Nitride semiconductor devices
The nitride semiconductor device addresses the trade-off between on-resistance and off-state characteristics by strategically positioning the p-type layer to manage the electric field and channel resistance, resulting in improved performance.
Patent Information
- Application Number
- JP2023061829
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-04-06
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2043-04-06
AI Technical Summary
Conventional nitride semiconductor devices face a trade-off between reducing on-resistance and maintaining off-state characteristics due to the extension of the depletion layer affecting the two-dimensional electron gas channel.
The nitride semiconductor device is designed with a specific angle configuration of the p-type nitride semiconductor layer relative to the substrate, allowing the p-type layer to be positioned away from the channel in the upper portion while being closer to the gate electrode in the lower portion, thereby mitigating the electric field during the off-state and reducing on-resistance.
This configuration achieves both favorable off-state characteristics and reduced on-resistance by optimizing the position of the p-type layer, enhancing breakdown voltage and channel resistance management.
Smart Images

Figure 0007955215000001 
Figure 0007955215000002 
Figure 0007955215000003
Abstract
Description
[Technical Field]
[0001] This disclosure relates to nitride semiconductor devices. [Background technology]
[0002] Nitride semiconductors, exemplified by GaN, are wide-bandgap semiconductors with large band gaps of 3.4 eV and 6.2 eV at room temperature, respectively, for GaN and AlN. Nitride semiconductors have the advantage of a high dielectric breakdown field and a higher electron saturation drift rate compared to compound semiconductors such as GaAs or Si semiconductors. For these reasons, research and development of power transistors using nitride semiconductors, which are advantageous for increasing power output and breakdown voltage, is currently being actively pursued.
[0003] Furthermore, in the AlGaN / GaN heterostructure, spontaneous polarization and piezoelectric polarization occur on the (0001) plane, generating a high concentration of two-dimensional electron gas (2DEG) at the heterointerface, resulting in a concentration of 1 × 10⁻¹⁰ even when undoped. 13 cm -2 The above sheet carrier concentrations can be obtained.
[0004] Patent Document 1 discloses a vertical nitride semiconductor device. In the nitride semiconductor device disclosed in Patent Document 1, a GaN electron transport layer and an AlGaN electron supply layer are formed in that order within an opening that penetrates the p-type underlayer and reaches the drift layer. Transistor operation is achieved by opening and closing a two-dimensional electron gas channel generated at the AlGaN / GaN heterointerface formed on the side wall of the opening using a gate voltage. [Prior art documents] [Patent Documents]
[0005] [Patent Document 1] Patent No. 6511645 [Overview of the Initiative] [Problems that the invention aims to solve]
[0006] In conventional nitride semiconductor devices, when the transistor is turned on, a depletion layer extends from the p-type underlayer into the electron transport layer. This narrows the two-dimensional electron gas channel within the electron transport layer, resulting in a problem where the on-resistance cannot be sufficiently reduced. On the other hand, if the p-type underlayer is moved away from the channel to a degree that avoids the influence of the extended depletion layer, the electric field during the off state cannot be sufficiently relaxed, and the off-voltage decreases. Thus, in conventional nitride semiconductor devices, there is a trade-off between reducing on-resistance and maintaining off-state characteristics.
[0007] This disclosure provides a nitride semiconductor device that can achieve both good off-characteristics and reduced on-resistance. [Means for solving the problem]
[0008] A nitride semiconductor device according to one aspect of the present disclosure includes a substrate, a first nitride semiconductor layer provided above the substrate, a first p-type nitride semiconductor layer provided above the first nitride semiconductor layer, a second nitride semiconductor layer provided above the first p-type nitride semiconductor layer, a first opening that penetrates the second nitride semiconductor layer and the first p-type nitride semiconductor layer and reaches the first nitride semiconductor layer, an electron transport layer and an electron supply layer provided in order from below so as to cover the upper surface of the second nitride semiconductor layer and the first opening, and the electron supply layer so as to cover the first opening. The first opening comprises a gate electrode provided above the first opening, a source electrode provided away from the gate electrode, and a drain electrode formed below the substrate, wherein, when the position between the lower and upper ends of the first p-type nitride semiconductor layer in the side wall portion of the first opening is defined as a predetermined position, in a cross section parallel to the direction in which the gate electrode and the source electrode are aligned and perpendicular to the main surface of the substrate, the first angle made with the main surface by the first line segment connecting the lower end and the predetermined position is greater than the second angle made with the main surface by the second line segment connecting the lower end and the upper end.
[0009] A nitride semiconductor device according to another aspect of the present disclosure includes a substrate, a first nitride semiconductor layer provided above the substrate, a first p-type nitride semiconductor layer provided above the first nitride semiconductor layer, a second nitride semiconductor layer provided above the first p-type nitride semiconductor layer, a first opening that penetrates through the second nitride semiconductor layer and the first p-type nitride semiconductor layer and reaches the first nitride semiconductor layer, an electron transit layer and an electron supply layer that are provided in order from below so as to cover an upper surface of the second nitride semiconductor layer and the first opening, a gate electrode provided above the electron supply layer so as to cover the first opening, a second opening that penetrates through the electron supply layer, the electron transit layer, and the second nitride semiconductor layer at a position separated from the gate electrode and reaches the first p-type nitride semiconductor layer, a source electrode that is provided so as to cover the second opening and is electrically connected to the first p-type nitride semiconductor layer, and a drain electrode formed below the substrate, wherein a side wall portion of the first opening has at least one step between an upper end and a lower end of the first p-type nitride semiconductor layer.
Advantageous Effects of Invention
[0010] According to the nitride semiconductor device of the present disclosure, it is possible to achieve both favorable off characteristics and a reduction in on-resistance.
Brief Description of Drawings
[0011] [Figure 1A] FIG. 1A is a cross-sectional view of a nitride semiconductor device according to Embodiment 1. [Figure 1B] FIG. 1B is a partially enlarged cross-sectional view of FIG. 1A. [Figure 2A] FIG. 2A is a cross-sectional view for explaining channel narrowing in a nitride semiconductor device according to a comparative example. [Figure 2B] FIG. 2B is a cross-sectional view for explaining an effect of the nitride semiconductor device according to Embodiment 1. [Figure 3A] FIG. 3A is a cross-sectional view of a nitride semiconductor device according to a modification of Embodiment 1. [Figure 3B] Figure 3B is a partially enlarged cross-sectional view of Figure 3A. [Figure 4] Figure 4 is a cross-sectional view of a nitride semiconductor device according to Embodiment 2. [Figure 5] Figure 5 is a cross-sectional view of a nitride semiconductor device according to a modified example of Embodiment 2. [Figure 6] Figure 6 is a cross-sectional view of a nitride semiconductor device according to Embodiment 3. [Figure 7A] Figure 7A is a cross-sectional view of a nitride semiconductor device according to Embodiment 4. [Figure 7B] Figure 7B is a partially enlarged cross-sectional view of Figure 7A. [Figure 8] Figure 8 is a cross-sectional view of a nitride semiconductor device according to Embodiment 5. [Figure 9A] Figure 9A is a cross-sectional view of a nitride semiconductor device according to Embodiment 6. [Figure 9B] Figure 9B is a partially enlarged cross-sectional view of Figure 9A. [Modes for carrying out the invention]
[0012] (Summary of this disclosure) To solve the above problems, nitride semiconductor devices according to multiple embodiments of this disclosure have the following configurations.
[0013] A nitride semiconductor device according to a first aspect of the present disclosure includes a substrate, a first nitride semiconductor layer provided above the substrate, a first p-type nitride semiconductor layer provided above the first nitride semiconductor layer, a second nitride semiconductor layer provided above the first p-type nitride semiconductor layer, a first opening that penetrates the second nitride semiconductor layer and the first p-type nitride semiconductor layer and reaches the first nitride semiconductor layer, an electron transport layer and an electron supply layer provided in order from below so as to cover the upper surface of the second nitride semiconductor layer and the first opening, and the electron supply layer so as to cover the first opening. The first opening comprises a gate electrode provided above the layer, a source electrode provided away from the gate electrode, and a drain electrode formed below the substrate, wherein, when the position between the lower and upper ends of the first p-type nitride semiconductor layer on the side wall of the first opening is defined as a predetermined position, in a cross section parallel to the direction in which the gate electrode and the source electrode are aligned and perpendicular to the main surface of the substrate, the first angle made with the main surface by the first line segment connecting the lower end and the predetermined position is greater than the second angle made with the main surface by the second line segment connecting the lower end and the upper end.
[0014] As a result, in the upper portion away from the bottom surface of the first opening, the first p-type nitride semiconductor layer can be moved away from the channel of the two-dimensional electron gas, thereby suppressing an increase in channel resistance. In the lower portion near the bottom surface of the first opening, by bringing the first p-type nitride semiconductor layer closer to the gate electrode side, the electric field during the off state can be mitigated, improving the breakdown voltage. Thus, the nitride semiconductor device according to this embodiment can achieve both good off-state characteristics and reduced on-state resistance.
[0015] A nitride semiconductor device according to a second aspect of the present disclosure, in the nitride semiconductor device according to the first aspect, the side wall portion includes a first side wall surface which is the section from the lower end to the first end located at the predetermined position; a second side wall surface which is the section from the second end located between the first end and the upper end in a plan view to the upper end; and a third side wall surface located between the first end and the second end and having a different inclination from both the first side wall surface and the second side wall surface.
