Substrate processing apparatus, substrate processing method, and article manufacturing method

The substrate processing apparatus addresses uneven film surfaces by employing a two-step drying process with controlled gas supply and pressure conditions, achieving a flat and efficient drying of films on substrates.

JP7955140B2Active Publication Date: 2026-11-24CANON KK
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2022180660
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-07-12
Filing Date
2022-11-11
Publication Date
2026-11-24
Estimated Expiration
2042-11-11

AI Technical Summary

Technical Problem

Existing substrate processing methods using gas supply for rapid drying can result in an uneven or non-flat film surface on the substrate.

Method used

A substrate processing apparatus that employs a two-step drying process with different pressure conditions and gas supply methods, utilizing a first drying step at a pressure higher than the vapor pressure of the solvent and a second drying step at a lower pressure, along with controlled gas introduction into separate spaces within the chamber to achieve uniform film thickness and rapid drying.

Benefits of technology

The apparatus ensures a flat and stable film surface by controlling pressure and gas distribution, enhancing drying efficiency and uniformity while shortening the drying time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007955140000001
    Figure 0007955140000001
  • Figure 0007955140000002
    Figure 0007955140000002
  • Figure 0007955140000003
    Figure 0007955140000003
Patent Text Reader

Abstract

To dry a film on a substrate.SOLUTION: A substrate processing apparatus for drying a film on a substrate by a drying step including a first drying step for drying the film on the substrate under a pressure higher than a predetermined pressure and a second drying step for drying the film under a pressure lower than the predetermined pressure includes: a substrate holding part that holds the substrate; a chamber; a depressurization mechanism that depressurizes an interior of the chamber; a cover that has an opening and covers the substrate held by the substrate holding part inside the chamber; a first supply part that supplies gas to a first space inside the chamber and outside the cover; and a second supply part that supplies gas to a second space inside the chamber and outside the cover, wherein: the first supply part supplies the gas to the first space in the first drying step; and the second supply part supplies the gas to the second space in the second drying step.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a substrate processing apparatus, a substrate processing method, and a method for manufacturing an article.

Background Art

[0002] In manufacturing an article such as an organic EL (OLED) panel, a method of applying a solution film onto a substrate using an inkjet apparatus is known. The solution film applied onto the substrate is preferably dried in a short time using a substrate processing apparatus (reduced pressure drying apparatus) in order to stably form a film. Patent Document 1 discloses a content related to a substrate processing apparatus that performs reduced pressure and drying while supplying nitrogen into a chamber for the purpose of shortening the drying time.

Prior Art Documents

Patent Documents

[0003]

Patent Document 1

Summary of Invention

Problems to be Solved by the Invention

[0004] However, when a gas is supplied into the chamber for the purpose of shortening the drying time, the film surface on the substrate may not be flat. In order to stably and flatly dry the film surface on the substrate, it is necessary to devise a gas supply method in each of the drying steps performed under a plurality of pressure conditions.

[0005] Accordingly, an object of the present invention is to provide a substrate processing apparatus that is advantageous in drying a film on a substrate.

Means for Solving the Problems

[0006] To achieve the above objective, a substrate processing apparatus as one aspect of the present invention is a substrate processing apparatus that dries a film on a substrate by a drying process comprising: a first drying step of drying the film on the substrate under a pressure higher than a predetermined pressure; and a second drying step of drying the film under a pressure lower than the predetermined pressure, the apparatus comprising: a substrate holding part for holding the substrate; a chamber; a depressurization mechanism for depressurizing the inside of the chamber; a cover having an opening and covering the substrate held by the substrate holding part inside the chamber; a first supply part for supplying gas to a first space which is inside the chamber and outside the cover; and a second supply part for supplying gas to a second space which is inside the chamber and inside the cover, wherein the first supply part supplies gas to the first space in the first drying step, and the second supply part supplies gas to the second space in the second drying step. Furthermore, in the first drying step, the amount of gas supplied per unit time from the first supply unit to the first space is greater than the amount of gas supplied per unit time from the second supply unit to the second space. It is characterized by the following: [Effects of the Invention]

[0007] According to the present invention, it is possible to provide a substrate processing apparatus that is advantageous for drying films on a substrate. [Brief explanation of the drawing]

[0008] [Figure 1] This figure shows the configuration of the substrate processing apparatus in the first embodiment. [Figure 2] This diagram shows the configuration of the baffle cover. [Figure 3] This figure illustrates the advantages of the substrate processing apparatus in the first embodiment. [Figure 4] This diagram illustrates the control of internal pressure during the drying process. [Figure 5] This diagram schematically illustrates the process of transporting (loading and unloading) circuit boards. [Figure 6] This figure illustrates a substrate processing method as an example of how to use a substrate processing apparatus. [Figure 7] This figure shows the configuration of the substrate processing apparatus in the second embodiment. [Figure 8]This figure shows the configuration of the substrate processing apparatus in the sixth embodiment. [Figure 9] This is a top view of the substrate processing apparatus in the sixth embodiment. [Modes for carrying out the invention]

[0009] Preferred embodiments of the present invention will be described in detail below with reference to the accompanying drawings. In each figure, the same reference numeral is used for identical components, and redundant descriptions are omitted. In the embodiments and drawings described below, directions are indicated by the XYZ coordinate system. In the XYZ coordinate system, the XY plane is horizontal, and the negative direction of the Z axis can be vertical.

