solid content. [4] The gas absorption material according to any one of [1] to [3], which is for absorbing acidic gas from a gas containing water vapor and acidic gas. [5] The gas absorption material according to any one of [1] to [4], wherein the polymer compound constituting the polymer compound particles is a polymer of a monomer component containing a monomer having an amino group. [6] The gas absorption material according to [5], wherein the monomer contained in the monomer component is a substituted acrylamide monomer. [7] The gas absorption material according to [5] or [6], wherein the monomer having an amino group is N-(aminoalkyl)acrylamide. [8] The gas absorption material according to any one of [5] to [7], wherein the monomer having an amino group is a monomer having a tertiary amino group. [9] The gas absorption material according to any one of [5] to [8], wherein the proportion of the monomer having an amino group in the monomer component is 5 to 95 mol%.
[10] The monomer component comprises a monomer having an amino group and a monomer having a hydrophobic group, The gas absorption material according to any one of [5] to [9], wherein the molar ratio of the monomer having an amino group to the monomer having a hydrophobic group is 5:95 to 95:5.
[11] The gas absorption material according to
[10] , wherein the monomer having an amino group is N-(aminoalkyl)acrylamide, and the monomer having a hydrophobic group is N-alkylacrylamide.
[12] A gas absorbing material according to any one of the following [1] to
[11] , wherein the polymer density within the particles in the dispersed state after swelling of polymer compound particles in water is 0.3 to 80%.
[13] The gas absorbing material according to any one of the items [1] to
[12] , wherein the particle size of the polymer compound particles in a dry state is 5 nm to 10 μm.
[14] The polymer compound particles undergo a phase transition due to a change in temperature, The gas absorbing material according to any one of the following [1] to
[13] , wherein the phase transition temperature of the polymer compound particles is in the range of 10 to 95°C.
[15] The gas absorbing material according to any one of the items [1] to
[14] , wherein a crosslinking structure is formed between at least some of the polymer compound particles.
[16] The gas absorbing material according to any one of the items [1] to
[15] , wherein the hydrodynamic particle size after swelling and dispersion of the polymer compound particles in water is 10 nm to 50 μm.
[17] A gas-absorbing material according to any one of the items [1] to
[16] for absorbing and releasing gases.
[18] A gas-absorbing material as described in
[17] for repeating a cycle of gas absorption and release.
[19] A gas absorbent material described in any one of the items [1] to
[16] for absorbing carbon dioxide gas.
[0010]
[20] Use of polymer compound particles having amino groups for gas absorption.
[21] Use of polymer compound particles having amino groups for the absorption of acidic gases from gases including water vapor and acidic gases.
[0011]
[22] A gas absorber characterized by having a gel particle film of a polymer compound having an amino group and a carrier that supports the gel particle film.
[23] The gas absorber according to
[22] , characterized in that the gel particle film contains the gas absorbent material described in any one of [1] to
[19] .
[24] The gas absorber according to
[22] or
[23] , wherein the gel particle membrane is a hydrogel particle membrane containing 10% by mass or more of water relative to the total amount of the gel particle membrane.
[25] The rate of carbon dioxide gas release is 0.1 mmol / m³ 2 A gas absorber described in any one of the following items
[22] to
[24] , which is 1 / sec or more.
[26] The absorption rate of carbon dioxide gas is 0.05 mmol / m³ 2 A gas-absorbing material described in any one of the following items
[22] to
[25] , which is 1 / sec or greater.
[27] The gas absorber according to any one of the claims
[22] to
[26] , wherein the carrier is a thin plate or a tube.
[28] The gas absorber according to any one of the following
[22] to
[26] , wherein the carrier is a laminate formed by stacking a plurality of thin plates.
[29] The gas absorber according to
[27] or
[28] , wherein the thin plate is a metal foil.
[30] The gas absorber according to
[27] or
[28] , wherein the thin plate is made of carbon material.
[31] The gas absorber according to
[27] or
[28] , wherein the thin plate is a resin film.
[32] The gas absorber according to any one of the following
[22] to
[26] , wherein the carrier is a fiber aggregate.
[33] The gas absorber according to any one of the following
[22] to
[26] , wherein the carrier is an aggregate of multiple fiber aggregates stacked on top of each other.
[34] The gas absorber according to
[32] or
[33] , wherein the fiber aggregate comprises inorganic fibers.
[35] The gas absorber according to
[34] , wherein the inorganic fiber is a metal fiber.
[36] The gas absorber according to
[35] , wherein the metal fibers include at least one of stainless steel fibers and aluminum fibers.
[37] The gas absorber according to
[35] , wherein the metal fibers include nickel fibers.
[38] The gas absorber according to any one of the following
[35] to
[37] , wherein the metal fiber is a sintered metal fiber.
[39] The gas absorber according to
[34] , wherein the inorganic fiber is a carbon fiber.
[40] The fiber aggregate is a gas absorber according to any one of the
[32] to
[39] paragraphs, which includes organic fibers.
[41] The gas absorber described in
[40] , wherein the fiber aggregate is paper.
[42] The gas absorber according to any one of
[22] to
[26] , wherein the carrier is a porous body.
[43] The gas absorber according to
[42] , wherein the porous body is a foamed metal.
[44] The carrier has a constant pressure specific heat of 2500 kJ / (m³ 3 K) A gas absorber according to any one of the following items
[22] to
[43] , consisting of the following materials.
[45] The gas absorber according to any one of the following
[22] to
[44] , wherein the carrier is made of a material with a thermal conductivity of 10 W / (mK) or more.
[46] The carrier is a gas absorber according to any one of
[22] to
[45] , wherein its surface functions as a heat transfer surface of a heat exchanger.
[47] The carrier is a gas absorber according to any one of
[22] to
[46] , which functions as a heat exchanger.
[48] The gas absorber according to any one of the items
[22] to
[47] , wherein the packing rate of the gel particle membrane is 20% or more.
[49] The gas absorber according to any one of the following
[22] to
[48] , wherein the gel particle film further comprises a film stabilizer.
[50] The gas absorber according to
[49] , comprising a polymer compound as the film stabilizer.
[51] The gas absorber according to
[49] , wherein the membrane stabilizer comprises a polymer compound having at least one of a primary amino group, a secondary amino group, and a tertiary amino group.
[52] The gas absorber according to
[51] , wherein the film stabilizer comprises polyvinylamine or a derivative of polyvinylamine.
[53] The film stabilizer comprises a polymerizable compound as described in any one of the following
[49] to
[52] gas absorber.
[54] The gas absorber according to any one of the claims
[49] to
[53] , wherein the membrane stabilizer comprises a polymer compound produced by a polymerization reaction of a polymerizable compound within the gel particle membrane.
[55] The gas absorber according to
[53] or
[54] , wherein the polymerizable compound is acrylamide or an acrylamide derivative.
[56] The gas absorber according to
[55] , comprising a substituted aminoalkylacrylamide and an acrylamide derivative having two polymerizable groups as the polymerizable compound.
[57] The film stabilizer is a gas absorber according to any one of the
[49] to
[56] items, comprising a crosslinking agent.
[58] The gas absorber according to
[57] , wherein the crosslinking agent is a titanium crosslinking agent.
[59] The gas absorber according to any one of the claims
[49] to
[58] , wherein the content of the membrane stabilizer in the gel particle membrane is 1 to 89% by mass relative to the total amount of the gel particle membrane.
[60] The gel particle membrane is a gas absorber according to any one of the items
[22] to
[59] , comprising an absorption enhancer.
[61] The gel particle film comprises an amine-containing compound having a molecular weight of 61 to 10000, as described in any one of
[22] to
[60] , and is a gas absorber.
[62] The gas absorber according to
[61] , wherein the gel particle film comprises at least one of an amine having an amino group and a hydroxyl group, or an amine having three amino groups.
[63] The gel particle film is made of Isopropylaminoethanol, N,N,N',N'-Tetramethyl-1,6-hexanediamine, Imino-bis(N,N-dimethylpropylamine) and N,N ’ ,N ” A gas absorber according to
[61] , comprising at least one of the following: -pentamethyldiethylenetriamine.
[64] The gas absorber according to any one of the following
[22] to
[63] , wherein the gel particle film surface is supported on the heat transfer surface of a heat exchanger.
[65] The gas absorber according to any one of the following
[22] to
[64] , wherein the gel particle film is capable of reversibly absorbing at least an acidic gas.
[66] The gas absorber according to
[65] , wherein the acidic gas is carbon dioxide.
[67] The gas absorber according to
[65] , wherein the acidic gas is hydrogen sulfide.
[68] The gas absorber according to any one of the following
[22] to
[67] , wherein the gel particle film is capable of reversibly absorbing at least water vapor.
[0012]
[69] A method for absorbing gas, characterized by absorbing gas into a gel particle film of a polymer compound having an amino group.
[70] The gas absorption method according to
[69] , wherein after absorbing the gas, the temperature of the gel particle film is increased to release the absorbed gas from the gel particle film.
[71] The gas absorption method according to
[70] , wherein the temperature is increased until a volume phase transition occurs in the polymer compound.
[72] The gas absorption method according to
[70] or
[71] , wherein after the gas has been released, the temperature of the gel particle film is lowered and the gas is absorbed again by the gel particle film.
[73] A gas absorption method according to any one of the items
[70] to
[72] , wherein the cycle consisting of absorption and emission is repeated a plurality of times.
[0013] An acidic gas absorber characterized by having a gas absorber described in any one of the items
[74]
[22] to
[68] . An acidic gas recovery device characterized by having a gas absorber as described in any one of items
[75]
[22] to
[68] . A water vapor absorber characterized by having a gas absorber as described in any one of items
[76]
[22] to
[68] . A water vapor recovery device characterized by having a gas absorber as described in any one of items
[77]
[22] to
[68] . A heat exchanger characterized by having a gas absorber as described in any one of the items
[78]
[22] to
[68] . A heat recovery device characterized by having a gas absorber as described in any one of the items
[79]
[22] to
[68] . [Effects of the Invention]
[0014] According to the gas-absorbing material of the present invention, it is possible to realize a gas absorber that has a large reversible gas absorption capacity per unit volume, can absorb and release gas at high speed, and can keep the amount of heat required for gas release low. Furthermore, the gas absorber of the present invention has a large reversible gas absorption capacity per unit volume, allowing for high-speed absorption and release of gas. In addition, its gel particle film has high stability, ensuring that the initial performance is reliably maintained even when gas absorption and release are repeated. The acid gas absorption device, acid gas recovery device, water vapor absorption device, water vapor recovery device, heat exchanger, and heat recovery device of the present invention, by having such gas absorbers, can efficiently absorb and recover acid gases and water vapor gases, and can greatly contribute to the realization of a low-carbon society. [Brief explanation of the drawing]
[0015] [Figure 1] This is a schematic diagram illustrating the mechanism by which the amino group-containing polymer compound particles used in this invention undergo a phase transition and the mechanism by which they absorb and release carbon dioxide. [Figure 2] This is a schematic diagram showing a first embodiment of a carbon dioxide gas recovery device to which the acid gas recovery device of the present invention is applied. [Figure 3] This is a schematic diagram showing a second embodiment of a carbon dioxide gas recovery device to which the acid gas recovery device of the present invention is applied. [Figure 4] This graph shows the temperature-dependent change in particle size of amine-containing gel particles from synthesis example 2. [Figure 5] This graph shows the temperature dependence of the pH of the particle solution containing amine-containing gel particles from Synthesis Example 2. [Figure 6] This is the titration curve of the particle solution containing amine-containing gel particles from Synthesis Example 2 with hydrochloric acid. [Figure 7] This graph shows the change over time in the amount of carbon dioxide emitted by the amine-containing gel particles of synthesis example 2. [Figure 8]This graph shows the film thickness dependence of the carbon dioxide emission rate in the gel particle film and the gel homogeneous film of amine-containing gel particles (particle size 300 nm) from Synthesis Example 2. [Figure 9] This graph shows the film thickness dependence of the carbon dioxide emission rate for gel particle films containing amine-containing gel particles (particle size 300 nm) from Synthesis Example 2 and gel particle films containing amine-containing gel particles (particle size 1 μm) from Synthesis Example 3. [Figure 10] This graph shows the film thickness dependence of the carbon dioxide absorption rate for gel particle films of amine-containing gel particles (particle size 300 nm) from Synthesis Example 2, gel particle films and homogeneous gel films of amine-containing gel particles (particle size 1 μm) from Synthesis Example 3, and gel particle films of amine-containing gel particles (crosslinked gel particles) from Synthesis Example 4. [Figure 11] This is a schematic diagram showing a reactor used to evaluate the gas absorption and release performance of a gas absorber. [Figure 12] This graph shows the time-dependent changes in the amount of carbon dioxide absorbed and emitted per unit mass of amine-containing dry gel particles in a gas absorber, which uses a stainless steel plate with a thickness of 0.1 mm or 0.3 mm as a support and carries a gel particle film made of amine-containing gel particles. [Figure 13] This graph shows the time-dependent changes in the amount of carbon dioxide absorbed and emitted per unit mass of amine-containing dry gel particles in a gas absorber, which uses a 0.1 mm thick stainless steel sheet, iron sheet, or graphite sheet as a support and carries a gel particle film made of amine-containing gel particles. [Figure 14] This graph shows the time-dependent changes in the amount of carbon dioxide absorbed and emitted per unit reactor volume when the thickness of the gel in a gas absorber, which uses a 0.1 mm thick graphite sheet as a support and carries a gel particle film made of amine-containing gel particles, is varied. [Figure 15] These are schematic diagrams, perspective views (photographs), and top views (photographs) showing other reactors used to evaluate the gas absorption and release performance of the gas absorber. [Figure 16]This graph shows the time course of carbon dioxide absorption and emission per fiber aggregate volume for various gas absorbers using fiber aggregates as a carrier, with varying amounts of amine-containing dry gel particles (100, 200, and 400 mg) loaded (water addition amounts of 0.4, 0.8, and 1.6 mL, respectively). [Figure 17] This graph shows the time-dependent changes in carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles for various gas absorbers using a fiber aggregate as a carrier, with varying amounts of amine-containing dry gel particles (100, 200, and 400 mg, respectively) and water added (0.4, 0.8, and 1.6 mL, respectively). [Figure 18] This graph shows the time course of carbon dioxide absorption and emission per fiber aggregate volume for various gas absorbers, where the water content of the gel particle membrane (containing amine-containing dry gel particles, 200 mg) differs between 0.4 mL and 0.8 mL. [Figure 19] This graph shows the time course of carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles in various gas absorbers, where the water content of the gel particle membrane (200 mg of amine-containing dry gel particles supported on a fiber aggregate) differs between 0.4 mL and 0.8 mL. [Figure 20] This graph shows the time-dependent changes in the amount of carbon dioxide absorbed and emitted per unit volume of fiber aggregates used as carriers, with fiber diameters of 12 μm and 100 μm for gas absorbers. [Figure 21] This graph shows the time course of carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles in gas absorbers with fiber diameters of 12 μm and 100 μm, using fiber aggregates as carriers. [Figure 22] This graph shows the time-dependent changes in the amount of carbon dioxide absorbed and emitted per unit volume of fiber aggregates used as carriers, with fiber diameters of 8 μm and 12 μm for gas absorbers. [Figure 23]This graph shows the time course of carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles in gas absorbers with fiber diameters of 8 μm and 12 μm, used as a carrier. [Figure 24] This graph shows the time-dependent changes in carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles when a gas absorbent consisting of a gel particle membrane made of amine-containing gel particles supported on a carrier made of a fiber aggregate is placed inside a reaction vessel, and when the same amount of gel particle membrane made of amine-containing gel particles is directly placed inside the same reaction vessel. [Figure 25] This graph shows the relationship between gel packing density and carbon dioxide emission and absorption when using metal fibers and sintered metal fibers. [Figure 26] This graph shows the time-dependent changes in carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles when using sintered metal fibers, foamed metal, and sintered nickel fibers. [Figure 27] This graph shows the time course of carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles in a gas absorber supported by a gel particle film made of amine-containing gel particles from Synthesis Example 1. [Figure 28] This graph shows the change in vapor pressure with temperature as a gas absorber supporting a gel particle film made of amine-containing gel particles from Synthesis Example 1 is subjected to temperature changes. [Figure 29] This graph shows the time course of carbon dioxide emission per unit mass of amine-containing dry gel particles in a gas absorber, which is a gel particle membrane composed of amine-containing gel particles to which a polyvinyl alcohol / polyethylene copolymer has been added. [Figure 30] This graph shows the time course of carbon dioxide absorption per unit mass of amine-containing dry gel particles in a gas absorber, which is a gel particle membrane composed of amine-containing gel particles to which a polyvinyl alcohol / polyethylene copolymer has been added. [Figure 31] This photograph shows the changes that occur when a film formed from a solution containing a stabilizer and amine-containing dry gel particles is heat-treated. The solution was prepared by adding a titanium-based crosslinking agent solution to the solution. [Figure 32]This graph shows the time-dependent changes in the amount of carbon dioxide absorbed and emitted per unit mass of amine-containing dry gel particles in a gas absorber, which is a gel particle membrane composed of amine-containing gel particles to which polyvinyl alcohol / polyethylene copolymer and titanium crosslinking agent have been added. [Figure 33] This graph shows the time course of carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles in a gas absorber obtained by polymerizing a methanol solution of amine-containing gel particles with a polymerizable compound (DMAPM:BIS=95:5). [Figure 34] This graph shows the time course of carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles in a gas absorber obtained by polymerizing a methanol solution of amine-containing gel particles with a polymerizable compound (DMAPM:BIS:NIPAM = 55:5:45). [Figure 35] This graph shows the time course of carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles in a gas absorber obtained by polymerizing a methanol solution of amine-containing gel particles with a polymerizable compound (DMAPM:BIS:NIPAM = 30:5:65). [Figure 36] This graph shows the time course of carbon dioxide absorption and emission per unit mass of amine-containing dry gel particles in a gas absorber obtained by polymerizing an aqueous solution of amine-containing gel particles with a polymerizable compound (DMAPM:BIS=95:5). [Figure 37] This graph shows the time course of carbon dioxide emission from a gas absorber, which is a gel particle film composed of amine-containing gel particles to which various amines have been added. [Figure 38] This graph shows the time course of carbon dioxide absorption by a gas absorber in which various amines are added to a gel particle membrane composed of amine-containing gel particles. [Figure 39] This graph shows the time course of carbon dioxide emission from a gas absorber, which is a gel particle film composed of amine-containing gel particles to which various amines have been added. [Figure 40] This graph shows the time course of carbon dioxide absorption by a gas absorber in which various amines are added to a gel particle membrane composed of amine-containing gel particles. [Figure 41] This graph shows the time course of carbon dioxide emission from a gas absorber in a gel particle membrane to which amine-containing dried gel particles have been added aqueous solutions of PMDETA at various concentrations (equivalent to amine concentrations of 0M, 1M, 3M, and 10M) or PMDETA containing almost no water. [Figure 42] This graph shows the time-dependent change in carbon dioxide absorption of a gas absorber in a gel-like membrane, where amine-containing dried gel particles are mixed with aqueous solutions of PMDETA at various concentrations (equivalent to amine concentrations of 0M, 1M, 3M, and 10M) or PMDETA containing almost no water. [Figure 43] This graph shows the amount of carbon dioxide emitted from a gas absorber in a gel-like film formed by adding a 3N amine aqueous solution to amine-containing dried gel particles. [Figure 44] This graph shows the amount of carbon dioxide emitted from a gas absorber in a gel-like film formed by adding 3N, 6N, and 8N amine aqueous solutions to amine-containing dried gel particles. [Modes for carrying out the invention]
[0016] The present invention will be described in detail below. The following descriptions of constituent elements may be based on representative embodiments or specific examples, but the present invention is not limited to such embodiments. In this specification, numerical ranges represented by "~" mean a range that includes the numbers written before and after "~" as the lower and upper limits. In this specification, "(meth)acrylamide" means "acrylamide" and "methacrylamide".