[0016] This allows the second sidewall surface, located above the first p-type nitride semiconductor layer, to be moved even further away from the channel, thereby reducing the on-resistance.
[0017] In a nitride semiconductor device according to a third aspect of the present disclosure, the third sidewall surface is parallel to the main surface, in the nitride semiconductor device according to the second aspect.
[0018] As a result, the third sidewall can be, for example, the bottom surface of an opening formed by etching. Therefore, the first opening can be formed easily and accurately by a two-stage etching process. For example, it becomes easier to form the first opening according to the design specifications, thereby improving the reliability and yield of nitride semiconductor devices.
[0019] In a nitride semiconductor device according to a fourth aspect of the present disclosure, in a nitride semiconductor device according to a second or third aspect, the first inclination angle, which is the angle that the first sidewall surface makes with respect to the main surface, is different from the second inclination angle, which is the angle that the second sidewall surface makes with respect to the main surface.
[0020] This allows for a larger inclination angle on either the first or second sidewall, thereby shortening the unit cell length of the nitride semiconductor device. A shorter unit cell length allows for more cells to be placed within the same area, further reducing on-resistance. Note that a cell refers to the smallest unit configuration that performs transistor operation.
[0021] In the nitride semiconductor device according to the fifth aspect of this disclosure, in the nitride semiconductor device according to the fourth aspect, the first tilt angle is smaller than the second tilt angle.
[0022] This makes channel constriction less likely to occur in the upper portion of the channel within the first opening. As a result, the unit cell length can be shortened while achieving both good off-resistance and reduced on-resistance.
[0023] In the nitride semiconductor device according to the sixth aspect of this disclosure, the second tilt angle is 70° or more and 90° or less in the nitride semiconductor device according to the fifth aspect.
[0024] As a result, the effect of shortening the unit cell length becomes greater when the inclination angle of the second side wall surface, which is located above the first side wall surface, is between 70° and 90°. Therefore, on-resistance can be further reduced while maintaining good off-characteristics.
[0025] In a nitride semiconductor device according to a seventh aspect of the present disclosure, in a nitride semiconductor device according to any one of the second to sixth aspects, the first p-type nitride semiconductor layer includes an AlGaN layer, and the third sidewall surface is a part of the upper surface of the AlGaN layer.
[0026] This allows for the use of dry etching conditions that stop etching at the AlGaN layer, thereby stabilizing the shape and depth of the step. This makes it easier to form the first opening according to the design specifications, improving the reliability and yield of nitride semiconductor devices.
[0027] In the nitride semiconductor device according to the eighth aspect of the present disclosure, in the nitride semiconductor device according to any one of the first to seventh aspects, the first nitride semiconductor layer consists of two or more layers with different impurity concentrations, and among the two or more layers, the uppermost layer has the lowest impurity concentration.
[0028] This promotes electric field relaxation during the off state, resulting in better off-state characteristics.
[0029] A nitride semiconductor device according to the ninth aspect of the present disclosure is a nitride semiconductor device according to any one of the first to eighth aspects, comprising a second p-type nitride semiconductor layer provided between the gate electrode and the electron supply layer.
[0030] This allows the potential at the conduction band edge of the channel to be raised, thereby increasing the threshold voltage. Therefore, for example, a normally-off field-effect transistor (FET) can be realized. Furthermore, the second p-type nitride semiconductor layer and the first p-type nitride semiconductor layer optimize the electric field relaxation during the off state, resulting in improved off-state characteristics.
[0031] A nitride semiconductor device according to a tenth aspect of the present disclosure is a nitride semiconductor device according to any one of the first to ninth aspects, comprising a second opening located away from the gate electrode, penetrating the electron supply layer, the electron transport layer and the second nitride semiconductor layer, and reaching the first p-type nitride semiconductor layer, wherein the source electrode is provided within the second opening and electrically connected to the first p-type nitride semiconductor layer.
[0032] This allows the two-dimensional electron gas exposed on the side wall of the second opening to come into contact with the source electrode, thereby reducing the on-resistance. Furthermore, since the first p-type nitride semiconductor layer can be strongly fixed to the source potential, the electric field relaxation effect during the off state can be enhanced, resulting in improved off-state characteristics.
[0033] In the nitride semiconductor device according to the eleventh aspect of this disclosure, in the nitride semiconductor device according to any one of the second to tenth aspects, the third sidewall surface is the section from the first end to the second end.
[0034] This allows for reduced on-resistance by suppressing the increase in channel resistance while maintaining good off-resistance characteristics. Furthermore, by using only one step, the formation of the first aperture can be easily facilitated. This eliminates the need for high-precision mask alignment and makes it easier to form the first aperture according to the design specifications, thereby improving the reliability and yield of nitride semiconductor devices.
[0035] In a nitride semiconductor device according to a twelfth aspect of the present disclosure, in a nitride semiconductor device according to any one of the second to tenth aspects, the side wall portion includes a plurality of third side wall surfaces, and further includes one or more fourth side wall surfaces that connect two adjacent third side wall surfaces and have a different inclination from any of the plurality of third side wall surfaces.
[0036] This makes it possible to reduce on-resistance by suppressing the increase in channel resistance while maintaining good off-resistance characteristics.
[0037] In a nitride semiconductor device according to a thirteenth aspect of the present disclosure, in a nitride semiconductor device according to a first aspect, the side wall portion includes a first side wall surface which is the section from the lower end to the first end located at the predetermined position, and a second side wall surface which is the section from the first end to the upper end.
[0038] This makes it possible to achieve both good off-resistance and reduced on-resistance.
[0039] A nitride semiconductor device according to a 14th aspect of this disclosure includes a substrate, a first nitride semiconductor layer provided above the substrate, a first p-type nitride semiconductor layer provided above the first nitride semiconductor layer, a second nitride semiconductor layer provided above the first p-type nitride semiconductor layer, a first opening that penetrates the second nitride semiconductor layer and the first p-type nitride semiconductor layer and reaches the first nitride semiconductor layer, and an electron transport layer and an electron supply layer provided in order from below so as to cover the upper surface of the second nitride semiconductor layer and the first opening, and The device comprises a gate electrode provided above the electron supply layer so as to cover the first opening, a second opening located away from the gate electrode, penetrating the electron supply layer, the electron transport layer, and the second nitride semiconductor layer, and reaching the first p-type nitride semiconductor layer, a source electrode provided so as to cover the second opening and electrically connected to the first p-type nitride semiconductor layer, and a drain electrode formed below the substrate, wherein the side wall portion of the first opening has at least one step between the upper and lower ends of the first p-type nitride semiconductor layer.
[0040] As a result, a step is provided on the end face of the first p-type nitride semiconductor layer on the first opening side. This allows the first p-type nitride semiconductor layer to be moved away from the two-dimensional electron gas channel in the upper portion away from the bottom surface of the first opening, thereby suppressing an increase in channel resistance. Furthermore, in the lower portion near the bottom surface of the first opening, the first p-type nitride semiconductor layer is brought closer to the gate electrode side, which mitigates the electric field when the device is off and improves the breakdown voltage. Thus, the nitride semiconductor device according to this embodiment can achieve both good off-characteristics and reduced on-resistance.
[0041] The embodiments of this disclosure will be described below with reference to the drawings.
[0042] The embodiments described below are all comprehensive or specific examples. The numerical values, shapes, materials, components, arrangement and connection configurations of components, steps, and the order of steps shown in the following embodiments are examples only and are not intended to limit this disclosure. Furthermore, any components in the following embodiments that are not described in an independent claim will be described as optional components.
[0043] Furthermore, each figure is a schematic diagram and not necessarily a strictly accurate representation. Therefore, for example, the scale may not necessarily match in each figure. Also, in each figure, substantially identical components are given the same reference numerals, and redundant explanations are omitted or simplified.
[0044] Furthermore, in this specification, terms indicating relationships between elements such as parallel or orthogonal, terms indicating shapes of elements such as rectangles or trapezoids, and numerical ranges do not represent only strict meanings, but also include substantially equivalent ranges, such as differences of a few percent.
[0045] In this specification and in the drawings, the x, y, and z axes represent the three axes of a three-dimensional Cartesian coordinate system. The x and y axes are parallel to the first side and the second side perpendicular to the first side of the rectangle, respectively, when the plan view shape of the substrate is rectangular. The z axis is the thickness direction of the substrate. In this specification, the "thickness direction" of the substrate refers to the direction perpendicular to the main surface of the substrate. The thickness direction is the same as the stacking direction of the semiconductor layer and is also referred to as the "vertical direction". In addition, the direction parallel to the main surface of the substrate may be referred to as the "horizontal direction".
[0046] Furthermore, the side of the substrate on which the gate electrode and source electrode are provided (the positive side of the z-axis) is considered "up" or "upper," and the side of the substrate on which the drain electrode is provided (the negative side of the z-axis) is considered "down" or "lower."
[0047] In this specification, the terms “above” and “below” do not refer to upward direction (vertically upward) and downward direction (vertically downward) in absolute spatial recognition, but are used as terms defined by a relative positional relationship based on the stacking order in a stacked structure. The terms “above” and “below” are applied not only when two components are spaced apart from each other and another component is present between the two components, but also when two components are placed in close contact with each other and the two components are in contact with each other.
