Separation membrane system and method for heating a separation membrane
The system detects membrane abnormalities by supplying a mixed gas of polar and nonpolar gases to heat and measure the nonpolar gas flow rate, addressing the sensitivity challenge in existing systems.
Patent Information
- Application Number
- JP2024570163
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2023-05-17
- Filing Date
- 2023-12-28
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2043-12-28
AI Technical Summary
Existing separation membrane systems struggle to detect abnormalities such as seal leaks, defect leaks, or membrane ruptures with high sensitivity during preparation and use.
A separation membrane system that supplies a mixed gas of polar and nonpolar gases to the membrane, utilizing a heating device and measuring the flow rate of the nonpolar gas permeated through the membrane to detect abnormalities.
Enables early and sensitive detection of membrane abnormalities by efficiently heating the membrane and correlating flow rate changes with membrane integrity issues.
Smart Images

Figure 0007954733000001 
Figure 0007954733000002 
Figure 0007954733000003
Abstract
Description
TECHNICAL FIELD
[0001] The present invention relates to a separation membrane system and a method for raising the temperature of a separation membrane.
BACKGROUND ART
[0002] Conventionally, various methods aimed at separating a desired component from a fluid containing two or more types of components have been studied. As such a method, for example, a method using a separation membrane capable of selectively permeating a specific component is known. In such a separation method using a separation membrane, an abnormality of the separation membrane (e.g., seal leak, defect leak, membrane rupture) may occur during preparation for use and / or during use, and it is required to detect the abnormality at an early stage with high sensitivity.
RELATED ART DOCUMENTS
PATENT DOCUMENTS
[0003]
PATENT DOCUMENT 1
PATENT DOCUMENT 2
SUMMARY OF THE INVENTION
PROBLEMS TO BE SOLVED BY THE INVENTION
[0004] A main object of the present invention is to provide a separation membrane system including a separation membrane, which is capable of detecting an abnormality of the separation membrane at an early stage with high sensitivity.
MEANS FOR SOLVING THE PROBLEMS
[0005] [1] A separation membrane system according to an embodiment of the present invention includes: a supply line that supplies a mixed gas of a polar gas and a nonpolar gas to a separation membrane; and a measuring instrument that measures a flow rate of the nonpolar gas that has permeated through the separation membrane. [2] In the separation membrane system according to the above [1], the mixed gas may be a heated gas. [3] In the separation membrane system described in [2] above, the separation membrane system may be equipped with a heating device upstream of the separation membrane. [4] In the separation membrane system described in any of [1] to [3] above, the separation membrane may be a zeolite membrane. [5] A method for heating a separation membrane according to an embodiment of the present invention includes the steps of supplying a heated mixed gas of a polar gas and a nonpolar gas to a separation membrane, and measuring the flow rate of the nonpolar gas that has permeated the separation membrane. [6] In the method for raising the temperature of the separation membrane described in [5] above, the concentration of the nonpolar gas supplied to the separation membrane may be less than 50% by volume. [7] In the method for raising the temperature of the separation membrane described in [5] or [6] above, the concentration of the nonpolar gas supplied to the separation membrane may be less than 25% by volume. [Effects of the Invention]
[0006] According to embodiments of the present invention, a separation membrane system comprising a separation membrane can be provided that can sensitively and early detect abnormalities in the separation membrane. [Brief explanation of the drawing]
[0007] [Figure 1] This is an explanatory diagram illustrating an overview of a separation membrane system according to one embodiment of the present invention. [Figure 2] This is an explanatory diagram illustrating the schematic configuration of a separation membrane complex in one embodiment of the present invention. [Figure 3] This is a schematic cross-sectional view showing the configuration of a separation membrane complex in one embodiment of the present invention. [Modes for carrying out the invention]
[0008] A. Separation membrane system Figure 1 is an explanatory diagram illustrating an overview of a separation membrane system according to one embodiment of the present invention. The separation membrane system 100 comprises a supply line 20 for supplying a mixed gas of a polar gas and a nonpolar gas to a separation membrane 1, and a measuring instrument 30 for measuring the flow rate of the nonpolar gas that has permeated through the separation membrane 1. In one embodiment, the separation membrane may constitute a separation membrane composite 10. The separation membrane 1 can separate the mixed fluid supplied to it based on its permeability. Figure 1 schematically shows an embodiment in which the mixed gas is supplied to a cylindrical separation membrane 1, and the flow rate of the nonpolar gas in the gas that has permeated through the separation membrane (permeated gas) is measured by the measuring instrument 30. In this specification, a polar gas is a gas containing molecules made up of atoms of different types with different electronegativity. Examples of polar gases include CO2, NH3, H2O, and CO. A nonpolar gas is a gas composed of monatomic molecules or molecules made up of atoms of the same type with equal electronegativity. Examples of nonpolar gases include He, H2, and N2. In one embodiment, a polar gas may be a gas composed of polar molecules, and a nonpolar gas may be a gas composed of nonpolar molecules. In other words, in one embodiment, a polar gas may be a gas in which the molecules constituting the gas have an electric dipole moment, and a nonpolar gas may be a gas in which the molecules constituting the gas do not have an electric dipole moment.