[0017] <Gas absorbent material> The gas-absorbing material of the present invention contains polymer compound particles having amino groups. Polymer compound particles containing amino groups change in swelling, internal structure, or the acid dissociation constant of the amino groups when subjected to small temperature changes. This change alters the gas absorption capacity. As a result, this gas-absorbing material can switch between absorbing and releasing gases. This switching between the two states is presumed to be achieved by the mechanism described below. In the following explanation, when a specific gas contained in the gas being treated is absorbed and released, that specific gas may be referred to as the "target gas." First, when a gas is brought into contact with polymer compound particles containing amino groups at a specific temperature, anions from the gas and the amino groups of the polymer compound particles form a salt, and the polymer compound particles reversibly absorb the gas. When the polymer compound particles are heated from this state, even a slight increase in temperature changes the degree of swelling of the particles, the internal structure, or the acid dissociation constant of the amino groups. This change makes the polymer compound particles more likely to release gas. As a result, gas is released from the polymer compound particles, and amino groups are regenerated in the polymer compound. If the polymer compound particles with regenerated amino groups are then repeatedly cooled and heated to a specific temperature, the cycle of gas absorption and release is repeated through the same mechanism as described above. The gas-absorbing material of the present invention can be effectively used as a material for a gas absorber that absorbs and releases gas, and can also reduce the amount of heat required for gas release, because the polymer compound particles having amino groups possess these functions. Furthermore, in the gas-absorbing material of the present invention, since the polymer compound having amino groups is in the form of particles, when a deposited film on which these particles are deposited is exposed to the gas to be treated, the gas is absorbed at the surface of the deposited film, and then the absorbed carbon dioxide molecules and bicarbonate ions rapidly diffuse into the interior of the film through the voids between the particles. Also, when the absorbed target gas is released, carbon dioxide molecules and bicarbonate ions rapidly diffuse through the voids between the particles, and the target gas is released from the surface of the deposited film and also from the interior of the deposited film, creating a gas phase in the voids between the particles. For this reason, a gas absorbent formed using this gas-absorbing material has a larger reversible gas absorption capacity per unit volume compared to a homogeneous gas absorbent without voids, and can absorb and release gas at high speeds.
[0018] In the gas-absorbing material of the present invention, the gas to be absorbed and released is not particularly limited, but it is preferably an acidic gas such as carbon dioxide or hydrogen sulfide, and more preferably carbon dioxide, because it can be easily absorbed by the polymer compound particles by forming a salt with the amino groups of the particles. Because the gas-absorbing material of the present invention can efficiently perform reversible absorption and release of gas through the mechanism described above, it can be effectively used for the separation and recovery of acidic gases such as carbon dioxide and hydrogen sulfide, and is particularly suitable for the separation and recovery of carbon dioxide, which has a large emission volume. Furthermore, unlike adsorbents, the gas-absorbing material of the present invention can absorb large amounts of acidic gas even when a high concentration of water vapor is present in the gas. For this reason, for example, when treating a gas containing water vapor and carbon dioxide, carbon dioxide can be directly separated and recovered without having to remove the water vapor beforehand, thereby simplifying the process required for treating the gas. The following describes in detail the polymer compound particles having amino groups used in the gas-absorbing material of the present invention.
[0019] (Chemical structure and preparation of polymer compound particles containing amino groups) The polymer compound particles having amino groups are particles made of polymer compounds having amino groups, and it is preferable that they consist only of polymer compounds having amino groups, but they may also contain materials used in preparing the particles, such as particle size adjusting components such as surfactants, crosslinking agents, unreacted monomers, etc.
[0020] The polymer compounds having amino groups are not particularly limited, but examples include (meth)acrylamide polymers and their derivatives, polyethyleneimines and their derivatives, polyvinyl alcohols and their derivatives, polyallylamines and their derivatives, and the like. Specific constituent monomers include N,N-dimethylaminopropyl methacrylamide, N,N-diethylaminopropyl methacrylamide, N,N-dimethylaminoethyl methacrylamide, N,N-diethylaminoethyl methacrylamide, N,N-dimethylaminopropyl methacrylate, N,N-diethylaminopropyl methacrylate, N,N-dimethylaminoethyl methacrylate, N,N-diethylaminoethyl methacrylate, N,N-dimethylaminopropyl acrylamide, N,N-diethylaminopropyl acrylamide, N,N-diethylaminoethyl acrylamide, N,N-diethylaminoethyl acrylamide, 3-aminopropyl methacrylamide hydrochloride, 3-aminopropyl acrylamide hydrochloride, N,N-dimethylaminopropyl acrylate, N,N-diethylaminopropyl acrylate, N,N-dimethylaminoethyl acrylate, N,N-diethylaminoethyl acrylate, 3-aminopropyl methacrylate hydrochloride, 3-aminopropyl acrylate hydrochloride, etc., and it is preferable that they are acrylamide polymers. The amino groups in the polymer compound having amino groups may be primary, secondary, or tertiary amino groups, but it is preferable that the acid dissociation constant of their conjugate acid changes in response to stimuli such as temperature changes. In particular, it is preferable that the acid dissociation constant when absorbing carbon dioxide is equal to or greater than that of carbonic acid, and the acid dissociation constant when releasing carbon dioxide is equal to or smaller than that of carbonic acid. Among these, tertiary amino groups are preferred because they allow for high efficiency in releasing acidic gases, and dialkylamino groups such as dimethylamino groups are more preferred. Furthermore, the amino groups in the polymer compound may be bonded to the main chain or to the side chains, but it is preferable that they are bonded to the side chains.
[0021] Furthermore, it is preferable that the polymer compound having an amino group also has a hydrophobic group. This causes the polymer compound particles to undergo a significant change in swelling and internal structure (phase transition) in response to temperature changes, enabling efficient absorption and release of gases such as carbon dioxide in response to temperature changes. Below, the phase transition of polymer compound particles having an amino group and a hydrophobic group will be explained using the case of absorption and release of carbon dioxide as the target gas as an example. Figure 1 is a schematic diagram showing the absorption and release cycle of carbon dioxide gas when the polymer compound particles having an amino group and a hydrophobic group are hydrogel particles. As shown in the upper left of Figure 1, at low temperatures, these gel particles have no steric hindrance around the amino groups, and the amino groups are in a state where they readily absorb acidic gas (high basicity). When a gas to be treated containing carbon dioxide gas is brought into contact with these gel particles, nucleophilic attack of hydroxy anions on carbon dioxide generates bicarbonate anions, and one molecule of this bicarbonate anion forms a salt with one amino group. As a result, the gel particles enter a state of having absorbed carbon dioxide gas. At the same time, the pH of water decreases, causing the gel particles to swell. When the gel particles are heated from this state, the hydrophobic interaction within the molecules increases, causing the gel particles to shrink (undergo phase transition). As a result, the periphery of the amino groups is covered with low-polarity polymer chains, increasing the steric hindrance, and the amino groups enter a state where they readily release acidic gas (low basicity). Thereby, carbon dioxide gas is released, and at the same time, the pH of water rises. Next, when the gel particles are cooled, the pH of water further increases, and the gel particles swell to return to the initial state. As described above, the gel particles of the polymer compound having amino groups and hydrophobic groups can be switched from a state of absorbing acidic gas to a state of releasing acidic gas with a slight temperature difference that causes a phase transition. Therefore, by using a gas absorbing material containing such gel particles, the amount of energy required for the acidic gas separation and recovery process can be reduced. As the hydrophobic group to be introduced into the polymer compound, C X H 2X or C X H 2X+1 hydrocarbon groups represented by can be cited, which are preferably methyl group, ethyl group, propyl group, isopropyl group, butyl group, isobutyl group, tert-butyl group, pentyl group, cyclopentyl group, isopentyl group, hexyl group, cyclohexyl group and the like. Among them, isobutyl group and tert-butyl group are more preferable. Alternatively, groups in which a hydroxyl group is bonded to the above hydrophobic group, such as hydroxyethyl group, hydroxypropyl group, and hydroxybutyl group, may be used.
[0022] The polymer compound having an amino group preferably has a polymer density of 0.3 to 80% in the dispersed state after the polymer compound particles are swollen in water, and more preferably 1 to 60%.
[0023] Polymeric compound particles having amino groups can be prepared using a solution containing monomer components (hereinafter referred to as "particle preparation solution"). In this specification, "monomer components" refers to all monomers used in the synthesis of the polymer of the polymeric compound particles having amino groups. The method for preparing the polymeric compound particles is not particularly limited, and conventionally known methods such as emulsion polymerization, dispersion polymerization, suspension polymerization, and seed polymerization can be used.
[0024] The monomer components used in preparing the particles preferably contain at least a monomer having an amino group, and more preferably both a monomer having an amino group and a monomer not having an amino group. That is, the polymer compound having an amino group may be a homopolymer or copolymer of monomers having an amino group, or it may be a copolymer of a monomer having an amino group and a monomer not having an amino group. By controlling the proportion of these monomers, the density of amino groups in the polymer compound particles can be adjusted to an appropriate range. The monomer having an amino group and the monomer not having an amino group, if used as needed, are preferably substituted (meth)acrylamide monomers, and more preferably substituted acrylamide monomers.
[0025] For a description of the amino groups in monomers having amino groups and their preferred ranges, refer to the description of the amino groups in polymer compounds having amino groups. The number of amino groups in a monomer is not particularly limited and may be one or two or more. If a monomer has two or more amino groups, each amino group may be the same or different. The monomer having an amino group is not particularly limited, but examples include N-(aminoalkyl)acrylamide and N-(aminoalkyl)methacrylamide, and N-(aminoalkyl)acrylamide is preferred.
[0026] The monomer component preferably includes a monomer having a hydrophobic group along with a monomer having an amino group. For a description of the hydrophobic group and its preferred range, refer to the description of the hydrophobic group and its preferred range that can be used in polymer compounds having an amino group. The hydrophobic group is preferably located at the terminal. The monomer having a hydrophobic group may or may not have an amino group. The monomer having a hydrophobic group is not particularly limited, but examples include N-alkylacrylamide, N-alkylmethacrylamide, N-alkyl acrylate, N-alkyl methacrylate, N,N-dialkylacrylamide, N-(hydroxyalkyl)methacrylamide, N,N-dialkyl acrylate, N-(hydroxyalkyl)methacrylate, N,N-dialkylmethacrylamide, N-(hydroxyalkyl)acrylamide, N,N-dialkyl methacrylate, and N-(hydroxyalkyl)acrylate, with N-alkylacrylamide being preferred.
[0027] A preferred combination of monomers having an amino group and monomers having a hydrophobic group is the combination of N-(aminoalkyl)(meth)acrylamide and N-alkyl(meth)acrylamide, with the combination of N-(aminoalkyl)methacrylamide and N-alkylacrylamide being preferred. In the copolymer of N-(aminoalkyl)(meth)acrylamide and N-alkyl(meth)acrylamide, the hydrophobic alkyl group and the hydrogen-bonding amide are evenly and balanced within the molecule. Therefore, at low temperatures, it readily dissolves in water and forms swollen gel particles that efficiently absorb the gas contained in the gas to be treated. When heated after absorbing gas, the gel particles contract with only a slight increase in temperature, significantly reducing their gas absorption capacity and efficiently releasing the gas. Therefore, by using particles made of this copolymer as a gas absorbent material, gas absorption and release can be performed at high speed, and the amount of heat required for gas release can be kept low. Furthermore, the gel particles of this copolymer are less likely to precipitate even when heated above the phase transition temperature, and can maintain very stable solution properties.
