Porous plug assembly, electrostatic chuck, and plasma etching apparatus

The porous plug assembly with a lateral and transverse portion enhances breakdown resistance in electrostatic chucks, addressing arc generation and adhesive layer corrosion issues in plasma etching apparatuses, ensuring reliable wafer processing.

JP7955036B2Active Publication Date: 2026-11-24ADVANCED MICRO FAB EQUIP INC CHINA
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2025536344
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-12-29
Filing Date
2023-11-29
Publication Date
2026-11-24
Estimated Expiration
2043-11-29

AI Technical Summary

Technical Problem

Existing electrostatic chucks in plasma etching apparatuses face challenges with breakdown resistance due to high-frequency power, leading to arc generation and damage from cooling gas breakdown, especially with increased precision and thermal expansion, affecting the adhesive layer's integrity and wafer processing.

Method used

A porous plug assembly with a porous plug body and an insulating dense layer, featuring a lateral portion and transverse portion, reduces discharge space and protects the adhesive layer from plasma corrosion, enhancing breakdown resistance.

Benefits of technology

The design effectively prevents arc generation and adhesive layer corrosion, improving breakdown voltage resistance and ensuring reliable wafer processing even under high-frequency conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007955036000001
    Figure 0007955036000001
  • Figure 0007955036000002
    Figure 0007955036000002
  • Figure 0007955036000003
    Figure 0007955036000003
Patent Text Reader

Abstract

The present invention discloses a porous plug assembly, an electrostatic chuck, and a plasma etching apparatus. The porous plug assembly includes a porous plug body having a porous structure, in which gas enters from the bottom surface of the porous plug body, passes through the porous plug body, and exits from the top surface of the porous plug body. The porous plug assembly also includes an insulating dense layer having side portions and lateral portions, the side portions being formed on side walls of the porous plug body, and the lateral portions extending from tips of the lateral portions in at least one direction between a direction away from the porous plug body and a direction toward the porous plug body. The lateral portions reduce the risk of the adhesive layer being corroded by plasma. The porous plug assembly also reduces the discharge space and the risk of arcing. Furthermore, the porous plug assembly can effectively solve the problem of the adhesive layer clogging the porous plug body.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The present invention relates to the technical field of plasma equipment, and in particular, to a porous plug assembly, an electrostatic chuck, and a plasma etching apparatus. BACKGROUND ART

[0002] An electrostatic chuck is a core component of a plasma etching apparatus. A dielectric plate serving as a wafer support platform is bonded to a base of the electrostatic chuck, and gas holes are formed in the electrostatic chuck. A cooling gas flows through the gas holes to the back surface of a wafer, absorbs heat of the wafer, and lowers a temperature of the wafer. With development of storage technologies, high-frequency power used in the plasma etching apparatus becomes higher and higher, and a voltage applied to the electrostatic chuck also becomes higher and higher. When the wafer is processed by using plasma, the cooling gas in the gas holes is easily broken down to generate arcing, causing damage to the wafer and the electrostatic chuck.

[0003] In the prior art, a porous plug is disposed in a gas hole to improve a breakdown voltage at the gas hole. However, currently, requirements for processes are increasingly strict. Factors such as uncertainty in a production and processing process and various impacts (for example, adverse impact caused by thermal expansion and contraction of the electrostatic chuck) generated during use of the electrostatic chuck impose higher requirements on breakdown resistance of the porous plug. SUMMARY PROBLEMS TO BE SOLVED BY THE INVENTION

[0004] An objective of the present invention is to provide a porous plug assembly with breakdown resistance, an electrostatic chuck, and a plasma etching apparatus. MEANS FOR SOLVING PROBLEMS

[0005] To achieve the above objectives, the present invention provides a porous plug assembly comprising: a porous plug body having a porous structure, the porous plug body comprising a top surface, a bottom surface, and a side wall, wherein gas can enter from the bottom surface and exit from the top surface via the porous plug body; and an insulating dense layer comprising a lateral portion and a transverse portion, wherein the lateral portion is provided on the side wall of the porous plug body, the lateral portion has a tip and a bottom end, the bottom end is flush with the bottom surface, and the tip is not lower than the top surface, the transverse portion extending from the tip of the lateral portion in at least one direction away from the porous plug body and a direction approaching the porous plug body, and the upper surface of the transverse portion is flush with the tip.

[0006] Selectively, the lateral portion extends at least in a direction approaching the porous plug body, and the lower surface of the lateral portion is not higher than the top surface.

[0007] Selectively, the lower surface of the lateral portion becomes flush with the top surface and covers a portion of the top surface.