[0010] <First Embodiment> Figure 1 is a schematic cross-sectional view showing the configuration of a substrate processing apparatus (SPA) of this embodiment. The substrate processing apparatus SPA may be configured to process a substrate S having a film F. More specifically, the substrate processing apparatus SPA may be configured to perform a drying process to dry the film F on the substrate S.

[0011] The film F may be, for example, a film composed of a solution containing a solute and a solvent for forming an organic film (hereinafter referred to as a solution film). The solvent may have properties that promote evaporation in a reduced pressure environment below atmospheric pressure. Evaporation of the solvent may be promoted at temperatures higher than room temperature (25°C), for example. The organic film may be, for example, a hole injection layer, hole transport layer, light-emitting layer, electron transport layer, or electron injection layer of an organic light-emitting diode (OLED) device. The manufacturing of an organic EL device may include a process of forming each organic film, such as a hole injection layer, hole transport layer, light-emitting layer, electron transport layer, or electron injection layer, on a substrate. The film F may be applied to the substrate S by a coating device before the substrate S is transported to a substrate processing apparatus (SPA).

[0012] The substrate processing apparatus SPA may include a chamber 10. The chamber 10 is a component that defines an internal space SP1 (first space) separated from the external space. The chamber 10 may also be understood as a component that surrounds the internal space SP1. Hereinafter, the internal space SP1 whose outer edge is defined by the chamber 10 will also be referred to as the internal space SP1 of the chamber 10. In this embodiment, the internal space SP1 is defined as the space inside the chamber 10 and outside the baffle cover 40, which will be described later. In this embodiment, the space on the side where the substrate S is placed will be referred to as "internal," and the space on the side where the substrate S is not placed will be referred to as "external." The chamber 10 may include at least one gate valve 12. The substrate S to be dried can be transported from the external space of the chamber 10 to the internal space SP1 through the gate valve 12. The substrate S that has undergone the drying process can be transported from the internal space SP1 to the external space through the gate valve 12.

[0013] The substrate processing apparatus SPA may further include a depressurization mechanism 30 for reducing the internal space SP1 of the chamber 10. The depressurization mechanism 30 may include, for example, a plurality of pumps, which may include, for example, at least one of a dry pump and a diaphragm vacuum pump. The plurality of pumps may further include, for example, at least one of a turbomolecular pump, cryopump, sorption pump, oil diffusion pump, mechanical booster pump, ejector pump, and oil rotary vacuum pump.

[0014] The substrate processing apparatus SPA may further comprise a substrate holding section 20 for holding a substrate S having a film F. The substrate holding section 20 is located in an internal space SP1. The substrate processing apparatus SPA may further comprise a temperature control section 70 for controlling the temperature of the substrate holding section 20. The temperature control section 70 may typically include a heater for heating the substrate holding section 20, but may also include a cooler for cooling the substrate holding section 20, and the temperature control section 70 performs at least one of heating and / or cooling on the substrate holding section 20. The temperature control section 70 may also be understood as a component for controlling the temperature of the substrate S or the film F on the substrate S.

[0015] The temperature control unit 70 can uniformly control the temperature of each region of the substrate holder 20 so that the substrate S has a uniform temperature distribution. Alternatively, the temperature control unit 70 can control the temperature of each region of the substrate holder 20 at different temperatures so that the substrate S has a uniform temperature distribution. The temperature control unit 70 controls the temperature difference in each region of the substrate S held by the substrate holder 20 to be within 10 degrees. More preferably, the temperature control unit 70 controls the temperature difference in each region of the substrate S held by the substrate holder 20 to be within 5 degrees. The temperature control unit 70 can control the temperature of the substrate holder 20 so that the temperature of the substrate S is any temperature within the range of 0 degrees to 100 degrees. By heating the substrate holder 20, the drying rate of the film F disposed on the substrate S can be improved. In this respect, the substrate processing apparatus SPA including the temperature control unit 70 is more advantageous than the substrate processing apparatus SPA without the temperature control unit 70.

[0016] The substrate processing apparatus SPA may further include a baffle cover 40 (cover) that covers the substrate S held by the substrate holder 20 in the internal space SP1. FIG. 2 is a diagram illustrating an example of the configuration of the baffle cover 40. The baffle cover 40 may have a plurality of openings 42, as illustrated in FIGS. 1 and 2. The arrangement and size of the plurality of openings 42 may be determined so that the film F on the substrate S is uniformly dried. The substrate holder 20 and the baffle cover 40 may define a substrate accommodation space SP2 (second space) surrounded by the substrate holder 20 and the baffle cover 40 in a state where the baffle cover 40 covers the substrate S. In the present embodiment, the internal space SP1 is defined as the space inside the chamber 10 and inside the baffle cover 40 described later. The baffle cover 40 only needs to have a configuration that allows the substrate accommodation space SP2 to communicate with the internal space SP1 while covering the substrate S, and does not necessarily need to have openings. The baffle cover 40 may be configured such that the openings located farther from the center are smaller than the openings located near the center.