[0028] The proportion of monomers having amino groups in the monomer component is preferably 5 to 95 mol%, more preferably 30 to 70 mol%, and even more preferably 50 to 65 mol% relative to the total number of moles of the monomer component. Furthermore, if the monomer component includes monomers having hydrophobic groups, the molar ratio of monomers having amino groups to monomers having hydrophobic groups is preferably 95:5 to 5:95, and more preferably 2:1 to 1:2. Monomers having both amino groups and hydrophobic groups are classified as monomers having amino groups. The ability of polymer compounds to absorb acidic gases tends to increase as the number of amino groups increases, but if there are too many amino groups, the electrical repulsion between the amino groups makes it difficult for the particles to shrink at high temperatures and for acidic gases to be released. By setting the proportion of monomers having amino groups and the molar ratio of monomers having amino groups to monomers having hydrophobic groups within the above ranges, polymer compound particles can be obtained in which a phase transition easily occurs upon heating and acidic gases are efficiently released.
[0029] The particle preparation solution may contain only monomer components or may contain other components. Examples of other components include surfactants, crosslinking agents, and polymerization initiators. By using surfactants, the particle size of the resulting polymer compound particles can be controlled by changing their concentration in the particle preparation solution. Furthermore, by using crosslinking agents, the swelling properties of the particles can be controlled to prevent excessive swelling by forming crosslinked structures within the polymer compound. Additionally, by using a relatively large amount of crosslinking agent or by setting a relatively high monomer concentration during polymerization, crosslinked structures can be formed between the particles themselves. This creates a relatively large continuous void structure between the composite particles linked by the crosslinked structure, promoting gas absorption and release. As the surfactant, cationic surfactants such as cetyltrimethylammonium bromide can be used. The crosslinking agent can be any agent capable of forming a crosslinked structure between the monomers used, and N,N'-alkylenebisacrylamide is preferably used. The number of carbon atoms in the alkylene group of N,N'-alkylenebisacrylamide is not particularly limited, but is preferably 1 to 12, more preferably 1 to 4, and even more preferably 1 to 2. Instead of the alkylene group, the crosslinking agent may be one in which oligoethyleneimine or oligoethylene glycol functions as the crosslinking agent chain.
[0030] The solvent for the particle preparation solution is not particularly limited, but examples of polar solvents include water, methanol, ethanol, isopropanol, acetonitrile, N,N-dimethylformamide, and dimethyl sulfoxide. A mixed solvent may also be a combination of two or more of these polar solvents. In particular, it is preferable to use water or a mixed solvent of water and another polar solvent.
[0031] (Properties of polymer compound particles containing amino groups) The polymer compound particles containing amino groups may be gel particles swollen with a liquid or dry particles (solid particles), but gel particles are preferred. In gel particles, the gas dissolves in the liquid contained within the gel particles, allowing the amino groups inside the gel particles to contribute to gas absorption. This makes it possible to obtain a large reversible absorption amount for the gas.
[0032] The polymer compound particles preferably have a particle size of 5 nm to 10 μm in their dry state. The hydrodynamic particle size of polymer compound particles after swelling in water is preferably 10 nm to tens of μm, more preferably 10 nm to 50 μm, and even more preferably 20 nm to 10 μm, as measured by dynamic light scattering. The "particle size after swelling in water" of polymer compound particles refers to the particle size after immersing dried polymer compound particles in water for 24 hours, and is the average particle size measured by dynamic light scattering. By ensuring that the particle size of the polymer compound particles during drying and after swelling are within the above range, the reversible absorption amount of gas per unit volume, the absorption rate of gas, and the emission rate of gas can be sufficiently increased.
[0033] The liquid contained in the gel particles is not particularly limited, but examples include polar solvents such as water, methanol, ethanol, isopropanol, acetonitrile, N,N-dimethylformamide, and dimethyl sulfoxide, and may also be a mixed solvent of two or more of these polar solvents. In particular, it is preferable to use water or a mixed solvent of water and another polar solvent. That is, it is preferable that the gel particles are hydrogel particles. Because the gel particles are hydrogel particles, gas can be efficiently dissolved within the particles, and a larger volume of gas can be reversibly absorbed. The water content in the gel particles is preferably 0.1 mL or more per gram of solids, more preferably 0.5 mL or more, and even more preferably 1 mL or more. Furthermore, the water content in the gel particles is preferably 20 mL or less, more preferably 10 mL or less, and even more preferably 8 mL or less. By setting the water content of the gel particles within the above range, excessive swelling of the gel particles is suppressed, and the gas can be sufficiently dissolved within the gel particles, thereby increasing the amount of gas absorbed and released.
[0034] The polymer compound particles having amino groups used in the present invention preferably change their gas absorption capacity in response to stimuli such as temperature changes. Factors that change the gas absorption capacity include changes in the acid dissociation constant of the functional group, changes in stereostructure, changes in swelling degree, changes in hydrophilicity, changes in water content, changes in bicarbonate ion solubility, and changes in hydrogen sulfide ion solubility. The gas absorption capacity of the polymer compound particles having amino groups may change due to any of these factors, but it is preferable that the gas absorption capacity changes due to a change in the acid dissociation constant of the ammonium ion, which is the conjugate acid of the amino group, in response to temperature changes. In particular, it is preferable that the change in the acid dissociation constant is caused by swelling and shrinking of the gel (volume phase transition) in response to temperature changes, or by a coil-globule structure transition or hydrophilic / hydrophobic change of the polymer in response to temperature changes. As a result, the gas absorption capacity of the polymer compound particles can be greatly changed with small temperature changes through the mechanism shown in Figure 1, and the amount of energy required for gas absorption and dissipation can be reduced.
[0035] The phase transition temperature of polymer compound particles is preferably 10 to 95°C, more preferably 20 to 90°C, and even more preferably 30 to 80°C. In this specification, "phase transition temperature" means the temperature at which the acid dissociation constant of the ammonium ion, which is the conjugate acid of the amino group, becomes equal to or smaller than the acid dissociation constant of carbonic acid, or the temperature at which the particle size of the polymer compound particles in water becomes 30% or more smaller than the particle size at 5°C. This phase transition temperature can be determined by immersing the polymer compound particles in water at 5°C and, while raising the water temperature from 15°C, sequentially or continuously measuring the pH or particle size of the aqueous solution of the polymer compound particles at regular temperature intervals. The particle size of the polymer compound particles can be measured by dynamic light scattering.
[0036] <Gas absorber> The gas absorber of the present invention comprises a gel particle membrane of a polymer compound having amino groups, and a carrier that supports the gel particle membrane. The gel particle membrane used in this invention is a membrane containing gel particles obtained by swelling solid particles of a polymer compound having amino groups with water. Confirmation that it is a gel particle membrane can be made visible by adding fluorescently modified gel particles and observing it with a focused laser microscope. Fluorescence modification of the gel particles can be performed by introducing 4-Acrylamidofluorescein, etc. The gel particle film may be a deposited film of particles in which gel particles are deposited in layers on a carrier, or it may be a film in which gel particles are embedded between the fibers or in the pores of the carrier to form layers. For a description of polymer compounds having amino groups and their gel particles and preferred ranges, refer to the description of polymer compounds having amino groups and their gel particles in gas absorbent materials and preferred ranges.
[0037] This gel particle film can be formed, for example, by coating a particle solution obtained by dissolving amino group-containing polymer compound particles in a polar solvent onto a support, drying it to form a film of solid polymer compound particles, and then adding water to this film of polymer compound particles to cause swelling. In this case, a polymerizable compound and a polymerization initiator may be added to the particle solution, the polymerizable compound may be polymerized after coating and drying, and then water may be added to cause swelling. For the polymerizable compound to be added, refer to the description of the stabilizer described later. The polymerization initiator can be any agent that can initiate the polymerization of the polymerizable compound, and may be a photopolymerization initiator or a thermal polymerization initiator. A photopolymerization initiator is preferred. When a photopolymerization initiator is used, polymerization is initiated by irradiation with active energy rays such as ultraviolet light. By performing polymerization in this manner, a gel particle film that is highly stable and does not swell excessively can be produced. As the polar solvent for the particle solution, any of the polar solvents exemplified above for inclusion in the gel particles can be used, and among them, water or a mixed solvent of water and another polar solvent is preferred. The water content in the gel particle film is preferably 10% by mass or more, and more preferably 50 to 2000% by mass, relative to the total amount of the gel particle film. The thickness of the gel particle film is not particularly limited, but is preferably 1 to 1000 μm, more preferably 10 to 600 μm, and even more preferably 20 to 400 μm. By setting the thickness of the gel particle film within the above range, the reversible absorption amount of gas per unit volume can be made sufficient, and gas absorption and dissipation can be performed at high speed. In the case where the gel particles form a layer by being embedded between the fibers constituting the carrier or in the pores, the thickness of the gel particle layer on the fiber surface or pore surface corresponds to the thickness of the gel particle film.
[0038] The gel particle film has a carbon dioxide gas emission rate of 0.1 mmol / m³. 2 Preferably, it is 0.15 mmol / m³ or more. 2 It is more preferable that the value be 0.2 mmol / m³ or higher. 2It is even more preferable that the absorption rate be 0.05 mmol / m³ or higher. 2 Preferably, it is 0.1 mmol / m³ or more. 2 It is more preferable that the value be 0.2 mmol / m³ or higher. 2 It is even more preferable that the value be greater than or equal to / sec. In this specification, the "carbon dioxide gas absorption rate of the gel particle membrane" is determined by measuring the amount of carbon dioxide in the outlet gas when nitrogen gas (mixed gas) containing 10% carbon dioxide (10%) is humidified at 60°C and passed through the surface of the gel particle membrane using gas chromatography or an infrared carbon dioxide concentration meter. Furthermore, the above emission rate and absorption rate are results obtained for a gel particle membrane with 5 mol% DMAPM introduced, and will be even higher when the amount of DMAPM is increased or when an accelerator is added.
[0039] [Components other than polymer compound particles containing amino groups] The gel particle film may contain polymer compounds other than polymer compounds having amino groups, as well as additives. While polymer compounds other than those containing amino groups are not particularly limited, it is preferable that they are polymer compounds that react to stimuli such as temperature changes. Examples of reactions to stimuli include changes in the acid dissociation constant of functional groups, changes in stereostructure, changes in swelling degree, changes in hydrophilicity, changes in water content, changes in bicarbonate ion solubility, and changes in hydrogen sulfide ion solubility.
[0040] Examples of additives include membrane stabilizers, absorption enhancers, and release enhancers. Examples of film stabilizers include polymer compounds, polymerizable molecules (polymerizable compounds), crosslinking agents such as titanium crosslinking agents, primary amines, secondary amines, etc. Among these, polymer compounds that can be preferably used include polymer compounds having primary amino groups such as polyvinylamine, polymer compounds having secondary amino groups, polymer compounds having tertiary amino groups, polymer compounds having multiple types of primary, secondary, and tertiary amino groups, polyvinyl alcohol, polyethylene, polyvinyl alcohol / polyethylene copolymers, etc. Furthermore, when polymerizable molecules are used as membrane stabilizers, the polymer compounds produced by the polymerization reaction of these molecules within the gel particle membrane also function as membrane stabilizers. This makes it easier to maintain a uniform membrane structure without excessive swelling even after water is added after membrane formation or after gas absorption and release. Polymerizable molecules include monomers having polymerizable groups, such as acrylic monomers. Among these, acrylamide or acrylamide derivatives are preferably used. For example, alkylacrylamide, substituted or unsubstituted aminoalkylacrylamide, and acrylamide derivatives having two polymerizable groups can be cited, and among these, substituted aminoalkylacrylamide and acrylamide derivatives having two polymerizable groups are preferably used. It is preferable to use substituted aminoalkylacrylamide and acrylamide derivatives having two polymerizable groups in combination, with a mole fraction of 60-99:40-1 being preferred, more preferably 80-99:20-1, and even more preferably 90-99:10-1. Specific examples of monomers having polymerizable groups include N-isopropylacrylamide (NIPAM), tert-butylacrylamide (TBAM), N,N-dimethylaminopropyl methacrylamide (DMAPM), N,N'-methylenebisacrylamide (BIS), and acrylamide. These polymerizable compounds may be used individually or in combination of two or more. When using two or more in combination, a preferred example is the combination of N,N-dimethylaminopropyl methacrylamide (DMAPM) and N,N'-methylenebisacrylamide (BIS). The content of the membrane stabilizer in the gel particle membrane is preferably 1 to 89% by mass relative to the total amount of the gel particle membrane.
[0041] Absorption accelerators are compounds that have the function of promoting the absorption of acidic gases into the gel particle membrane. Desorption accelerators are compounds that have the function of promoting the desorption of acidic gases from polymer compound particles. In the present invention, it is preferable to use an absorption-desorption accelerator that has both the functions of an absorption accelerator and a desorption accelerator. These absorption accelerators, desorption accelerators, and absorption-desorption accelerators may also have the function of membrane stabilizers. The total content of the absorption accelerator, desorption accelerator, and absorption-desorption accelerator in the gel particle membrane is preferably 1 to 20% by mass relative to the total amount of the gel particle membrane. The content of the absorption accelerator in the gel particle membrane is preferably 0.1 to 12 N in terms of amine concentration, more preferably 1 to 10 N, and even more preferably 3 to 9 N. Low molecular weight amines can preferably be used as absorption enhancers, release enhancers, and absorption / release enhancers. The molecular weight of the low molecular weight amine is preferably 61 to 10000, more preferably 75 to 1000, and even more preferably 90 to 500. The boiling point of the low molecular weight amine is preferably 80°C or higher, more preferably 120°C or higher, and even more preferably 150°C or higher, as this is practical and allows for repeated use.
[0042] Low molecular weight amines may contain primary, secondary, or tertiary amino groups, and may contain multiple amino groups, preferably 1 to 3. Secondary and tertiary amino groups may also be cyclic amino groups. Furthermore, low molecular weight amines may contain functional groups other than amino groups, such as hydroxyl groups. It is preferable that low molecular weight amines contain 0 to 2 hydroxyl groups. Examples of preferred low molecular weight amines include amines having an amino group and a hydroxyl group, or amines having three amino groups. Examples of more preferred low molecular weight amines include amines having a secondary amino group and a hydroxyl group. Amines having a secondary amino group and a hydroxyl group with a boiling point of 150°C or higher are particularly preferred because they can dramatically increase the amount of acidic gas released, especially in the high concentration range, and are suitable for repeated use. Examples of low molecular weight amines include specific compounds represented by the following formula. Furthermore, the absorption and release enhancer used in Example (9) can also be preferably used.
[0043] [ka]
[0044] Of these, DMAE, IPAE, Bis(2DMAE)ER, 1-2HE-PRLD, 1-2HE-PP, TM-1,4-DAB, TMHAD, and PMDETA are particularly preferred because they can release a large amount of acidic gas. Among these, IPAE, Bis(2DMAE)ER, 1-2HE-PP, TM-1,4-DAB, TMHAD, and PMDETA are more preferred because they have relatively high boiling points and do not evaporate easily. IPAE, TM-1,4-DAB, TMHAD, and PMDETA are even more preferred because their concentration can significantly increase the amount of acidic gas released. IPAE, TMHAD, and PMDETA are particularly preferred because they are readily available. Furthermore, IPAE is most preferred because it can dramatically increase the amount of acidic gas released, especially in the high-concentration range, and can significantly increase the amount of acidic gas released even when the amount of water relative to the amine is small. The additives described above may be used individually or in combination of two or more types.
[0045] The gel particle film constructed as described above reversibly absorbs gas under certain conditions, releases the gas in response to stimuli such as temperature changes, and then reversibly absorbs the gas again by returning to the aforementioned conditions or by applying other stimuli. Examples of gases that the gel particle film reversibly absorbs include acidic gases such as carbon dioxide and hydrogen sulfide, and water vapor.