[0008] Selectively, the lower surface of the lateral portion is lower than the top surface, and the area of ​​the top surface is smaller than the area of ​​the bottom surface.

[0009] Selectively, the lateral portion further extends in a direction away from the porous plug body.

[0010] An elastic member is selectively provided at the bottom end of the lateral portion.

[0011] Selectively, the porosity of the porous plug body is 30% to 60%.

[0012] Selectively, the porous plug body is made of porous ceramic, and the dense layer is made of ceramic.

[0013] The present invention further provides an electrostatic chuck comprising a base having a first through-hole, wherein the porous plug assembly described above is provided in the first through-hole; and a dielectric plate having electrodes for generating electrostatic attraction, wherein the upper surface of the dielectric plate is used to fix a wafer, the lower surface of the dielectric plate is connected to the base via an adhesive layer, and the lateral portion includes a dielectric plate located between the lower surface of the dielectric plate and the base, wherein the dielectric plate is provided with a second through-hole penetrating the dielectric plate axially, and the second through-hole communicates with the first through-hole.

[0014] Selectively, the lateral portion extends at least in a direction away from the porous plug body, and an adhesive layer is provided between the lower surface of the lateral portion and the base.

[0015] Selectively, the upper surface of the base is stepped and has a relatively low first upper surface and a relatively high second upper surface, and an adhesive layer is provided between the lower surface of the lateral portion and the first upper surface.

[0016] Selectively, an insulating layer is provided between the adhesive layer and the base.

[0017] Selectively, the insulating layer is alumina.

[0018] Selectively, an adhesive layer is provided between the lateral portion and the base.

[0019] The present invention further provides a plasma etching apparatus comprising a reaction chamber, the electrostatic chuck described above, an upper electrode, a cooling device, and a high-frequency power supply, wherein the electrostatic chuck is placed in the reaction chamber and used to support a wafer and serves as the lower electrode of the reaction chamber, the cooling device is in communication with the electrostatic chuck and used to transport a cooling gas to the wafer, the upper electrode is provided opposite the electrostatic chuck, and the high-frequency power supply is applied to the upper electrode or the electrostatic chuck, generating a high-frequency electric field between the upper electrode and the electrostatic chuck to dissociate the reaction gas into plasma and etch the wafer. [Effects of the Invention]

[0020] Compared to the prior art, the present invention includes at least the following beneficial effects.

[0021] (1) The porous plug assembly of the present invention comprises a porous plug body having a porous structure and an insulating dense layer, the dense layer comprising a lateral portion and a transverse portion, the transverse portion being able to effectively protect the adhesive layer, reducing the risk of the adhesive layer being corroded by plasma and improving the corrosion resistance of the electrostatic chuck.

[0022] (2) The lateral portion of the dense layer of the present invention prevents the adhesive layer from entering from the top surface of the porous plug body and blocking the holes in the porous plug body.

[0023] (3) In the present invention, an adhesive layer is provided between the lateral portion of the dense layer and the base, and an elastic member is provided at the bottom end of the lateral portion of the dense layer, providing compensation for the slit between the dielectric plate and the lateral portion of the dense layer, thereby preventing the generation of an arc due to the slit being too large.

[0024] (4) The dense layer of the present invention can also reduce the discharge space, thereby lowering the risk of arc generation. The outwardly extending lateral portion overlaps with the bonding layer and the alumina insulating layer in some areas, which can greatly improve the breakdown voltage resistance. Even if there are defects in the bonding layer or the alumina insulating layer, excellent breakdown resistance can still be achieved. [Brief Description of the Drawings]

[0025] [Figure 1] A structural schematic diagram of a plasma etching chamber. [Figure 2] A structural schematic diagram of a conventional electrostatic chuck. [Figure 3] A structural schematic diagram of a porous plug assembly according to the present invention. [Figure 4] A structural schematic diagram of a porous plug assembly according to the present invention. [Figure 5] A structural schematic diagram of a porous plug assembly according to the present invention. [Figure 6] A structural schematic diagram of a porous plug assembly according to the present invention. [Figure 7] A structural schematic diagram of a porous plug assembly according to the present invention. [Figure 8] A structural schematic diagram of a porous plug assembly according to the present invention. [Figure 9] A structural schematic diagram of an electrostatic chuck according to the present invention. [Figure 10] A structural schematic diagram of an electrostatic chuck according to the present invention. [Figure 11] A structural schematic diagram of an electrostatic chuck according to the present invention. [Figure 12] A structural schematic diagram of an electrostatic chuck according to the present invention. [Figure 13] A structural schematic diagram of an electrostatic chuck according to the present invention. [Figure 14] A structural schematic diagram of an electrostatic chuck according to the present invention. [Figure 15] A structural schematic diagram of an electrostatic chuck according to the present invention. [Modes for carrying out the invention]

[0026] The technical aspects of the present invention are described below clearly and completely with reference to the drawings, and it is clear that the embodiments described are only some, not all, embodiments of the present invention. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without any creative effort are all within the scope of the protection of the present invention.

