Fabric for improving the gloss of the surface of metal glasses frame and its manufacturing method
A fabric with a specific compositional solution and two-step drying process addresses the issues of scratches and corrosion on metal eyeglass frames, maintaining gloss and preventing rust for extended use.
Patent Information
- Application Number
- KR1020250058871
- Authority / Receiving Office
- KR · KR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-05-07
- Publication Date
- 2026-11-16
AI Technical Summary
Metal eyeglass frames are prone to scratches and corrosion due to their thinness, leading to a shorter lifespan and reduced cleanliness, with existing polishing fabrics ineffective in addressing these issues.
A fabric impregnated with a compositional solution comprising carbon black, aluminum oxide, paraffin refined oil, hydrotreated heavy naphtha, silicon oxide, and water, followed by a two-step drying process to ensure absorption, enhances the gloss and prevents scratches on metal eyeglass frames.
The fabric effectively removes rust and maintains gloss on metal eyeglass frames by filling in scratches and preventing corrosion, ensuring longevity and cleanliness.
Smart Images

Figure PAT00001_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a fabric for improving the surface gloss of metal eyeglass frames and a method for manufacturing the same, and more specifically, to a fabric for improving the surface gloss of metal eyeglass frames and a method for manufacturing the same that effectively removes scratches occurring on the surface of a thin wire metal eyeglass frame, fills in the scratched parts on the surface of the frame, and makes it glossy so that the eyeglass frame can be used for a long time. Background Technology
[0002] Metal eyeglass frames are thinner than other metal materials, and prolonged use leads to frequent scratches, resulting in a shorter lifespan. Furthermore, along with the scratches, foreign substances accumulate on the frames, reducing cleanliness and causing the plated parts to corrode quickly.
[0003] Meanwhile, some polishing fabrics are currently being released for polishing automobiles, shoes, leather sofas, furniture, etc.
[0004] However, there is still a need to develop new glossy fabric materials that can effectively fill in surface scratches on thin metal materials, such as eyeglass frames. Prior art literature
[0006] 1. Republic of Korea Registered Patent No. 10-2420782 The problem to be solved
[0007] Therefore, the problem that the present invention aims to solve is to provide a compositional solution for preventing scratches and producing gloss on metal eyeglass frames, and a fabric impregnated therewith. means of solving the problem
[0008] To solve the above problem, the present invention provides a fabric for improving the surface gloss of a metal eyeglass frame, wherein the fabric is impregnated with a compositional solution comprising: 0.5 to 2 parts by weight of carbon black (acetylene black); 1 to 10 parts by weight of aluminum oxide (alundum); 1 to 8 parts by weight of paraffin refined oil (petroleum) (distillates (petroleum)); 25 to 39 parts by weight of hydrogenated heavy naphtha (petroleum) (naphtha (petroleum), hydrottreaded heavy); 4 to 12 parts by weight of silicon oxide (silica); and a water content of 35% to 60 parts by weight.
[0009] In one embodiment of the present invention, the fabric is a microfiber of 70% by weight polyester and 30% by weight nylon.
[0010] The present invention also provides a method for manufacturing a fabric for improving the surface gloss of metal eyeglass frames, comprising the steps of: impregnating a fabric of 70% by weight of polyester and 30% by weight of nylon in a compositional solution; drying the fabric impregnated with the compositional solution in a first step; and drying the fabric dried in the first step in a second step, wherein the compositional solution comprises 0.5 to 2 parts by weight of carbon black (ACETYLENE BLACK); and 1 to 10 parts by weight of aluminum oxide (ALUNDUM); The present invention provides a method for manufacturing a fabric for improving the surface gloss of metal eyeglass frames, characterized by comprising 1 to 8 parts by weight of paraffin refined oil (petroleum) (DISTILLATES (PETROLEUM); 25 to 39 parts by weight of hydrotreated heavy naphtha (petroleum) (NAPHTHA (PETROLEUM), HYDROTREATED HEAVY); 4 to 12 parts by weight of silicon oxide (SILICA); and a water content of 35% to 60 parts by weight.
[0011] In one embodiment of the present invention, the first drying is carried out at 100°C to 120°C for 30 to 60 minutes, and the second drying is carried out by pressing at 120°C to 140°C for 24 seconds.
