Humidity-adaptive vapor barrier
A PA-based humidity-adaptive vapor barrier with a PA reinforcing layer ensures recyclability by eliminating auxiliary agents, addressing the separation challenges of multi-layer barriers and promoting material reuse.
Patent Information
- Application Number
- JP2024030884
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2023-03-13
- Filing Date
- 2024-03-01
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2044-03-01
AI Technical Summary
Existing humidity-adaptive vapor barriers combining polyamide (PA) with other materials like PE, PET, or PP face challenges in recyclability due to the difficulty in separating the layers after use.
A humidity-adaptive vapor barrier composed of a PA functional layer and a PA reinforcing layer, connected without auxiliary agents, ensuring high recyclability by using the same PA material for both layers, with optional adhesive use limited to ≤5 g/m² to maintain recyclability.
The solution provides a mechanically reinforced vapor barrier with enhanced recyclability, allowing for high-value material reuse and effective moisture management in buildings.
Abstract
Description
[Background technology]
[0001] Humidity-adaptive vapor barriers, used for thermal insulation in buildings, particularly in new construction and renovation of older buildings, are known, for example, from the attribute-corresponding German Patent No. 195 14 420.
[0002] The humidity-adaptive vapor barrier described therein includes a single layer of functional material in the form of a polyamide film (PA film) with a film thickness ranging from 20 to 100 μm. This humidity-adaptive vapor barrier ensures water vapor exchange between indoor air and the interior of building components under various environmental conditions, and prevents damage to building materials used due to moisture, strictly speaking, S d It can be eliminated as much as possible by humidity-adaptive water vapor diffusion resistance, which is expressed as a value. S of the vapor barrier in German Patent Invention No. 195 14 420 d The values indicate that when the relative humidity surrounding the vapor barrier is in the range of 30-50%, the equivalent diffusion air layer thickness is on the order of 2-5m, and when the relative humidity is in the range of 60-80%, the equivalent diffusion air layer thickness is less than 1m. Therefore, the resistance to water vapor diffusion is higher in winter conditions than in summer conditions, which means that the supply of moisture does not damage materials and buildings under winter conditions, while the drying of building components is promoted in summer.
[0003] In German Patent No. 195 14 420, the functional layer can exist as a film or as a coating on a carrier material. Fiber-reinforced cellulose material, films made from synthetic fiber spun woven fabrics, or perforated polyethylene films are proposed as carrier materials, which can be further coated with polymers such as modified polyvinyl alcohol, plastic dispersions, methylcellulose, linseed oil alkyd, bone linseed, or protein derivatives. The carrier material has low water vapor diffusion resistance and serves to protect the vapor barrier from mechanical influences, for example.
[0004] Advanced forms of humidity-adaptive vapor barriers relate, for example, to sandwich-like structures of composite films consisting of a core layer made of PA and an outer layer made of another material. European Patent Application Publication No. 3 088 174 describes a configuration in which, for example, two outer layers made of PA material house a layer made of another humidity-adaptive material, thereby providing a higher S-value than the case of PA material alone. d The vapor barrier, which has a wide range of values, is described.
[0005] International Publication No. 2014 / 118241 describes a humidity-adaptive vapor barrier in which a PA layer is combined with a non-polar layer made of PE. The vapor barrier is humidity-variable, and the combination of layers in this vapor barrier makes it direction-sensitive with respect to water vapor permeability. Thus, undesirable movement of moisture into the structure is prevented, and this vapor barrier can be used to dry humid spaces such as kitchens and bathrooms. International Publication No. 2014 / 118241 intends to optionally include a reinforcing layer which may be made of PA-based nonwoven fabric material in particular, but due to the special structure of the invention, the vapor barrier always has (at least) two material properties.
[0006] A drawback of vapor barriers combining a functional layer made of PA with a reinforced layer made of PE, PET, or PP is their limited recyclability. These layers become difficult to separate after use. [Overview of the Initiative] [Problems that the invention aims to solve]
[0007] The object of the present invention is to provide a humidity-adaptive vapor barrier with a functional layer made of PA material that is mechanically reinforced and meets higher requirements regarding recyclability. [Means for solving the problem]
[0008] The humidity-adaptive vapor barrier according to the present invention comprises a functional layer in the form of a film made of PA material, a reinforcing layer made of further PA material, preferably the same PA material as the functional layer, an auxiliary layer, particularly an adhesive layer, optionally disposed between the functional layer and the reinforcing layer, and further optionally printing. Preferably, in this case, the side of the film-like functional layer opposite to the reinforcing layer is optionally printed.
