Indication device
A display device with a high refractive index layer, phase difference layer, and linear polarization layer structure addresses the issue of reflected light interference on sensors, enhancing display area efficiency by minimizing sensor malfunctions.
Patent Information
- Application Number
- JP2022095695
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-06-23
- Filing Date
- 2022-06-14
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2042-06-14
AI Technical Summary
The placement of light receiving sensors within the display area of display devices leads to malfunctions due to reflected light from the high refractive index layer incident on the sensors, which is not addressed by existing technologies.
A display device structure comprising a high refractive index layer, a first phase difference layer, and a linear polarization layer, with specific refractive indices and phase difference values, is designed to minimize reflected light incidence on light receiving sensors by converting it into elliptically polarized light that is then absorbed.
The proposed structure effectively suppresses the incidence of reflected light on light receiving sensors, reducing malfunctions and enhancing the display area utilization.
Smart Images

Figure 0007954520000006 
Figure 0007954520000007 
Figure 0007954520000008
Abstract
Description
Technical Field
[0001] The present invention relates to a display device, and further relates to an optical laminate used therein.
Background Art
[0002] A polarizing plate including a linear polarizing layer is widely used as a polarization supply element and a polarization detection element in display devices such as liquid crystal display devices and organic electroluminescent (EL) display devices, and as a member that suppresses the emission of reflected light reflected by a display element to the outside. Display devices provided with polarizing plates are also being deployed in mobile devices such as notebook personal computers, smartphones, and tablet terminals. From the viewpoints of expanding the display area on the display surface of mobile devices such as smartphones and improving design properties, Patent Document 1 describes, for example, providing a non-display area by notching the outer edge of the display area in a concave shape in a plan view.
[0003] Normally, no display element or polarizing plate is arranged in the non-display area provided in the concave shape. Therefore, by arranging various sensors such as a camera lens and a light receiving sensor in the non-display area, it is possible to reduce the likelihood of adversely affecting camera performance and sensor sensitivity.
Prior Art Documents
Patent Documents
[0004]
Patent Document 1
Summary of the Invention
Problems to be Solved by the Invention
[0005] To further expand the display area on the display surface, it is necessary to reduce the non-display area. In this case, it is conceivable to place various sensors, such as light receiving sensors, within the display area where the display elements and polarizing plates are provided. When light receiving sensors are placed within the display area, the light emitted from the display elements is more likely to be reflected by the high refractive index layer located on the viewing side of the polarizing plate and incident on the light receiving sensor. Reflected light incident on the light receiving sensor is likely to cause malfunctions of the light receiving sensor.
[0006] The present invention aims to provide a display device and an optical laminate used therein that can suppress the incidence of reflected light reflected by a high refractive index layer onto a light receiving sensor, even if the viewing side is equipped with a high refractive index layer. [Means for solving the problem]
[0007] The present invention provides the following display device. [1] A display device having, from the viewing side, a high refractive index layer, a first phase difference layer, a linear polarization layer, and a display unit in this order, The refractive index of the aforementioned high refractive index layer is 1.60 or higher. The display unit has a display element and a light receiving sensor, A display device in which the first phase difference layer and the linear polarization layer are laminated to cover the display element and the light receiving sensor. [2] The display device according to [1], wherein the first phase difference layer covers the entire visible side of the linear polarization layer in a plan view. [3] The display device according to [1] or [2], wherein the luminous efficiency correction transmittance of the linear polarization layer is 42% or more. [4] The display device according to any one of [1] to [3], wherein the angle between the slow axis of the first phase difference layer and the absorption axis of the linear polarization layer is 10° or more and 80° or less. [5] The display device according to any one of [1] to [4], wherein the in-plane phase difference value of the first phase difference layer at a wavelength of 550 nm is 80 nm or more and 170 nm or less. [6] The display device according to [5], wherein the first phase difference layer has inverse wavelength dispersion. [7] Furthermore, a second phase difference layer is provided between the high refractive index layer and the linear polarization layer, The second phase difference layer is laminated so as to cover the display element and the light receiving sensor. The display device according to [5] or [6], wherein the phase difference value in the thickness direction of the second phase difference layer at a wavelength of 550 nm is -140 nm or more and -20 nm or less. [8] The display device according to any one of [1] to [7], wherein the stimulus value Y of the reflected light when the light emitted from the display element is reflected by the high refractive index layer is 3.45% or more and 4.54% or less. [9] The light receiving sensor is capable of detecting light with a wavelength of 320 nm or more and 4000 nm or less, as described in any of [1] to [8].
[10] The display device according to any one of [1] to [9], wherein the light emitted from the display element has a wavelength of 320 nm or more and 4000 nm or less.
[11] The display device according to any one of [1] to
[10] , further comprising a third phase difference layer between the linear polarization layer and the display unit.
[0008] The present invention provides the following optical laminate.
[12] An optical laminate having a high refractive index layer, a first phase difference layer, and a linear polarization layer in this order, An optical laminate in which the refractive index of the high refractive index layer is 1.60 or higher.
[13] The optical laminate according to
[12] , wherein the first phase difference layer covers the entire visible side of the linear polarization layer in a plan view.
[14] The optical laminate according to
[12] or
[13] , wherein the luminous efficiency correction transmittance of the linearly polarized layer is 42% or more.
[15] The optical laminate according to
[12] or
[13] , wherein the angle between the slow axis of the first phase difference layer and the absorption axis of the linear polarization layer is 10° or more and 80° or less.
[16] The optical laminate according to
[12] or
[13] , wherein the in-plane phase difference value of the first phase difference layer at a wavelength of 550 nm is 80 nm or more and 170 nm or less. 〔17〕 The optical laminate according to〔12〕 or〔13〕, wherein the first retardation layer has reverse wavelength dispersibility. 〔18〕 The optical laminate according to〔12〕 or〔13〕, further comprising a second retardation layer between the high refractive index layer and the linear polarizing layer, wherein a thickness-direction retardation value of the second retardation layer at a wavelength of 550 nm is -140 nm or more and -20 nm or less. 〔19〕 The optical laminate according to〔12〕 or〔13〕, further comprising a third retardation layer on a side of the linear polarizing layer opposite to the first retardation layer side.
Effects of the Invention
[0009] According to the display device of the present invention, it is possible to suppress the reflected light reflected by the high refractive index layer from entering the light receiving sensor. Further, according to the optical laminate of the present invention, the above display device of the present invention can be provided.
Brief Description of the Drawings
[0010] [Figure 1] It is a schematic cross-sectional view schematically showing a display device according to one embodiment of the present invention. [Figure 2] It is a schematic cross-sectional view schematically showing a display device according to another embodiment of the present invention. [Figure 3] It is a schematic cross-sectional view schematically showing a display device according to still another embodiment of the present invention. [Figure 4] It is a schematic cross-sectional view schematically showing a display device according to yet another embodiment of the present invention.
Modes for Carrying Out the Invention
[0011] Hereinafter, preferred embodiments of the display device and the optical laminate will be described with reference to the drawings. In each drawing, the same members as those previously described are denoted by the same reference numerals, and descriptions thereof are omitted.
[0012] [Embodiment 1] (Display Device and Optical Laminate) Figures 1 and 2 are schematic cross-sectional views illustrating a display device according to one embodiment of the present invention. In Figures 1 and 2, the upper side is the viewing side. As shown in Figures 1 and 2, the display devices 1 and 2 of this embodiment have, in this order from the viewing side, a high refractive index layer 45, a first phase difference layer 31, a linear polarization layer 11, and a display unit 40. Of these, the high refractive index layer 45, the first phase difference layer 31, and the linear polarization layer 11 constitute optical laminates 51 and 52. The refractive index of the high refractive index layer 45 is 1.60 or higher, preferably 1.75 or higher, more preferably 1.80 or higher, usually 2.70 or lower, preferably 2.40 or lower, more preferably 2.30 or lower, and even more preferably 2.10 or lower. The refractive index of the high refractive index layer 45 can be measured by the method described in the embodiments described later.
[0013] The display unit 40 includes a display element 41 and a light receiving sensor 42. As shown in Figures 1 and 2, the display unit 40 may have a structure in which the light receiving sensor 42 is stacked on the viewing side of the display element 41, or it may have a structure in which the light receiving sensor 42 is stacked on the side opposite to the viewing side of the display element 41. Alternatively, the light receiving sensor 42 may be fitted into a through hole or recess provided in the display element 41. In the display unit 40, the area of the display element 41 can be used as the display area of the display devices 1 and 2. Therefore, from the viewpoint of expanding the display area, it is preferable that the area of the display element 41 surrounds the light receiving sensor 42 in a plan view of the display unit 40.
[0014] In the display devices 1 and 2, the first phase difference layer 31 and the linear polarization layer 11 are laminated so as to cover the display element 41 and the light receiving sensor 42. Preferably, the first phase difference layer 31 and the linear polarization layer 11 are laminated so as to cover the entire viewable surface of the display unit 40, that is, so as to cover the entire viewable surface of the display element 41 and the light receiving sensor 42. By providing the linear polarization layer 11 as described above, in a plan view, the area of the display element 41 surrounding the light receiving sensor 42 is covered by the linear polarization layer 11, making it easier to enlarge the display area of the display devices 1 and 2. The first phase difference layer 31 may cover the entire linear polarization layer 11 or only a part of it in a plan view, as long as it is laminated so as to cover the display element 41 and the light receiving sensor 42. The plan view shape of the first phase difference layer 31 may be the same as or different from the plan view shape of the linear polarization layer 11.