[0009] In the above-described separation membrane system, the flow rate of nonpolar gas permeating through the separation membrane can be measured, allowing for the detection of abnormalities in the separation membrane based on the flow rate of the nonpolar gas. Specifically, if the flow rate of nonpolar gas permeating through the separation membrane exceeds a predetermined value, it can be determined that there is an abnormality such as a seal leak or membrane crack. Conversely, if the flow rate of nonpolar gas is less than a predetermined value, it can be determined that there is an abnormality such as clogging or deterioration of the membrane material. Since the contribution of adsorption to the permeability of the separation membrane of nonpolar gas is small, the temperature dependence of the permeation rate is low, and there is a high correlation between abnormalities in the separation membrane permeation flow rate and abnormalities in the separation membrane. Therefore, by supplying a mixed gas containing nonpolar gas to the separation membrane and measuring the flow rate of the nonpolar gas, abnormalities in the separation membrane can be detected early and with high sensitivity. In particular, as described later, when heated gas is used as the mixed gas, the effects of this embodiment of the present invention become especially pronounced.
[0010] In one embodiment, the mixed gas supplied to the separation membrane may be a heated gas. In this embodiment, typically, an arbitrary suitable heating device (not shown) may be provided upstream of the separation membrane. For example, the supply line may be equipped with an arbitrary suitable heating device (not shown). In this specification, a heated gas is a gas at or above room temperature, for example, a gas at 100°C or higher, preferably 120°C or higher, and more preferably 150°C or higher.
[0011] In one embodiment, the separation membrane is heated by a heated mixed gas. Polar gases have high affinity and adsorption properties to the separation membrane, and therefore, by using a gas containing a polar gas as the mixed gas, the separation membrane can be heated efficiently. On the other hand, polar gases have a high temperature dependence on the permeability of the separation membrane, making it difficult to detect abnormalities in the separation membrane from the permeation flow rate of the polar gas through the separation membrane. In the present invention, by configuring the system so that a mixed gas of polar gas and non-polar gas is supplied to the separation membrane, abnormalities in the separation membrane can be detected sensitively and early, as described above.
[0012] Examples of nonpolar gases include He, H2, and N2. From the viewpoint of low adsorption to the separation membrane and lower temperature dependence of the separation membrane permeability, He and H2 are preferably used. The concentration of the nonpolar gas in the mixed gas supplied to the separation membrane is not particularly limited, but it is preferably a concentration that can be accurately measured by an analyzer. In one embodiment, the concentration of the nonpolar gas in the mixed gas supplied to the separation membrane may be 0.001 volume% or more. At such a concentration, the concentration can preferably be measured by GC-TCD, for example. In one embodiment, the concentration of the nonpolar gas in the mixed gas supplied to the separation membrane may be 1 volume% or more. At such a concentration, the concentration can preferably be measured by online measurement using a thermal conduction gas analyzer, for example. Furthermore, the concentration of the nonpolar gas in the mixed gas supplied to the separation membrane is preferably 50 volume% or less, more preferably less than 50 volume%, even more preferably less than 25 volume%, and particularly preferably less than 10 volume%. Within this range, the effects of the present invention can be achieved while efficiently heating the separation membrane with a polar gas.
