Semiconductor equipment
By incorporating a semi-insulating film with a controlled silicon-to-nitrogen atomic ratio, the semiconductor device stabilizes breakdown voltage and prevents cracking, addressing fluctuations in existing devices.
Patent Information
- Application Number
- JP2023080585
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-05-16
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2043-05-16
AI Technical Summary
The semiconductor device described in Patent Document 1 experiences fluctuations in withstand voltage due to the semi-insulating film's composition and structure, leading to instability in breakdown voltage.
The semiconductor device incorporates a semi-insulating film containing silicon and nitrogen, with a specific atomic ratio of silicon to nitrogen atoms between 0.64 and 0.74, which enhances the conductivity and stability of the film, reducing fluctuations in breakdown voltage.
The semi-insulating film with controlled silicon-to-nitrogen ratio suppresses fluctuations in breakdown voltage and prevents cracking, ensuring consistent performance.
Smart Images

Figure 0007955220000001 
Figure 0007955220000002 
Figure 0007955220000003
Abstract
Description
[Technical Field]
[0001] The present disclosure relates to a semiconductor device. [Background Art]
[0002] For example, Japanese Laid-Open Patent Publication No. 2022-074323 (Patent Document 1) describes a semiconductor device. The semiconductor device described in Patent Document 1 includes a semiconductor substrate, a first electrode, a second electrode, an insulating film, and a semi-insulating film. The semiconductor substrate has a first region and a second region surrounding the first region in a plan view. The semiconductor substrate has a first surface and a second surface opposite to the first surface in a thickness direction of the semiconductor substrate. The semiconductor substrate has an impurity region formed on the first surface in the first region. The insulating film covers the first surface in the second region. The first electrode faces the impurity region with the insulating film interposed therebetween. The second electrode is arranged on the insulating film so as to surround the first electrode while being spaced apart from the first electrode in a plan view. The semi-insulating film is arranged so as to straddle the insulating film between the first electrode and the second electrode. [Prior Art Document] [Patent Document]
[0003] [Patent Document 1] Japanese Laid-Open Patent Publication No. 2022-074323 [Summary of Invention] [Problem to be Solved by the Invention]
[0004] In the semiconductor device described in Patent Document 1, the withstand voltage may fluctuate every time a voltage is applied. Other problems and novel features will become apparent from the description of the present specification and the accompanying drawings. [Means for Solving the Problems]
[0005] The semiconductor device of this disclosure comprises a semiconductor substrate, an insulating film, a first electrode and a second electrode, and a semi-insulating film. The semiconductor substrate has a first surface. In a plan view, the semiconductor substrate has an element region and a termination region surrounding the element region. The semiconductor substrate has a first impurity region formed on the first surface in the termination region. The insulating film covers the first surface in the termination region. The first electrode is electrically connected to the first impurity region and faces the first impurity region with the insulating film in between. In a plan view, the second electrode is arranged on the insulating film so as to surround the first electrode while being spaced apart from it. In a plan view, the semi-insulating film is arranged so as to straddle the insulating film between the first electrode and the second electrode. The semi-insulating film contains silicon and nitrogen. In the semi-insulating film, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms is 0.64 or more. [Effects of the Invention]
[0006] The semiconductor device of this disclosure makes it possible to suppress fluctuations in breakdown voltage. [Brief explanation of the drawing]
[0007] [Figure 1] This is a plan view of semiconductor device DEV1. [Figure 2] This is a cross-sectional view of semiconductor device DEV1 in line II-II in Figure 1. [Figure 3] This is a manufacturing process diagram for semiconductor device DEV1. [Figure 4] This is a cross-sectional view illustrating the preparation process S1. [Figure 5] This is a cross-sectional view illustrating the epitaxial growth process S2. [Figure 6] This is a cross-sectional view illustrating the first insulating film formation step S3. [Figure 7] This is a cross-sectional view illustrating the impurity region formation process S4. [Figure 8] This is a cross-sectional view illustrating the second insulating film formation step S5. [Figure 9] This is a cross-sectional view illustrating the first electrode formation step S6. [Figure 10] It is sectional drawing explaining semi-insulating film formation process S7. [Figure 11] It is sectional drawing explaining 2nd electrode formation process S8. [Figure 12] It is a graph which shows the relationship between the ratio of the number of atoms of silicon to the sum of the number of atoms of silicon and the number of atoms of nitrogen in the semi-insulating film SIF and the number of silicon-hydrogen bonds. [Figure 13] It is a graph which shows the relationship between the number of measurements of withstand voltage and withstand voltage. [Figure 14] It is a graph which shows the relationship between the refractive index of the semi-insulating film SIF and the ratio of the number of atoms of silicon to the sum of the number of atoms of silicon and the number of atoms of nitrogen in the semi-insulating film SIF. [Figure 15] It is a graph which shows the relationship between the refractive index of the semi-insulating film SIF and the variation of the thickness T1 of the semi-insulating film SIF. [Figure 16] It is sectional drawing of semiconductor device DEV2. [Figure 17] It is a manufacturing process figure of semiconductor device DEV2. [Figure 18] It is sectional drawing of semiconductor device DEV3. [Figure 19] It is a manufacturing process figure of semiconductor device DEV3. [Figure 20] It is sectional drawing explaining 1st impurity region formation process S10. [Figure 21] It is sectional drawing explaining 1st insulating film formation process S3 in the manufacturing method of semiconductor device DEV3. [Figure 22] It is sectional drawing explaining 2nd impurity region formation process S11. [Figure 23] It is sectional drawing of semiconductor device DEV4. [Figure 24] It is a manufacturing process figure of semiconductor device DEV4. [Figure 25] It is sectional drawing explaining 1st insulating film formation process S3 in the manufacturing method of semiconductor device DEV4. [Figure 26] It is sectional drawing explaining 3rd impurity region formation process S12. [Figure 27]It is sectional drawing explaining 4th impurity region formation process S13. (Mode for Carrying Out the Invention)
[0008] Embodiments of the present disclosure will be described in detail with reference to the drawings. In the following drawings, the same or corresponding parts are denoted by the same reference numerals, and redundant descriptions will not be repeated.