[0009] The present invention provides a composite material having a functional layer and a reinforcing layer, wherein both the functional layer and the reinforcing layer are made from polyamide. Preferably, the functional layer and the reinforcing layer are made from the same PA material. This is advantageous as it enables the recycling of different types of humidity-adaptive vapor barriers, i.e., high-value material reuse to obtain marketable secondary raw materials. Hereinafter, the functional layer in the form of a film made of PA material will also be referred to as a PA film.
[0010] The PA film and the PA reinforcing layer together form a flexible, preferably flat, and in some embodiments, elastic, structure that is mechanically reinforced compared to a single PA film. In this case, the PA reinforcing layer abuts the PA film across its entire surface, i.e., the film and the reinforcing layer overlap each other. Thus, the humidity-adaptive vapor barrier can be understood as a layered structure, with the reinforcing layer positioned on the film. [Modes for carrying out the invention]
[0011] Purity of materials for recyclability The purity of raw materials is extremely important for the quality of recycled products.
[0012] Therefore, the connection of the functional layer to the reinforcing layer is preferably achieved by a method that does not use auxiliary agents, particularly by melting, welding, lamination, or embossing. In this case, any auxiliary layer can be advantageously omitted.
[0013] In alternative embodiments, the functional layer can be connected to the reinforcing layer using an auxiliary agent, particularly an adhesive, which can be applied, for example, in dots, lines, or surfaces. The amount of the auxiliary agent, particularly the adhesive, should not hinder high-value recycling, preferably ≤5 g / m². 2 It is preferable to use it in this way.
[0014] In terms of high-value material recycling, it is preferable to keep the mass content of optional adhesives and / or optional printing as low as possible. The mass content is preferably ≤10%, particularly ≤7%, particularly ≤5%, ≤3%, or even ≤1% relative to the mass of the vapor barrier. With regard to material recycling, it is particularly preferable to avoid the use of adhesives and printing.
[0015] In other words, according to the present invention, the humidity-adaptive vapor barrier according to the present invention comprises a functional layer made of PA material, a reinforcing layer made of further PA material, preferably the same PA material as the functional layer, an auxiliary layer optionally placed between the functional layer and the reinforcing layer to connect the functional layer and the reinforcing layer, and further optionally printing, wherein the vapor barrier is made of PA material with a content of ≥90%, preferably ≥93%, particularly preferably ≥95%, even more preferably ≥97%, and most preferably ≥99%.
[0016] reinforcement layer The reinforcing layer may exist in the form of a nonwoven layer, woven fabric, woven mat, and / or mesh woven fabric. In particular, the reinforcing layer may be a nonwoven fabric reinforced with woven fabric, woven mat, or mesh woven fabric.
[0017] Nonwoven fabrics are also commonly referred to in the technical field simply as "nonwovens", and woven fabrics as "wovens". Within the scope of the present disclosure, a nonwoven fabric (nonwoven) is understood as a flat, flexible formation. The structural elements of a nonwoven fabric form fibers of limited length. Usually, the fibers are interlaced, in particular felted. The fibers are usually not present in a regular configuration such as, for example, in a spun woven fabric (woven). The production of the nonwoven fabric is preferably carried out by needling, but can also be carried out, for example, by hydroentanglement or chemical methods. A person skilled in the art is aware of numerous possibilities for producing nonwoven fabrics and woven fabrics.
[0018] A reinforcing layer in the form of a nonwoven fabric layer made of a further PA material is also referred to below as PA nonwoven, and in the form of a woven fabric, woven mat and / or mesh woven fabric made of a further PA material, also referred to as PA woven fabric.
[0019] It should always be understood that the PA materials of the PA film, PA nonwoven and PA woven fabric may be different, but are preferably identical.
[0020] Properties of the Material Layers The PA film, and the PA nonwoven and PA woven fabric have a humidity-variable S d value. However, due to the diffusion openness of nonwoven and woven fabrics, whose S d value usually has a diffusion-equivalent air layer thickness of less than 0.05 m, the humidity variability of the PA nonwoven or PA woven fabric is negligible compared to the PA film. As already described in German Patent No. 195 14 420, the humidity-adaptable vapor barrier can be used advantageously for the thermal insulation of new buildings and for the renovation of old buildings. This humidity-adaptable vapor barrier does not exhibit moisture behavior other than the embodiments described in German Patent No. 195 14 420.
[0021] The material of the PA film is preferably PA3, PA4, PA6, PA6.6, PA4.6, or a combination thereof. The material of the PA film is particularly preferably PA6 or PA6.6, or a combination thereof.