[0046] [carrier] The gas absorber of the present invention is also characterized in that the gel particle film is held on a support. Gel-like films have lower fluidity compared to liquids, making convection less likely. Therefore, in the absorption process of acidic gases in gel-like films, the diffusion of ions becomes the rate-limiting step. Furthermore, ion diffusion to depths of several hundred micrometers or more from the film surface is restricted, and consequently, the amount of acidic gas that a gel-like film can absorb is also limited. In contrast, when the gel particle film is supported on a suitable carrier, as described above, diffusion of the gas to be treated into the film and diffusion of acidic gas from within the film are achieved through the voids between the particles. Furthermore, heat is efficiently transferred to the gel particle film via the carrier, so the temperature of the entire gel particle film changes responsively to changes in the external temperature. In addition, by stacking carriers, a large amount of gel particle film with a thickness of several hundred μm or less can be packed into a reactor of a fixed volume. As a result, the absorption and emission rates of acidic gases and water vapor gases increase, and acidic gases diffuse to the depths of the film, resulting in a large gas absorption capacity. Moreover, being supported on a carrier makes the gel particle film less prone to collapse, allowing the shape of the gel particle film to be stably maintained. Furthermore, a large amount of gas can be reversibly absorbed in a reactor of a fixed volume.
[0047] Thin plates or fiber aggregates can be used as carriers. In this invention, "thin plate" refers to a flat plate, sheet, or foil with a thickness of 2 mm or less and 5 μm or more. The thin sheet material has a constant-pressure specific heat of 2500 kJ / (m²). 3 It is preferable that the temperature is 10 W / (mK) or less, and it is also preferable that the thermal conductivity is 10 W / (mK) or more. A thin plate having such thermal properties can change temperature responsively in response to external temperature changes and efficiently transmit that temperature change throughout the gel particle film. In this specification, "specific heat at constant pressure" refers to a value measured by a calorimeter such as a hydrometer or differential scanning calorimeter. "Thermal conductivity" refers to a value measured by the laser flash method or the steady-state heat flow method.
[0048] As thin sheets, metal sheets (metal foils), sheets made of carbon materials, carbon sheets, resin films (polymer compound films), etc., can be used. Examples of sheets made of carbon materials include graphite sheets, and examples of resin films include polyethylene, polypropylene, PET, polyimide, etc. As thin sheets, aluminum sheets, iron sheets, or graphite sheets are preferred due to their high thermal conductivity. Alternatively, as thin sheets, aluminum sheets, graphite sheets, or resin films are preferred due to their low specific heat. Furthermore, as metal sheets, examples include stainless steel sheets, iron sheets, aluminum sheets, or nickel sheets. Of these, iron sheets, aluminum sheets, and nickel sheets are preferred due to their relatively high thermal conductivity, and nickel sheets are more preferred.
[0049] The thin plate may be a plate with a homogeneous internal structure, or it may be a porous material or a honeycomb structure. In the case of a porous material or honeycomb structure, a gel particle film can be filled into its pores, allowing heat from the thin plate to be easily transferred to the gel particle film, thereby improving the responsiveness of the gas absorber to temperature changes. In particular, porous materials such as foamed metal, foamed nickel, and porous carbon have high heat transfer properties to the gel particle film, and by using these as carriers, the responsiveness of the gas absorber to temperature changes can be greatly improved. The pore size of porous materials such as foamed metal is preferably 0.1 to 10 mm, and more preferably 0.4 to 4 mm. The specific surface area is 100 to 10000 m². 2 / m 3 Preferably, it is 200-6000m 2 / m 3 It is more preferable that the material behaves as described above. Furthermore, if a porous support made of porous resin or porous carbon is used as the porous support, the heat capacity is small, which can improve the thermal efficiency of the absorber. The porous material used as the support preferably has a porosity of 1 to 99%, more preferably 10 to 99%, and even more preferably 20 to 95%. In this specification, "porosity of a sheet" means the porosity measured by the apparent volume and mass of the sheet and the density of the material. Furthermore, the carrier may be a laminate formed by stacking multiple of these thin plates. In the laminate, each thin plate may be the same, or multiple thin plates with different materials and thicknesses may be combined.
[0050] A fiber aggregate is made by processing a large number of fibers into a thin, wide plate. Examples of fiber aggregates include cloth and paper, and among these, porous materials such as filters are preferred. The cloth may be woven, felt, or nonwoven. Sintered metal fiber felt can also be preferably used as a carrier. This material has a shape in which the fibers, which are sintered fibers, are densely aggregated, and high heat transfer properties can be obtained. For example, sintered felt made from stainless steel fibers or sintered felt made from nickel fibers can be preferably used, and among these, sintered felt made from nickel fibers is particularly preferred. The fibers used in the fiber aggregate have a constant-pressure specific heat of 2500 kJ / (m²). 3 It is preferable that the temperature is 10 W / (mK) or less, and it is also preferable that the thermal conductivity is 10 W / (mK) or more. A fiber aggregate having such thermal properties can respond well to changes in external temperature, and can efficiently transmit these temperature changes throughout the gel-like film.
[0051] The fibers used in the fiber aggregate may be inorganic fibers, organic fibers, or composite fibers combining inorganic and organic fibers. Examples of inorganic fibers include stainless steel fibers, aluminum fibers, nickel fibers, and other metal fibers, as well as carbon fibers. Nickel fibers are preferred because they provide high heat transfer properties. As for organic fibers, natural fibers such as cotton and linen, and synthetic fibers such as rayon and polyester can all be used. The fiber diameter is not particularly limited, but is preferably 8 to 100 μm. This makes it possible to obtain a gel particle film with excellent gas absorption and release properties. Furthermore, the carrier may be an aggregate formed by stacking multiple layers of these fiber aggregates. In the aggregate, each fiber aggregate may be identical, or multiple fiber aggregates with different fiber types, fiber diameters, fiber densities, etc., may be combined. Alternatively, the carrier may be a laminate formed by stacking thin plates and fiber aggregates.
[0052] When a fiber aggregate is used as the carrier, the packing rate of the gel particle film is preferably 10 to 100%, more preferably 15 to 80%, and even more preferably 20 to 70%. The packing rate of the gel particle film referred to here is the occupancy rate of the gel particle film relative to the total volume of the gas absorber. This allows the gel particle film to efficiently absorb and release gas. In particular, if a sintered body is used, it is possible to maintain a high gas absorption and release capacity of the gel particle film even at a high packing rate. For example, it is possible to maintain a high gas absorption and release capacity even at a packing rate of 60% or more.
[0053] The shape of the carrier is not particularly limited and can be selected as appropriate depending on the application. Specific examples of carrier shapes include plate-like and cylindrical shapes, and the planar shape of the plate and the cross-sectional shape of the cylinder may be any of the following: polygonal shapes such as squares and rectangles, circular shapes, elliptical shapes, etc.
[0054] <Gas absorption method> The gas absorption method of the present invention is a method of absorbing gas into amino groups within a gel particle membrane. For a description of the gel particle membrane of a polymer compound having amino groups, refer to the description of the gel particle membrane in the <Gas Absorber> section above. When the amino groups inside the gel particle film come into contact with gas at a specific temperature, the acids derived from the gas react with the bases derived from the amino groups of each gel particle to form salts, thereby enabling efficient gas absorption. Furthermore, gas can be released from this gel particle film by increasing its temperature. Increasing the temperature of the gel particle film reduces the basicity inside the film. It also decreases the pKa of the conjugate acid of the amines within the gel particle film. In addition, the hydrophobic interactions between each gel particle increase, causing each gel particle to contract, i.e., a volume phase transition occurs in the gel particles, and the steric hindrance around the amino groups increases. As a result, gas is released from the gel particle film. Subsequently, lowering the temperature of the gel particle film increases the basicity inside the film. It also increases the pKa of the conjugate acid of the amines within the gel particle film. Furthermore, the particles swell again, and the gel particle film returns to its state before the phase transition. The gel particle film, having returned to a highly basic state, can absorb gas again. Subsequently, when the temperature is increased, it releases the absorbed gas through the same mechanism as described above. By repeatedly decreasing and increasing the temperature, the cycle of gas absorption and release is repeated in sync with the temperature. By repeatedly performing this gas absorption and release, it becomes possible to separate and recover specific gases even from large volumes of exhaust gas. For detailed mechanisms of the phase transition of gel particles and the absorption and emission of gases, please refer to Figure 1 and the explanation of Figure 1 in the section on <Gas Absorbing Materials>. For gas absorption and release to occur through this mechanism, it is important to raise the temperature of the gel particle film that has absorbed the gas until its basicity decreases. In particular, it is important to raise the temperature until the basicity is equal to or lower than that of carbonic acid's pKa. If this temperature increase is insufficient, the gas absorbed by the gel particle film cannot be sufficiently released, resulting in a decrease in the subsequent gas absorption rate, release rate, and reversible absorption amount. For example, if the gel particles are (meth)acrylamide polymer gel particles, the temperature of the gel particle film during gas absorption is preferably 1 to 60°C, and the temperature of the gel particle film during gas release is preferably 40 to 200°C.
[0055] <Applications of gas absorbers> As described above, the gas absorber of the present invention can absorb and release gases such as carbon dioxide at high speed and has a large gas absorption capacity, making it suitable for use as a gas absorber in acidic gas absorbers, acidic gas recovery devices, water vapor absorbers, and water vapor recovery devices. Furthermore, the gas absorber of the present invention can have its carrier function as both a heat transfer surface of a heat exchanger and the heat exchanger itself, and can be effectively applied to heat exchangers and heat recovery devices. In this case, for example, a gel-like film is provided on the surface of the carrier that functions as a heat transfer surface (the surface of the heat transfer surface).
[0056] In the following, as an example of an acidic gas recovery device to which the gas absorber of the present invention is applied, a first embodiment and a second embodiment of a carbon dioxide gas recovery device will be described. Figure 2 is a schematic diagram showing the carbon dioxide gas recovery device of the first embodiment, and Figure 3 is a schematic diagram showing the carbon dioxide gas recovery device of the second embodiment.
[0057] As shown in Figure 2, the carbon dioxide gas recovery device of the first embodiment has a heat exchanger 21, a desulfurizer 22, a cylindrical gas absorber 23, and first to third pipes 24, 25, and 26 connected to these parts. One end of the first pipe 24 is a gas inlet for introducing exhaust gas (gas to be treated), and the other end is connected to the desulfurizer 22. One end of the second pipe 25 is connected to the desulfurizer 22, and the other end is connected to one side of the gas absorber 23. The third pipe 26 has a circulation path 26a connected to one side and the other side of the gas absorber 23, and a branch path 26b that branches off from the circulation path 26a on one side of the gas absorber 23, with one end of the branch path 26b being a gas outlet for discharging the recovered carbon dioxide gas. Furthermore, the connecting portions of the second pipe 25 and the third pipe 26 on one side of the gas absorber 23 are provided on approximately the same diameter of the circular side surface, flanking the center. The heat exchanger 21 is connected to the middle section of the first pipe 24 and the middle section of the circulation path 26a, respectively. The gas absorber 23 is composed of the gas absorber of the present invention. In this embodiment, the gas absorber 23 has a carrier consisting of a cylindrical honeycomb rotor made by processing a fiber aggregate into a honeycomb shape, and a gel particle film supported on this carrier, and is configured to be continuously rotated with the center of the disc as the axis of rotation. When the operation of the carbon dioxide gas device is turned OFF, the gas absorber 23 is at a temperature similar to the ambient temperature.
[0058] To recover carbon dioxide gas from exhaust gas using this acid gas recovery device, the operation of each part is turned ON, and the high-temperature exhaust gas after dust collection is introduced from one end of the first pipe 24. The introduced exhaust gas passes through the first pipe 24 and is introduced into a desulfurizer 22 which has a cooling capacity to about 30°C. Here, the desulfurizer and the cooler may be separate devices. As the exhaust gas passes through the first pipe 24, some of the heat of the exhaust gas is transferred to the circulation path 26a of the third pipe 26 via the heat exchanger 21, and the gas in the circulation path 26a is heated to about 75°C. After the exhaust gas introduced into the desulfurizer 22 undergoes desulfurization treatment in the desulfurizer 22, it flows into the second pipe 25. The mixed gas that flows into the second pipe 25 has a temperature of about 30°C, and at around this temperature it is introduced into the gas absorber 23. In the gas absorber 23, because the temperature of the mixed gas is about 30°C, carbon dioxide is efficiently absorbed by the gel particle film in the region in contact with the mixed gas, and gases other than carbon dioxide are discharged to the outside of the gas absorber 23. Meanwhile, the region of the gas absorber 23 that has absorbed carbon dioxide moves to the vicinity of the connection point of the third pipe 26 due to the rotation of the gas absorber 23, and comes into contact with the gas introduced from the circulation path 26a of the third pipe 26. Since the gas introduced from the circulation path 26a is heated to about 75°C by heat exchange with the exhaust gas, the gel particle film in the region of the gas absorber 23 that comes into contact with this gas undergoes a phase transition and carbon dioxide gas is released. A portion of the released carbon dioxide gas flows into the branch path 26b of the third pipe 26 and is discharged to the outside from the gas outlet of the branch path 26b and recovered. Another portion of the released carbon dioxide gas flows into the circulation path 26a of the third pipe 26. The carbon dioxide flowing into circulation path 26a is heated by the heat exchanger 21 along the way in circulation path 25a, and then reintroduced into the gas absorber 23, where the heat is used to heat the gel particle membrane.
[0059] As described above, in this first embodiment of the carbon dioxide gas recovery device, the heat from the exhaust gas is reused to heat the gas absorber and switch it from a state of absorbing acidic gas to a state of releasing it. In this embodiment, the heat from the exhaust gas is effectively utilized, so the energy consumption in the carbon dioxide gas separation and recovery process can be significantly reduced. In the first embodiment, if the temperature of the exhaust gas and the absorber cannot be controlled to a temperature suitable for carbon dioxide absorption and release, the temperature control is improved by adding an external heat exchange mechanism or an additional heating mechanism to the piping and the absorber.
[0060] Next, a second embodiment of the carbon oxide gas recovery device will be described. As shown in Figure 3, the acid gas recovery apparatus of the second embodiment includes a first heat exchanger 31 and a second heat exchanger 32, a desulfurizer 33, a first tank 34 and a second tank 35, and a first pipe 36 and a second pipe 37 connected to these parts. One end of the first pipe 36 is a gas inlet for introducing exhaust gas (gas to be treated), and the other end is connected to the desulfurizer 33 which has a cooling capacity. Here, the desulfurizer and the cooler may be separate devices. The second pipe 37 has a main path 37a, one end of which is connected to the desulfurizer 33, and a first path 37b and a second path 37c that branch off from the other end of the main path 37a. One end of the first path 37b is in communication with the main path 37a, and the other end is connected to the first tank 34. One end of the second path 37c is in communication with the main path 37a, and the other end is connected to the second tank 35. Valves (not shown) for opening and closing each path 37b and 37c are provided near the other ends of the first path 37b and the second path 37c. The first heat exchanger 31 is connected to the first intermediate section of the first pipe 36 and the first tank 34, respectively, and the second heat exchanger 32 is connected to the second intermediate section of the first pipe 36 and the second tank 35, respectively. In the carbon dioxide gas recovery apparatus of the second embodiment, gel particle films 38 and 39 are applied to the heat exchange surface of the first heat exchanger 31 in the first tank 34 and the heat exchange surface of the second heat exchanger 32 in the second tank 35, respectively. In this embodiment, the first heat exchanger 31 in the first tank 34 and the second heat exchanger 32 in the second tank 35, along with the gel particle films 38 and 39 loaded in these tanks, constitute the gas absorber of the present invention, and function as a carbon dioxide gas absorption tower and a carbon dioxide gas diffusion tower, respectively. When the operation of the carbon dioxide gas device is turned OFF, the gel particle films 38 and 39 in each tank 34 and 35 are at a temperature similar to the ambient temperature (approximately 30°C).