[0048] Further, in this specification, unless otherwise specified, “plan view” refers to a view from a direction perpendicular to a main surface of a substrate of a nitride semiconductor device, that is, a view of the main surface of the substrate from the front.
[0049] Further, in this specification, unless otherwise specified, ordinal numbers such as “first” and “second” do not mean the number or order of components, but are used for the purpose of avoiding confusion and distinguishing between components of the same type.
[0050] Further, in this specification, AlGaN means a ternary mixed crystal Al x Ga 1-x N (0<x<1). Hereinafter, multi-component mixed crystals are abbreviated by arrangement of respective constituent element symbols, for example, AlInN, GaInN, or the like. For example, Al x Ga 1-x-y In y N (0<x<1, 0<y<1, and 0<x+y<1), which is an example of a nitride semiconductor, is abbreviated as AlGaInN.
[0051] (Embodiment 1) [Configuration] First, a configuration of a nitride semiconductor device according to Embodiment 1 will be described with reference to FIGS. 1A and 1B.
[0052] Figure 1A is a cross-sectional view of the nitride semiconductor device 1 according to this embodiment. Figure 1B is a partially enlarged cross-sectional view of Figure 1A. Specifically, Figure 1B shows the vicinity of the side wall portion 40b of the gate opening 40 in Figure 1A. Note that, in order to ensure clarity, the electron transport layer 22 is not shaded with diagonal lines to represent its cross-section in each cross-sectional view.
[0053] As shown in Figure 1A, the nitride semiconductor device 1 of this embodiment is a so-called vertical field-effect transistor (FET). Specifically, in the nitride semiconductor device 1, current flows between the drain electrode 36 and the source electrode 32 in a direction perpendicular to the main surface 10a of the substrate 10.
[0054] Nitride semiconductor device 1 is a device having a stacked semiconductor layer structure mainly composed of nitride semiconductors such as GaN and AlGaN. Note that "A mainly composed of B" means that the content of B in A is 50% or more.
[0055] The nitride semiconductor device 1 according to this embodiment is a normally-off type FET. In the nitride semiconductor device 1, for example, the source electrode 32 is grounded (i.e., the potential is 0V), and a positive potential is applied to the drain electrode 36. The potential applied to the drain electrode 36 is, for example, 100V to 1200V, but is not limited to this. When the nitride semiconductor device 1 is in the off state, 0V or a negative potential (e.g., -5V) is applied to the gate electrode 34. When the nitride semiconductor device 1 is in the on state, a positive potential (e.g., +5V) is applied to the gate electrode 34. Note that the nitride semiconductor device 1 may also be a normally-on type FET.
[0056] As shown in FIG. 1A, the nitride semiconductor device 1 includes a substrate 10, a drift layer 12, a first base layer 14, a second base layer 16, an electron transit layer 22, an electron supply layer 24, a threshold adjustment layer 28, a source opening 30, a source electrode 32, a gate electrode 34, a drain electrode 36, and a gate opening 40. A two-dimensional electron gas (2DEG) 26 that functions as a channel is generated at an interface between the electron transit layer 22 and the electron supply layer 24.
[0057] Hereinafter, details of each component included in the nitride semiconductor device 1 will be described.
[0058] The substrate 10 is a substrate made of a nitride semiconductor, and has main surfaces 10a and 10b facing each other as shown in FIG. 1A. The main surface 10a is a main surface (upper surface) on the side where the drift layer 12 is formed. Specifically, the main surface 10a substantially coincides with the c-plane. The main surface 10b is a main surface (lower surface) on the side where the drain electrode 36 is formed. The planar view shape of the substrate 10 is, for example, a rectangle, but is not limited thereto.
[0059] The substrate 10 is, for example, a substrate made of n 18 -type GaN having a thickness of 300 μm and a carrier concentration of 1×10 -3 cm + . Note that n-type and p-type indicate conductivity types of the semiconductor. The n + -type represents a state in which an n-type dopant is added to a semiconductor at a high concentration, so-called heavy doping. Further, the n - -type represents a state in which an n-type dopant is added to a semiconductor at a low concentration, so-called light doping. The same applies to p + -type and p - -type. The n-type, n + -type and n - -type are an example of a first conductivity type. The p-type, p + -type and p - -type are an example of a second conductivity type. The second conductivity type is a conductivity type having a polarity opposite to that of the first conductivity type. In the present specification, the n + -type and the n - -type may be described as n-type without being distinguished from each other. Similarly, p+ type and p - Sometimes, the term "p-type" is used without distinguishing between different types.
[0060] Note that the substrate 10 does not have to be a nitride semiconductor substrate. For example, the substrate 10 may be a silicon (Si) substrate, a silicon carbide (SiC) substrate, or a zinc oxide (ZnO) substrate.
[0061] The drift layer 12 is an example of a first nitride semiconductor layer provided above the substrate 10. The drift layer 12 is, for example, n with a thickness of 8 μm. - The film is made of GaN of type 1. The donor concentration of the drift layer 12 is 1 × 10⁻¹⁶. 15 cm -3 The above 1 x 10 17 cm -3 The following is an example: 1 × 10 16 cm -3 Furthermore, the carbon concentration (C concentration) of the drift layer 12 is 1 × 10⁻⁶. 15 cm -3 The above 2 x 10 17 cm -3 The following applies:
[0062] The drift layer 12 is provided, for example, in contact with the main surface 10a of the substrate 10. The drift layer 12 is formed on the main surface 10a of the substrate 10 by crystal growth such as metal-organic vapor phase epitaxy (MOVPE) or hydride vapor phase epitaxy (HVPE).
[0063] The first sublayer 14 is an example of a first p-type nitride semiconductor layer provided above the drift layer 12. The first sublayer 14 is also called a p-type block layer. The first sublayer 14 has, for example, a thickness of 400 nm and a carrier concentration of 1 × 10⁻¹⁶ 17 cm -3The film is made of p-type GaN. The first underlayer 14 is provided in contact with the upper surface of the drift layer 12. The first underlayer 14 is formed on the drift layer 12 by crystal growth such as the MOVPE method or the HVPE method.
[0064] The first underlayer 14 is formed by crystal growth, but it may also be formed, for example, by injecting magnesium (Mg) into a deposited undoped GaN (i-GaN) film. Undoping will be explained later.
[0065] The first underlayer 14 suppresses leakage current between the source electrode 32 and the drain electrode 36. For example, when a reverse voltage is applied to the pn junction formed by the first underlayer 14 and the drift layer 12, specifically when the drain electrode 36 becomes higher in potential than the source electrode 32, a depletion layer extends in the drift layer 12. This enables the nitride semiconductor device 1 to have a high breakdown voltage. In this embodiment, the drain electrode 36 is at a higher potential than the source electrode 32 in both the off and on states, except in the case of reverse conduction. Therefore, the nitride semiconductor device 1 has a high breakdown voltage.
[0066] In this embodiment, as shown in Figure 1A, the first sublayer 14 is in contact with the source electrode 32. Therefore, the first sublayer 14 is fixed at the same potential as the source electrode 32.
[0067] The second underlayer 16 is an example of a second nitride semiconductor layer provided above the first underlayer 14. The second underlayer 16 is a high-resistance layer with higher resistance than the first underlayer 14. The second underlayer 16 is, for example, a film made of undoped GaN (i-GaN) with a thickness of 200 nm. The second underlayer 16 is provided in contact with the first underlayer 14. The second underlayer 16 is formed on the first underlayer 14 by crystal growth such as the MOVPE method or the HVPE method.
[0068] Furthermore, the second underlayer 16 is assumed to be an undoped semiconductor layer, but it may also be an insulating layer or a semi-insulating layer. Here, "undoped" means that it is not doped with dopants such as Si or Mg that change the polarity of GaN to n-type or p-type. In this embodiment, the second underlayer 16 is doped with carbon (C). Specifically, the carbon concentration of the second underlayer 16 is higher than the carbon concentration of the first underlayer 14.
[0069] For example, the carbon concentration of the second subsoil layer 16 is 3 × 10 17 cm -3 That's all, but 1 × 10 18 cm -3 The above is also acceptable. In this case, the concentrations of silicon (Si) or oxygen (O), which are n-type impurities, are lower than the carbon concentration. For example, the silicon concentration or oxygen concentration of the second sublayer 16 is 5 × 10⁻⁶. 16 cm -3 The following is 2 × 10 16 cm -3 The following is also acceptable.
[0070] The second sublayer 16 may be formed by ion implantation of ions other than carbon, such as magnesium (Mg), iron (Fe), or boron (B). Other ionic species may be used as long as they can increase the resistance of GaN.
[0071] Here, if the nitride semiconductor device 1 does not have a second underlayer 16, a parasitic NPN structure, i.e., a parasitic bipolar transistor, will exist between the source electrode 32 and the drain electrode 36, consisting of an electron transport layer 22, a p-type first underlayer 14, and an n-type drift layer 12. Therefore, when the nitride semiconductor device 1 is in the off state, if current flows through the p-type first underlayer 14, the parasitic bipolar transistor will turn on, potentially reducing the breakdown voltage of the nitride semiconductor device 1. In this case, malfunction of the nitride semiconductor device 1 is likely to occur. In this embodiment, by providing a high-resistance second underlayer 16, the formation of a parasitic NPN structure can be suppressed, thereby preventing malfunction of the nitride semiconductor device 1.