[0015] In the display devices 1 and 2, images are displayed by light emitted from the display element 41. Some of the light emitted from the display element 41 may be reflected by the high refractive index layer 45, as shown by the arrows in Figure 1, and incident on the light receiving sensor 42. In particular, in a plan view of the display unit 40, if the region of the display element 41 is arranged around the light receiving sensor 42, for example, if the regions of the light receiving sensor 42 and the display element 41 are adjacent and close to each other, reflected light reflected by the high refractive index layer 45 is likely to incident on the light receiving sensor 42. When reflected light is incident on the light receiving sensor 42, malfunctions of the light receiving sensor 42 are likely to occur. In the display devices 1 and 2 of this embodiment, a first phase difference layer 31 is laminated on the viewing side of the linear polarization layer 11 that covers the display element 41 and the light receiving sensor 42. The reflected light reflected by the high refractive index layer 45 is incident on the first phase difference layer 31, and its phase changes as it passes through the first phase difference layer 31. Therefore, at least a portion of the reflected light that has passed through the first phase difference layer 31 is more easily absorbed by the linear polarization layer 11. This reduces the amount of reflected light incident on the light receiving sensor 42, thereby suppressing malfunctions of the light receiving sensor 42.
[0016] The luminous efficiency correction single-unit transmittance of the linear polarization layer 11 is preferably 42% or higher, more preferably 43% or higher, and may be 45% or higher. When the luminous efficiency correction single-unit transmittance of the linear polarization layer 11 is high, the amount of reflected light transmitted through the linear polarization layer 11 increases, making the light receiving sensor 42 more prone to malfunction. According to the display devices 1 and 2 of this embodiment, even when a linear polarization layer 11 with a high luminous efficiency correction single-unit transmittance is used, the amount of reflected light incident on the light receiving sensor 42 can be suppressed, thereby suppressing malfunction of the light receiving sensor 42. The luminous efficiency correction single-unit transmittance of the linear polarization layer 11 can be measured by the method described in the embodiments described later.
[0017] The first phase difference layer 31 only needs to have a phase difference, but it is preferable that it has a phase difference such that the in-plane phase difference value Re(550) at a wavelength of 550 nm is between 80 nm and 170 nm. The in-plane phase difference value Re(550) of the first phase difference layer 31 is more preferably 100 nm or more, particularly preferably 130 nm or more, may be 135 nm or more, more preferably 160 nm or less, and even more preferably 150 nm or less. The in-plane phase difference value Re(550) of the first phase difference layer 31 can be measured by the method described in the examples below.
[0018] When the first phase difference layer 31 has an in-plane phase difference value Re(550) within the above range, the light emitted from the display element 41 in the display devices 1 and 2 is converted to elliptically polarized light when it passes through the first phase difference layer 31. The reflected light (elliptically polarized) reflected by the high refractive index layer 45 is converted to linearly polarized light when it passes through the first phase difference layer 31. As a result, the reflected light that has passed through the first phase difference layer 31 is more easily absorbed by the linearly polarized layer 11, and the amount of reflected light incident on the light receiving sensor 42 can be further suppressed.
[0019] When the in-plane phase difference value Re(550) of the first phase difference layer 31 is within the above range, the angle between the absorption axis of the linear polarization layer 11 and the slow phase axis of the first phase difference layer 31 is preferably within the range of 10° to 80°. The above angle may be 30° or more, and more preferably 40° or more. The above angle may also be 60° or less, and more preferably 50° or less.
[0020] The first phase difference layer 31, in which the in-plane phase difference value Re(550) is within the above-mentioned range, preferably has inverse wavelength dispersion properties. This broadens the wavelength range of reflected light absorbed by the linear polarization layer 11, thereby suppressing the amount of reflected light of various wavelengths incident on the light receiving sensor 42.
[0021] In the display devices 1 and 2, the stimulus value Y of the reflected light when the light emitted from the display element 41 is reflected by the high refractive index layer 45 is preferably 3.45% or more and 4.54% or less. The stimulus value Y of the reflected light is the ratio of the light intensity of the reflected light to the light intensity of the light emitted from the display element 41. A smaller stimulus value Y indicates that the amount of reflected light reflected by the high refractive index layer 45 is smaller, which is less likely to cause malfunction of the light receiving sensor 42. The stimulus value Y of the reflected light can be measured by the method described in the examples below. The stimulus value Y of the reflected light may be 3.48% or more, 3.50% or more, 4.30% or less, 4.10% or less, 3.90% or less, or 3.76% or less.
[0022] In display devices 1 and 2 where the stimulus value Y of the emitted light is within the above range, the amount of reflected light incident on the light receiving sensor 42 is easily suppressed. If the stimulus value Y of the emitted light is smaller than the above range, it is thought that the refractive index of the high refractive index layer 45 is small, or the luminous efficiency correction unit transmittance of the linear polarization layer 11 is small. Therefore, in display devices where the stimulus value Y of the emitted light is smaller than the above range, the amount of reflected light incident on the light receiving sensor 42 is small, and malfunctions of the light receiving sensor 42 are unlikely to occur. On the other hand, in display devices where the stimulus value Y of the emitted light is larger than the above range, the amount of reflected light incident on the light receiving sensor 42 is large, and malfunctions of the light receiving sensor 42 are likely to occur.
[0023] (Layer structure of display devices and optical laminates) Below, we will describe layers that may be present in the display devices 1 and 2 and the optical laminates 51 and 52, in addition to the layers described above.
[0024] The display devices 1 and 2 and the optical laminates 51 and 52 preferably have a first bonding layer 21 between the high refractive index layer 45 and the first phase difference layer 31, as shown in Figures 1 and 2. The first bonding layer 21 may be in direct contact with the high refractive index layer 45 and the first phase difference layer 31.
[0025] The display devices 1, 2 and the optical laminates 51, 52 may have one or more second refractive index layers (not shown) in addition to the high refractive index layer 45. The refractive index of the second refractive index layer can be within the refractive index range described above for the high refractive index layer 45. The second refractive index layer may be provided on the viewing side of the high refractive index layer 45, or it may be provided between the high refractive index layer 45 and the first phase difference layer 31. In this case, the display devices 1, 2 and the optical laminates 51, 52 may have a bonding layer (adhesive layer or bonding agent layer described later) between the high refractive index layer 45 and the second refractive index layer, and this bonding layer may be in direct contact with the high refractive index layer 45 and the second refractive index layer. When the display devices 1, 2 and the optical laminates 51, 52 have a second refractive index layer between the high refractive index layer 45 and the first phase difference layer 31, the first bonding layer 21 may be in direct contact with the first phase difference layer 31 and the second refractive index layer.
[0026] The display devices 1 and 2 and the optical laminates 51 and 52 preferably have a second bonding layer 22 between the first phase difference layer 31 and the linear polarization layer 11. The second bonding layer 22 may be in direct contact with the first phase difference layer 31 and the linear polarization layer 11.
[0027] As shown in Figures 1 and 2, the display devices 1 and 2 and the optical laminates 51 and 52 may have a first protective film 12 between the first phase difference layer 31 and the linear polarization layer 11. The first protective film 12 may be a layer for protecting the visible surface of the linear polarization layer 11, and the first protective film 12 and the linear polarization layer 11 may constitute a linear polarizing plate. When the display devices 1 and 2 and the optical laminates 51 and 52 have the first protective film 12, the second bonding layer 22 may be in direct contact with the first phase difference layer 31 and the first protective film 12.
[0028] When the display devices 1, 2 and the optical laminates 51, 52 have a first protective film 12, the first protective film 12 and the linear polarizing layer 11 may be in direct contact with each other, but it is preferable to have a third bonding layer 23 between the first protective film 12 and the linear polarizing layer 11. The third bonding layer 23 may constitute a linear polarizing plate and is preferably in direct contact with the first protective film 12 and the linear polarizing layer 11.
[0029] The display devices 1 and 2 may have a fourth bonding layer 24 between the linear polarization layer 11 and the display unit 40 (on the opposite side of the linear polarization layer 11 from the first phase difference layer 31). The linear polarization layer 11 and the display unit 40 may be in direct contact with the fourth bonding layer 24, as shown in Figure 1. As shown in Figures 1 and 2, the fourth bonding layer 24 may be provided by optical laminates 51 and 52.
[0030] The display devices 1, 2 and the optical laminates 51, 52 may have a second protective film (not shown) between the linear polarization layer 11 and the display unit 40 (on the side opposite to the first phase difference layer 31 of the linear polarization layer 11). The second protective film may be a layer for protecting the surface of the linear polarization layer 11 opposite to the viewing side, and the second protective film and the linear polarization layer 11 may constitute a linear polarizing plate. When the display devices 1, 2 and the optical laminates 51, 52 have a second protective film, the second protective film and the linear polarization layer 11 may be in direct contact, or there may be a bonding layer (adhesive layer or bonding agent layer described later) between the second protective film and the linear polarization layer 11. This bonding layer may constitute a linear polarizing plate, and it is preferable that it is in direct contact with the second protective film and the linear polarization layer 11. In this case, the fourth bonding layer 24 may be provided between the second protective film and the display unit 40, or it may be in direct contact with the second protective film and the display unit 40.
