Proton Flow Reactor System
The proton flow reactor system addresses inefficiencies in hydrogen storage by using a slurry electrode with carbon-based particles, achieving high energy density and efficient hydrogen production, surpassing existing systems in energy efficiency and storage capacity.
Patent Information
- Application Number
- JP2022580250
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-06-25
- Filing Date
- 2021-06-25
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2041-06-25
AI Technical Summary
Existing energy storage systems, such as proton exchange membrane fuel cells, face challenges in storing fuels like hydrogen efficiently, with low round-trip energy efficiency and difficulties in storing gases like hydrogen, leading to high costs and inefficiencies compared to other energy storage methods.
A proton flow reactor system utilizing a slurry electrode with specific carbon-based storage particles in a liquid electrolyte, allowing for the reversible storage and release of hydrogen through a slurry flow process, enabling high gravimetric and volumetric energy density.
The system achieves high energy density and efficient energy transfer by separating the charging and storage processes, allowing for the production of high-purity hydrogen gas and improving round-trip efficiency, surpassing the limitations of existing technologies.
Smart Images

Figure 0007955166000001 
Figure 0007955166000002 
Figure 0007955166000003
Abstract
Description
[Technical Field]
[0001] The present invention generally relates to a proton flow reactor system having a slurry electrode containing particles in a liquid electrolyte. [Background technology]
[0002] An electrochemical cell is a device that converts electrical energy into chemical energy, or vice versa. Electrochemical cells that generate electric current are generally called voltacells or galvanicells, while those that use electric current to generate chemical reactions are generally called electrolytic cells. Devices with a large number of voltacells connected in series or parallel are generally called batteries, while electrochemical devices that receive a continuous supply of reactants are generally called fuel cells (fuel cells). Another type of device is a flow battery. In a flow battery, one or both electrodes of a cell have a continuous flow of material, usually in liquid form, which is continuously charged and discharged. Additional electrode material is stored externally, usually in a tank, and is typically circulated between one or more cells using a pump.
[0003] Electrochemical cells, such as fuel cells, have recently attracted attention as an efficient and environmentally friendly alternative to conventional power sources like combustion engines and generators. Power systems that can achieve zero or reduced emissions of greenhouse gases and other pollutants are considered essential to enabling the continued use of power systems, including power transmission via roads, rail, or ships.
[0004] One type of fuel cell is the proton exchange membrane fuel cell ("PEMFC"). In PEMFCs, Nafion is used as the electrolyte. TM A proton exchange membrane ("PEM"), typically containing polymers such as [specific polymers], separates the anode from the cathode. In a typical PEMFC, hydrogen gas is supplied to the anode and separated into protons and electrons. The separated protons can then move to the cathode through the PEM. Here, the protons react with oxygen to form water, generating electricity.
[0005] When one or more reactants are supplied as gases, the storage of fuels or reactants for cleaner energy is a current concern. Taking PEMFCs as an example, the reactants used are typically gaseous oxygen and hydrogen. While in-situ air can be used as the oxygen source, certain fuel cell structures may require purified oxygen that needs to be stored. Hydrogen gas is also difficult to store, so several options, including the storage of pressurized hydrogen, have been developed to address this problem. More generally, technologies developed for storing hydrogen for use in combustion systems and fuel cells include the storage of pressurized hydrogen, the storage of liquefied hydrogen, and the storage of metal hydrides before supplying them as hydrogen gas. In any electrical energy storage system, "round-trip" energy efficiency (which is the main reason for preparing hydrogen for storage) is a matter of great interest. There is a process in which an electrolytic cell generates hydrogen gas by decomposing water, that hydrogen gas is stored as gas, and a fuel cell uses this gas to generate electricity. This process typically provides a relatively low round-trip energy efficiency of less than 50%. This is a disadvantage compared to other energy storage methods, such as lithium batteries, which offer round-trip efficiency exceeding 80% for short-term storage.
[0006] Despite developments in this field, there is still a need for technologies to store fuels or reactants such as hydrogen. Ideally, such technologies should offer storage with one or more of the following characteristics: small volume, minimal additional weight, low cost, and adequate energy efficiency.
[0007] Heidari et al., “Technical Feasibility of a Proton Battery with an Activated Carbon Electrode,” International Journal of Hydrogen Energy 43 (2018) 6197-6209 (“Heidari”), discloses the development of a small-scale “proton battery.” This entire disclosure is incorporated herein by reference. The small-scale “proton battery” is described as a reversible PEMFC with an integrated solid electrode for storing hydrogen in atomic form. Heidari explains that the proton battery is a hybrid of a hydrogen fuel cell system and a battery-based system because the proton battery contains a fuel source trapped in the solid electrode within the device.
[0008] According to Heidari, the first proton battery was essentially a renewable PEMFC with an integrated solid electrode for storing atomic hydrogen. During electrolysis (i.e., "charging mode"), protons are generated and enter the solid electrode through the PEM. Here, the protons are neutralized by excess electrons to form hydrogen atoms bonded with the electrode material. During galvanic operation (i.e., "discharging mode"), the stored protons return to the oxygen side through the PEM, where they combine with oxygen and electrons from the external circuit to generate water again, thereby generating electricity.
[0009] Heidari states that the first solid electrodes for hydrogen storage mainly consisted of expensive metal alloys made of nickel, cobalt, lanthanum, and cerium. Heidari then proposes porous carbon as a possible alternative to metal electrodes. In porous carbon, atomic hydrogen is stored in the porous carbon electrode during electrolysis. Figure 1 shows Heidari's proton battery design 100, where a carbon electrode 116 is located on one side of the "battery". The other side of the battery includes an oxygen side with a channel 104 for air movement. The proton battery 100 is typically held together by stainless steel end plates 102, 120, which are clamped integrally with bolts 122. Between the end plates 102 and 120, from the oxygen side, are provided a silicone seal gasket 106, a porous sintered titanium felt 108 used as a gas diffusion layer material, a catalyst material 110 formed from iridium / ruthenium oxide and platinum black, a Nafion PEM 114, an activated carbon electrode 116 immersed in sulfuric acid, and a stainless steel mesh supporting the electrode 118.
[0010] According to Heidari's conclusions, the gravimetric density of material-based hydrogen storage at atmospheric pressure is already comparable to that of metal hydroxide hydrogen storage technologies with hydrogen gas pressures of 10 bar or higher, but inferior to that of hydrogen gas storage compressed to 700 bar. Heidari further mentions research areas including the use of novel graphene-based materials within storage electrodes, and research areas for optimizing charging and discharging techniques (including reducing the hydrogen gas generation rate and improving the kinetics of the hydrogen storage process).
[0011] Despite continuous advancements in alternative energy generation and storage technologies, there remains a need for new systems to replace conventional fossil fuel combustion systems for energy generation and storage.
[0012] References to prior publications, information derived therefrom, or known matters in this specification shall not be deemed, nor shall they be deemed, as an acknowledgment or admission, or any form of suggestion, that the prior publications, information derived therefrom, or known matters form part of the common general knowledge in the field of endeavor to which this specification relates. [Summary of the Invention]
[0013] According to a first aspect of the present invention, there is provided a method of storing electrical energy as chemical energy, the method comprising: feeding an input slurry comprising uncharged storage particles and an electrolyte to a first half-cell of an electrochemical cell; H + or H3O + feeding a source of ions to a second half-cell of the electrochemical cell; applying a voltage to the electrochemical cell to cause H + or H3O + ions to move from the second half-cell to the first half-cell to convert the uncharged storage particles to charged storage particles; and removing an output slurry comprising charged storage particles and electrolyte from the first half-cell.
[0014] In an embodiment according to the first aspect, the uncharged storage particles have one or more of the following characteristics: (A) high electrical conductivity; (B) an average diameter of 0.5 to 5 microns; (C) a porosity in the range of 20% to 50%; (D) substantial "ultramicropores" having a diameter of 0.5 to 2 nanometers (nm), or substantial layered domains having an interlayer spacing of 0.5 to 2 nm; (E) mesopores having a diameter or width of 2 to 50 nm; (F) an electrochemical hydrogen storage capacity of 0.5 to 8 wt%.
[0015] In the embodiment according to the first aspect, the uncharged storage particles have each of the above-described characteristics (A) to (F).
[0016] In the embodiment according to the first aspect, the uncharged storage particles include carbon particles.
[0017] In embodiments according to the first aspect, the carbon particles are selected from particles mainly formed from one or more materials selected from activated carbon, graphene, oxygen-functionalized graphene, nitrogen-functionalized graphene or nitrogen-doped graphene, graphitic carbonitride, graphene aerogel, or carbon nanotubes.
[0018] In the embodiment according to the first aspect, the carbon particles include particles derived from a phenolic resin and activated with potassium hydroxide.
[0019] In an embodiment according to the first aspect, the input slurry contains 5-35% (w / w), selectively 5-15% (w / w), or 15-35% (w / w) of uncharged storage particles.
[0020] In the embodiment according to the first aspect, H supplied to the second half cell + or H3O + The aforementioned source of ions is water.
[0021] In an embodiment according to the first aspect, the method further comprises the steps of mixing uncharged storage particles and an electrolyte outside the first half cell to form the input slurry, and supplying the mixed input slurry to the first half cell.
[0022] In an embodiment according to the first aspect, the method further comprises the step of separating charged storage particles from the electrolyte in the output slurry, after the step of removing the output slurry from the first half cell.