[0072] The second sublayer 16 may be located below the first sublayer 14 and between it and the drift layer 12. Alternatively, the second sublayer 16 may be located either above or below the first sublayer 14.
[0073] Furthermore, a layer may be provided on the upper surface of the second underlayer 16 to suppress the diffusion of p-type impurities such as Mg from the first underlayer 14. For example, an AlGaN layer with a thickness of 20 nm may be provided on the second underlayer 16.
[0074] The gate opening 40 is an example of a first opening that penetrates the second sublayer 16 and the first sublayer 14 and reaches the drift layer 12. The gate opening 40 has a bottom portion 40a and a side wall portion 40b.
[0075] The bottom portion 40a is part of the surface of the drift layer 12. As shown in Figure 1A, the bottom portion 40a is located below the lower surface of the first substrate layer 14. The lower surface of the first substrate layer 14 corresponds to the interface between the first substrate layer 14 and the drift layer 12. The bottom portion 40a is, for example, parallel to the main surface 10a of the substrate 10.
[0076] The side wall portion 40b is part of the surface of the drift layer 12, the first sublayer 14, and the second sublayer 16. As shown in Figure 1A, the side wall portion 40b has a step. The specific shape of the side wall portion 40b will be explained later using Figure 1B.
[0077] The electron traveling layer 22 is an example of a first regrowth layer provided to cover the upper surface of the second substrate layer 16 and the gate opening 40. Specifically, a portion of the electron traveling layer 22 is provided along the bottom 40a and side wall 40b of the gate opening 40, while the other portion of the electron traveling layer 22 is provided on the upper surface of the second substrate layer 16. The electron traveling layer 22 is, for example, a film made of undoped GaN with a thickness of 150 nm. Although the electron traveling layer 22 is assumed to be undoped, it may be made n-type by Si doping or the like.
[0078] The electron traveling layer 22 is in contact with the drift layer 12 at the bottom 40a and side wall 40b of the gate opening 40. The electron traveling layer 22 is in contact with the first substrate layer 14 and the second substrate layer 16 at the side wall 40b of the gate opening 40. Furthermore, the electron traveling layer 22 is in contact with the upper surface of the second substrate layer 16. The electron traveling layer 22 is formed by crystal regrowth after the gate opening 40 has been formed.
[0079] The electron transport layer 22 has a channel region. Specifically, a two-dimensional electron gas 26, which acts as a channel, is generated near the interface between the electron transport layer 22 and the electron supply layer 24. The two-dimensional electron gas 26 functions as a channel in the electron transport layer 22. In Figure 1A, the two-dimensional electron gas 26 is schematically shown with a dashed line. The two-dimensional electron gas 26 is bent along the interface between the electron transport layer 22 and the electron supply layer 24, that is, along the inner surface of the gate opening 40.
[0080] Furthermore, although not shown in Figure 1A, an AlN layer with a thickness of approximately 1 nm is provided as a second regrowth layer between the electron transport layer 22 and the electron supply layer 24. This suppresses alloy scattering, improves channel mobility, and reduces on-resistance. Note that the regrowth-grown AlN layer is not necessarily required.
[0081] The electron supply layer 24 is an example of a third regrowth layer provided to cover the upper surface of the second substrate layer 16 and the gate opening 40. The electron transport layer 22 and the electron supply layer 24 are provided in this order from the substrate 10 side. The electron supply layer 24 is formed with a shape along the upper surface of the electron transport layer 22 and has a substantially uniform thickness. The electron supply layer 24 is, for example, a film made of undoped AlGaN with a thickness of 20 nm. The electron supply layer 24 is formed by crystal regrowth following the formation process of the electron transport layer 22.
[0082] The electron supply layer 24 has a larger band gap than the electron transport layer 22. Therefore, an AlGaN / GaN heterointerface is formed between the electron supply layer 24 and the electron transport layer 22. This generates a two-dimensional electron gas 26 within the electron transport layer 22. The electron supply layer 24 supplies electrons to the channel region (i.e., the two-dimensional electron gas 26) formed in the electron transport layer 22.
[0083] The threshold adjustment layer 28 is an example of a second p-type nitride semiconductor layer provided between the electron supply layer 24 and the gate electrode 34. Specifically, the threshold adjustment layer 28 is formed with a substantially uniform thickness and a shape that follows the upper surface of the electron supply layer 24.
[0084] The threshold adjustment layer 28 has, for example, a thickness of 100 nm and a carrier concentration of 1 × 10⁻⁶ 17 cm -3 It is a nitride semiconductor layer made of p-type GaN or AlGaN. The threshold adjustment layer 28 is formed by regrowth using the MOVPE method or HVPE method following the formation process of the electron supply layer 24, and then patterned.
[0085] The presence of the threshold adjustment layer 28 raises the potential at the conduction band edge of the channel portion. This allows the threshold voltage of the nitride semiconductor device 1 to be increased. Therefore, the nitride semiconductor device 1 can be realized as a normally-off type FET. In other words, the nitride semiconductor device 1 can be turned off when a potential of 0V is applied to the gate electrode 34. Note that the threshold adjustment layer 28 is not required.
[0086] Furthermore, the threshold adjustment layer 28 may be an insulating layer made of SiN and / or SiO2 instead of the p-type AlGaN layer. Even in this case, normally-off operation can be achieved by suppressing the gate current and shifting the threshold in the positive direction.
[0087] The gate electrode 34 is positioned above the electron supply layer 24 so as to cover the gate opening 40. Specifically, the gate electrode 34 is positioned above the threshold adjustment layer 28 and overlaps the gate opening 40 in a plan view. More specifically, the gate electrode 34 is positioned in contact with the upper surface of the threshold adjustment layer 28 so as to cover the gate opening 40. The gate electrode 34 is formed, for example, with a substantially uniform film thickness in a shape along the upper surface of the threshold adjustment layer 28. Alternatively, the gate electrode 34 may be formed to fill a recess in the upper surface of the threshold adjustment layer 28.
[0088] The gate electrode 34 is formed using a conductive material such as a metal. For example, the gate electrode 34 is formed using palladium (Pd). The material for the gate electrode 34 can be a material that is ohmic-connected to the p-type GaN layer. For example, nickel (Ni)-based materials, tungsten silicide (WSi), gold (Au), etc., can be used. The gate electrode 34 is formed after the deposition of the threshold adjustment layer 28, after the formation of the source opening 30, or after the formation of the source electrode 32, by patterning a conductive film deposited by sputtering or vapor deposition, for example.
[0089] The source opening 30 is an example of a second opening located away from the gate electrode 34, penetrating the electron supply layer 24, the electron transport layer 22, and the second underlayer 16, and reaching the first underlayer 14. In a plan view, the source opening 30 is located away from the gate electrode 34.
[0090] The bottom 30a of the source opening 30 is part of the upper surface of the first substrate 14. As shown in Figure 1A, the bottom 30a is located below the lower surface of the second substrate 16. The lower surface of the second substrate 16 corresponds to the interface between the second substrate 16 and the first substrate 14. The bottom 30a is parallel to, for example, the main surface 10a of the substrate 10.
[0091] As shown in Figure 1A, the source opening 30 is formed such that its opening area is constant regardless of its distance from the substrate 10. Specifically, the side wall portion 30b of the source opening 30 is perpendicular to the bottom portion 30a. In other words, the cross-sectional shape of the source opening 30 is rectangular.
[0092] Alternatively, the source opening 30 may be formed such that its opening area increases as it moves away from the substrate 10. Specifically, the side wall portion 30b of the source opening 30 may be inclined at an angle. For example, the cross-sectional shape of the source opening 30 may be an inverted trapezoid, or more specifically, an inverted isosceles trapezoid. In this case, the inclination angle of the side wall portion 30b with respect to the bottom portion 30a may be, for example, in the range of 30° to 60°. The inclination of the side wall portion 30b increases the contact area between the source electrode 32 and the electron transport layer 22 (two-dimensional electron gas 26), making ohmic connection easier. The two-dimensional electron gas 26 is exposed on the side wall portion 30b of the source opening 30 and is connected to the source electrode 32 at the exposed portion.
[0093] The source opening 30 is not necessarily required. The presence of the source opening 30 reduces the ohmic contact resistance with the two-dimensional electron gas 26 (channel). It also allows for electrical connection between the first substrate 14 and the source electrode 32.
[0094] The source electrode 32 is positioned spaced apart from the gate electrode 34. In this embodiment, the source electrode 32 is provided along the inner surface of the source opening 30. Specifically, the source electrode 32 is connected to the electron supply layer 24, the electron transport layer 22, and the first underlayer 14. The source electrode 32 is ohmic connected to the electron transport layer 22 and the electron supply layer 24. The source electrode 32 is in contact with the two-dimensional electron gas 26 (channel) at the side wall portion 30b of the source opening 30. This reduces the contact resistance between the source electrode 32 and the two-dimensional electron gas 26 (channel).
[0095] The source electrode 32 is formed using a conductive material such as a metal. As the material for the source electrode 32, for example, a material such as Ti / Al that becomes ohmic connected to the n-type GaN layer through heat treatment can be used. The source electrode 32 is formed, for example, by patterning a conductive film deposited by sputtering or vapor deposition.