[0031] As shown in Figure 2, the display device 2 and optical laminate 52 may have a third phase difference layer 13 between the linear polarization layer 11 and the display unit 40 (on the opposite side of the linear polarization layer 11 from the first phase difference layer 31). In this case, the display device 2 and optical laminate 52 may have a fifth bonding layer 25 between the linear polarization layer 11 and the third phase difference layer 13, and the linear polarization layer 11 and the third phase difference layer 13 may be in direct contact with the fifth bonding layer 25. If the display device 2 and optical laminate 52 have a second protective film, the fifth bonding layer 25 may be provided between the second protective film and the third phase difference layer 13 and may be in direct contact with the second protective film and the third phase difference layer 13. In the display device 2 having a third phase difference layer 13, the fourth bonding layer 24 may be provided between the third phase difference layer 13 and the display unit 40 and may be in direct contact with the third phase difference layer 13 and the display unit 40. In the optical laminate 52 having the third phase difference layer 13, the fourth bonding layer 25 may be in direct contact with the third phase difference layer 13. Preferably, the linear polarizing layer 11 and the third phase difference layer 13 constitute a circular polarizing plate, and the third phase difference layer 13 is preferably a λ / 4 phase difference layer, and more preferably an inverse wavelength dispersive λ / 4 phase difference layer.
[0032] The display device 2 and the optical laminate 52 may have one or more fourth phase difference layers (not shown) separate from the third phase difference layer 13, between the linear polarization layer 11 and the display unit 40 (on the opposite side of the linear polarization layer 11 from the first phase difference layer 31). The fourth phase difference layer may be provided between the linear polarization layer 11 and the third phase difference layer 13, or between the third phase difference layer 13 and the display unit 40 (on the opposite side of the third phase difference layer 13 from the linear polarization layer 11). In this case, there may be a bonding layer (an adhesive layer or bonding agent layer described later) between the third phase difference layer 13 and the fourth phase difference layer, and this bonding layer may be in direct contact with the third phase difference layer 13 and the fourth phase difference layer. When the display device 2 and the optical laminate 52 have a fourth phase difference layer between the linear polarization layer 11 and the third phase difference layer 13, the fifth bonding layer 25 may be in direct contact with the linear polarization layer 11 and the fourth phase difference layer. If the display device 2 has a fourth phase difference layer between the third phase difference layer 13 and the display unit 40, the fourth bonding layer 24 may be in direct contact with the fourth phase difference layer and the display unit 40. If the optical laminate 52 has a third phase difference layer on the side of the third phase difference layer 13 opposite to the linear polarization layer 11, the fourth phase difference layer may be in direct contact with the fourth bonding layer. The linear polarization layer 11, the third phase difference layer 13, and the fourth phase difference layer preferably constitute a circular polarizer. The fourth phase difference layer constituting the circular polarizer is preferably a λ / 2 phase difference layer or a positive C layer.
[0033] [Embodiment 2] Figures 3 and 4 are schematic cross-sectional views illustrating a display device according to another embodiment of the present invention. In Figures 3 and 4, the upper side is the viewing side. The display devices 3 and 4 and optical laminates 53 and 54 of this embodiment differ from the display devices 1 and 2 and optical laminates 51 and 52 described in the previous embodiment in that they have a second phase difference layer 32 between the high refractive index layer 45 and the linear polarization layer 11. This point will be explained below.
[0034] In the display devices 3 and 4, the second phase difference layer 32 is laminated so as to cover the display element 41 and the light receiving sensor 42. Preferably, the second phase difference layer 32 is laminated so as to cover the entire viewing surface of the display unit 40, that is, so as to cover the entire viewing surface of the display element 41 and the light receiving sensor 42.
[0035] The display devices 3, 4 and optical laminates 53, 54 shown in Figures 3 and 4 have a second phase difference layer 32 between the high refractive index layer 45 and the first phase difference layer 31. Preferably, the second phase difference layer 32 covers the entire first phase difference layer 31 in a plan view, and more preferably, the plan view shape of the second phase difference layer 32 is the same as the plan view shape of the first phase difference layer 31.
[0036] The second phase difference layer 32 only needs to have a phase difference, but it is preferable that the phase difference Rth(550) in the thickness direction at a wavelength of 550 nm is between -140 nm and -20 nm. The phase difference Rth(550) in the thickness direction of the second phase difference layer 32 may be greater than -140 nm, greater than or equal to -120 nm, greater than or equal to -100 nm, greater than or equal to -90 nm, less than or equal to -20 nm, less than or equal to -30 nm, less than or equal to -40 nm, or less than or equal to -50 nm.
[0037] The phase difference value Rth(550) in the thickness direction of the second phase difference layer 32 is a value calculated based on equation (i). Rth(550)=[{(nx+ny) / 2}-nz]×d (i) [In formula (i), nx is the principal refractive index at a wavelength of 550 nm in the plane of the second phase difference layer 32. ny is the refractive index at a wavelength of 550 nm in a direction perpendicular to nx, within the same plane as nx. nz is the refractive index at a wavelength of 550 nm in the thickness direction of the second phase difference layer 32, and when nx = ny, nx can be the refractive index in any direction within the plane of the second phase difference layer 32. d is the film thickness of the second phase difference layer 32.
[0038] Because the display devices 3 and 4 have a second phase difference layer 32, as shown by the arrow in Figure 3, the amount of reflected light incident on the light receiving sensor 42, including reflected light incident from an oblique direction, can also be reduced. Reflected light incident from an oblique direction is mainly light that, in a plan view of the display unit 40, is emitted from a region of the display element 41 that is far from the light receiving sensor 42 and reflected by the high refractive index layer 45. The amount of reflected light incident from an oblique direction is easily reduced when the phase difference value Rth(550) in the thickness direction of the second phase difference layer 32 is within the above range. This further suppresses malfunctions of the light receiving sensor 42.
[0039] As shown in Figures 3 and 4, the first bonding layer 21 may be provided between the high refractive index layer 45 and the second phase difference layer 32, or it may be in direct contact with the high refractive index layer 45 and the second phase difference layer 32. The display devices 3, 4 and the optical laminates 53, 54 preferably have a sixth bonding layer 26 between the second phase difference layer 32 and the first phase difference layer 31, and the second phase difference layer 32 and the first phase difference layer 31 are in direct contact with the sixth bonding layer 26.
[0040] The display devices 3, 4 and optical laminates 53, 54 shown in Figures 3 and 4 describe a case where a second phase difference layer 32 is provided between the high refractive index layer 45 and the first phase difference layer 31. However, the case is not limited to this, as long as the second phase difference layer 32 is provided between the high refractive index layer 45 and the linear polarization layer 11. For example, the second phase difference layer 32 may be provided between the first phase difference layer 31 and the linear polarization layer 11. In this case, it is preferable that the second phase difference layer 32 covers the entire linear polarization layer 11. It is preferable that the planar shape of the second phase difference layer 32 is the same as the planar shape of the first phase difference layer 31.
[0041] Even when the display devices 3, 4 and the optical laminates 53, 54 have a second phase difference layer 32 between the first phase difference layer 31 and the linear polarization layer 11, the display devices 3, 4 and the optical laminates 53, 54 may have a sixth bonding layer 26 between the second phase difference layer 32 and the first phase difference layer 31. The second bonding layer 22 may also be provided between the second phase difference layer 32 and the linear polarization layer 11, for example, the second bonding layer 22 may be in direct contact with the second phase difference layer 32 and the first protective film 12.
[0042] The display device and the layers that make up the display device, as described above, will be explained in more detail below.
[0043] (display device) The above-mentioned display device can be used as a liquid crystal display device or an organic EL (electroluminescent) display device. The display device may also be a mobile device such as a smartphone or tablet. The display device may also be a flexible display that can be bent.
[0044] The planar external shape of the display area of the display device is not particularly limited, but may be a rectangle, a square, a polygon other than a rectangle and a square, or a rounded-corner shape where the corners are rounded (a shape with a radius). The rectangular, square, polygonal, or rounded-corner display area may have through holes for arranging cameras or the like.
[0045] (Display this element) The display element may be a liquid crystal display element or an organic EL display element. A liquid crystal display element may have, for example, a liquid crystal cell in which a liquid crystal layer is sandwiched between two cell substrates and a backlight. An organic EL display element may have, for example, a light-emitting layer and electrodes.
[0046] The light emitted from the display element is preferably light with a wavelength of 320 nm to 4000 nm, more preferably light with a wavelength of 380 nm to 780 nm (visible light region), and may also be light with a wavelength of 380 nm to 720 nm.
[0047] (Light receiving sensor) The light receiving sensor detects incident light. The light receiving sensor may also be an illuminance sensor that detects the illuminance around the display device, a proximity sensor that detects the proximity of an object, or a camera. Preferably, the light receiving sensor is capable of detecting light with a wavelength of 320 nm to 4000 nm, and more preferably is capable of detecting light with a wavelength of 380 nm to 780 nm (visible light region) and / or light with a wavelength of 780 nm to 4000 nm (infrared region).
[0048] (Touch sensor panel) The display device and optical laminate may include a touch sensor panel. The touch sensor panel can detect the position touched by the user with their finger or the like. Examples of touch sensor panels include resistive, capacitive, optical, ultrasonic, electromagnetic induction, and surface acoustic wave types, among which resistive and capacitive touch sensor panels are preferred.
[0049] In a display device and an optical laminate, the touch sensor panel may be provided on the viewing side of the linear polarization layer (the side of the first phase difference layer of the linear polarization layer), or on the opposite side from the viewing side of the linear polarization layer. When the touch sensor panel is provided on the viewing side of the linear polarization layer, the touch sensor panel may constitute a high refractive index layer, as described later. When the touch sensor panel is provided on the opposite side from the viewing side of the linear polarization layer, it is preferable that the touch sensor panel is provided between the linear polarization layer and the display unit.
[0050] (High refractive index layer) The high refractive index layer is not particularly limited as long as the refractive index is within the range specified in this embodiment (1.60 or higher). The high refractive index layer may be the front panel of a display device or a touch sensor panel, as long as it has the refractive index described above. The high refractive index layer may have a single-layer structure or a multilayer structure. If the high refractive index layer has a multilayer structure, it may include layers with a refractive index of less than 1.60, provided that the high refractive index layer has the refractive index described above.