[0009] (First Embodiment) A semiconductor device DEV1 according to the first embodiment will be described.
[0010] <Configuration of Semiconductor Device DEV1> The configuration of the semiconductor device DEV1 will be described below.
[0011] FIG. 1 is a plan view of the semiconductor device DEV1. FIG. 2 is a cross-sectional view of the semiconductor device DEV1 taken along line II-II in FIG. As shown in FIGS. 1 and 2, the semiconductor device DEV1 has a semiconductor substrate SUB. The semiconductor substrate SUB has a first surface FS and a second surface SS on the opposite side of the first surface FS in the thickness direction of the semiconductor substrate SUB. The constituent material of the semiconductor substrate SUB is, for example, single crystal silicon (Si).
[0012] The semiconductor substrate SUB has an element region SUB1 and a termination region SUB2. The termination region SUB2 surrounds the element region SUB1 in plan view.
[0013] The semiconductor substrate SUB has an impurity region R1, an impurity region R2, an impurity region R3, an impurity region R4, and an impurity region R5. The conductivity type of the impurity region R1 and the conductivity type of the impurity region R2 are of a first conductivity type. The first conductivity type is, for example, n-type. The conductivity type of the impurity region R3 and the conductivity type of the impurity region R4 are of a second conductivity type. The second conductivity type is, for example, p-type. The conductivity type of the impurity region R5 is of the first conductivity type or the second conductivity type.
[0014] Impurity region R1 is formed on the second surface SS. Impurity region R2 is formed on the first surface FS. Impurity region R2 is in contact with impurity region R1 on the opposite side of the first surface FS. Impurity regions R1 and R2 form the cathode of, for example, an FRD (Fast Recovery Diode).
[0015] The impurity region R3 is formed on the first surface FS in the element region SUB1. The impurity region R4 is formed on the first surface in the termination region SUB2. The impurity region R3 is pn junctioned with the impurity region R2. The impurity region R3 forms, for example, the anode of the FRD. Thus, the semiconductor device DEV1 has an FRD formed in the element region SUB1.
[0016] The impurity region R4 is formed on the first surface FS in the termination region SUB2. In a plan view, the impurity region R4 straddles the boundary between the element region SUB1 and the termination region SUB2. In a plan view, the impurity region R4 surrounds the impurity region R3. The impurity region R4 is in contact with the impurity region R3. That is, the impurity region R4 is electrically connected to the impurity region R3. The impurity region R4 is pn junctioned with the impurity region R2. The impurity concentration in the impurity region R4 is lower than the impurity concentration in the impurity region R3. That is, the impurity region R4 has a RESURF (REduced Surface Field) structure. The impurity region R5 is formed on the first surface FS in the termination region SUB2. In a plan view, the impurity region R5 surrounds the impurity region R4. The impurity region R5 is spaced apart from the impurity region R4.
[0017] The semiconductor device DEV1 further has an insulating film ISL. The insulating film ISL is located on a first surface FS. The insulating film ISL covers at least the first surface FS in the terminal region SUB2. The insulating film ISL partially covers the first surface FS in the device region SUB1. The insulating film ISL has an opening OP1 and an opening OP2 formed therein. The opening OP1 is formed on an impurity region R3. The opening OP2 is formed on an impurity region R5.
[0018] The insulating film ISL comprises a first insulating film ISL1 and a second insulating film ISL2. The constituent materials of the first insulating film ISL1 and the second insulating film ISL2 are, for example, silicon oxide (SiO2). The first insulating film ISL1 covers the first surface FS located between impurity regions R3 and R5. The second insulating film ISL2 covers the first insulating film ISL1. Therefore, a step is formed on the upper surface of the insulating film ISL.
[0019] The semiconductor device DEV1 further includes a first electrode EL1 and a second electrode EL2. The constituent materials of the first electrode EL1 and the second electrode EL2 are, for example, aluminum (Al) or an aluminum alloy.
[0020] The first electrode EL1 has an outer peripheral edge EL1a. The outer peripheral edge EL1a faces the impurity region R4 with the insulating film ISL interposed therebetween. The outer peripheral edge EL1a functions as a field plate. The first electrode EL1 is connected to the impurity region R3 via the opening OP1. As described above, the impurity region R3 is in contact with the impurity region R4, so the first electrode EL1 is electrically connected to the impurity region R4. The second electrode EL2 is positioned on the insulating film ISL. In a plan view, the second electrode EL2 surrounds the first electrode EL1. The second electrode EL2 is spaced apart from the first electrode EL1. The second electrode EL2 is connected to the impurity region R5 via the opening OP2. The second electrode EL2 is, for example, at ground potential.
[0021] The semiconductor device DEV1 further has a semi-insulating film (SIF). The constituent material of the semi-insulating film (SIF) contains silicon and nitrogen (N). The constituent material of the semi-insulating film (SIF) is, for example, a mixed crystal of silicon nitride (Si3N4) and amorphous silicon. From another perspective, some of the silicon contained in the semi-insulating film (SIF) is bonded with hydrogen.