[0017] The substrate processing apparatus SPA may include a gas analyzer 60 for detecting a specific gas in the substrate accommodation space SP2 surrounded by the substrate holder 20 and the baffle cover 40. The gas analyzer 60 may be a residual gas analyzer (RGA) such as a mass spectrometer. The specific gas detected by the gas analyzer 60 is a gas evaporated from the film F on the substrate S, that is, a gas to be detected. More specifically, the specific gas may be (a gas of) a solvent.

[0018] The substrate processing apparatus SPA may further include a connection part 62 that connects the gas inlet of the gas analyzer 60 to the substrate accommodation space SP2. The gas inlet is an opening through which the gas analyzer 60 takes in gas. The connection part 62 may be a flexible tube, for example, a glass fiber tube. Alternatively, the connection part 62 may be a bellows. The connection part 62 has a first end E1 and a second end E2. The first end E1 is connected to the gas inlet of the gas analyzer 60, and the second end E2 may be arranged so as to protrude into the substrate accommodation space SP2 from the inner surface of the baffle cover 40. The second end E2 may be arranged so as to protrude into the substrate accommodation space SP2 from the inner surface of the side wall of the baffle cover 40, for example.

[0019] The substrate processing apparatus SPA may include a controller 90. The controller 90 may be configured to control the drying process for drying the film F on the substrate S. The controller 90 may control each part of the substrate processing apparatus SPA. The controller 90 may be configured to determine the completion of drying the film F on the substrate S based on the output of a gas analyzer 60, for example. The controller 90 may be configured to determine that the drying of the film F on the substrate S (the drying process for drying the film F) is complete when the output of the gas analyzer 60 indicates that the amount of a specific gas is a preset amount. The controller 90 may be composed of, for example, a PLD (Programmable Logic Device) such as an FPGA (Field Programmable Gate Array), or an ASIC (Application Specific Integrated Circuit), or a general-purpose or dedicated computer with a program installed, or a combination of all or part of these.

[0020] Figure 3 shows the concentrations of a specific gas (solvent evaporated from the film F of the substrate S) in the internal space SP1 and the substrate containment space SP2. In Figure 3, the dotted curve illustrates the concentration of the specific gas in the internal space SP1, and the solid curve illustrates the concentration of the specific gas in the substrate containment space SP2. Heating the substrate S accelerates the evaporation of the film F, causing the solvent concentration in the substrate containment space SP2 to decrease faster than in the internal space SP1. The solvent released by evaporation from the film F of the substrate S placed in the substrate containment space SP2 moves to the internal space SP1 through the multiple openings 42 of the baffle cover 40 and can condense on the inner surface of the chamber 10 and adhere to that surface. While a large amount of solvent adheres to the inner surface of the chamber 10, the pressure in the internal space SP1 can be maintained at a pressure close to the vapor pressure of the solvent. Then, when the solvent is largely removed from the inner surface of the chamber 10, the pressure in the internal space SP1 can begin to drop from a pressure close to the vapor pressure of the solvent to an even lower pressure. Therefore, even if the solvent concentration in the substrate containment space SP2 decreases sufficiently, the solvent concentration in the internal space SP1 between the baffle cover 40 and the chamber 10 does not decrease easily and can continue to maintain a much higher value than the solvent concentration in the substrate containment space SP2. Thus, the configuration in which the gas analyzer 60 detects a specific gas in the substrate containment space SP2 surrounded by the substrate holding section 20 and the baffle cover 40 is advantageous for quickly detecting the completion of the drying process of the film F on the substrate S.

[0021] Figure 4 illustrates the control of the pressure in the internal space SP1 during a drying process, which can be controlled by the controller 90. This pressure control may include the control of the depressurization mechanism 30. The drying process may include, for example, multiple drying steps, and the controller 90 may control the depressurization mechanism 30 so that multiple drying steps are performed. In the example in Figure 4, the drying process includes drying steps D1 to D4, but the number of drying steps included in the drying process is not limited to a specific number.

[0022] In drying step D1, for example, the film F on the substrate S is dried while the pressure in the internal space SP1 is lowered from atmospheric pressure to a first pressure higher than the vapor pressure of the solvent in the film F on the substrate S. In drying step D2 (first drying step), for example, the film F on the substrate S is dried while the pressure in the internal space SP1 is maintained at the first pressure. In drying step D3, for example, the film F on the substrate S is dried while the pressure in the internal space SP1 is lower than the first pressure and lower than the solvent pressure to a second pressure. In drying step D4 (second drying step), for example, the film F on the substrate S is dried while the pressure in the internal space SP1 is maintained at the second pressure. In order to dry the film F on the substrate S quickly, it is preferable to have low pressure conditions. However, as described above, in this embodiment, drying is performed by multiple drying steps D1 to D4 with different pressure conditions. The reason for this may be, for example, to make the film thickness of the film F uniform. For example, if the pressure is suddenly reduced during the drying process D1, the film thickness of film F may not be uniform. On the other hand, if the film has already dried to some extent, the effect on the film thickness is reduced even if the pressure is lowered. Therefore, by gradually reducing the pressure during the drying process, it is possible to achieve both flattening of the film thickness in film F and shortening the drying time of film F.