[0051] The front panel can constitute the frontmost surface of the display device. The front panel can be any plate-like material that can transmit light, such as a resin plate, resin film, glass plate, or glass film. The front panel may have a single-layer structure or a multi-layer structure. The refractive index of the front panel may be between 1.45 and 1.9.
[0052] The polymer constituting the resin plate or resin film is not particularly limited as long as it is a light-transmitting resin. Examples of such polymers include triacetylcellulose, acetylcellulose butyrate, ethylene-vinyl acetate copolymer, propionylcellulose, butyrylcellulose, acetylpropionylcellulose, polyester, polystyrene, polyamide, polyetherimide, poly(meth)acrylic, polyimide, polyethersulfone, polysulfone, polyethylene, polypropylene, polymethylpentene, polyvinyl chloride, polyvinylidene chloride, polyvinyl alcohol, polyvinyl acetal, polyether ketone, polyetherether ketone, polyethersulfone, polymethyl(meth)acrylate, polyethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, polycarbonate, polyamideimide, and the like. These polymers can be used individually or in combination of two or more. In this specification, (meth)acrylic means acrylic and / or methacrylic, and (meth)acrylate means acrylicate and / or methacrylate.
[0053] If the front panel is a resin film, the front panel may have a hard coat layer on at least one side of the resin film. The hard coat layer is, for example, a cured layer of an ultraviolet-curable resin. Examples of ultraviolet-curable resins include (meth)acrylic resins such as monofunctional (meth)acrylic resins, polyfunctional (meth)acrylic resins, and polyfunctional (meth)acrylic resins having a dendrimer structure; silicone resins; polyester resins; urethane resins; amide resins; epoxy resins, etc. The hard coat layer may contain additives to improve its strength. The additives are not particularly limited and include inorganic fine particles, organic fine particles, or mixtures thereof. If the resin film has hard coat layers on both sides, the composition and thickness of each hard coat layer may be the same or different.
[0054] When the front panel is a glass plate or glass film, tempered glass for displays is preferably used.
[0055] Examples of touch sensor panels that constitute a high refractive index layer include the touch sensor panels described above. When a touch sensor panel constitutes a high refractive index layer, the refractive index of the touch sensor panel is 1.60 or higher, preferably 1.70 or higher, more preferably 1.90 or higher, usually 2.70 or lower, preferably 2.60 or lower, and more preferably 2.40 or lower.
[0056] (1st retardation layer, 2nd retardation layer, 3rd retardation layer, 4th retardation layer) The first phase difference layer, the second phase difference layer, the third phase difference layer, and the fourth phase difference layer (hereinafter collectively referred to as the "phase difference layer") may be a stretched film, or they may contain a cured layer of polymerizable liquid crystal compound.
[0057] When the phase difference layer is a stretched film, conventionally known stretched films can be used, and films in which a phase difference has been imparted by uniaxial or biaxial stretching of a resin film can be used. Examples of resin films that can be used include, but are not limited to, cellulose films such as triacetylcellulose and diacetylcellulose, polyester films such as polyethylene terephthalate, polyethylene isophthalate and polybutylene terephthalate, acrylic resin films such as polymethyl (meth)acrylate and polyethyl (meth)acrylate, polycarbonate films, polyethersulfone films, polysulfone films, polyimide films, polyolefin films, and polynorbornene films.
[0058] When the phase difference layer is a stretched film, the thickness of the phase difference layer is usually 5 μm to 200 μm, preferably 10 μm to 80 μm, and more preferably 40 μm or less.
[0059] When the phase difference layer includes the above-mentioned cured layer, conventionally known polymerizable liquid crystal compounds can be used as the polymerizable liquid crystal compound. The polymerizable liquid crystal compound is a compound having at least one polymerizable group and possessing liquid crystalline properties.
[0060] The type of polymerizable liquid crystal compound is not particularly limited, and rod-shaped liquid crystal compounds, disc-shaped liquid crystal compounds, and mixtures thereof can be used. The cured layer formed by polymerizing the polymerizable liquid crystal compound exhibits a phase difference when cured with the polymerizable liquid crystal compound oriented in a suitable direction. When a rod-shaped polymerizable liquid crystal compound is oriented horizontally or vertically with respect to the planar direction of the display device, the optical axis of the polymerizable liquid crystal compound coincides with the long axis direction of the polymerizable liquid crystal compound. When a disc-shaped polymerizable liquid crystal compound is oriented, the optical axis of the polymerizable liquid crystal compound exists in a direction perpendicular to the disc surface of the polymerizable liquid crystal compound. As a rod-shaped polymerizable liquid crystal compound, for example, those described in Japanese Patent Publication No. 11-513019 (Claim 1, etc.) can be suitably used. As disc-shaped polymerizable liquid crystal compounds, those described in Japanese Patent Publication No. 2007-108732 (paragraphs
[0020] to
[0067] , etc.) and Japanese Patent Publication No. 2010-244038 (paragraphs
[0013] to
[0108] , etc.) can be suitably used.
[0061] The polymerizable groups in a polymerizable liquid crystal compound refer to groups that participate in polymerization reactions, and are preferably photopolymerizable groups. Photopolymerizable groups are groups that can participate in polymerization reactions through active radicals or acids generated from photopolymerization initiators. Examples of polymerizable groups include vinyl groups, vinyloxy groups, 1-chlorovinyl groups, isopropenyl groups, 4-vinylphenyl groups, (meth)acryloyloxy groups, oxyranyl groups, oxetanyl groups, styryl groups, and allyl groups. Among these, (meth)acryloyloxy groups, vinyloxy groups, oxyranyl groups, and oxetanyl groups are preferred, with acryloyloxy groups being more preferred. The liquid crystalline properties of a polymerizable liquid crystal compound may be thermotropic or lyotropic, and if thermotropic liquid crystals are classified by their degree of order, they may be nematic or smectic. When two or more polymerizable liquid crystal compounds are used in combination to form a cured layer of the polymerizable liquid crystal compound, it is preferable that at least one of them has two or more polymerizable groups in its molecule. In this specification, (meth)acryloyl means acryloyl and / or methacryloyl.
[0062] If the phase difference layer includes the cured layer, the phase difference layer may also include an orientation layer. The orientation layer has an orientation restricting force that orients the polymerizable liquid crystal compound in a desired direction. The orientation layer may be a vertical orientation layer in which the molecular axis of the polymerizable liquid crystal compound is oriented perpendicular to the plane direction of the display device, a horizontal orientation layer in which the molecular axis of the polymerizable liquid crystal compound is oriented horizontally to the plane direction of the display device, or a tilt orientation layer in which the molecular axis of the polymerizable liquid crystal compound is tilted relative to the plane direction of the display device. If the phase difference layer includes two or more orientation layers, the orientation layers may be the same or different from each other.
[0063] The orientation layer is preferably one that has solvent resistance, meaning it does not dissolve when coated with a liquid crystal layer forming composition containing a polymerizable liquid crystal compound, and has heat resistance to solvent removal and heat treatment for orientation of the polymerizable liquid crystal compound. Examples of orientation layers include an orientation polymer layer formed from an orientation polymer, a photo-orientation polymer layer formed from a photo-orientation polymer, and a groove orientation layer having an uneven pattern or multiple grooves on its surface.
[0064] The above-mentioned cured layer can be formed by applying a composition for forming a phase difference layer, which contains a polymerizable liquid crystal compound, a solvent, and various additives as needed, onto an orientation layer to form a coating film, and then solidifying (curing) this coating film. Alternatively, the above composition may be applied onto a substrate layer to form a coating film, and the cured layer may be formed by stretching this coating film together with the substrate layer. In addition to the polymerizable liquid crystal compound and solvent described above, the above composition may also contain polymerization initiators, reactive additives, leveling agents, polymerization inhibitors, etc. Known polymerizable liquid crystal compounds, solvents, polymerization initiators, reactive additives, leveling agents, polymerization inhibitors, etc., can be used as appropriate.
[0065] As the base layer, a film made of a resin material can be used, for example, a film made of a resin material described as a thermoplastic resin used to form the first protective film described later. The thickness of the base layer is not particularly limited, but generally it is preferably 1 to 300 μm or less, more preferably 20 to 200 μm, and even more preferably 30 to 120 μm, from the viewpoint of strength and workability such as handling. The base layer may be incorporated into the display device together with the cured product layer of the polymerizable liquid crystal compound, or the base layer may be peeled off and only the cured product layer of the polymerizable liquid crystal compound, or the cured product layer and the orientation layer may be incorporated into the display device. When the base layer is incorporated into the display device together with the cured product layer of the polymerizable liquid crystal compound, the thickness of the base layer may be less than 30 μm, for example, 25 μm or less.
[0066] When the phase difference layer includes the above-mentioned cured material layer, the thickness of the phase difference layer is preferably 0.1 μm or more, more preferably 0.2 μm or more, and preferably 3 μm or less, and more preferably 2 μm or less.
[0067] (Linearly polarized layer) The linearly polarized layer has the property of transmitting linearly polarized light having a vibration plane perpendicular to the absorption axis when unpolarized light is incident on it. The linearly polarized layer may be a polyvinyl alcohol-based resin film (hereinafter sometimes referred to as "PVA-based film") on which iodine is adsorbed and oriented, or it may be a film containing a liquid crystalline polarized layer formed by coating a base film with a composition containing a compound having absorption anisotropy and liquid crystalline properties. The compound having absorption anisotropy and liquid crystalline properties may be a mixture of a dye having absorption anisotropy and a compound having liquid crystalline properties, or it may be a dye having absorption anisotropy and liquid crystalline properties.