[0027] Furthermore, in the description of this invention, directions or positional relationships indicated by terms such as "up," "down," "left," "right," "vertical," "horizontal," "inside," and "outside" are based on the directions or positional relationships shown in the drawings and are merely for the purpose of easily describing or simplifying the description of this invention. They do not indicate or imply that the referred device or element necessarily has a specific direction or must be constructed or operated in a specific direction, and therefore should not be understood as limitations on this invention. Furthermore, the terms "first," "second," and "third" are used solely for descriptive purposes and should not be understood as indicating or implying relative importance.

[0028] In the description of this invention, unless otherwise explicitly specified and limited, the terms “attach,” “connect,” and “connect” should be understood in a broad sense. For example, a connection may be fixed, detachable, integral, mechanical, directly, indirectly via an intermediate medium, or internally connected to two elements. Those skilled in the art will be able to understand the specific meaning of these terms in this invention depending on the specific situation.

[0029] The plasma processing procedure in the plasma etching chamber is shown in Figure 1. The electrostatic chuck 100 serves as both a support platform for the wafer 200 and the lower electrode of the reaction chamber. The upper electrode 400 of the reaction chamber is provided opposite the electrostatic chuck 100. A high-frequency power supply is applied to the upper electrode 400 or the electrostatic chuck 100, generating a high-frequency electric field between the upper electrode 400 and the electrostatic chuck 100, thereby dissociating the reaction gas into plasma 300 and processing the wafer 200 fixed to the electrostatic chuck 100. The electrostatic chuck 100 can further adjust and control the temperature of the wafer 200 placed on it. The electrostatic chuck 100 is provided with gas holes and is connected to a cooling device 500. The cooling gas in the cooling device 500 flows through the gas holes to the back of the wafer 200, absorbing heat from the wafer 200 and thus lowering its temperature.

[0030] As shown in Figure 2, the electrostatic chuck 100 includes a base 110 and a dielectric plate 130 provided on the base 110. The dielectric plate 130 is connected to the base 110 via an adhesive layer 120. The dielectric plate 130 is provided with electrodes for generating electrostatic attraction. To regulate the temperature of the wafer 200, the base 110 is provided with a first through-hole 111, and the dielectric plate 130 is provided with a second through-hole 131 that penetrates the dielectric plate 130 axially. The second through-hole 131 communicates with the first through-hole 111. The first through-hole 111 is connected to a cooling device (not shown) via a passage 112, and cooling gas flows out from the cooling device, passes through the passage 112, the first through-hole 111, and the second through-hole 131 in sequence, and contacts the back surface of the wafer 200 fixed to the dielectric plate 130, thereby regulating and controlling the temperature of the wafer 200.

[0031] A high-power, high-frequency electric field easily causes an arc reaction in the cooling gas within the first through-hole 111, leading to arc damage to the electrostatic chuck 100. The conditions for the cooling gas to break down include (1) the voltage difference being greater than the voltage threshold at which the cooling gas breaks down, and (2) the discharge space being sufficiently large, i.e., the discharge space being much larger than the mean free path of the cooling gas, thus satisfying the continuity of the arc action.

[0032] In conventional technology, a porous plug assembly 700, which includes a porous plug body 710 and a dense layer 720, is typically provided in the first through-hole 111. The porous plug body 710 has a porous structure, and the cooling gas enters from the bottom surface 711 of the porous plug body 710, flows out from the top surface 712 through the porous plug body 710, enters the second through-hole 131, and can come into contact with the wafer 200. After filling the porous plug assembly 700, the discharge space for the cooling gas in the first through-hole 111 is reduced, which can decrease the possibility of the cooling gas breaking down. The insulating dense layer 720 is provided on the sidewall of the porous plug body 710, which can improve the breakdown resistance of the porous plug body 710.

[0033] However, as the precision of the wafer processing process increases, the high-frequency power applied to the electrostatic chuck 100 also increases, and the breakdown resistance of the porous plug assembly 700 needs to be further improved to withstand the effects of such high-power high-frequency electric fields. When the above porous plug assembly 700 is used, the slit between the dielectric plate 130 and the porous plug assembly 700 is too large (usually the thickness of the adhesive layer 120), and it is advantageous for arc discharge to occur at this slit, especially at the edge face 121 of the adhesive layer 120. In addition, the adhesive layer 120 generally uses an organic adhesive, and compared to the dense layer 720, the adhesive layer 120 is more susceptible to corrosion by plasma. A corroded adhesive layer 120 cannot effectively cover the base 110, increasing the risk of arc generation.