[0013] The gas used as the nonpolar gas is preferably one that has a dynamic molecular diameter smaller than the average pore diameter of the separation membrane. Since such gases permeate the separation membrane easily, the effects of the embodiments of the present invention are particularly pronounced.
[0014] The gas used as a nonpolar gas has a permeation rate (mol / m³) at 100°C. 2 ( / s / Pa) is the permeation rate (mol / m³) at P100, 200℃. 2 When P200 is defined as ( / s / Pa), it is preferable that the rate of change in permeation rate, expressed as |P100-P200| / P100, is 0.6 or less. Within this range, the effects of the above embodiment of the present invention become significant. The above permeation rate can be calculated by introducing the gas to be measured into the primary side of the separation membrane at 100 kPaG and measuring the permeation flow rate when the secondary side of the separation membrane is held at 0 kPaG. At this time, P100 and P200 can be measured by controlling the temperature of the separation membrane to 100°C and 200°C.
[0015] Examples of the polar gas include CO₂ and the like. In the mixed gas supplied to the separation membrane, the concentration of the polar gas is preferably higher than 50% by volume. Within such a range, the effect of the present invention can be exhibited while efficiently heating the separation membrane with the polar gas.
[0016] In one embodiment, the separation membrane composite may be configured in a tubular shape. When the fluid to be treated is introduced into the inner side of the tubular structure of the separation membrane composite at a predetermined introduction pressure (for example, 0.5 MPa or higher), the fluid that permeates the separation membrane composite (substantially the separation membrane) is delivered from the surface of the separation membrane composite, while the non-permeating fluid can be passed in the longitudinal direction of the tubular separation membrane composite, and as a result, separation of the fluid to be treated becomes possible. The separation membrane composite may be composed of a single tubular structure or a plurality of tubular structures. Preferably, the separation membrane composite includes a plurality of tubular cells penetrating in the longitudinal direction.
[0017] Figure 2 is an explanatory view schematically showing the configuration of a separation membrane composite according to one embodiment of the present invention. Figure 3 is a schematic cross-sectional view showing the configuration of a separation membrane composite according to one embodiment of the present invention. A plurality of cells 11 are formed in the separation membrane composite 10. The cells 11 are formed in a tubular shape so as to penetrate the separation membrane composite 10 in the longitudinal direction. The cells 11 can serve as flow paths for the fluid to be treated. The separation membrane composite 10 includes a separation membrane 1, and the separation membrane 1 is provided on a porous base material 2. In one embodiment, the separation membrane 1 may be provided so as to cover substantially the entire inner side surface (i.e., the cell side surface) of the porous base material 2. Among the fluids to be treated that pass through the cells 11, the fluid with high permeability to the separation membrane 1 (permeating fluid) permeates the separation membrane composite 10 and is delivered from the side surface 13 of the separation membrane composite 10. On the other hand, the fluid with low permeability to the separation membrane 1 (non-permeating fluid) is delivered through the flow paths of the cells 11. Although not illustrated, the above separation membrane composite can be used by being housed in any appropriate outer cylinder.
[0018] In order to exert the separation function as described above, it is preferable to heat the separation membrane composite 10 (substantially the separation membrane 1) before supplying the fluid to be treated. At the time of the temperature increase, as described above, if the mixed gas of the polar gas and the non-polar gas is supplied to the separation membrane 1, the temperature of the separation membrane can be increased efficiently, and an abnormality in the separation membrane can be detected at an early stage with high sensitivity. The mixed gas of the polar gas and the non-polar gas may be a gas composed of the same components as the fluid to be treated, or may be a gas composed of different components.