[0096] The drain electrode 36 is located below the substrate 10. In other words, the drain electrode 36 is located on the opposite side from the drift layer 12. Specifically, the drain electrode 36 is located in contact with the main surface 10b of the substrate 10.
[0097] The drain electrode 36 is formed using a conductive material such as a metal. Similar to the material of the source electrode 32, the material of the drain electrode 36 can be a material that is ohmic-connected to n-type GaN, such as Ti / Al. The drain electrode 36 is formed, for example, by patterning a conductive film deposited by sputtering or vapor deposition.
[0098] [Distinctive structure] Next, the main characteristic configuration of the nitride semiconductor device 1 according to this embodiment will be explained using Figure 1B.
[0099] [Edge shape of the first sublayer] Figure 1B shows a cross-section (xz plane) parallel to the direction in which the gate electrode 34 and source electrode 32 are aligned (x-axis direction) and perpendicular to the main surface 10a of the substrate 10. Figure 1B shows the lower end PL, first end P1, second end P2, and upper end PH, which represent the positions on the surface of the first underlayer 14.
[0100] The lower end PL, the first end P1, the second end P2, and the upper end PH are all located on the surface of the first substrate layer 14, in the portion that constitutes the side wall portion 40b of the gate opening 40. In other words, the lower end PL, the first end P1, the second end P2, and the upper end PH are all located within the contact surface between the first substrate layer 14 and the electron traveling layer 22.
[0101] In a plan view, the lower end PL, the first end P1, the second end P2, and the upper end PH are arranged in this order from the bottom 40a of the gate opening 40 toward the opening end (i.e., the upper end). As shown in Figure 1B, the first end P1 is located above the lower end PL. The second end P2 is located below the upper end PH. In this embodiment, the first end P1 and the second end P2 are located at the same height.
[0102] Figure 1B shows two dashed lines, VL1 and VL2. Dashed line VL1 is an extension of the first line segment connecting the lower end PL and the first point P1. Dashed line VL2 is an extension of the second line segment connecting the lower end PL and the upper end PH. The angle α1 that dashed line VL1 makes with the main surface 10a is greater than the angle α2 that dashed line VL2 makes with the main surface 10b.
[0103] By satisfying α1 > α2, nitride semiconductor device 1 can achieve both good off-characteristics and reduced on-resistance. This principle will be explained using Figures 2A and 2B, in comparison with comparative examples.
[0104] Figure 2A is a cross-sectional view illustrating channel constriction in a nitride semiconductor device 1x according to a comparative example. In Figure 2A, the side surface of the first underlayer 14x is a flat inclined surface among the sidewall portion 40bx of the gate opening 40x. Therefore, the side surface of the first underlayer 14x and the two-dimensional electron gas 26 (channel) are approximately parallel. As a result, as shown in Figure 2A, when the device is ON, a depletion layer extends from the side surface of the first underlayer 14x toward the two-dimensional electron gas 26 (channel) in the electron transport layer 22. This depletion layer constricts most of the inclined portion of the two-dimensional electron gas 26, resulting in a higher ON resistance.
[0105] Figure 2B is a cross-sectional view illustrating the channel constriction of the nitride semiconductor device 1 according to this embodiment. Compared to the comparative example shown in Figure 2A, in this embodiment, by satisfying α1 > α2, as shown in Figure 1B, the upper end PH is located closer to the source electrode 32 than the dashed line VL1, i.e., in a direction that widens the opening of the gate opening 40. As a result, it is possible to maintain a short distance between the lower end PL and the first end P1 of the first underlayer 14 and the two-dimensional electron gas 26, while ensuring a long distance between the upper end PH of the first underlayer 14 and the two-dimensional electron gas 26. Therefore, as shown in Figure 2B, the depletion layer extending from the first underlayer 14 into the electron transport layer 22 constricts only a portion of the sloped portion of the two-dimensional electron gas 26. As is clear from comparison with Figure 2A, the portion of the sloped portion of the two-dimensional electron gas 26 that is not constricted by the depletion layer increases, thus reducing the on-resistance.
[0106] Furthermore, the lower end PL and first end P1 of the first base layer 14 are located on the bottom 40a side of the gate opening 40, similar to the comparative example. The distance between the lower part of the first base layer 14 and the threshold adjustment layer 28, which functions as part of the gate electrode 34, is the same as in the comparative example. Therefore, good off-field characteristics can be maintained in terms of electric field relaxation during the off state, similar to the comparative example. In addition, the contact area between the first base layer 14 and the drift layer 12 is also large, similar to the comparative example, so the pressure resistance due to the expansion of the depletion layer by the pn junction between the first base layer 14 and the drift layer 12 can be ensured.
[0107] As described above, the nitride semiconductor device 1 according to this embodiment makes it possible to achieve both good off-characteristics and reduced on-resistance.
[0108] In this embodiment, specifically, the side wall portion 40b is formed such that α1 > α2 is satisfied by having a step between the lower end PL and the upper end PH of the first base layer 14. Specifically, as shown in Figures 1A and 1B, the side wall portion 40b includes inclined surfaces 41 and 42 and an intermediate surface 43.
[0109] The inclined surface 41 is an example of a first side wall surface, and is the section from the lower end PL to the first end P1 of the first subsoil layer 14 in the side wall portion 40b of the gate opening 40. The inclined surface 41 is a plane inclined with respect to the main surface 10a of the substrate 10. The inclination angle β1 is an example of a first inclination angle, and is the angle that the inclined surface 41 makes with respect to the main surface 10a.
[0110] The inclined surface 42 is an example of a second side wall surface, and is the section from the second end P2 to the upper end PH of the first subsoil layer 14 in the side wall portion 40b of the gate opening 40. The inclined surface 42 is a plane inclined with respect to the main surface 10a of the substrate 10. The inclination angle β2 is an example of a second inclination angle, and is the angle that the inclined surface 42 makes with respect to the main surface 10a.
[0111] In this embodiment, the inclination angle β2 is equal to the inclination angle β1. For example, the inclination angles β1 and β2 are between 20° and 80°. Alternatively, the inclination angles β1 and β2 may be between 30° and 45°. The larger the inclination angles β1 and β2, the shorter the unit cell length can be. The unit cell length corresponds, for example, to the distance (pitch) between the centers of the source electrodes 32 arranged on either side of the gate opening 40. The smaller the inclination angles β1 and β2, the closer the inclined surfaces 41 and 42 are to the c-plane, so the film quality of the electron transport layer 22 and other layers formed along the inclined surfaces 41 and 42 by crystal regrowth can be improved.
[0112] The intermediate surface 43 is an example of a third side wall surface, and is the section from the first end P1 to the second end P2 of the first sublayer 14 in the side wall portion 40b of the gate opening 40. The intermediate surface 43 has a different inclination from both the inclined surfaces 41 and 42. Specifically, the intermediate surface 43 is a plane parallel to the main surface 10a of the substrate 10. However, the intermediate surface 43 may be inclined with respect to the main surface 10a.
[0113] The intermediate surface 43 is located, for example, approximately in the center of the thickness direction of the first sublayer 14. Alternatively, the intermediate surface 43 may be located below the center of the thickness direction of the first sublayer 14. This can further reduce the area in which the channel is narrowed, thereby further reducing the on-resistance.
[0114] Such stepped gate openings 40 are formed by etching in two stages. Specifically, a drift layer 12, a first underlayer 14, and a second underlayer 16 are deposited in that order over the entire surface 10a of the substrate 10, and then a first resist mask patterned to a predetermined shape is formed and etched. In the first etching, the first underlayer 14 is not penetrated. This forms the inclined surface 42 and the intermediate surface 43.
[0115] Next, a second resist mask with smaller openings than the first resist mask is formed, and a second etching is performed. In the second etching, the first underlayer 14 is penetrated, and the surface portion of the drift layer 12 is removed. This forms the inclined surface 41 and the bottom portion 40a. In this way, by etching in two stages, a step is formed in the first underlayer 14.
[0116] Thus, in the upper part of the stepped first substrate layer 14, the distance between the first substrate layer 14 and the inclined portion of the two-dimensional electron gas 26 increases. Therefore, as shown in Figure 2B, the narrowed channel region can be shortened, and the on-resistance can be reduced. Furthermore, in the lower part of the stepped first substrate layer 14, the distance to the threshold adjustment layer 28 can be kept short, enabling appropriate electric field relaxation. Thus, good off-characteristics can be maintained.
[0117] Note that the inclined surfaces 41 and 42 do not have to be flat. At least one of the inclined surfaces 41 and 42 may be a concave or convex curved surface. In the case of a curved surface, the inclination angles β1 and β2 can be defined, for example, by the angle that the line segment connecting the lower and upper ends of each inclined surface makes with respect to the main surface 10a. In this case, β1 may be greater than or less than α1.
[0118] [Position of the edge of the threshold adjustment layer] In this embodiment, the threshold voltage of the transistor can be adjusted depending on whether the threshold adjustment layer 28 completely covers the gate opening 40 or covers only a portion of it. In other words, the threshold voltage can be adjusted according to the position of the edge of the threshold adjustment layer 28. If the threshold adjustment layer 28 is not provided, the position of the edge of the gate electrode 34 corresponds to the position of the edge of the threshold adjustment layer 28.