[0034] Based on this, the present invention provides a porous plug assembly that can reduce the risk of electrostatic chuck breakdown. As shown in Figures 3 to 8, the porous plug assembly 600 of the present invention includes a porous plug body 610 having a porous structure and an insulating dense layer 620. The porous plug body 610 may be cylindrical or any other shape, and the dense layer 620 surrounds the side walls of the porous plug body 610. The porous plug body 610 may be a porous ceramic, such as alumina or aluminum nitride, and the through holes in the porous ceramic may be straight passages or curved passages.

[0035] The cooling gas enters from the bottom surface 611 of the porous plug body 610, passes through the porous plug body 610, and exits from the top surface 612 of the porous plug body 610. Selectively, the porosity of the porous plug body 610 is 30% to 60%. If the porosity is too low, the flow rate of the cooling gas passing through the porous plug body 610 is too low, and if the porosity is too high, the pressure resistance of the porous plug body 610 is too low. Preferably, the porosity of the porous plug body 610 is 50%.

[0036] The dense layer 620 includes a lateral portion 621 and a transverse portion 622. The lateral portion 621 is formed on the side wall of the porous plug body 610, and the transverse portion 622 is formed at the tip 6211 of the lateral portion 621. The transverse portion 622 extends in at least one direction away from the porous plug body 610 (i.e., outward) and towards the porous plug body 610 (i.e., inward). The upper surface of the transverse portion 622 is substantially flush with the tip 6211 of the lateral portion 621. The dense layer 620 is at least one of ceramic, epoxy resin, and silicone resin.

[0037] In the embodiment shown in Figure 3, the lateral portion 622 extends outward, and the top surface 612 of the porous plug body is not covered by the dense layer 620. In this embodiment, the top surface of the lateral portion 622 and the tip 6211 of the lateral portion 621 are substantially flush with the top surface 612 of the porous plug body 610, and the bottom end 6212 of the lateral portion 621 is substantially flush with the bottom surface 611 of the porous plug body 610.

[0038] In the embodiment shown in Figure 4, the bottom end 6212 of the lateral portion 621 is substantially flush with the bottom surface 611 of the porous plug body 610, and the tip 6211 of the lateral portion 621 is higher than the top surface 612 of the porous plug body 610. That is, the distance from the bottom end 6212 to the tip 6211 of the lateral portion 621 is greater than the axial length of the porous plug body 610.

[0039] In the embodiment shown in Figure 5, the lateral portion 622 extends inward, and the lower surface of the lateral portion 622 is substantially flush with the top surface 612. That is, the lateral portion 622 covers a portion of the top surface 612, and the gas flows out from the area of ​​the top surface 612 that is not covered by the dense layer 620.

[0040] In the embodiment shown in Figure 6, the lateral portion 622 extends inward, the upper surface of the lateral portion 622 is not lower than the top surface 612, the lower surface of the lateral portion 622 is lower than the top surface 612, the area of ​​the top surface 612 is smaller than the bottom surface 611, and the porous plug body 610 is roughly convex in shape. In this case, the distance from the bottom end 6212 to the tip 6211 of the lateral portion 621 is not smaller than the distance from the bottom surface 611 to the top surface 612 of the porous plug body 610.

[0041] In contrast to Figures 5 and 6, in the embodiments shown in Figures 7 and 8, the lateral portion 622 extends simultaneously inward and outward, and the cross-section of the dense layer 620 has a substantially T-shaped structure.

[0042] The present invention further provides an electrostatic chuck including the porous plug assembly 600 described above. As shown in Figure 9, the base 110 of the electrostatic chuck is provided with a first through hole 111, and the porous plug assembly 600 is provided in the first through hole 111. A dielectric plate 130 is placed on the base 110, and the upper surface of the dielectric plate 130 is used to fix the lateral portion of the wafer. The dielectric plate 130 is provided with a second through hole 131 that penetrates the dielectric plate 130 axially, and the second through hole 131 communicates with the first through hole 111. An adhesive layer 120 is provided between the lower surface of the dielectric plate 130 and the base 110 for bonding the dielectric plate 130 and the base 110.