[0019] The length of the separation membrane composite is, for example, 10 cm to 200 cm. The outer diameter of the separation membrane composite is, for example, 0.5 cm to 30 cm. The distance between the central axes of adjacent cells is, for example, 0.3 mm to 10 mm. The inner diameter of the cell is, for example, 1 mm to 10 mm.
[0020] (Separation Membrane) In one embodiment, the separation membrane can separate a mixed fluid by the difference in permeability to the separation membrane having micropores. For example, the fluid to be treated can be separated by a so-called molecular sieving action that controls the permeability depending on the size of the molecules constituting the fluid and the pore diameter of the separation membrane.
[0021] Preferably, the separation membrane is an inorganic membrane. Examples of the material constituting the separation membrane include zeolite, silica, carbon and the like. Since the separation membrane composed of the inorganic membrane is used at a high temperature, the possibility of occurrence of an abnormality tends to increase. However, by using the separation membrane system, an abnormality in the separation membrane can be detected at an early stage with high sensitivity.
[0022] In one embodiment, a zeolite membrane is used as the separation membrane. The zeolite membrane is configured by forming zeolite in a film form on the surface of a porous base material. The zeolite membrane may contain two or more types of zeolites different in structure and composition.
[0023] The zeolite constituting the above zeolite film can be any zeolite in which the central atom (T atom) of the oxygen tetrahedron (TO4) constituting the zeolite is only Si, or composed of Si and Al, AlPO type zeolite in which the T atom is composed of Al and P, SAPO type zeolite in which the T atom is composed of Si, Al and P, MAPSO type zeolite in which the T atom is composed of magnesium (Mg), Si, Al and P, or ZnAPSO type zeolite in which the T atom is composed of zinc (Zn), Si, Al and P. Some of the T atoms may be substituted with other elements.
[0024] Examples of the above-mentioned zeolites include AEI type, AEN type, AFN type, AFV type, AFX type, BEA type, CHA type, DDR type, ERI type, ETL type, FAU type (X type, Y type), GIS type, LEV type, LTA type, MEL type, MFI type, MOR type, PAU type, RHO type, SAT type, and SOD type. The maximum number of rings in the zeolite is preferably 12 or less, more preferably 10 or less, and even more preferably 8 or less. It is also preferably 6 or more, and even more preferably 8 or more.
[0025] The above-mentioned zeolite film contains, for example, Si. The zeolite film may contain, for example, two or more of Si, Al, and P. The zeolite film may also contain alkali metals. The alkali metals are, for example, sodium (Na) or potassium (K). When the zeolite film contains Si atoms and Al atoms, the Si / Al ratio in the zeolite film is, for example, 1 or more and 100,000 or less. The Si / Al ratio is the molar ratio of Si elements to Al elements contained in the zeolite film. The Si / Al ratio is preferably 5 or more, more preferably 20 or more, and even more preferably 100 or more, and the higher the ratio, the better. The Si / Al ratio in the zeolite film can be adjusted by adjusting the mixing ratio of Si source and Al source in the raw material solution, as described later.
[0026] The average pore size of the above separation membrane is, for example, 0.2 nm to 1 nm, and more preferably 0.3 nm to 0.5 nm. The pore size of the separation membrane can be adjusted according to the desired composition of the permeable fluid. Reducing the average pore size of the separation membrane increases selectivity. The average pore size of the separation membrane is smaller than the average pore size of the porous substrate. If the separation membrane is a zeolite membrane, the average pore size is defined as the arithmetic mean of the short and long axes of the n-membered ring pores, with n being the maximum number of member rings in the zeolite. An n-membered ring pore is a pore in which the number of oxygen atoms in the ring structure formed by oxygen atoms bonded with T atoms is n. If there are multiple n-membered ring pores with equal n, the average pore size of the zeolite is defined as the arithmetic mean of the short and long axes of all n-membered ring pores. The average pore size of a zeolite membrane is determined by the skeletal structure of the zeolite, and can be found in the International Zeolite Society's "Database of Zeolite Structures" [online], and the Internet.<URL:http: / / www.iza-structure.org / databases / > It can be determined from the values disclosed. Alternatively, it can be estimated by measuring the permeability of gases with different molecular diameters. One such method is described in Japanese Patent Application Publication No. 2008-247654.