[0023] In this embodiment, the first pressure is a value higher than the vapor pressure of the solvent contained in the film F (hereinafter also referred to as the predetermined pressure). This allows the film F to dry to a flat thickness. In this embodiment, the second pressure is a value lower than the vapor pressure of the solvent contained in the film F (the predetermined pressure). This allows the drying time of the film F to be shortened.

[0024] In one example, the controller 90 may be configured to determine the completion of the last drying step D4 among the multiple drying steps D1 to D4 based on the output of the gas analyzer 60. As illustrated in Figure 4, the pressures in the internal space SP1 may differ among the multiple drying steps included in the drying process. However, the multiple drying steps included in the drying process may include two or more drying steps in which the pressures in the internal space SP1 are the same.

[0025] The substrate processing apparatus SPA further includes a gas introduction unit 51 (first supply unit) for introducing an inert gas into the internal space SP1 of the chamber 10. The substrate processing apparatus SPA further includes a gas introduction unit 52 (second supply unit) for introducing an inert gas into the substrate housing space SP2 covered by the baffle cover 40. The gas introduction units 51 and 52 may be flexible tubes. The inert gas may be nitrogen, for example. In this embodiment, the gas supplied by the gas introduction units 51 and 52 may be a gas other than an inert gas, as long as it has a different composition from the solvent of the film F, for example, clean dry air (air).

[0026] The gas introduction unit 51 can adjust the pressure inside the chamber 10 by supplying an inert gas to the internal space SP1. For example, even when the depressurization mechanism 30 is operating during the drying process D2 (first drying process), the pressure in the internal space SP1 can be maintained at the first pressure. That is, the gas introduction unit 51 supplies an inert gas to the internal space SP1 (first space) so that the internal space of the chamber 10 exceeds a predetermined pressure during the drying process D2 (first drying process). Furthermore, the gas introduction unit 51 may supply an inert gas to the internal space SP1 not only during the drying process D2 (first drying process) but also during other drying processes (for example, the second drying process).

[0027] Here, it was explained above that the predetermined pressure is the vapor pressure of the solvent contained in the film F. However, the predetermined pressure may be a different pressure from the vapor pressure of the solvent contained in the film F, as long as it is a value based on the vapor pressure of the solvent contained in the film F. For example, in order to make the film thickness of the film F more stable and flattened, the predetermined pressure may be a pressure slightly higher than the vapor pressure of the solvent contained in the film F.

[0028] The gas introduction unit 52 can accelerate the drying of the substrate housing space SP2 by supplying an inert gas to the substrate housing space SP2. For example, in the drying process D4 (second drying process), the gas introduction unit 52 supplies an inert gas to the substrate housing space SP2 (second space) while maintaining the pressure in the internal space SP1 at a second pressure, thereby drying the film F on the substrate S. The gas introduction unit 52 may also supply an inert gas to the substrate housing space SP2 in other drying processes (for example, the first drying process) as well as drying process D4 (second drying process). That is, an inert gas may be supplied to the second space in at least one of the first drying process and the second drying process. The gas introduction unit 52 is provided penetrating the side surface of the baffle cover 40 and is configured to supply an inert gas to the substrate housing space SP2.

[0029] Furthermore, supplying an inert gas to the substrate containment space SP2 is advantageous for enabling the noise filter of certain gas analyzers 60 to function. Such noise filters may require that the space being detected has a pressure above a predetermined pressure. Specifically, certain gas analyzers 60 may have an ion source, a quadrupole mass filter, and a detector, as well as a noise filter placed between the ion source and the quadrupole mass filter. The noise filter is configured to allow stable elements ionized in the ion source to pass through the noise filter and reach the quadrupole mass filter, but to block metastable molecules (noise sources). However, if the space being detected has a pressure lower than the predetermined pressure, the free path of the elements becomes longer and faster, so even ionized stable molecules cannot pass through the noise filter. If the space being detected has a pressure lower than the predetermined pressure, the detection accuracy may decrease.