[0061] To recover carbon dioxide gas from exhaust gas using this carbon dioxide gas recovery device, first, the valve of the first path 37b of the second pipe 37 is opened, the valve of the second path 37c of the second pipe 37 is closed, the first heat exchanger 31 is turned OFF, and the second heat exchanger 32 is turned ON. In this state, the first tank 34 functions as an absorption tower. That is, in this state, when the high-temperature exhaust gas after dust collection is introduced from one end of the first pipe 36, the introduced exhaust gas passes through the first pipe 36 and is introduced into the desulfurizer 33. As it passes through the first pipe 36, some of the heat of the exhaust gas is transferred to the second tank 35 via the second heat exchanger 32, and the exhaust gas is cooled. The exhaust gas introduced into the desulfurizer 33 undergoes desulfurization treatment in the desulfurizer 33, which has a cooling capacity, and after being further cooled, flows into the main path 37a of the second pipe 37. The mixed gas flowing into the main path 37a is at approximately 30°C, and at this temperature, it is introduced into the first tank 34 via the main path 37a and the first path 37b. Inside the first tank 34, because the mixed gas is at approximately 30°C, carbon dioxide is efficiently absorbed by the gel particle membrane 38, and gases other than carbon dioxide are discharged to the outside through a gas outlet provided in the first tank 34.
[0062] After the gel particle membrane 38 has sufficiently absorbed carbon dioxide, the valve of the first path 37b of the second pipe 37 is closed, the valve of the second path 37c of the second pipe 37 is opened, the first heat exchanger 31 is turned ON, and the second exchanger 32 is turned OFF. As a result, the heat of the exhaust gas passing through the first pipe 36 is transferred to the first tank 34 and the gel particle membrane 38 via the first heat exchanger 31. The gel particle membrane 38 in the first tank 34 is heated to about 75°C by the heat from the first heat exchanger 31 and releases carbon dioxide gas. The released carbon dioxide gas is discharged and recovered from a gas outlet provided in the first tank 34. Meanwhile, a mixed gas at about 30°C that has flowed into the second pipe 37 via the same path as above is introduced into the second tank 35 via the second path 37c, and carbon dioxide is absorbed by the gel particle membrane 39 loaded in the tank 35. In other words, in this state, the first tank 34 functions as a diffusion tower and the second tank 35 functions as an absorption tower, and carbon dioxide gas absorption and diffusion occur in parallel.
[0063] After sufficient release of carbon dioxide gas from the gel particle membrane 38 and absorption of carbon dioxide gas into the gel particle membrane 39, as shown in Figure 3, the valve of the first path 37b of the second pipe 37 is opened, the valve of the second path 37c of the second pipe 37 is closed, the first heat exchanger 31 is turned OFF, and the second heat exchanger 32 is turned ON, so that the first tank functions as an absorption tower and the second tank as a diffusion tower. As a result, carbon dioxide gas absorption and diffusion occur in parallel in the opposite towers compared to before the switch. Furthermore, by repeatedly performing the above switching operation, the absorption and diffusion of carbon dioxide gas from the exhaust gas can be performed continuously, and carbon dioxide gas can be efficiently separated and recovered from a large amount of exhaust gas.
[0064] As described above, in this second embodiment of the carbon dioxide gas recovery apparatus, the heat from the exhaust gas is reused to cause a phase transition in the gas absorber, switching it from a state that absorbs acidic gases to a state that releases them. Therefore, the energy utilization efficiency can be greatly increased compared to when using a conventional carbon dioxide gas separation and recovery process. In the second embodiment, if the temperature of the exhaust gas and the absorber cannot be controlled to a temperature suitable for carbon dioxide absorption and release, the temperature control is improved by adding an external heat exchange mechanism or an additional heating mechanism to the piping and the absorber. [Examples]
[0065] The features of the present invention will be further described below with reference to examples and comparative examples. The materials, amounts used, proportions, processing content, and processing procedures shown in the following examples can be modified as appropriate without departing from the spirit of the present invention. Therefore, the scope of the present invention should not be interpreted as being limited by the following specific examples.
[0066] [I] Synthesis of amine-containing gel particles Polymer compound particles containing amino groups were synthesized as follows. In the following explanation, the gel of the polymer compound particles containing amino groups may be referred to as "amine-containing gel particles," and the particles obtained by drying the "amine-containing gel particles" may be referred to as "amine-containing dried gel particles."
[0067] (Synthesis Example 1) One liter of pure water was added to a two-liter three-necked flask and heated to 70°C. Then, 2 mM of a surfactant (cetyltrimethylammonium bromide) and three monomers were dissolved in the mixture to a total monomer concentration of 312 mM. The three monomers were composed of 55 mol% N-(dimethylaminopropyl)methacrylamide, 43 mol% N-tert-butylacrylamide, and 2 mol% N,N'-methylenebisacrylamide. The N-(dimethylaminopropyl)methacrylamide was prepared by removing the polymerization inhibitor using an alumina column. The N-tert-butylacrylamide was pre-dissolved in a small amount of methanol to a 0.68 g / mL solution before being added. This mixture was stirred with a mechanical stirrer while maintaining the temperature at 70°C, and oxygen was removed from the system by bubbling with nitrogen gas for one hour. To the monomer solution obtained in this way, a solution of 700 mg of 2,2'-azobis(2-methylpropionamidine)dihydrochloride dissolved in 5 mL of pure water was added, and the mixture was reacted at 70°C for 3 hours under a nitrogen atmosphere. After the reaction, the precipitate was filtered, and unreacted monomers and surfactants were removed by dialysis for 3 days using a dialysis membrane (MWCO12-14.000, width: 75 mm, vol / length: 18 mL / mL) [Spectrum Laboratories]. Counteranions were removed from the precipitate after dialysis using a strongly basic ion exchange resin to obtain amine-containing gel particles. Similar experiments were conducted on materials that did not undergo dialysis or ion exchange, and it was confirmed that they had almost equivalent functionality. The particle size of the obtained amine-containing gel particles was 800 nm.
[0068] (Synthesis Example 2) Amine-containing gel particles were obtained in the same manner as in Synthesis Example 1, except that N-isopropylacrylamide was used instead of N-tert-butylacrylamide, and the composition of the three monomers was changed to 5 mol% N-(dimethylaminopropyl)methacrylamide, 93 mol% N-isopropylacrylamide, and 2 mol% N,N'-methylenebisacrylamide. The hydrodynamic particle diameter of the obtained amine-containing gel particles in a dispersed state in water at 30°C was approximately 200 nm under a nitrogen atmosphere and approximately 400 nm in the presence of 10% CO2.
[0069] (Synthesis Example 3) Amine-containing gel particles were obtained in the same manner as in Synthesis Example 2, except that the concentration of the surfactant was changed to 0.16 mM. The hydrodynamic particle size of the obtained amine-containing gel particles in a dispersed state in water at 30°C was 600 nm.
[0070] (Synthesis Example 4) A monomer solution was obtained in the same manner as in Synthesis Example 2, except that the composition of the three monomers was changed to 5 mol% N-[(3-dimethylamino)propyl]methacrylamide, 93 mol% N-isopropylacrylamide, and 2 mol% N,N'-methylenebisacrylamide, and the total monomer concentration was set to 1040 mM. Nitrogen gas was passed through 2.4 mL of this solution for 10 minutes, then an aqueous solution of the initiator 2,2'-azobis(2-methylpropionamidine)dihydrochloride was mixed and introduced into the bottom of a stainless steel reactor for carbon dioxide absorption. A silicone rubber spacer (100 μm thick) and mold were placed in the reactor, and a glass plate was placed on top of the spacer, sandwiching the monomer solution, so that the monomer solution formed a liquid film with a thickness of 100 μm. The reactor was heated to 70°C and the polymerization reaction was carried out for 2 hours. After 2 hours, the glass plate and spacer were removed, and a hydrogel film with amine-containing gel particles crosslinked was obtained, adhered to the bottom of the stainless steel reactor. Observation of the primary diameter of gel particles within the obtained hydrogel film using a scanning electron microscope after drying the film revealed that the primary particle diameter of the particles ranged from several tens to several micrometers, and that cross-linking structures were formed between the particles.
[0071] [II] Synthesis of stabilizers A polymer compound containing an amino group, which acts as a stabilizer, was synthesized as follows.
[0072] (Synthesis Example 5) Synthesis of Polyvinylamine 5.0 g of N-vinylformamide (NVF), purified by distillation, was added to 44 mL of pure water, and the mixture was bubbled with nitrogen for 30 minutes while stirring in an oil bath at 60°C. Then, 1.0 mL of an aqueous solution (19 mg / mL) of the initiator 2,2'-azobis[2-(2-imidazolin-2-yl)propane] dihydrochloride (VA-044) [Wako Pure Chemical Industries, Ltd.] was added to this solution, and the mixture was reacted under a nitrogen atmosphere for 24 hours. Acetone was added to the reaction solution to precipitate the polymer, and the supernatant was removed. The resulting precipitate was dissolved in a solvent of pure water and ethanol in a 3:1 volume ratio. Further, the precipitation of the polymer with acetone, removal of the supernatant, and dissolution in the aqueous solvent were repeated several times to remove unreacted monomers. The resulting precipitate solution was concentrated under reduced pressure using an evaporator, and then vacuum-dried to obtain solid poly(NVF). The dried solid was dissolved in a 2N sodium hydroxide aqueous solution to a polymer concentration of 2% by mass, and stirred in an oil bath at 80°C for 24 hours to obtain a clear, viscous liquid. Hydrochloric acid was added to this liquid to form the hydrochloride salt, and excess hydrochloric acid was removed using an evaporator. The liquid was dialyzed for 3 days using a dialysis membrane (MWCO12-14.000, width: 75 mm, vol / length: 18 mL / mL) [Spectrum Laboratories], and the volume of solution in the dialysis membrane was measured. Subsequently, the entire volume was freeze-dried to obtain poly(vinylamine) hydrochloride (PVAm·HCl). The progress of the reaction at each step was as follows: 1 This was confirmed by 1H NMR (D2O). The counter anions were removed from this PVAm·HCl using a strongly basic ion exchange resin to obtain polyvinylamine.
[0073] (Synthesis Example 6) Synthesis of Hydrophobized Polyvinylamine To give temperature responsiveness to the PVAm·HCl synthesized in Synthesis Example 5, a carboxylic acid with a bulky hydrophobic moiety was condensed. Two types of carboxylic acids were used: isobutyric acid [Sigma-Aldrich] and pivalic acid [Wako Pure Chemical Industries], each having either an isopropyl group or a tert-butyl group. The compound condensed with isobutyric acid is denoted as Isobutyl PVAm, and the compound condensed with pivalic acid is denoted as PivalPVAm. Specifically, hydrophobic polyvinylamine was obtained by the following process. 100 mg (1.25 mmol-amine) of PVAm·HCl was dissolved in 20 mL of Milli-Q water. Triethylamine (TEA) and isobutyric acid or pivalic acid were added to this aqueous solution. Since pivalic acid is solid at room temperature, it was dissolved in 100 L of methanol before being added. After stirring for 10 minutes, the condensing agent 1-ethyl-3-(3-dimethylaminopropyl) carbodiimide hydrochloride (EDC) [TCI] or 4-(4,6-dimethoxy-1,3,5-triazin-2-yl)-4-methylmorpholinium Chloride n-Hydrate (DMT-MM) [Wako Pure Chemical Industries, Ltd.] was added and the mixture was stirred for 6 hours. After the reaction was complete, the reaction solution was dialyzed for 3 days using a dialysis membrane (MWCO12-14,000, width: 45 mL, vol / length: 6.42 mL / cm) [Thermo Fisher Scientific Corporation]. The condensation rate was 1 The results were calculated by 1HNMR (D2O). After dialysis, counteranions were removed from the reaction solution using a strongly basic ion exchange resin to obtain hydrophobized polyvinylamine.
[0074] [Evaluation of gas absorbent materials] Here, amine-containing gel particles synthesized in Synthesis Examples 2-4 were used as the gel particles. (1) Investigation of phase transitions of amine-containing gel particles The amine-containing gel particles synthesized in Synthesis Example 2 were dissolved in water to prepare a particle solution (4 mg / mL). Figure 4 shows the results of investigating the temperature-dependent particle size change of amine-containing gel particles by heating the particle solution under conditions where carbon dioxide is present or absent. Figure 5 shows the change in solution pH when carbon dioxide is absorbed into the particle solution at 20°C, heated to around 60°C to release the carbon dioxide, and then cooled back down to 20°C. Figure 6 shows the results of titration tests with hydrochloric acid performed by holding the particle solution at 30°C, 45°C, 60°C, and 75°C, respectively. Figure 7 shows the change in carbon dioxide release over time when carbon dioxide gas is absorbed into the particle solution at 30°C and then heated to around 75°C to release the carbon dioxide. In the measurements shown in Figures 5 and 7, carbon dioxide gas was absorbed into the particle solution by immersing a stainless steel reactor containing the particle solution in a water bath at 20°C or 30°C and passing a mixed gas of carbon dioxide gas and nitrogen gas (10:90) through the container for 240 minutes. Furthermore, carbon dioxide gas was released by immersing the stainless steel reactor in a water bath at 60°C or 75°C. The amount of carbon dioxide released was determined by measuring the increase or decrease in carbon dioxide in the gas passing through the reactor during the release process. Figure 7 also shows the results of investigating the amount of carbon dioxide gas released under similar conditions for homopolymer polymers of N-[(3-dimethylamino)propyl]methacrylamide (low molecular weight amine) and N-(dimethylaminopropyl)acrylamide.
[0075] As shown in Figures 4 and 5, the particle size and pH of these amine-containing gel particles change depending on the temperature. Furthermore, from Figure 6, the apparent pKa of this particle solution was approximately 8 at 30°C and approximately 5.5 at 75°C. These findings confirm that these amine-containing gel particles are temperature-responsive particles that undergo a phase transition in response to temperature changes. Additionally, from Figure 7, it was confirmed that these amine-containing gel particles efficiently release absorbed carbon dioxide gas when heated to 75°C. Notably, since almost no carbon dioxide release was observed in aqueous solutions of low-molecular-weight amines with similar structures or homopolymer polymers of N-(diethylaminopropyl)acrylamide that do not form particles, it is suggested that the efficient release of carbon dioxide in the amine-containing gel particles was triggered by the particle phase transition.
[0076] (2) Comparison of gas absorption and release characteristics of gel particle film and gel homogeneous film (Example 1) The amine-containing gel particle aqueous solutions obtained in Synthesis Examples 2-4 were dried by freeze-drying to prepare methanol solutions (10 mg / mL). This methanol solution was poured into stainless steel containers, dried at 80°C, and then water was added to induce swelling, thereby producing gel particle films of varying thicknesses. The thickness of the gel particle films was adjusted by changing the amount of methanol solution poured into the containers.
[0077] (Comparative Example 1) An ethanol solution of monomers with the same composition as those prepared in Synthesis Example 2 was poured into a stainless steel container, degassed under a nitrogen atmosphere for 30 minutes, and then a benzoyl peroxide DMF solution was added. A polymer film was prepared by reacting under a nitrogen atmosphere at room temperature for more than 6 hours. After washing this polymer film with water and drying it at 80°C, various gel homogeneous films of different thicknesses were obtained by adding water and causing swelling. The thickness of the gel homogeneous film was adjusted by changing the amount of monomer solution poured into the container. Here, "gel homogeneous film" refers to a dense, film-like membrane that does not contain particles.
[0078] The reactors in which a gel particle film was formed in Example 1 and the reactors in which a gel homogeneous film was formed in Comparative Example 1 were immersed in a 30°C water bath. A carbon dioxide-containing gas mixture (10:90) of carbon dioxide and nitrogen gas, humidified in a 60°C humidifier, was passed through these containers at a rate of 300 mL / min for approximately 10 minutes. After confirming that the absorption of carbon dioxide into the film was complete using an infrared carbon dioxide concentration meter, the containers were moved to a 75°C water bath and held there for 3 minutes. During this time, the amount of carbon dioxide in the gas passing through the containers was quantified using an infrared carbon dioxide concentration meter, and the carbon dioxide emission rate and absorption rate were calculated from the increase or decrease in the amount. Figures 8 and 9 show the results of measuring the carbon dioxide gas emission rate for the gel particle film of Example 1 and the gel homogeneous film of Comparative Example 1, and Figure 10 shows the results of measuring the carbon dioxide absorption rate. The numerical values in "nm" in Figures 8-10 represent the particle size of the gel particles, where "300nm gel particle film" represents the gel particle film synthesized in Synthesis Example 2, "1μm gel particle film" represents the gel particle film synthesized in Synthesis Example 3, and "crosslinked gel particle film" represents the gel particle film synthesized in Synthesis Example 4. As shown in Figures 8-10, all gel particle films absorbed and emitted carbon dioxide more significantly than the gel homogeneous film, confirming that the absorption and emission capacity of carbon dioxide is improved by making the polymer compound containing amino groups into particulate matter. Furthermore, the fact that the carbon dioxide emission rate of the gel particle film is particularly higher than the absorption rate is presumed to be because, in the carbon dioxide absorption process, the gel particles swell significantly and the voids between particles are small, whereas in the emission process, the gel particles contract, creating large voids that contribute to gas diffusion.