[0027] The thickness of the separation membrane is, for example, 0.05 μm to 30 μm, preferably 0.1 μm to 20 μm, and more preferably 0.5 μm to 10 μm. Increasing the thickness of the separation membrane increases selectivity. Increasing the thickness of the separation membrane increases the permeation rate.
[0028] The surface roughness (Ra) of the separation membrane is, for example, 5 μm or less, preferably 2 μm or less, more preferably 1 μm or less, and even more preferably 0.5 μm or less. In this specification, surface roughness (Ra) is the arithmetic surface roughness Ra measured in accordance with JIS B 0601.
[0029] The separation membrane can be formed by any suitable method depending on the materials constituting the membrane. For example, a zeolite membrane can be obtained by coating a zeolite seed crystal onto a porous substrate, immersing the porous substrate with the attached seed crystal in a raw material solution, and growing the zeolite using the seed crystal as a nucleus by hydrothermal synthesis. The raw material solution includes, for example, a silica source, an alumina source, organic matter, an alkali source, and water. The heating temperature in hydrothermal synthesis is, for example, 60°C to 200°C. The heating time is, for example, 1 hour to 240 hours. Alternatively, a separation membrane may be formed using a raw material slurry obtained by mixing an organic binder, ceramic raw materials, and a solvent.
[0030] (Porous base material) The porous substrate is configured to allow gas to pass through. In the example shown in Figure 2, the porous substrate 12 is a so-called monolithic substrate, in which a plurality of through-holes extending in the longitudinal direction are provided on a single, integrally molded columnar body. In the example shown in Figure 2, the porous substrate 12 is approximately cylindrical. The cross-section perpendicular to the longitudinal direction of the through-holes is, for example, approximately circular. A separation membrane composite (porous substrate / separation membrane) with cells can be obtained by forming a separation membrane on the inner surface of the through-holes. Note that the shape of the porous substrate is not limited to the above example, and may be honeycomb, flat, tubular, cylindrical, columnar, or polygonal prismatic, for example. In one embodiment, a separation membrane may be formed on the outer surface of a tubular porous substrate.
[0031] The length of the porous substrate is, for example, 10 cm to 200 cm. The outer diameter of the porous substrate is, for example, 0.5 cm to 30 cm. If the porous substrate has through holes, the distance between the central axes of adjacent through holes is, for example, 0.3 mm to 10 mm. If the porous substrate is tubular or cylindrical, the thickness of the porous substrate is, for example, 0.1 mm to 10 mm.
[0032] Any suitable material can be used as the material for the porous substrate. In one embodiment, the porous substrate is formed from a ceramic sintered body. Examples of ceramic sintered bodies selected as the material for the porous substrate include alumina, silica, mullite, zirconia, titania, yttria, silicon nitride, and silicon carbide.
[0033] The porous substrate may contain an inorganic binder. At least one of the following can be used as the inorganic binder: titania, mullite, easily sinterable alumina, silica, glass frit, clay minerals, and easily sinterable cordierite.
[0034] The porous substrate may be a single-layer or multi-layer structure. In one embodiment, the porous substrate is a multi-layer structure consisting of layers with different pore sizes, as shown in Figure 3. It is preferable that the pore size is smaller closer to the inside (i.e., the separation membrane side).
[0035] The average pore size of the porous substrate is, for example, 0.01 μm to 70 μm, preferably 0.05 μm to 25 μm. The average pore size of the porous substrate on the separation membrane side is 0.01 μm to 1 μm, preferably 0.05 μm to 0.5 μm. Regarding the distribution of pore size throughout the porous substrate, including the surface and interior, D5 is, for example, 0.01 μm to 50 μm, D50 is, for example, 0.05 μm to 70 μm, and D95 is, for example, 0.1 μm to 2000 μm. The porosity of the porous substrate on the separation membrane side is, for example, 25% to 50%. The average pore size of the porous substrate can be measured by a mercury porosimeter, palm porometer, nanopalm porometer, etc.