[0023] In the embodiment according to the first aspect, the step of separating the charged storage particles from the electrolyte comprises the step of filtering the charged storage particles from the electrolyte, selectively using a movement filtering membrane.
[0024] In the embodiment according to the first aspect, the step of separating the charged storage particles from the electrolyte comprises the step of drying the charged storage particles.
[0025] In the embodiment according to the first aspect, the step of drying the charged storage particles comprises the step of applying an inert gas to the charged storage particles.
[0026] In the embodiment according to the first aspect, the method further comprises the step of storing the charged storage particles after the step of separating the charged storage particles from the electrolyte.
[0027] In the embodiment according to the first aspect, in the step of storing the charged storage particles, the charged storage particles are stored in an inert atmosphere.
[0028] According to the second aspect of the present invention, there is provided a method of generating electricity, the method comprising: supplying an input slurry containing charged storage particles and an electrolyte to a first half-cell of an electrochemical cell; supplying an oxidant stream to a second half-cell of the electrochemical cell; H + or H3O + generating electricity by moving ions from the first half-cell and reacting them with the oxidant in the second half-cell; removing an output slurry containing uncharged storage particles and an electrolyte from the first half-cell; comprising.
[0029] In the embodiment according to the second aspect, the charged storage particles are: (A) high electrical conductivity, (B) an average diameter of 0.5 to 5 microns, (C) Porosity in the range of 20% to 50%, (D) Substantially "ultrafine pores" with a diameter of 0.5 to 2 nanometers (nm), or substantial layered domains with interlayer spacing of 0.5 to 2 nm. (E) Mesopores having a diameter or width of 2 to 50 nm, (F) Electrochemical hydrogen storage capacity of 0.5-8 wt%, It possesses one or more of the following characteristics.
[0030] In the embodiment according to the second aspect, the charged storage particle has all of the above-described characteristics (A) to (F).
[0031] In the embodiment according to the second aspect, the charged storage particles include carbon particles.
[0032] In embodiments of the second aspect, the carbon particles are selected from particles mainly formed from one or more materials selected from activated carbon, graphene, oxygen-functionalized graphene, nitrogen-functionalized graphene or nitrogen-doped graphene, graphitic carbonitride, graphene aerogel, or carbon nanotubes.
[0033] In the embodiment according to the second aspect, the carbon particles include particles derived from a phenolic resin and activated with potassium hydroxide.
[0034] In an embodiment according to the second aspect, the input slurry contains 5-35% (w / w), selectively 5-15% (w / w), or 15-35% (w / w) of uncharged storage particles.
[0035] In the embodiment according to the second aspect, the charged storage particles are manufactured and processed according to the first aspect of the present invention.
[0036] In the embodiment according to the second aspect, the oxidizing agent stream supplied to the second half-cell contains oxygen gas.
[0037] In the embodiment according to the second aspect, the oxidizing agent stream supplied to the second half-cell is air.
[0038] In an embodiment according to the second aspect, the method comprises the step of heating the cell while generating electricity.
[0039] In an embodiment according to the second aspect, the method comprises the steps of: mixing charged storage particles and an electrolyte outside the first half cell to form the input slurry; and supplying the mixed input slurry to the first half cell.
[0040] In an embodiment according to the second aspect, the method further comprises the step of separating uncharged storage particles from the electrolyte after the step of removing the output slurry from the first half cell.
[0041] In the embodiment according to the second aspect, the step of separating the uncharged storage particles from the electrolyte comprises the step of drying the uncharged storage particles.
[0042] In an embodiment according to the second aspect, the method comprises a step of storing the uncharged storage particles after a step of separating the uncharged storage particles from the electrolyte.
[0043] In embodiments according to the first or second aspect, the electrochemical cell comprises a proton exchange membrane separating the first half-cell and the second half-cell, the proton exchange membrane comprising a layer substantially formed from a tetrafluoroethylene-based fluoropolymer copolymer, wherein the proton exchange membrane comprises a layer substantially formed from a tetrafluoroethylene-based fluoropolymer copolymer.
[0044] In embodiments according to the first or second aspect, the step of supplying the input slurry to the electrochemical cell and the step of removing the output slurry from the electrochemical cell are carried out as a continuous process.
[0045] In embodiments according to the first or second aspect, the steps of supplying the input slurry to the electrochemical cell and removing the output slurry from the electrochemical cell are carried out as a batch process.
[0046] In embodiments according to the first or second aspect, the electrolyte is selected from a mineral acid in an aqueous solution, an ionic liquid, an ionic liquid in an aqueous solution, an organic acid in an aqueous solution, or a combination thereof.
[0047] In an embodiment according to the first or second aspect, the method comprises the step of generating the output slurry by processing the input slurry through a plurality of electrochemical cells arranged in series.
[0048] In embodiments of the first or second aspect, the method comprises the step of generating an output slurry by processing the input slurry through a plurality of electrochemical cells arranged in parallel, wherein the plurality of electrochemical cells are selectively arranged in a stack.
[0049] In embodiments according to the first or second aspect, the charged storage particles contain, on average, at least 0.5 wt% of captured hydrogen, and selectively 1.0 to 8.0 wt% of captured hydrogen.
[0050] According to a third aspect of the present invention, charged storage particles generated according to the first aspect are provided.
[0051] In an embodiment according to a third aspect, a slurry is provided that includes the charged storage particles and an electrolyte.
[0052] In the embodiment according to the third aspect, the charged storage particles are stored in an inert atmosphere.
[0053] In a fourth aspect of the present invention, uncharged storage particles processed according to the second aspect are provided.
[0054] In an embodiment according to a fourth aspect, a slurry is provided that includes the uncharged storage particles and an electrolyte.
[0055] In a fifth embodiment of the present invention, a method for generating hydrogen gas is provided, and the method is The steps include supplying an input slurry containing charged storage particles and an electrolyte to the first half cell of an electrochemical cell, While ensuring that substantially no oxidizing agent is present, or only a minimal amount of oxidizing agent is present, H + or H3O + A step of moving ions from the first half cell, The steps include: starting the generation of hydrogen gas in the second half cell, The steps include: extracting the output flow containing hydrogen gas from the second half-cell; It is equipped with.
[0056] In the embodiment according to the fifth aspect, the step of initiating the generation of hydrogen gas comprises one or more of the following steps: applying a low potential to the electrochemical cell, applying gentle heat to the electrochemical cell, or keeping the cell stopped for at least one hour.
[0057] In an embodiment according to the fifth aspect, the step of ensuring that there is substantially no oxidizing agent, or only a minimal amount of oxidizing agent, in the second half-cell is: The step of pouring water into the second half cell, A step of filling the second half cell with a non-oxidizing gas such as argon or nitrogen, The step of applying a vacuum to the second half cell, It can be equipped with.
[0058] In an embodiment according to the fifth aspect, the method comprises the step of generating electricity while generating hydrogen gas.
[0059] In a sixth aspect of the present invention, a system is provided for carrying out a method according to the first, second, or fifth aspect, the system comprising an electrochemical cell, The electrochemical cell further comprises a first half-cell, a second half-cell, and a proton exchange membrane that separates the first half-cell from the second half-cell. The first half-cell is configured to receive a slurry containing storage particles and an electrolyte.
[0060] In an embodiment according to the sixth aspect, the proton exchange membrane comprises a layer substantially formed from a tetrafluoroethylene-based fluoropolymer copolymer.
[0061] In an embodiment according to the sixth aspect, the system further comprises a pump for pumping a slurry containing storage particles and an electrolyte into the first half cell.
[0062] In an embodiment according to the sixth aspect, the system includes a separator, The separator is configured to receive an output slurry containing storage particles and an electrolyte from the first half cell and separate the storage particles from the electrolyte.
[0063] In the sixth embodiment, the separator includes a mobile filter membrane.
[0064] In the sixth embodiment, the separator includes a dryer.
[0065] In the sixth embodiment, the dryer is configured to pass an inert gas through the stored particles.
[0066] In an embodiment according to the sixth aspect, the system comprises a storage device configured to store storage particles separated from the electrolyte.
[0067] In the sixth embodiment, the storage device is configured to store the storage particles in an inert atmosphere.
