Snorkel and constructing method thereof
The immersion pipe design with a tubular iron shell and structured refractory blocks addresses corrosion and thermal shock issues, improving durability and stability by enhancing bonding strength and reducing refractory detachment.
Patent Information
- Application Number
- KR1020250060221
- Authority / Receiving Office
- KR · KR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-05-09
- Publication Date
- 2026-11-17
AI Technical Summary
Conventional immersion pipes in RH facilities suffer from poor corrosion resistance and thermal shock resistance, leading to cracks and detachment of refractory materials, which reduces durability and operating efficiency.
The immersion pipe design incorporates a tubular iron shell with multiple refractory blocks, including a reinforcing plate welded to the steel shell, and a structured arrangement of refractory blocks to enhance bonding strength and stability, using pre-cast refractory materials to mitigate thermal stress.
The improved design reduces erosion and detachment of refractory bricks, enhancing the durability and operational stability of the immersion pipe.
Smart Images

Figure PAT00002_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to an immersion pipe for an RH facility and a method for constructing the same. Background Technology
[0002] Vacuum degassing equipment is called RH equipment, where RH stands for Rheinstahl-Heraus. RH equipment is a facility used in steel mills during the secondary steelmaking refining process to control fine components in molten steel after primary refining in the converter, utilizing the partial pressure difference of elements. Depending on the method of oxygen blowing into the molten steel in the ladle, such RH equipment includes RH, RH-OB, RH-TOB, RH-KTB, and RH-POSB.
[0003] The immersion pipe is immersed in the ladle facility containing the molten steel in the RH facility and provides a passage for the recirculation of the molten steel. The immersion pipe is constructed with a structure in which shaped or unshaped refractory materials surround a steel shell.
[0004] Specifically, conventional immersion pipes are fitted with alumina-based amorphous refractories or alumina-MgO-Cr-based amorphous refractories on the exterior and bottom, which are easy to install and offer excellent thermal shock resistance. However, amorphous refractories have the disadvantage of poor corrosion resistance to acidic slag contained in molten steel and weak resistance to thermal shock.
[0005] After the immersion tube is immersed in molten steel at approximately 1650°C and the operation is finished, the temperature drops to 400°C. This temperature difference acts as thermal stress, causing cracks to form in the irregular refractory material, and as the cracks expand, they lead to detachment. The detachment of the irregular refractory material causes the erosion of the steel shell and the detachment of the internal refractory bricks.
[0006] In particular, as the production of high-value steel grades and special steels increases, there is a need for increased recirculation speed and operating time due to improved vacuum levels in RH facilities. Consequently, cracks in irregular refractory materials occur easily, and as a result, the durability of the immersion tubes is reduced, leading to a serious problem of reduced operating rates in RH facilities. Prior art literature
[0007] Published Patent No. 10-2017-0129423 (Published Nov. 27, 2017) The problem to be solved
[0008] According to one embodiment of the present invention, an auger tube with improved fastening stability and durability can be provided.
[0009] According to another embodiment of the present invention, a method for constructing an immersion pipe with improved shape and fastening method of the refractory block may be provided.
[0010] The problems of the present invention are not limited to those described above. A person skilled in the art to which the present invention pertains will have no difficulty understanding additional problems of the present invention from the overall contents of this specification. means of solving the problem
[0011] A immersion tube according to one embodiment of the present invention has a tubular iron shell; It may include: a first refractory block disposed facing at least one end of the steel shell and including a reinforcing plate for welding with the steel shell; a second refractory block disposed inside the steel shell with a gap from the first refractory block to form a space for welding the steel shell and the reinforcing plate; a third refractory block disposed outside the steel shell and in contact with the first refractory block; and a fourth refractory block disposed inside the steel shell in the space to cover at least the welded portion of the steel shell and the reinforcing plate.
[0012] In addition, the reinforcing plate may be an annular metal plate welded continuously or spacedly along the circumferential direction to one end of the steel shell through the space.
[0013] In addition, the first refractory block may further include a protrusion that protrudes in the longitudinal direction of the steel shell to support at least the reinforcing plate from the outer side of the reinforcing plate.
[0014] In addition, the first refractory block may be made of shaped refractory material or pre-cast refractory material manufactured into a specific shape.
[0015] In addition, the third refractory block and the protrusion may include at least a portion of an inclined surface facing each other.
