Semiconductor equipment
By employing a control transistor with an oxide semiconductor channel and a comparator circuit, the memory device addresses the issues of large circuit area and high power consumption, achieving stable data storage with reduced power usage.
Patent Information
- Application Number
- JP2025140679
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2011-05-19
- Filing Date
- 2025-08-26
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2032-04-10
AI Technical Summary
Conventional associative memory devices face issues such as large circuit area, high power consumption due to leakage current, and data instability, particularly when power is interrupted.
The use of a control transistor with an oxide semiconductor channel and reduced transistor count, along with a comparator circuit to manage data storage and retrieval, minimizes circuit area and leakage current, ensuring data stability even when power is interrupted.
This configuration reduces circuit area, stabilizes stored data, and lowers power consumption by allowing power to be intermittently supplied, enhancing the efficiency and reliability of the memory device.
Smart Images

Figure 0007955454000007 
Figure 0007955454000008 
Figure 0007955454000009
Abstract
Description
[Technical Field]
[0001] One embodiment of the present invention relates to a memory device. [Background Art]
[0002] In recent years, memory devices capable of rewriting data have been developed.
[0003] Examples of the memory device include an associative memory.
[0004] An associative memory is a memory device that can not only rewrite data but also determine what kind of data is stored in a memory cell with respect to search data. .
[0005] An associative memory is used for, for example, a set associative cache memory. The set associative method is a data storage structure composed of a plurality of tags, and an associative memory is used as the tag. By using an associative memory for the cache memory, data communication between the CPU and the cache memory can be accelerated.
[0006] A memory cell in the associative memory is configured using, for example, a storage circuit that holds data and a plurality of comparison circuits that compare data stored in the storage circuit with specific data (for example, Patent Document 1).
[0007] In Patent Document 1, data can be determined even for multi-bit data by a magnitude comparison circuit and a coincidence detection circuit. [Prior Art Document] [Patent Document]
[0008] [Patent Document 1] Japanese Patent Publication No. 2004-295967 [Overview of the Initiative] [Problems that the invention aims to solve]
[0009] Conventional associative memory had problems such as the large circuit area required for each memory cell. For example, in the associative memory shown in Patent Document 1, the number of transistors in each memory cell is 11. There are many, and the circuit area is large.
[0010] Furthermore, in conventional associative memory, the leakage current of the transistor in the off state is used for retention. There was a problem where the data stored in the memory cell would change depending on the state. For example, in the associative memory shown in Patent Document 1, when the power supply is stopped, the transistor's regeneration Data can be lost due to current surges, etc. Therefore, the power supply must be turned off while data is being retained. The supply must continue, which leads to higher power consumption.
[0011] In one aspect of the present invention, the circuit area is reduced, and the memory cell is stored in the retention state. One of the challenges is to suppress fluctuations in stored data. [Means for solving the problem]
[0012] In one aspect of the present invention, a comparison circuit compares data stored in a memory cell with retrieval data, A control transistor is used to control the settings of the data stored in the memory cell. By configuring this, the number of transistors in the memory cell is reduced, and the circuit area is reduced. To measure small.
[0013] Furthermore, in one aspect of the present invention, the control transistor is a wide-gear semiconductor such as an oxide semiconductor. By using a field-effect transistor that includes a channel formation layer using a CAP semiconductor, Reduces the leakage current of the control transistor when it is off, and the control transistor is in the off state. At that time, the aim is to suppress fluctuations in the data stored in the memory cell. By suppressing data fluctuations, for example, while retaining data in memory cells, power supply Since the power supply can be stopped as needed, power consumption can also be reduced.
[0014] One aspect of the present invention is a memory cell for storing data as memory data, an output signal line, and an electric The memory cell is equipped with wiring to which pressure is applied, and performs a comparison operation between stored data and retrieved data. When the value of the stored data is smaller than the value of the searched data, a conduction state is reached, and the stored data When the value matches the search data, or when the value of the stored data is greater than the value of the search data, A comparator circuit that becomes non-conductive at that time, and an electric field effect circuit that controls the writing and retention of stored data. It includes a transistor, and when the comparison circuit is in a conducting state, the voltage value of the output signal line is equal to the voltage of the wiring. It is a memory device that will have a value equivalent to [the other value].
[0015] One aspect of the present invention is a memory cell for storing data as memory data, an output signal line, and an electric The memory cell is equipped with wiring to which pressure is applied, and performs a comparison operation between stored data and retrieved data. When the value of the stored data is greater than the value of the searched data, a conductive state is reached, and the stored data When the value matches the search data, or when the value of the stored data is less than the value of the search data, A comparator circuit that becomes non-conductive at that time, and an electric field effect circuit that controls the writing and retention of stored data. It includes a transistor, and when the comparison circuit is in a conducting state, the voltage value of the output signal line is equal to the voltage of the wiring. It is a memory device that will have a value equivalent to [the other value].
[0016] Furthermore, one aspect of the present invention is an N-stage system in which each of the N-stage systems stores 1 bit of data as stored data. A memory cell (where N is a natural number greater than or equal to 2), a first output signal line, a second output signal line, and It has a voltage supply line and first to N-1 connecting lines, and each of the N stages of memory cells is Perform a first comparison operation between 1 bit of stored data and 1 bit of retrieved data, and store 1 bit. Conduction occurs when the data value is smaller than the value of the 1-bit search data. When the value of the stored data matches the 1-bit search data, or when the value of the stored data is 1 bit A first comparator circuit that becomes non-conductive when is greater than the value of 1 bit of search data, and 1 A second comparison operation is performed between the stored bit data and the 1-bit search data, and the 1-bit stored data When the value of the data is smaller than the value of the 1-bit search data, or when the value of the 1-bit stored data is smaller than the value of the search data. When it matches the value of 1 bit of search data, it enters a conductive state, and 1 bit of stored data A second comparator circuit that becomes non-conductive when its value is greater than the value of the 1-bit search data, It comprises a field-effect transistor that controls the writing and holding of 1-bit memory data, The first comparison circuit of the first-stage memory cell becomes either conductive or non-conductive, thereby... It has the function of controlling the electrical connection between the voltage supply line and the first output signal line, and the first stage memory cell The second comparison circuit, by becoming conductive or non-conductive, connects the voltage supply line to the first contact. It has a function to control the electrical connection with the subsequent wiring, and is the Kth stage (K is a natural number between 2 and N-1). The first comparison circuit of the memory cell becomes either conductive or non-conductive, which determines the K-1 It has a function to control the electrical connection between the connection wiring and the first output signal line, and the K-stage memory The second comparison circuit of the first K-1 connection wiring becomes either conductive or non-conductive depending on whether it is in a conductive or non-conductive state. It has the function of controlling the electrical connection between the Kth connecting wire and the first ratio of the Nth memory cell. The comparison circuit, by being in a conductive or non-conductive state, connects the N-1 connection wiring to the first output The second comparison circuit of the Nth stage memory cell has a function to control the electrical connection with the signal line, By becoming conductive or non-conductive, the connection between the N-1 connection wiring and the second output signal line It is a storage device that has a function to control electrical connections.
[0017] Furthermore, one aspect of the present invention is an N-stage system in which each of the N-stage systems stores 1 bit of data as stored data. A memory cell (where N is a natural number greater than or equal to 2), a first output signal line, a second output signal line, and It has a voltage supply line and first to N-1 connecting lines, and each of the N stages of memory cells is Perform a first comparison operation between 1 bit of stored data and 1 bit of retrieved data, and store 1 bit. Conduction occurs when the data value is greater than the value of the 1-bit search data, and 1 bit When the value of the stored data matches the 1-bit search data, or when the value of the stored data is 1 bit A first comparator circuit that becomes non-conductive when it is smaller than the value of a 1-bit search data, and 1 A second comparison operation is performed between the stored bit data and the 1-bit search data, and the 1-bit stored data When the value of the data is greater than the value of the 1-bit search data, or when the value of the 1-bit stored data is greater than the value of the search data. When it matches the value of 1 bit of search data, it enters a conductive state, and 1 bit of stored data A second comparator circuit that becomes non-conductive when its value is smaller than the value of the 1-bit search data, It comprises a field-effect transistor that controls the writing and holding of 1-bit memory data, The first comparison circuit of the first-stage memory cell becomes either conductive or non-conductive, thereby... It has the function of controlling the electrical connection between the voltage supply line and the first output signal line, and the first stage memory cell The second comparison circuit, by becoming conductive or non-conductive, connects the voltage supply line to the first contact. It has a function to control the electrical connection with the subsequent wiring, and is the Kth stage (K is a natural number between 2 and N-1). The first comparison circuit of the memory cell becomes either conductive or non-conductive, which determines the K-1 It has a function to control the electrical connection between the connection wiring and the first output signal line, and the K-stage memory The second comparison circuit of the first K-1 connection wiring becomes either conductive or non-conductive depending on whether it is in a conductive or non-conductive state. It has the function of controlling the electrical connection between the Kth connecting wire and the first ratio of the Nth memory cell. The comparison circuit, by being in a conductive or non-conductive state, connects the N-1 connection wiring to the first output The second comparison circuit of the Nth stage memory cell has a function to control the electrical connection with the signal line, By becoming conductive or non-conductive, the connection between the N-1 connection wiring and the second output signal line It is a storage device that has a function to control electrical connections.
[0018] In the above embodiment of the present invention, a field-effect transistor is formed in an oxide semiconductor where a channel is formed. The structure may also include layers. [Effects of the Invention]
[0019] According to one aspect of the present invention, the number of transistors in a memory cell is reduced, and the circuit area is reduced. It can be cut. Also, according to one aspect of the present invention, the control transistor is in the off state. This allows for the suppression of fluctuations in the data stored in the memory cell. [Brief explanation of the drawing]
[0020] [Figure 1] A diagram illustrating an example of a storage device. [Figure 2] A diagram illustrating an example of a storage device. [Figure 3] A diagram illustrating an example of a storage device. [Figure 4] A diagram illustrating an example of a storage device. [Figure 5] A schematic cross-sectional diagram showing an example of transistor structure. [Figure 6] A schematic cross-sectional diagram illustrating an example of a transistor fabrication method. [Figure 7] A diagram illustrating an example of a storage device structure. [Figure 8] A diagram illustrating an example of a processing unit. [Figure 9] A diagram illustrating an example of an electronic device. [Figure 10] A diagram illustrating the crystal structure of oxide materials. [Figure 11] A diagram illustrating the crystal structure of oxide materials. [Figure 12] A diagram illustrating the crystal structure of oxide materials. [Figure 13] A diagram illustrating the gate voltage dependence of the mobility obtained through calculation. [Figure 14] A diagram illustrating the gate voltage dependence of drain current and mobility obtained through calculations. [Figure 15] A diagram illustrating the gate voltage dependence of drain current and mobility obtained through calculations. [Figure 16] A diagram illustrating the gate voltage dependence of drain current and mobility obtained through calculations. [Figure 17] A diagram illustrating the cross-sectional structure of the transistor used in the calculations. [Figure 18] A diagram showing the characteristics of a transistor. [Figure 19] A diagram showing the characteristics of a transistor. [Figure 20] A diagram showing the characteristics of a transistor. [Figure 21] A diagram showing the characteristics of a transistor. [Figure 22] A diagram showing the characteristics of a transistor. [Figure 23] A figure showing the XRD spectrum of an oxide material. [Figure 24] A diagram showing the characteristics of a transistor. [Figure 25] Cross-sectional and plan views of a semiconductor device. [Figure 26] Cross-sectional and plan views of a semiconductor device. [Modes for carrying out the invention]
[0021] An example of an embodiment illustrating the present invention will be described below with reference to the drawings. The contents of the embodiments may be modified without departing from the spirit and scope of the present invention. This will be easy for those skilled in the art. Therefore, the present invention is not limited to the embodiments described below. It will not be done.
[0022] Furthermore, the contents of each embodiment can be combined with each other as appropriate. The contents of these can be interchanged.
[0023] Furthermore, ordinal numbers such as 1st, 2nd, etc. are added to avoid confusion of the constituent elements, and each constituent element The number is not limited to ordinal numbers.
[0024] (Embodiment 1) This embodiment describes an example of a storage device capable of discriminating stored data.
[0025] The storage device in this embodiment comprises a memory cell and an output signal line. The process involves comparing stored data (also called stored data) with retrieved data. It has a function to identify the stored data and is provided, for example, in a memory cell array. The number of memory cells may be multiple. Furthermore, the stored data and retrieval data are as follows: One bit of data can be used. Additionally, the output signal line is used for comparison in the memory cell. This wiring sets a voltage value according to the calculation. The voltage of the output signal line mentioned above becomes the output signal.
[0026] Furthermore, examples of memory cells will be explained using Figures 1 and 2.
[0027] As shown in Figures 1 and 2(A), the memory cell is connected to the comparator circuit 101 (also called Comp1). It comprises a comparator circuit 102 (also called Comp2) and a transistor 131. Oh, it is not always necessary to provide the comparison circuit 102, but for example, if the memory device has multiple memory cells If the device is equipped with such a feature, a comparison circuit 102 is provided to distinguish between multiple bits of data. A memory device can be configured. In this case, the comparison circuit 102 is shown in Figures 1 and 2(A). It controls the conductivity between the indicated memory cell and other memory cells.
[0028] For example, a field-effect transistor can be used as the transistor.
[0029] The comparison circuit 101 compares the stored data (also called data Dm) stored in the memory cell with the search results. The first comparison operation is performed using the data (also called data Dsch), and the output is determined according to the result of the operation. It has a function to control whether or not to change the voltage value of the power signal line OUT. For example, a comparator circuit. 101 is the power of the output signal line OUT when the value of data Dm is less than the value of data Dsch. Function to change the pressure value, or output when the value of data Dm is greater than the value of data Dsch. It has the function of changing the voltage value of the signal line OUT.
[0030] The comparator circuit 101 can be constructed using transistors. For example, as shown in Figure 2(A) As shown, the comparison circuit 101 comprises transistor 111 and transistor 112. In this case, transistor 111 is an N-channel transistor, 112 is a P-channel transistor. Source and drain of transistor 111. On one side, a voltage Vx is applied, and the gate voltage of transistor 111 is the data Dsch This is the result. Also, one of the sources and drains of transistor 112 is connected to transistor 111. The source and drain of transistor 112 are electrically connected to the other side. The other end of the input is electrically connected to the output signal line OUT, and the gate of transistor 112 is electrically connected. The pressure becomes the data Dm.
[0031] The comparison circuit 102 compares the stored data (data Dm) stored in the memory cell with the search data ( It has the function to perform a second comparison operation using data Dsch).
[0032] The comparator circuit 102 can be constructed using transistors. For example, as shown in Figure 2(A) As shown, the comparison circuit 102 comprises transistor 121 and transistor 122. In this case, transistor 121 is an N-channel transistor, 122 is a P-channel transistor. Source and drain of transistor 121. On one side, a voltage Vx is applied, and the gate voltage of transistor 121 is the data Dsch This is the result. Also, one of the sources and drains of transistor 122 is connected to transistor 121. It is electrically connected to one of the source and drain of transistor 122. The other end of the input is electrically connected to the other end of the source and drain of transistor 121. The gate voltage of transistor 122 becomes the data Dm. The value of voltage Vx is obtained from comparator circuit 101. The polarity of the transistor in the comparison circuit 102 is set appropriately.
[0033] Transistor 131 has the function of controlling the writing and holding of data Dm. For example A data signal is input to either the source or drain of transistor 131. The source and drain of transistor 131 are connected to transistor 112 (comparison circuit 101). It is electrically connected to the gate and the gate of transistor 122 (comparison circuit 102). Transistor 131 is also called a control transistor. Furthermore, a capacitive element is provided in the memory cell, and the transistor... One of the pair of electrodes of the capacitive element is electrically connected to the source and the other of the drain of the converter 131. It may be continued. In this case, the voltage of the other electrode of the pair of electrodes of the capacitive element is equal to the ground potential. Alternatively, the voltage will be any value.
[0034] The transistor 131 is, for example, a transistor including an oxide semiconductor layer in which a channel is formed. DISTRAs and the like can be used. The above oxide semiconductor layer has a band gap greater than silicon. The voltage is high, for example, 2 eV or more, preferably 2.5 eV or more, more preferably 3 eV or more. ru.
[0035] Furthermore, the transistor containing the above oxide semiconductor layer has a low off-current and a channel width of 1 μm. 10aA per unit (1 × 10 -17 A) Preferably 1 aA per 1 μm of channel width 1 x 10 -18 A) More preferably, 10 zA (1 × 10) per 1 μm of channel width. -20 A) More preferably, 1 zA (1 × 10⁻¹⁶) per 1 μm of channel width. -21 A) More preferably, 100 yA (1 × 10⁻¹⁶) per 1 μm of channel width. -22 A) Below be.
[0036] Furthermore, as shown in Figures 1 and 2(A), for example, the storage device in this embodiment is It comprises a Data line and a Word line.
[0037] Data lines are wiring used for exchanging data with memory cells. A data signal is input to the Data line. For example, the Data line shown in Figure 2(A) This refers to the gate of transistor 111, the gate of transistor 121, and transistor 1 It is electrically connected to either the source or drain of 31. This reduces the number of wires. This can be done. Furthermore, one of the source and drain of transistor 131 is connected to the data line D. Instead of ATA, you can electrically connect to another wire. In this case, the data line Data One wire receives the first data signal, and another wire receives the second data signal. Another type of wiring is also called a bit line.
[0038] The Word line is a signal that controls the writing and retention of data in the memory cell. This is the wiring that is powered. The Word wire is electrically connected to the gate of transistor 131. It will be done.