[0068] Throughout this specification and the subsequent claims, and unless otherwise required by context, it shall be understood as follows: The term "carbon particles" should be understood to mean particles primarily formed from electrically conductive carbon-based materials. Examples of suitable electrically conductive carbon-based materials include, but are not limited to, activated carbon, graphene, oxygen-functionalized graphene, nitrogen-functionalized or nitrogen-doped graphene, graphitic carbonitrides, graphene aerogels, or carbon nanotubes. The term "charged storage particle" should be understood to mean a storage particle on which a chemically significant amount of hydrogen atoms or ions are bound or attached via an electrochemical process. The term "uncharged storage particles" should be understood to mean storage particles that are not charged storage particles, but which were previously charged and whose hydrogen atoms or ions, bound to or otherwise stored within the particles, have been discharged, lost, or depleted. The term "slurry" should be understood as a mixture of particles in a liquid, ranging from a low particle concentration of 5% (weight particles / weight liquid) to a paste concentration of 40-60% (w / w). The term “storage particles” should be understood to mean particles suitable for storing hydrogen on their surface or internally. Preferably, according to certain embodiments of the present invention, storage particles may have each of the following characteristics: high electrical conductivity, an average diameter of 0.5 to 5 microns, a porosity in the range of 20% to 50%, substantial “hyperfine pores” with a diameter of 0.5 to 2 nanometers (nm) or substantial layered domains with an interlayer spacing of 0.5 to 2 nm, mesopores with a diameter or width of 2 to 50 nm, and an electrochemical hydrogen storage capacity of 0.5 to 8 wt%. According to embodiments of the present invention, storage particles may be carbon particles. In alternative embodiments, storage particles may be formed substantially from silicon. A description of a range of numbers disclosed herein (e.g., 1 to 10) is intended to include all rational numbers within that range (e.g., 1, 1.1, 2, 3, 3.9, 4, 5, 6, 6.5, 7, 8, 9, 10), and thereby any range of rational numbers within that range (e.g., 2 to 8, 1.5 to 5.5, 3.1 to 4.7). Therefore, all subranges of all ranges expressly disclosed herein are expressly disclosed. These are merely examples of what is specifically intended, and all possible combinations of numerical values between the listed minimum and maximum values should be considered expressly disclosed herein as well. The term "or" shall be understood to include "and" to the extent that the context allows. The term "(w / w)" should be understood as referring to the weight of the particles relative to the weight of the electrolyte. The term "comprise" and variations such as "include" should be understood to mean that they include the integer or step, or group of integers or steps, but do not exclude other integers or steps, or groups of integers or steps. Terms such as “side,” “end,” “top,” “bottom,” “upper,” and “downward” are used solely to describe related elements and do not in any way describe a specific orientation of the device, indicate or suggest a required or essential orientation of the device, or specify how the inventions described herein are used, mounted, displayed, or positioned in use. [Brief explanation of the drawing]
[0069] [Figure 1] Figure 1 shows the proton battery described in Heidari. [Figure 2] Figure 2 shows a "proton flow reactor" operating in charging mode, or electrolytic cell mode, according to an embodiment of the present invention. [Figure 3] Figure 3 shows a proton flow reactor operating in discharge mode, i.e., fuel cell mode for power supply, according to an embodiment of the present invention. [Figure 4] Figure 4 shows a proton flow reactor according to an embodiment of the present invention, in which the oxygen-side electrode and the hydrogen-side electrode are heated, and the proton flow reactor does not have titanium GDL on the oxygen side. [Figure 5] Figure 5 shows a slurry electrode for a proton flow reactor incorporating a carbon foam current collector according to an embodiment of the present invention. [Figure 6] Figure 6 shows one embodiment of a continuous system for separating solid storage particles from a liquid electrolyte. [Figure 7] Figure 7 shows an embodiment of the present invention illustrating a domestic and international energy storage and transfer system. [Figure 8] Figure 8 shows experimental results demonstrating the performance of a paste electrode using phenolic resin activated carbon and 1M sulfuric acid as the electrolyte, as a limited example of a slurry electrode according to an embodiment of the present invention. [Figure 9] Figure 9 shows experimental results demonstrating the performance of a paste electrode using phenolic resin activated carbon and 1M sulfuric acid as the electrolyte, as a limited example of a slurry electrode according to an embodiment of the present invention. [Figure 10] Figure 10 shows experimental results demonstrating the performance of a paste electrode using activated carbon of phenolic resin and 1M sulfuric acid as the electrolyte, as a limited example of a slurry electrode according to an embodiment of the present invention. [Figure 11] Figure 11 shows experimental results demonstrating the performance of a paste electrode using activated carbon of phenolic resin and 1M sulfuric acid as the electrolyte, as a limited example of a slurry electrode according to an embodiment of the present invention. [Figure 12] Figure 12 shows (top) a schematic vertical cross-section of an inflow / outflow paste proton flow reactor according to an embodiment of the present invention, and (bottom) a 3D view showing the H-side end plate of the reactor, the channel through which the paste flows in and out, and the rectangular active region of the cell. [Figure 13]Figure 13 shows a microfluidic proton flow reactor according to an embodiment of the present invention, where (a) is a schematic side view of the proton flow reactor, (b) is a photograph of the reactor, and (c) is a photograph of the reactor in a charged mode showing oxygen bubbles on the oxygen side of the cell. [Figure 14] Figure 14 shows a cyclic voltammogram of an activated carbon sample from phenol resin in a 1M dilute sulfuric acid electrolyte, taken in a three-electrode cell at a scan rate of 2 mV / s over a potential range of -0.4 to +0.9 V relative to a standard hydrogen electrode. [Modes for carrying out the invention]
[0070] In a broad sense, the present invention relates to a method for storing chemical energy, a method for generating electricity, storage particles resulting from such a method, and a system for carrying out such a method. Proton Flow Reactor
[0071] One embodiment of the present invention provides a “proton flow reactor” that operates electrochemically, similar to the proton battery disclosed in Heidari. However, unlike the proton battery described in Heidari, in which the first half-cell is configured to house a fixed carbon electrode, the first half-cell in the proton flow reactor is configured to process a slurry consisting of incoming storage particles. Surprisingly, the use of the proton flow reactor has been found to offer many advantages and favorable conditions in terms of energy storage, energy transfer, and use compared to existing energy storage and transfer technologies, as well as those described in Heidari.
[0072] A proton flow reactor typically includes an electrochemical cell. In the electrochemical cell, Nafion TMA PEM, such as a PEM containing layers, separates two half-cells. The first half-cell is configured to allow a slurry consisting of storage particles suspended in an electrolyte to flow through it. The second half-cell, on the other hand, is configured to allow either water (in the charging mode) or an oxygen-containing gas (in the discharge mode) to flow through it. In certain embodiments, the operation of the proton flow reactor may be reversible. This allows the same proton flow reactor to operate in both the charging and discharge modes. The operation of an exemplary proton flow reactor is described below.
[0073] The slurry, consisting of storage particles passing through the first half-cell, effectively acts as a “slurry electrode.” Compared to a porous fixed electrode, the slurry electrode allows the storage particles to function as a hydrogen storage medium, which can gradually become charged as the slurry flows slowly through the hydrogen-side half-cell of the electrochemical cell. Thus, the charged storage particles (charged storage particles) emerging from this half-cell into the slurry can be separated from the liquid electrolyte and stored in bulk as dry particles in a separate container from the proton flow reactor. These dry, charged storage particles are therefore an energy-rich fuel, which can be transported away from its charged location as an export product on a bulk ocean tanker. By separating the device used to charge the particles (i.e., the electrochemical cell) from the bulk storage of the charged storage particles, a very high gravimetric and volumetric energy density can be achieved overall in the storage system. Charging mode
[0074] Figure 2 shows an electrochemical cell 2A operating as a proton flow reactor in a charged mode according to an embodiment of the present invention. As shown, a slurry 18 consisting of uncharged storage particles 10 flows slowly through the first half cell 4 (hydrogen-side half cell). Here, the uncharged storage particles 10 are given negative polarity by an end plate or other suitable means, such as a mesh or foam, that protrude into the slurry 18 to provide electrical contact. Simultaneously, water 14 is supplied to the second half cell 6 (oxygen-side half cell). When electricity is passed through the water 14, it combines with oxygen 16 and H + or H3O + Separates into ion 42. H + or H3O + Ions 42 pass through the PEM 8 and enter the first half-cell 4, where they primarily bind to the inner surface of the negatively polarized storage particles 10, thereby forming charged storage particles 12. Thus, hydrogen is effectively stored in the charged storage particles 12 for later use.
[0075] In the illustrated embodiment, as the uncharged storage particles 10 flow continuously through the first half-cell 4 (i.e., in a continuous flow process), they are gradually given polarity and H + or H3O + It binds to ion 42. In another embodiment, a repeatable batch process may be carried out in which a slurry 18 consisting of uncharged storage particles 10 is first introduced into the first half cell 4. The storage particles are then given negative polarity while remaining held in the first half cell 4, and H + or H3O + Ions 42 are attracted and stored. Subsequently, the slurry 20 consisting of charged storage particles 12 is removed from the first half cell 4.
[0076] The slurry may pass through a series of electrochemical cells 2 to ensure that the storage particles are sufficiently charged with hydrogen. Each electrochemical cell 2 may be similarly configured or configured to optimize a particular stage of charging the storage particles. A recycling loop system may also be implemented, in which the slurry and some of the storage electrons that have left the electrochemical cell are returned to the electrochemical cell for further processing. Discharge mode
[0077] Figure 3 shows an electrochemical cell 2B operating in discharge mode according to an embodiment of the present invention. A slurry 20 consisting of charged storage particles 12 flows slowly through the first half cell 4. Simultaneously, air or other oxygen-containing gas 16 is supplied to the second half cell 6. H + or H3O + Ion 42 passes through PEM8 and reacts with oxygen 16 in the second half cell 6, generating water and electricity. The reaction between hydrogen and oxygen in the second half cell 6 dehydrogenates the charged carbon cell in the first half cell 2, and H + or H3O + The ions 42PEM8 flow through the particles. In this way, the hydrogen stored on the surface of the charged storage particles 12 can be used to participate in a redox reaction between oxygen and hydrogen that results in the production of water.
[0078] Similar to the charging modes described above, the electrochemical cell 2B may operate in a continuous flow system or as a batch system, depending on the operating requirements. Also, similar to the charging modes, the system according to the embodiment of the present invention may comprise a series of electrochemical cells 2 in which stored particles are gradually discharged. And again, depending on the specific operating requirements, a recycling loop system may be implemented separately or additionally.