[0012] In one embodiment of the present invention, after the second drying, the weight of the fabric increases to 24 to 36% of the weight before impregnation. Effects of the invention
[0013] The fabric according to the present invention can maintain gloss by effectively removing rust, etc., from eyeglass frames with a fine structure while maintaining gloss removal for a long time. Brief explanation of the drawing
[0014] FIG. 1 is a step diagram of a method for manufacturing a fabric to improve the surface gloss of a metal eyeglass frame according to one embodiment of the present invention. FIGS. 2 and 3 are the results of a comparative experiment in which secondary drying was not performed (Comparative Example 1) and secondary drying was performed (Example) according to one embodiment of the present invention. Figures 4 and 5 are the results of the gloss removal experiment of Comparative Example 2 and the Example after 24 hours. Specific details for implementing the invention
[0015] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the attached drawings.
[0016] Before describing the invention in detail, the terms and words used in this specification should not be interpreted as being limited to their ordinary or dictionary meanings, and the inventor of the invention may appropriately define and use the concepts of various terms to best describe his invention.
[0017] Furthermore, it should be understood that these terms or words should be interpreted in a meaning and concept consistent with the technical spirit of the present invention.
[0018] In other words, the terms used in this specification are used merely to describe preferred embodiments of the invention and are not intended to specifically limit the content of the invention.
[0019] It should be noted that these terms are defined in consideration of the various possibilities of the present invention.
[0020] Additionally, in this specification, singular expressions may include plural expressions unless the context clearly indicates a different meaning.
[0021] In addition, you should be aware that even if it is expressed in the plural, it may contain a singular meaning.
[0022] Throughout this specification, where it is stated that a component "includes" another component, unless specifically stated otherwise, this may mean that it does not exclude any other component but may include any other component.
[0023] Furthermore, in cases where it is stated that a component "exists inside or is installed in connection with" another component, this component may be installed in direct connection with or in contact with the other component.
[0024] In addition, they may be installed spaced apart at a certain distance, and in the case where they are installed spaced apart at a certain distance, there may be a third component or means for fixing or connecting the component to another component.
[0025] Meanwhile, it should be noted that the description of the third component or means mentioned above may be omitted.
[0026] On the other hand, if it is stated that one component is "directly connected" or "directly connected" to another component, it should be understood that there is no third component or means.
[0027] Likewise, other expressions describing the relationship between each component, such as “between” and “right between”, or “adjacent to” and “directly adjacent to”, should be interpreted as having the same intent.
[0028] In addition, terms such as “one side,” “other side,” “one side,” “other side,” “first,” “second,” etc., in this specification are used to ensure that one component can be clearly distinguished from another component.
[0029] However, it should be noted that the meaning of the component is not used restrictively by such terminology.
[0030] In the drawings attached to this specification, the size, location, connection relationships, etc., of each component constituting the present invention may be described in a partially exaggerated, reduced, or omitted manner for the convenience of explanation or to sufficiently clearly convey the concept of the present invention, and therefore, the proportions or scale may not be strictly accurate.
[0031] In addition, in describing the present invention below, detailed descriptions of components that are deemed to unnecessarily obscure the essence of the invention, such as known technologies including prior art, may be omitted.
[0032] To solve the above-mentioned problem, the present invention provides a polishing composition for polishing metal eyeglass frames and a fabric impregnated with said composition.
[0033] A composition according to one embodiment of the present invention comprises 0.5 to 2 parts by weight of carbon black (acetylene black); 1 to 10 parts by weight of aluminum oxide (alundum); 1 to 8 parts by weight of paraffin refined oil (petroleum, CAS No.: 64742-54-7); 25 to 39 parts by weight of hydrotreated heavy naphtha (petroleum, CAS No.: 64742-82-1); 4 to 12 parts by weight of silicon oxide (silica); and a water content of 35% to 60 parts by weight.
[0034] In particular, the present invention uses two types of hydrocarbon materials (paraffin refined oil and hydrogenated heavy naphtha (petroleum)) to effectively disperse aluminum oxide and silicon oxide with abrasive functions, while preventing the composition from easily evaporating from the fabric during drying.
[0035] In addition, in one embodiment of the present invention, the fabric is a fabric composed of 70% by weight of polyester + 30% by weight of nylon, made of microfibers with micropores.
[0036] FIG. 1 is a step diagram of a method for manufacturing a fabric to improve the surface gloss of a metal eyeglass frame according to one embodiment of the present invention.