[0030] The substrate processing apparatus SPA may further include a lifting mechanism 80 for raising and lowering the baffle cover 40. The lifting mechanism 80 may be used when transporting a substrate S to the substrate holding section 20 and when transporting the substrate S from the substrate holding section 20. Transporting the substrate S may be performed by a transport mechanism RB, as illustrated in Figure 5. The lifting mechanism 80 may, for example, in response to a command from a controller 90, position the baffle cover 40 at a first height when transporting (loading) a substrate to the substrate holding section 20 and when transporting (unloading) a substrate S from the substrate holding section 20. Here, the first height is the height at which the substrate transport mechanism RB can transport the substrate S on the substrate holding section 20. When drying the film F on the substrate S, the lifting mechanism 80 may, for example, in response to a command from a controller 90, position the baffle cover 40 at a second height lower than the first height. Here, the second height is the height for performing a drying process to dry the film F on the substrate S, as illustrated in Figure 1.

[0031] In order to uniformly dry the film F on the substrate S across the entire substrate S, it is advantageous to secure a suitable distance between the upper surface of the baffle cover 40 and the ceiling surface of the chamber 10. However, this requires an increase in the height dimension of the substrate processing apparatus SPA. The substrate holding section 20 may be lowered when transporting the substrate S to and from the substrate holding section 20, but in this case, the height dimension of the substrate processing apparatus SPA may be further increased. On the other hand, as described above, the configuration in which the baffle cover 40 is raised and lowered by the lifting mechanism 80 is advantageous because it utilizes the space provided between the upper surface of the baffle cover 40 and the ceiling surface of the chamber 10 in order to uniformly dry the film on the substrate S. In other words, the configuration in which the baffle cover 40 is raised and lowered by the lifting mechanism 80 is advantageous in order to suppress a further increase in the height dimension of the substrate processing apparatus SPA.

[0032] Figure 6 illustrates a substrate processing method as an example of how to use the substrate processing apparatus SPA. The substrate processing method shown in Figure 6 can be controlled by a controller 90. In step S1, a substrate S having a film F is transported (loaded) to a substrate holding unit 20 located in the internal space SP1 of the chamber 10 and placed on the substrate holding unit 20. In step S2, the substrate S placed on the substrate holding unit 20 can be covered with a baffle cover 40. In step S3, a drying process is performed to dry the film F on the substrate S by reducing the pressure in the internal space SP1 of the chamber 10. As described above, the drying process can consist of multiple drying processes with different pressure conditions. In step S4, it is determined whether all drying processes have been completed. The completion of the drying process can be determined based on the output of the gas analyzer 60. Here, if the drying process includes multiple drying processes, step S4 may be performed after the start of the last of the multiple drying processes. In step S4, if it is determined that all drying steps have been completed, step S5 is executed; otherwise, the remaining drying steps of step S4 are executed again. In step S6, the substrate S held by the substrate holding unit 20 is transported (unloaded) to the space outside the chamber 10.

[0033] <Second Embodiment> In the first embodiment, an example was described in which the gas introduction unit 51 (first supply unit) is installed on the side of the chamber 10. In this embodiment, an example is described in which the gas introduction unit 51 (first supply unit) is installed at the bottom of the chamber 10 (below the substrate S). Note that the configuration other than the gas introduction unit 51 is the same as in the first embodiment and will therefore not be described. Furthermore, matters not mentioned in this embodiment will follow those of the first embodiment.

[0034] Figure 7 is a schematic cross-sectional view showing the configuration of the substrate processing apparatus SPA (vacuum drying apparatus) in this embodiment. The arrows in Figure 7 indicate the airflow, with Figure 7(a) showing the airflow within the chamber 10 during drying process D2 (first drying process) described in Figure 4, and Figure 7(b) showing the airflow within the chamber 10 during drying process D4 (second drying process) described in Figure 4. The gas introduction unit 51 (first supply unit) is located at the bottom of the chamber 10, as shown in Figure 7, and can be installed near the center of the substrate holding unit 20. Below the substrate holding unit 20, a space into which gas can flow is formed, and in this embodiment, this space is also defined as part of the internal space SP1 (first space). By supplying inert gas to the space near the center below the substrate holding unit 20 through the gas introduction unit 51, the exhaust volume of inert gas from each vacuum mechanism 30 becomes equal, and uneven pressure distribution occurring in the internal space SP1 can be reduced. As a result, the film F can be dried at the same speed across the entire surface of the substrate S.

[0035] In drying step D2, the gas inlet 51 and gas inlet 52 can be controlled to form an airflow as shown in Figure 7(a). Specifically, in drying step D2, the amount of inert gas supplied per unit time from the gas inlet 51 to the first space is controlled to be greater than the amount of inert gas supplied per unit time from the gas inlet 52 to the second space.

[0036] In drying step D4, the gas inlet 51 and gas inlet 52 can be controlled to form an airflow as shown in Figure 7(b). Specifically, in drying step D4, the amount of inert gas supplied per unit time from the gas inlet 51 to the first space is controlled to be less than the amount of inert gas supplied per unit time from the gas inlet 52 to the second space.

[0037] Furthermore, the first supply unit may be controlled so that the amount of inert gas supplied to the first space per unit time in the first drying process is greater than the amount of inert gas supplied to the first space per unit time in the second drying process. Furthermore, the second supply unit may be controlled so that the amount of inert gas supplied to the second space per unit time in the first drying process is less than the amount of inert gas supplied to the second space per unit time in the second drying process.