[0022] In a semi-insulating film (SIF), the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms (i.e., the number of silicon atoms divided by the total number of silicon atoms and nitrogen atoms) is 0.64 or greater. Alternatively, the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in a semi-insulating film (SIF) may be 0.74 or less. The ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in a semi-insulating film (SIF) is measured by XPS (X-ray Photoelectron Spectroscopy).
[0023] The refractive index of the semi-insulating film SIF is, for example, 2.55 or higher. The refractive index of the semi-insulating film SIF is, for example, 2.90 or lower. The refractive index of the semi-insulating film SIF is determined by optical measurement using a spectroscopic ellipsometer.
[0024] The semi-insulating film SIF is positioned to straddle the insulating film ISL located between the first electrode EL1 and the second electrode EL2. The semi-insulating film SIF has an inner peripheral edge SIFa. The inner peripheral edge SIFa is positioned on the outer peripheral edge EL1a. The semi-insulating film SIF covers the second electrode EL2.
[0025] The thickness T1 of the semi-insulating film SIF is, for example, between 50 nm and 1000 nm. The variation in thickness T1 is, for example, 0.02 or less. The variation in thickness T1 is defined as the larger of the value obtained by dividing the difference between the maximum value of thickness T1 and the average value of thickness T1 by the average value of thickness T1, and the value obtained by dividing the difference between the average value of thickness T1 and the minimum value of thickness T1 by the average value of thickness T1. The thickness T2 of the insulating film ISL is, for example, between 0.5 μm and 3.0 μm. Thickness T2 is measured in the portion between the first surface FS and the semi-insulating film SIF. The thickness T3 of the first electrode EL1 and the second electrode EL2 is, for example, between 2.0 μm and 6.0 μm or more, from the viewpoint of ensuring a margin during wire bonding.
[0026] The semiconductor device DEV1 further has a third electrode EL3. The material of the third electrode EL3 is, for example, aluminum or an aluminum alloy. The third electrode EL3 is positioned on the second surface SS.
[0027] The semiconductor device DEV1 further includes a passivation film PV. The constituent material of the passivation film PV is, for example, polyimide. The passivation film PV is disposed on a semi-insulating film SIF.
[0028] <Manufacturing method for semiconductor device DEV1> The manufacturing method for the semiconductor device DEV1 is described below.
[0029] Figure 3 is a manufacturing process diagram for semiconductor device DEV1. As shown in Figure 3, the manufacturing method for semiconductor device DEV1 includes a preparation step S1, an epitaxial growth step S2, a first insulating film formation step S3, an impurity region formation step S4, a second insulating film formation step S5, a first electrode formation step S6, a semi-insulating film formation step S7, a second electrode formation step S8, and a passivation film formation step S9.
[0030] Figure 4 is a cross-sectional view illustrating the preparation step S1. As shown in Figure 4, in the preparation step S1, the semiconductor substrate SUB is prepared. At this stage, the semiconductor substrate SUB has only an impurity region R1. Figure 5 is a cross-sectional view illustrating the epitaxial growth step S2. As shown in Figure 5, in the epitaxial growth step S2, an impurity region R2 is epitaxially grown on the impurity region R1. The formation of the impurity region R2 is carried out, for example, by the CVD (Chemical Vapor Deposition) method.
[0031] Figure 6 is a cross-sectional view illustrating the first insulating film formation step S3. As shown in Figure 6, the first insulating film ISL1 is formed in the first insulating film formation step S3. In the first insulating film formation step S3, firstly, the constituent material of the first insulating film ISL1 is deposited on the first surface FS by thermal oxidation or CVD. Secondly, the deposited constituent material of the first insulating film ISL1 is etched using a resist pattern formed by photolithography.
[0032] Figure 7 is a cross-sectional view illustrating the impurity region formation process S4. As shown in Figure 7, impurity regions R3, R4, and R5 are formed in the impurity region formation process S4. In the impurity region formation process S4, firstly, a resist pattern is formed on the first surface FS and the first insulating film ISL1 by photolithography. Secondly, ion implantation is performed from the first surface FS side using the resist pattern as a mask. Thirdly, the resist pattern is removed. Fourthly, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB. This forms impurity region R4. Impurity regions R3 and R5 are also formed by a similar process.
[0033] Figure 8 is a cross-sectional view illustrating the second insulating film formation step S5. As shown in Figure 8, the second insulating film ISL2 is formed in the second insulating film formation step S5. In the second insulating film formation step S5, firstly, the constituent material of the second insulating film ISL2 is deposited so as to cover the first insulating film ISL1, for example by CVD. Secondly, the constituent material of the deposited second insulating film ISL2 is etched using a resist pattern formed by photolithography.
[0034] Figure 9 is a cross-sectional view illustrating the first electrode formation step S6. As shown in Figure 9, the first electrode EL1 and the second electrode EL2 are formed in the first electrode formation step S6. In the first electrode formation step S6, firstly, the constituent material of the first electrode EL1 (second electrode EL2) is deposited on the first surface FS and the insulating film ISL, for example by sputtering. Secondly, the deposited constituent material of the first electrode EL1 (second electrode EL2) is etched using a resist pattern formed by photolithography.
[0035] Figure 10 is a cross-sectional view illustrating the semi-insulating film formation process S7. As shown in Figure 10, the semi-insulating film SIF is formed in the semi-insulating film formation process S7. In the semi-insulating film formation process S7, firstly, the constituent material of the semi-insulating film SIF is deposited, for example by CVD, so as to cover the first electrode EL1, the second electrode EL2, and the insulating film ISL. Secondly, the constituent material of the deposited semi-insulating film SIF is patterned by etching using a resist pattern formed by photolithography. The ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is controlled by adjusting the flow rate ratio of monosilane (SiH4) and nitrogen gas (N2) in the reaction gas when the CVD method is performed. The larger the value obtained by dividing the monosilane flow rate by the nitrogen gas flow rate, the larger the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF.