[0043] In this embodiment, as the lateral portion 622 extends outward, the adhesive layer 120 is surrounded by the base 110, the dense layer 620, and the dielectric plate 130, and the end face 121 of the adhesive layer 120 is shielded by the dense layer 620 and not directly exposed to the plasma environment. The dense layer 620 has good corrosion resistance and can protect the end face 121 of the adhesive layer 120. Compared to the prior art, the discharge space between the dielectric plate 130 and the porous plug assembly 600 is relatively small, which is disadvantageous for arc discharge generation. The dense layer 620 also has a very high breakdown voltage resistance, which can improve the breakdown resistance of the peripheral region of the porous plug body 610.

[0044] In the embodiment shown in Figure 10, the upper surface of the lateral portion 622 is higher than the top surface 612 of the porous plug body 610. In this embodiment, a gap 6120 exists between the lower surface and the top surface 612 of the dielectric plate 130. The dielectric plate 130 does not contact the top surface 612, and the obstruction of gas outflow by the dielectric plate 130 can be reduced. The dense layer 620 has a very high breakdown voltage resistance, which can improve the breakdown resistance of the peripheral region of the porous plug body 610.

[0045] In the embodiment shown in Figure 11, the lateral portion 622 extends inward. The dielectric plate 130 is positioned in the lateral portion 622 of the dense layer 620, the upper surface of the base 110 is not higher than the upper surface of the lateral portion 622, and an adhesive layer 120 is filled between the base 110 and the dielectric plate 130. The adhesive layer 120 is surrounded by the base 110, the dense layer 620, and the dielectric plate 130, and the end face 121 of the adhesive layer 120 is shielded by the dense layer 620 and not directly exposed to the plasma environment. The extended lateral portion 622 covers a portion of the top surface 612, and the plasma cannot penetrate the lateral portion 622 of the dense layer 620 along the top surface 612 of the porous plug body 610 and corrode the adhesive layer 120.

[0046] The adhesive layer 120 is usually formed from a fluid gel-like substance. When the adhesive layer 120 is processed, the gel-like substance tends to flow onto the porous plug body 610, causing blockage and affecting the permeability of the porous plug body 610. In this embodiment, the lateral portion 622 of the dense layer 620 covers a portion of the top surface 612. The extended lateral portion 622 increases the distance between the area on the top surface 612 of the porous plug body 610 from which gas flows out (i.e., the area not covered by the lateral portion 622) and the adhesive layer 120, making it less likely for the adhesive layer 120 to flow onto the top surface 612 of the porous plug body 610 and cause blockage. The outwardly extending lateral portion 622 can also serve to prevent blockage by the adhesive gel-like substance. Compared to the conventional technology, the discharge space between the dielectric plate 130 and the porous plug assembly 600 is relatively small, which is disadvantageous for arc discharge generation. The dense layer 620 also has a very high breakdown voltage resistance, which can improve the breakdown resistance of the area surrounding the porous plug body 610.

[0047] When manufacturing an electrostatic chuck, typically, a first through-hole is first formed in the base, and the porous plug assembly is filled into the first through-hole. Then, the dielectric plate is bonded to the base via an adhesive layer. The dielectric plate is pressed along the axial direction to reduce the slit between the dielectric plate and the lateral portion of the dense layer, thereby firmly bonding the dielectric plate to the base. The lower surface of the dielectric plate is adjacent to the upper surface of the lateral portion, and if a slit exists between the two surfaces, this slit is advantageous for arc generation. However, tolerances may exist in each component during the production process, errors may occur during the manufacturing process, and the dielectric plate material is relatively brittle. If both the porous plug assembly and the base are in hard contact, pressing the dielectric plate along the axial direction may cause the dielectric plate to rupture, and the slit between the lower surface of the dielectric plate and the upper surface of the lateral portion may be relatively large.

[0048] As shown in Figure 12, in the present invention, an adhesive layer 120 is further provided between the lower surface of the lateral portion 622 and the base 110. Specifically, the upper surface of the base 110 is stepped, having a relatively low first upper surface and a relatively high second upper surface, and the adhesive layer 120 is provided between the lower surface of the lateral portion 622 and the first upper surface. The adhesive layer 120 is a soft gel-like material, and when the dielectric plate 130 is pressed, the adhesive layer 120 between the lower surface of the lateral portion 622 and the base 110 can compensate for the slit 6121 between the upper surface of the lateral portion 622 and the dielectric plate 130. After bonding, the width of the slit 6121 is 0.1 mm or less, and consequently the slit 6121 disappears, achieving complete bonding between the lateral portion 622 and the dielectric plate 130.