[0022] The layer thickness of the PA film is preferably 20 μm to 100 μm. In particular, films of all types of materials as described in German Patent No. 195 14 420, especially films consisting exclusively of polyamide 6 with a film thickness of 50 μm as described in German Patent No. 195 14 420, are also suitable.
[0023] The PA nonwoven fabric also includes nonwoven fibers made of PA material, preferably PA3, PA4, PA6, PA6.6 or PA4.6, or combinations thereof. PA6 or PA6.6, or a combination thereof, is particularly preferred here.
[0024] The layer thickness of the PA nonwoven fabric is preferably 150 μm to 2000 μm. The PA woven fabric consists of (continuous) woven fibers made of PA material, preferably PA3, PA4, PA6, PA6.6 or PA4.6, or combinations thereof. PA6 or PA6.6, or a combination thereof, is particularly preferred here.
[0025] The layer thickness of the PA woven fabric is preferably of the same order as the layer thickness of the PA nonwoven fabric, and is 100 μm to 2000 μm.
[0026] Properties of the vapor barrier The materials and layer thicknesses of the PA nonwoven fabric, PA woven fabric and PA film are preferably selected such that the S d value of the humidity-adaptive vapor barrier is humidity-variable at an equivalent air layer thickness of preferably 0.1 to 7 m, particularly preferably 0.3 to 5 m, and strictly speaking, variable with respect to the average relative humidity. In this case, S d The value is measured in accordance with DIN EN ISO 12572:2017-05. In this case, S d As is known, the value is defined by the water vapor diffusion resistance coefficient μ and the layer thickness used.
[0027] S dValue [m] = water vapor diffusion resistance coefficient μ × layer thickness [m]. The vapor barrier is provided as a roll having a width of, for example, 0.2m to 2m, preferably 0.5m to 1.5m. The length can be, for example, 10 to 50m, preferably 20 to 40m. The vapor barrier is preferably 30 to 60m 2 It is provided as a roll having a web area.
[0028] The basis weight of the vapor barrier is preferably 50 to 500 g / m². 2 Preferably 70-100 g / m 2 Particularly preferably about 80 g / m 2 Therefore, the steam barrier is also suitable for use on sloped roofs.
[0029] The maximum tensile force of the vapor barrier is preferably greater than 80 N, and more preferably >110 N. The maximum tensile force is determined in accordance with DIN EN ISO 13984:2013-05. Therefore, the vapor barrier is also advantageously suited for use on sloped roofs.
[0030] According to one embodiment, the humidity-adaptive vapor barrier has a UV additive. In one embodiment, the humidity-adaptive vapor barrier is coated to enable, for example, UV resistance to direct irradiation for at least three months. The UV additive is added and mixed in small amounts so as not to hinder high-value recycling, and the proportion of the UV additive is preferably less than 0.2% of the total PA mass of the vapor barrier.
[0031] Alternative functional layer According to a further aspect of the present invention, the material of the functional layer is not limited to PA.
[0032] The functional layer, in principle, has humidity adaptability S dIt can be formed from any material having a value, in particular from, for example, ionomers, EVOH, PVOH, or generally polar materials. In terms of high-value material recycling, according to the present invention, the reinforcing layer is intended to consist of the same material as the functional layer, or at least the same material class. In other respects, the humidity-adaptive vapor barrier can be formed as described above.
[0033] Examples of ionomer-containing layer materials used in humidity-adaptive vapor barriers are disclosed in European Patent Application Publication No. 1372956. In practice, ionomers are marketed, for example, by DuPont under the Surlyn trademark. Examples of humidity-adaptive vapor barriers having functional layers containing EVOH and / or PVOH are disclosed in U.S. Patent Application Publication No. 2007 / 015424. Further examples of polar materials used in humidity-adaptive vapor barriers are polyethylene (PE) or polypropylene (PP) films containing acrylic acid as a polar component.
[0034] According to yet another aspect of the present invention, the vapor barrier (not humidity-adaptive) may also consist of a functional layer in the form of a film made of a material, particularly PE or PP, a reinforcing layer made of the same material, optionally an auxiliary layer placed between the functional layer and the reinforcing layer to connect the functional layer and the reinforcing layer, and further optionally printing.
[0035] Therefore, in that case, the above descriptions regarding the implementation of the reinforcing layer as a (possibly reinforced) nonwoven layer, woven fabric, woven mat and / or mesh woven fabric, connecting the reinforcing layer to the functional layer with or without the use of auxiliary agents, the thickness of the layer, and in particular the description regarding the purity of the vapor barrier also apply to other embodiments of the functional layer made of materials other than PA.