[0038] Furthermore, the amount of inert gas supplied from the gas introduction section 52 to the second space during the first drying process may be 0, and the amount of inert gas supplied from the gas introduction section 51 to the first space during the second drying process may also be 0.

[0039] As described above, by controlling the gas introduction section 51 and the gas introduction section 52, the film F can be flattened in the first drying step. Furthermore, as described above, by controlling the gas introduction section 51 and the gas introduction section 52, the drying of the film F can be accelerated in the second drying step, and the time required to remove residual solvent from the film F can be shortened.

[0040] <Third Embodiment> In this embodiment, we will describe an example in which the gas supplied from the gas introduction unit 52 (second supply unit) has higher kinetic energy due to its higher temperature compared to the inert gas supplied from the gas introduction unit 51 (first supply unit). Note that the configuration other than the gas introduction unit 52 is the same as in the first embodiment and will therefore not be described. Furthermore, matters not mentioned in this embodiment will follow any of the first or second embodiments.

[0041] The substrate processing apparatus SPA is equipped with an inert gas heating mechanism and gas temperature measuring means (not shown). This makes it possible to supply heated inert gas to the substrate housing space SP2. By supplying inert gas to the substrate housing space SP2, the drying of the substrate housing space SP2 can be accelerated. For example, in drying step D4 (second drying step), heated inert gas is supplied to the substrate housing space SP2 (second space) while maintaining the pressure in the internal space SP1 at the second pressure, to dry the film F on the substrate S. Alternatively, heated inert gas may be supplied to the substrate housing space SP2 not only in drying step D4 (second drying step) but also in other drying steps.

[0042] The gas heating mechanism has the function of heating the inert gas supplied to the substrate housing space SP2. The gas heating mechanism may be installed directly in the substrate housing space SP2, or it may be installed outside the internal space SP1. The gas heating mechanism can also be installed in the gas introduction section 52. However, the heat from the heating part of the gas heating mechanism is insulated from the wall surface forming the substrate housing space SP2, and the temperature rise of the wall surface is sufficiently suppressed.

[0043] The inert gas supplied from the gas inlet 52 may be ejected either towards the substrate or towards the wall surface forming the substrate housing space SP2. Furthermore, the tip of the ejection section may be branched, or it may have multiple nozzles like a showerhead.

[0044] As described above, the gas supplied from the gas introduction section 52 has a higher temperature and therefore higher kinetic energy compared to the inert gas supplied from the gas introduction section 51, which can accelerate the drying of the solvent in the substrate containment space SP2. As a result, the drying of the film F is promoted, and the time required to remove residual solvent from the film F can be shortened.

[0045] <Fourth Embodiment> In this embodiment, we will describe an example in which the gas supplied from the gas introduction unit 52 (second supply unit) has a larger molecular weight than the inert gas supplied from the gas introduction unit 51 (first supply unit). Note that the configuration other than the gas introduction unit 52 is the same as in the first embodiment and will therefore not be described. Furthermore, matters not mentioned in this embodiment will follow any of the first to third embodiments.

[0046] In this embodiment, the inert gas supplied from the gas inlet 52 has a larger molecular weight than the inert gas supplied from the gas inlet 51. For example, the inert gas supplied from the gas inlet 52 may be a noble gas such as argon, krypton, xenon, or radon. Furthermore, any gas with a different composition from the solvent of the film F may be used, such as carbon dioxide. The direction in which the inert gas supplied from the gas inlet 52 is ejected may be directed towards the substrate or towards the wall surface forming the substrate housing space SP2. The tip of the ejection part may be branched, or it may have multiple nozzles like a showerhead.

[0047] As described above, the gas supplied from the gas introduction section 52 has a larger molecular weight and therefore higher kinetic energy compared to the inert gas supplied from the gas introduction section 51, which can accelerate the drying of the solvent in the substrate containment space SP2. As a result, the drying of the film F is promoted, and the time required to remove residual solvent from the film F can be shortened.

[0048] <Fifth Embodiment> Specific examples of the height and direction of the gas outlet will be described. Note that the basic configuration is the same as in the first embodiment, so the explanation will be omitted. Furthermore, matters not mentioned in this embodiment will follow those of the first embodiment.

[0049] The height of the gas outlet supplied from the gas inlet 52 into the baffle cover 40 is preferably near the substrate S, which is below the height of the baffle cover 40. The upper limit of the height of the gas outlet is 1 / 2 or less of the height of the baffle cover 40. The direction of gas discharge is parallel to the substrate S, preferably in the direction of the multiple openings 42 in the baffle cover 40. The horizontal position of the gas outlet from the inner wall surface of the baffle cover 40 is such that the gas is sprayed onto the inner wall surface of the baffle cover 40 (for example, the top surface of the cover). It is also desirable that the outlet is installed so that gas is sprayed onto all the inner walls of the baffle cover 40. The tip of the discharge section may be branched, and there may be multiple discharge openings like a shower head.