[0068] The linearly polarized layer is preferably a PVA-based film on which iodine is adsorbed and oriented. Examples of PVA-based films for the linearly polarized layer include polyvinyl alcohol films, partially formalized polyvinyl alcohol films, and partially saponified ethylene-vinyl acetate copolymer films, which have been subjected to iodine dyeing and stretching treatments. If necessary, the PVA-based film on which iodine has been adsorbed and oriented by the dyeing treatment may be treated with an aqueous boric acid solution, followed by a washing step to wash off the aqueous boric acid solution. Known methods can be used for each step.
[0069] Polyvinyl alcohol-based resins (hereinafter sometimes referred to as "PVA-based resins") can be produced by saponifying polyvinyl acetate-based resins. Polyvinyl acetate-based resins can be polyvinyl acetate, which is a homopolymer of vinyl acetate, or copolymers of vinyl acetate and other monomers copolymerizable with vinyl acetate. Examples of other monomers copolymerizable with vinyl acetate include unsaturated carboxylic acids, olefins, vinyl ethers, unsaturated sulfonic acids, and acrylamides having ammonium groups.
[0070] The degree of saponification of PVA resins is typically around 85-100 mol%, preferably 98 mol% or higher. PVA resins may be modified; for example, polyvinyl formal or polyvinyl acetal modified with aldehydes can also be used. The average degree of polymerization of PVA resins is typically around 1,000-10,000, preferably 1,500-5,000. The degree of saponification and average degree of polymerization of PVA resins can be determined in accordance with JIS K 6726 (1994). If the average degree of polymerization is less than 1,000, it is difficult to obtain desirable polarization performance, and if it exceeds 10,000, film processability may be poor.
[0071] A method for manufacturing a linearly polarized film made of PVA may include the steps of preparing a base film, applying a resin solution such as a PVA resin onto the base film, and drying to remove the solvent to form a resin layer on the base film. A primer layer may be formed in advance on the surface of the base film on which the resin layer will be formed. As the base film, a film made of a resin material described later as a thermoplastic resin used to form the first protective film can be used. As the material for the primer layer, examples include a resin obtained by crosslinking a hydrophilic resin used in the linearly polarized film.
[0072] Next, the amount of solvent, such as water, in the resin layer is adjusted as needed. Then, the base film and the resin layer are uniaxially stretched, and subsequently, the resin layer is stained with iodine to adsorb and orient the iodine into the resin layer. Next, if necessary, the resin layer with the adsorbed and oriented iodine is treated with an aqueous boric acid solution, and then a washing step is performed to wash off the aqueous boric acid solution. This produces a PVA-based film in which the resin layer with the adsorbed and oriented iodine, i.e., the linearly polarized layer, is formed. Known methods can be used for each step.
[0073] The amount of boric acid in the boric acid-containing aqueous solution used to treat the PVA-based film or resin layer on which iodine is adsorbed and oriented is usually about 2 to 15 parts by mass per 100 parts by mass of water, and preferably 5 to 12 parts by mass. This boric acid-containing aqueous solution preferably contains potassium iodide. The amount of potassium iodide in the boric acid-containing aqueous solution is usually about 0.1 to 15 parts by mass per 100 parts by mass of water, and preferably 5 to 12 parts by mass. The immersion time in the boric acid-containing aqueous solution is usually about 60 to 1,200 seconds, preferably about 150 to 600 seconds, and more preferably about 200 to 400 seconds. The temperature of the boric acid-containing aqueous solution is usually 50°C or higher, preferably 50 to 85°C, and more preferably 60 to 80°C.
[0074] Uniaxial stretching of the PVA film, as well as the base film and resin layer, may be performed before dyeing, during dyeing, or during the boric acid treatment after dyeing, or uniaxial stretching may be performed at each of these multiple stages. The PVA film, as well as the base film and resin layer, may be uniaxially stretched in the MD direction (film transport direction), in which case uniaxial stretching may be performed between rolls with different peripheral speeds, or uniaxial stretching may be performed using a heated roll. The PVA film, as well as the base film and resin layer, may also be uniaxially stretched in the TD direction (direction perpendicular to the film transport direction), in which case the so-called tenter method can be used. Furthermore, the stretching may be dry stretching performed in air, or wet stretching performed while the PVA film or resin layer is swollen with a solvent. In order to exhibit the performance of the linearly polarized layer, the stretching ratio is 4 times or more, preferably 5 times or more, and particularly preferably 5.5 times or more. There is no particular upper limit to the stretching ratio, but from the viewpoint of suppressing breakage, etc., 8 times or less is preferred.
[0075] A linearly polarized film layer produced using a manufacturing method that utilizes a base film can be obtained by laminating a first protective film or a second protective film and then peeling off the base film. This method allows for further thinning of the linearly polarized film layer.
[0076] The thickness of the linearly polarizing layer, which is a PVA-based film, is preferably 1 μm or more, may be 2 μm or more, may be 5 μm or more, preferably 30 μm or less, more preferably 15 μm or less, may be 10 μm or less, or may be 8 μm or less.
[0077] A film containing a liquid crystalline polarizing layer includes a linear polarizing layer obtained by coating a base film with a composition containing a dye having liquid crystalline properties and absorption anisotropy, or a composition containing a dye having absorption anisotropy and a polymerizable liquid crystal. Examples of base films include films using resin materials described as thermoplastic resins used to form the first protective film, which will be discussed later. Examples of films containing a liquid crystalline polarizing layer include the polarizing layer described in Japanese Patent Application Publication No. 2013-33249, etc.
[0078] The total thickness of the base film and the linearly polarized layer formed as described above is preferably small, but if it is too small, the strength decreases and the processability tends to be poor. Therefore, it is usually 20 μm or less, preferably 5 μm or less, and more preferably 0.5 to 3 μm.
[0079] The linear polarizing layer obtained as described above (PVA-based film, film including a liquid crystalline polarizing layer) may be incorporated into a display device in the form of a linear polarizing plate, with the first protective film and / or second protective film described later laminated to one or both sides of the layer via an adhesive. In the case of a film including a liquid crystalline polarizing layer, the above-mentioned base film may be used as the first protective film or the second protective film.
[0080] (First protective film, second protective film) The first and second protective films may be films made from thermoplastic resins that have excellent transparency, mechanical strength, thermal stability, moisture barrier properties, isotropy, stretchability, etc. Specific examples of thermoplastic resins include cellulose resins such as triacetylcellulose; polyester resins such as polyethylene terephthalate and polyethylene naphthalate; polyethersulfone resins; polysulfone resins; polycarbonate resins; polyamide resins such as nylon and aromatic polyamides; polyimide resins; polyolefin resins such as polyethylene, polypropylene, and ethylene-propylene copolymers; cyclic polyolefin resins having cyclo and norbornene structures (also called norbornene resins); (meth)acrylic resins; polyarylate resins; polystyrene resins; polyvinyl alcohol resins; and mixtures thereof. The resin compositions of the first and second protective films may be the same or different.
[0081] The first protective film may have anti-reflective properties, anti-glare properties, hard coat properties, etc. (Hereinafter, a protective film having such properties may be referred to as a "functional protective film"). If the first protective film is not a functional protective film, a surface functional layer such as an anti-reflective layer, anti-glare layer, or hard coat layer may be provided on one side of the linear polarizing plate. It is preferable that the surface functional layer is provided so as to be in direct contact with the first protective film. It is preferable that the surface functional layer is provided on the side of the first protective film opposite to the linear polarizing layer.
[0082] The first protective film and the second protective film are each preferably 3 μm or thicker, more preferably 5 μm or thicker, and more preferably 50 μm or less, and more preferably 30 μm or less.
[0083] (1st lamination layer, 2nd lamination layer, 3rd lamination layer, 4th lamination layer, 5th lamination layer, 6th lamination layer) The first lamination layer, the second lamination layer, the third lamination layer, the fourth lamination layer, the fifth lamination layer, the sixth lamination layer, and the lamination layer (hereinafter collectively referred to as the "lamination layer") are each independently an adhesive layer or a bonding agent layer.
[0084] When the bonding layer is an adhesive layer, it is an adhesive layer formed using an adhesive composition. The adhesive composition or the reaction product of the adhesive composition exhibits adhesive properties by being attached to a substrate such as a metal layer, and is referred to as a pressure-sensitive adhesive. Furthermore, the adhesive layer formed using the active energy ray curable adhesive composition described later can have its degree of crosslinking and adhesive strength adjusted by irradiation with active energy rays.
[0085] As the adhesive composition, any conventionally known adhesive with excellent optical transparency can be used without particular limitation. For example, adhesive compositions containing base polymers such as acrylic polymers, urethane polymers, silicone polymers, and polyvinyl ethers can be used. The adhesive composition may also be an active energy ray curing adhesive composition or a thermosetting adhesive composition. Among these, an adhesive composition using an acrylic resin as the base polymer, which has excellent transparency, adhesive strength, re-peelability (reworkability), weather resistance, and heat resistance, is preferred. The adhesive layer is preferably composed of reaction products of an adhesive composition containing (meth)acrylic resin, a crosslinking agent, and a silane compound, and may contain other components.
[0086] The adhesive layer may be formed using an active energy ray curable adhesive. An active energy ray curable adhesive can be formed by blending an ultraviolet-curable compound such as a polyfunctional acrylate with the above-mentioned adhesive composition, forming the adhesive layer, and then curing it by irradiation with ultraviolet light, thereby creating a harder adhesive layer. Active energy ray curable adhesives have the property of curing when irradiated with energy rays such as ultraviolet light or electron beams. Because active energy ray curable adhesives are tacky even before irradiation with energy rays, they adhere closely to the adherend, and the adhesion strength can be adjusted by curing with energy ray irradiation.