Claims
1. A humidity-adaptive vapor barrier comprising exactly three layers: a functional layer in the form of a film made of PA material, a reinforcing layer made of further PA material, and an auxiliary layer disposed between the functional layer and the reinforcing layer to connect the functional layer and the reinforcing layer, wherein the mass content of the auxiliary layer is ≤10% of the mass of the vapor barrier.
2. The humidity-adaptive vapor barrier according to claim 1, wherein the mass content of the auxiliary layer is ≤ 7% of the mass of the vapor barrier.
3. The humidity-adaptive vapor barrier according to claim 1, wherein the mass content of the auxiliary layer is ≤ 5% of the mass of the vapor barrier.
4. The humidity-adaptive vapor barrier according to claim 1, wherein the mass content of the auxiliary layer is ≤3% of the mass of the vapor barrier.
5. The humidity-adaptive vapor barrier according to claim 1, wherein the mass content of the auxiliary layer is ≤ 1% of the mass of the vapor barrier.
6. A humidity-adaptive vapor barrier comprising exactly two layers: a functional layer in the form of a film made of PA material and a reinforcing layer made of the same PA material as the functional layer, wherein the functional layer is connected to the reinforcing layer by a method that does not use auxiliary agents.
7. A humidity-adaptive vapor barrier according to claim 1 or 6, further comprising printing, wherein the mass content of the printing is ≤ 10% of the mass of the vapor barrier.
8. The humidity-adaptive vapor barrier according to claim 7, wherein the mass content of the printing is ≤ 7% of the mass of the vapor barrier.
9. The humidity-adaptive vapor barrier according to claim 7, wherein the mass content of the printing is ≤ 5% of the mass of the vapor barrier.
10. The humidity-adaptive vapor barrier according to claim 7, wherein the mass content of the printing is ≤ 3% of the mass of the vapor barrier.
11. The humidity-adaptive vapor barrier according to claim 7, wherein the mass content of the printing is ≤ 1% of the mass of the vapor barrier.
12. A humidity-adaptive vapor barrier comprising exactly two layers: a functional layer in the form of a film made of PA material and a reinforcing layer made of further PA material, wherein the functional layer is connected to the reinforcing layer by a method without the use of auxiliary agents, and the humidity-adaptive vapor barrier further comprises printing, wherein the mass content of the printing is ≤10% of the mass of the vapor barrier.
13. The humidity-adaptive vapor barrier according to claim 12, characterized in that the mass content of the printing is ≤ 7% of the mass of the vapor barrier.
14. The humidity-adaptive vapor barrier according to claim 12, characterized in that the mass content of the printing is ≤ 5% of the mass of the vapor barrier.
15. The humidity-adaptive vapor barrier according to claim 12, characterized in that the mass content of the printing is ≤ 3% of the mass of the vapor barrier.
16. The humidity-adaptive vapor barrier according to claim 12, characterized in that the mass content of the printing is ≤ 1% of the mass of the vapor barrier.
17. The humidity-adaptive vapor barrier according to claim 1, claim 6, or claim 12, characterized in that the reinforcing layer exists in the form of a nonwoven fabric layer, a woven fabric, a woven mat, and / or a mesh woven fabric.
18. The humidity-adaptive vapor barrier according to claim 1, claim 6, or claim 12, characterized in that the reinforcing layer is a woven fabric, a woven mat, or a nonwoven fabric reinforced with a mesh woven fabric.
19. The humidity-adaptive vapor barrier according to claim 1, claim 6, or claim 12, characterized in that the PA material of the film is PA3, PA4, PA6, PA6.6, PA4.6, or a combination thereof.
20. The humidity-adaptive vapor barrier according to claim 17, characterized in that the material of the nonwoven fabric and / or the woven fabric is PA3, PA4, PA6, PA6.6, PA4.6, or a combination thereof.
21. The humidity-adaptive vapor barrier according to claim 18, characterized in that the material of the nonwoven fabric and / or the woven fabric is PA3, PA4, PA6, PA6.6, PA4.6, or a combination thereof.
22. The humidity-adaptive vapor barrier according to claim 1 or claim 12, characterized in that the PA material of the reinforcing layer is the same polyamide as the functional layer or the same combination.
23. S of the humidity-adaptive vapor barrier d The humidity-adaptive vapor barrier according to claim 1, claim 6, or claim 12, characterized in that the value is variable in humidity from 0.1 to 7 m.
Citation Information
Patent Citations
plasterable adhesive tape and use
DE102017105028A1
Insulation system for industrial installations
JP2007508511A
Humidity-variable directional moisture-proof material
JP2016511343A