[0016] In addition, the first refractory block may further include a flange connected to one end of the reinforcing plate and formed integrally with the reinforcing plate inside the first refractory block.
[0017] Additionally, the steel shell includes a first support member protruding from the outer surface, and the third refractory block includes a step formed on the side facing the first refractory block and the outer surface of the steel shell, and the first support member may be disposed on one side of the step.
[0018] In addition, the steel shell includes a second support protruding from the inner surface, and the second support may be positioned between the second refractory block and the fourth refractory block.
[0019] In addition, the reinforcing plate is spaced apart from the outer surface of the steel shell at a predetermined distance, and at least a portion of the gap may be filled with irregular refractory material to prevent deformation of the steel shell.
[0020] A method for constructing a immersion pipe according to one embodiment of the present invention may include the steps of: preparing a pipe-shaped steel shell; preparing a first refractory block including a reinforcing plate for welding with the steel shell; placing a third refractory block on the outer side of the steel shell and placing a second refractory block on a part of the inner side of the steel shell to form a space for welding the steel shell and the reinforcing plate; placing a first refractory block to face at least one end of the steel shell and forming the space with the second refractory block; welding the steel shell and the reinforcing plate through the space; and placing a fourth refractory block in the space to seal at least the welded portion of the steel shell and the reinforcing plate to the inner side of the steel shell.
[0021] In addition, in the step of welding the steel shell and the reinforcing plate, the reinforcing plate may be welded continuously or at intervals along the circumferential direction with one end of the steel shell through a welding device that moves in and out through the space.
[0022] In addition, the first refractory block may further include a protrusion protruding in the longitudinal direction of the steel shell, and may be configured to support the reinforcing plate from the outside of the reinforcing plate at least during welding of the steel shell and the reinforcing plate.
[0023] Additionally, the method may further include the step of filling the space between the iron shell, the first refractory block, the second refractory block, the third refractory block, and the fourth refractory block with an irregular refractory material.
[0024] In addition, in the step of preparing the first refractory block, the first refractory block may be manufactured as a shaped refractory or a pre-cast refractory having a specific shape. Effects of the invention
[0025] According to the present invention, by separating the refractory material inside the immersion tube, welding through the inner space of the immersion tube is made possible, thereby providing an immersion tube with improved bonding strength.
[0026] According to the present invention, the erosion of the iron shell and the detachment of the internal refractory bricks are significantly reduced, and cracking of the refractory material is reduced, thereby providing an immersion pipe with improved durability.
[0027] According to the present invention, a method for constructing a immersion pipe can be provided in which the shape and fastening method of the refractory block are improved by installing pre-cast refractories on the exterior and bottom of the immersion pipe. Brief explanation of the drawing
[0028] Figure 1 is a cross-sectional view of an example of a vacuum degassing facility. FIG. 2a is a cross-sectional view of a immersion tube according to one embodiment of the present invention. FIG. 2b is a cross-sectional view of a immersion tube according to another embodiment of the present invention. FIG. 3a is a perspective view of a first refractory block positioned below the sedimentation tube shown in FIG. 2a. FIG. 3b is a perspective view of a first refractory block positioned below the sedimentation tube shown in FIG. 2b. FIG. 4a is a perspective view of a third refractory block arranged on the outside of the immersion tube shown in FIG. 2a. FIG. 4b is a perspective view of a third refractory block arranged on the outside of the immersion tube shown in FIG. 2b. FIG. 4c is a perspective view of a third refractory block arranged on the outer side of a immersion tube according to another embodiment of the present invention. FIG. 5 is a flowchart of a construction method for an immersion pipe according to one embodiment of the present invention. FIG. 6 is a diagram illustrating a partial sequence of a construction method for an immersion pipe according to one embodiment of the present invention. Specific details for implementing the invention
[0029] Preferred embodiments of the present invention will be described below with reference to the attached drawings. However, embodiments of the present invention may be modified in various other forms, and the scope of the present invention is not limited to the embodiments described below.
[0030] In addition, embodiments of the present invention are provided to more fully explain the present invention to those with average knowledge in the relevant technical field.
[0031] In drawings, the shapes and sizes of elements may be exaggerated for clearer explanation.
[0032] In describing the embodiments of the present invention, if it is determined that a detailed description of known technology related to the present invention may unnecessarily obscure the essence of the present invention, such detailed description will be omitted. Furthermore, the terms described below are defined considering their functions in the present invention, and these may vary depending on the intentions or conventions of the user or operator. Therefore, such definitions should be based on the content throughout this specification. The terms used in the detailed description are merely for describing the embodiments of the present invention and should not be limited in any way. Unless explicitly stated otherwise, expressions in the singular form include the meaning of the plural form.