[0079] [Evaluation of gas absorbers] For the evaluation of the gas absorber, amine-containing gel particles synthesized in Synthesis Example 1 were used as the gel particles. (3) Effects of supporting gel particle films on various thin plates as carriers As carriers, thin stainless steel sheets with a thickness of 0.1 mm or 0.3 mm (thermal conductivity of approximately 16 W / (m·K)), thin iron sheets with a thickness of 0.1 mm (thermal conductivity of approximately 80 W / (m·K)), and graphite sheets with a thickness of 0.1 mm (Panasonic Corporation, PGS Graphite Sheet EYGS182310, thermal conductivity of 600-800 W / (mK)) were prepared, and silicone rubber sheets with holes were attached to these carriers as molds. Meanwhile, the amine-containing dried gel particles synthesized in Synthesis Example 1 were dissolved in methanol to prepare a particle solution (50 mg / 3 mL). This particle solution was applied to the molds of the carriers and dried under reduced pressure in a 40°C incubator. The particle solution was similarly applied to the back surface of the carriers and dried in an 80°C dryer for 30 minutes to obtain a laminate consisting of the carrier and the dried particle film. However, since the silicone rubber sheet of the mold did not adhere to the graphite sheet, the silicone rubber sheet was fixed with clips and used. The particle solution was spread onto the carrier using a brush while heating it on an 80°C hot plate. Then, as with other carriers, the carrier coated with the particle solution was dried in an 80°C dryer to obtain a laminate. The weight of the dried laminate was measured, and the weight of the supported amine-containing dry gel particles was quantified. After that, 4 equivalents (4 mL / g) of water were added to gel the amine-containing dry gel particles. Through the above process, a gas absorber with a gel particle film supported on a carrier was obtained. The thickness of the gel particle film of each obtained gas absorber was 37 μm.
[0080] Next, a reactor as shown in Figure 11 was prepared. This reactor has a pair of acrylic plates 1, butyl rubber gaskets 2 placed on the opposing surfaces of the pair of acrylic plates 1, and a number of screws 4 that fix the pair of acrylic plates 1 together, with a gas absorber 3 sandwiched between the pair of butyl rubber gaskets 2. The upper acrylic plate 1 of this reactor is provided with a gas inlet 5 and a gas outlet 6, and gas from a gas supply means (not shown) is supplied to the gas absorber 3 through the gas inlet 5 and then discharged to the outside through the gas outlet 6. In this experiment, a gas absorber was fixed in the reactor shown in Figure 11, and carbon dioxide absorption and release experiments were conducted by flowing carbon dioxide-containing gas through it (10 mL / min). As the carbon dioxide-containing gas, a 60°C gas was used, which was nitrogen gas containing 10% carbon dioxide humidified in a 60°C humidifier. Carbon dioxide absorption was performed by placing the reactor in a 30°C water bath, and carbon dioxide release was performed by placing the reactor in a 75°C water bath. The amount of carbon dioxide released and absorbed by the gas absorber was calculated from the increase and decrease in carbon dioxide in the gas passing through the reactor. The changes in the amount of carbon dioxide absorbed and released over time for each gas absorber are shown in Figures 12 and 13. In Figures 12 and 13, "sus" represents a support made of stainless steel sheet, "Fe" represents a support made of iron sheet, and "C" represents a support made of graphite sheet. In Figure 12, the amount of carbon dioxide emitted was measured by placing the reactor in a 75°C water bath at 0 and 75 minutes from the start of the experiment, and the amount of carbon dioxide absorbed was measured by placing it in a 30°C water bath at 25 and 100 minutes from the start of the experiment. Figure 12 graphs the amount of emission and absorption of the gas absorber from 0, 25, 75, and 100 minutes. In Figure 13, the amount of emission was measured by placing the reactor in a 75°C water bath at 0, 75, and 140 minutes from the start of the experiment, and the amount of absorption was measured by placing it in a 30°C water bath at 30, 100, and 170 minutes from the start of the experiment. Figure 13 graphs the amount of emission and absorption of the gas absorber from 0, 30, 75, 100, 140, and 170 minutes. In the graphs in Figures 12 and 13, the vertical axis represents the amount of carbon dioxide emitted per unit mass of amine-containing dry gel particles of the gas absorber, and a negative emission indicates that carbon dioxide is being absorbed.
[0081] When a stainless steel sheet with a thickness of 0.1 mm (thermal conductivity of approximately 16 W / (m·K)) was used as a support, it took approximately 14 minutes to release 25 mL of carbon dioxide per gram of amine-containing dry gel particles, and approximately 26 minutes to absorb 25 mL of carbon dioxide. The maximum reversible carbon dioxide release and absorption per gram of amine-containing dry gel particles was 31-38 mL (Figures 12 and 13). On the other hand, when the thickness of the stainless steel sheet was reduced to 0.3 mm, the release rate accelerated by approximately 1.5 times and the absorption rate by approximately 2 times compared to when a 0.1 mm thick stainless steel sheet was used. It took only approximately 10 minutes to release 25 mL of carbon dioxide per gram of amine-containing dry gel particles, and only approximately 13 minutes to absorb 25 mL of carbon dioxide (Figure 12). Similarly, the reversible carbon dioxide release and absorption per gram of amine-containing dry gel particles improved to 42-48 mL (Figure 12). On the other hand, when a thin sheet of iron with relatively high thermal conductivity (thermal conductivity of approximately 80 W / (m·K)) was used as the support, the emission rate was accelerated by approximately 1.8 times and the absorption rate by approximately 2.2 times, even though the sheet was the same thickness of 0.1 mm. It took only about 8 minutes to emit 25 mL of carbon dioxide per gram of amine-containing dry gel particles and about 12 minutes to absorb 25 mL of carbon dioxide. Similarly, the reversible carbon dioxide emission and absorption per gram of amine-containing dry gel particles was 33-42 mL (Figure 13). Furthermore, when a graphite sheet with a thickness of 0.1 mm (Panasonic PGS Graphite Sheet EYGS182310, thermal conductivity 600-800 W / (mK)) was used, both the emission rate and absorption rate were accelerated by approximately 2.3 times compared to when a stainless steel sheet with a thickness of 0.1 mm was used. It took only about 6 minutes to emit 25 mL of carbon dioxide per gram of amine-containing dry gel particles, and only about 10 minutes to absorb 25 mL of carbon dioxide. Similarly, the reversible carbon dioxide emission and absorption amount per gram of amine-containing dry gel particles improved to 60 mL (Figure 13). In the same way, when an aluminum sheet with a thickness of 0.1 mm was used, the emission rate was accelerated by approximately 1.8 times and the absorption rate by approximately 1.5 times compared to when a stainless steel sheet with a thickness of 0.1 mm was used.
[0082] (4) Effects of supporting gel particle films containing various amounts of amine When a graphite sheet with a thickness of 0.1 mm (Panasonic PGS Graphite Sheet EYGS182310, thermal conductivity 600-800 W / (mK)) was used as a support, and the thickness of the supported amine-containing gel particle film was changed from 37 μm to 230 μm, the reversible absorption of carbon dioxide per unit volume of the reactor improved from 208 mL / L to 1160 mL / L (Figure 14). In Figure 14, carbon dioxide was sufficiently absorbed at 30°C to reach equilibrium, and then the temperature was raised to 75°C to release the carbon dioxide. Carbon dioxide was released starting at 0 minutes, and then 30 minutes after the start of the experiment, the reactor was placed in a 30°C water bath and the amount of carbon dioxide absorbed was measured. Figure 14 is a graph of the amount of gas absorber released and absorbed from 0 minutes and 30 minutes, with the vertical axis of the graph representing the amount of carbon dioxide released per unit volume of the reactor. A negative absorption rate indicates that carbon dioxide is being absorbed.
[0083] (5) Effects of supporting a gel particle film containing an accelerator-containing amine When a 0.1 mm thick graphite sheet (Panasonic Corporation, PGS Graphite Sheet EYGS182310, thermal conductivity 600-800 W / (mK)) was used as a support, a 230 μm amine-containing gel particle film was supported on it, and 1 M N,N',N''-pentamethyldiethylenetriamines was added as an accelerator, the reversible carbon dioxide absorption per reactor volume increased from 1160 mL / L to 4000 mL / L.
[0084] (6) Effects of supporting gel thin films on various fibers as carriers Figure 15 shows the stainless steel reactor used in this experiment. This reactor has a capacity of 60,000 mm². 3 The reactor has a space 11 with a volume of (80 mm in length, 150 mm in width, and 5 mm in depth), and 13 flow-rectifying plates 12 are arranged within this space 11 at 10 mm intervals. The reactor is also provided with a gas inlet 13 for introducing gas from a gas supply means (not shown) into the space 11 and a gas outlet 14 for discharging the gas from the space 11.
[0085] A predetermined amount of amine-containing dry gel particles was dissolved in methanol and stirred overnight. The solution was prepared to a concentration of approximately 17 mg / mL. Next, stainless steel fiber felt cut to 80 mm × 8 mm × 5 mm (Nippon Seisen Co., Ltd., Naslon Felt 12-5-1500 and 8-5-1500, fiber diameter 12 μm and 8 μm, thickness 5 mm, basis weight 1500 g / m²) was used as a carrier. 2) and aluminum fiber felt (fiber diameter 100 μm) were prepared. These supports were fixed in the space 11 of the reactor shown in Figure 15 and heated on a hot plate at 80°C. A methanol solution of amine-containing dry gel particles was evenly applied to the heated supports using a syringe. If the evaporation of methanol was slow with heating from below, heat was applied from above using a hairdryer to evaporate the methanol so that the amine-containing dry gel particles could be uniformly supported. A predetermined amount of water was added to the amine-containing dry gel particles supported on the supports to gel them, creating an amine-containing gel support material (gas absorber). This gas absorber was placed inside the reactor shown in Figure 15, and carbon dioxide absorption and release experiments were conducted by flowing carbon dioxide-containing gas (10 mL / min) through it. As the carbon dioxide-containing gas, nitrogen gas containing 10% carbon dioxide was used, humidified in a 60°C humidifier to 60°C. Carbon dioxide absorption was performed by placing the reactor in a 30°C water bath, and carbon dioxide release was performed by placing the reactor in a 75°C water bath. The gas passing through the reactor was passed through a condenser at 5°C to remove moisture, and the amount of carbon dioxide in the gas was quantified at regular intervals using gas chromatography (Shimadzu Corporation, product name GC-TCD). The amount of carbon dioxide emitted and absorbed by the gas absorber was calculated from the increase and decrease in the amount of carbon dioxide in the gas. Figures 16 to 23 show the changes in the amount of carbon dioxide absorbed and emitted over time for each gas absorber. Figures 16 to 19 are graphs of gas absorbers with Naslon Felt 12-5-1500 as the support. In Figures 20 to 23, "AlΦ100" represents a gas absorber with aluminum fiber felt as the support, "susΦ12" or "12-5-1500" represents a gas absorber with Naslon Felt 12-5-1500 as the support, and "8-5-1500" represents a gas absorber with Naslon Felt 8-5-1500 as the support. Furthermore, in Figures 16-23, the values in "mg / ml" represent the amount of amine-containing dry gel particles applied to the carrier. In Figures 16-23, the reactor was placed in a 75°C water bath at 0, 71, and 142 minutes from the start of the experiment to measure the amount of carbon dioxide released, and in a 30°C water bath at 25 and 96 minutes from the start of the experiment to measure the amount of carbon dioxide absorbed. Figures 16-23 graph the amount of gas absorber released or absorbed from the gas absorber at 0, 25, 71, 96, and 142 minutes.In Figures 16-23, the vertical axis of the graphs in Figures 16, 18, 20, and 22 represents the amount of carbon dioxide emitted per unit volume of fiber aggregate, while the values represented by the vertical axis of the other graphs are the same as those represented by the vertical axis in Figure 12.
[0086] When fibers are used as a carrier, it was found that the thickness of the fibers and the amount of gel carried affect the reversible absorption amount and absorption rate. Specifically, stainless steel fiber felt (Nippon Seisen Co., Ltd., Naslon Felt 12-5-1500, fiber diameter 12 μm, thickness 5 mm, basis weight 1500 g / m²) 2 When various amounts of amine-containing gel particles (water added at 4 mL / g) were applied to the material, increasing the amount of applied amine-containing dry gel particles from 100 mg to 200 mg increased the reversible carbon dioxide absorption by approximately twofold, but increasing it from 200 mg to 400 mg dramatically decreased the reversible carbon dioxide absorption (Figures 16, 17). Furthermore, when the amount of water added was varied while keeping the amount of amine-containing dry gel particles constant, even with a large amount of amine-containing dry gel particles, reducing the amount of water added from 4 mL / g to 2 mL / g slightly improved the reversible carbon dioxide absorption (Figures 18, 19). From these results, it was found that limiting the gel packing density, including water, to around 15-40% is necessary for efficient reversible carbon dioxide absorption. When the fiber diameter was changed from 12 μm to 100 μm (aluminum fiber) with the optimized packing density, the reversible carbon dioxide absorption performance decreased despite the high thermal conductivity of the material (aluminum) (Figures 20, 21). This is thought to be because the increased fiber diameter reduces the surface area of the fiber, resulting in a thicker gel particle film. On the other hand, when the fiber diameter was changed from 12 μm to 8 μm, the emission and absorption behavior remained almost unchanged (Figures 22 and 23). This indicates that if fibers thinner than 100 μm are used, the absorption and emission performance does not depend so strongly on the fiber diameter, and high performance can be achieved.
[0087] (7) Comparison of results with and without the gel particle film supported on the carrier. (Examples of fabrication and evaluation of gel particle films not supported on a carrier) 2.4 g of amine-containing dried gel particles were dissolved in methanol and stirred overnight to obtain a methanol solution of amine-containing dried gel particles (particle solution). The stainless steel reactor (Figure 15) described above was placed on a hot plate at 80°C and heated, and the prepared particle solution was applied to the inner surface of the reactor while the methanol evaporated. Specifically, one-third of the total solution volume was applied to the bottom of the stainless steel reactor, one-third to the top lid, and one-third to the comb portion of the lid. After drying the particle solution, 4.8 mL of water was added to gel the film, forming an amine-containing gel particle film on the inner surface of the reactor. Carbon dioxide absorption and release experiments were conducted by flowing a carbon dioxide-containing gas (50 mL / min) through this reactor. As the carbon dioxide-containing gas, a 60°C gas was used, which was nitrogen gas containing 10% carbon dioxide humidified in a 60°C humidifier. Carbon dioxide absorption was performed by placing the reactor in a 30°C water bath, and carbon dioxide release was performed by placing the reactor in a 75°C water bath. The gas passing through the reactor was passed through a 5°C condenser to remove water from the gas, and the amount of carbon dioxide in the gas was quantified at regular intervals using gas chromatography (Shimadzu Corporation, product name GC-TCD). From the increase and decrease in carbon dioxide in the gas, the amount of carbon dioxide released and absorbed by the gel particle membrane was calculated. Figure 24 shows the changes in the amount of carbon dioxide absorbed and released by the gel particle membrane over time.