[0079] According to the embodiment, as illustrated in Figure 4, the discharge performance can be improved by moderately heating the proton flow reactor cell (for example, to below 100°C). While we do not wish to be bound by theory, moderate heating is thought to improve discharge performance. This is because (a) drying the catalyst layer on the oxygen side improves the access of oxygen gas to the catalyst layer, thereby significantly increasing the rate of water production; (b) the increased temperature increases the reaction rate of all electrochemical reactions; and (c) locally increasing the electrolyte concentration allows Nafion to be produced from carbon particles. TM This is due to a decrease in the overpotential of ion transfer to the membrane and to the catalyst layer on the oxygen side.
[0080] According to the embodiment, oxygen access to the catalyst can be improved by removing the gas diffusion layer from the oxygen side, or by replacing the gas diffusion layer with a very thin layer, in combination with heating. While we do not wish to be bound by theory, it is thought that hydrogen extraction from a charged sample, and consequently its effective reversible storage capacity (in wt%H), can potentially be increased by more than three times by a combination of moderate heating and removal of the gas diffusion layer or the use of a very thin one.
[0081] According to one embodiment, heat can be supplied by incorporating an electric heating cartridge into the end plate of the proton flow reactor cell, or by installing a similar heating system.
[0082] In embodiments, the proton flow reactor according to the present invention may include a current collector comprising carbon foam. Figure 5 shows schematic diagrams of a conventional slurry electrode (a) and a slurry electrode incorporating a carbon foam current collector (b). While we do not wish to be bound by theory, it is believed that incorporating a carbon foam current collector can significantly improve the performance of the proton flow reactor by minimizing flow resistance to the slurry flow, increasing the surface area of the current collector, and facilitating charge transfer to carbon particles in the slurry. The slurry can flow through a 3D connected porosity network of carbon foam. As a result, the carbon particles are surrounded by carbon walls containing excess charge. This configuration maximizes charge transfer by maximizing the collision velocity between the particles and the walls.
[0083] Carbon foam possesses relatively high electronic conductivity, a large internal surface area, and sufficient mechanical strength to withstand compression from the end plates of the proton flow reactor cells. Furthermore, the 3D pore network of carbon foam can promote a uniform distribution of the liquid electrolyte within the current collector. While carbon foam has lower conductivity and hardness compared to stainless steel metal foam, it is a far less effective catalyst for hydrogen evolution reactions. Therefore, according to certain embodiments, undesirable hydrogen gas generation is suppressed.
[0084] The use of carbon foam current collectors may help overcome one of the main drawbacks of slurry electrodes: relatively low electronic conductivity (lower than the ionic conductivity of the electrolyte) due to the discontinuous electron transport network formed by carbon particles. This low electronic conductivity also leads to underutilization of particles and the lack of available charge for capacity storage (Mourshed et al., 2021).
[0085] As an alternative discharge mode according to embodiments of the present invention, access of oxygen to the catalyst layer on the oxygen side (cathode) of the proton flow reactor may be blocked. Blocking is achieved, for example, by pouring water into the proton flow reactor, filling it with another gas such as argon or nitrogen, or by applying a vacuum. In this embodiment, the discharge reaction transitions from water generation to the chemiadsorption of hydronium ions onto the available metal on the oxygen side. In this mode, the discharge rate is slightly reduced. If a small positive potential (e.g., less than 0.5V) is applied to the oxygen side, the cell is gently heated, and / or the cell is stopped for a certain period of time, the hydrogen (gas) generation reaction will begin, and hydrogen bubbles will appear on the oxygen side.
[0086] In this embodiment, the charged powder can be discharged simultaneously with the generation of hydrogen gas formed from electricity and stored hydrogen atoms. Therefore, the proton flow reactor system can be used to produce high-purity hydrogen gas from charged carbon powder and can be used as a primary source of hydrogen gas in a refueling system for transport vehicles using hydrogen fuel cells.
[0087] Furthermore, the electricity generated during this alternative discharge mode may have beneficial applications. This may include providing a small potential necessary to increase the hydrogen gas generation rate after short-term storage in another capacitor. Experiments conducted by the inventors suggest that the energy required to improve hydrogen generation is significantly less than the energy generated during the cell's discharge. Therefore, a favorable and beneficial energy balance can be achieved while producing high-purity hydrogen gas. Storage particles
[0088] Storage particles are part of an energy storage strategy. + or H3O +There is a need to provide a practical capacity for storing ions. Ideally, the storage particles should offer high reversible electrochemical hydrogen storage capacity per unit mass and unit volume, hydrogen retention after drying, and the ability to maintain high round-trip efficiency for hydrogen storage after multiple charge-discharge cycles.
[0089] While we do not wish to be bound by theory, these characteristics are thought to be attainable through the following desirable particle properties: high electrical conductivity (in the form of electronic conduction); the presence of surface functional groups that can facilitate opportunities for bonding with hydrogen, especially oxygen and nitrogen; a large volume and surface area of ultrafine pores or layered domains with appropriate interlayer distances that tend to provide a site for bonding with hydrogen; and mesopores that provide channels for hydronium ion transport within the storage particles.
[0090] If the particles constitute carbon particles, it is even more desirable that a significant region of graphite carbon exists on the inner surface of the pores. As mentioned above, the term carbon particles is understood to mean particles primarily formed from electrically conductive carbon-based materials. Examples of electrically conductive carbon-based materials include activated carbon, graphene, graphene oxide, nitrogen-functionalized or nitrogen-doped graphene, graphite carbonitrides, graphene aerogels, and carbon nanotubes. Other carbon-based materials, in particular those that provide the properties listed above, may also be utilized.
[0091] Carbon particles do not necessarily have to be formed from, for example, pure carbon, but H may be present on the surface of the particles. + or H3O +It must provide a practical ability to bind or attach ions. Numerous raw materials, including biomass materials, charcoal, or lignite, can be used to provide raw materials for the production of carbon particles. The electrochemical hydrogen storage capacity of activated carbon and other forms of carbon, such as multilayer graphene, can be enhanced by the presence of oxygen and nitrogen-containing functional groups on the internal pore surfaces. Oxygen-based surface functional groups that can promote hydrogen storage include acidic groups such as carboxylic acids, lactones, phenols, and lactol groups, and basic groups such as quinones, pyrones, ketones, and epoxides (Montes-Moran et al., 2004; Shafeeyan et al., 2010). Nitrogen-based surface functional groups such as amides, imides, pyrroles, lactams, and pyridine groups can also enhance hydrogen storage (Pels et al., 1995; Lahaye, 1998). While we do not wish to be bound by theory, these surface functional groups are thought to store hydrogen via reversible Faraday reactions, in addition to bilayer capacitance.
[0092] In alternative embodiments, the storage particles may be formed from a material other than carbon, such as silicon. Silicon may similarly provide the particularly desirable properties listed above: namely, high electrical conductivity (in the form of electronic conduction); the presence of surface functional groups that can facilitate opportunities for bonding with hydrogen, especially oxygen and nitrogen; a large volume and surface area of ultrafine pores or layered domains with appropriate interlayer distances that tend to provide sites for bonding with hydrogen; and mesopores that provide channels for hydronium ion transport within the storage particles.
[0093] According to certain embodiments of the present invention, the storage particles may have one or more of the following characteristics: high reversible electrochemical hydrogen storage capacity per unit mass and unit volume, hydrogen retention after drying, and maintenance of high reciprocal efficiency for hydrogen storage after multiple charge-discharge cycles.
[0094] As mentioned above, H + or H3O +Previous studies have demonstrated that ions can be electrochemically neutralized and hydrogen can be stored in porous activated electrochemical cells (Jurewicz et al., 2001; Jurewicz et al., 2002; Vix-Guterl et al., 2005; Fang et al., 2006; Bleda-Martinez et al., 2008; Jurewicz and Babel, 2008; Yang et al., 2010). For these porous activated carbon electrodes, promising gravimetric energy densities of up to 2.2 wt% of hydrogen have been reported (Jurewicz, 2009), which is superior to the best metal hydrides currently available (~1.6 wt%).
[0095] According to certain embodiments, carbon particles may be provided as particles made of activated carbon. Such particles may be formed from a variety of raw materials, including phenolic resin and lignite. In embodiments, carbon particles may include activated carbon composed of phenolic resin activated in a 1:7 potassium hydroxide ratio. Such a manufacturing method allows for a high BET surface area and a wide range of pore sizes down to less than 0.7 nm.
[0096] In addition to activated carbon, other suitable materials for providing carbon particles include graphene hydrogels with adjustable interlayer spacing (Cheng and Li, 2013); other graphene-based materials such as graphene oxide derivatives terminated with hydroxyl and epoxyhydroxyl groups (Gupta et al., 2017); activated carbon modified by electroactive anthraquinones (Pognon et al., 2011a) (Pognon et al., 2011b), or quinones (Isikli et al., 2014); or by oxidation with 5% O2 in Ar (Figueiredo et al., 1999), HNO3 (Nevskaia and Martin-Aranda, 2003), or H2O2 / steam (Heo and Park, 2018); and laminated monolayer carbon nitride materials (Tan et al., 2015).