[0049] In other embodiments, particularly in embodiments where the lateral portion 622 extends inward, the lateral portion 622 does not overlap the base 110, and the slit 6121 cannot be compensated by installing the adhesive layer 120 on the lateral portion 622. In order to sufficiently bond the lateral portion 622 and the dielectric plate 130, in the embodiment shown in Figure 13, an elastic member 630 is installed at the bottom end of the lateral portion 621 of the dense layer 620. When the dielectric plate 130 is pressed, the entire porous plug assembly 600 moves downward along the axial direction together with the dielectric plate 130, and the elastic member 630 is compressed between the porous plug assembly 600 and the base 110, thereby compensating for the slit between the lateral portion 622 and the dielectric plate 130.

[0050] In other embodiments, an insulating layer is provided between the adhesive layer 120 and the base 110. The insulating layer is alumina. The insulating layer further protects the base and can block direct arc damage between the base 110 and the wafer 200.

[0051] In other embodiments, an adhesive layer is provided between the lateral portion 621 and the base 110. The adhesive layer 120 between the lower surface of the dielectric plate 130 and the base 110, the adhesive layer 120 between the lower surface of the lateral portion 622 and the base 110, and the adhesive layer between the lateral portion 621 and the base 110 are in communication with each other.

[0052] The present invention further provides a plasma etching apparatus comprising a reaction chamber, the electrostatic chuck described above, an upper electrode, a cooling device, and a high-frequency power supply, wherein the electrostatic chuck is placed in the reaction chamber and used to support a wafer and serves as the lower electrode of the reaction chamber, the cooling device is in communication with the electrostatic chuck and used to transport a cooling gas to the wafer, the upper electrode is installed opposite the electrostatic chuck, and the high-frequency power supply is applied to the upper electrode or the electrostatic chuck, generating a high-frequency electric field between the upper electrode and the electrostatic chuck to dissociate the reaction gas into plasma and etch the wafer.

[0053] The technical means according to the present invention will be introduced below through two preferred embodiments.

[0054] (Example 1) As shown in Figure 14, this embodiment provides an electrostatic chuck comprising a base 110 and a dielectric plate 130 placed on the base 100, the dielectric plate 130 being connected to the base 110 via an adhesive layer 120. To regulate the temperature of a wafer (not shown), the base is provided with a first through-hole 111, and the dielectric plate 130 is provided with a second through-hole 131 that penetrates the dielectric plate 130 axially, the second through-hole 131 communicating with the first through-hole 111. Cooling gas can be brought into contact with the back surface of the wafer fixed to the dielectric plate 130 by passing through the first through-hole 111 and the second through-hole 131 in sequence, thereby regulating and controlling the wafer temperature. In this embodiment, the cooling gas is helium gas.

[0055] A porous plug assembly 600 is provided in the first through hole 111. The porous plug assembly 600 includes a porous plug body 610 having a porous structure and an insulating dense layer 620. The porousness of the porous plug body 610 is 50%, and gas enters from the bottom surface 611 of the porous plug body 610, passes through the porous plug body 610, and flows out from the top surface 612 of the porous plug body 610. The dense layer 620 is a ceramic material with a porosity smaller than that of the porous plug body 610, and includes a lateral portion 621 and a transverse portion 622, the transverse portion 622 extending simultaneously inward and outward, the upper surface of the transverse portion 622 being substantially flush with the tip 6211 of the lateral portion 621, and the lower surface of the transverse portion 622 being substantially flush with the top surface 612.

[0056] The lateral section 622 includes a first unit 6221 extending outward and a second unit 6222 extending inward. The second unit 6222 covers a portion of the top surface 612, and the gas flows out from the area of ​​the top surface 612 not covered by the second unit 6222.

[0057] The adhesive layer 120 is stepped, consisting of a first adhesive layer 1201 and a second adhesive layer 1202 that communicate with each other. The first adhesive layer 1201 is provided between the lower surface of the dielectric plate 130 and the base 110, and adheres the dielectric plate 130 to the base 110. The extended first unit 6221 occupies the filling space of the first adhesive layer 1201, and the first adhesive layer 1201 is separated from the area where the porous plug assembly 600 and the plasma come into contact, so that the plasma is less likely to corrode the adhesive layer 120. The second adhesive layer 1202 is provided between the lower surface of the first unit 6221 and the base 110. The dielectric plate 130 is pressed axially to connect it to the base 110, and the first unit 6221 is pressed downward together with the dielectric plate 130, pushing out the second adhesive layer 1202, and the soft second adhesive layer 1202 provides compensation for the slit between the lateral portion 622 and the dielectric plate 130, reducing the slit to within 0.1 mm.