[0036] (A measuring instrument for measuring the flow rate of nonpolar gases) Any suitable measuring instrument can be used to measure the flow rate of a nonpolar gas, depending on the type of nonpolar gas used. For example, the flow rate of the permeated nonpolar gas can be measured by using a mass flow meter to measure the flow rate of the permeate gas and a gas chromatograph to measure the concentration of the nonpolar gas in the permeate gas.
[0037] The above-described separation membrane system may further comprise any suitable elements. For example, it may include a supply unit for supplying fluid, a recovery unit for recovering fluid after it has passed through the separation membrane complex, a pressure adjustment unit for adjusting the pressure in the fluid flow path, and so on. The configuration of the separation membrane system is described, for example, in International Publication No. 2018 / 225325. The description in said publication is incorporated herein by reference.
[0038] B. Method for heating the separation membrane A method for heating a separation membrane according to one embodiment of the present invention includes a step I of supplying a heated mixed gas of a polar gas and a nonpolar gas to the separation membrane, and a step II of measuring the flow rate of the nonpolar gas that has permeated the separation membrane. As described above, by using a mixed gas of a polar gas and a nonpolar gas, the separation membrane can be heated efficiently, and abnormalities in the separation membrane can be detected early with high sensitivity.
[0039] The concentration of the nonpolar gas supplied to the separation membrane may be as described in Section A.
[0040] The above-mentioned separation membrane may have the configuration described in Section A. In one embodiment, as described above, the separation membrane may constitute a separation membrane complex.
[0041] The flow rate of the mixed gas supplied to the separation membrane can be any appropriate flow rate.
[0042] For example, by pre-measuring (or predicting) the permeation rate of nonpolar gas when the separation membrane is functioning normally, setting that rate as the normal rate, and then comparing the normal rate with the rate measured in step II, it is possible to detect abnormalities in the separation membrane. [Industrial applicability]
[0043] The separation membrane system of the present invention can be suitably used in the process of separating components in a mixed gas. [Explanation of Symbols]
[0044] 1. Separation membrane 2 Porous substrate 10 Separation Membrane Complex
Claims
1. A supply line that supplies a mixed gas of polar and nonpolar gases to a separation membrane, The system includes a measuring instrument for measuring the flow rate of nonpolar gas that has permeated the separation membrane, The mixed gas is a heated gas, The temperature of the mixed gas is 100°C or higher. The nonpolar gas is He or N2. Separation membrane system.
2. The separation membrane system according to claim 1, further comprising a heating device upstream of the separation membrane.
3. The separation membrane system according to claim 1 or 2, wherein the separation membrane is a zeolite membrane.
4. A mixed gas of a polar gas and a nonpolar gas, comprising the steps of supplying the heated mixed gas to a separation membrane, The process includes measuring the flow rate of the nonpolar gas that has permeated the separation membrane, The nonpolar gas is He or N2, In the process of supplying the heated mixed gas to the separation membrane, the temperature of the separation membrane is raised. Method for raising the temperature of a separation membrane.
5. The method for raising the temperature of a separation membrane according to claim 4, wherein the concentration of the nonpolar gas supplied to the separation membrane is less than 50% by volume.
6. The method for raising the temperature of a separation membrane according to claim 4, wherein the concentration of the nonpolar gas supplied to the separation membrane is less than 25% by volume.
Citation Information
Patent Citations
Production of argon having high purity
JP1989282108A
Hydrogen separation membrane and hydrogen purifying apparatus
JP2006000698A
Defect inspection method of porous structure, and manufacturing method of separation membrane structure
JP2017087192A
Defect detection method for monolithic separation membrane structures, repair method, and monolithic separation membrane structures
WO2014050702A1
Gas separation method and device
WO2022092031A1