[0036] Figure 11 is a cross-sectional view illustrating the second electrode formation step S8. As shown in Figure 11, in the second electrode formation step S8, the third electrode EL3 is formed by depositing the constituent material of the third electrode EL3 on the second surface SS, for example, by sputtering. In the passivation film formation step S9, a passivation film PV is formed. In the passivation film formation step S9, firstly, the constituent material of the passivation film PV is deposited so as to cover the semi-insulating film SIF and the first electrode EL1. Secondly, the constituent material of the deposited passivation film PV is patterned by photolithography. Through these steps, the structure of the semiconductor device DEV1 shown in Figures 1 and 2 is formed.
[0037] In the above example of the manufacturing method, a semiconductor substrate SUB having only impurity region R1 was prepared in preparation step S1, but a semiconductor substrate SUB having only impurity region R2 may also be prepared in preparation step S1. In this case, the epitaxial growth step S2 is not performed, and impurity region R1 is formed by ion implantation from the second surface SS side. This formation of impurity region R1 by ion implantation is performed before the second electrode formation step S8.
[0038] <Variation> In the above example, an FRD is formed in the device region SUB1, but semiconductor devices other than FRDs may be formed in the device region SUB1. For example, an IGBT (Insulated Gate Bipolar Transistor) may be formed in the device region SUB1.
[0039] <Effects of Semiconductor Device DEV1> The effects of semiconductor device DEV1 are explained below in comparison with the semiconductor device of the comparative example. The configuration of the semiconductor device of the comparative example is the same as that of semiconductor device DEV1, except that the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is less than 0.64.
[0040] In semiconductor devices DEV1 and the comparative example, since the semi-insulating film SIF is semi-insulating, a weak leakage current flows through the semi-insulating film SIF, which relaxes the electric field in the semiconductor substrate SUB facing the semi-insulating film SIF via the insulating film ISL, thereby improving the breakdown voltage. At this time, electrons are induced and trapped in the semi-insulating film SIF.
[0041] Figure 12 is a graph showing the relationship between the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in a semi-insulating film (SIF) and the number of silicon-hydrogen bonds. The graph in Figure 12 was obtained by performing FT-IR (Fourier Transformation InfraRed spectroscopy) analysis on samples 1 to 6 of the semi-insulating film (SIF). The ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in each sample is highest in sample 1, followed by sample 2, sample 3, sample 4, sample 5, and sample 6. The ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in samples 1 to 3 is less than 0.64, while the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in samples 4 to 6 is 0.64 or higher.
[0042] As shown in Figure 12, silicon-hydrogen bonds were not detected in samples 1 to 3. On the other hand, peaks originating from silicon-hydrogen bonds were detected in samples 4 to 6. In other words, semiconductor device DEV1 contains amorphous silicon in the semi-insulating film SIF, while the semiconductor device in the comparative example does not contain amorphous silicon in the semi-insulating film SIF.
[0043] In the semiconductor device of the comparative example, the semi-insulating film SIF does not contain amorphous silicon, which is a good conductor of current. Therefore, electrons induced and trapped in the semi-insulating film SIF have difficulty escaping from the SIF. These electrons induced and trapped in the semi-insulating film SIF become a factor that causes fluctuations in breakdown voltage. On the other hand, in semiconductor device DEV1, the semi-insulating film SIF contains amorphous silicon, which is a good conductor of current. Therefore, induced and trapped electrons flow to the second electrode EL2 and can easily escape from the semi-insulating film SIF. As a result, semiconductor device DEV1 makes it possible to suppress fluctuations in breakdown voltage.
[0044] Figure 13 is a graph showing the relationship between the number of breakdown voltage measurements and the breakdown voltage. In Figure 13, Sample 2 from Figure 12 is used as the semi-insulating film SIF for the semiconductor device in the comparative example, while Sample 4 or Sample 6 is used as the semi-insulating film SIF for semiconductor device DEV1. The vertical axis of the graph in Figure 13 shows the difference between the breakdown voltage at the nth measurement (n is an integer between 1 and 10) and the breakdown voltage at the first measurement. The value on the vertical axis for the first measurement is (breakdown voltage at the first measurement) - (breakdown voltage at the first measurement), which is 0. As shown in Figure 13, in the semiconductor device in the comparative example, where the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is less than 0.64, the breakdown voltage fluctuates significantly with increasing numbers of measurements. On the other hand, in semiconductor device DEV1, where the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more, the fluctuation in breakdown voltage is small even with increasing numbers of measurements.
[0045] Figure 14 is a graph showing the relationship between the refractive index of the semi-insulating film (SIF) and the ratio of silicon atoms to the total number of silicon and nitrogen atoms in the SIF. As shown in Figure 14, as the refractive index of the SIF increases, the refractive index of the SIF and the ratio of silicon atoms to the total number of silicon and nitrogen atoms in the SIF also increase. More specifically, if the ratio of silicon atoms to the total number of silicon and nitrogen atoms in the SIF is 0.64 or higher, the refractive index of the SIF will be 2.55 or higher. Also, if the refractive index of the SIF and the ratio of silicon atoms to the total number of silicon and nitrogen atoms in the SIF are 0.74 or lower, the refractive index of the SIF will be 2.90 or lower. Thus, by setting the refractive index of the SIF to 2.55 or higher, the semiconductor device DEV1 can suppress fluctuations in breakdown voltage.