[0087] The thickness of the adhesive layer is not particularly limited, but is preferably 5 μm or more, may be 10 μm or more, may be 15 μm or more, may be 20 μm or more, may be 25 μm or more, and is usually 300 μm or less, may be 250 μm or less, may be 100 μm or less, or may be 50 μm or less.
[0088] When the bonding layer is an adhesive layer, the adhesive layer can be formed by curing the curable component in the adhesive composition. Examples of adhesive compositions for forming the adhesive layer include adhesives other than pressure-sensitive adhesives (tacks), such as water-based adhesives and active energy ray-curable adhesives.
[0089] Examples of water-based adhesives include adhesives in which polyvinyl alcohol resin is dissolved or dispersed in water. There are no particular limitations on the drying method when using water-based adhesives, but methods such as using a hot air dryer or an infrared dryer can be employed.
[0090] Examples of active energy ray curing adhesives include solvent-free active energy ray curing adhesives containing curable compounds that harden upon irradiation with active energy rays such as ultraviolet light, visible light, electron beams, and X-rays. By using a solvent-free active energy ray curing adhesive, the adhesion between layers can be improved.
[0091] As an active energy ray curable adhesive, it is preferable to include either a cationic curable compound, a radical curable compound, or both, as these exhibit good adhesion. The active energy ray curable adhesive may further contain a cationic polymerization initiator, such as a photocationic polymerization initiator, or a radical polymerization initiator for initiating the curing reaction of the above-mentioned curable compound.
[0092] Examples of cationically polymerizable curable compounds include epoxy compounds such as alicyclic epoxy compounds having epoxy groups bonded to an alicyclic ring, polyfunctional aliphatic epoxy compounds having two or more epoxy groups but no aromatic ring, monofunctional epoxy groups having one epoxy group (excluding those included in alicyclic epoxy compounds), and polyfunctional aromatic epoxy compounds having two or more epoxy groups and an aromatic ring; oxetane compounds having one or more oxetane rings in the molecule; and combinations thereof.
[0093] Examples of radically polymerizable curable compounds include (meth)acrylic compounds (compounds having one or more (meth)acryloyloxy groups in the molecule), other vinyl compounds having radically polymerizable double bonds, or combinations thereof.
[0094] Active energy ray curing adhesives may contain sensitizers, such as photosensitizers, as needed. Using sensitizers improves reactivity and further enhances the mechanical strength and adhesive strength of the adhesive layer. Known sensitizers can be appropriately applied. When sensitizers are included, the amount is preferably in the range of 0.1 to 20 parts by mass per 100 parts by mass of the total amount of the active energy ray curing adhesive.
[0095] Active energy ray curing adhesives may contain additives such as ion trapping agents, antioxidants, chain transfer agents, tackifiers, thermoplastic resins, fillers, flow regulators, plasticizers, defoamers, antistatic agents, leveling agents, and solvents, as needed.
[0096] When using an active energy ray curing adhesive, the adhesive coating layer can be cured by irradiating it with active energy rays such as ultraviolet light, visible light, electron beams, or X-rays to form an adhesive layer. Ultraviolet light is preferred as the active energy ray, and in this case, low-pressure mercury lamps, medium-pressure mercury lamps, high-pressure mercury lamps, ultra-high-pressure mercury lamps, chemical lamps, black light lamps, microwave-excited mercury lamps, metal halide lamps, etc., can be used as light sources.
[0097] When the bonding layer is an adhesive layer, its thickness is preferably 0.1 μm or more, may be 0.5 μm or more, and preferably 10 μm or less, and may be 5 μm or less. [Examples]
[0098] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.
[0099] [Measuring the refractive index] The refractive index of the high refractive index layer was measured at 25°C using a multi-wavelength Abbe refractometer (DR-M4, manufactured by Atago Co., Ltd.) with a measurement wavelength of 589 nm.
[0100] [Measurement of luminous efficiency correction single unit transmittance Ty] For the linearly polarized layer, the MD transmittance and TD transmittance in the wavelength range of 380 to 780 nm were measured using a spectrophotometer with an integrating sphere [JASCO Corporation's "V7100"], and the following formula was used: Single-unit transmittance (%) = (MD + TD) / 2 Based on this, the transmittance of each element at each wavelength was calculated.
[0101] "MD transmittance" is the transmittance when the direction of polarization emitted from the Grant-Thomson prism is parallel to the transmission axis of the linearly polarized layer, and is represented as "MD" in the above formula. "TD transmittance" is the transmittance when the direction of polarization emitted from the Grant-Thomson prism is perpendicular to the transmission axis of the linearly polarized layer, and is represented as "TD" in the above formula. The obtained single-element transmittances are referred to in JIS Z 8701:1999 "Methods of color representation - XYZ color system and X 10 Y 10 Z 10 The luminous efficiency was corrected using a two-degree field of view (C light source) of the "color system," and the transmittance of the luminous efficiency-corrected unit was determined.
[0102] [Measurement of in-plane phase difference] The in-plane phase difference values of the first phase difference layer and the first protective film were measured using a phase difference measuring device (KOBRA-WPR, manufactured by Oji Instruments Co., Ltd.).
[0103] [Measurement of phase difference in the thickness direction] The phase difference value in the thickness direction of the second phase difference layer was measured using a phase difference measuring device (KOBRA-WPR, manufactured by Oji Keisoku Kiki Co., Ltd.). During the measurement, the angle of incidence of light to the second phase difference layer was varied, and the front phase difference value of the second phase difference layer and the phase difference value when tilted 40° around the phase advance axis were measured. The average refractive index at each wavelength was measured using an ellipsometer M-220 manufactured by JASCO Corporation. The thickness of the second phase difference layer was measured using an Optical NanoGauge film thickness gauge C12562-01 manufactured by Hamamatsu Photonics K.K. From the front phase difference value, the phase difference value when tilted 40° around the phase advance axis, the average refractive index, and the thickness of the second phase difference layer measured above, the three-dimensional refractive index was calculated with reference to the Oji Keisoku Kiki technical document (https: / / oji-keisoku.co.jp / cms / uploads / kbr_shiryo04.pdf). From the obtained three-dimensional refractive index, the phase difference value Rth in the thickness direction of the second phase difference layer was calculated according to equation (i) above.
[0104] [Measurement of stimulus value Y] A spectrophotometer (CM2600d, manufactured by Konica Minolta) was used to measure the stimulus value Y. Light from the spectrophotometer was incident on the moth-eye film side of the laminate, and the stimulus value Y of the reflected light was measured. Since the reflectivity of the moth-eye film is very low, the effect of interfacial reflection between the air and the moth-eye film is negligible. For the measurement, it was confirmed that there were no light-reflective objects within 1 m of the light-emitting / receiving part of the spectrophotometer in the direction of light propagation, and the measurement was performed in a sufficiently dark environment to eliminate the influence of ambient light. When the spectrophotometer was measured in this measurement environment without a measurement sample (laminated material), it was confirmed that the stimulus value Y was 0.1% or less. Therefore, when the stimulus value Y of the laminate is measured in the above measurement environment, the light detected by the spectrophotometer is only the light that has been partially absorbed by the polarizer and reflected by the high refractive index layer.
[0105] [Example 1] (Fabrication of polarizer (1)) A 20 μm thick polyvinyl alcohol-based resin film (average degree of polymerization approximately 2400, degree of saponification 99.9 mol% or higher) was uniaxially stretched to a stretch ratio of approximately 4.5 times by dry stretching. While maintaining tension after stretching, it was immersed in pure water at 30°C for 60 seconds. Subsequently, while maintaining tension, it was immersed in an iodine-potassium iodide aqueous solution with a mass ratio of iodine / potassium iodide / water of 0.05 / 5 / 100 and a temperature of 28°C for 60 seconds. Subsequently, while maintaining tension, it was immersed in a potassium iodide-boric acid aqueous solution with a mass ratio of potassium iodide / boric acid / water of 15 / 5.5 / 100 and a temperature of 64°C for 170 seconds. While maintaining tension, the film was washed with pure water at 10°C for 5 seconds, and then dried at 80°C in ambient air for 70 seconds while maintaining tension, to produce a polarizer (1) (linear polarization layer) with a thickness of 8 μm, in which iodine was adsorbed and oriented on a polyvinyl alcohol-based resin film. The luminous efficiency corrected single-unit transmittance Ty of this polarizer (1) was 42.2 ± 0.5%.
[0106] (Preparation of the first phase difference layer (1)) A 25 μm thick cyclic polyolefin resin film with a hard coat layer was prepared as the first phase difference layer (1). The in-plane phase difference value of the first phase difference layer (1) at a wavelength of 550 nm was 100 nm.
[0107] (Preparation of water-based adhesives) Three parts by mass of carboxyl group-modified polyvinyl alcohol [KL-318, manufactured by Kuraray Co., Ltd.] were dissolved in 100 parts by mass of water to obtain an aqueous polyvinyl alcohol solution. To this aqueous polyvinyl alcohol solution (100 parts by mass of water), 1.5 parts by mass of water-soluble polyamide epoxy resin [Sumirez Resin 650 (30), manufactured by Taoka Chemical Industry Co., Ltd., solid content concentration 30% by mass] (solid content 0.45 parts by mass) were added to obtain a water-based adhesive.
[0108] (Fabrication of linear polarizing plate (1)) A cyclic polyolefin resin film with a thickness of 13 μm was prepared as the first protective film. In addition, a triacetylcellulose resin film (KC4UY, manufactured by Konica Minolta, Inc., with a thickness of 40 μm) that had not been treated with saponification on its surface was prepared as the second protective film.