[0088] (Examples of fabrication and evaluation of gel particle films supported on a carrier) 2.4 g of amine-containing dried gel particles were dissolved in methanol and stirred overnight to obtain a methanol solution of amine-containing gel particles (particle solution). Stainless steel fiber felt (Naslon felt, 12-5-1500 / m) was placed inside a stainless steel reactor (Figure 15). 2Twelve felt tubes were filled, and the reactor was placed on a hot plate at 80°C and heated. The particle solution was evenly applied using a syringe so that 200 mg of amine-containing dry gel particles were supported on each felt in the reactor, and the methanol in the particle solution was evaporated by leaving it in this state. If the evaporation of methanol was slow, heat was applied from above using a hairdryer to evaporate the methanol so that the amine-containing dry gel particles were uniformly supported. 400 μL (4.8 mL total) of water was added to each of the twelve carriers supporting the amine-containing dry gel particles to gel the particles, and a gas absorber with an amine-containing gel particle film supported on the carrier was obtained. Carbon dioxide absorption and release experiments were conducted by circulating a carbon dioxide-containing gas (50 mL / min) through a container in which a gas absorber was formed. The carbon dioxide-containing gas used was nitrogen gas containing 10% carbon dioxide, humidified in a 60°C humidifier to 60°C. Carbon dioxide absorption was performed by placing the reactor in a 30°C water bath, and carbon dioxide release was performed by placing the reactor in a 75°C water bath. The gas passing through the reactor was passed through a 5°C condenser to remove water, and the amount of carbon dioxide in the gas was quantified at regular intervals using gas chromatography (Shimadzu Corporation, product name GC-TCD). The amount of carbon dioxide released and absorbed by the gas absorber was calculated from the increase and decrease in carbon dioxide in the gas. Figure 24 shows the changes in carbon dioxide absorption and release over time for each absorber. In Figure 24, "12-5-1500 felt" represents a gas absorber using stainless steel fiber felt (Naslon Felt 12-5-1500) as a support, and the numerical value in "mg / ml" represents the amount of amine-containing dry gel particles coated onto the support or container. In Figure 24, the amount of carbon dioxide absorbed was measured at 25, 96, and 167 minutes after the start of the initial emission by placing the reactor in a 30°C water bath, and the amount of carbon dioxide emitted was measured at 0, 71, and 142 minutes after the start of the experiment by placing it in a 75°C water bath. Figure 24 graphs the amount of emission or absorption of the gas absorber from 0, 25, 71, 96, 142, and 167 minutes. The numerical values represented on the vertical axis of the graph in Figure 24 are the same as the numerical values represented on the vertical axis in Figure 12.
[0089] The results of the above experiments showed that a gel particle film directly formed inside the reactor could only reversibly absorb 50-120 mL of carbon dioxide, while a gas absorber in which the gel particle film was supported on felt made of 12 μm diameter stainless steel fibers, packed inside the same reactor, could reversibly absorb 98-130 mL of carbon dioxide. Furthermore, when the gel particle film was formed directly inside the reactor, it took 23 minutes to release 120 mL of carbon dioxide gas in the above reversible absorption process, whereas when the gel particle film was supported on stainless steel fiber felt, the release of carbon dioxide gas could be completed in less than 9 minutes. Similarly, when the gel particle film was formed directly inside the reactor, it took 45 minutes to absorb approximately 120 mL of carbon dioxide gas in the above reversible absorption process, whereas when the gel-like film was supported on stainless steel fiber felt, 120 mL of carbon dioxide gas could be absorbed in less than 18 minutes. As described above, it was confirmed that by using metal fibers as a support and loading a gel particle film with an appropriate packing ratio, the average reversible absorption amount can be improved by 1.3 times, the emission rate by 2.6 times, and the absorption rate by 2.5 times.
[0090] Next, experiments were conducted using felt made from stainless steel fibers and sintered metal fibers obtained by sintering felt made from stainless steel fibers. On a hot iron plate heated to 80°C, place a felt made of stainless steel fibers (Naslon felt, 12-5-1500 / m²). 2 ) Sintered metal fiber made from metal fibers or stainless steel fibers (manufactured by Nippon Seisen, SUS316L, basis weight 1600g / m²) 2A fiber with a diameter of 50 μm and a porosity of 89% was placed on a surface, and 550 μL of a solution prepared by dissolving the amine-containing gel particles obtained in Synthesis Example 1 in methanol at a concentration of 20 mg / mL was added and dried. Then, the surface was set in a reactor, and 4 equivalents of water were added relative to the amine-containing gel particles. In each experiment, three samples were prepared with varying packing rates of gel particles, and the carbon dioxide emission and absorption amounts were measured for each sample using the same method as described above. Figure 25 is a graph showing the relationship between gel packing rate and carbon dioxide emission and absorption amounts. From Figure 25, it was confirmed that when sintered metal fibers are used, the high carbon dioxide absorption and emission capacity of the gel particles can be maintained even when the packing rate of the gel particles is high (e.g., 60% or more). Next, carbon dioxide absorption and emission experiments were conducted using sintered metal fibers (fiber diameters of 12 μm and 50 μm) made from stainless steel fibers, foamed metal (Sumitomo Metal Industries, Cellmet #4, #5, and #7), and sintered nickel fibers (fiber diameter of 40 μm), respectively, in the same manner as described above. In Figure 26, the amount of carbon dioxide absorbed was measured at 25 minutes and 96 minutes after the start of emission by placing the reactor in a 30°C water bath, and the amount of carbon dioxide emitted was measured at 0 minutes and 71 minutes after the start of the experiment by placing it in a 75°C water bath. Figure 26 graphs the amount of emission or absorption of the gas absorber from 0 minutes, 25 minutes, 71 minutes, and 96 minutes. The values represented by the vertical axis of the graph in Figure 26 are the same as the values represented by the vertical axis in Figure 12. Figure 26 shows that foamed metal can be used in the same way as sintered metal fibers. Furthermore, sintered nickel fibers were found to be excellent in terms of carbon dioxide absorption rate, absorption amount, emission amount, and emission rate, and were confirmed to be a desirable material for use.
[0091] When 2.4 grams of amine-containing dry gel particles were dissolved in methanol and uniformly coated inside the reactor shown in Figure 15, and after drying, 4.8 mL of water was added to create a gel particle film, only 50-120 mL of carbon dioxide could be reversibly absorbed. However, for a volume of approximately 60,000 mm³, almost the same volume could be absorbed. 3Four 0.1mm thick graphite sheets (Panasonic PGS Graphite Sheet EYGS182310, thermal conductivity 600-800 W / (mK)) are laminated inside a space measuring (40mm vertically, 170mm horizontally, and approximately 8.8mm deep), with each sheet having a width of 6800mm on both sides. 2 When 2.4 grams of gel particles were uniformly coated onto a sheet (40 mm long, 170 mm wide) and 4.8 mL of water was added to support the gel film, it was possible to reversibly absorb 120-140 mL of carbon dioxide. Furthermore, when the gel particle film was formed directly inside the reactor, it took 23 minutes to release 120 mL of carbon dioxide gas in the above reversible absorption process, whereas when four graphite sheets supporting the gel film were stacked, the release of carbon dioxide gas could be completed in less than 15 minutes. Similarly, when the gel particle film was formed directly inside the reactor, it took 45 minutes to release approximately 20 mL of carbon dioxide gas in the above reversible absorption process, whereas when four graphite sheets supporting the gel film were stacked, the release of carbon dioxide gas could be completed in less than 25 minutes. As described above, by supporting a gel particle film on a graphite sheet, which serves as the support, we were able to improve the average reversible absorption by 1.5 times, the emission rate by 1.5 times, and the absorption rate by 1.8 times. Furthermore, when 2.4 grams of amine-containing dry gel particles were dissolved in methanol and uniformly coated inside the reactor shown in Figure 15, and after drying, 4.8 mL of water was added to create a gel particle film, only 50-120 mL of carbon dioxide could be reversibly absorbed. However, with a gas flow path volume of approximately 60,000 mm³, almost the same amount of carbon dioxide could be absorbed. 3 A plate-type heat exchanger (Hisaka Works, Ltd., UX-0005A-J-8-plate configuration) with six stainless steel thin plates (40mm long, 170mm wide, and approximately 8.8mm deep) has a heat transfer surface of 18,000mm each. 2When 2.4 grams of amine-containing dry gel particles were dissolved in methanol and uniformly coated onto a surface, dried, and then 4.8 mL of water was added to support the gel particle film, 120-140 mL of carbon dioxide could be reversibly absorbed. Furthermore, when the gel particle film was formed directly inside the reactor, it took 23 minutes to release 120 mL of carbon dioxide gas in the above reversible absorption process, whereas when four stainless steel plates supporting the gel film were laminated, the release of carbon dioxide gas could be completed within 14 minutes. Similarly, when the gel particle film was formed directly inside the reactor, it took 45 minutes to release approximately 120 mL of carbon dioxide gas in the above reversible absorption process, whereas when four stainless steel plates supporting the gel film were laminated, the release of carbon dioxide gas could be completed within 24 minutes. As described above, by supporting a gel particle film on a stainless steel thin sheet, which serves as the carrier, we were able to improve the average reversible absorption by 1.5 times, the emission rate by 1.6 times, and the absorption rate by 1.9 times.
[0092] Furthermore, the heat transfer surface of the six stainless steel thin plates of the plate-type heat exchanger (Hisaka Works, Ltd., UX-0005A-J-8-plate configuration) is 18,000 mm each. 2 In the case where 3.9 grams of amine-containing dried gel particles obtained in Synthesis Example 1 were dissolved in methanol, uniformly coated, and dried, then 4.8 mL of water was added to support the gel particle film, 10.9% CO2-containing nitrogen gas was flowed through at 200 mL / min to perform carbon dioxide release and absorption. At 25, 96, and 167 minutes from the start of the initial release, the reactor was placed in a 30°C water bath to measure the amount of carbon dioxide absorbed, and at 0, 71, and 142 minutes from the start of the experiment, it was placed in a 75°C water bath to measure the amount of carbon dioxide released. Figure 27 graphs the amount of gas absorber released or absorbed from 0, 25, 71, 96, 142, and 167 minutes. The values represented by the vertical axis in the graph in Figure 27 are the same as the values represented by the vertical axis in Figure 12. Extremely good results were obtained for carbon dioxide absorption rate, absorption amount, release amount, and release rate. Figure 28 shows the change in vapor pressure when the temperature of the water tank is varied between 30 and 75°C. The results in Figure 28 indicate that the gel particle film reversibly absorbs water vapor along with carbon dioxide.
[0093] (8) Investigation of methods for stabilizing gel-like films Gel particle films consisting solely of amine-containing gel particles have high water absorption, and under repeated use conditions, this can lead to an increase in film thickness, potentially causing blockage of gas channels and a decrease in gas absorption / release rates and reversible absorption. Furthermore, the gel particle film may become fluid and flow out from the carrier surface. To solve these problems, we investigated conditions under which a stable film could be obtained even under conditions of high water addition by adding a stabilizer to the gel particle film.
[0094] (8-1) Stabilization of amine-containing gel particle films using polyvinyl alcohol / polyethylene copolymer as a stabilizer The behavior of gel particles was observed when an amine-containing gel particle film, consisting of amine-containing gel particles, was stabilized with a polyvinyl alcohol / polyethylene copolymer at a concentration of 33% by mass or 50% by mass (mass fraction of the solid excluding the dispersion medium), and an excess amount of water was added. Specifically, the following experiment was conducted. First, a particle solution was prepared by dissolving amine-containing dry gel particles labeled with a fluorescent dye (dansyl group), unlabeled amine-containing dry gel particles, and a stabilizer, polyvinyl alcohol / polyethylene copolymer, in a solvent. The dry gel particle coating amount was 113 mg / m². 2The material was coated into glass vials and dried in an 80°C oven for 1.5 hours to form a gel particle film. The polyvinyl alcohol / polyethylene copolymers used were EVOH (E29) (manufactured by Nippon Synthetic Chemical Industry Co., Ltd., polyethylene copolymer ratio: 29%) or EVOH (E44) (manufactured by Nippon Synthetic Chemical Industry Co., Ltd., polyethylene copolymer ratio: 44%). Similarly, gel particle films were formed in glass vials, except that no stabilizer was used. After injecting an excess amount of water (10 mL / 20 mg polymer) into each glass vial and leaving it for 48 hours, the amount of amine-containing gel particles dissolved from the gel particle film into the aqueous layer was calculated from the amount of fluorescent dye. As a result, the amine-containing gel particle film without a stabilizer completely dissolved, and strong fluorescence above the detection limit was observed. When a polyvinyl alcohol / polyethylene copolymer (EVOH (E29)) with a polyethylene copolymer ratio of 29% was used as a stabilizer, adding 33% by mass reduced the amount of amine-containing gel particle film eluted to less than half compared to the case without the stabilizer. In a gel particle film to which 50% by mass of stabilizer was added, elution was almost completely suppressed, and the amount of fluorescent dye-labeled amine-containing gel particles eluted into water was below the detection limit. On the other hand, with a stabilizer (EVOH (E44)) having a polyethylene polymerization ratio of 44%, it was found that the amount of fluorescent dye eluted into the aqueous layer was suppressed to below the detection limit in both cases by adding 33% by mass or 50% by mass. From the above, it was found that adding a polymer with a high polyethylene content and high crystallinity as a stabilizer is effective in suppressing the elution of amine-containing gel particles at room temperature. Furthermore, the amount of carbon dioxide absorbed and emitted by the gel particle film prepared under the same conditions was determined using the reactor in Figure 15. The change in the amount of carbon dioxide emitted by the gel particle film over time is shown in Figure 29, and the change in the amount of carbon dioxide absorbed by the gel particle film over time is shown in Figure 30. In Figures 29 and 30, the vertical axis represents the amount of carbon dioxide emitted or absorbed per unit mass of amine-containing dry gel particles. As shown in Figures 29 and 30, the carbon dioxide absorption and emission rates of the gel particle membrane with added stabilizer were equivalent to those of the gel particle membrane without stabilizer. However, the absorption rate tended to slow down slightly with increasing amounts of stabilizer.