[0046] Figure 15 is a graph showing the relationship between the refractive index of the semi-insulating film SIF and the variation in the thickness T1 of the semi-insulating film SIF. As shown in Figure 15, when the refractive index of the semi-insulating film SIF exceeds 2.90, that is, when the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF exceeds 0.74, the variation in thickness T1 becomes large. On the other hand, when the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is within the range of 0.64 to 0.74, the variation in thickness T1 is 0.02 or less. From this, it can be seen that by keeping the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF between 0.64 and 0.74, it is possible to suppress variations in thickness T1 while suppressing fluctuations in breakdown voltage.
[0047] As the thickness T1 increases, current flows more easily through the semi-insulating film SIF, and induced and trapped electrons can escape more easily. On the other hand, if the thickness T1 is too large, the semi-insulating film SIF becomes hard, making it prone to cracking. Therefore, by setting the thickness T1 to between 50 nm and 1000 nm, it is possible to suppress cracking in the semi-insulating film SIF while suppressing fluctuations in breakdown voltage.
[0048] As the thickness T2 increases, the capacitance composed of the semi-insulating film SIF, insulating film ISL, and semiconductor substrate SUB decreases, suppressing fluctuations in breakdown voltage. On the other hand, if the thickness T2 is too large, the embedding of the first electrode EL1 and the second electrode EL2 deteriorates. Also, if the thickness T2 is too large, the step formed on the upper surface of the insulating film ISL becomes larger, and cracks are more likely to occur in the semi-insulating film SIF due to this step. Therefore, by setting the thickness T2 to 0.5 μm or more and 3.0 μm or less, it is possible to suppress fluctuations in breakdown voltage while suppressing the occurrence of cracks in the semi-insulating film SIF and the deterioration of the embedding of the first electrode EL1 and the second electrode EL2.
[0049] (Second Embodiment) The semiconductor device DEV2 according to the second embodiment will be described. Here, the differences from the semiconductor device DEV1 will be mainly explained, and redundant explanations will not be repeated.
[0050] <Configuration of Semiconductor Device DEV2> The configuration of the semiconductor device DEV2 is described below.
[0051] Figure 16 is a cross-sectional view of semiconductor device DEV2. Figure 16 shows a cross-section at the position corresponding to II-II in Figure 1. As shown in Figure 16, semiconductor device DEV2 comprises a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In semiconductor device DEV2, the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or higher. In these respects, the configuration of semiconductor device DEV2 is the same as that of semiconductor device DEV1.
[0052] In semiconductor device DEV2, the semi-insulating film SIF is placed on the insulating film ISL. More specifically, in semiconductor device DEV2, the semi-insulating film SIF is placed inside a step formed on the upper surface of the insulating film ISL. In semiconductor device DEV2, the semi-insulating film SIF has an inner peripheral edge SIFa and an outer peripheral edge SIFb. The inner peripheral edge SIFa and the outer peripheral edge SIFb are covered by the first electrode EL1 and the second electrode EL2, respectively. In these respects, the configuration of semiconductor device DEV2 differs from the configuration of semiconductor device DEV1.
[0053] <Variation> In the above, an example was described in which the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more. However, in semiconductor device DEV2, the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF may be less than 0.64. Furthermore, in semiconductor device DEV2, the semi-insulating film SIF may be formed from a material other than one containing silicon and nitrogen (for example, polycrystalline silicon).
[0054] <Manufacturing method for semiconductor device DEV2> The manufacturing method for the semiconductor device DEV2 is described below.
[0055] Figure 17 is a manufacturing process diagram for semiconductor device DEV2. As shown in Figure 17, the manufacturing method for semiconductor device DEV2 includes a preparation step S1, an epitaxial growth step S2, a first insulating film formation step S3, an impurity region formation step S4, a second insulating film formation step S5, a first electrode formation step S6, a semi-insulating film formation step S7, a second electrode formation step S8, and a passivation film formation step S9. In this respect, the manufacturing method for semiconductor device DEV2 is the same as that for semiconductor device DEV1.
[0056] In the manufacturing method of semiconductor device DEV2, the semi-insulating film formation step S7 is performed after the second insulating film formation step S5. In the manufacturing method of semiconductor device DEV2, the first electrode formation step S6 is performed after the semi-insulating film formation step S7. In this respect, the manufacturing method of semiconductor device DEV2 differs from the manufacturing method of semiconductor device DEV1.
[0057] <Effects of Semiconductor Device DEV2> The effects of the semiconductor device DEV2 are explained below.
[0058] Steps are formed on the upper surface of the insulating film ISL. As a result, in semiconductor device DEV1, steps are also formed on the upper surfaces of the first electrode EL1 and the second electrode EL2, and the semi-insulating film SIF may be placed on top of these steps. Stress concentration is likely to occur near such steps, so cracks are likely to occur in the semi-insulating film SIF in semiconductor device DEV1. The semi-insulating film SIF becomes more brittle as its silicon composition ratio increases, so when the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or higher, the occurrence of such cracks is a concern.
[0059] On the other hand, in semiconductor device DEV2, the inner peripheral edge SIFa and the outer peripheral edge SIFb are covered by the first electrode EL1 and the second electrode EL2, respectively. In other words, in semiconductor device DEV2, there are no portions where the semi-insulating film SIF is located on the first electrode EL1 and the second electrode EL2. Therefore, in semiconductor device DEV2, the semi-insulating film SIF is not affected by the steps formed on the upper surfaces of the first electrode EL1 and the second electrode EL2, and cracks are less likely to occur in the semi-insulating film SIF.
[0060] (Third embodiment) The semiconductor device DEV3 according to the third embodiment will be described. Here, the differences from the semiconductor device DEV1 will be mainly explained, and redundant explanations will not be repeated.