[0039] In general, voltage refers to the difference in electric potential between two points (also called potential difference). However, voltage and potential values are both expressed in volts (V) in circuit diagrams, etc. Because of this, it is difficult to distinguish between them. Therefore, in this specification, unless otherwise specified, The potential difference between the potential at a given point and a reference potential (also called the reference potential) is defined as the voltage at that point. It may be used in some cases.
[0040] Next, as an example of a method for driving a storage device in this embodiment, the storage device shown in Figure 2(A) An example of a driving method will be described. Here, as an example, the data signal will be driven at high level and low level. The level is a binary digital signal, and the above-mentioned D when the voltage Vx value is high level The voltage of the digital signal should be equivalent to that of the digital signal. Also, the voltage of the data signal when it is high should be the same as the data signal. Let's assume that TA (1) represents data, and the voltage of the data signal when it's low level represents data (0). Oh, but it's not limited to this; the voltage of the data signal when it's high level represents data (0), The voltage of the data signal at a certain level may represent data (1).
[0041] In this embodiment of the memory device drive method, first the transistor 131 is turned ON. The data signal then determines the gate voltages of transistors 112 and 122, Next, set the value of data Dm. This writes the data to the memory cell. Furthermore, by turning off transistor 131, transistors 112 and 131 The gate voltage of STA122 (value of data Dm) is held. Therefore, the memory cell is stored. The data is stored. Note that the supply of voltage Vx to the memory cell may be stopped at this time. This can reduce power consumption. For example, by using a switch, the voltage can be reduced. The supply of Vx can be controlled.
[0042] Next, the data signal determines the gate voltages of transistors 111 and 121. In other words, set the data Dsch.
[0043] At this time, the values of data Dm and data Dsch determine the comparison circuit 101 and the comparison circuit The 102 states change. Each state is explained using Figure 2(B). Figure 2 (B) is the value of data Dm, the value of data Dsch, comparator circuit 101, and comparator circuit 102 This is a diagram showing the state.
[0044] As shown in Figure 2(B), the value of data Dm is (0) and the value of data Dsch is ( 1) When the value of data Dm is smaller than the value of data Dsch, the transistor When transistors 111 and 112 are turned on, the comparator circuit 101 is in a conducting state (state pa (Also known as ss) otherwise transistors 111 and 112 At least one of them turns off, and the comparator circuit 101 becomes non-conductive (also called state ×). When the comparison circuit 101 is conducting, the voltage value of the output signal line OUT changes, and the voltage Vx and The values will be equivalent. Also, when the comparison circuit 101 is in a non-conducting state, the voltage value of the output signal line OUT This does not change. Therefore, data D depends on whether or not the voltage value of the output signal line OUT changes. It is possible to determine whether the value of m is smaller than the value of data Dsch.
[0045] Also, when the value of data Dm is (1) and the value of data Dsch is (0), that is When the value of data Dm is greater than the value of data Dsch, transistors 121 and 121 When the starter 122 is turned off, the comparator circuit 102 becomes non-conductive, and otherwise it is turned off. At least one of transistors 121 and 122 is turned ON, and the comparator circuit 102 becomes conductive. For example, if a memory device has multiple memory cells, the comparison cycle When path 102 is in a conductive state, there is conductivity between the memory cell on which it is installed and other memory cells. When this state occurs and the comparison circuit 102 is in a non-conductive state, the memory cell provided with it and other memory cells The connection with the Morisel becomes non-conductive.
[0046] The above is a description of an example of a method for driving a storage device in this embodiment.
[0047] Note that the configuration of the memory cell is not limited to the configuration shown in Figure 2(A), and the configuration of the memory cell can be used as an example. For example, as shown in Figure 3(A), if transistor 111 is a P-channel type transistor, Transistor 112 is an N-channel type transistor, and transistor 121 is a P-channel type This can be a transistor, and transistor 122 may be an N-channel transistor. When, as shown in Figure 3(B), the value of data Dm is greater than the value of data Dsch The comparison circuit 101 is in a conducting state and in a non-conducting state at all other times. Also, data D When the value of m is smaller than the value of data Dsch, the comparison circuit 102 becomes non-conductive, and It becomes conductive at all other times. Therefore, it depends on whether the voltage value of the output signal line OUT changes or not. This allows us to determine whether the value of data Dm is greater than or equal to the value of data Dsch. The configurations of the comparison circuit 101 and the comparison circuit 102 are as shown in Figures 2(A) and 3(A). The configuration is not limited to this one; other configurations are acceptable as long as they can provide equivalent functionality.
[0048] As explained with reference to Figures 1 to 3, in the example of the storage device in this embodiment, the comparison cycle Using a path and a control transistor that controls the setting of the data value stored in the memory cell, By configuring a memory cell capable of discriminating data, the transients in the memory cell Because the number of components can be reduced, the circuit area can be reduced.
[0049] Furthermore, in the example of the memory device in this embodiment, the control transistor is a channel By using a transistor that includes an oxide semiconductor layer in which the off state is formed, The leakage current of the transistor can be reduced. Therefore, the control transistor is in the off state. It is possible to suppress fluctuations in the data stored in the memory cell when it is in a certain state. By suppressing fluctuations in data stored in the Moriscell, the data is retained in the memory cell. Since the power supply can be stopped as needed, power consumption can also be reduced.
[0050] (Embodiment 2) This embodiment describes an example of a storage device capable of distinguishing between multiple bits of data.
[0051] An example of a storage device in this embodiment will be explained with reference to Figure 4.
[0052] The memory device shown in Figure 4 has N stages (where N is a natural number greater than or equal to 2) of memory cells 201 (memory cells 2 01_1 to memory cell 201_N), output signal line OUT1, output signal line OUT2 , connecting wiring CL_1 to CL_N-1, wiring VL to which voltage is applied, and transistor 2 It comprises 02, transistor 203, buffer 204, and buffer 205. Oh, a circuit composed of N stages of memory cells 201 is considered as a single row of memory circuit, and the memory Multiple circuits may be provided to create a configuration with multiple rows of memory circuits.
[0053] Each of the N-stage memory cells 201 is a memory cell with the configuration shown in Figure 1. This is possible, and each of the N-stage memory cells 201 is connected to a comparator circuit 101, a comparator circuit 102, and It comprises a transistor 131 and, for example, each of the N-stage memory cells 201 is described It stores 1 bit of data as a single unit of data.
[0054] In each of the N-stage memory cells 201, the comparison circuit 101 checks 1 bit of stored data Perform the first comparison operation between (data Dm) and the 1-bit search data (data Dsch). It has a function to control whether or not to change the voltage value of the output signal line OUT1 according to the calculation result. For example, when the value of data Dm is smaller than the value of data Dsch, the comparison circuit 101 When a conduction state is established and the value of data Dm matches the value of data Dsch, or when data D It has a function that causes it to become non-conductive when the value of m is greater than the value of data Dsch. The comparison circuit 101 is not limited to this, but if the value of data Dm is greater than the value of data Dsch When it is not connected, it becomes conductive, and when the value of data Dm matches the value of data Dsch, or when It has a function that causes it to become non-conductive when the value of data Dm is smaller than the value of data Dsch. It is also possible. In addition, the comparison circuit 101 (the other of the source and drain of transistor 112) It is electrically connected to the output signal line OUT1.
[0055] Furthermore, in each of the N-stage memory cells 201, the comparison circuit 102 stores 1 bit of memory. The second comparison operation between the data (data Dm) and the 1-bit search data (data Dsch) is performed. It has the function of performing the following. For example, the memory cell 20 of the Kth stage (where K is a natural number between 2 and N-1) In 1_K, the comparator circuit 102 determines that if the value of data Dm is less than the value of data Dsch, The memory cells 201_K-1 in the K-1 stage and 201_K+1 in the K+1 stage A function to deconduct the connection between them, or when the value of data Dm is greater than the value of data Dsch. Between memory cell 201_K-1 of the K-1 stage and memory cell 201_K+1 of the K+1 stage It has a function to make it non-conductive. For example, the comparator circuit 102 determines the value of data Dm from data D When the value of sch is smaller, or when the value of data Dm matches the value of data Dsch. When it is conducting, and when the value of data Dm is greater than the value of data Dsch, it is not conducting. It has the function of becoming. However, it is not limited to this, and the comparison circuit 102 has the function of determining the value of data Dm When the value of data Dm is greater than the value of data Dsch, or when the value of data Dm matches the value of data Dsch It becomes conductive when the data Dm value is smaller than the data Dsch value, and non-conductive when the data Dm value is smaller than the data Dsch value. It may have a function to enter a normal state. Also, the ratio in the K-stage memory cell 201_K The comparison circuit 102 is a comparison circuit 102 in the K-1 stage memory cell 201_K-1 and K It is connected to the comparator circuit 102 in the first-stage memory cell 201_K+1.
[0056] Furthermore, the comparison circuit 101 of the first-stage memory cell 201_1 is either in a conductive state or a non-conductive state. This provides a function to control the electrical connection between wiring VL and output signal line OUT1.
[0057] Furthermore, the comparison circuit 102 of the first-stage memory cell 201_1 is either in a conductive state or a non-conductive state. This provides a function to control the electrical connection between wiring VL and the first connecting wiring CL_1. ru.
[0058] Furthermore, the comparison circuit 101 of the K-stage memory cell 201_K is either in a conductive state or a non-conductive state. By doing so, the electrical connection between the K-1 connection wiring CL_K-1 and the output signal line OUT1 is established. It has a control function.
[0059] Furthermore, the comparison circuit 102 of the K-stage memory cell 201_K is either in a conductive state or a non-conductive state. By doing so, the electrical connection between the K-1 connection wiring CL_K-1 and the K connection wiring CL_K is It has a function to control the continuation.
[0060] Furthermore, the comparison circuit 101 of the Nth-stage memory cell 201_N is either in a conductive state or a non-conductive state. By doing so, the electrical connection between the N-1 connection wiring CL_N-1 and the output signal line OUT1 is established. It has a control function.
[0061] Furthermore, the comparison circuit 102 of the Nth memory cell 201_N is either in a conductive state or a non-conductive state. By doing so, the electrical connection between the N-1 connection wiring CL_N-1 and the output signal line OUT2 is established. It has a control function.
[0062] In each of the N-stage memory cells 201, the source and drain of transistor 131 One of them is electrically connected to a different data line, and the other is electrically connected to a different data line. Different data signals are input through them. The gate of transistor 131 is a common w It is electrically connected to the Word line.
[0063] Furthermore, in the first stage memory cell 201_1, the comparison circuit 101 (transistor 111) (one of the source and drain) and comparison circuit 102 (source and drain of transistor 121) On one side of the input, and on one side of the source and drain of transistor 122, the wiring VL A voltage Va is applied via this. Therefore, the output signal line OUT2 is connected to the N-stage memory cell 201 Each of these is connected to a wire to which a voltage Va is applied via a comparison circuit 102. The pressure Va is set appropriately according to the polarity of the transistors constituting the memory cell 201.
[0064] Furthermore, output signal lines OUT1 and OUT2 are each of the N-stage memory cells 201 This is a wiring configuration where the voltage value is set according to the comparison operation. The output signal line OUT2 is N The memory cell 201_N of the first stage (the source and drain of transistor 121, and It is electrically connected to the source and drain (other side) of transistor 122.
[0065] For descriptions of other components, refer to the description in Embodiment 1 as appropriate.
[0066] Transistor 202 controls whether or not to set the voltage of the output signal line OUT1 to the reference voltage. It has the function of having a reference current. For example, one of the source and drain of transistor 202 has a reference current. When pressure is applied, the source and the other drain of transistor 202 are connected to the output signal line OUT1. They are electrically connected, and a control signal is input to the gate of transistor 202. The value of the quasi-voltage is set appropriately, for example, according to the polarity of the transistor in the memory device.
[0067] Transistor 203 controls whether or not to set the voltage of the output signal line OUT2 to the reference voltage. It has the function of having a reference current. For example, one of the source and drain of transistor 203 has a reference current. When pressure is applied, the source and the other drain of transistor 203 are connected to the output signal line OUT2. They are electrically connected, and a control signal is input to the gate of transistor 203. The signal and reference voltage may be the same as those for transistor 202.
[0068] Buffer 204 adjusts the voltage value on the output signal line OUT1 and outputs the adjusted voltage to the output signal line. It has the function to output as a number. Note that buffer 204 is not necessarily required.
[0069] Buffer 205 adjusts the voltage value on the output signal line OUT2 and outputs the adjusted voltage to the output signal line. It has the function to output as a number. Note that a buffer 205 is not necessarily required.
[0070] Next, as an example of a method for driving a storage device in this embodiment, the method for driving a storage device shown in Figure 4 Let's explain the legal regulations. Here, as an example, we will discuss data signals at high level and low level. This is a binary (1-bit) digital signal, and the voltage of the data signal when it is high is Let's assume that the data (1) is represented by the voltage of the data signal when it is low level, and that the data (0) is represented by the voltage of the data signal when it is low level.
[0071] First, the first data signal to the Nth data signal is used to process memory cells 201_1 to memory cells Data is written to each of the 201_N cells and stored in their respective memory cells 201. Set the value of data Dm. Here, write 1 bit of data to each memory cell 201. By doing so, N bits of data are stored in memory cells 201_1 through 201_N. Write the data. Note that at this time, the voltage Va supply to the first memory cell 201_1 is stopped. This is also good. This can reduce power consumption. For example, by using a switch, This allows for the control of the voltage Va supply.
[0072] Next, turn on transistor 202 and output signal lines OUT1 and OUT2 Set the voltage to the reference voltage.
[0073] Next, the memory cells 201_1 to the memory cells are processed by the first data signal to the Nth data signal. Set the data Dsch for each cell 201_N. By setting the data Dsch to data for each bit, memory cell 201_1 to In Morisel 201_N, it is possible to set N bits of search data.
[0074] At this time, in each memory cell 201, the values of data Dm and data Dsch The states of comparison circuits 101 and 102 change.
[0075] For example, when the value of data Dm is smaller than the value of data Dsch, the comparator circuit 101 is in a conductive state. When the comparator circuit 101 is in this state, the comparator circuit 101 is in a non-conductive state at all other times. When conducting, the voltage value of the output signal line OUT1 changes. Also, when the comparator circuit 101 is deconducted... When the device is in the normal state, the voltage value of the output signal line OUT1 does not change.
[0076] Furthermore, when the value of data Dm is greater than the value of data Dsch, the comparison circuit 102 is non-conductive. In this state, the comparator circuit 102 is in a conducting state at all other times. For example, the K-stage memo When the comparison circuit 102 in recell 201_K is in a conducting state, the K-stage memory cell 201 The connection between _K and the K+1-stage memory cell 201_K+1 becomes conductive, and the K-stage memory cell When the comparison circuit 102 in 201_K is in a non-conductive state, the K-stage memory cell 201_ The connection between K and the K+1 memory cell 201_K+1 becomes non-conductive.
[0077] As illustrated by the above example, from the stored data Dm stored in each memory cell 201 The value of the N bits of data is obtained from the data Dsch set in each memory cell 201. When the value of the N-bit data is greater than or less than the output signal line OUT1 The voltage value changes, and otherwise the voltage value of the output signal line OUT1 does not change.
[0078] Furthermore, the N-bit data value consisting of the data Dm stored in each memory cell 201 is each Less than the value of the N-bit data consisting of the data Dsch set in Morissel 201 When the number of cells is small or large, the space between adjacent memory cells 201 becomes non-conductive. In each of the N-stage memory cells 201, the data stored in each memory cell 201 The data Ds, which consists of N bits of data Dm, is set in each memory cell 201. When the values of the N bits of data consisting of channels are equal, the voltage value of the output signal line OUT2 changes. To transform.
[0079] Furthermore, the comparison operation in each memory cell 201 determines the output signal line OUT1 and the output signal The voltage values of each line OUT2 are set and stored in each memory cell 201. N bits of data consisting of the data Dm are identified.
[0080] For example, the voltage value of the output signal line OUT1 is the value that represents data (1), and the output signal line OUT When the voltage value of 2 is a value representing data (1) or data (0), each memory cell 201 The N-bit data consisting of stored data Dm is the N-bit data that will be used as search data. It is determined to be smaller.
[0081] Furthermore, the voltage value of output signal line OUT1 represents the data (0), and output signal line OUT2 When the voltage value is the value representing data (1), the data D stored in each memory cell 201 The N-bit data consisting of m is determined to be equal to the N-bit data that will be used as the search data. For example, in each of the N-stage memory cells 201, the value of data Dm is equal to the value of data Ds When the value is equal to the value of ch, the voltage value of the output signal line OUT2 represents the value of data (1).
[0082] Furthermore, the voltage value of output signal line OUT1 represents the data (0), and output signal line OUT2 When the voltage value of represents the data (0), the data D stored in each memory cell 201 The N-bit data consisting of m is determined to be larger than the N-bit data that will be used as the search data. It can be done.
[0083] Furthermore, similar to the storage device shown in Embodiment 1, each memory cell 201 has a comparison circuit 10 If you reverse the polarity of the transistors in circuit 1 and comparison circuit 102 and change the value of the voltage Va, The relative magnitudes of the voltage values on the power signal line OUT1 and the output signal line OUT2, and the judgment result, are inversely related.
[0084] As described above, whether or not the voltage values of output signal lines OUT1 and OUT2 change depends on the following: Therefore, the N bits of data consisting of the data Dm stored in each memory cell 201 are identified. It is possible.
[0085] Furthermore, if multiple memory circuits are provided, each of the N-stage memory cells 201 is used. The data Dsch setting operation in each memory cell 201 may be performed simultaneously. stomach.
[0086] The above is a description of an example of a method for driving a storage device in this embodiment.