[0095] As described above, it was confirmed that the addition of polyvinyl alcohol / polyethylene copolymer dramatically suppressed the elution of amine-containing gel particles at room temperature. However, when the temperature was repeatedly changed between 75°C and 30°C in an environment with water present, and carbon dioxide was repeatedly released and absorbed, the stability of the membrane decreased under certain conditions, and the gel particle membrane sometimes fragmented. Therefore, we investigated a method for creating a gel particle membrane that maintains its shape more stably even in environments where the temperature and carbon dioxide absorption rate change significantly. A predetermined amount of stabilizer (EVOH (E44)) and amine-containing dry gel particles were dissolved in a mixed solvent of isopropanol and water (6:4 volume ratio) and coated onto a glass vial, which was stirred at 60°C for 4 hours. To this stabilizer-containing particle solution, a titanium-based crosslinking agent (TC-310 or TC-400 manufactured by Matsumoto Fine Chemical Co., Ltd.), diluted in the same solvent, was added in a mass ratio of approximately 1 / 8 to the stabilizer (EVOH (E44)). After stirring for 1 hour, the mixture was dried in a hot air dryer at 60°C for 12 hours to form a particle film. Subsequently, the particle film was stabilized by heat treatment at 110°C or 150°C for 1 hour. 200 equivalents of water were added to this particle film to gel it, and it was left to stand at room temperature for 12 hours. As a result, the gel particle film that gelled after heat treatment at 110°C showed some stabilization with the addition of a stabilizer of 9% by mass (mass fraction of solid excluding the dispersion medium) or more, but the film fragmented and peeled off from the glass vial (Figure 31(A)). On the other hand, the gel particle film that gelled after heat treatment at 150°C did not break even after being left at room temperature for 12 hours, and it was confirmed that it was sufficiently stabilized with the addition of a stabilizer of 3% by mass (mass fraction of solid excluding the dispersion medium). Furthermore, the phenomenon of the gel particle film dissolving was almost completely suppressed (Figure 31(B)). Furthermore, when the temperature was repeatedly changed between 75°C and 30°C in the presence of 10% carbon dioxide, swelling of the gel particle film with a crosslinked structure formed with titanium crosslinking agent (TC-400) was observed upon addition of 6% by mass and 33% by mass of stabilizer (mass fraction of solid excluding the dispersion medium), and swelling of the gel particle film with titanium crosslinking agent (TC-310) was observed upon addition of 6% by mass of stabilizer (mass fraction of solid excluding the dispersion medium), but no fragmentation or rupture of the film was observed (Figure 31(C)). For the gel particle film with a crosslinked structure formed with TC-310 and 33% by mass (mass fraction of solid excluding the dispersion medium) of stabilizer added, no significant change in the degree of swelling was observed even after two cycles of temperature changes.Furthermore, when the reversible carbon dioxide absorption performance of a gel particle membrane with a cross-linked structure formed with TC-310 and 33% by mass (mass fraction of solid excluding the dispersion medium) of stabilizer added was evaluated using the reactor shown in Figure 15, it was confirmed that the amount of carbon dioxide absorbed and emitted decreased by about 10% compared to the gel particle membrane without the stabilizer, but there was almost no adverse effect on the emission rate and absorption rate (Figure 32). In Figure 32, "EVOH & TC-310" represents the membrane with a cross-linked structure formed with TC-310 and the stabilizer EVOH (E44) added, and "No Additive" represents the membrane with a cross-linked structure formed with TC-310 but without the stabilizer EVOH (E44). In Figure 32, the amount of carbon dioxide absorbed was measured by placing the reactor in a 30°C water bath at 14 minutes and 74 minutes from the start of the experiment, and the amount of carbon dioxide emitted was measured by placing it in a 75°C water bath at 0 minutes and 60 minutes from the start of the experiment. Figure 32 graphs the emission and absorption amounts of the gas absorber at 0 minutes, 14 minutes, 60 minutes, and 74 minutes. The values represented on the vertical axis of the graph in Figure 32 are the same as those represented on the vertical axis in Figure 12.
[0096] (8-2) Stabilization of gel particle films using polyvinylamine as a stabilizer In addition to polyvinyl alcohol / polyethylene copolymer, polyvinylamine was also investigated as a stabilizer for gel particle films. Aqueous solutions containing amine-containing gel particles were mixed with polyvinylamine aqueous solutions in various mass ratios. After stirring for 3 days, the mixture was coated onto glass vials and dried under reduced pressure at 40°C, followed by drying at atmospheric pressure at 80°C for 1 hour. This formed a dried amine-containing gel particle film within the glass vials. Four equivalents of water were added to this dried amine-containing gel particle film to form a gel particle film, and 10% carbon dioxide-containing gas was passed through it at room temperature for 3 hours to dissolve the carbon dioxide. Next, the gel particle film was heated to 75°C and allowed to stand for 12 hours in the presence of 10% carbon dioxide-containing gas. This was done to investigate whether the primary amines of polyvinylamine were crosslinked by carbon dioxide and whether the film was stabilized. 200 mass of water was injected into the glass vials and allowed to stand for 1 hour, after which the film stability was observed. As a result, it was found that gel particle films with 9% by mass (mass fraction of solid excluding dispersion medium) or more of polyvinylamine added were relatively stable. Instead of raising the temperature to 75°C and letting it stand for 12 hours in the presence of a 10% carbon dioxide-containing gas, letting it stand at room temperature in the presence of a 10% carbon dioxide-containing gas for 12 hours did not improve the stability of the membrane. This suggests that the carbon dioxide dissolved in the membrane undergoes a cross-linking reaction at 75°C, stabilizing the membrane.
[0097] (8-3) Stabilization of gel particle thin films using polymerizable compounds as stabilizers We investigated the stabilization of gel particle films by using polymerizable compounds as stabilizers and polymerizing them in the presence of a polymerization initiator. 100 mg of amine-containing gel particles obtained in Synthesis Example 1 were dissolved in 6 mL of methanol. Additionally, 95 parts by mass of N,N-dimethylaminopropyl methacrylamide (DMAPM) and 5 parts by mass of N,N'-methylenebisacrylamide (BIS) were dissolved in methanol to prepare a methanol solution with a concentration of 0.05 mg / mL. Furthermore, a methanol solution of the polymerization initiator (IRGACURE 184) was also prepared, and these three methanol solutions were mixed. The mixing ratio was such that the total amount of DMAPM and BIS was 56 parts by mass per 100 parts by mass of amine-containing gel particles. The polymerization initiator was added in an amount equivalent to 1 / 60 mole relative to the monomer. This mixed solution was cast into a stainless steel reactor, slowly dried at room temperature, and then dried in a constant temperature bath at 35°C. Polymerization was then carried out by irradiation with ultraviolet light. Water was then added to obtain a gel particle film with a uniform film-like structure. In this method, even with the addition of a large amount of water, only a portion swelled, resulting in a gel particle film with a nearly uniform film-like structure. Carbon dioxide absorption and release experiments were conducted using the same method as described above. In Figure 33, the amount of carbon dioxide absorbed was measured at 25, 96, and 167 minutes after the start of the initial release by placing the reactor in a 30°C water bath, and the amount of carbon dioxide released was measured at 0, 71, and 142 minutes after the start of the experiment by placing it in a 75°C water bath. In Figure 33, the amount of release or absorption of the gas absorber from 0, 25, 71, 96, 142, and 167 minutes is graphed. The values represented by the vertical axis of the graph in Figure 33 are the same as the values represented by the vertical axis in Figure 12. Figure 33 shows that the obtained gel particle film achieved extremely high absorption rate, absorption amount, release amount, and release rate. The gel particle film after measurement was not excessively swollen and was stable. In the above experiment, instead of using DMAPM:BIS=95:5 as the polymerizable compound, a mixture of DMAPM:BIS:NIPAM=55:5:45 was used, and a gel-like film was prepared in the same manner. Carbon dioxide absorption and emission tests were then conducted to confirm the film state. Here, NIPAM is N-isopropylacrylamide. Figure 34 shows the graphs of the emission and absorption amounts of the gas absorber. As shown in Figure 34, good absorption rate, absorption amount, emission amount, and emission rate were achieved. Even when a large amount of water was added when forming the gel-like film, the film remained uniform. Furthermore, the gel particle film was stable and not excessively swollen even after the gas absorption and emission tests. Furthermore, in the above experiment, instead of using DMAPM:BIS=95:5 as the polymerizable compound, a mixture of DMAPM:BIS:NIPAM=30:5:65 was used, and a gel-like film was prepared in the same manner. Carbon dioxide absorption and emission tests were then conducted to confirm the film state. Figure 35 shows the graphs of the emission and absorption amounts of the gas absorber. As shown in Figure 35, good absorption rate, absorption amount, emission amount, and emission rate were achieved. Even when a large amount of water was added when forming the gel-like film, the film remained uniform. In addition, the gel particle film was stable and not excessively swollen even after the gas absorption and emission tests. Furthermore, in the above experiment, while keeping the use of DMAPM:BIS=95:5 as the polymerizable compound unchanged, the solvent was changed from methanol to water, and the polymerization initiator was changed to 2-hydroxy-4'-(2-hydroxyethoxy)-2-methylpropiophenone. A gel-like film was prepared in the same manner, and carbon dioxide absorption and emission tests were conducted to confirm the film state. Figure 36 shows the graphs of the emission and absorption amounts of the gas absorber. As shown in Figure 36, good absorption and emission amounts were achieved, but the absorption and emission rates were somewhat slow. Even when a large amount of water was added when forming the gel-like film, the film remained uniform. Also, even after the gas absorption and emission test, the gel particle film was not excessively swollen and remained stable.
[0098] (9) Effects of adding absorption and release promoters Various low-molecular-weight compounds were added to gel particle membranes as absorption and desorption enhancers, and their effects on improving the amount of carbon dioxide absorbed, absorbed, desorbed, and desorbed by the gel-like membrane were investigated. A gel particle film was formed in the reactor shown in Figure 15, and a low molecular weight compound represented by the following formula was added to the gel particle film, or amine-containing dry gel particles were introduced into the reactor, and water, PMDETA containing almost no water, or an aqueous solution of PMDETA was added. Then, under the same conditions as used in the measurement in Figure 16, one cycle of carbon dioxide absorption and emission was performed, and the changes in the amount of carbon dioxide absorbed and emitted over time were investigated. The results are shown in Figures 37 to 42. In Figures 37 to 40, "GP + H2O" represents a gel particle film that does not contain the low molecular weight compound represented by the following formula, while the others represent gel particle films to which the low molecular weight compound shown in the table was added at a concentration of 3N or 13% by mass in terms of amine concentration. In Figures 41-42, "GP+H2O" represents amine-containing dry gel particles with water added, "GP+PMDEA" represents amine-containing dry gel particles with PMDETA containing almost no water added, and the others represent amine-containing dry gel particles with PMDETA aqueous solutions of 1N, 3N, and 10N (amine equivalent concentrations) added. Figures 37-42 show that the absorption rate, absorption amount, emission amount, and emission rate were dramatically improved in gel particle membranes to which amine compounds, particularly Imino-bis(N,N-dimethylpropylamine) (IBDPA) and N,N',N''-pentamethyldiethylenetriamine (PMDETA), were added. However, if the concentration of the amine compound was too high, the amount of water relative to the amine was too large, and conversely, the absorption amount tended to decrease. This suggests that the presence of an appropriate amount of water is important for improving absorption capacity (Figures 41, 42). Preferably, the amount of water is 5 times or more molars relative to the amine, more preferably 8 times or more molars, and even more preferably 10 times or more molars. In gel particle membranes to which amine compounds were added under optimal conditions, both the absorption amount and emission amount improved by 3 to 4 times compared to gel particle membranes without the accelerator (Figures 41, 42).
[0099] [ka]
[0100] We investigated the effect of adding various low-molecular-weight amines as emission enhancers to gel particle membranes to improve the amount of carbon dioxide emitted from the gel-like membrane. A methanol solution (100 mg / 6 mL) of the amine-containing gel particles obtained in Synthesis Example 1 was injected into a stainless steel container and dried at 80°C. The stainless steel container was then cooled from the outside with ice to produce a dried nanogel film. 400 μL of 3N amine aqueous solution was uniformly added dropwise to this dried nanogel film. One cycle of carbon dioxide absorption and emission was performed on the resulting gel particle film under the same conditions as used in the measurement in Figure 16, and the amount of carbon dioxide emitted was investigated. The results of investigating the amount of emission using various low-molecular-weight amines are shown in Figure 43. As shown in Figure 43, it was confirmed that the emission could be promoted by adding low-molecular-weight amines. Furthermore, gel particle films were prepared in the same manner when 400 μL of amine aqueous solution with a concentration of 6N was added, and when 800 μL of amine aqueous solution with a concentration of 8N was added, and the amount of carbon dioxide emitted was investigated. The results are shown in Figure 44. As shown in Figure 44, TMDAH showed a tendency for the amount of carbon dioxide emitted to decrease when the amine concentration was too high, but PMDETA and IPAE were confirmed to be able to achieve high amounts of carbon dioxide emitted even at high amine concentrations. In particular, IPAE achieved remarkably high amounts of carbon dioxide emitted even at high amine concentrations, showing a remarkably superior effect. A high amine concentration means a situation where the amount of water relative to the amine is small, but even under such conditions of low water content, IPAE achieved remarkably high amounts of carbon dioxide emitted. [Industrial applicability]
[0101] According to the present invention, a gas absorber capable of efficiently absorbing and releasing acidic gases such as carbon dioxide and water vapor in response to external temperature changes is realized. Such a gas absorber can be effectively used in the separation and recovery process of acidic gases in CCS and in the separation process of acidic gases from fuel gases, and has extremely high industrial applicability. [Explanation of Symbols]
[0102] 1 Acrylic sheet 2. Butyl rubber gasket 3. Gas absorber 4 screws 5 Gas Inlet 6. Gas outlet 11 Space section 12. Rectifier plate 13 Gas Inlet 14 Gas outlet 21 Heat exchanger 22, 33 Desulfurizer 23 Gas absorber 24. First pipe 25 Second pipe 26 Third pipe 26a Circulation pathway 26b Branching Route 31 1st heat exchanger 32 Second heat exchanger 34 Tank No. 1 35 Tank No. 2 36 First pipe 37. Second pipe 37a Main route 37b Route 1 37c Second Route 38, 39 Gel particle film
Claims
1. A gas inlet section for introducing a gas to be treated containing carbon dioxide into a gas absorbent material containing polymer compound particles having amino groups. A heat supply unit that applies heat to the gas absorbent material, A gas discharge path for discharging a portion of the gas from the gas-absorbing material, and A circulation path is used that branches off from the aforementioned gas discharge path and introduces another portion of the gas into the gas absorbent material. A method for recovering carbon dioxide, comprising: maintaining the temperature of the gas absorbent material at 1 to 60°C during absorption, allowing the gas absorbent material to absorb carbon dioxide from the gas to be treated; then applying heat to the gas absorbent material using the heat supply unit to raise its temperature to 40 to 200°C, thereby releasing carbon dioxide from the gas absorbent material and recovering the carbon dioxide; The gas absorbing material satisfies at least one of the following conditions (1) and (2): (1) The water content per gram of solids is 0.1 mL or more. (2) The polymer compound particles having an amino group are (meth)acrylamide polymer compound particles. A method for recovering carbon dioxide, wherein the gas introduction section has a heat exchange mechanism with the outside, the heat exchange mechanism controls the temperature of the gas to be treated, and the gas absorbent material is supported on a carrier, and the temperature of the gas absorbent material is controlled by heat exchange between the gas to be treated and the gas absorbent material via the carrier.
2. The carbon dioxide recovery method according to claim 1, wherein a desulfurizer is provided upstream of the gas absorbent material, and the gas to be treated introduced from the gas inlet is introduced into the desulfurizer for desulfurization treatment before being introduced into the gas absorbent material.
3. The carbon dioxide recovery method according to claim 2, wherein the desulfurizer has a cooling function.
4. A method for recovering carbon dioxide according to any one of claims 1 to 3, wherein the heat supply unit is a heat exchanger connected to the gas introduction unit and the circulation path, and the gas in the circulation path heated by the heat exchanger is introduced into the gas absorbent material to heat the gas absorbent material.
5. A gas inlet section for introducing a gas to be treated containing carbon dioxide into a gas absorbent material containing polymer compound particles having amino groups. A heat supply unit that applies heat to the gas absorbent material, A gas discharge path for discharging a portion of the gas from the gas-absorbing material, and A carbon dioxide recovery device having a circulation path that branches off from the aforementioned gas discharge path and introduces another portion of the gas into the gas absorption material, The gas absorbent material is configured to absorb carbon dioxide from the gas being treated by maintaining a temperature of 1 to 60°C during absorption, and then the heat supply unit heats the gas absorbent material to raise its temperature to 40 to 200°C, thereby releasing carbon dioxide from the gas absorbent material. The gas absorbing material satisfies at least one of the following conditions (1) and (2): (1) The water content per gram of solids is 0.1 mL or more. (2) The polymer compound particles having an amino group are (meth)acrylamide polymer compound particles. A carbon dioxide recovery device having a heat exchange mechanism with the outside at the gas introduction section, the heat exchange mechanism controlling the temperature of the gas to be treated, and the gas absorbent material being supported on a carrier, the temperature of the gas absorbent material being controlled by heat exchange between the gas to be treated and the gas absorbent material via the carrier.
Citation Information
Patent Citations
Desorber
JP1983058819U
JP1986083433U
Continuously adsorbing and reproducing-type carbon dioxide separating and removing apparatus
JP1992083509A
Carbon dioxide removing apparatus integrated with desulfurization device and boiler equipment equipped with carbon dioxide removing apparatus
JP2003181242A
Adsorption / desorption type concentrator
JP2012115773A