[0109] A first protective film (cyclic polyolefin resin film) prepared above was superimposed on one side of the polarizer (1) obtained above via the water-based adhesive obtained above, and a second protective film (triacetyl cellulose resin film) prepared above was superimposed on the other side of the polarizer (1) via pure water. The polarizer (1) was then passed between a pair of laminating rolls and heated and dried at 85°C for 3 minutes to cure the water-based adhesive and form an adhesive layer as a third laminating layer, thereby producing a linear polarizer (1) having a layer structure of first protective film / third laminating layer / polarizer (1) / second protective film. The in-plane phase difference value of the first protective film at a wavelength of 550 nm was 0 nm.
[0110] (Fabrication of high refractive index layers) A 100 μm thick ITO layer was formed by vacuum deposition on one side of an alkali-free glass plate (Corning Eagle XG, refractive index 1.50) to create an ITO layer. This resulted in a high refractive index layer, which is a laminated structure of the alkali-free glass plate and the ITO layer. The refractive index of this high refractive index layer was measured from the ITO layer side and found to be 2.00.
[0111] (Fabrication of laminate (1)) Next, the second protective film was peeled off the linear polarizer (1), and a moth-eye film (G.moth, manufactured by Geomatec) was laminated to the exposed polarizer (1) side via a fourth bonding layer (an acrylic adhesive layer with a thickness of 25 μm). Then, on the first protective film side of the linear polarizer (1), the second bonding layer (an acrylic adhesive layer with a thickness of 5 μm), the first phase difference layer (1), the first bonding layer (an acrylic adhesive layer with a thickness of 25 μm), a laminated structure of alkali-free glass plate with a refractive index of 1.50 (Eagle XG, refractive index 1.50) and a high refractive index layer (ITO layer) (refractive index 2.00), and a black acrylic plate were laminated in this order to create a laminate (1). The laminate (1) was laminated so that the high refractive index layer was on the black acrylic plate side. The space between the high refractive index layer and the black acrylic plate was filled with ethanol that had been dropped before lamination to eliminate the air layer. The first phase difference layer (1) was laminated such that the hard coat layer side was the high refractive index layer side. In the laminate (1), the angle between the slow axis of the first phase difference layer (1) and the absorption axis of the polarizer (1) of the linear polarizer (1) was 45°. The layer structure of the obtained laminate (1) was black acrylic plate / ethanol / high refractive index layer / first bonding layer / first phase difference layer (1) / second bonding layer / first protective film / third bonding layer / polarizer (1) / fourth bonding layer / moth-eye film. The results of measuring the stimulus value Y of the laminate (1) are shown in Table 1. The moth-eye film was provided so that the laminate (1) could be evaluated while ignoring the effect of interfacial reflection between the fourth bonding layer and the air layer. In an actual display device, the display unit is positioned on the opposite side of the polarizer (1) of the fourth bonding layer.
[0112] [Example 2] (Preparation of the first phase difference layer (2)) A cyclic polyolefin resin film with a thickness of 50 μm was prepared as the first phase difference layer (2). The in-plane phase difference value of the first phase difference layer (2) at a wavelength of 550 nm was 141 nm.
[0113] (Fabrication of laminate (2)) Laminate (2) was obtained using the same procedure as in Example 1, except that the first phase difference layer (2) was used instead of the first phase difference layer (1). The layer structure of the obtained laminate (2) was black acrylic plate / ethanol / high refractive index layer / first bonding layer / first phase difference layer (2) / second bonding layer / first protective film / third bonding layer / polarizer (1) / fourth bonding layer / moth-eye film. The results of measuring the stimulus value Y of laminate (2) are shown in Table 1.
[0114] [Example 3] (Preparation of composition for forming horizontally aligned films) A composition for forming a horizontally aligned film was obtained by mixing 5 parts by mass of a photo-oriented polymer with the following structure (described in Japanese Patent Publication No. 2013-33249) with 95 parts by mass of cyclopentanone (solvent) and stirring at a temperature of 80°C for 1 hour. • Photo-oriented polymer (5 parts by mass): [ka] • Solvent (95 parts by mass): Cyclopentanone
[0115] (Preparation of polymerizable liquid crystal composition (A1) for forming the first phase difference layer (3)) Polymerizable liquid crystal compound (X1) and polymerizable liquid crystal compound (X2) were mixed in a mass ratio of 90:10 to obtain a mixture. To 100 parts of the obtained mixture, 0.1 parts of the leveling agent "BYK-361N" (manufactured by BM Chemie) and 6 parts of 2-dimethylamino-2-benzyl-1-(4-morpholinophenyl)butan-1-one ("Irgacure® 369 (Irg369)" manufactured by BASF Japan Ltd.) were added as photopolymerization initiators. Furthermore, N-methyl-2-pyrrolidone (NMP) was added to achieve a solid content concentration of 13%. By stirring this mixture at 80°C for 1 hour, a polymerizable liquid crystal composition (A1) for forming the first phase difference layer (3) was obtained.
[0116] Polymerizable liquid crystal compound (X1): [ka]
[0117] Polymerizable liquid crystal compound (X2): [ka]
[0118] (Fabrication of the first phase difference layer (3)) After corona treatment on a COP (cyclic olefin resin) film (ZF-14-50) manufactured by Nippon Zeon Co., Ltd., the horizontal alignment film-forming composition obtained above was applied using a bar coater, dried at 80°C for 1 minute, and then subjected to integrated light intensity of 100 mJ / cm² at a wavelength of 313 nm using a polarized UV irradiation device (SPOT CURE SP-9; manufactured by Ushio Inc.). 2 Polarized UV exposure was performed to obtain a horizontally aligned film. The thickness of the obtained horizontally aligned film was measured with an ellipsometer and found to be 200 nm.
[0119] Next, the polymerizable liquid crystal composition (A1) obtained above was applied to the horizontal alignment film using a bar coater, heated at 120°C for 60 seconds, and then ultraviolet light was irradiated from the surface coated with polymerizable liquid crystal composition (A1) using a high-pressure mercury lamp (UniCure VB-15201BY-A, manufactured by Ushio Inc.) (under a nitrogen atmosphere, integrated light intensity at a wavelength of 365 nm: 500 mJ / cm²). 2 By doing so, a horizontally aligned liquid crystal layer (a cured layer of polymerizable liquid crystal compound) was formed, and a laminated structure (A1) having a layer structure of COP film / horizontally aligned film / horizontally aligned liquid crystal layer was obtained. After confirming that there was no phase difference in the COP film, the in-plane phase difference values Re(450) and Re(550) of the laminated structure (A1) at wavelengths of 450 nm and 550 nm were measured as the in-plane phase difference values Re(450) and Re(550) of the first phase difference layer (3), and Re(550) was found to be 139 nm. When Re(450) / Re(550) was calculated to be 0.87, it was confirmed that this laminate exhibits inverse wavelength dispersion.
[0120] The COP film of the laminated structure (A1) was peeled off, and the horizontal alignment film / horizontally aligned liquid crystal layer was used as the first phase difference layer (3).
[0121] (Fabrication of laminate (3)) Laminate (3) was obtained using the same procedure as in Example 1, except that the first phase difference layer (3) was used instead of the first phase difference layer (1). The first phase difference layer (3) was laminated so that the horizontally aligned film side was the high refractive index layer side. The layer structure of the obtained laminate (3) was black acrylic plate / ethanol / high refractive index layer / first bonding layer / first phase difference layer (3) / second bonding layer / first protective film / third bonding layer / polarizer (1) / fourth bonding layer / moth-eye film. The results of measuring the stimulus value Y of laminate (3) are shown in Table 1.
[0122] [Example 4] (Preparation of compositions for forming vertically aligned films) The silane coupling agent "KBE-9103" (manufactured by Shin-Etsu Chemical Co., Ltd.) was dissolved in a mixed solvent of ethanol and water in a ratio of 9:1 (by weight) to obtain a vertically aligned film-forming composition with a solid content of 1%.
[0123] (Preparation of polymerizable liquid crystal composition (A2) for forming the second phase difference layer (1)) To 100 parts of the polymerizable liquid crystal compound Paliocolor LC242 (a registered trademark of BASF), 0.1 parts of F-556 were added as a leveling agent, and 3 parts of Irgacure 369 were added as a polymerization initiator. Cyclopentanone was added to achieve a solid content concentration of 13% to obtain polymerizable liquid crystal composition (A2).
[0124] (Fabrication of the second phase difference layer (1)) After corona treatment was performed on a COP (cyclic olefin resin) film (ZF-14-50) manufactured by Nippon Zeon Co., Ltd., a composition for forming a vertically aligned film was applied using a bar coater and dried at 120°C for 1 minute to obtain a vertically aligned film. The thickness of the obtained vertically aligned film was measured with an ellipsometer and found to be 100 nm.
[0125] Next, the polymerizable liquid crystal composition (A2) obtained above was applied to the vertical alignment film using a bar coater, dried at 120°C for 1 minute, and then ultraviolet light was irradiated from the side coated with the polymerizable liquid crystal composition (A2) using a high-pressure mercury lamp (UniCure VB-15201BY-A, manufactured by Ushio Inc.) (under a nitrogen atmosphere, integrated light intensity at a wavelength of 365 nm: 500 mJ / cm²). 2 By doing so, a vertically aligned liquid crystal layer (a cured layer of polymerizable liquid crystal compound) was formed, and a laminated structure (A2) having a layer structure of COP film / vertically aligned film / vertically aligned liquid crystal layer was obtained. After confirming that there was no phase difference in the COP film, the thickness direction phase difference value Rth(550) of the laminated structure (A2) at a wavelength of 550 nm was measured as the thickness direction phase difference value Rth(550) of the second phase difference layer (1), and Rth(550) was found to be -70 nm.