[0087] As explained with reference to Figure 4, multiple stages of memory cells are used with the configuration shown in Embodiment 1. By configuring a memory device equipped with a Moriscell, it becomes possible to distinguish between multiple bits of data. We can provide a memory device.
[0088] (Embodiment 3) In this embodiment, an oxide semiconductor applicable to the transistor of the memory device shown in the above embodiment is used. Let's describe an example of a transistor that includes a conductive layer.
[0089] An example of a transistor structure including the above oxide semiconductor layer will be explained using Figure 5. Figure 5 This is a schematic cross-sectional diagram showing an example of the transistor structure in this embodiment.
[0090] The transistor shown in Figure 5(A) consists of a conductive layer 601_a, an insulating layer 602_a, and a semiconductor layer. 603_a, conductive layer 605a_a, conductive layer 605b_a, insulating layer 606_a, Includes the electrochemical layer 608_a.
[0091] The conductive layer 601_a is provided on top of the element formation layer 600_a.
[0092] The insulating layer 602_a is provided on top of the conductive layer 601_a.
[0093] The semiconductor layer 603_a is superimposed on the conductive layer 601_a via the insulating layer 602_a.
[0094] Each of the conductive layers 605a_a and 605b_a is provided on the semiconductor layer 603_a. It is then connected electrically to the semiconductor layer 603_a.
[0095] The insulating layer 606_a consists of the semiconductor layer 603_a, the conductive layer 605a_a, and the conductive layer 605b_ It is placed above a.
[0096] The conductive layer 608_a is superimposed on the semiconductor layer 603_a via the insulating layer 606_a.
[0097] Furthermore, it is not necessary to provide either the conductive layer 601_a or the conductive layer 608_a. If the conductive layer 608_a is not provided, the insulating layer 606_a may also be omitted.
[0098] The transistor shown in Figure 5(B) consists of a conductive layer 601_b, an insulating layer 602_b, and a semiconductor layer. 603_b, conductive layer 605a_b, conductive layer 605b_b, insulating layer 606_b, Includes the electrode layer 608_b.
[0099] The conductive layer 601_b is provided on the element formation layer 600_b.
[0100] The insulating layer 602_b is provided on top of the conductive layer 601_b.
[0101] Each of the conductive layers 605a_b and 605b_b is located on a portion of the insulating layer 602_b. It will be established in [location].
[0102] The semiconductor layer 603_b is provided on the conductive layer 605a_b and the conductive layer 605b_b, It is electrically connected to the electrolytic layer 605a_b and the conductive layer 605b_b. Also, semiconductor layer 603 _b is superimposed on the conductive layer 601_b via the insulating layer 602_b.
[0103] The insulating layer 606_b consists of the semiconductor layer 603_b, the conductive layer 605a_b, and the conductive layer 605b_ It is placed above b.
[0104] The conductive layer 608_b is superimposed on the semiconductor layer 603_b via the insulating layer 606_b.
[0105] Note that it is not necessary to provide either conductive layer 601_b or conductive layer 608_b. If layer 608_b is not provided, then insulating layer 606_b may not be provided.
[0106] The transistor shown in Figure 5(C) consists of a conductive layer 601_c, an insulating layer 602_c, and a semiconductor layer. It includes 603_c, conductive layer 605a_c, and conductive layer 605b_c.
[0107] The semiconductor layer 603_c includes regions 604a_c and 604b_c. Region 604a_ Regions c and 604b_c are separated from each other and each has a dopant added to it. Furthermore, the region between region 604a_c and region 604b_c becomes the channel-forming region. The semiconductor layer 603_c is provided on the element formation layer 600_c. Note that the region is not necessarily It is not necessary to provide regions 604a_c and 604b_c.
[0108] The conductive layer 605a_c and conductive layer 605b_c are provided on the semiconductor layer 603_c, and It is electrically connected to the conductive layer 603_c. Also, conductive layers 605a_c and 605b The sides of _c are tapered.
[0109] Furthermore, the conductive layer 605a_c is superimposed on a portion of region 604a_c, but is not necessarily limited to this. It is not determined. By superimposing the conductive layer 605a_c onto a part of region 604a_c, The resistance between the electrochemical layer 605a_c and region 604a_c can be reduced. Even if the entire region of the semiconductor layer 603_c superimposed on the conductive layer 605a_c is region 604a_c good.
[0110] Furthermore, the conductive layer 605b_c is superimposed on a portion of region 604b_c, but is not necessarily limited to this. It is not determined. By superimposing the conductive layer 605b_c onto a part of region 604b_c, The resistance between the electrode layer 605b_c and region 604b_c can be reduced. Even if the entire region of the semiconductor layer 603_c superimposed on the electrochemical layer 605b_c is region 604b_c, stomach.
[0111] The insulating layer 602_c is composed of the semiconductor layer 603_c, the conductive layer 605a_c, and the conductive layer 605b_ It is placed above c.
[0112] The conductive layer 601_c is superimposed on the semiconductor layer 603_c via the insulating layer 602_c. The region of the semiconductor layer 603_c superimposed on the conductive layer 601_c via 602_c is channel-shaped It becomes a developed region.
[0113] Furthermore, the transistor shown in Figure 5(D) consists of a conductive layer 601_d, an insulating layer 602_d, and a semi-transistor. It includes a conductive layer 603_d, a conductive layer 605a_d, and a conductive layer 605b_d.
[0114] The conductive layers 605a_d and 605b_d are provided on the element formation layer 600_d. Furthermore, the sides of conductive layers 605a_d and 605b_d are tapered.
[0115] Semiconductor layer 603_d includes region 604a_d and region 604b_d. Region 604 Regions a_d and 604b_d are separated from each other, and each is a region to which a dopant has been added. Yes. Also, the region between region 604a_d and region 604b_d becomes a channel-forming region. The semiconductor layer 603_d is, for example, a conductive layer 605a_d, a conductive layer 605b_d, and a substrate. Provided on the substrate-forming layer 600_d, and electrically conductive to the conductive layer 605a_d and conductive layer 605b_d They are connected. Note that it is not always necessary to provide regions 604a_d and 604b_d. good.
[0116] Region 604a_d is electrically connected to the conductive layer 605a_d.
[0117] Region 604b_d is electrically connected to the conductive layer 605b_d.
[0118] The insulating layer 602_d is provided on top of the semiconductor layer 603_d.
[0119] The conductive layer 601_d is superimposed on the semiconductor layer 603_d via the insulating layer 602_d. The region of semiconductor layer 603_d superimposed on conductive layer 601_d via 602_d is channel-shaped It becomes a developed region.
[0120] Furthermore, we will explain each component shown in Figures 5(A) to 5(D).
[0121] The element-forming layers 600_a to 600_d are, for example, an insulating layer, or an insulating layer. A substrate with a surface can be used. Furthermore, a layer with pre-formed elements can be used as the element-type substrate. It can also be used as layered 600_a to element-forming layer 600_d.
[0122] Each of the conductive layers 601_a to 601_d is a transistor gate. It has the ability. Furthermore, the layer that functions as the gate of a transistor is called the gate electrode or gate. Also called T-wiring.
[0123] Examples of conductive layers 601_a to 601_d include molybdenum, magnesium, and thiosulfate. Tan, chromium, tantalum, tungsten, aluminum, copper, neodymium, or scan A layer of metallic material such as zinc, or an alloy material mainly composed of these materials, can be used. Furthermore, by laminating layers of materials applicable to the formation of conductive layers 601_a to 601_d , the conductive layers 601_a to 601_d can also be formed.
[0124] Each of the insulating layers 602_a to 602_d serves as a gate insulating layer of the transistor and has a function as such.
[0125] Examples of the insulating layers 602_a to 602_d include a silicon oxide layer, a silicon nitride layer, a silicon oxynitride layer, a silicon nitride oxide layer, an aluminum oxide layer, an aluminum nitride layer, an aluminum oxynitride layer, an aluminum nitride oxide layer, a hafnium oxide layer, or a lanthanum oxide layer can be used. Further, the insulating layers 602_a to 602_d can be formed by stacking layers of materials applicable to the insulating layers 602_a to 602_d. Further, the insulating layers 602_a to 602_d can also be formed by stacking layers of applicable materials.
[0126] Further, as the insulating layers 602_a to 602_d, for example, an insulating layer made of a material containing a Group 13 element and an oxygen element in the periodic table can be used. For example, when the semiconductor layers 603_a to 603_d contain a Group 13 element, by using an insulating layer containing a Group 13 element as the insulating layer in contact with the semiconductor layers 603_a to 603_d, the state of the interface between the insulating layer and the oxide semiconductor layer can be improved. An insulating layer made of a material containing a Group 13 element and an oxygen element in the periodic table can also be used. For example, when the semiconductor layers 603_a to 603_d contain a Group 13 element, by using an insulating layer containing a Group 13 element as the insulating layer in contact with the semiconductor layers 603_a to 603_d, the state of the interface between the insulating layer and the oxide semiconductor layer can be improved. When the semiconductor layers 603_a to 603_d contain a Group 13 element, by using an insulating layer containing a Group 13 element as the insulating layer in contact with the semiconductor layers 603_a to 603_d, the state of the interface between the insulating layer and the oxide semiconductor layer can be improved. By using an insulating layer containing a Group 13 element as the insulating layer in contact with the semiconductor layers 603_a to 603_d, the state of the interface between the insulating layer and the oxide semiconductor layer can be improved.
[0127] Examples of the material containing a Group 13 element and an oxygen element include gallium oxide, aluminum oxide, aluminum gallium oxide, gallium aluminum oxide, and the like. Note that aluminum gallium oxide refers to a substance in which the content of aluminum (atomic%) is higher than the content of gallium (atomic%), and gallium aluminum oxide refers to a substance in which the content of gallium (atomic%) is higher than the content of aluminum (atomic%). Note that aluminum gallium oxide refers to a substance in which the content of aluminum (atomic%) is higher than the content of gallium (atomic%), and gallium aluminum oxide refers to a substance in which the content of gallium (atomic%) is higher than the content of aluminum (atomic%). atomic %) is greater than or equal to the aluminum content (atomic %). For example, Al2O x (x=3+α, where α is a value greater than 0 and less than 1), Ga2O x (x=3+α, where α is greater than 0 and less than 1), or Ga x Al 2-x O 3+α (where x is greater than 0 and less than 2 and α is greater than 0 and less than 1) can also be used.
[0128] Alternatively, the insulating layers 602_a to 602_d may be formed by stacking layers of materials applicable to the insulating layers 602_a to 602_d. For example, a plurality of Ga2O layers may be stacked to form the insulating layers 602_a to 602_d. For example, a plurality of Ga2O x represented by gallium oxide-containing layers may be stacked to form the insulating layers 602_a to 602_d. Alternatively, Ga2O may be configured. Alternatively, Ga2O x represented by gallium oxide-containing insulating layers and Al2O x represented by aluminum oxide-containing insulating layers may be stacked to form the insulating layers 602_a to 602_d. 602_d may be configured.
[0129] Each of the semiconductor layers 603_a to 603_d functions as a layer in which a transistor channel is formed. Examples of oxide semiconductors applicable to the semiconductor layers 603_a to 603_d include quaternary metal oxides, ternary metal oxides, binary metal oxides, and single-element metal oxides. It functions as a layer to be formed. Examples of oxide semiconductors applicable to the semiconductor layers 603_a to 603_d include quaternary metal oxides, ternary metal oxides, binary metal oxides, and single-element metal oxides. Examples of usable oxide semiconductors include quaternary metal oxides, ternary metal oxides, binary metal oxides, and single-element metal oxides. compounds or single-element metal oxides can be used.
[0130] The oxide semiconductor preferably contains at least indium (In) or zinc (Zn). In particular, it preferably contains In and Zn. Further, a transistor using the oxide semiconductor is preferred. In particular, it preferably contains In and Zn. Further, a transistor using the oxide semiconductor As a stabilizer to reduce variations in the electrical characteristics of the inverter, in addition to those, It is preferable to have lium (Ga). It is also preferable to have tin (Sn) as a stabilizer. It is preferable to do so. It is also preferable to have hafnium (Hf) as a stabilizer. It is preferable to have aluminum (Al) as a stabilizer.
[0131] Also, other stabilizers include lanthanides such as lanthanum (La) and cerium ( Ce, praseodymium (Pr), neodymium (Nd), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), hol Mium (Ho), Erbium (Er), Thulium (Tm), Ytterbium (Yb), Lu It may contain one or more types of tecium (Lu).
[0132] Examples of quaternary metal oxides include In-Sn-Ga-Zn-O metal oxides and In-H f-Ga-Zn-O metal oxides, In-Al-Ga-Zn-O metal oxides, In-S n-Al-Zn-O metal oxide, In-Sn-Hf-Zn-O metal oxide, In-H f-Al-Zn-O metal oxides and the like can be used.
[0133] Examples of ternary metal oxides include In-Ga-Zn-O metal oxides and In-Sn-Z nO metal oxide, In-Al-Zn-O metal oxide, Sn-Ga-Zn-O metal Oxides, Al-Ga-Zn-O metal oxides, or Sn-Al-Zn-O metal oxides, In-Hf-Zn-O metal oxides, In-La-Zn-O metal oxides, In-Ce- Zn-O metal oxide, In-Pr-Zn-O metal oxide, In-Nd-Zn-O gold metal oxide, In-Sm-Zn-O-based metal oxide, In-Eu-Zn-O-based metal oxide, I n-Gd-Zn-O-based metal oxide, In-Tb-Zn-O-based metal oxide, In-Dy-Z n-O-based metal oxide, In-Ho-Zn-O-based metal oxide, In-Er-Zn-O-based metal oxide, In-Tm-Zn-O-based metal oxide, In-Yb-Zn-O-based metal oxide, In -Lu-Zn-O-based metal oxide, or the like can be used.
[0134] As the binary metal oxide, for example, an In-Zn-O-based metal oxide, a Sn-Zn-O-based metal oxide, an Al-Zn-O-based metal oxide, a Zn-Mg-O-based metal oxide, a Sn-Mg-O-based metal oxide, an In-Mg-O-based metal oxide, an In-Sn-O-based metal oxide, or an In-G a-O-based metal oxide, or the like can be used.
[0135] As the unitary metal oxide, for example, an In-O-based metal oxide, a Sn-O-based metal oxide, or a Zn-O-based metal oxide, or the like can also be used. In addition, applicable as the above oxide semiconductor The metal oxide may contain silicon oxide.
[0136] Note that the In-Ga-Zn-O-based metal oxide refers to a metal oxide containing In, Ga, and Zn as main components, and the ratio of In, Ga, and Zn is not limited. In addition, In, Ga, and Metal elements other than Zn may be contained.
[0137] When an In-Zn-O-based metal oxide is used, for example, In:Zn=50:1 to In:Z n=1:2 (converted to a molar ratio, In2O3:ZnO=25:1 to In2O3:Zn O=1:4), preferably In:Zn=20:1 to In:Zn=1:1 (converted to a molar ratio Calculations show that In2O3:ZnO=10:1 to In2O3:ZnO=1:2, and even more preferably... Alternatively, In:Zn=15:1 or In:Zn=1.5:1 (which translates to In2 in mole ratios). Oxide target with a composition ratio of O3:ZnO=15:2 to In2O3:ZnO=3:4 A semiconductor layer of In-Zn-O based metal oxide can be formed using a tactic. For example, The target used for forming In-Zn-O oxide semiconductors has an atomic ratio of In:Zn:O. When =S:U:R, assume R>1.5S+U. By increasing the amount of In, This can improve Zista's mobility.
[0138] Furthermore, the composition ratio of the target used in In-Sn-Zn-O metal oxides is expressed in terms of atomic ratio. In:Sn:Zn=1:2:2, In:Sn:Zn=2:1:3, In:Sn:Zn=1 Using an oxide target with a ratio of 1:1, or In:Sn:Zn = 20:45:35, etc. ru.
[0139] In addition, as an oxide semiconductor, InLO3(ZnO) m (m is a number greater than 0, and m Materials represented by (where is not an integer) can also be used. For example, InLO3(ZnO). m The L is This indicates one or more metallic elements selected from Ga, Fe, Al, Mn, and Co. As an oxide semiconductor, In3SnO5(ZnO) n (n is a number greater than 0, and n is Materials can also be expressed using integers.
[0140] Also, In:Ga:Zn = 1:1:1 (= 1 / 3:1 / 3:1 / 3) or In:Ga In-Ga-Zn-O system with an atomic ratio of Zn=2:2:1 (=2 / 5:2 / 5:1 / 5) Metal oxides or oxides with a similar composition can be used. Alternatively, In:Sn:Z n=1:1:1(=1 / 3:1 / 3:1 / 3), In:Sn:Zn=2:1:3(=1 / 3:1 / 6:1 / 2) or In:Sn:Zn=2:1:5 (=1 / 4:1 / 8:5 / 8) Use In-Sn-Zn-O metal oxides with the atomic ratio of the above, or oxides with a similar composition. That's good.
[0141] However, this is not limited to these, and includes the semiconductor characteristics required (mobility, threshold, variability, etc.). A suitable composition should be used depending on the requirements. Furthermore, in order to obtain the desired semiconductor properties, Carrier concentration, impurity concentration, defect density, atomic ratio of metal elements to oxygen, interatomic bond distance, density It is preferable to set the degree and other parameters appropriately.
[0142] For example, high mobility can be obtained relatively easily with In-Sn-Zn-O metal oxides. However, even with In-Ga-Zn-O based metal oxides, the bulk defect density can be reduced. This allows for increased mobility.