[0097] Regarding graphene, the maximum weight density achievable by chemisorption is 8.3% (=1 / 12), significantly higher than the 5.7 wt% achieved in Toyota's 700-bar advanced composite compressed hydrogen gas storage cylinders (Toyota, 2016) (Toyota, 2017). This corresponds to the formation of a fully saturated graphene sheet, or "Graphane." The stability of the latter was hypothesized in theoretical studies based on DFT (Sofo et al., 2007) and subsequently studied experimentally (Elias et al., 2009).
[0098] Synthetic graphite-like carbonitrides are considered particularly promising as proton storage electrodes in proton batteries and, consequently, as slurries in proton flow reactors. For example, g-C3N4 is a semiconductor, and g-C4N3 is the most stable allotrope at room temperature and pressure, exhibiting semimetallic properties (Du et al., 2012). Both of these two-dimensional structures have regular pores on their surfaces, and in multilayer materials, hydrogen transport occurs not only between layers but also through these pores, thus increasing the rates of charging and discharging. Furthermore, the nitrogen atoms in the structure have a pair of orbitals with high electron density, which can attract particularly positively charged hydronium ions and form NH bonds. In recent years (Tan et al., 2015), density functional theory simulations have demonstrated that charging of g-C4N3 and g-C3N4 nanosheets provides a promising technology for high-capacity and electrically switchable hydrogen storage.
[0099] According to certain embodiments, the carbon particles may be smaller in size. This provides a high surface area-to-volume ratio while ensuring ease of handling when in a slurry. According to certain embodiments, the storage particles may have a diameter of approximately 0.5 to 1 micron. This ensures that Brownian motion maintains a suspended state in the slurry. However, in other embodiments, larger or smaller storage particles may be used. Other suitable particle sizes include 0.1 to 5 microns, but the present invention is not broadly considered to be limited to any particular particle size as long as a transferable slurry can be formed. Methods such as grinding (e.g., ball milling) may be used to reduce the size of the storage particles.
[0100] According to certain embodiments, the storage particles may offer high porosity. This provides a high surface area-to-volume ratio for hydrogen to bind or adhere. Suitable porosity levels can selectively range from 20% to 40%. electrolyte
[0101] A suitable electrolyte to be used in the slurry according to the embodiments of the present invention is generally H + or H3O + It may contain any electrolyte capable of conducting ions. Suitable electrolytes include dilute sulfuric acid (e.g., 1 M to 4 M); protic ionic liquids containing pure diethylmethylammonium triflate (DEMATf); 10 mol% DMATf in water; triflic acid (H0Tf): H20 mol% DEMATf; dilute nitric acid; organic acids such as acetic acid, or formic acid; and redox-activated electrolytes (Roldan et al., 2011b, Roldan et al., 2011a) (Roldan et al., 2011c).
[0102] When selecting an appropriate electrolyte, conflicting considerations may arise, for example, H + or H3O +The proposed electrolyte's ability to conduct ions may be balanced with the potential for the electrolyte to cause or promote adverse reactions with respect to the storage particles. Ideally, the selected electrolyte should offer high proton conductivity, low electronic conductivity, a suitable size for ion-carrying protons to transfer to porous storage particles, low reactivity with storage particles, and low reactivity with components of an electrochemical cell (e.g., Nation PEM). Slurry mixing
[0103] In certain embodiments, a slurry consisting of an electrolyte and pre-mixed uncharged storage particles (or charged storage particles) may be supplied to the first half-cell. Similarly, in certain embodiments, the storage particles (or charged storage particles) may be removed from the first half-cell as a slurry together with the electrolyte. In alternative embodiments, the slurry may be supplied to the first half-cell by supplying the electrolyte and storage particles separately, and the slurry may be removed from the half-cell by removing the electrolyte and particles separately.
[0104] A suitable slurry can be formed simply by mixing storage particles or (optionally) charged storage particles with an electrolyte. Standard methods of mixing can be carried out as understood in the art. In certain embodiments, the storage particles may constitute 5–35% (w / w) in a conventional slurry (on a particle weight / liquid weight basis), or selectively 5–15% (w / w). 15–35% may be used for a thicker, paste-like slurry.
[0105] The viscosity of the slurry used in slurry electrodes can vary from a relatively viscous liquid to a highly viscous paste. Viscous liquids have the advantage of flowing easily through the hydrogen-side half-cell of an electrochemical cell, requiring less parasitic pump power and energy. However, they have the disadvantages of low electrical conductivity, ohmic resistive energy loss, and slow, sometimes incomplete, hydrogen filling of storage particles. Pastes have the advantages of high electrical conductivity, low resistive energy loss, and fast, complete particle filling, but they require high pump power and the associated parasitic energy consumption, and the paste does not adhere well to the gaps in the electrode structure. Slurry separation
[0106] According to certain embodiments, the storage particles can be separated from the electrolyte after being removed from the electrochemical cell. For example, this makes it possible to transport and store the storage particles. Similarly, the electrolyte can be stored for reuse, such as creating a new slurry containing the storage particles at a later date.
[0107] The appropriate separation technique may depend on the properties of the slurry and storage particles. A relevant consideration is the ability of the separation technique used to separate the electrolyte without adversely affecting the degree of hydrogen bonding / adhesion to the surface of the charged storage particles. This may include blowing an inert gas through the storage particles, filtration, sedimentation (with coagulation or condensation where appropriate), hydrocyclone, etc. The size of the storage particles may also influence the selection of the separation technique. If the storage particles are, for example, less than 3 microns, certain existing techniques, such as hydrocyclone separation, may not be very suitable.
[0108] In embodiments, the separation technique may include blowing / evaporating the liquid from the slurry and storage particles by exposure to an inert gas under pressure. The storage particles may be heated under a controlled environment to facilitate the evaporation process.
[0109] In embodiments, the separation technique may include filtration using a moving membrane dead-end filter 24, as illustrated in Figure 6. In use, charged storage particles 12 may accumulate on the moving membrane 24 while the liquid electrolyte 22 passes through the moving membrane 24. The charged storage particles 12 can then be removed from the membrane 24 by physical means, such as a knife 26, or by vibration. Alternatively, the charged storage particles 12 can be stored on the membrane 24 for an extended period. In this case, the charged storage particles 12 can be removed from the membrane 24 by forming a slurry through which the electrolyte 22 is flowed in the reverse direction. The same or a corresponding apparatus can similarly be used to remove uncharged storage particles from the slurry.
[0110] According to certain embodiments, after separation from the slurry by filtration or other methods, the separated storage particles can be further dried. This can be achieved by blowing an inert gas through the storage particles.
[0111] In an alternative embodiment where the charged storage particles are stored locally after manufacturing and not transported to another location, the charged storage particles may be stored together with the electrolyte in the output slurry until needed for power generation. Such a configuration is suitable, for example, for domestic storage of energy generated using solar cells. Thus, energy generated during the day can be stored for use at night. Storage and distribution of storage particles
[0112] According to certain embodiments, the stored particles may be transported and stored in a large container until needed for use, for example, in power generation.
[0113] Existing technologies can be utilized for the storage of storage particles. For example, a suitable storage device for carbon particles should preferably consider the storage of very large quantities of potentially micron-sized fine solid carbon-based powders, the relatively low density of the storage particles, the ability of the charged storage particles to "self-discharge" in flammable, oxidizing atmospheres (to address this problem, charged storage particles may be stored in an inert nitrogen atmosphere), and the ability to withstand any physical shock or extreme atmospheric temperatures without releasing particles into the atmosphere.
[0114] Considering the potential applications of the present invention, new designs may be developed for cost-effectively storing vast quantities of materials, namely tons of flammable materials. Such new designs can be derived from experience in handling powdered materials in bulk, such as cement, fertilizer, or bulk grains. Energy production and storage systems
[0115] According to certain embodiments, the methods and apparatus of the present invention can be used as part of a broader energy generation and storage system, such as the renewable energy storage and generation system shown in Figure 7.
[0116] In Figure 7, uncharged storage particles are obtained from one of several potential sources, including renewable or non-renewable inorganic or organic sources 28. The uncharged storage particles are then stored in the uncharged storage particle storage unit 30. Prior to charging, the uncharged storage particles are mixed with an electrolyte in a mixer 32A before being supplied to an electrochemical cell (i.e., a "proton flow reactor") 2A configured in a charged mode. The electrochemical cell 2A is powered by a renewable energy source 26 to supply electricity to water, oxygen, and H₂ + or H3O + Electrolysis is performed with ions to generate charged storage particles. The slurry containing the charged storage particles is sent to the separator 34A, where the electrolyte is separated and recycled to the electrolyte storage unit 36A. The dried charged storage particles are then sent to the charged storage particle storage unit 43 for subsequent use.
[0117] Figure 7 illustrates an alternative use of charged storage particles, where they are used for power generation both domestically and internationally. In domestic use, the charged storage particles are sent to mixer 32B, where they are mixed with an electrolyte from electrolyte storage unit 36B. The slurry consisting of the charged storage particles is then sent to proton flow reactor 2B, where hydrogen reacts with oxygen to produce water and electricity for electricity user 38A. As a result of this process, the charged storage particles deplete their hydrogen and become uncharged storage particles. These are separated from the slurry in separator 34B and returned to uncharged storage particle storage unit 30. Such a system can provide a means of storing surplus electricity from inherently intermittent or variable renewable resources (e.g., solar and wind resources) in major, regional, or community-scale power grids, and thus can help achieve national greenhouse gas reduction targets.