[0058] The adhesive layer 120 may further include a third adhesive layer 1203 provided between the lateral portion 621 and the base 110. The third adhesive layer 1203 communicates with the second adhesive layer 1202, and the adhesive layer 120 is formed as a connected overall structure. In other embodiments, the third adhesive layer 1203 may not be provided. An insulating layer 140 is further provided between the adhesive layer 120 and the base 110, and the insulating layer 140 is made of alumina.

[0059] The outward-extending first unit 6221, the adhesive layer 120, and the alumina insulating layer have overlapping portions, which significantly improves the breakdown voltage resistance and allows for excellent breakdown resistance even if defects are present in the adhesive layer 120 or the alumina insulating layer. Compared to the conventional technology, the discharge space between the dielectric plate 130 and the porous plug assembly 600 is relatively small, which is disadvantageous for arc discharge generation. The lateral portion 622 effectively protects the adhesive layer 120 and reduces the risk of the adhesive layer 120 being corroded by the plasma. Furthermore, the lateral portion allows the adhesive layer 120 to penetrate from the top surface of the porous plug body 610, preventing blockage of the holes in the porous plug body 610.

[0060] (Example 2) As shown in Figure 15, the electrostatic chuck according to this embodiment is substantially the same as that of Embodiment 1. In this embodiment, the lateral portion 622 extends simultaneously inward and outward, the upper surface of the lateral portion 622 is substantially flush with the tip 6211 of the lateral portion 621, the lower surface 612 of the lateral portion 622 is lower than the top surface, the area of ​​the top surface 612 is smaller than that of the bottom surface 611, and the porous plug body 610 is substantially convex.

[0061] The dielectric plate 130 can extend above the top surface 612, and a gap 6120 exists between the lower surface of the dielectric plate 130 and the top surface 612. The dielectric plate 130 does not come into contact with the top surface 612, thereby reducing obstruction to gas outflow.

[0062] In this embodiment, an elastic member 630 is installed at the bottom end of the lateral portion 621, and together with the second adhesive layer 1202, the elastic member 630 can provide compensation for the slit between the dielectric plate 130 and the lateral portion 622.

[0063] Based on the above, the present invention provides a porous plug assembly, an electrostatic chuck, and a plasma etching apparatus. The porous plug assembly comprises a porous plug body having a porous structure and an insulating dense layer. The lateral portion of the dense layer is formed on the side wall of the porous plug body, and the lateral portion is formed at the tip of the lateral portion, extending substantially horizontally. The extended lateral portion extends the distance between the adhesive layer of the electrostatic chuck and the plasma, reducing the risk of the adhesive layer being corroded by the plasma and improving the corrosion resistance of the electrostatic chuck. The porous plug assembly can further reduce the discharge space and reduce the risk of arc generation. The porous plug assembly can effectively solve the problem of the adhesive layer blocking the porous plug body.

[0064] Although the present invention has been described in detail through the preferred embodiments described above, this description should not be considered a limitation of the invention. Various modifications and substitutions to the invention will be obvious to those skilled in the art after reading the above. Therefore, the scope of protection of the present invention is limited to the claims. [Explanation of Symbols]

[0065] 100 electrostatic chucks 110 base 111 First through hole 112 Passage 120 Adhesive layer 1201 First adhesive layer 1202 Second adhesive layer 1203 Third adhesive layer 121 End face 130 Dielectric Plate 131 Second through hole 140 Insulating layer 200 wafers 300 Plasma 400 Upper electrode 500 Cooling device 600, 700 Porous Plug Assembly 610, 710 Porous Plug Body 611, 711 base 612, 712 top surface 6120 Gap 6121 Slit 620, 720 compact layer 621 Lateral part 6211 Tip 6212-bottom end 622 Lateral section 630 Elastic member

Claims

1. A porous plug assembly, A porous plug body having a porous structure, comprising a top surface, a bottom surface, and side walls, wherein gas can enter from the bottom surface and exit from the top surface via the porous plug body, An insulating dense layer comprising a lateral portion and a transverse portion, wherein the lateral portion is provided on the side wall of the porous plug body and has a tip and a bottom, the bottom being flush with the bottom surface and the tip not being lower than the top surface, The lateral portion extends from the tip of the lateral portion in at least one direction from a direction away from the porous plug body and a direction approaching the porous plug body, The upper surface of the aforementioned lateral portion is flush with the tip, A porous plug assembly characterized in that an elastic member is provided at the bottom end of the lateral portion.

2. The aforementioned lateral portion extends at least in a direction approaching the porous plug body, The porous plug assembly according to claim 1, characterized in that the lower surface of the lateral portion is not higher than the top surface.