[0143] For example, if the atomic ratio of In, Ga, and Zn is In:Ga:Zn=a:b:c(a+b+ The composition of an oxide with c=1 is such that the atomic ratio is In:Ga:Zn=A:B:C(A+B+C The composition of the oxide in the vicinity of (a-A) = 1) means that a, b, and c are in the vicinity of (a-A) 2 +(b-B) 2 + (c-C) 2 ≤r 2 This means satisfying the following condition. For example, r can be set to 0.05. The same applies to other oxides.
[0144] Oxide semiconductors can be single crystals or non-single crystals. In the latter case, they can be amorphous or polycrystalline. But that's fine too. Also, even if the structure contains crystalline parts within the amorphous material, it can be non-amorphous. But that's fine.
[0145] Amorphous oxide semiconductors can be made relatively easily to obtain a flat surface, This can reduce interfacial scattering when fabricating transistors, and it can be done relatively easily and relatively high You can obtain a high degree of mobility.
[0146] Furthermore, in crystalline oxide semiconductors, bulk defects can be reduced even further, and surface By improving the flatness, it is possible to obtain mobility higher than that of an amorphous oxide semiconductor. To improve surface flatness, it is preferable to form an oxide semiconductor on a flat surface. Specifically, the average surface roughness (Ra) is 1 nm or less, preferably 0.3 nm or less, more preferably Alternatively, it is preferable to form it on a surface with a nm or smaller.
[0147] Note that Ra is the centerline average roughness defined in JIS B0601, applied to the surface. This is a three-dimensional extension that allows for "averaging the absolute values of the deviations from the reference plane to the specified plane." It can be expressed as "the value" and is defined by the following formula.
[0148]
number
[0149] In the above, S0 is the measurement surface (coordinates (x1,y1)(x1,y2)(x2,y1 Z0 refers to the area of the rectangle enclosed by the four points represented by (x2, y2), and Z0 is This refers to the average height of the measurement surface. Ra stands for Atomic Force Microscope (AFM). Evaluation is possible using a microscope. Note that the measurement surface refers to the surface indicated by all measurement data. It consists of three parameters (x, y, z) and can be expressed as z = F(x, y). The range of x (and y) is from 0 to xMAX (and yMAX), and the range of z is zMIN to zMAX.
[0150] Furthermore, the region in which at least channels are formed of semiconductor layers 603_a to 603_d The region is crystalline, non-single crystal, and, when viewed from a direction perpendicular to the ab plane, is triangular or hexagonal. , having an equilateral triangular or regular hexagonal atomic arrangement, and being a metal when viewed from a direction perpendicular to the c-axis. A phase in which atoms are arranged in layers, or in which metal atoms and oxygen atoms are layered when viewed from a direction perpendicular to the c-axis. The material having the above phases may have phases arranged in a specific direction. It is also called ned crystal.
[0151] Furthermore, when the channel length of the transistor is 30 nm, the semiconductor layer 603_a to the semiconductor layer The thickness of 603_d may be, for example, about 5 nm. In this case, semiconductor layer 603_a to If semiconductor layer 603_d is a CAAC oxide semiconductor layer, then short-circuiting in the transistor The Nell effect can be suppressed.
[0152] Regions 604a_c, 604b_c, 604a_d, and 604b_d are N A dopant is added to impart a type-1 or P-type conductivity, and the source or drain of the transistor... It functions as a dopant. For example, the elements of Group 13 in the periodic table. (For example, boron), elements of Group 15 in the periodic table (for example, nitrogen, phosphorus, and arsenic) (one or more), and noble gas elements (e.g., helium, argon, and xenon, or one or more) One or more of the following can be used. Note that the function as a source for the transistor The region containing this is also called the source region, and it is the region that functions as the drain of the transistor. This is also called the drain region. Region 604a_c, region 604b_c, region 604a_d, and By adding a dopant to region 604b_d, the connection resistance with the conductive layer is reduced. This allows for miniaturization of transistors.
[0153] conductive layers 605a_a to 605a_d, and conductive layers 605b_a to 605 Each of b_d functions as either the source or drain of the transistor. The layer that functions as the source of a transistor is also called the source electrode or source wiring. The layer that functions as the drain of a transistor is also called the drain electrode or drain wiring. .
[0154] conductive layers 605a_a to 605a_d, and conductive layers 605b_a to 605 Examples of b_d include aluminum, magnesium, chromium, copper, tantalum, titanium, Metallic materials such as molybdenum or tungsten, or materials mainly composed of these metallic materials A layer of alloy material can be used. For example, copper, magnesium, and aluminum Due to the layer of alloy material it contains, conductive layer 605a_a to conductive layer 605a_d, and conductive layer 60 5b_a to conductive layer 605b_d can be formed. Also, conductive layer 605a_a Materials applicable to conductive layer 605a_d and conductive layers 605b_a to conductive layer 605b_d By laminating layers of material, conductive layers 605a_a to 605a_d and conductive layer 605b _a to conductive layer 605b_d can also be formed. For example, copper, magnesium, and A conductive layer 605a_a to a conductive layer is formed by laminating a layer of alloy material containing aluminum and a layer containing copper. The electrical layer 605a_d and the conductive layers 605b_a to 605b_d can be formed. Cut.
[0155] Furthermore, conductive layers 605a_a to 605a_d, and conductive layers 605b_a to conductive layers For 605b_d, a layer containing a conductive metal oxide can also be used. Examples of group oxides include indium oxide, tin oxide, zinc oxide, and indium oxide. Z, or indium zinc oxide can be used. Note that conductive layers 605a_a to Conductive layers 605a_d and conductive layers 605b_a to 605b_d are applicable to conductive layers The metal oxide may also contain silicon oxide.
[0156] The insulating layers 606_a and 606_b are the insulating layers 602_a to 602_ A layer of material applicable to d can be used. Also, insulating layer 606_a and insulating layer 60 The insulating layer 606_a and insulating layer 606_b are constructed by laminating materials applicable to 6_b. For example, an insulating layer 606_a and an insulating layer such as a silicon oxide layer or an aluminum oxide layer may be used. An insulating layer 606_b may be formed. For example, by using an aluminum oxide layer This further enhances the effect of suppressing the penetration of impurities into semiconductor layer 603_a and semiconductor layer 603_b. This allows for the suppression of oxygen desorption in semiconductor layer 603_a and semiconductor layer 603_b. It can be improved.
[0157] Conductive layer 608_a and conductive layer 608_b each serve as the gate of a transistor. It has the ability. Note that the transistor is either conductive layer 601_a and conductive layer 608_a or In the case of a structure that includes both conductive layer 601_b and conductive layer 608_b, conductive layer 601_a and one of the conductive layers 608_a, or one of the conductive layers 601_b and 608_b, Also called a back gate, back gate electrode, or back gate wiring. It functions as a gate. By providing multiple conductive layers via a channel forming layer, the threshold voltage of the transistor can be increased. This makes it easier to control the pressure.
[0158] Examples of conductive layers 608_a and 608_b include conductive layers 601_a to 6 A layer of material applicable to 01_d can be used. In addition, conductive layer 608_a and conductive The conductive layer 608_a and conductive layer 608_b are formed by laminating layers of material applicable to layer 608_b. It may be configured as follows:
[0159] Furthermore, the transistor of this embodiment is an oxide semiconductor having the function of a channel formation layer. A insulating layer is included on a portion of the body layer, and the insulating layer is superimposed on the oxide semiconductor layer, The structure may include a conductive layer that functions as a drain or a suction layer. In this case, the insulating layer is a layer that protects the channel formation layer of the transistor (also called the channel protection layer). It has the function of a channel protection layer. An insulating layer that has the function of a channel protection layer is, for example, A layer of material applicable to insulating layers 602_a to 602_d can be used. Furthermore, channel protection is achieved by laminating materials applicable to insulating layers 602_a to 602_d. An insulating layer that functions as a layer may be constructed.
[0160] Furthermore, a base layer is formed on the element-forming layer 600_a to the element-forming layer 600_d, and the A transistor may be formed on top of a geological layer. In this case, the underlying layer may be, for example, an insulating layer 6. A layer of material applicable to 02_a to insulating layer 602_d can be used. The underlayer may be constructed by laminating materials applicable to layer 602_a to insulating layer 602_d. i. For example, the base layer is constructed by laminating an aluminum oxide layer and a silicon oxide layer. As a result, oxygen contained in the underlying layer is removed via semiconductor layer 603_a to semiconductor layer 603_d It can prevent them from letting go.
[0161] Furthermore, as an example of the transistor fabrication method in this embodiment, the transistor shown in Figure 5(A) An example of a method for manufacturing a generator will be explained using Figure 6. Figure 6 shows the transformer shown in Figure 5(A). This is a schematic cross-sectional diagram illustrating an example of a method for manufacturing a generator.
[0162] First, as shown in Figure 6(A), prepare the element formation layer 600_a, and the element formation layer 600 A first conductive film is formed on _a, and a portion of the first conductive film is etched to make it conductive. Forms layer 601_a.
[0163] For example, by using the sputtering method to form a film of a material applicable to the conductive layer 601_a A first conductive film can be formed by this. Furthermore, materials applicable to the first conductive film It is also possible to form a first conductive film by stacking films.
[0164] Furthermore, impurities such as hydrogen, water, hydroxyl groups, or hydrides may be used as the sputtering gas. By using a highly purified gas from which impurities have been removed, the concentration of the above-mentioned impurities in the formed film is reduced. It is possible.
[0165] Before forming the film using the sputtering method, the preheating chamber of the sputtering apparatus is used. A preheating treatment may be performed. By performing the above preheating treatment, hydrogen and moisture are removed. Which impurities can be removed?
[0166] Furthermore, before forming the film using the sputtering method, for example, argon, nitrogen, helium, Alternatively, in an oxygen atmosphere, without applying voltage to the target side, apply voltage to the substrate side using an RF power supply. A process is performed to modify the surface to be formed by applying a plasma (also called reverse sputtering). This is also good. By performing reverse sputtering, powdery material (particles) adhering to the surface to be formed can be removed. It can remove (also called garbage).
[0167] Furthermore, when forming a film using the sputtering method, an adsorption-type vacuum pump is used, It can remove residual moisture in the film deposition chamber where the film is formed. For example, using a cryopump, ion pump, or titanium sublimation pump. This can be done. In addition, a turbomolecular pump equipped with a cold trap can be used to control the temperature inside the deposition chamber. It can also remove residual moisture. By using the vacuum pump described above, impurities can be removed from the waste. It can reduce the backflow of energy.
[0168] Furthermore, as in the method for forming the conductive layer 601_a described above, the transistor in this embodiment In the example of a fabrication method, when a layer is formed by etching a part of the film, for example, photolithography A resist mask is formed on a portion of the film using a graphing process, and the resist mask is used to film A layer can be formed by etching. In this case, after the layer is formed... Remove the resist mask.
[0169] Alternatively, a resist mask may be formed using an inkjet method. By using this method, photomasks become unnecessary, thus reducing manufacturing costs. Furthermore, by using an exposure mask (also called a multi-tone mask) that has multiple regions with different transmittances... A resist mask may be formed. By using a multi-gradation mask, regions of different thicknesses can be formed. A resist mask with a region can be formed, and the resist used in the fabrication of transistors The number of tomasks can be reduced.
[0170] Next, as shown in Figure 6(B), a first insulating film is formed on the conductive layer 601_a. Further insulating layer 602_a is formed.
[0171] For example, methods such as sputtering and plasma CVD can be used to apply to the insulating layer 602_a. A first insulating film can be formed by forming a film of such a material. Also, an insulating layer 6 A first insulating film can also be formed by laminating films of materials applicable to 02_a. It is possible. Also, high-density plasma CVD (for example, μ-wave (for example, μ with a frequency of 2.45 GHz) A film of material applicable to the insulating layer 602_a using high-density plasma CVD (using waves) By forming this, the insulating layer 602_a can be made denser, and the insulating layer 602_a The dielectric strength can be improved.
[0172] Next, as shown in Figure 6(C), an oxide semiconductor film is formed on the insulating layer 602_a, A semiconductor layer 603_a is formed by etching a portion of the post-oxide semiconductor film.
[0173] For example, an oxide semiconductor material applicable to the semiconductor layer 603_a using the sputtering method By forming a film, an oxide semiconductor film can be formed. Note that under a noble gas atmosphere. The oxide semiconductor film may be formed under an oxygen atmosphere, or under a mixed atmosphere of a noble gas and oxygen. Furthermore, when forming an oxide semiconductor layer which is CAAC as the semiconductor layer 603_a, spa Using the taring method, the temperature of the layer to be formed where the oxide semiconductor film is created is set to 100°C or higher. The oxide semiconductor film is formed at a temperature of 0°C or lower, preferably between 200°C and 350°C. In this case, it is preferable that the concentration of impurities such as hydrogen or water in the sputtering apparatus is extremely low. For example, by performing heat treatment before the formation of the oxide semiconductor film, the inside of the sputtering apparatus The concentration of impurities such as hydrogen or water can be reduced. Also, at this time, the insulating layer 60 2_a is preferably flat. For example, the average surface roughness of the insulating layer 602_a is 0.5 It is preferable that the size is less than nm, and even more preferably 0.1 nm or less.
[0174] Also, as a sputtering target, In2O3:Ga2O3:ZnO=1:1:1 Forming an oxide semiconductor film using an oxide target with a composition ratio of [molar ratio]. This is possible. Also, for example, In2O3:Ga2O3:ZnO = 1:1:2 [molar ratio] An oxide semiconductor film may be formed using an oxide target with the following composition ratio.
[0175] Furthermore, when using the sputtering method, for example, under a noble gas (typically argon) atmosphere... The semiconductor layer 603_a is formed under an oxygen atmosphere, or under a mixed atmosphere of a noble gas and oxygen. In this case, when forming the semiconductor layer 603_a in a mixed atmosphere of noble gas and oxygen, the noble gas A higher amount of oxygen relative to the amount of other substances is preferable.
[0176] Next, as shown in Figure 6(D), a second layer is placed on the insulating layer 602_a and the semiconductor layer 603_a. A conductive film is formed, and a portion of the second conductive film is etched to form the conductive layer 605a_a and A conductive layer 605b_a is formed.
[0177] For example, a suitable method can be used to apply the conductive layers 605a_a and 605b_a to the conductive layer 605a_a using a sputtering method. A second conductive film can be formed by forming a film of a usable material. By laminating films of materials applicable to the electrical layer 605a_a and the conductive layer 605b_a, A second conductive film can also be formed.
[0178] Next, as shown in Figure 6(E), the insulating layer 606_a is placed in contact with the semiconductor layer 603_a. To form.
[0179] For example, under a noble gas (typically argon) atmosphere, under an oxygen atmosphere, or a mixture of noble gas and oxygen In a suitable atmosphere, a film applicable to the insulating layer 606_a is formed using the sputtering method. By doing so, an insulating layer 606_a can be formed. Using the sputtering method, an insulating layer By forming 606_a, it functions as the back channel of the transistor. The decrease in resistance in the semiconductor layer 603_a can be suppressed. The substrate temperature when forming 06_a is preferably between room temperature and 300°C.
[0180] Furthermore, before forming the insulating layer 606_a, a plastic using a gas such as N2O, N2, or Ar is used. Zuma treatment is performed to remove adsorbed water and other substances adhering to the surface of the exposed semiconductor layer 603_a. It is also acceptable. If plasma treatment is performed, the insulating layer 606_ may be left untreated afterward without being exposed to the atmosphere. It is preferable to form a.
[0181] Furthermore, in the example of the transistor fabrication method shown in Figure 5(A), for example, 600°C or more and 75°C Heat treatment is performed at a temperature below 0°C, or above 600°C but below the strain point of the substrate. For example, oxide After forming a semiconductor film, a portion of the oxide semiconductor film is etched, and then a second conductive film is formed. After that, after etching a portion of the second conductive film, or after forming the insulating layer 606_a The above heat treatment is performed.
[0182] The heat treatment apparatus used for the above heat treatment may include an electric furnace or a heat source such as a resistance heating element. A device can be used that heats the object to be processed by heat conduction or thermal radiation, for example, GR TA (Gas Rapid Thermal Annealing) device or LRTA ( RTA (Ra) devices such as Lamp Rapid Thermal Annealing (RA) A pid (thermal annealing) device can be used. LRTA device Examples of lamps include halogen lamps, metal halide lamps, xenon arc lamps, and carbon Light emitted from lamps such as arc lamps, high-pressure sodium lamps, or high-pressure mercury lamps ( It is a device that heats the object to be processed by radiation (electromagnetic waves). Furthermore, the GRTA device is a high-temperature device. This is a device that performs heat treatment using gas. Examples of high-temperature gases include noble gases, or heating gases. An inert gas (such as nitrogen) that does not react with the material being treated during the process can be used.
[0183] Furthermore, after the above heat treatment, the temperature is maintained or reduced from that temperature. In the process, high-purity oxygen gas, high-purity N2O gas, and You may also introduce ultra-dry air (an atmosphere with a dew point of -40°C or lower, preferably -60°C or lower). In this case, it is preferable that the oxygen gas or N2O gas does not contain water, hydrogen, etc. Furthermore, the purity of the oxygen gas or N2O gas introduced into the heating apparatus should be 6N or higher, preferably 7N. The impurity concentration in oxygen gas or N2O gas should be 1 ppm or less, preferably above N, i.e., 1 ppm or less. It is preferable to keep it at 0.1 ppm or less. Due to the action of oxygen gas or N2O gas, semiconductor Oxygen is supplied to layer 603_a, reducing defects caused by oxygen deficiency in the semiconductor layer 603_a. This can be done using the above-mentioned high-purity oxygen gas, high-purity N2O gas, or ultra-dry air. The introduction of this may be performed during the heat treatment described above.