[0118] In international use, the process is similar in that charged storage particles are sent to mixer 32C and mixed with electrolyte from electrolyte storage unit 36C. The slurry consisting of charged storage particles is then sent through electrochemical cell (i.e., "proton flow reactor") 2C, where hydrogen reacts with oxygen to produce water and electricity for the electricity user 38B. Uncharged storage particles are separated from the slurry in separator 34C and returned to uncharged storage particle storage unit 30. The main difference is that charged storage particles can be sent overseas via sea freight 40A and returned as uncharged storage particles via sea freight 40B. Such a system can provide a zero-emission power source to countries with insufficient domestic renewable energy sources by importing charged carbon materials from other countries with surplus renewable energy capacity. Such a form of exchange contributes to reducing greenhouse gas emissions and addressing global climate change.
[0119] By applying this technology to a wider range of energy generation and storage systems, the increased flexibility that can be provided by certain embodiments of the present invention will be demonstrated. That is, H + or H3O +The use of storage particles to which ions bind or adhere enables flexible storage and transfer of chemical energy, because the storage particles can be removed from the proton flow reactor and transferred and stored as a bulk product. Fixed porous electrode technology, such as that disclosed in Heidari, cannot be easily removed from the proton battery without disassembling the electrochemical cell. Thus, Heidari's proton battery effectively functions as a rechargeable battery containing an internally stored fuel source, instead of a fuel cell that utilizes an external fuel source / energy storage unit.
[0120] According to one embodiment, another application of hydride particles is shown in Figure 7 (element 41A domestically, 41B internationally). Here, hydrogen gas can be directly extracted from a proton flow reactor system while generating electricity during the emission of carbon particles. The hydrogen gas can be used in fuel cell vehicles, electric passenger cars, trucks, ships, aircraft, or forklifts. Thus, according to this application mode, it is possible to export hydrogen in the form of hydride particles produced from abundant renewable energy in one country, and to use a proton flow reactor system in the importing country to generate electricity while directly generating hydrogen gas for transport.
[0121] Hydrogen storage using storage particles is considered to have advantages over existing hydrogen storage methods. For example, if hydrogen is to be stored as a compressed gas or cryogenic liquid, these methods require a large amount of energy to bring the hydrogen into storage condition. Compared to existing technologies, storing hydrogen in particles is considered to potentially offer advantages such as superior and practical gravimetric and volumetric energy densities obtainable under near-ambient temperature and pressure conditions, improved safety due to storing hydrogen as a solid non-explosive, a lower or at least similar ratio of total energy input per unit of electrical energy delivered and supplied, and the possibility of relying on relatively abundant materials (e.g., carbon particles) as a hydrogen storage mechanism.
[0122] According to the present invention and the concept of the proton flow reactor, the concept of a proton battery can be extended to large-scale hydrogen storage required for electrical energy storage for primary power grids with intermittent solar and wind energy inputs. Furthermore, the present invention is thought to enable the production of hydrogen-based fuels suitable for export in large quantities from zero-emission renewable energy sources. experiment
[0123] The inventors of this study conducted experimental work to confirm the technical feasibility of storing hydrogen in porous carbon particles by applying an electrochemical process. In this experiment, a paste of carbon particles in a liquid acidic electrolyte was supplied to an electrochemical cell having the same configuration as that shown in Figure 1. That is, a particulate paste electrode was used instead of the fixed porous electrode in the proton reactor in Figure 1. The particulate paste is a limited example of a particulate slurry with a near-maximum particle density. The experiment was conducted in batch mode, and the paste was held stationary in the first half-cell while the carbon particles were charged.
[0124] Regarding the other aspects, the experiment was conducted as follows. The paste electrode was prepared by mixing 24 mg of carbon powder (activated carbon from phenolic resin activated with 1:7 KOH) and sulfuric acid (1 M) as an electrolyte in a mass ratio of approximately 1:4. This paste was placed on the carbon felt of the first half-cell, and the entire electrochemical cell was assembled. The electrochemical cell was charged at a potential of 1.8 V for 30 minutes. The charging conditions were maintained for longer than necessary to ensure that the paste was completely charged with hydrogen. Figure 8 shows the relationship between charging current and time when charged at a potential of 1.8 V for 30 minutes. Immediately afterward, discharges were continuously performed at low currents of 5mA, 2mA, 1mA, and 0.5mA. There was a 5-minute pause between each step. From the total amount of charge that flowed, the maximum amount of hydrogen stored in the paste under minimum self-discharge conditions was calculated.
[0125] Figure 9 shows the potential change during discharge in a four-stage current discharge with a 5-minute pause between each discharge step. From Figure 9, it was calculated that a charge of 14.97C flowed during the discharge. This was equivalent to 0.65 wt% hydrogen stored in the electrode. This level of charge was lower than expected and was later found to be due to iron contamination. Nevertheless, it demonstrated that energy can be stored in a carbon powder paste. In another experiment using a similar sample of 11 mg in mass, 23.62C was discharged by employing the same charging and discharge process except that the cell was heated during discharge. This was equivalent to 2.23 wt% hydrogen storage.
[0126] The procedure described in paragraphs 0123, 0124, and 0125, which does not involve heating during discharge, was then repeated in a second cycle. The second cycle included an additional step of drying the paste electrode and re-wetting it with the electrolyte to demonstrate that charged carbon particles could be retained after drying. The drying and re-wetting steps of the paste electrolyte involved removing the liquid acid electrolyte from the electrode by blowing argon gas on it for 30 minutes, leaving the dried charged carbon particles in place as a powder in an argon environment for 16 hours, and re-adding the liquid acid to reconstitute the paste electrode.
[0127] In the second cycle, as shown in Figure 10, the cell was recharged at a potential of 1.8V for 30 minutes.
[0128] After the liquid acid extraction and drying procedure described in the above method, the liquid acid was reconnected to the hydrogen side, and discharged while gradually decreasing the current, as shown in Figure 11, in the same manner as in the first cycle.
[0129] From Figure 11, it was calculated that a charge of 8.85C flowed during the second cycle discharge, which was equivalent to the storage of 0.38 wt% of hydrogen within the electrode. This result demonstrates that more than half of the hydrogen stored in the electrode immediately after charging remained stored even after the drying and re-wetting processes.
[0130] At the end of the experiment, the following procedure was used to observe the possible state of the paste electrode after the acid extraction process. Specifically, the hydrogen side of the cell was disconnected from the acid source, and the internal electrode was dried by blowing argon gas on it for 30 minutes. The cell was then disassembled, and the dried electrode was observed directly.
[0131] After drying, the paste electrode returned to a powder state. Since the first and second drying processes were identical, it can be inferred that the state of the electrode at the time of cell disintegration and the state of the electrode at the start of the second discharge were identical.
[0132] Those skilled in the art to which the invention relates will find many structural modifications and a wide range of different embodiments and applications of the invention proposed without departing from the scope of the invention as defined in the appended claims. The disclosures and descriptions herein are purely illustrative and are not intended to be limiting in any sense. Where any particular integer having known equivalents in the art to which the invention relates is referred herein, such known equivalents are deemed to be incorporated herein as individually described.
[0133] The inventors developed a small-scale embodiment of a proton flow reactor as shown in Figure 12 (top - schematic cross-sectional view; bottom - 3D view showing the paste channel on the hydrogen side of the cell). This reactor was filled with a paste consisting of 25 wt% carbon particles and 75 wt% 1 M sulfuric acid, and operated in a charged mode at a potential of 1.85 V to store hydrogen in the pores of the carbon particles. Next, the charged carbon paste was moved to another location within the reactor, ensuring that the paste did not come into contact with the charged electrodes or end plates. The charged paste was held in this location for 1 hour. Then, the charged paste was returned to the charged location in contact with the electrodes and end plates, and discharged by applying continuous currents of 5 mA (0.36 A / g), 2 mA (0.14 A / g), 1 mA (0.072 A / g), and 0.5 mA (0.036 A / g). The total discharge amount was calculated, and the hydrogen storage weight percentage was determined. Using this demonstration setup, it was shown that the proton flow reactor successfully stored 75% of the charged hydrogen over a specified period.
[0134] The inventors also developed a microfluidic proton flow reactor as shown in Figure 13 according to embodiments of the present invention and measured its performance in charging and discharging modes. A carbon slurry electrode was prepared by adding 0.25 g of activated carbon from phenolic resin to 1.00 g of 1 M sulfuric acid solution. This slurry was injected into a microfluidic device using a syringe. Simultaneously, distilled water was injected into the PDMS channel toward the oxygen side, and 2.0 V was applied to partially charge the slurry electrode. In this experiment, the slurry was kept stationary during charging. It was found that the slurry could be discharged with a current of at least 0.5 mA. The same microfluidic proton flow reactor can be used similarly for discharging and discharging flowing slurries.
[0135] The inventors were able to obtain evidence of the C...H bond required for C-particles in a proton flow reactor system by performing cyclic voltammetry on activated carbon samples from phenolic resin in a 1M H2SO4 electrolyte within a potential range of -0.4 to 0.9V relative to a standard hydrogen electrode.
[0136] The cyclic voltammetry curve for the second cycle is shown in Figure 14. The non-rectangular shape of the curve with peaks indicates the presence of chemical reactions on the pure electric double-layer capacitance. Strong cathode and anode peaks at potentials of -0.2V and 0.25V indicate electrochemical reactions involving C…H bonds. Furthermore, evidence of weak cathode and anode reactions at potentials of 0.4V and 0.6V is thought to be due to electrochemical reactions of hydrogen and oxygen (such as quinone and hydroquinone pairs) and nitrogen surface functionalities (Kun Yang et al., 2013).