3. The porous plug assembly according to claim 2, characterized in that the lower surface of the lateral portion is flush with the top surface and covers a portion of the top surface.

4. The lower surface of the lateral portion is lower than the top surface. The porous plug assembly according to claim 2, characterized in that the area of ​​the top surface is smaller than the area of ​​the bottom surface.

5. The porous plug assembly according to claim 2, characterized in that the lateral portion further extends in a direction away from the porous plug body.

6. The porous plug assembly according to claim 1, characterized in that the porosity of the porous plug body is 30% to 60%.

7. The porous plug body is made of porous ceramic, The porous plug assembly according to claim 1, characterized in that the dense layer is made of ceramic.

8. It is an electrostatic chuck, A base having a first through-hole, wherein a porous plug assembly is provided in the first through-hole, the porous plug assembly comprising a porous plug body having a porous structure, including a top surface, a bottom surface, and a side wall, through which gas can enter from the bottom surface and exit from the top surface via the porous plug body, and an insulating dense layer comprising a lateral portion and a transverse portion, wherein the lateral portion is provided on the side wall of the porous plug body, has a tip and a bottom end, the bottom end is flush with the bottom surface, and the tip is not lower than the top surface, the transverse portion extends from the tip of the lateral portion in at least one direction from a direction away from the porous plug body and a direction approaching the porous plug body, the upper surface of the transverse portion is flush with the tip, A dielectric plate provided with electrodes for generating electrostatic attraction, wherein the upper surface of the dielectric plate is used to fix a wafer, the lower surface of the dielectric plate is connected to the base via an adhesive layer, and the lateral portion of the dielectric plate is located between the lower surface of the dielectric plate and the base, The dielectric plate is provided with a second through-hole that penetrates the dielectric plate in the axial direction. The second through hole communicates with the first through hole. An electrostatic chuck characterized by the following features.

9. The aforementioned lateral portion extends at least in a direction away from the porous plug body, The electrostatic chuck according to claim 8, characterized in that an adhesive layer is provided between the lower surface of the lateral portion and the base.

10. The upper surface of the base is stepped and has a relatively low first upper surface and a relatively high second upper surface. The electrostatic chuck according to claim 9, characterized in that an adhesive layer is provided between the lower surface of the lateral portion and the first upper surface.

11. The electrostatic chuck according to claim 8, characterized in that an insulating layer is provided between the adhesive layer and the base.

12. The electrostatic chuck according to claim 11, characterized in that the insulating layer is alumina.

13. The electrostatic chuck according to claim 8, characterized in that an adhesive layer is provided between the lateral portion and the base.

14. The lateral portion extends at least in a direction approaching the porous plug body, The electrostatic chuck according to claim 8, characterized in that the lower surface of the lateral portion is not higher than the top surface.

15. The electrostatic chuck according to claim 14, characterized in that the lower surface of the lateral portion is flush with the top surface and covers a portion of the top surface.

16. The lower surface of the lateral portion is lower than the top surface, The electrostatic chuck according to claim 14, characterized in that the area of ​​the top surface is smaller than the area of ​​the bottom surface.

17. The electrostatic chuck according to claim 14, characterized in that the lateral portion further extends in a direction away from the porous plug body.

18. The electrostatic chuck according to claim 8, characterized in that an elastic member is provided at the bottom end of the lateral portion.

19. The electrostatic chuck according to claim 8, characterized in that the porosity of the porous plug body is 30% to 60%.

20. The porous plug body is made of porous ceramic, The electrostatic chuck according to claim 8, characterized in that the dense layer is made of ceramic.

21. A plasma etching apparatus, The system includes a reaction chamber, an electrostatic chuck according to any one of claims 8 to 20, an upper electrode, a cooling device, and a high-frequency power supply. The electrostatic chuck is placed in the reaction chamber and used to support the wafer, and is also used as the lower electrode of the reaction chamber. The cooling device communicates with the electrostatic chuck and is used to transport cooling gas to the wafer. The upper electrode is provided facing the electrostatic chuck, A plasma etching apparatus characterized in that the high-frequency power supply is applied to the upper electrode or the electrostatic chuck, and a high-frequency electric field is generated between the upper electrode and the electrostatic chuck, thereby dissociating the reaction gas into plasma and etching the wafer.

Citation Information

Patent Citations

  • Electrostatic chuck and method of manufacturing the same

    JP2016143744A

  • Electrostatic chuck

    JP2020145280A

  • Electrostatic chuck, method of manufacturing electrostatic chuck, and plasma processing apparatus

    US20210118716A1

  • Sample holder

    WO2019082875A1

  • Sample holder

    WO2020111194A1