[0184] Furthermore, after the formation of the insulating layer 602_a, and after the formation of the oxide semiconductor film, the source electrode or drain electrode and After forming a conductive layer, after forming an insulating layer on the conductive layer that will become the source electrode or drain electrode, Oxygen doping treatment using oxygen plasma may be performed after heat treatment. For example, 2.45G Oxygen doping treatment may be performed using a high-density plasma at Hz. Alternatively, ion implantation may be used. Oxygen doping treatment may be performed using this method. By performing oxygen doping treatment, This can reduce variations in the electrical characteristics of transistors. For example, oxygen doping After performing a polishing treatment, one or both of the insulating layer 602_a and insulating layer 606_a are subjected to stoichiometric treatment. The oxygen content should be higher than the composition ratio.
[0185] By creating an excess of oxygen in the insulating layer in contact with the semiconductor layer 603_a, the semiconductor layer 603_ It becomes easier to supply to a. Therefore, in the semiconductor layer 603_a, or the insulating layer 602_a and the insulating layer Reduce oxygen vacancies at the interface between one or both of the marginal layers 606_a and the semiconductor layer 603_a. Therefore, the carrier concentration in the semiconductor layer 603_a can be further reduced. Furthermore, not limited to this, if the manufacturing process results in an excess of oxygen in the semiconductor layer 603_a Even in that case, the insulating layer in contact with the semiconductor layer 603_a prevents the semiconductor layer 603_ from This can suppress the elimination of oxygen from a.
[0186] For example, gallium oxide may be used as one or both of the insulating layers 602_a and 606_a. When forming an insulating layer containing oxygen, oxygen is supplied to the insulating layer, and the composition of gallium oxide is Ga2O x It can be done.
[0187] Furthermore, aluminum oxide may be used as one or both of the insulating layers 602_a and 606_a. When forming an insulating layer containing, oxygen is supplied to the insulating layer, and the composition of aluminum oxide is Al 20 x It can be done.
[0188] Furthermore, gallium oxide aluminum is used as one or both of the insulating layers 602_a and 606_a. When forming an insulating layer containing aluminum or aluminum gallium oxide, oxygen is added to the insulating layer. The composition of gallium aluminum oxide or aluminum gallium oxide is Ga x Al2 -x O 3+α It can be done this way.
[0189] Through the above process, hydrogen, water, hydroxyl groups, or hydrides (hydrogenated The purpose is to eliminate impurities such as compounds and to supply oxygen to the semiconductor layer 603_a. This allows for higher purity of the oxide semiconductor layer.
[0190] Furthermore, separate from the above heat treatment, after forming the insulating layer 606_a, under an inert gas atmosphere , or heat treatment under an oxygen gas atmosphere (preferably 200°C to 600°C, for example 25°C) You may also perform the procedure at temperatures between 0°C and 350°C.
[0191] Furthermore, as shown in Figure 6(E), a third conductive film is formed on the insulating layer 606_a, and the third A conductive layer 608_a is formed by etching a portion of the conductive film.
[0192] For example, by using the sputtering method to form a film of a material applicable to the conductive layer 608_a A third conductive film can be formed by this. Furthermore, materials applicable to the third conductive film It is also possible to stack films to form a third conductive film.
[0193] Although Figure 5(A) shows an example of a transistor fabrication method, it is not limited to this, for example... In each component shown in Figures 5(B) to 5(D), the names are those of each component shown in Figure 5(A). Even if the elements are the same and at least part of their function is the same as each component shown in Figure 5(A) The explanation of the example transistor fabrication method shown in Figure 5(A) can be appropriately referenced.
[0194] Furthermore, as shown in Figures 5(C) and 5(D), regions 604a_c and 604a_d , or when forming regions 604b_c to 604b_d, it functions as a gate. From the side where the conductive layer having is formed, through the insulating layer that functions as a gate insulating layer, semi By adding a dopant to the conductor layer, region 604a_c and region 604 are self-aligned. a_d, and regions 604b_c and 604b_d are formed.
[0195] For example, adding a dopant using an ion doping device or ion implantation device can.
[0196] As explained using Figures 5 and 6, an example of a transistor in this embodiment is a G A conductive layer that functions as a gate, an insulating layer that functions as a gate insulating layer, and A conductive layer that functions as a gate is superimposed via an insulating layer that functions as an insulating layer. And, an oxide semiconductor layer in which a channel is formed, and electrically connected to the oxide semiconductor layer, A conductive layer having the function of either a drain or a suction layer, and electrically connected to an oxide semiconductor layer. The structure includes a conductive layer that functions as both a source and a drain.
[0197] The oxide semiconductor layer in which the above channel is formed can be purified to be type I or substantially This is an oxide semiconductor layer that has become type I. By increasing the purity of the oxide semiconductor layer, acid The carrier concentration of the semiconductor layer is 1 × 10⁻⁶ 14 / cm 3 Less than 1 × 10 12 / c m 3 Less than 1 × 10 11 / cm 3 It can be less than the above. By using this structure, the off-current per 1 μm of channel width is 10 aA (1 × 10⁻¹⁰). -17 A) Keep it below this limit, and furthermore, set the off-current per 1 μm of channel width to 1 aA (1 × 10⁻¹⁰). - 18 A) Furthermore, the off-current per 1 μm of channel width should be 10 zA (1 × 10 -20 A) Furthermore, the off-current per 1 μm of channel width is 1 zA (1 × 10⁻¹⁰). -21 A) Below Furthermore, the off-current per 1 μm of channel width is 100 yA (1 × 10⁻¹⁰). -22 A) Below This can be done. The lower the transistor's off-current, the better, but in this implementation... The lower limit of the transistor's off-current in this state is approximately 10 -30 It is estimated to be A / μm. It can be done.
[0198] A transistor including the oxide semiconductor layer of this embodiment, for example, as described in the above embodiment By using it in the control transistor of a memory device, data retention in the memory cell is achieved. The duration can be extended.
[0199] (Embodiment 4) This embodiment describes an example of the structure of the storage device in the above embodiment.
[0200] The memory device in this embodiment has channels formed and contains elements from Group 14 of the periodic table. A transistor containing a semiconductor layer containing a semiconductor (such as silicon), and a channel formed It is constructed using a transistor that includes an oxide semiconductor layer. At this time, a channel is formed. A transistor containing an oxide semiconductor layer is a semiconductor of Group 14 in the periodic table (silicon It can be stacked on top of a transistor containing a semiconductor layer containing elements (such as ions). Transitions containing semiconductor layers that include semiconductors (such as silicon) of Group 14 in the periodic table For example, the transistors in the comparison circuit 101 and comparison circuit 102 in Figure 1 are suitable. It is used.
[0201] A transistor containing a semiconductor layer containing semiconductors (such as silicon) from Group 14 of the periodic table. An example of stacking transistors containing an oxide semiconductor layer on which a channel is formed on a zista. This is shown in Figure 7. Note that Figure 7 includes components that differ from the actual dimensions.
[0202] In Figure 7, the semiconductor layer 780, the insulating layer 784a, the insulating layer 784b, and the conductive layer 785a are shown. , conductive layer 785b, insulating layer 786a, insulating layer 786b, insulating layer 786c, insulating layer 786d, insulating layer 788, semiconductor layer 753, conductive layer 754a, conductive layer 754b , insulating layer 755, conductive layer 756, insulating layer 757a, insulating layer 757b, insulating layer 75 8, insulating layer 759, conductive layer 760a, conductive layer 760b, in the periodic table of elements A P-channel type transistor containing a semiconductor layer containing a Group 14 semiconductor (such as silicon) Transistors (for example, corresponding to transistor 112 shown in Figure 2(A)) and N-channel transistors (For example, this corresponds to transistor 111 shown in Figure 2(A)) and the oxide semiconductor in which the channel is formed A transistor containing a conductive layer (for example, corresponding to transistor 131 shown in Figure 2(A)) is formed. It will be done.
[0203] Furthermore, the semiconductor layer 780 comprises regions 782a, 782b, 782c, and 78 It has 2d. Furthermore, the semiconductor layer 780 is provided by insulating regions 781a to 781c Each transistor is electrically isolated.
[0204] For example, a semiconductor substrate can be used as the semiconductor layer 780. Alternatively, on another substrate... The semiconductor layer provided therein can also be used as semiconductor layer 780.
[0205] Furthermore, in the semiconductor layer 780, insulating isolation regions may be provided between multiple memory cells. stomach.
[0206] Regions 782a and 782b are provided spaced apart from each other and provide a P-type conductivity. This is the region to which the pant is added. Regions 782a and 782b are the P-channel type described above. It functions as the source or drain region of a transistor. For example, region 782 Regions a and 782b may each be electrically connected to a separately provided conductive layer.
[0207] Regions 782c and 782d are provided spaced apart from each other and provide an N-type conductivity. This is the region to which the pant has been added. Regions 782c and 782d are the above N-channel type It functions as the source or drain region of a transistor. For example, region 782 Each of regions c and 782d is a separately provided conductive layer (for example, functioning as a data line). It may be electrically connected to a conductive layer having [a certain characteristic].
[0208] Furthermore, a low-concentration region may be provided in part of regions 782a to 782d. Even if the depth of the degree region is smaller than the depth of the other regions 782a to 782d That's good, but it's not limited to that.
[0209] The insulating layer 784a is the semiconductor layer 780 sandwiched between insulating region 781a and insulating region 781b. It is provided on top of the region. The insulating layer 784a is the gate insulating layer of the P-channel transistor. It functions as a layer.
[0210] The insulating layer 784b is sandwiched between the insulating region 781b and the insulating region 781c of the semiconductor layer 780. It is provided on top of the region. The insulating layer 784b is the gate insulating layer of the N-channel transistor. It functions as a layer.
[0211] Examples of insulating layers 784a and 784b include silicon oxide, silicon nitride, and oxide Silicon nitride, silicon nitride oxide, aluminum oxide, aluminum nitride, aluminum oxide nitride Aluminum, aluminum nitride oxide, hafnium oxide, organic insulating materials (e.g., polyimide or A layer of material such as acrylic can be used. In addition, insulating layer 784a and insulating The insulating layer 784a and insulating layer 784b are constructed by laminating a material applicable to layer 784b. That's good too.
[0212] The conductive layer 785a is superimposed on the semiconductor layer 780 via the insulating layer 784a. The region of the semiconductor layer 780 superimposed on it is the channel formation region of the P-channel type transistor. The conductive layer 785a functions as the gate of the P-channel transistor. .
[0213] The conductive layer 785b is superimposed on the semiconductor layer 780 via the insulating layer 784b. The region of the semiconductor layer 780 superimposed on it is the channel formation region of the above N-channel type transistor. The conductive layer 785b functions as the gate of the above N-channel transistor. .
[0214] Examples of conductive layers 785a and 785b include molybdenum, magnesium, and titanium. chromium, tantalum, tungsten, aluminum, copper, neodymium, or scandium Layers of metallic materials such as lum, or alloy materials mainly composed of these, can be used. By laminating materials applicable to conductive layer 785a and conductive layer 785b, conductive layer 785a and It is also possible to form a conductive layer 785b.
[0215] The insulating layer 786a is provided on top of the insulating layer 784a, and in the conductive layer 785a, opposite each other It is in contact with one of the pair of facing sides.
[0216] The insulating layer 786b is provided on top of the insulating layer 784a, and in the conductive layer 785a, opposite each other It is in contact with the other of the pair of sides facing it.
[0217] The insulating layer 786c is provided on the insulating layer 784b, and in the conductive layer 785b, opposite each other It is in contact with one of the pair of facing sides.
[0218] The insulating layer 786d is provided on the insulating layer 784b, and in the conductive layer 785b, opposite each other It is in contact with the other of the pair of sides facing it.
[0219] The insulating layer 788 consists of insulating layer 786a, insulating layer 786b, insulating layer 786c, and insulating layer 786 It is placed above d.
[0220] The insulating layers 786a to 786d, and insulating layer 788 are insulating layer 784a and insulating layer 784a. Among the materials applicable to the edge layer 784b, the materials applicable to the insulating layer 784a and insulating layer 784b A layer of the same material as the material or a layer of a different material can be used. In addition, insulating layers 786a to By laminating materials applicable to insulating layer 786d and insulating layer 788, insulating layer 786a to Insulating layers 786d and 788 can also be formed.
[0221] The semiconductor layer 753 is provided on top of the insulating layer 788. The semiconductor layer 753 is located in region 752a and This includes region 752b. Regions 752a and 752b are regions to which the dopant has been added. It exists and has the function of a source area or drain area. As a dopant, the above actual Applicable dopants to transistors containing oxide semiconductor layers in the form of application are used as appropriate. It is possible.
[0222] For the semiconductor layer 753, for example, a material applicable to the semiconductor layer 603_a shown in Figure 5(A) is suitable. The following layers can be used.
[0223] The insulating layer 755 is provided on top of the semiconductor layer 753.
[0224] The insulating layer 755 functions as the gate insulating layer of the transistor.
[0225] The insulating layer 755 is, for example, a layer of material applicable to the insulating layer 602_a shown in Figure 5(A). It can be used. In addition, the insulating layer 755 can be made by laminating a material applicable to the insulating layer 755. It may be configured as follows:
[0226] The conductive layer 756 is superimposed on the semiconductor layer 753 via the insulating layer 755. The conductive layer 756 is It functions as a gate for the lunger.
[0227] The conductive layer 756 is, for example, a layer of material applicable to the conductive layer 601_a shown in Figure 5(A). It can be used. In addition, the conductive layer 756 can be formed by laminating a material applicable to the conductive layer 756. It may be configured as follows:
[0228] The insulating layer 757a and insulating layer 757b are in contact with the side surface of the conductive layer 756 and on top of the insulating layer 755. It will be established.
[0229] The conductive layer 754a is electrically connected to the semiconductor layer 753 by contact. It is electrically connected to the conductive layer 785a. The conductive layer 754a contains the above oxide semiconductor layer It functions as either the source or drain of a transistor.
[0230] The conductive layer 754b is electrically connected to the semiconductor layer 753 by contact. It is electrically connected to the conductive layer 785b. The conductive layer 754b contains the oxide semiconductor layer mentioned above. It functions as either the source or drain of a transistor.
[0231] For example, conductive layer 754a and conductive layer 754b are conductive layer 605a_ shown in Figure 5(A). A layer of material applicable to a and conductive layer 605b_a can be used. Also, conductive layer 7 Lamination of materials applicable to 54a and conductive layer 754b results in conductive layer 754a and conductive layer 75 4b may also be constructed.
[0232] The insulating layer 758 is composed of the conductive layer 756, insulating layer 757a, insulating layer 757b, conductive layer 754a, and It is provided on top of the conductive layer 754b.
[0233] The insulating layer 758 is, for example, a layer of material applicable to the insulating layer 602_a shown in Figure 5(A). It can be used. In addition, the insulating layer 758 can be made by laminating a material applicable to the insulating layer 758. The insulating layer 758 has the function of a protective layer that suppresses the intrusion of impurities. ru.
[0234] The insulating layer 759 is provided on top of the insulating layer 758.
[0235] The insulating layer 759 is, for example, a layer of material applicable to the insulating layer 602_a shown in Figure 5(A). It can be used. In addition, the insulating layer 759 can be made by laminating a material applicable to the insulating layer 759. It may be configured as follows:
[0236] The conductive layer 760a is connected to the conductive layer 7 through openings provided in the insulating layer 758 and the insulating layer 759. It is electrically connected to 54a. The conductive layer 760a is a transistor containing an oxide semiconductor layer. It functions as either a source or a drain.
[0237] The conductive layer 760b is transmitted to the conductive layer 7 through openings provided in the insulating layer 758 and the insulating layer 759. It is electrically connected to 54b. The conductive layer 760b is a transistor containing an oxide semiconductor layer. It functions as either a source or a drain.
[0238] For example, conductive layer 760a and conductive layer 760b are conductive layer 605a_ shown in Figure 5(A). A layer of material applicable to a and conductive layer 605b_a can be used. Also, conductive layer 7 Lamination of materials applicable to 60a and conductive layer 760b results in conductive layer 760a and conductive layer 76 You may also construct 0b.
[0239] The above is a description of the example structure of the storage device shown in Figure 7.
[0240] As explained with reference to Figure 7, in the example of the storage device structure in this embodiment, different materials By stacking transistors using semiconductor layers to construct a memory device, the circuit area It can be made smaller.
[0241] (Embodiment 5) This embodiment describes an example of a processing unit such as a CPU.
[0242] An example of the arithmetic processing unit in this embodiment will be explained with reference to Figure 8.
[0243] The arithmetic processing unit shown in Figure 8 consists of a bus interface (also called IF) 801 and a control unit. (Also called CTL) 802, cache memory (also called CACH) 803, and M pieces ( M is a natural number greater than or equal to 3) Register 804 (also called Regi) (register 804_1 to Register 804_M), instruction decoder (also called IDecoder) 805, and operation theory It is equipped with a processing unit (also called an ALU) 806.
[0244] The bus interface 801 facilitates the exchange of signals with the outside world and the various circuits within the arithmetic processing unit. It has the function of exchanging signals with other devices.
[0245] The control device 802 has the function of controlling the operation of each circuit in the arithmetic processing unit.
[0246] The cache memory 803 is controlled by the control unit 802 and controls the operation of the arithmetic processing unit. It has a function to temporarily hold data at any given time. For example, a primary cache and a secondary cache. Multiple cache memories 803 may be provided in the arithmetic processing unit as caches. For example, The memory device in the above embodiment is used as an associative memory in the cache memory 803. It is possible.