[0126] The COP film and vertical alignment film of the laminated structure (A2) were peeled off, and the vertical alignment liquid crystal layer was used as the second phase difference layer (1).
[0127] (Fabrication of laminate (4)) The horizontally aligned liquid crystal layer side of the first phase difference layer (3), which was prepared using the same procedure as in Example 3, and the second phase difference layer (1) were bonded together using an ultraviolet-curing adhesive. The ultraviolet-curing adhesive was then cured to form an adhesive layer (1 μm thick) as the sixth bonding layer, thereby creating a phase difference laminate consisting of the second phase difference layer (1) / sixth bonding layer / first phase difference layer (3).
[0128] Laminate (4) was obtained using the same procedure as in Example 1, except that a phase difference laminate was used instead of the first phase difference layer (1). The phase difference laminate was laminated so that the second phase difference layer (1) side was the high refractive index layer (1) side. The layer structure of the obtained laminate (4) was black acrylic plate / ethanol / high refractive index layer / first bonding layer / second phase difference layer (1) / sixth bonding layer / first phase difference layer (3) / second bonding layer / first protective film / third bonding layer / polarizer (1) / fourth bonding layer / moth-eye film. The results of measuring the stimulus value Y of laminate (4) are shown in Table 1.
[0129] [Table 1]
[0130] [Example 5] (Fabrication of polarizer (2)) A 20 μm thick polyvinyl alcohol-based resin film (average degree of polymerization 2400, degree of saponification 99.9 mol% or higher) was uniaxially stretched to a stretch ratio of approximately 4.5 times by dry stretching. While maintaining tension after stretching, it was immersed in pure water at 30°C for 60 seconds. Subsequently, while maintaining tension, it was immersed in an iodine-potassium iodide aqueous solution with a mass ratio of iodine / potassium iodide / water of 0.02 / 5 / 100 and a temperature of 28°C for 60 seconds. Subsequently, while maintaining tension, it was immersed in a potassium iodide-boric acid aqueous solution with a mass ratio of potassium iodide / boric acid / water of 15 / 5.5 / 100 and a temperature of 64°C for 45 seconds. While maintaining tension, the film was washed with pure water at 10°C for 5 seconds, and while maintaining tension, it was dried at an ambient temperature of 80°C for 75 seconds to produce a polarizer (2) (linear polarizing layer) with iodine adsorbed and oriented on a polyvinyl alcohol-based resin film and a thickness of 8 μm. The luminous efficiency corrected single-unit transmittance Ty of this polarizer (2) was 46.0 ± 0.5%.
[0131] (Fabrication of laminate (5)) Laminate (5) was obtained using the same procedure as in Example 1, except that polarizer (2) was used instead of polarizer (1). The layer structure of the obtained laminate (5) was black acrylic plate / ethanol / high refractive index layer / first bonding layer / first phase difference layer (1) / second bonding layer / first protective film / third bonding layer / polarizer (2) / fourth bonding layer / moth-eye film. The results of measuring the stimulus value Y of laminate (5) are shown in Table 2.
[0132] [Example 6] Laminate (6) was obtained using the same procedure as in Example 2, except that polarizer (2) was used instead of polarizer (1). The layer structure of the obtained laminate (6) was black acrylic plate / ethanol / high refractive index layer / first bonding layer / first phase difference layer (2) / second bonding layer / first protective film / third bonding layer / polarizer (2) / fourth bonding layer / moth-eye film. The results of measuring the stimulus value Y of laminate (6) are shown in Table 2.
[0133] [Example 7] Laminate (7) was obtained using the same procedure as in Example 3, except that polarizer (2) was used instead of polarizer (1). The layer structure of the obtained laminate (7) was black acrylic plate / ethanol / high refractive index layer / first bonding layer / first phase difference layer (3) / second bonding layer / first protective film / third bonding layer / polarizer (2) / fourth bonding layer / moth-eye film. The results of measuring the stimulus value Y of laminate (7) are shown in Table 2.
[0134] [Example 8] Laminate (8) was obtained using the same procedure as in Example 4, except that polarizer (2) was used instead of polarizer (1). The layer structure of the obtained laminate (8) was black acrylic plate / ethanol / high refractive index layer / first bonding layer / second phase difference layer (1) / sixth bonding layer / first phase difference layer (3) / second bonding layer / first protective film / third bonding layer / polarizer (2) / fourth bonding layer / moth-eye film. The results of measuring the stimulus value Y of laminate (8) are shown in Table 2.
[0135] [Comparative Example 1] A laminate (9) was obtained in the same manner as in Example 5, except that the first phase difference layer (1) and the second lamination layer were not laminated, and the high refractive index layer was laminated on the first protective film via the first adhesive layer. The layer structure of the obtained laminate (9) was black acrylic plate / ethanol / high refractive index layer / first lamination layer / first protective film / third lamination layer / polarizer (2) / fourth lamination layer / moth-eye film. The results of measuring the stimulus value Y of the laminate (9) are shown in Table 2.
[0136] [Table 2]
[0137] The results shown in Tables 1 and 2 indicate that when the in-plane phase difference value of the first phase difference layer is in the range of 80 nm to 170 nm, the stimulus value Y decreases, and the reflected light incident on the photodetector of the display unit can be reduced. Furthermore, even when the luminous efficiency correction single transmittance Ty of the polarizer included in the laminate is large, the stimulus value Y can be reduced, and the reflected light incident on the photodetector of the display unit can be reduced. [Explanation of Symbols]
[0138] 1-4 Display device, 11 Linear polarization layer, 12 First protective film, 13 Third phase difference layer, 21 First bonding layer, 22 Second bonding layer, 23 Third bonding layer, 24 Fourth bonding layer, 25 Fifth bonding layer, 26 Sixth bonding layer, 31 First phase difference layer, 32 Second phase difference layer, 40 Display unit, 41 Display element, 42 Light receiving sensor, 45 High refractive index layer, 51-54 Optical laminate.
Claims
1. A display device having, from the viewing side, a high refractive index layer, a first phase difference layer, a linear polarization layer, and a display unit in this order, The refractive index of the aforementioned high refractive index layer is 1.60 or higher. The display unit has a display element and a light receiving sensor, A display device in which the first phase difference layer and the linear polarization layer are laminated so as to cover the display element and the light receiving sensor, and cover the entire viewing surface of the light receiving sensor.
2. The display device according to claim 1, wherein the first phase difference layer covers the entire visible side of the linear polarization layer in a plan view.
3. The display device according to claim 1 or 2, wherein the luminous efficiency correction single transmittance of the linearly polarized layer is 42% or more.
4. The display device according to claim 1 or 2, wherein the angle between the slow axis of the first phase difference layer and the absorption axis of the linear polarization layer is 10° or more and 80° or less.
5. The display device according to claim 1 or 2, wherein the in-plane phase difference value of the first phase difference layer at a wavelength of 550 nm is 80 nm or more and 170 nm or less.
6. The display device according to claim 5, wherein the first phase difference layer has inverse wavelength dispersion.
7. Furthermore, a second phase difference layer is provided between the high refractive index layer and the linear polarization layer. The second phase difference layer is laminated so as to cover the display element and the light receiving sensor. The display device according to claim 5, wherein the phase difference value in the thickness direction of the second phase difference layer at a wavelength of 550 nm is -140 nm or more and -20 nm or less.
8. The display device according to claim 1 or 2, wherein the stimulus value Y of the reflected light when the light emitted from the display element is reflected by the high refractive index layer is 3.45% or more and 4.54% or less.
9. The display device according to claim 1 or 2, wherein the light receiving sensor is capable of detecting light with a wavelength of 320 nm or more and 4000 nm or less.
10. The display device according to claim 1 or 2, wherein the light emitted from the display element has a wavelength of 320 nm or more and 4000 nm or less.
11. Furthermore, the display device according to claim 1 or 2, further comprising a third phase difference layer between the linear polarization layer and the display unit.
12. The display device according to claim 1 or 2, wherein the first phase difference layer and the linear polarization layer cover the entire viewing surface of the display element.
13. An optical laminate having a high refractive index layer, a first phase difference layer, and a linear polarization layer in this order, The refractive index of the aforementioned high refractive index layer is 1.60 or higher. An optical laminate in which the in-plane phase difference value of the first phase difference layer at a wavelength of 550 nm is 80 nm or more and 170 nm or less.
14. The optical laminate according to claim 13, wherein the first phase difference layer covers the entire visible side of the linear polarization layer in a plan view.
15. The optical laminate according to claim 13 or 14, wherein the luminous efficiency correction single transmittance of the linearly polarized layer is 42% or more.
16. The optical laminate according to claim 13 or 14, wherein the angle between the slow axis of the first phase difference layer and the absorption axis of the linear polarization layer is 10° or more and 80° or less.
17. The optical laminate according to claim 13 or 14, wherein the first phase difference layer has inverse wavelength dispersion.
18. Furthermore, a second phase difference layer is provided between the high refractive index layer and the linear polarization layer. The optical laminate according to claim 13 or 14, wherein the phase difference value in the thickness direction of the second phase difference layer at a wavelength of 550 nm is -140 nm or more and -20 nm or less.
19. The optical laminate according to claim 13 or 14, further comprising a third phase difference layer on the side of the linearly polarized layer opposite to the first phase difference layer side.
Citation Information
Patent Citations
Display panel and display equipment
CN112054044A
Polarizing film, polarizing film with adhesive layer, and image display device
JP2019219528A
Liquid crystal display
JP2020201510A
Fingerprint sensor, display device including the same, and method of operating fingerprint sensor
US20190034688A1
Electronic device with optical sensor
US20190102595A1