[0061] <Configuration of Semiconductor Device DEV3> The configuration of semiconductor device DEV3 is described below.
[0062] Figure 18 is a cross-sectional view of semiconductor device DEV3. Figure 18 shows a cross-section at the position corresponding to II-II in Figure 1. As shown in Figure 18, semiconductor device DEV3 comprises a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In semiconductor device DEV3, the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or higher. In these respects, the configuration of semiconductor device DEV3 is the same as that of semiconductor device DEV1.
[0063] In semiconductor device DEV3, a recess RCS1 is formed on the first surface FS. The first surface FS is recessed toward the second surface SS in the recess RCS1. The recess RCS1 is positioned so as to overlap with the impurity region R4 in a plan view. The recess RCS1 may extend adjacent to the impurity region R5. In semiconductor device DEV3, the first insulating film ISL1 is embedded in the recess RCS1, and the second insulating film ISL2 is positioned on the first surface FS in the terminal region SUB2 so as to cover the first insulating film ISL1. In semiconductor device DEV3, the first insulating film ISL1 is thicker than, for example, the second insulating film ISL2. In these respects, the configuration of semiconductor device DEV3 differs from the configuration of semiconductor device DEV1.
[0064] <Variation> In the above, an example was described in which the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more. However, in semiconductor device DEV3, the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF may be less than 0.64. Furthermore, in semiconductor device DEV3, the semi-insulating film SIF may be formed from a material other than one containing silicon and nitrogen (for example, polycrystalline silicon).
[0065] <Manufacturing method for semiconductor device DEV3> The manufacturing method for the semiconductor device DEV3 is described below.
[0066] Figure 19 is a manufacturing process diagram for semiconductor device DEV3. As shown in Figure 19, the manufacturing method for semiconductor device DEV3 includes a preparation step S1, an epitaxial growth step S2, a first insulating film formation step S3, a second insulating film formation step S5, a first electrode formation step S6, a semi-insulating film formation step S7, a second electrode formation step S8, and a passivation film formation step S9. In this respect, the manufacturing method for semiconductor device DEV3 is the same as that for semiconductor device DEV1.
[0067] The manufacturing method for semiconductor device DEV3 includes a first impurity region formation step S10 and a second impurity region formation step S11 instead of the impurity region formation step S4.
[0068] The first impurity region formation step S10 is performed after the epitaxial growth step S2. Figure 20 is a cross-sectional view illustrating the first impurity region formation step S10. As shown in Figure 20, an impurity region R4 is formed in the first impurity region formation step S10. In the first impurity region formation step S10, firstly, a resist pattern is formed on the first surface FS by photolithography. Secondly, ion implantation is performed from the first surface FS side using the resist pattern as a mask. Thirdly, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB.
[0069] In the manufacturing method of semiconductor device DEV3, the first insulating film formation step S3 is performed after the first impurity region formation step S10. Figure 21 is a cross-sectional view illustrating the first insulating film formation step S3 in the manufacturing method of semiconductor device DEV3. As shown in Figure 21, in the manufacturing method of semiconductor device DEV3, recess RCS1 and first insulating film ISL1 are formed in the first insulating film formation step S3. In the manufacturing method of semiconductor device DEV2, in the first insulating film formation step S3, firstly, a resist pattern is formed on the first surface FS by photolithography. Secondly, recess RCS1 is formed by etching the first surface FS using the resist pattern as a mask. Thirdly, polycrystalline silicon is partially embedded in the recess RCS1, for example by CVD. Fourthly, the embedded polycrystalline silicon is thermally oxidized to become the first insulating film ISL1. If the first insulating film ISL1 extends beyond the recess RCS1, the excess first insulating film ISL1 may be removed by CMP (Chemical Mechanical Polishing). In the above example, the first insulating film ISL1 was formed by partially embedding polycrystalline silicon in the recess RCS1 and then performing thermal oxidation. However, the first insulating film ISL1 may also be formed by thermal oxidation alone.
[0070] In the manufacturing method of semiconductor device DEV3, the second impurity region formation step S11 is performed after the first insulating film formation step S3. Figure 22 is a cross-sectional view illustrating the second impurity region formation step S11. As shown in Figure 22, impurity region R3 and impurity region R5 are formed in the second impurity region formation step S11. In the second impurity region formation step S11, firstly, ion implantation is performed from the first surface FS side using the first insulating film ISL1 as a mask. Secondly, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB.
[0071] In the manufacturing method of semiconductor device DEV3, the second impurity region formation step S11 is followed sequentially by the second insulating film formation step S5, the first electrode formation step S6, the semi-insulating film formation step S7, the second electrode formation step S8, and the passivation film formation step S9.
[0072] <Effects of Semiconductor Device DEV3> The effects of the semiconductor device DEV3 are explained below.
[0073] In semiconductor device DEV3, the first insulating film ISL1 is embedded in the recess RCS1, and the second insulating film ISL2 is positioned to cover the first insulating film ISL1. As a result, steps are less likely to form on the upper surface of the insulating film ISL, and consequently on the upper surfaces of the first electrode EL1 and the second electrode EL2. Therefore, with semiconductor device DEV3, even if the semi-insulating film SIF is positioned on the first electrode EL1 and the second electrode EL2, cracks caused by stress concentration are less likely to occur in the semi-insulating film SIF.