[0247] The M registers 804 are controlled by the control unit 802 and contain data used for arithmetic processing. It has the function of storing. For example, a register 804 is a register for the arithmetic logic unit 806. Alternatively, another register 804 may be used as the register for the instruction decoder 805.
[0248] The instruction decoder 805 has the function of translating the received instruction signal. The command signal is input to the control device 802, and the control device 802 calculates the control signal corresponding to the command signal. Output to processing unit 806.
[0249] The arithmetic logic unit 806 is controlled by the control device 802 and responds to input command signals. It has the function of performing calculations.
[0250] As explained with reference to Figure 8, the arithmetic processing unit in this embodiment has a cache memory By reducing the area of the arithmetic processing unit, the area of the processing unit can be reduced.
[0251] Furthermore, in an example of the arithmetic processing unit in this embodiment, the cache memory is configured as described above. By using a state memory device, data stored in the cache memory according to the search data A function to select whether or not to output data can be added to the cache memory.
[0252] Furthermore, in the arithmetic processing unit of this embodiment, when the supply of power voltage is stopped, Also, in the cache memory, some of the internal data is retained immediately before the power supply voltage is cut off. It can maintain the state of the processing unit when the power supply voltage is restored. It is possible to return to the state just before the power supply was stopped. Therefore, the power supply voltage can be selectively stopped. Even if power consumption is reduced, normal operation will only begin after the power supply voltage is restored. This can shorten the time it takes to complete the task.
[0253] (Embodiment 6) In this embodiment, the c-axis oriented and triangular in shape when viewed from the direction of the ab-plane, surface, or interface. It has a hexagonal atomic arrangement, and along the c-axis, metal atoms are layered or metal atoms and oxygen atoms are arranged They are arranged in layers, and in the ab plane, the orientation of the a axis or b axis is different (rotating around the c axis). This section describes oxides containing the phase (oxides containing CAAC).
[0254] CAAC-containing oxides, in a broad sense, are non-single crystals that can be viewed from a direction perpendicular to their ab-plane. The atoms have a triangular, hexagonal, equilateral triangle, or regular hexagonal arrangement, and are perpendicular to the c-axis direction. When viewed from the front, the oxide contains a layered structure of metal atoms, or a layered structure of metal atoms and oxygen atoms. It refers to.
[0255] CAAC is not a single crystal, but it is not formed solely from amorphous material either. AC contains crystalline parts (crystalline portions), but the boundary between one crystalline portion and another is not clearly defined. Sometimes it's impossible to determine for sure.
[0256] If CAAC contains oxygen, some of the oxygen may be replaced with nitrogen. The c-axis of each individual crystal portion that makes up the structure is in a specific direction (for example, the substrate surface on which CAAC is formed). They may be aligned in a direction perpendicular to the surface of the CAAC, etc. Or, each of the components of the CAAC The normal to the ab plane of the crystalline portion is in a certain direction (for example, the substrate surface on which CAAC is formed, CAA It may be oriented perpendicular to the surface of C, etc.
[0257] CAAC can be a conductor, a semiconductor, or an insulator, depending on its composition. Depending on its composition, it may be transparent or opaque to visible light. To do.
[0258] An example of such CAAC is one which is formed in a film-like manner and has a surface perpendicular to the film surface or the supporting substrate surface. When observed from the front, a triangular or hexagonal atomic arrangement is observed, and when the cross-section of the film is observed... Examples of crystals in which metal atoms or a layered arrangement of metal atoms and oxygen atoms (or nitrogen atoms) are observed. It is also possible to do so.
[0259] An example of the crystal structure contained in CAAC will be explained in detail using Figures 10 to 12. Unless otherwise specified, Figures 10 through 12 define the upward direction as the c-axis, and the direction perpendicular to the c-axis is used. Let the surface be called surface ab. Note that when simply referring to the upper half and the lower half, the boundary is surface ab. This refers to the upper half and the lower half. Also, in Figure 10, the circled O represents O with 4 coordination, and two The O enclosed in a double circle indicates a three-coordinate O.
[0260] Figure 10(A) shows one 6-coordinate In atom and six 4-coordinate oxygen atoms adjacent to the In atom (hereinafter referred to as 4 The structure shows a coordinated O) and a nearby oxygen atom. Here, for each metal atom, A structure showing only the children is called a small group. The structure in Figure 10(A) takes the form of an octahedron, but For simplicity, it is shown as a planar structure. Note that the upper and lower halves of Figure 10(A) each contain 3 There are 4-coordinate oxygen atoms in each group. The small group shown in Figure 10(A) has a charge of 0.
[0261] Figure 10(B) shows one 5-coordinate Ga atom and three 3-coordinate oxygen atoms adjacent to the Ga atom (hereinafter referred to as 3 The structure shows a coordinated oxygen atom and two adjacent four-coordinate oxygen atoms. The three-coordinate oxygen atoms are all It also exists in the ab plane. Figure 10(B) has one 4-coordinate O in the upper half and one in the lower half. There is also In, since In also takes on a 5-coordinate structure, it can take on the structure shown in Figure 10(B). Figure 10( The subgroup shown in B) has a charge of 0.
[0262] Figure 10(C) shows a structure having one 4-coordinate Zn and four 4-coordinate O adjacent to the Zn. The structure is shown. The upper half of Figure 10(C) has one 4-coordinate oxygen atom, and the lower half has three 4-coordinate oxygen atoms. There is an O. Also, there are three 4-coordinate Os in the upper half of Figure 10(C) and one 4 in the lower half. Coordinating oxygen may be present. The small group shown in Figure 10(C) has a charge of 0.
[0263] Figure 10(D) shows a structure having one 6-coordinate Sn and six 4-coordinate O adjacent to the Sn. The structure is shown. The upper half of Figure 10(D) has 3 four-coordinate oxygen atoms, and the lower half has 3 four-coordinate oxygen atoms. There is an O. The small group shown in Figure 10(D) has a charge of +1.
[0264] Figure 10(E) shows a small group containing two Zn molecules. The upper half of Figure 10(E) shows one There is a 4-coordinate oxygen atom, and the lower half has one 4-coordinate oxygen atom. The subgroup is shown in Figure 10(E). The charge becomes -1.
[0265] Here, a collection of multiple small groups is called a medium group, and a collection of multiple medium groups is This is called a large group (also known as a unit cell).
[0266] Here, we will explain the rules by which these subgroups combine. These rules are shown in Figure 10(A). The three oxygen atoms in the upper half of the 6-coordinate In each have three adjacent oxygen atoms in the lower half, and the three oxygen atoms in the lower half... Each oxygen atom has three adjacent in atoms in the upward direction. The single oxygen atom in the upper half of the 5-coordinate Ga is One adjacent Ga is located downwards, and one O in the lower half has one adjacent Ga located upwards. The single oxygen atom in the upper half of the 4-coordinate Zn has one adjacent Zn atom below it, and the three oxygen atoms in the lower half are Each atom has three adjacent Zn atoms in the upward direction. Thus, the metal atom has four-coordinate oxygen atoms in the upward direction. The number of atoms is equal to the number of nearby metal atoms below that O, and similarly, the number of metal atoms below the 4 The number of oxygen atoms in coordination is equal to the number of nearby metal atoms above that oxygen atom. Since oxygen is 4-coordinate, The sum of the number of nearby metal atoms below and the number of nearby metal atoms above is 4. Therefore, The number of 4-coordinate oxygen atoms above a metal atom and the number of 4-coordinate oxygen atoms below another metal atom When the sum of the number of atoms is 4, two small groups of metal atoms can bond together. For example, a 6-coordinate metal atom (In or Sn) is bonded via a 4-coordinate oxygen atom in the lower half. In this case, since there are three 4-coordinate oxygen atoms, a 5-coordinate metal atom (Ga or In) or a 4-coordinate gold atom is required. It will bond with one of the group atoms (Zn).
[0267] Metal atoms with these coordination numbers are bonded in the c-axis direction via 4-coordinate oxygen atoms. In addition, multiple small groups combine such that the total charge of the layered structure becomes 0. It forms a middle group.
[0268] Figure 11(A) shows a model diagram of the intermediate groups that constitute the layered structure of the In-Sn-Zn-O system. Figure 11(B) shows the large group, which is composed of three medium groups. C) shows the atomic arrangement when the layer structure of Figure 11(B) is observed from the c-axis direction.
[0269] In Figure 11(A), for simplicity, three-coordinate oxygen atoms are omitted, and only the number of four-coordinate oxygen atoms is shown. For example, the upper and lower halves of Sn each contain three 4-coordinate oxygen atoms, as shown in the circle. It is shown as 3. Similarly, in Figure 11(A), the upper and lower halves of In are shown as 3. Each of these has one O with 4 coordination, which is shown as 1 in the circle. Similarly, Figure 11(A In this case, the lower half has one 4-coordinate oxygen atom, and the upper half has three 4-coordinate oxygen atoms. n and Zn, which has one 4-coordinate oxygen atom in the upper half and three 4-coordinate oxygen atoms in the lower half. It is showing.
[0270] In Figure 11(A), the middle group constituting the layered structure of the In-Sn-Zn-O system is from the top In order, Sn has three 4-coordinate oxygen atoms in the upper half and three in the lower half, and one 4-coordinate oxygen atom in the upper half. It bonds with In in the lower half, and that In bonds with Zn which has three 4-coordinate O atoms in the upper half. Bonded, and through one four-coordinate oxygen atom in the lower half of the Zn, three four-coordinate oxygen atoms are bonded to the upper half and It bonds with In in the lower half, and that In then bonds with two Zn atoms that have one 4-coordinate O in the upper half. It combines with a small group, and through one 4-coordinate O in the lower half of this small group, a 4-coordinate O The structure consists of three oxygen atoms bonded to Sn atoms in the upper half and three in the lower half. Multiple groups are combined to form a larger group.
[0271] Here, in the case of 3-coordinate oxygen and 4-coordinate oxygen, the charge per bond is -0.66, respectively. 7, can be considered as -0.5. For example, In (6-coordinate or 5-coordinate), Zn (4-coordinate) The charges of ) and Sn (5-coordinate or 6-coordinate) are +3, +2, and +4, respectively. Therefore, S The small group containing n has a charge of +1. Therefore, in order to form a layered structure containing Sn Therefore, a charge of -1 is needed to cancel out the charge of +1. As an example of a structure that takes on a charge of -1, see Figure 10(E As shown in ( ), a small group containing two Zn is an example. For example, a small group containing Sn If there is one small group containing two Zn atoms for each single Zn atom, the charges cancel each other out. The total charge of the layered structure can be set to 0.
[0272] Specifically, the large groups shown in Figure 11(B) are repeated, resulting in In-Sn-Zn -O-based crystals (In2SnZn3O8) can be obtained. -The layered structure of the Zn-O system is In2SnZn2O7(ZnO) m (m is 0 or a natural number.) It can be represented by the following empirical formula.
[0273] In addition, there are other metal oxides of quaternary metals, such as In-Sn-Ga-Zn-O metal oxides. These are substances, or ternary metal oxides, specifically In-Ga-Zn-O metal oxides (also written as IGZO). (To do.), In-Al-Zn-O metal oxides, Sn-Ga-Zn-O metal oxides, A l-Ga-Zn-O metal oxides, Sn-Al-Zn-O metal oxides, and In-Hf- Zn-O metal oxide, In-La-Zn-O metal oxide, In-Ce-Zn-O gold Group oxides, In-Pr-Zn-O metal oxides, In-Nd-Zn-O metal oxides, I n-Sm-Zn-O metal oxide, In-Eu-Zn-O metal oxide, In-Gd-Z nO-based metal oxides, In-Tb-Zn-O-based metal oxides, In-Dy-Zn-O-based metals Oxides, In-Ho-Zn-O metal oxides, In-Er-Zn-O metal oxides, In -Tm-Zn-O metal oxide, In-Yb-Zn-O metal oxide, In-Lu-Zn -O-based metal oxides, and binary metal oxides such as In-Zn-O-based metal oxides and Sn-Z nO metal oxide, Al-Zn-O metal oxide, Zn-Mg-O metal oxide, Sn -Mg-O-based metal oxides, In-Mg-O-based metal oxides, and In-Ga-O-based metal oxides In-O metal oxides, Sn-O metal oxides, and Zn-O metal oxides are oxides of monocrystalline metals. The same applies when using metal oxides, etc.
[0274] For example, Figure 12(A) shows the intermediate group that constitutes the layered structure of the In-Ga-Zn-O system. A diagram is shown.
[0275] In Figure 12(A), the middle group constituting the layered structure of the In-Ga-Zn-O system is from the top In order, the in atoms have three 4-coordinate oxygen atoms in the upper half and three in the lower half, while the in atoms have one 4-coordinate oxygen atom in the upper half. It bonds with a Zn atom, and through the three 4-coordinate oxygen atoms in the lower half of that Zn atom, one 4-coordinate oxygen atom is bonded to each of them. It bonds with Ga in the upper and lower halves, and via one 4-coordinate O in the lower half of that Ga In this configuration, three 4-coordinate oxygen atoms are bonded to the in atoms in the upper and lower halves. Multiple groups combine to form a larger group.
[0276] Figure 12(B) shows the large group, which is composed of three medium groups. Figure 12(C) is Figure 12(B) shows the atomic arrangement when the layered structure is observed from the c-axis direction.
[0277] Here, the charges of In (6-coordinate or 5-coordinate), Zn (4-coordinate), and Ga (5-coordinate) are as follows: Since the values are +3, +2, and +3, the subgroup containing any of In, Zn, and Ga is electric. The load becomes 0. Therefore, with these combinations of small groups, the sum of the medium groups is The charge is always 0.
[0278] Furthermore, the intermediate groups that constitute the layered structure of the In-Ga-Zn-O system are shown in Figure 12(A). Not limited to medium groups, but combining medium groups with different arrangements of In, Ga, and Zn. The group could also be included.
[0279] (Embodiment 7) In this embodiment, the field-effect mobility of the transistor will be described.
[0280] The field-effect mobility of insulated-gate transistors, which is actually measured, is not limited to oxide semiconductors. For various reasons, mobility may be lower than it would be otherwise. Factors that reduce mobility include This includes defects within the semiconductor and defects at the interface between the semiconductor and the insulating film, but the Levinson model... Using this method, we can theoretically derive the field-effect mobility assuming there are no defects inside the semiconductor. Let it.
[0281] Let μ0 be the intrinsic mobility of the semiconductor, and μ be the measured field-effect mobility. Assuming the existence of tactical barriers (such as grain boundaries), the following equation can be used to express this.
[0282]
number
[0283] Here, E is the height of the potential barrier, k is the Boltzmann constant, and T is the absolute temperature. Furthermore, assuming that the potential barrier originates from a defect, in the Levinson model... It can be expressed by the following formula.
[0284]
number
[0285] Here, e is the elementary charge, N is the average defect density per unit area in the channel, and ε is the semiconductor's Dielectric constant, n is the number of carriers in the channel per unit area, Cox is per unit area The capacitance is Vg, the gate voltage is Vg, and the channel thickness is t. Note that semiconductors with a thickness of 30 nm or less In the case of a body layer, the channel thickness can be considered the same as the semiconductor layer thickness. The drain current Id is given by the following formula:
[0286]
number
[0287] Here, L is the channel length and W is the channel width, and in this case, L = W = 10 μm. Also, Vd is the drain voltage. Dividing both sides of the above equation by Vg and then taking the logarithm of both sides gives , it will be as follows.
[0288]
number
[0289] The right-hand side of equation 5 is a function of Vg. As can be seen from this equation, the vertical axis is ln(Id / Vg), The defect density N can be determined from the slope of a straight line with the horizontal axis being 1 / Vg. That is, in a transistor. The defect density can be evaluated from the Id-Vg characteristics. As an oxide semiconductor, indium (I In the case where the ratio of n, tin (Sn), and zinc (Zn) is In:Sn:Zn=1:1:1 The defect density N is 1 × 10⁻⁶ 12 / cm 2 It is to that extent.
[0290] Based on the defect density and other factors determined in this way, we can use equations 2 and 3 to conclude that μ0 = 120 cm². 2 / Vs The following is derived. The mobility measured in defective In-Sn-Zn oxide is 35 cm². 2 / V It is approximately s. However, oxide semiconductors without defects inside the semiconductor and at the interface between the semiconductor and the insulating film... Body mobility μ0 is 120 cm 2 It can be expected that the result will be / Vs.
[0291] However, even if there are no defects inside the semiconductor, scattering at the interface between the channel and the gate insulating layer can cause problems. The transport characteristics of the transistor are affected, specifically at the interface between the channel and the gate insulating layer. The mobility μ1 at a distance x from the point is expressed by the following formula:
[0292]
number
[0293] Here, D is the electric field in the gate direction, and B and G are constants. B and G are derived from actual measurement results. It can be calculated, and from the above measurement results, B = 4.75 × 10 7 cm / s, G=10n m is the depth to which interfacial scattering occurs. When D increases (i.e., the gate voltage increases) Since the second term of equation 6 increases, it can be seen that the mobility μ1 decreases.
[0294] Transistor mobility using an ideal oxide semiconductor channel with no defects inside the semiconductor. The results of the calculation of μ2 are shown in Figure 13. Note that the calculation was performed using a Synopsys device simulator. Using Sentaurus Device, a bandgap in oxide semiconductors. The top, electron affinity, relative permittivity, and thickness were measured at 2.8 electron volts and 4.7 electron volts, respectively. The values were set to 15 nm and 15 nm. These values were obtained by measuring thin films formed by the sputtering method. This was obtained through [method / method].