[0119] In a plan view, if the edge of the threshold adjustment layer 28 is located inside the upper end of the side wall portion 40b of the gate opening 40, the threshold voltage of the transistor is determined only by the sloping portion of the two-dimensional electron gas 26 (specifically, the portion along the side wall portion 40b). In such a configuration, the carrier concentration in the flat portion of the two-dimensional electron gas 26 (specifically, the portion located above the second underlying layer 16) can be increased, thereby reducing the on-resistance.
[0120] In a plan view, if the end of the threshold adjustment layer 28 is located outside the upper end of the side wall portion 40b of the gate opening 40, the threshold voltage of the transistor is determined by the higher threshold voltage of either the sloped portion or the flat portion of the two-dimensional electron gas 26. For example, if the threshold voltage of the transistor is to be determined by the flat portion, it is necessary to reduce only the threshold voltage of the sloped portion (for example, to a negative voltage).
[0121] In this case, the film thickness Gx1 of the electron transport layer 22 in the direction parallel to the main surface 10a of the substrate 10 is made greater than the film thickness Gz of the electron transport layer 22 in the direction perpendicular to the main surface 10a of the substrate 10. This makes it possible to make the distance between the first underlayer 14 and the inclined portion of the two-dimensional electron gas 26 greater than the distance between the first underlayer 14 and the flat portion of the two-dimensional electron gas 26. As a result, the influence of the depletion layer extending from the first underlayer 14 on the inclined portion of the two-dimensional electron gas 26 can be reduced compared to the flat portion, and the threshold voltage of the inclined portion can be selectively reduced. Therefore, the threshold voltage of the transistor can be determined in the flat portion of the two-dimensional electron gas 26.
[0122] [Thickness of the electron transport layer] As shown in Figure 1A, the electron transport layer 22 has a larger film thickness Gx2 in the direction parallel to the main surface 10a of the substrate 10 than the film thickness Gz in the direction perpendicular to the main surface 10a of the substrate 10. The film thickness Gx2 is the distance in the direction parallel to the main surface 10a between the upper end of the gate opening 40 and the electron supply layer 24. By increasing the film thickness Gx2, the distance between the two-dimensional electron gas 26 generated along the side wall portion 40b of the gate opening 40 and the first underlying layer 14 can be increased, thereby suppressing a decrease in carrier concentration.
[0123] Generally, in vertical FETs, GaN crystal growth is carried out so that the c-plane of the GaN crystal is parallel to the main surface 10a of the substrate 10. In this case, the two-dimensional electron gas 26 experiences less polarization in the portion inclined with respect to the c-plane compared to the portion parallel to the c-plane, resulting in a decrease in carrier concentration. In other words, the carrier concentration of the two-dimensional electron gas 26 is lower in the portion along the side wall portion 40b of the gate opening 40 than in the flat portion. Therefore, the inclined portion of the two-dimensional electron gas 26 is more susceptible to the constriction effect of the depletion layer extending from the first underlying layer 14, and the on-resistance can be reduced further by moving it away from the first underlying layer 14.
[0124] Furthermore, if the thickness of the electron transport layer 22 perpendicular to the main surface 10a of the substrate 10 is thin, the depth of the source opening 30 for contacting the source electrode 32 and the first underlayer 14 can be made shallower. A shallower source opening 30 not only shortens the process time but also improves the coverage of the source electrode 32 formed later. This makes it possible to simplify the process while reducing on-resistance.
[0125] Thus, by having a larger film thickness Gx2 in the direction parallel to the main surface 10a of the substrate 10 than the film thickness Gz in the direction perpendicular to the main surface 10a of the substrate 10 of the electron transport layer 22, it becomes possible to simplify the process while reducing on-resistance.
[0126] [Differentiation] Next, modified examples of the nitride semiconductor device according to this embodiment will be described using Figures 3A and 3B. In the following, the differences from Embodiment 1 will be the main focus of the explanation, and the common points will be omitted or simplified.
[0127] Figure 3A is a cross-sectional view of a nitride semiconductor device 2 according to a modified example of this embodiment. Figure 3B is a partially enlarged cross-sectional view of Figure 3A. Specifically, Figure 3B shows the vicinity of the side wall portion 40b of the gate opening 40 in Figure 3A.
[0128] As shown in Figures 3A and 3B, in the nitride semiconductor device 2 according to this modified example, the inclination angle β1 of the inclined surface 41 and the inclination angle β2 of the inclined surface 42 are different. Specifically, the inclination angle β1 is smaller than the inclination angle β2. For example, the inclination angle β1 is between 30° and 45°. The inclination angle β2 is between 70° and 90°.
[0129] Thus, even when the tilt angle β1 is smaller than the tilt angle β2, if the upper end PH is located below the dashed line VL1, the condition α1 > α2 is satisfied, as shown in Figure 3B. This allows for a shorter unit cell length of the nitride semiconductor device 2 while maintaining good off-resistance and suppressing an increase in on-resistance. A shorter unit cell length allows for more cells to be placed in the same area. Therefore, on-resistance can be further reduced.
[0130] Note that the tilt angle β1 may be greater than the tilt angle β2. Even in this case, since α1 > α2 is satisfied, it is possible to achieve both good off-mode characteristics and reduced on-resistance.
[0131] The inclined surfaces 41 and 42 are formed such that the edge shape of the resist mask during etching is transferred to them. Therefore, when etching is performed in two stages, the inclination angle β1 of inclined surface 41 and the inclination angle β2 of inclined surface 42 can be made different by making the inclination angles of the edges of the resist mask different. For example, the edge shape of the resist mask can be made different by adjusting conditions such as whether or not the resist mask is baked, the temperature, and the time.
[0132] Furthermore, if a step is provided in the first sublayer 14, that is, if an intermediate surface 43 is provided, then α1 > α2 does not necessarily have to be satisfied. Specifically, in Figure 3B, if the upper end PH is located on or above the dashed line VL1, then α1 ≤ α2 may be satisfied. In this case, not only the lower part of the inclined portion of the two-dimensional electron gas 26 but also the upper part is constricted, but the constriction in the intermediate portion is suppressed. Therefore, compared to the comparative example shown in Figure 2A, the region in which the two-dimensional electron gas 26 is constricted is narrower, so the on-resistance can be reduced. As for the off-characteristics, they are the same as in the comparative example, so good off-characteristics can be maintained. Thus, when a step is provided in the first sublayer 14, even if α1 ≤ α2, it is possible to achieve both good off-characteristics and reduced on-resistance.
[0133] (Embodiment 2) Next, Embodiment 2 will be described.
[0134] Embodiment 2 differs from Embodiment 1 in that the first p-type underlayer includes an AlGaN layer. Below, we will focus on explaining the differences from Embodiment 1, and omit or simplify the explanation of the common points.
[0135] Figure 4 is a cross-sectional view of the nitride semiconductor device 101 in this embodiment. As shown in Figure 4, the nitride semiconductor device 101 in this embodiment differs from the nitride semiconductor device 1 in Embodiment 1 in that it has a first underlayer 114 instead of the first underlayer 14.
[0136] The first underlayer 114 includes a p-type AlGaN layer 114c. Specifically, the first underlayer 114 includes p-type GaN layers 114a and 114b and a p-type AlGaN layer 114c. The AlGaN layer 114c is provided between the GaN layer 114a and the GaN layer 114b. The AlGaN layer 114c can be formed at a desired location and with a desired thickness by changing the supplied gas for film formation by epitaxial growth.
[0137] The AlGaN layer 114c functions as an etch stopper layer. That is, when forming the gate opening 40, the first dry etching conditions can be set so that the etching rates of the GaN layer 114b and the AlGaN layer 114c are different.
[0138] Specifically, a dry etching condition is used in which the etching rate of the AlGaN layer 114c is drastically reduced compared to the etching rate of the GaN layer 114b. This allows the intermediate surface 43 in the first underlayer 114 to be made the upper surface of the AlGaN layer 114c. Even if the actual etching rate of the GaN layer 114b differs from the expected rate due to variations within the wafer, stable etching becomes possible.
[0139] The heights of the inclined surfaces 41 and 42 can be predetermined by determining the position of the AlGaN layer 114c within the first base layer 114. This allows for the stabilization of the step shape and depth. By stabilizing the step shape, a highly reliable nitride semiconductor device 101 can be realized.
[0140] The AlGaN layer 114c only needs to function as an etch stopper, so its thickness can be, for example, around 5 nm. Furthermore, the AlGaN layer 114c may be composed of undoped AlGaN.
[0141] Furthermore, in this embodiment as well, similar to the modification of Embodiment 1, the inclination angle β1 of the inclined surface 41 and the inclination angle β2 of the inclined surface 42 may be different.
[0142] Figure 5 is a cross-sectional view of a nitride semiconductor device 102 according to a modified example of this embodiment. As shown in Figure 5, in the nitride semiconductor device 102 according to this modified example, the first underlayer 114 includes an AlGaN layer 114c, and the inclination angles of the inclined surface 41 and the inclination angles of the inclined surface 42 are different. For example, the inclination angle of the inclined surface 41 is 30° or more and 45° or less. The inclination angle of the inclined surface 42 is 70° or more and 90° or less.
[0143] This allows for a shorter unit cell length of the nitride semiconductor device 102 while simultaneously achieving good off-resistance and reduced on-resistance. Furthermore, the shape and depth of the step in the first underlayer 114 can be stabilized. Therefore, by stabilizing the shape, a highly reliable nitride semiconductor device 102 can be realized.