[0137] 2-Electrochemical cell 2A - Electrochemical cell in charging mode Electrochemical cells in 2B and 2C discharge modes 4-1st Half Cell 6 - Second Half Cell 8-PEM 10-Uncharged Storage Particles 12-Charged Storage Particles 14-Water flow 16- Oxidizing agent flow 18-Slurry consisting of uncharged storage particles 20-Particles consisting of charged storage particles 22-Electrolytes 24-Filter film 26. Renewable energy sources 28. Uncharged Storage Particle Source 30 - Non-charged storage particle storage section 32A, 32B, 32C - Slurry Mixer 34A, 34B, 34C - Slurry Separator 36A, 36B, 36C - Electrolyte storage section 38A, 38B - Electrical Users 40A, 40B-transfer vessel 41A, 41B - Hydrogen gas storage section 42-H + or H3O + ion 43. Storage cylinder for slurry consisting of charged storage particles reference
[0138] The entirety of the disclosures in the following documents is incorporated herein. BABEL, K. & JUREWICZ, K. 2008. KOH-activated lignin-based nanostructured carbon exhibiting high hydrogen electrolytic adsorption. Carbon, 46, 1948-1956. BLEDA-MARTINEZ, MJ, PEREZ, J., LINARES-SOLANO, A., MORALLON, E. & CAZORLA-AMOROS, D. 2008. Effects of surface chemistry on the electrochemical storage of hydrogen in porous carbon materials. Carbon, 46, 1053-1059. Cheng, C. & Li, D. 2013. Solvated graphene: A new class of functional flexible materials. Adv Mater, 25, 13-30. DU, A., SANVITO, S. & SMITH, SC2012. First-principles calculations predicting metal-free magnetism and intrinsic half-metalness in graphitic carbonitrides. Physical Review Letters, 108. ELIAS, DC, NAIR, RR, MOHIUDDIN, TMG, MOROZOV, SV, BLAKE, P., HALSALL, MP, FERRARI, AC, BOUCHVALOV, DW, KATSNELSON, MI, GEIM, AK & NOVOSELOV, KS2009. Control of graphene properties by reversible hydrogenation reaction. Evidence for Graphane. Science, 323, 610-613. FANG, B., ZHOU, H. & HONMA, I. 2006. Ordered porous carbon with controlled pore size for electrochemical hydrogen storage applications. The Journal of Physical Chemistry B, 110, 4875-4880. FIGUEIREDO, JL, PEREIRA, MFR, FREITAS, MMA & ORFAO, JJM 1999. Modification of surface chemistry of activated carbon. Carbon, 37, 1379-1389. GUPTA, B., KUMAR, N., PANDA, K., KANAN, V., JOSHI, S. & VISOLY-FISHER, I. 2017. The role of oxygen functional groups in reduced graphene oxide for lubrication. Scientific Reports, 7, 45030. HEIDARI, S., SEIF MOHAMMADI, S., OBEROI, AS & ANDREWS, J. 2018. Technical feasibility of a proton battery using activated carbon electrodes. International Journal of Hydrogen Energy, 43, 6197-6209. HEO, Y.-J. & PARK, S.-J. 2018. Porousing of carbonaceous materials by H2O2 / steam activation as an environmentally friendly and efficient top-down approach: the inevitable effect of oxygen functional groups in CO2 capture. Green Chemistry, 20, 5224-5234. ISIKLI, S., LECEA, M., RIBAGORDA, M., CARRENO, MC & DIAZ, R. 2014. Effects of quinone grafts mediated by the Riedel-Craft reaction on carbon porous structure and supercapacitor performance. Carbon, 66, 654-661. JUREWICZ, K. 2009. Effects of charging parameters on the effectiveness of electrochemical hydrogen storage in activated carbon. International Journal of Hydrogen Energy, 34, 9431-9435. JUREWICZ, K. & BABEL, K. 2008. KOH-activated lignin-based nanostructured carbon exhibiting high hydrogen electrolytic adsorption. Carbon, 46, 1948-1956. JUREWICZ, K., FRACKOWIAK, E. & BEGUIN, F. 2001. Reversible improvement of hydrogen capacity in activated carbon by water electrolysis. Electrochemical and Solid-State Letters, 4, A27-A29. JUREWICZ, K., FRACKOWIAK, E. & BEGUIN, F. 2002. Electrochemical storage of hydrogen in activated carbon. Fuel Processing Technology, 77, 415-421. KUN YANG, A, LIANGBO PENG A, DONG SHU A, B, D, CUIJUAN LV A, CHUN HE C, LU LONG A, 2013. Capacitive characteristics of heteroatom-enriched activated carbon in concentrated sulfuric acid. Journal of Power Sources, 239, 553-560. LAHAYE, J. 1998. Chemical properties of carbon surfaces. Fuel, 77, 543-547. MONTES-MORAN, MA, SUAREZ, D., MENENDEZ, J. & FUENTE, E. 2004. On the properties of basic sites on carbon surfaces: Overview. Carbon, 42, 1219-1225. MOURSHED M., REZAEI NIYA SM, OJHA R., ROSENGARTEN G., ANDREWS J. AND SHABANI B., 2021. Carbon-based slurry electrodes for energy storage and power systems, energy storage materials, publication permission granted. NEVSKAIA, DM & MARTIN-ARANDA, RM2003. Nitrate-carbon oxide for ester preparation under ultrasonic activity. Catalysis Letters, 87, 143-147. PELS, JR, KAPTEIJN, F., MOULIJN, JA, ZHU, Q. & THOMAS, KM 1995. Evolution of nitrogen functional groups during thermal decomposition in carbonaceous materials. Carbon, 33, 1641-1653. POGNON, G., BROUSSE, T. & BELANGER, D. 2011a. Effect of molecular graft polymerization on pore size distribution and double-layer capacitance of activated carbon for electrochemical double-layer capacitors. Carbon, 49, 1340-1348. POGNON, G., BROUSSE, T., DEMARCONNAY, L. & BELANGER, D. 2011b. Performance and stability of electrochemical capacitors based on anthraquinone-modified activated carbon. Journal of Power Sources, 196, 4117-4122. ROLDAN, S., BLANCO, C., GRANDA, M., MENENDEZ, R. & SANTAMARIA, RJACIE 2011a. Towards further generational advancements in high-energy carbon-based capacitors using redox-activated electrolytes. 50, 1699-1701. ROLDAN, S., GONZALEZ, Z., BLANCO, C., GRANDA, M., MENENDEZ, R. & SANTAMARIA, RJEA2011b. Redox active electrolyte for electric double-layer capacitors using carbon nanotubes. 56, 3401-3405. ROLDAN, S., GRANDA, M., MENENDEZ, R., SANTAMARIA, R. & BLANCO, C. 2011c. Mechanism of energy storage in carbon-based supercapacitors modified with quinoid-type redox-activated electrolytes. J. Phys. Chem. C, 115, 17606-17611. SHAFEEYAN, M.S., DAUD, WMAW, HOUSHMAND, A. & SHAMIRI, A. 2010. A review on surface modification of activated carbon for carbon dioxide adsorption. Journal of Analytical and Applied Py Rolysis, 89, 143-151. SOFO, JO, CHAUDHARI, AS & BARBER, GD2007. Graphan: Two-dimensional hydrocarbons. Physical Review B, 75, 153401. TAN, X., KOU, L, TAHINI, HA & SMITH, SC2015. Charge modulation in graphitic carbon nitride as a switchable approach to high-capacity hydrogen storage. ChemSusChem, 8, 3626-31. TOYOTA.2016. Fuel cell vehicle technology file [Online] Available: http: / / www.toyota- giobai.com / innovation / environmentai technology / technology file / fuel cell hybrid. htmi#h306[Accessed]. TOYOTA,2017,2017 Mirai Product Information, accessed from https: / / www.toyota.com / mirai / assets / core / Docs / Mirai%20Specs.pdf VIX-GUTERL, C., FRACKOWIAK, E., JUREWICZ, K., FRIEBE, M., PARMENTIER, J. & BEGUIN, F. 2005. Electrochemical energy storage in ordered porous carbon materials. Carbon, 43, 1293-1302. YANG, C., LI, Y., and CHEN, W., 2010. Electrochemical hydrogen storage behavior of single-walled carbon nanotubes (Swcnts) coated with Ni nanoparticles.
Claims
1. A method of storing electrical energy as chemical energy, The steps include supplying an input slurry containing uncharged storage particles and an electrolyte to the first half cell of an electrochemical cell, The steps include supplying a source of H+ or H3O+ ions to the second half-cell of the electrochemical cell, The steps include applying a voltage to the electrochemical cell to move H+ or H3O+ ions from the second half cell to the first half cell, thereby converting the uncharged storage particles into charged storage particles, The steps include removing the output slurry containing charged storage particles and an electrolyte from the first half cell, Equipped with, The charged storage particles and the uncharged storage particles include carbon particles. Storage particles refer to particles suitable for storing hydrogen on their surface or inside. The charged storage particles mean storage particles on which a chemically significant amount of hydrogen atoms or ions are bound or attached via an electrochemical process, The non-charged storage particles mean the storage particles that are not the charged storage particles. The carbon particles in this method refer to particles mainly formed from a conductive carbon-based material.