[0295] Furthermore, the work functions of the gate, source, and drain were set to 5.5 electron volts and 4.6 electron volts, respectively. The voltage was set to 4.6 electron volts. The gate insulating layer thickness was 100 nm, and the relative permittivity was set to 4.6 electron volts. The specification was set to 4.1. Both the channel length and channel width were 10 μm, and the drain voltage Vd was 0. It is 1V.
[0296] As shown in Figure 13, with a gate voltage of slightly over 1V, the mobility is 100cm. 2 Peaks greater than / Vs However, as the gate voltage increases further, interfacial scattering increases, and mobility decreases. Furthermore, in order to reduce interfacial scattering, the semiconductor layer surface must be made atomically flat (At (Crypto Layer Flatness) is desirable.
[0297] When a miniature transistor is fabricated using an oxide semiconductor with such mobility, The results of the calculations are shown in Figures 14 to 16. Note that the cross-sectional structure of the transistor used in the calculations is shown. The structure is shown in Figure 17. The transistor shown in Figure 17 has an oxide semiconductor layer n + It exhibits the following conductivity type. It has semiconductor region 2103a and semiconductor region 2103c. The resistivity of the conductor region 2103c is 2 × 10⁻⁶. -3 Let it be Ωcm.
[0298] The transistor shown in Figure 17(A) is embedded in the base insulating layer 2101 and in the base insulating layer 2101. Formed on top of an embedded insulator 2102 made of aluminum oxide that is formed to be embedded. The transistor consists of semiconductor region 2103a, semiconductor region 2103c, and the area sandwiched between them. It has an intrinsic semiconductor region 2103b that forms a channel formation region and a gate 2105. The width of gate 2105 is set to 33 nm.
[0299] A gate insulating layer 2104 is provided between the gate 2105 and the semiconductor region 2103b, and also, On both sides of gate 2105 are side wall insulators 2106a and 2106b, gate 2 Above 105 is an insulator 2107 to prevent short circuits between gate 2105 and other wiring. It has the width of the side wall insulator to be 5 nm. Also, semiconductor region 2103a and semiconductor region It has a source 2108a and a drain 2108b in contact with 2103c. The channel width in the transistor is set to 40 nm.
[0300] The transistor shown in Figure 17(B) consists of an underlay insulating layer 2101 and aluminum oxide. Semiconductor region 2103a, semiconductor region 2103c are formed on the embedded insulator 2102. And sandwiched between them is the true semiconductor region 2103b, and the gate 2105 with a width of 33 nm and The insulating layer 2104 and the side wall insulators 2106a and 2106b and the insulator 2107 The transistor shown in Figure 17(A) has a source 2108a and a drain 2108b. It is the same as Ta.
[0301] The difference between the transistor shown in Figure 17(A) and the transistor shown in Figure 17(B) is the side wall insulation. This is the conductivity type of the semiconductor region below the edge material 2106a and the side wall insulator 2106b. Figure 17(A In the transistor shown, the semiconductor under the side wall insulators 2106a and 2106b The body region is n + Semiconductor regions 2103a and 2103c exhibit the following conductivity type. In the transistor shown in Figure 17(B), this is the intrinsic semiconductor region 2103b. The semiconductor region 2103a (semiconductor region 2103c) and gate 2105 overlap by Loff. A region that cannot be accessed is created. This region is called the offset region, and its width Loff is the offset. This is called the offset length. As is clear from the diagram, the offset length is the side wall insulator 2106a (side wall insulator It is the same width as item 2106b).
[0302] Other parameters used in the calculations are as described above. The calculations were performed using a Synopsys device. The simulation software, Sentaurus Device, was used. Figure 14 shows The drain current (Id, solid line) and mobility of the transistor with the structure shown in Figure 17(A) are shown. This shows the dependence of μ (dotted line) on the gate voltage (Vg, potential difference between gate and source). Drain current Id is defined as the drain voltage (potential difference between drain and source) being +1V, and mobility μ is defined as the drain voltage. This calculation was performed assuming a voltage of +0.1V.
[0303] Figure 14(A) shows the gate insulating layer thickness as 15 nm, while Figure 14(B) shows it as 10 nm. This is set to m, and Figure 14(C) is set to 5 nm. The gate insulating layer becomes thinner. The drain current Id (off current), especially in the off state, decreases significantly. On the other hand, mobility There is no significant change in the peak value of μ or the drain current Id (on-current) in the ON state. It was shown that the drain current exceeds 10 μA at a power voltage of around 1 V.
[0304] Figure 15 shows a transistor with the structure shown in Figure 17(B), where the offset length Loff is 5n Dependence of drain current Id (solid line) and mobility μ (dotted line) of m on gate voltage Vg. This shows that the drain current Id is calculated with a drain voltage of +1V, and the mobility μ is calculated with a drain voltage of + This calculation was performed assuming a voltage of 0.1V. Figure 15(A) shows the gate insulating layer thickness as 15nm. Figure 15(B) shows the result with a 10nm wavelength, and Figure 15(C) shows the result with a 5nm wavelength. It is.
[0305] Furthermore, Figure 16 shows a transistor with the structure shown in Figure 17(B), with an offset length Loff The drain current Id (solid line) and mobility μ (dotted line) of a 15nm diode depend on the gate voltage. Existence is shown. Drain current Id is given by taking the drain voltage as +1V, and mobility μ is given by taking the drain voltage as +1V. This calculation was performed assuming a voltage of +0.1V. Figure 16(A) shows a gate insulating layer thickness of 15nm. Figure 16(B) shows the result at 10 nm, and Figure 16(C) shows the result at 5 nm. That is what happened.
[0306] In both cases, the thinner the gate insulating layer, the more significantly the off-current decreases, while the mobility μ is reduced. There are no significant changes in the quelcher value or on-current.
[0307] Note that the peak of mobility μ is at 80 cm in Figure 14. 2 It is approximately / Vs, but in Figure 15 it is 60 cm 2 Approximately / Vs, 40cm in Figure 16 2 / Vs and the offset length Loff increase It decreases significantly. Similarly, the off-current also shows a similar trend. On the other hand, the on-current has an offset length of Lo It decreases with increasing ff, but this decrease is much more gradual than the decrease in off-current. Furthermore, it was shown that in all cases, the drain current exceeded 10 μA at a gate voltage of around 1 V. .
[0308] (Embodiment 8) In this embodiment, an oxide semiconductor mainly composed of In, Sn, and Zn is used as the oxide semiconductor. I will now explain the transistors used.
[0309] A transistor that uses an oxide semiconductor with In, Sn, and Zn as its main components as the channel formation region is , heating the substrate to form the oxide semiconductor film, or oxide semiconductor film Good properties can be obtained by heat treatment after forming the material. Note that the main component is combined with This refers to elements present in a composition ratio of 5 atomic percent or more.
[0310] Intentionally heating the substrate after depositing an oxide semiconductor film mainly composed of In, Sn, and Zn. This makes it possible to improve the field-effect mobility of the transistor. This makes it possible to shift the threshold voltage positively and enable normal off mode.
[0311] For example, Figures 18(A) to (C) show a channel with In, Sn, and Zn as the main components and a channel length L of 3μ. A 10 μm thick oxide semiconductor film with a channel width W of 10 μm and a 100 nm thick gate insulating layer These are the characteristics of the transistor used. Vd was set to 10V.
[0312] Figure 18(A) shows the process of sputtering In, Sn, and Zn as the main components without intentionally heating the substrate. This is the transistor characteristic when an oxide semiconductor film is formed in this manner. At this time, the field effect transfer... The degree is 18.8cm 2 / Vsec is obtained. On the other hand, the substrate is intentionally heated and In, S Forming an oxide semiconductor film mainly composed of n and Zn improves the field effect mobility. This becomes possible. Figure 18(B) shows the substrate heated to 200°C, with In, Sn, and Zn as the main components. This shows the transistor characteristics when an oxide semiconductor film is formed, with a field-effect mobility of 32.2. cm 2 / Vsec is obtained.
[0313] The field-effect mobility is determined by the thermal treatment of an oxide semiconductor film mainly composed of In, Sn, and Zn. By applying this principle, it can be further enhanced. Figure 18(C) shows In, Sn, and Zn. An oxide semiconductor film mainly composed of [component name] is deposited by sputtering at 200°C, and then heat-treated at 650°C. The transistor characteristics under the specified conditions are shown. At this time, the field-effect mobility is 34.5 cm⁻¹. 2 / V sec has been obtained.
[0314] By intentionally heating the substrate, moisture during sputtering deposition is incorporated into the oxide semiconductor film. It is expected to reduce the amount of acid produced. In addition, by heat treatment after film formation, acid can also be reduced. Hydrogen, hydroxyl groups, or water can be released and removed from the ionized semiconductor film, as described above. This can improve the field effect mobility. Such improvement in field effect mobility leads to dehydration. In addition to the removal of impurities through chemical and dehydrogenation, the interatomic distance is shortened due to increased density. It is also presumed that crystallization can be achieved by removing impurities from oxide semiconductors to increase their purity. This can be measured. In this way, the highly purified non-single-crystal oxide semiconductor can ideally be 10 0cm 2 It is estimated that it will also be possible to achieve field-effect mobility exceeding / Vsec.
[0315] Oxygen ions are implanted into an oxide semiconductor mainly composed of In, Sn, and Zn, and then heat-treated to remove the acid By releasing hydrogen, hydroxyl groups, or water contained in the ion semiconductor, and simultaneously with the heat treatment or The oxide semiconductor may be crystallized by subsequent heat treatment. By performing a crystallization treatment, non-single-crystal oxide semiconductors with good crystallinity can be obtained.
[0316] The effect of intentionally heating the substrate to form a film and / or heat treating it after film formation is due to the electric field. In addition to improving effective mobility, it also contributes to enabling normally-off transistors. It exists. Oxide semiconductors mainly composed of In, Sn, and Zn formed without intentionally heating the substrate. In a transistor where a conductive film is used as the channel formation region, the threshold voltage is shifted to the negative. There is a tendency for this to happen. However, in the case of using an oxide semiconductor film formed by intentionally heating the substrate... In total, this negative shift of the threshold voltage is eliminated. In other words, the threshold voltage is The ZISTA is moving towards being normally off, and this trend is shown in Figures 18(A) and 18(B). This can also be confirmed by the comparison.
[0317] Furthermore, the threshold voltage can also be controlled by changing the ratio of In, Sn, and Zn. It is possible, and by setting the composition ratio to In:Sn:Zn=2:1:3, the transistor's noise - Mari-off formation can be expected. Also, the target composition ratio is In:Sn:Zn By setting the ratio to 2:1:3, a highly crystalline oxide semiconductor film can be obtained.
[0318] The intentional substrate heating temperature or heat treatment temperature is 150°C or higher, preferably 200°C or higher. More preferably, the temperature is 400°C or higher, and by forming the film or heat treating at a higher temperature, the translucency is achieved. This makes it possible to disable the normal operation of the ZISTA.
[0319] Furthermore, by intentionally heating the substrate during film deposition and / or performing heat treatment after film deposition, gate-by It can improve stability against asthma stress. For example, 2 MV / cm, 150°C. Under the condition of being applied for 1 hour, the drift should be less than ±1.5V, preferably 1.0V. It is possible to obtain less than this.
[0320] In fact, sample 1, which has not undergone heat treatment after oxide semiconductor film deposition, and sample 1, which has undergone heat treatment at 650°C. A BT test was performed on the transistor of sample 2.
[0321] First, the substrate temperature was set to 25°C and Vd to 10V, and the Vg-Id characteristics of the transistor were measured. Next, the substrate temperature was set to 150°C and Vd to 0.1V. Then, the gate insulating layer was... Apply 20V to Vg so that the applied electric field strength is 2MV / cm, and leave it as is for 1 hour. It was held. Next, Vg was set to 0V. Next, the substrate temperature was set to 25°C, and Vd was set to 10V. We performed a Vg-Id measurement using a lungist. This is called the PlusBT test.
[0322] Similarly, first set the substrate temperature to 25°C and Vd to 10V, and then the Vg-Id characteristics of the transistor. The following measurements were taken. Next, the substrate temperature was set to 150°C and Vd to 0.1V. Next, the gate A voltage of -20V is applied to Vg such that the electric field strength applied to the insulating layer is -2MV / cm, It was held in that state for 1 hour. Next, Vg was set to 0V. Next, the substrate temperature was set to 25°C and Vd was set to 1 The voltage was set to 0V, and the Vg-Id measurement of the transistor was performed. This is called the negative BT test.
[0323] The results of the positive BT test for sample 1 are shown in Figure 19(A), and the results of the negative BT test are shown in Figure 19(B). The results of the positive BT test for sample 2 are shown in Figure 20(A), and the results of the negative BT test are shown in Figure 20(A). The results are shown in Figure 20(B).
[0324] The threshold voltage fluctuations obtained from the positive BT test and negative BT test of sample 1 were, respectively, 1 The values were 0.80V and -0.42V. Also, the positive BT test and negative BT test of sample 2 were performed. The threshold voltage fluctuations observed during the experiment were 0.79V and 0.76V, respectively. Sample 1 and Both sample 1 and sample 2 showed small fluctuations in threshold voltage before and after the BT test, indicating high reliability. This can be understood.
[0325] Heat treatment can be carried out in an oxygen atmosphere, but first use nitrogen or an inert gas, or under reduced pressure. The heat treatment may be performed in an oxygen-containing atmosphere first. By performing a chemical reaction before adding oxygen to the oxide semiconductor, the effect of the heat treatment can be further enhanced. Yes, it is possible. Also, to add oxygen later, oxygen ions can be accelerated by an electric field into the oxide semiconductor film. An injection method may also be applied.
[0326] Defects due to oxygen vacancies are likely to be generated in oxide semiconductors and at the interface with the stacked films. By introducing an excess of oxygen into the oxide semiconductor through this heat treatment, it can be continuously generated. The resulting oxygen deficiency can be compensated for by excess oxygen. Excess oxygen is mainly found in the interstitial space. It is oxygen present in the atmosphere, and its oxygen concentration is 1 × 10⁻⁶. 16 / cm 3 The above 2 x 10 20 / cm 3 The following method allows the crystal to be incorporated into the oxide semiconductor without causing any distortion. .
[0327] Furthermore, by heat treatment, the oxide semiconductor can contain at least some crystals. This allows for the creation of more stable oxide semiconductor films. For example, a composition ratio of In:Sn:Zn = 1 Using a 1:1 target, an oxide film was deposited by sputtering without intentionally heating the substrate. The halo pattern of a semiconductor film can be determined by X-ray diffraction (XRD). A crystalline substance is observed. This deposited oxide semiconductor film is then subjected to heat treatment to induce crystallization. This can be done. The heat treatment temperature is arbitrary, but for example, by performing heat treatment at 650°C, X-rays Clear diffraction peaks can be observed through diffraction.
[0328] In fact, we performed XRD analysis on the In-Sn-Zn-O film. For the XRD analysis, we used Bruker Using the AXS D8 ADVANCE X-ray diffractometer, the Out-of-Plane method was used. It was measured.
[0329] Sample A and Sample B were prepared for XRD analysis. Samples A and B are shown below. The method for making it will be explained.
[0330] An In-Sn-Zn-O film with a thickness of 100 nm was deposited on a dehydrogenated quartz substrate. .
[0331] The In-Sn-Zn-O film was formed using a sputtering apparatus in an oxygen atmosphere with a power of 100W. The film was deposited as DC. The target was I with an atomic ratio of In:Sn:Zn = 1:1:1. An n-Sn-Zn-O target was used. The substrate heating temperature during film deposition was 200°C. The sample prepared in this manner was designated as Sample A.
[0332] Next, a sample prepared in the same manner as sample A was subjected to heat treatment at a temperature of 650°C. The heat treatment involves first heating in a nitrogen atmosphere for 1 hour, and then, without lowering the temperature, in an oxygen atmosphere. The sample prepared in this manner was subjected to a further heat treatment for one hour.
[0333] Figure 23 shows the XRD spectra of sample A and sample B. In sample A, the peak originating from the crystal is Although not observed, in sample B, 2θ was near 35 degrees and between 37 and 38 degrees. A peak originating from the crystal was observed.
[0334] Thus, oxide semiconductors mainly composed of In, Sn, and Zn are intentionally heated during film deposition. By doing and / or by heat treatment after film formation, the characteristics of the transistor can be improved. Cut.
[0335] This substrate heating and heat treatment removes hydrogen and hydroxyl groups, which are harmful impurities for oxide semiconductors, from the film. It has the effect of preventing them from being included or removing them from the film. In other words, oxides By removing hydrogen, which acts as a donor impurity in semiconductors, higher purity can be achieved. Therefore, it is possible to normally turn off the transistor, and the oxide semiconductor can be made highly pure. By doing so, the off-current can be reduced to 1 aA / μm or less. Here, the above off-current value The unit indicates the current value per 1 μm of channel width.
[0336] Figure 24 shows the relationship between the transistor's off-current and the reciprocal of the substrate temperature (absolute temperature) during measurement. Here, for simplicity, we multiply the reciprocal of the substrate temperature at the time of measurement by 1000 (1000 / The horizontal axis is T).
[0337] Specifically, as shown in Figure 24, when the substrate temperature is 125°C, the ratio is 1 aA / μm(1×1 0 -18 (A / μm) or less, at 85℃ it is 100zA / μm (1×10 -19 A / μm ) Below this, at room temperature (27℃), it is 1 zA / μm (1 × 10⁻⁶). -21 (A / μm) should be less than or equal to the specified limit. This is possible. Preferably, at 125°C, 0.1 aA / μm (1 × 10⁻¹⁶). -19 A / μ m) or less, at 85°C, 10 zA / μm (1 × 10 -20 A / μm) or less, at room temperature At 0.1 zA / μm (1 × 10⁻⁶ -22 These can be reduced to A / μm or less. The off-current value is extremely low compared to transistors using Si as the semiconductor film. It is clear that...