[0033] In this description, expressions such as “include” or “equipped” are intended to refer to certain characteristics, numbers, steps, actions, elements, parts or combinations thereof, and should not be interpreted to exclude the existence or possibility of one or more other characteristics, numbers, steps, actions, elements, parts or combinations thereof other than those described.
[0034] In this specification, terms such as 'top', 'upper', 'upper surface', 'lower', 'lower', 'lower surface', 'side', etc. are based on the drawings and may actually vary depending on the direction in which the components are arranged.
[0035] Additionally, throughout the specification, when it is said that one part is 'connected' to another part, this includes not only cases where they are 'directly connected,' but also cases where they are 'indirectly connected' with other elements in between.
[0036] The present invention will be described in detail below through each embodiment or example of the invention. It should be noted that each embodiment or example described in this specification is not limited to a single embodiment or example, but may also be combined with other embodiments or examples. Accordingly, the citation of claims in the patent claims is merely an example of an embodiment, and the technical concept of the present invention should not be interpreted as being limited only to a combination with the cited claims; rather, combinations with various claims are also included within the scope of the technical concept of the present invention.
[0037] The present invention will be described in detail below through examples. However, it should be noted that the examples described below are intended merely to illustrate and embody the present invention and are not intended to limit the scope of the present invention. This is because the scope of the present invention is determined by the matters described in the patent claims and matters reasonably inferred therefrom.
[0038] FIG. 1 is an overall configuration diagram of an example of an RH vacuum degassing facility related to the present invention. The RH facility (1) has a ladle (L) positioned at the bottom, and after immersing a plurality of immersion tubes (2a, 2b) in the molten steel inside the ladle (L), the interior is formed into a vacuum. When argon (Ar) gas is supplied to one immersion tube (2a) through a spray hole, it acts as a rising tube through which the molten steel rises, and the molten steel rises from the ladle (L) into the interior of the RH facility. This molten steel then descends from the RH facility back to the ladle (L) through the immersion tube (2b), which acts as a descending tube on the other side. This flow of molten steel is repeated, and impurities in the molten steel are removed during the repeated process.
[0039] First, preferred embodiments of the immersion pipe according to the present invention and the construction method thereof, which are applied to the RH facility (1) described in FIG. 1, will be described in detail below. FIG. 2a is an enlarged view showing a cross-sectional view of an immersion pipe according to one embodiment of the present invention and a welded structure of a steel shell and a lower block. FIG. 3a is a perspective view of a refractory block arranged at the bottom of the immersion pipe shown in FIG. 2a. FIG. 2b is a cross-sectional view of an immersion pipe according to another embodiment of the present invention, FIG. 3b is a perspective view of a refractory block arranged at the bottom of the immersion pipe shown in FIG. 2b. FIG. 4a is a perspective view of a refractory block arranged on the outside of the immersion pipe shown in FIG. 2a, FIG. 4b is a perspective view of a refractory block arranged on the outside of the immersion pipe shown in FIG. 2b, and FIG. 4c is a perspective view of a refractory block arranged on the outside of the immersion pipe according to yet another embodiment of the present invention.
[0040] Referring to FIGS. 2a and 2b, the immersion tube according to embodiments of the present invention includes a steel shell (10) and refractory blocks (100, 200, 300, 400) that protect the steel shell (10). In one embodiment, the refractory blocks of the present invention may include a first refractory block (100) disposed at the bottom of the steel shell (10), a second refractory block (200) and a fourth refractory block (400) disposed inside the steel shell (10), and a third refractory block (300) disposed outside the steel shell (10). An irregular refractory material (500) may be filled between the steel shell (10) and the first refractory block (100), between the steel shell (10) and the second refractory block (200) and the fourth refractory block (400), and between the steel shell (10) and the third refractory block (300).
[0041] In one embodiment, the steel shell (10) has a tubular shape and extends in the longitudinal direction. One end (p1) of the steel shell (10) is connected to the first refractory block (100), and the other end (p2) is connected to the flange block (20). To prevent detachment and corrosion of the steel shell (10), the steel shell (10) is protected by a refractory material on its front surface so as not to be exposed to the outside.