[0144] (Embodiment 3) Next, Embodiment 3 will be described.
[0145] Embodiment 3 differs from Embodiment 1 in that the bottom of the threshold adjustment layer is located below the bottom end of the first sublayer. Below, we will focus on explaining the differences from Embodiment 1, and omit or simplify the explanation of the common points.
[0146] Figure 6 is a cross-sectional view of the nitride semiconductor device 201 according to this embodiment. As shown in Figure 6, the nitride semiconductor device 201 according to this embodiment differs from the nitride semiconductor device 1 according to Embodiment 1 in that it has a gate opening 240 instead of a gate opening 40.
[0147] The bottom 240a of the gate opening 240 is formed by removing a large portion of the surface layer of the drift layer 12. As the bottom 240a approaches the substrate 10, the bottom of the threshold adjustment layer 28 is closer to the drain electrode 36 than the bottom of the first underlayer 14 (i.e., the lower end PL).
[0148] When a high voltage is applied to the drain electrode 36 while the device is off, the pn junction formed between the p-type threshold adjustment layer 28 located within the gate opening 240 and the electron supply layer 24 and electron transport layer 22, and the pn junction formed between the p-type first underlayer 14 and the drift layer 12 are each subjected to an electric field. Generally, since the gate opening 240 is formed by dry etching, the etched surface at the edge of the first underlayer 14 is susceptible to damage. Therefore, the dielectric breakdown electric field strength of the pn junction formed between the first underlayer 14 and the drift layer 12 near the gate opening 240 may be low.
[0149] On the other hand, the pn junction formed between the threshold adjustment layer 28 and the electron supply layer 24 and electron transport layer 22 is formed by crystal growth, so there is no etching damage. In other words, the dielectric breakdown field strength is more likely to be obtained at an ideal value. Therefore, by bringing the bottom of the threshold adjustment layer 28 closer to the drain electrode 36 than the bottom of the first underlayment layer 14, the pn junction formed between the threshold adjustment layer 28 and the electron supply layer 24 and electron transport layer 22 can receive more of the electric field strength when off. This makes it possible to reduce the off-leak current and obtain high breakdown voltage characteristics.
[0150] In this embodiment, the first underlayer 14 may also include an AlGaN layer 114c that functions as an etch stopper, similar to the second embodiment.
[0151] (Embodiment 4) Next, Embodiment 4 will be described.
[0152] Embodiment 4 differs from Embodiment 1 in that two steps are provided in the first sub-layer. Below, we will focus on explaining the differences from Embodiment 1, and omit or simplify the explanation of the common points.
[0153] Figure 7A is a cross-sectional view of the nitride semiconductor device 301 according to this embodiment. Figure 7B is a partially enlarged cross-sectional view of Figure 7A. Specifically, Figure 7B shows the vicinity of the side wall portion 340b of the gate opening 340 in Figure 7A.
[0154] As shown in Figure 7A, the nitride semiconductor device 301 according to this embodiment differs from the nitride semiconductor device 1 according to Embodiment 1 in that it has a gate opening 340 instead of a gate opening 40. The side wall portion 340b of the gate opening 340 has two steps. Specifically, the side wall portion 340b includes inclined surfaces 341, 342 and 344 and intermediate surfaces 343a and 343b.
[0155] The inclined surface 341 is an example of a first side wall surface, and is the section from the lower end PL to the first end P1 of the first subsoil layer 14 in the side wall portion 340b of the gate opening 340. The inclined surface 341 is a plane inclined with respect to the main surface 10a of the substrate 10. The inclination angle β1 is an example of a first inclination angle, and is the angle that the inclined surface 341 makes with respect to the main surface 10a.
[0156] The inclined surface 342 is an example of a second side wall surface, and is the section from the second end P2 to the upper end PH of the first subsoil layer 14 in the side wall portion 340b of the gate opening 340. The inclined surface 342 is a plane inclined with respect to the main surface 10a of the substrate 10. The inclination angle β2 is an example of a second inclination angle, and is the angle that the inclined surface 342 makes with respect to the main surface 10a.
[0157] Intermediate surfaces 343a and 343b are examples of third sidewall surfaces, respectively, located between the first end P1 and the second end P2. Specifically, intermediate surface 343a is the section from the first end P1 to the third end P3 of the first subfloor 14. Intermediate surface 343b is the section from the fourth end P4 to the second end P2 of the first subfloor 14.
[0158] The intermediate surfaces 343a and 343b have different inclinations from both the inclined surfaces 341 and 342. Specifically, the intermediate surfaces 343a and 343b are planes parallel to the main surface 10a of the substrate 10. At least one of the intermediate surfaces 343a and 343b may be inclined with respect to the main surface 10a.
[0159] The inclined surface 344 is an example of a fourth side wall surface, connecting two adjacent intermediate surfaces 343a and 343b. Specifically, the inclined surface 344 is the section from the third end P3 to the fourth end P4 of the first subsoil layer 14. The inclined surface 344 has a different inclination from both the intermediate surfaces 343a and 343b. Specifically, the inclined surface 344 is a plane inclined with respect to the main surface 10a of the substrate 10. The inclination angle β4 is an example of a fourth inclination angle, and is the angle that the inclined surface 344 makes with respect to the main surface 10a.
[0160] In this embodiment, the inclination angles β1, β2, and β4 are equal to each other. For example, the inclination angles β1, β2, and β4 are between 20° and 80°. Alternatively, the inclination angles β1, β2, and β4 may be between 30° and 45°. The larger at least one of the inclination angles β1, β2, and β4, the shorter the unit cell length can be. Furthermore, the smaller at least one of the inclination angles β1, β2, and β4, the closer the inclined surfaces 41, 42, or 44 are to the c-plane, thereby improving the film quality of the electron transport layer 22 and other layers formed along the inclined surfaces 41, 42, or 44 by crystal regrowth.
[0161] The lower end PL, the first end P1, the second end P2, the third end P3, the fourth end P4, and the upper end PH are all located on the surface of the first substrate layer 14, in the portion that constitutes the side wall portion 340b of the gate opening 340. In other words, the lower end PL, the first end P1, the second end P2, the third end P3, the fourth end P4, and the upper end PH are all located within the contact surface between the first substrate layer 14 and the electron traveling layer 22.
[0162] In a plan view, the lower end PL, the first end P1, the third end P3, the fourth end P4, the second end P2, and the upper end PH are arranged in this order from the bottom 40a of the gate opening 340 toward the opening end (i.e., the upper end). As shown in Figure 7B, the first end P1 and the third end P3 are located above the lower end PL. The second end P2 and the fourth end P4 are located below the upper end PH and above the first end P1 and the third end P3. In this embodiment, the first end P1 and the third end P3 are located at the same height. The fourth end P4 and the second end P2 are located at the same height. If the side wall portion 340b has multiple steps, the first end P1 is the upper end of the inclined surface 341 closest to the lower end, and the second end P2 is the lower end of the inclined surface 342 closest to the upper end. Both the third end P3 and the fourth end P4 are located below the dashed line VL1. The fourth end P4 is located above the dashed line VL2, but it may also be located below the dashed line VL2.
[0163] As described above, the side wall portion 340b, which includes the two intermediate surfaces 343a and 343b, is formed by etching the gate opening 340 in three separate steps. The side wall portion 340b may have three or more steps (specifically, intermediate surfaces). By performing etching in stages for the number of steps + 1, a side wall portion 340b with multiple steps can be formed.
[0164] This allows the film thickness of the first substrate layer 14 to be reduced more gradually toward the bottom 40a. Compared to the case with a single step, the off-pass characteristics can be maintained more stably.
[0165] In this embodiment as well, α1 > α2 is satisfied. This allows the nitride semiconductor device 301 to achieve both good off-characteristics and reduced on-resistance. In this embodiment, at least two of the tilt angles β1, β2, and β4 may be different from each other. For example, by increasing one of the tilt angles β1, β2, and β4, the unit cell length can be shortened, and the on-resistance can be further reduced.
[0166] Furthermore, in this embodiment, the first base layer 14 may include an AlGaN layer 114c that functions as an etch stopper, similar to Embodiment 2. In this case, multiple AlGaN layers 114c may be included for each step. Alternatively, the first base layer 14 may include only one AlGaN layer 114c to form the lowest step (specifically, the intermediate surface 343a).
[0167] Furthermore, similar to Embodiment 3, the bottom of the threshold adjustment layer 28 may be located below the bottom of the first base layer 14.
[0168] (Embodiment 5) Next, Embodiment 5 will be described.
[0169] Embodiment 5 differs from Embodiment 1 in that the drift layer includes multiple layers. Below, we will focus on explaining the differences from Embodiment 1, and omit or simplify the explanation of the common points.
[0170] Figure 8 is a cross-sectional view of the nitride semiconductor device 401 according to this embodiment. As shown in Figure 8, the nitride semiconductor device 401 of this embodiment differs in that it has a drift layer 412 instead of a drift layer 12.
[0171] The drift layer 412 includes multiple layers 412a and 412b with different impurity concentrations. Here, the drift layer 412 is shown to consist of two layers, but it may also consist of three or more layers. Layer 412b is the uppermost layer among all the layers included in the drift layer 412. The upper surface of layer 412b is in contact with the lower surface of the first substrate layer 14.