[0074] In semiconductor device DEV3, impurity region R4 is formed before the first insulating film ISL1 is formed, so ion implantation to form impurity region R4 is performed without going through the first insulating film ISL1. Therefore, in semiconductor device DEV3, it is possible to lower the acceleration voltage when performing ion implantation to form impurity region R4. In addition, in semiconductor device DEV3, the first insulating film ISL1 can be used as a mask when ion implanting to form impurity regions R3 and R5, so it is not necessary to separately form a resist pattern for ion implantation to form impurity regions R3 and R5, and the process can be simplified.
[0075] (Fourth Embodiment) The semiconductor device DEV4 according to the fourth embodiment will now be described. Here, we will mainly explain the differences from the semiconductor device DEV3, and will avoid repeating redundant explanations.
[0076] <Configuration of semiconductor device DEV4> The configuration of semiconductor device DEV4 is described below.
[0077] Figure 23 is a cross-sectional view of semiconductor device DEV4. Figure 23 shows a cross-section at the position corresponding to II-II in Figure 1. As shown in Figure 23, semiconductor device DEV4 comprises a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In semiconductor device DEV4, the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or higher. In these respects, the configuration of semiconductor device DEV4 is the same as that of semiconductor device DEV3.
[0078] In semiconductor device DEV4, multiple recesses RCS2 and RCS3 are formed on the first surface FS. The first surface FS is recessed toward the second surface SS in recesses RCS2 and RCS3. The multiple recesses RCS2 are arranged to overlap with the impurity region R4 in a plan view. The multiple recesses RCS2 are spaced apart along the direction from the device region SUB1 to the termination region SUB2. Recess RCS3 is located between the outermost recess RCS2 and the impurity region R5 in the direction from the device region SUB1 to the termination region SUB2. Recess RCS3 may extend adjacent to the impurity region R5.
[0079] In semiconductor device DEV4, the first insulating film ISL1 is embedded in each of the multiple recesses RCS2 and recess RCS3, and the second insulating film ISL2 is arranged on the first surface FS in the terminal region SUB2 so as to cover the first insulating film ISL1. In these respects, the configuration of semiconductor device DEV4 differs from that of semiconductor device DEV3.
[0080] <Variation> In the above, an example was described in which the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more. However, in semiconductor device DEV4, the ratio of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF may be less than 0.64. Furthermore, in semiconductor device DEV4, the semi-insulating film SIF may be formed from a material other than one containing silicon and nitrogen (for example, polycrystalline silicon).
[0081] Figure 24 is a manufacturing process diagram for semiconductor device DEV4. As shown in Figure 24, the manufacturing method for semiconductor device DEV4 includes a preparation step S1, an epitaxial growth step S2, a first insulating film formation step S3, a second insulating film formation step S5, a first electrode formation step S6, a semi-insulating film formation step S7, a second electrode formation step S8, and a passivation film formation step S9. In this respect, the manufacturing method for semiconductor device DEV4 is the same as that for semiconductor device DEV3.
[0082] In the manufacturing method of semiconductor device DEV4, the first insulating film formation step S3 is performed after the epitaxial growth step S2. Figure 25 is a cross-sectional view illustrating the first insulating film formation step S3 in the manufacturing method of semiconductor device DEV4. As shown in Figure 25, in the manufacturing method of semiconductor device DEV4, a plurality of recesses RCS2, recesses RCS3 and the first insulating film ISL1 are formed in the first insulating film formation step S3.
[0083] In the first insulating film formation step S3 of the manufacturing method for semiconductor device DEV4, firstly, a resist pattern is formed on the first surface FS by photolithography. Secondly, multiple recesses RCS2 and RCS3 are formed by etching the first surface FS using the resist pattern as a mask. Thirdly, polycrystalline silicon is partially embedded in the multiple recesses RCS2 and RCS3, for example by CVD. Fourthly, the embedded polycrystalline silicon is thermally oxidized to form the first insulating film ISL1. If the first insulating film ISL1 extends beyond the recesses RCS1, the excess first insulating film ISL1 may be removed by CMP.
[0084] The manufacturing method for semiconductor device DEV4 includes a third impurity region formation step S12 instead of the first impurity region formation step S10. The third impurity region formation step S12 is performed after the first insulating film formation step S3. Figure 26 is a cross-sectional view illustrating the third impurity region formation step S12. As shown in Figure 26, an impurity region R4 is formed in the third impurity region formation step S12. In the third impurity region formation step S12, firstly, ion implantation is performed from the first surface FS side using the first insulating film ISL1 as a mask. This implants impurity ions between two adjacent recesses RCS2. Thirdly, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB.
[0085] The manufacturing method for semiconductor device DEV4 includes a fourth impurity region formation step S13 instead of the second impurity region formation step S11. The fourth impurity region formation step S13 is performed after the third impurity region formation step S12. Figure 27 is a cross-sectional view illustrating the fourth impurity region formation step S13. As shown in Figure 27, impurity region R3 and impurity region R5 are formed in the fourth impurity region formation step S13. In the fourth impurity region formation step S13, firstly, a resist pattern is formed on the first surface FS by photolithography. Secondly, ion implantation is performed from the first surface FS side using the resist pattern as a mask. Thirdly, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB.
[0086] In the manufacturing method of semiconductor device DEV4, the second insulating film formation step S5, the first electrode formation step S6, the semi-insulating film formation step S7, the second electrode formation step S8, and the passivation film formation step S9 are carried out sequentially after the fourth impurity region formation step S13.
[0087] In semiconductor device DEV4, the first insulating film ISL1 is embedded in recesses RCS2 and RCS3, and the second insulating film ISL2 is positioned to cover the first insulating film ISL1. As a result, steps are less likely to form on the upper surface of the insulating film ISL, and consequently on the upper surfaces of the first electrode EL1 and the second electrode EL2. Therefore, with semiconductor device DEV4, even if the semi-insulating film SIF is positioned on the first electrode EL1 and the second electrode EL2, cracks caused by stress concentration are less likely to occur in the semi-insulating film SIF.