[0037] Referring to FIG. 1, the fabric is first impregnated with the compositional solution described above. Subsequently, it is dried first at 100°C to 120°C. During the first drying, the compositional solution on the surface of the fabric evaporates. However, since the compositional solution is not sufficiently absorbed into the actual fabric in this case, in one embodiment of the present invention, a second drying is performed for 24 seconds by pressing at 120°C to 140°C. In this manner, the present invention ensures that the compositional solution is sufficiently absorbed into the actual fabric, and the weight of the fabric increases to 24 to 36% of the weight before impregnation due to the first and second drying.
[0038] FIGS. 2 and 3 are the results of a comparative experiment in which secondary drying was not performed (Comparative Example 1) and secondary drying was performed (Example) according to one embodiment of the present invention. In this experiment, the rust remaining on the inner surface of the eyeglass frame was compared after rubbing the frame with a fabric several times.
[0039] Referring to FIGS. 2 and 3, it can be seen that when secondary drying is not performed, nothing remains on the fabric after rubbing, whereas when secondary drying is performed, residue is present. This result indicates that the fabric subjected to secondary drying according to one embodiment of the present invention has an excellent gloss removal effect.
[0040] The present invention used two types of hydrocarbon materials (paraffin refined oil and hydrogenated heavy naphtha (petroleum)), and gloss tests were conducted with the case where only one type was used, and the results are shown in Table 1 below.
[0041] Initial gloss effect Gloss effect after 24 hours 2 types of hydrocarbon substances (Example) is available maintain Paramine refined oil alone (Comparative Example 2) is available weakening Hydrogenated heavy naphtha alone doesn't exist doesn't exist
[0042] In addition, Figures 4 and 5 are the results of the gloss removal experiment of Comparative Example 2 and the Example after 24 hours.
[0043] Referring to the results in Table 1 and Figures 4 and 5 above, it can be seen that the fabric according to the present invention using two types of hydrocarbon materials maintains a gloss removal effect.
[0044] As explained above, the fabric according to the present invention can maintain gloss by effectively removing rust, etc., from eyeglass frames with a fine structure while maintaining gloss removal for a long time.
Claims
Claim 1 A fabric for improving the surface gloss of metal eyeglass frames. The fabric is characterized by being impregnated with a compositional solution comprising: 0.5 to 2 parts by weight of carbon black (acetylene black); 1 to 10 parts by weight of aluminum oxide (alundum); 1 to 8 parts by weight of paraffin refined oil (petroleum) (distillates (petroleum)); 25 to 39 parts by weight of hydrogenated heavy naphtha (petroleum) (naphtha (petroleum), hydrottreaded heavy); 4 to 12 parts by weight of silicon oxide (silica); and a water content of 35% to 60 parts by weight. Claim 2 In Article 1, A fabric for improving the surface gloss of metal eyeglass frames, characterized by being a microfiber of 70% by weight of polyester and 30% by weight of nylon. Claim 3 A method for manufacturing a fabric for improving the surface gloss of metal eyeglass frames, A step of impregnating a fabric of 70% by weight polyester and 30% by weight nylon into a composition solution; A step of first drying the fabric impregnated with the above compositional solution; and A method for manufacturing a fabric for improving the surface gloss of metal eyeglass frames, comprising the step of drying the above-mentioned first-dried fabric a second time, wherein the composition liquid comprises 0.5 to 2 parts by weight of carbon black (acetylene black); 1 to 10 parts by weight of aluminum oxide (alundum); 1 to 8 parts by weight of paraffin refined oil (petroleum) (distillates (petroleum)); 25 to 39 parts by weight of hydrogenated heavy naphtha (petroleum) (naphtha (petroleum), hydrottreaded heavy); 4 to 12 parts by weight of silicon oxide (silica); and a water content of 35% to 60 parts by weight. Claim 4 A method for manufacturing a fabric for improving the surface gloss of a metal eyeglass frame, characterized in that, in claim 1, the first drying is carried out at 100°C to 120°C for 30 to 60 minutes, and the second drying is carried out by pressing at 120°C to 140°C for 24 seconds. Claim 5 In Article 1, A method for manufacturing a fabric for improving the surface gloss of metal eyeglass frames, characterized in that the weight of the fabric increases to 24 to 36% of the level before impregnation after the second drying.