[0050] As described above, by spraying gas from the gas introduction section 52 onto the inner wall surface of the baffle cover 40, the solvent adhering to the wall surface evaporates, and the evaporated solvent molecules are transported from inside the substrate housing space SP2 to the outside by collision with the gas, thereby accelerating the drying time. As a result, the time required to remove residual solvent from the film F in the second drying step can be shortened.

[0051] <Sixth Embodiment> In this embodiment, an example is described in which the gas outlet supplying gas from the gas introduction section 52 to the inside of the baffle cover 40 is installed within the substrate holding section 20. Note that the configuration other than the gas introduction section 51 is the same as in the first embodiment and therefore will not be described. Furthermore, matters not mentioned in this embodiment follow those of the first embodiment.

[0052] Figure 8 is a schematic cross-sectional view showing the configuration of the substrate processing apparatus SPA (vacuum drying apparatus) in this embodiment. The arrows in Figure 8 indicate the airflow, and the diagram shows the airflow inside the chamber 10 during the drying process D4 (second drying process) described in Figure 4. As shown in Figure 8, in this embodiment, gas outlets supplied from the gas introduction section 52 to the inside of the baffle cover 40 may be provided inside the substrate holding section 20. Figure 9 is a schematic top view of the configuration of the substrate S, baffle cover 40, substrate holding section 20, and gas introduction section 52. As shown in Figure 9, the gas outlets may be located between the inner wall surface of the baffle cover 40 and the edge of the substrate S, and should be in a position where gas is sprayed onto all the inner wall surfaces of the baffle cover 40. The number of gas outlets may also be numerous. Furthermore, if it is necessary to change the amount of gas according to the shape and volume of the baffle cover 40, such as the four corners of the baffle cover 40 in Figure 9, the number of outlets can be controlled. The timing of gas injection can be controlled in the first and second drying processes. The gas flow rate can be arbitrarily controlled within both drying processes. Furthermore, if there are multiple injection ports, the flow rate can be individually controlled depending on the injection position. In other words, the gas inlet 52 can control the amount of gas supplied by changing the time and location of gas supply.

[0053] As described above, by installing the gas introduction unit 52 in the substrate holding unit 20, a gas supply mechanism is not required within the space of the baffle cover 40. Therefore, in the first drying step, the areas where the dried solvent adheres from the substrate S are limited to the baffle cover 40. As a result, in the second drying step, the time required to remove residual solvent from the film F can be shortened.

[0054] <Seventh Embodiment> In this embodiment, the gas outlet supplied from the gas introduction section 52 is located outside the baffle cover 40. Furthermore, a mechanism may be provided to insert the gas outlet into the baffle cover 40 through the space created between the baffle cover 40 and the substrate holding section 20 when the baffle cover 40 is raised after the first drying process is completed. It is also desirable to lower the baffle cover 40 as much as possible after the gas outlet has been inserted into the baffle cover 40, in order to minimize the gap between the baffle cover 40 and the substrate holding section 20.

[0055] As described above, the gas introduction section 52 is inserted into the baffle cover 40 after the completion of the first drying step, and in the second drying step, the gas is sprayed onto the inner wall surface of the baffle cover 40. This suppresses solvent adhesion at the gas outlet in the first drying step, and as a result, in the second drying step, the drying of the film F is accelerated, and the time required to remove residual solvent from the film F can be shortened.

[0056] <Embodiment for manufacturing an article> The method for manufacturing an article according to an embodiment of the present invention is suitable for manufacturing articles such as organic EL (OLED) panels using an inkjet printing apparatus. The method for manufacturing an article according to this embodiment includes a step of obtaining a coated substrate by arranging or coating a solution film (a solution containing a solute and a solvent for forming an organic film) on a substrate by a printing method using an inkjet printing apparatus or the like (coating step). It also includes a step of drying the solution film on the coated substrate with the above-mentioned vacuum drying apparatus to obtain a dried substrate on which a dried film has been formed (drying step). Furthermore, this manufacturing method includes other well-known steps (firing, cooling, dehumidification, dry cleaning, electrode formation, sealing film formation, etc.). The method for manufacturing an article according to this embodiment is advantageous over conventional methods in at least one of the performance, quality, productivity, and production cost of the article.

[0057] Although preferred embodiments of the present invention have been described above, it goes without saying that the present invention is not limited to these embodiments, and various modifications and changes are possible within the scope of its essence. [Explanation of Symbols]

[0058] 10 Chambers 20 Board holding part 30. Pressure reduction mechanism 40 Baffle Cover (Cover) 51 Gas Inlet (First Supply Unit) 52 Gas Inlet (Second Supply Unit) D2 Drying process (1st drying process) D4 Drying process (second drying process) F membrane S substrate SP1 Internal space (1st space) SP2 board housing space (second space) SPA substrate processing equipment

Claims

1. A first drying step involves drying the film on the substrate under a pressure higher than a predetermined pressure, A substrate processing apparatus for drying a film on a substrate by a drying step including a second drying step of drying the film under a pressure lower than the predetermined pressure, A substrate holding portion for holding the substrate, Chamber and, A depressurization mechanism for reducing the pressure inside the chamber, An opening is provided, and a cover is provided to cover the substrate held by the substrate holding part inside the chamber, A first supply unit that supplies gas to a first space which is inside the chamber and outside the cover, A second supply unit that supplies gas to a second space which is inside the chamber and inside the cover, It has, The first supply unit supplies gas to the first space in the first drying process. The second supply unit supplies gas to the second space in the second drying step, A substrate processing apparatus characterized in that, in the first drying step, the amount of gas supplied per unit time from the first supply unit to the first space is greater than the amount of gas supplied per unit time from the second supply unit to the second space.