[0088] In semiconductor device DEV3, ion implantation to form the impurity region R4 is performed between two adjacent recesses RCS2 without going through the first insulating film ISL1. Therefore, in semiconductor device DEV3, it is possible to lower the acceleration voltage when performing ion implantation to form the impurity region R4. In semiconductor device DEV4, the first insulating film ISL1 can be used as a mask during ion implantation to form the impurity region R4, eliminating the need to separately form a resist pattern for ion implantation to form the impurity region R4, thus simplifying the process.
[0089] Although the present invention has been specifically described above based on embodiments, it goes without saying that the present invention is not limited to the above embodiments and can be modified in various ways without departing from its essence. [Explanation of Symbols]
[0090] DEV1,DEV2,DEV3,DEV4 Semiconductor device, EL1 1st electrode, EL1a outer edge, EL2 2nd electrode, EL3 3rd electrode, FS 1st surface, ISL insulation film, ISL1 1st insulation film, ISL2 2nd insulation film, OP1, OP2 opening, PV passivation film, R1,R2,R3,R4,R5 Impurity region, RCS1, RCS2, RCS3 recess, S1 preparation process, S2 epitaxial growth process, S3 first insulating film forming process, S4 impurity region forming process, S5 second insulating film forming process, S6 first electrode forming process, S7 forming process, S8 second electrode forming process, S9 passivation film forming process, S10 first impurity region forming process, S11 Second impurity region formation step, S12 Third impurity region formation step, S13 Fourth impurity region formation step, SIF semi-insulating film, SIFa Inner peripheral edge, SIFb outer peripheral edge, SS second surface, SUB semiconductor substrate, SUB1 element region, SUB2 termination region, T1, T2, T3 thickness.
Claims
1. Semiconductor substrate and insulating film and First electrode and second electrode, It comprises a semi-insulating film, The semiconductor substrate has a first surface, The semiconductor substrate, in a plan view, has an element region and a termination region surrounding the element region. The semiconductor substrate has a first impurity region formed on the first surface in the terminal region, The insulating film covers the first surface in the terminal region, The first electrode is electrically connected to the first impurity region and faces the first impurity region with the insulating film in between. The second electrode is arranged on the insulating film such that, in a plan view, it surrounds the first electrode while being spaced apart from it. The aforementioned semi-insulating film is arranged to straddle the insulating film located between the first electrode and the second electrode in a plan view. The aforementioned semi-insulating film contains silicon and nitrogen. In the aforementioned semi-insulating film, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms is 0.64 or more. The semiconductor device wherein the semi-insulating film is a mixed crystal of silicon nitride and amorphous silicon.
2. The semiconductor device according to claim 1, wherein in the semi-insulating film, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms is 0.74 or less.
3. The semiconductor device according to claim 1, wherein a portion of the silicon in the semi-insulating film is bonded to hydrogen.
4. The semiconductor device according to claim 1, wherein the thickness of the semi-insulating film is 50 nm or more and 1000 nm or less.
5. The semiconductor device according to claim 1, wherein the thickness of the insulating film is 0.5 μm or more and 3.0 μm or less.
6. The semiconductor device according to claim 1, wherein the first electrode and the second electrode are electrically connected by the semi-insulating film.
7. The semiconductor substrate has a second impurity region formed on the first surface in the element region, The first electrode is connected to the second impurity region, The semiconductor device according to claim 1, wherein the impurity concentration in the second impurity region is higher than the impurity concentration in the first impurity region.
8. The semiconductor device according to claim 1, further comprising a passivation film formed to cover the semi-insulating film.
9. The first electrode has an outer peripheral edge, The aforementioned semi-insulating film has an inner peripheral edge, The aforementioned semi-insulating film covers the second electrode, The semiconductor device according to claim 1, wherein the inner peripheral edge covers the outer peripheral edge.
10. The aforementioned semi-insulating film has an inner peripheral edge and an outer peripheral edge. The semiconductor device according to claim 1, wherein the first electrode and the second electrode each cover the inner peripheral edge and the outer peripheral edge, respectively.
11. The semiconductor substrate has a second surface that is opposite to the first surface in the thickness direction of the semiconductor substrate, The first surface has a first recess formed therein that is recessed toward the second surface, so as to overlap with the first impurity region in a plan view. The semiconductor device according to claim 1, wherein the insulating film comprises a first insulating film embedded in the first recess and a second insulating film disposed on the first surface so as to cover the first insulating film.
12. The semiconductor device according to claim 11, wherein the first insulating film is thicker than the second insulating film.
13. The semiconductor substrate has a second surface that is opposite to the first surface in the thickness direction of the semiconductor substrate, The first surface has a plurality of second recesses formed therein that are recessed toward the second surface so as to overlap with the first impurity region in a plan view. The plurality of second recesses are arranged at intervals along the direction from the element region toward the termination region, The semiconductor device according to claim 1, wherein the insulating film comprises a first insulating film embedded in each of the plurality of second recesses and a second insulating film disposed on the first surface so as to cover the first insulating film.
14. The semiconductor device according to claim 1, wherein an FRD is formed in the element region.
15. The semiconductor device according to claim 1, wherein an IGBT is formed in the element region.
Citation Information
Patent Citations
High withstand voltage planar element
JP1991171774A
High breakdown strength semiconductor device
JP1999214670A
Semiconductor device
JP2018147937A
Semiconductor device
JP2021068833A
Semiconductor device
JP2022074323A