[0338] However, to prevent hydrogen and moisture from entering the film during the deposition of oxide semiconductor films, the outside of the deposition chamber is used. This aims to sufficiently suppress leaks from outside and degassing from the inner walls of the deposition chamber, thereby increasing the purity of the sputtering gas. Preferably, the sputtering gas has a dew point of -70°C or lower so that moisture is not contained in the film. It is preferable to use the gas shown below. Also, the target itself should contain hydrogen, water, and other impurities. It is preferable to use a highly purified target so that it does not contain any pure substances. Oxide semiconductors, mainly composed of In, Sn, and Zn, can have moisture removed from the film through heat treatment. However, compared to oxide semiconductors mainly composed of In, Ga, and Zn, the moisture release temperature is Because of the high moisture content, it is preferable to form a film that does not contain moisture from the beginning.
[0339] Furthermore, in transistors of samples that underwent a heat treatment at 650°C after oxide semiconductor film deposition, The relationship between substrate temperature and electrical characteristics was evaluated.
[0340] The transistor used for the measurement had a channel length L of 3 μm, a channel width W of 10 μm, and Lov The thickness is 0 μm and dW is 0 μm. Vd was set to 10 V. The substrate temperature was -40°C. The tests were conducted at -25°C, 25°C, 75°C, 125°C, and 150°C. Here, the transistor In this case, the overlapping width between the gate electrode and the pair of electrodes is called Lov, and for an oxide semiconductor film... The overhang of the pair of electrodes is called dW.
[0341] Figure 21 shows the Vg dependence of Id (solid line) and field-effect mobility (dotted line). Also, Figure 22 (A) shows the relationship between substrate temperature and threshold voltage, and Figure 22(B) shows the relationship between substrate temperature and field effect mobility. To show a relationship.
[0342] Figure 22(A) shows that the threshold voltage decreases as the substrate temperature increases. The voltage range was 1.09V to -0.23V at -40℃ to 150℃.
[0343] Furthermore, Figure 22(B) shows that the field-effect mobility decreases as the substrate temperature increases. The temperature range is -40°C to 150°C and the length is 36 cm. 2 / Vs~32cm 2 It was / Vs. Therefore, it can be seen that the variation in electrical characteristics is small within the temperature range mentioned above.
[0344] The above-mentioned oxide semiconductor, mainly composed of In, Sn, and Zn, is used as the channel formation region. According to Rangista, the off-current is kept below 1 aA / μm while the field-effect mobility is 30c. m 2 / Vsec or greater, preferably 40cm 2 / Vsec or more, more preferably 60cm 2 It can be set to / Vsec or higher, satisfying the on-current value required by the LSI. For example, For a FET with L / W = 33nm / 40nm, gate voltage 2.7V, drain voltage 1.0V It can sometimes supply an on-current of 12 μA or more. Furthermore, it meets the requirements for transistor operation. Sufficient electrical characteristics can be ensured even within the temperature range. For example, transistors made of oxide semiconductors are embedded within integrated circuits made of Si semiconductors. Even so, it is possible to realize integrated circuits with new functions without sacrificing operating speed. Cut.
[0345] Below is an example of a transistor using an In-Sn-Zn-O film as the oxide semiconductor film. explain.
[0346] Figure 25 shows the top gate, top contact structure of a coplanar transistor. These are top views and cross-sectional views. Figure 25(A) shows a top view of the transistor. Also, Figure 25(B) Figure 25(A) shows the cross-section AB corresponding to the dashed line AB.
[0347] The transistor shown in Figure 25(B) consists of a substrate 1200 and a base provided on the substrate 1200. An insulating layer 1202, a protective insulating film 1204 provided around the base insulating layer 1202, and a base High-resistance region 1206a and low-resistance region provided on the insulating layer 1202 and protective insulating film 1204 An oxide semiconductor film 1206 having region 1206b, and provided on the oxide semiconductor film 1206 A gate insulating layer 1208 and an oxide semiconductor film 1206 via the gate insulating layer 1208 A gate electrode 1210 is provided in superimposition, and is provided in contact with the side surface of the gate electrode 1210. A pair of electric fields are provided in contact with the side wall insulating film 1212 and at least the low-resistance region 1206b. The electrode 1214, at least an oxide semiconductor film 1206, a gate electrode 1210, and a pair of electrodes. An interlayer insulating film 1216 is provided covering 1214, and an opening is provided in the interlayer insulating film 1216 A wiring 1218 is provided connected to one of at least one pair of electrodes 1214 via a port. , has.
[0348] Although not shown in the diagram, a protective film is provided covering the interlayer insulating film 1216 and the wiring 1218. It is acceptable to have it. By providing the protective film, surface conduction caused by the interlayer insulating film 1216 is eliminated. This reduces the minute leakage current that occurs, thereby reducing the transistor's off-current. It is possible.
[0349] Furthermore, a transistor using a different In-Sn-Zn-O film as the oxide semiconductor film... Here is another example.
[0350] Figure 26 shows a top view and a cross-sectional view of the structure of a transistor. Figure 26(A) shows the transistor This is a top view of the sta. Also, Figure 26(B) is a cross section corresponding to the dashed line AB in Figure 26(A). This is a view drawing.
[0351] The transistor shown in Figure 26(B) consists of a substrate 1600 and a base provided on the substrate 1600. An insulating layer 1602, an oxide semiconductor film 1606 provided on the underlying insulating layer 1602, and an oxide A pair of electrodes 1614 in contact with the monocrystalline semiconductor film 1606, and the oxide semiconductor film 1606 and a pair A gate insulating layer 1608 provided on electrode 1614, and acid via gate insulating layer 1608 A gate electrode 1610 is provided superimposed on the semiconductor film 1606, and a gate insulating layer 160 8 and the interlayer insulating film 1616 provided covering the gate electrode 1610, and the interlayer insulating film 161 Wiring 1618 that connects to a pair of electrodes 1614 through an opening provided in 6, and interlayer insulation It comprises a protective film 1620 provided to cover the film 1616 and the wiring 1618.
[0352] As the substrate 1600, a glass substrate is used, and as the underlying insulating layer 1602, a silicon oxide film is used. As the ionized semiconductor film 1606, an In-Sn-Zn-O film is used, and as the pair of electrodes 1614, A tungsten film is used as the gate insulating layer 1608, and a silicon oxide film is used as the gate electrode 161 As for 0, a laminated structure of tantalum nitride film and tungsten film is used as the interlayer insulating film 1616. The laminated structure consists of a silicon oxide nitride film and a polyimide film, and the wiring 1618 is a titanium film. A laminated structure in which an aluminum film and a titanium film are formed in this order is referred to as the protective film 1620. Liimide membranes were used in each case.
[0353] In the transistor with the structure shown in Figure 26(A), the gate electrode 1610 and a pair of electric electrodes The width of the overlap with pole 1614 is called Lov. Similarly, the width of the oxide semiconductor film 1606 The protrusion of the pair of electrodes 1614 is called dW.
[0354] (Embodiment 9) In this embodiment, an example of an electronic device equipped with the arithmetic processing unit in the above embodiment is described below. explain.
[0355] An example of the configuration of the electronic device in this embodiment will be explained using Figures 9(A) to 9(D). I will reveal it.
[0356] The electronic device shown in Figure 9(A) is an example of a portable information terminal. The terminal comprises a housing 1001a and a display unit 1002a provided on the housing 1001a. ru.
[0357] Furthermore, the side 1003a of the housing 1001a has a connection terminal for connecting to an external device, Figure 9 ( One or more buttons may be provided for operating the portable information terminal shown in A). .
[0358] The portable information terminal shown in Figure 9(A) has a CPU, a memory circuit, and an external enclosure 1001a. An interface for transmitting and receiving signals between the internal components, the CPU, and memory circuits, and for communicating with external devices. It includes an antenna for transmitting and receiving signals.
[0359] The portable information terminals shown in Figure 9(A) include, for example, telephones, e-readers, and personal computers. , and also function as one or more gaming machines.
[0360] The electronic device shown in Figure 9(B) is an example of a foldable portable information terminal. The portable information terminal consists of a housing 1001b and a display unit 1002b provided on the housing 1001b. The housing 1004, the display unit 1005 provided on the housing 1004, and the housing 1001b and It comprises a shaft portion 1006 for connecting the housing 1004.
[0361] Furthermore, in the portable information terminal shown in Figure 9(B), the shaft portion 1006 connects to the housing 1001b or the casing. By moving the body 1004, the housing 1001b can be superimposed on the housing 1004. ru.
[0362] Furthermore, external devices can be connected to the side 1003b of the housing 1001b or the side 1007 of the housing 1004. Connection terminals for connecting, buttons for operating the portable information terminal shown in Figure 9(B) You may provide one or more of them.
[0363] Furthermore, the display unit 1002b and the display unit 1005 may display different images or a continuous image. It may be shown. Note that the display unit 1005 does not necessarily have to be provided, and the display unit 1005 Alternatively, a keyboard, which serves as an input device, may be provided.
[0364] The portable information terminal shown in Figure 9(B) has a CPU and inside the housing 1001b or housing 1004. , a memory circuit, and an interface for transmitting and receiving signals between external devices, the CPU, and the memory circuit. It is equipped with the following. Furthermore, the portable information terminal shown in Figure 9(B) is capable of transmitting and receiving signals with the outside world. An antenna may be installed.
[0365] The portable information terminals shown in Figure 9(B) include, for example, telephones, e-readers, and personal computers. , and also function as one or more gaming machines.
[0366] The electronic device shown in Figure 9(C) is an example of a stationary information terminal. The terminal comprises a housing 1001c and a display unit 1002c provided on the housing 1001c. ru.
[0367] The display unit 1002c can also be provided on the deck portion 1008 of the housing 1001c. ru.
[0368] Furthermore, the stationary information terminal shown in Figure 9(C) contains a CPU and a memory circuit inside the casing 1001c. It includes an interface for transmitting and receiving signals between external devices, the CPU, and memory circuits. Furthermore, the stationary information terminal shown in Figure 9(C) is equipped with an antenna for transmitting and receiving signals to and from the outside. It may be established.
[0369] Furthermore, in the stationary information terminal shown in Figure 9(C), a ticket is placed on the side 1003c of the housing 1001c. The system may be provided with one or more ticket output units, coin slots, and banknote insertion units, which output information such as the above.
[0370] The stationary information terminal shown in Figure 9(C) is used, for example, by an automated teller machine or for ordering tickets. It functions as an information and communication terminal (also called a multimedia station) or as a gaming machine. To possess.
[0371] Figure 9(D) shows an example of a stationary information terminal. The stationary information terminal shown in Figure 9(D) has a housing 1 The housing comprises 001d and a display unit 1002d provided on the housing 1001d. A support base may be provided to support 1001d.
[0372] Furthermore, the side 1003d of the housing 1001d has a connection terminal for connecting to an external device, Figure 9 ( One or more buttons may be provided for operating the stationary information terminal shown in D). .
[0373] Furthermore, the stationary information terminal shown in Figure 9(D) contains a CPU and a memory circuit within the enclosure 1001d. It includes an interface for transmitting and receiving signals between external devices, the CPU, and memory circuits. It is also acceptable to use an external signaling and receiving system for the stationary information terminal shown in Figure 9(D). A tent may be provided.
[0374] The stationary information terminal shown in Figure 9(D) is, for example, a digital photo frame, monitor, or telecommunications device. It functions as a vision device.
[0375] The arithmetic processing unit of the above embodiment is the CPU of the electronic device shown in Figures 9(A) to 9(D) and It is used as such.
[0376] As explained with reference to Figure 9, an example of the electronic device in this embodiment is a CPU The configuration includes the arithmetic processing unit described in the embodiment.
[0377] By using the above configuration, even when power is not supplied, the information in the electronic device can be stored for a certain period of time. Because it can hold the power for a short period, the time from supplying power to starting normal operation is fast. This also allows for a reduction in power consumption. [Explanation of Symbols]
[0378] 101 Comparison circuit 102 Comparison circuit 111 transistors 112 transistors 121 transistors 122 transistors 131 transistors 201 memory cells 202 transistors 203 Transistors 204 buffer 205 buffer 600 Device formation layer 601 Conductive layer 602 Insulating layer 603 Semiconductor layer 604a area 604b area 605a conductive layer 605b conductive layer 606 Insulating layer 608 Conductive layer 751 Conductive layer 752 Insulating layer 752a area 752b area 753 Semiconductor layer 754a conductive layer 754b Conductive layer 755 Insulating layer 756 Conductive layer 757a Insulating layer 757b Insulating layer 758 Insulating layer 759 Insulating layer 760a conductive layer 760b conductive layer 761a Insulating layer 761b Insulating layer 780 Semiconductor Layers 781a Insulated area 781b Insulation area 781c Insulation Area 782a area 782b area 782c area 782d area 783a area 783b area 784a Insulating layer 784b Insulating layer 785a conductive layer 785b Conductive layer 786a Insulating layer 786b Insulating layer 786c insulating layer 786d Insulating layer 788 Insulating layer 801 Bus Interface 802 Control Unit 803 Cache memory 804 Register 805 Instruction Decoder 806 Logic Unit 1001a Enclosure 1001b enclosure 1001c enclosure 1001d enclosure 1002a Display section 1002b Display section 1002c Display section 1002d Display section 1003a side 1003b Side 1003c side 1003d side 1004 cabinet 1005 Display section 1006 Shaft 1007 Side view 1008 Deck section 1200 circuit boards 1202 Underlayment Insulation Layer 1204 Protective insulating film 1206 Oxide semiconductor film 1206a High resistance area 1206b Low resistance region 1208 Gate Insulation Layer 1210 Guard Station 1212 Sidewall insulating film 1214 Electrode 1216 Interlayer insulating film 1218 Wiring 1600 circuit boards 1602 Underlayment insulation layer 1606 Oxide semiconductor film 1608 Gate Insulation Layer 1610 Guard Station 1614 Electrode 1616 Interlayer insulating film 1618 Wiring 1620 Protective film 2101 Underlayment Insulation Layer 2102 Insulator 2103a Semiconductor Domain 2103b Semiconductor area 2103c Semiconductor Domain 2104 Gate Insulation Layer 2105 Gate 2106a Side wall insulator 2106b Sidewall insulation 2107 Insulator 2108a Source 2108b Drain
Claims
1. It has a first transistor and a second transistor, A semiconductor device in which either the source electrode or the drain electrode of the first transistor is always in electrical contact with the gate electrode of the second transistor, The first transistor has a channel formation region in the oxide semiconductor layer, The first conductive layer, which functions as the gate electrode of the first transistor, has a region located above the oxide semiconductor layer. The second conductive layer, which functions as either the source electrode or the drain electrode of the first transistor, has a region located above the oxide semiconductor layer. The third conductive layer, which functions as the other of the source electrode or drain electrode of the first transistor, has a region located above the oxide semiconductor layer. The first conductive layer, the second conductive layer, and the third conductive layer each have a region located below the first insulating layer. A fourth conductive layer having a region positioned above the second conductive layer via the first insulating layer is always electrically connected to the second conductive layer. The fifth conductive layer, which functions as the gate electrode of the second transistor, has a region located below the second conductive layer. The oxide semiconductor layer has a region positioned above the second insulating layer, which has a region facing the side surface of the fifth conductive layer. The region of the second conductive layer that is in contact with the fourth conductive layer has an overlap with the fifth conductive layer. Semiconductor equipment.
2. It comprises a first transistor, a second transistor, and a capacitive element. The aforementioned capacitive element is always in electrical contact with the gate electrode of the second transistor. A semiconductor device in which either the source electrode or the drain electrode of the first transistor is always in electrical contact with the gate electrode of the second transistor, The first transistor has a channel formation region in the oxide semiconductor layer, The first conductive layer, which functions as the gate electrode of the first transistor, has a region located above the oxide semiconductor layer. The second conductive layer, which functions as either the source electrode or the drain electrode of the first transistor, has a region located above the oxide semiconductor layer. The third conductive layer, which functions as the other of the source electrode or drain electrode of the first transistor, has a region located above the oxide semiconductor layer. The first conductive layer, the second conductive layer, and the third conductive layer each have a region located below the first insulating layer. A fourth conductive layer having a region positioned above the second conductive layer via the first insulating layer is always electrically connected to the second conductive layer. The fifth conductive layer, which functions as the gate electrode of the second transistor, has a region located below the second conductive layer. The oxide semiconductor layer has a region positioned above the second insulating layer, which has a region facing the side surface of the fifth conductive layer. The region of the second conductive layer that is in contact with the fourth conductive layer has an overlap with the fifth conductive layer. Semiconductor equipment.
3. In claim 1 or claim 2, In a cross-sectional view of the first transistor in the channel length direction, the region of the oxide semiconductor layer that overlaps with the first conductive layer is separated from the region of the oxide semiconductor layer that overlaps with the second conductive layer. In a cross-sectional view of the first transistor in the channel length direction, the region of the oxide semiconductor layer that overlaps with the first conductive layer is separated from the region of the oxide semiconductor layer that overlaps with the third conductive layer. Semiconductor equipment.
4. In any one of claims 1 to 3, The oxide semiconductor in the aforementioned oxide semiconductor layer is an In-O-based metal oxide. Semiconductor equipment.
Citation Information
Patent Citations
Merged logic circuit combining thin film and bulk silicon transistor and memory
JP2000114453A
Association memory
JP2004295967A
Semiconductor integrated circuit device and its manufacturing method
JP2005101141A
Display device
JP2009094492A
Fabricating method of semiconductor device
JP2009135350A