2. The substrate processing apparatus according to claim 1, characterized in that the first supply unit supplies gas to the space below the substrate holding unit.

3. The substrate processing apparatus according to claim 1, characterized in that the second supply unit is provided penetrating the side surface of the cover.

4. The substrate processing apparatus according to claim 1, characterized in that, in the second drying step, the amount of gas supplied per unit time from the first supply unit to the first space is less than the amount of gas supplied per unit time from the second supply unit to the second space.

5. The substrate processing apparatus according to claim 1, characterized in that the amount of gas supplied per unit time to the first space by the first supply unit in the first drying step is greater than the amount of gas supplied per unit time to the first space by the first supply unit in the second drying step.

6. The substrate processing apparatus according to claim 1, characterized in that the amount of gas supplied per unit time to the second space by the second supply unit in the first drying step is less than the amount of gas supplied per unit time to the second space by the second supply unit in the second drying step.

7. The substrate processing apparatus according to claim 1, further comprising a temperature control unit that performs at least one of heating and cooling of the substrate holding portion.

8. The substrate processing apparatus according to claim 7, characterized in that the temperature control unit controls the temperature so that the temperature difference in each region of the substrate held by the substrate holding unit is within 10 degrees.

9. The substrate processing apparatus according to claim 1, further comprising a lifting mechanism for raising and lowering the cover.

10. The substrate processing apparatus according to claim 1, characterized in that the predetermined pressure is a pressure determined based on the vapor pressure of the solvent contained in the film.

11. The substrate processing apparatus according to claim 10, characterized in that the predetermined pressure is the vapor pressure of the solvent contained in the film.

12. The substrate processing apparatus according to claim 1, characterized in that the gas supplied from the first supply unit and the second supply unit is an inert gas.

13. The substrate processing apparatus according to claim 1, characterized in that the gas supplied from the second supply unit has higher kinetic energy than the gas supplied from the first supply unit.

14. The substrate processing apparatus according to claim 1, characterized in that the gas supplied from the second supply unit is at a higher temperature than the gas supplied from the first supply unit.

15. The substrate processing apparatus according to claim 1, characterized in that the gas supplied from the second supply unit has a larger molecular weight than the gas supplied from the first supply unit.

16. The substrate processing apparatus according to claim 1, characterized in that the gas supplied from the second supply unit is supplied from a position that is 1 / 2 or less of the height of the cover.

17. The substrate processing apparatus according to claim 1, characterized in that the direction in which the gas supplied from the second supply unit is blown is the direction in which the gas is blown onto the upper surface of the cover.

18. The substrate processing apparatus according to claim 1, characterized in that the second supply unit is located in the substrate holding unit.

19. The substrate processing apparatus according to claim 1, characterized in that the second supply unit controls the amount of gas supplied by changing the time and location of gas supply.

20. A first drying step involves drying a film on a substrate under a pressure higher than a predetermined pressure using a substrate processing apparatus, A substrate processing method comprising a second drying step of drying the film at a pressure lower than the predetermined pressure using the substrate processing apparatus, The substrate processing apparatus is A substrate holding portion for holding the substrate, Chamber and, A depressurization mechanism for reducing the pressure inside the chamber, An opening is provided, and a cover is provided to cover the substrate held by the substrate holding part inside the chamber, A first supply unit that supplies gas to a first space which is inside the chamber and outside the cover, A second supply unit that supplies gas to a second space which is inside the chamber and inside the cover, It has, The first supply unit supplies gas to the first space in the first drying process. The second supply unit supplies gas to the second space in the second drying step, A substrate processing method characterized in that, in the first drying step, the amount of gas supplied per unit time from the first supply unit to the first space is greater than the amount of gas supplied per unit time from the second supply unit to the second space.

21. A coating process involves applying a solution film onto a substrate to obtain a coated substrate, A drying step to obtain a dried substrate by drying the coated substrate using the substrate processing method described in claim 20, A method for manufacturing an article, characterized by manufacturing an article from the aforementioned dried substrate.

Citation Information

Patent Citations

  • Dry treatment device and substrate processing device

    JP2004207484A

  • Supercritical treatment apparatus

    JP2005000853A

  • Paste material drying method and device

    JP2005049020A

  • Substrate processing apparatus and substrate processing method

    JP2008034674A

  • Reduced-pressure drying device and reduced-pressure drying method

    JP2011058656A