[0172] The impurity concentration in layer 412b is the lowest among all the layers included in the drift layer 412. Here, the impurity concentration is specifically the donor concentration, which is the concentration of Si or O. This promotes electric field relaxation at the pn junction formed between the first sublayer 14 and the drift layer 412 during the off state, resulting in good off characteristics.
[0173] In this embodiment, the first base layer 14 may include an AlGaN layer 114c that functions as an etch stopper, similar to Embodiment 2. Also, similar to Embodiment 3, the bottom of the threshold adjustment layer 28 may be located below the bottom of the first base layer 14. Furthermore, similar to Embodiment 4, the first base layer 14 may have multiple steps.
[0174] (Embodiment 6) Next, Embodiment 6 will be described.
[0175] Embodiment 6 differs from Embodiment 1 in that the side wall does not have a step. Below, we will mainly explain the differences from Embodiment 1, and the explanation of the common points will be omitted or simplified.
[0176] Figure 9A is a cross-sectional view of the nitride semiconductor device 501 according to this embodiment. Figure 9B is a partially enlarged cross-sectional view of Figure 9A. Specifically, Figure 9B shows the vicinity of the side wall portion 540b of the gate opening 540 in Figure 9A.
[0177] As shown in Figure 9A, the nitride semiconductor device 501 according to this embodiment differs from the nitride semiconductor device 1 according to Embodiment 1 in that it has a gate opening 540 instead of a gate opening 540. The side wall portion 540b of the gate opening 540 does not have a step. The side wall portion 540b includes two inclined surfaces with different inclinations. Specifically, the side wall portion 540b includes inclined surfaces 41 and 542. Inclined surface 41 is the same as in Embodiment 1.
[0178] The inclined surface 542 is an example of a second side wall surface, and is the section from the second end P2 to the upper end PH of the first subsoil layer 14 in the side wall portion 540b of the gate opening 540. The inclined surface 542 is a plane inclined with respect to the main surface 10a of the substrate 10. The inclination angle β2 is an example of a second inclination angle, and is the angle that the inclined surface 542 makes with respect to the main surface 10a.
[0179] In this embodiment, the first end P1 and the second end P2 are located at the same position. Therefore, the inclined surface 41 and the inclined surface 542 are continuous. The inclination angle β1 of the inclined surface 41 is greater than the inclination angle β2 of the inclined surface 542. As a result, α1 > α2 is satisfied, and similar to Embodiment 1, good off-resistance and reduced on-resistance can be achieved simultaneously.
[0180] (Other embodiments) Although nitride semiconductor devices according to one or more embodiments have been described above based on these embodiments, this disclosure is not limited to these embodiments. Without departing from the spirit of this disclosure, various modifications to these embodiments that a person skilled in the art could conceive of, as well as forms constructed by combining components from different embodiments, are also included within the scope of this disclosure.
[0181] For example, in a plan view, the end of the threshold adjustment layer 28 may coincide with the end of the gate opening 40. Alternatively, in a plan view, the end of the threshold adjustment layer 28 may be located inside the gate opening 40.
[0182] Furthermore, although the above embodiment provides a source opening 30 that reaches the first underlayer 14, it is not limited to this. For example, the source opening 30 may be an opening that reaches the electron traveling layer 22, and the source electrode 32 may be connected to the electron traveling layer 22 but not to the first underlayer 14.
[0183] Furthermore, each of the above embodiments can be modified, replaced, added, or omitted in various ways within the scope of the claims or their equivalents. [Industrial applicability]
[0184] The nitride semiconductor device described herein can be used in power transistors and the like in power supply circuits, inverter circuits, and the like for equipment. [Explanation of Symbols]
[0185] 1, 2, 101, 102, 201, 301, 401, 501 Nitride Semiconductor Devices 10 circuit boards 10a, 10b main surface 12,412 drift layers 14, 114 The first sublayer 16. Second sublayer 22 Electron transport layer 24 Electron supply layer 26 Two-dimensional electron gas 28. Threshold adjustment layer 30 Source openings 30a, 40a, 240a bottom 30b, 40b, 340b, 540b side wall 32 Source electrodes 34 gate 36 Drain electrode 40, 240, 340, 540 ゲート opening Inclined surfaces: 41, 42, 341, 342, 344, 542 43, 343a, 343b Intermediate surfaces 114a and 114b GaN layers 114c AlGaN layer 412a and 412b layers P1 End 1 P2 End 2 P3, third end P4, 4th end PH upper end PL lower end VL1, VL2 single-point locking wire
Claims
1. circuit board and A first nitride semiconductor layer provided above the substrate, A first p-type nitride semiconductor layer provided above the first nitride semiconductor layer, A second nitride semiconductor layer is provided above the first p-type nitride semiconductor layer, A first opening that penetrates the second nitride semiconductor layer and the first p-type nitride semiconductor layer and reaches the first nitride semiconductor layer, An electron transport layer and an electron supply layer are provided in order from the bottom so as to cover the upper surface of the second nitride semiconductor layer and the first opening, A gate electrode is provided above the electron supply layer so as to cover the first opening, A source electrode provided away from the gate electrode, The substrate comprises a drain electrode formed below the substrate, The side wall portion of the first opening is When the position between the lower and upper ends of the first p-type nitride semiconductor layer in the side wall portion of the first opening is defined as a predetermined position, in a cross section parallel to the direction in which the gate electrode and the source electrode are aligned and perpendicular to the main surface of the substrate, the first angle made with the main surface by the first line segment connecting the lower end and the predetermined position is greater than the second angle made with the main surface by the second line segment connecting the lower end and the upper end. Nitride semiconductor devices.
2. The aforementioned side wall portion is The first side wall surface is the section from the lower end to the first end located at the predetermined position, In a plan view, the second side wall surface is the section from the second end, which is located between the first end and the upper end, to the upper end, A third side wall surface located between the first end and the second end, having a different inclination from both the first side wall surface and the second side wall surface, The nitride semiconductor device according to claim 1.
3. The third side wall surface is parallel to the main surface. The nitride semiconductor device according to claim 2.
4. The first inclination angle, which is the angle that the first side wall surface makes with respect to the main surface, is different from the second inclination angle, which is the angle that the second side wall surface makes with respect to the main surface. The nitride semiconductor device according to claim 2.
5. The first inclination angle is smaller than the second inclination angle. The nitride semiconductor device according to claim 4.
6. The second inclination angle is 70° or more and 90° or less. The nitride semiconductor device according to claim 5.
7. The first p-type nitride semiconductor layer includes an AlGaN layer. The third side wall surface is part of the upper surface of the AlGaN layer. A nitride semiconductor device according to any one of claims 2 to 6.
8. The first nitride semiconductor layer comprises two or more layers with different impurity concentrations, and among these two or more layers, the uppermost layer has the lowest impurity concentration. A nitride semiconductor device according to any one of claims 1 to 6.
9. The system comprises a second p-type nitride semiconductor layer provided between the gate electrode and the electron supply layer. A nitride semiconductor device according to any one of claims 1 to 6.
10. A second opening is provided at a position away from the gate electrode, penetrating the electron supply layer, the electron transport layer, and the second nitride semiconductor layer, and reaching the first p-type nitride semiconductor layer. The source electrode is provided within the second opening and is electrically connected to the first p-type nitride semiconductor layer. A nitride semiconductor device according to any one of claims 1 to 6.
11. The third side wall surface is the section from the first end to the second end. A nitride semiconductor device according to any one of claims 2 to 6.
12. The aforementioned side wall portion is The third side wall surface includes a plurality of such surfaces, Furthermore, it includes one or more fourth side wall surfaces that connect two adjacent third side wall surfaces and whose inclination differs from any of the plurality of third side wall surfaces, A nitride semiconductor device according to any one of claims 2 to 6.
13. The aforementioned side wall portion is The first side wall surface is the section from the lower end to the first end located at the predetermined position, A second side wall surface, which is the section from the first end to the upper end, The nitride semiconductor device according to claim 1.
14. circuit board and A first nitride semiconductor layer provided above the substrate, A first p-type nitride semiconductor layer provided above the first nitride semiconductor layer, A second nitride semiconductor layer is provided above the first p-type nitride semiconductor layer, A first opening that penetrates the second nitride semiconductor layer and the first p-type nitride semiconductor layer and reaches the first nitride semiconductor layer, An electron transport layer and an electron supply layer are provided in order from the bottom so as to cover the upper surface of the second nitride semiconductor layer and the first opening, A gate electrode is provided above the electron supply layer so as to cover the first opening, A second opening is provided at a position away from the gate electrode, penetrating the electron supply layer, the electron transport layer, and the second nitride semiconductor layer, and reaching the first p-type nitride semiconductor layer, A source electrode is provided so as to cover the second opening and is electrically connected to the first p-type nitride semiconductor layer, The substrate comprises a drain electrode formed below the substrate, The side wall portion of the first opening has at least one step between the upper end and the lower end of the first p-type nitride semiconductor layer. Nitride semiconductor devices.
Citation Information
Patent Citations
Heterojunction transistor, and method of fabricating heterojunction transistor
JP2011077400A
Semiconductor device, power source circuit, and computer
JP2021145113A
Nitride Semiconductor Devices
JP6511645B2
Nitride semiconductor device
US20210167061A1
Semiconductor device, power supply circuit, and computer
US20210288175A1