2. The uncharged storage particles are (A) Electrical conductivity, (B) Average diameter of 0.5 to 5 microns, (C) Porosity in the range of 20% to 50%, (D) Substantially "ultrafine pores" having a diameter of 0.5 to 2 nanometers (nm), or substantial layered domains having an interlayer spacing of 0.5 to 2 nm. (E) Mesopores having a diameter or width of 2 to 50 nm, (F) Electrochemical hydrogen storage capacity of 0.5 to 8 wt%, Having one or more of the following characteristics The method according to claim 1.
3. The non-charged storage particles have each of the characteristics (A) to (F) listed in claim 2, The method according to claim 2.
4. The carbon particles are selected from particles mainly formed from one or more materials selected from activated carbon, graphene, oxygen-functionalized graphene, nitrogen-functionalized graphene or nitrogen-doped graphene, graphitic carbon nitride, graphene aerogel, or carbon nanotubes. The method according to any one of claims 1 to 3.
5. The carbon particles include particles derived from phenolic resin and activated with potassium hydroxide. The method according to any one of claims 1 to 4.
6. The input slurry contains 5–35% (w / w), selectively 5–15% (w / w), or 15–35% (w / w) of uncharged storage particles. The method according to any one of claims 1 to 5.
7. The source of H+ or H3O+ ions supplied to the second half-cell is water. The method according to any one of claims 1 to 6.
8. The steps include mixing uncharged storage particles and an electrolyte outside the first half cell to form the input slurry, The steps include supplying the mixed input slurry to the first half cell, The method according to any one of claims 1 to 7, comprising:
9. After the step of removing the output slurry from the first half cell, the step of separating the charged storage particles from the electrolyte in the output slurry, The method according to any one of claims 1 to 8, further comprising:
10. The step of separating the charged storage particles from the electrolyte comprises the step of selectively filtering the charged storage particles from the electrolyte using a mobile filtering membrane. The method according to claim 9.
11. The step of separating the charged storage particles from the electrolyte comprises the step of drying the charged storage particles. The method according to claim 9 or 10.
12. The step of drying the charged storage particles comprises the step of applying an inert gas to the charged storage particles. The method according to claim 11.
13. After the step of separating the charged storage particles from the electrolyte, the charged storage particles are stored. The method according to any one of claims 9 to 12.
14. In the step of storing the charged storage particles, the charged storage particles are stored in an inert atmosphere. The method according to claim 13.
15. A method for generating electricity, The steps include supplying an input slurry containing charged storage particles and an electrolyte to the first half-cell of an electrochemical cell, The steps include supplying an oxidizing agent stream to the second half-cell of the electrochemical cell, A step of generating electricity by moving H+ or H3O+ ions from the first half cell and reacting them with the oxidizing agent in the second half cell, The steps include removing the output slurry containing uncharged storage particles and an electrolyte from the first half cell, Equipped with, The charged storage particles and the uncharged storage particles include carbon particles. Storage particles refer to particles suitable for storing hydrogen on their surface or inside. The charged storage particles mean storage particles on which a chemically significant amount of hydrogen atoms or ions are bound or attached via an electrochemical process, The non-charged storage particles mean the storage particles that are not the charged storage particles. The carbon particles in this method refer to particles mainly formed from a conductive carbon-based material.
16. The charged storage particles are (A) Electrical conductivity, (B) Average diameter of 0.5 to 5 microns, (C) Porosity in the range of 20% to 50%, (D) Substantially "ultrafine pores" having a diameter of 0.5 to 2 nanometers (nm), or substantial layered domains having an interlayer spacing of 0.5 to 2 nm. (E) Mesopores having a diameter or width of 2 to 50 nm, (F) Electrochemical hydrogen storage capacity of 0.5 to 8 wt%, Having one or more of the following characteristics The method according to claim 15.
17. The charged storage particles have all of the characteristics (A) to (F) listed in claim 16. The method according to claim 16.
18. The carbon particles are selected from particles mainly formed from one or more materials selected from activated carbon, graphene, oxygen-functionalized graphene, nitrogen-functionalized graphene or nitrogen-doped graphene, graphitic carbon nitride, graphene aerogel, or carbon nanotubes. The method according to any one of claims 15 to 17.
19. The carbon particles include particles derived from phenolic resin and activated with potassium hydroxide. The method according to any one of claims 15 to 18.
20. The input slurry contains 5 to 35 (w / w), selectively 5 to 15% (w / w) or 15 to 35% (w / w) of uncharged storage particles. The method according to any one of claims 15 to 19.
21. The charged storage particles are manufactured and processed according to any one of claims 1 to 14. The method according to any one of claims 15 to 20.
22. The oxidizing agent stream supplied to the second half cell contains oxygen gas. The method according to any one of claims 15 to 21.
23. The oxidizing agent stream supplied to the second half-cell is air. The method according to claim 22.
24. The process includes a step of heating the cell while generating electricity. The method according to any one of claims 15 to 23.
25. The steps include mixing the charged storage particles and the electrolyte outside the first half cell to form the input slurry, The steps include supplying the mixed input slurry to the first half cell, The method according to any one of claims 15 to 24, comprising:
26. The step of removing the output slurry from the first half cell, followed by the step of separating the uncharged storage particles from the electrolyte, The method according to any one of claims 15 to 25, further comprising:
27. The step of separating the uncharged storage particles from the electrolyte comprises the step of drying the uncharged storage particles. The method according to claim 26.
28. The process includes a step of separating the uncharged storage particles from the electrolyte, followed by a step of storing the uncharged storage particles. The method according to claim 27.
29. The electrochemical cell comprises a proton exchange membrane separating the first half-cell and the second half-cell, and the proton exchange membrane comprises a layer selectively formed substantially from a tetrafluoroethylene-based fluoropolymer copolymer. The method according to any one of claims 1 to 28.
30. The step of supplying the input slurry to the electrochemical cell and the step of removing the output slurry from the electrochemical cell are performed as a continuous process. The method according to any one of claims 1 to 29.
31. The steps of supplying the input slurry to the electrochemical cell and removing the output slurry from the electrochemical cell are carried out as a batch process. The method according to any one of claims 1 to 29.
32. The electrolyte is selected from mineral acids in aqueous solutions, ionic liquids, ionic liquids in aqueous solutions, organic acids in aqueous solutions, or a combination thereof. The method according to any one of claims 1 to 31.
33. The process includes the step of generating the output slurry by processing the input slurry through a plurality of electrochemical cells arranged in series. The method according to any one of claims 1 to 32.
34. A step of generating an output slurry by processing the input slurry through a plurality of electrochemical cells arranged in parallel, comprising the step of selectively arranging the plurality of electrochemical cells in a stack, The method according to any one of claims 1 to 32.
35. The charged storage particles contain, on average, at least 0.5 wt% of captured hydrogen, and selectively 1.0 to 7.5 wt% of captured hydrogen. The method according to any one of claims 1 to 34.
36. A method for producing charged storage particles, comprising the step of producing the charged storage particles according to the method described in any one of claims 1 to 14 or any one of claims 29 to 35 when referring to any one of claims 1 to 14.
37. A method for producing a slurry, comprising the step of producing charged storage particles according to the method for producing charged storage particles described in claim 36 and combining them with an electrolyte.
38. A method for producing charged storage particles according to claim 36, further comprising the step of storing the charged storage particles in an inert atmosphere.
39. A method for producing uncharged storage particles, comprising the step of processing the uncharged storage particles according to the method described in any one of claims 15 to 32.
40. A method for producing a slurry, comprising the step of producing the uncharged storage particles by the method of claim 39 and combining them with an electrolyte.
41. A method for generating hydrogen gas, The steps include supplying an input slurry containing charged storage particles and an electrolyte to the first half-cell of an electrochemical cell, The steps include moving H+ or H3O+ ions from the first half-cell while ensuring that substantially no oxidizing agent is present, or only a minimal amount of oxidizing agent is present, in the second half-cell, The steps include: starting the generation of hydrogen gas in the second half cell, The steps include: extracting the output flow containing hydrogen gas from the second half cell; Equipped with, The charged storage particles include carbon particles, Storage particles refer to particles suitable for storing hydrogen on their surface or inside. The charged storage particles mean storage particles on which a chemically significant amount of hydrogen atoms or ions are bound or attached via an electrochemical process, The carbon particles in this method refer to particles mainly formed from a conductive carbon-based material.
42. The step of initiating the generation of hydrogen gas comprises one or more of the following steps: applying a low potential to the electrochemical cell; applying gentle heat to the electrochemical cell; or keeping the cell stopped for at least one hour from the supply of the input slurry to the first half cell. The method according to claim 41.
43. The step of ensuring that substantially no oxidizing agent is present, or only a minimal amount of oxidizing agent is present, The step of pouring water into the second half cell, A step of filling the second half cell with a non-oxidizing gas such as argon or nitrogen, The step of applying a vacuum to the second half cell, It can be equipped with, The method according to claim 41 or 42.
44. The above method includes a step of generating electricity while generating hydrogen gas. The method according to any one of claims 41 to 43.
Citation Information
Patent Citations
JP1971008746B1
JP1973025127A
Fuel cell
JP2006004893A
High energy density redox flow meter
JP2011524074A
Fluidized system and large-capacity power storage and water treatment method using the same