[0042] Meanwhile, although not illustrated in the drawings, it may be possible to arrange the first refractory block at one end and the other end of the present invention. However, as a preferred embodiment, the first refractory block being connected to one end is illustrated and described below.
[0043] The first refractory block (100) is positioned to face at least one end of the steel shell (10). The first refractory block (100) contacts the third refractory block (300) and the fourth refractory block (400) on its upper surface. The first refractory block (100) may be formed in an annular shape, or it may have a shape that matches the outer surface of the steel shell (10) to surround the steel shell (10).
[0044] As illustrated in FIG. 2a, the first refractory block (100) includes a reinforcing plate (120) for welding with the steel shell (10). The first refractory block (100) forms a space (v) for welding the steel shell (10) and the reinforcing plate (120) between the second refractory block (200) and the inner side of the steel shell (10). A predetermined space (v) for welding the steel shell (10) and the reinforcing plate (120) may be provided between the end (p1) of the steel shell (10) and the first refractory block (100).
[0045] In particular, as shown in the enlarged view of FIG. 2a, a welding device enters through a space (v) from the inner direction of the steel shell (10), and the steel shell (10) and the reinforcing plate (120) are welded in the space between the end (p1) of the steel shell and the first refractory block (100) to form a welded portion (w).
[0046] The reinforcing plate (120) may be an annular metal plate and may be continuously welded along the circumferential direction to one end (p1) of the steel shell (10) through the space (v) between the first refractory block (100) and the second refractory block (200). It may also be possible to spot weld the steel shell (10) and the reinforcing plate (120) at regular intervals. However, in terms of rigidity, continuous welding is preferable. The reinforcing plate (120) may have a shape that matches the outer shape of the steel shell (10) so that it can be welded to the steel shell (10). The circumference of the reinforcing plate (120) may be greater than or equal to the circumference of the steel shell (10), and the reinforcing plate (120) may be made of the same or different metal so that it can be welded to the steel shell (10).
[0047] The reinforcing plate (120) may be positioned at a predetermined distance from the outer surface of the steel shell (10), and to prevent deformation of the steel shell (10), at least a portion of the space formed by the distance may be filled with amorphous refractory materials such as fire-resistant materials and insulating materials. The amorphous refractory material may be mixed with a solvent in the form of powder and installed to fill the space between the reinforcing plate (120) and the steel shell (10). Thus, it is possible to prevent the steel shell (10) from expanding or deforming due to high heat.
[0048] The first refractory block (100) may further include a protrusion (110) that protrudes in the longitudinal direction of the steel shell (10) to support the reinforcing plate (120) from the outside of the reinforcing plate (120). The protrusion (110) may have a shape that matches the outer shape of the reinforcing plate (120) to support the reinforcing plate (120) from the outside of the reinforcing plate (120), and the circumference of the protrusion (110) may be greater than or equal to the circumference of the reinforcing plate (120).
[0049] As can be seen in the enlarged view of FIG. 2a, the protrusion (110) supports the reinforcing plate (120) from the outside of the reinforcing plate (120) while the steel shell (10) and the reinforcing plate (120) are welded. In addition, the immersion pipe of the existing RH facility often experiences problems where the lower part of the steel shell bends outward due to thermal deformation while operating at high temperatures. However, in the present invention, the reinforcing plate (120) and the protrusion (110) surround the steel shell (10) from the outside of the lower part of the steel shell (10), thereby preventing deformation and damage to the steel shell (10) that occurs during the operation of the immersion pipe, and thus the durability of the immersion pipe can be improved.
[0050] The first refractory block (100) may be made of shaped refractory material or pre-cast refractory material manufactured into a specific shape. Here, pre-cast refractory material refers to castable material that is filled into a mold and processed to have a specific shape, and may have the characteristic of being assembled into a steel shell while having a specific shape. Unlike shaped refractory material, pre-cast refractory material may not require a pressurizing process to form a specific shape, so it can be manufactured more easily than manufacturing shaped refractory material. In addition, since the performance of shaped refractory material can be induced through the production of pre-cast refractory material, problems such as reduced durability during use, melting of the steel shell, and subsequent detachment of internal bricks that occur when using unshaped refractory material for construction can be mitigated.
[0051] The first refractory block (100) may further include a flange (130). The flange (130) is connected to one end of the reinforcing plate (120) and may be formed integrally with the reinforcing plate (120) inside the first refractory block (100). The flange (130) may be manufactured integrally with the reinforcing plate (120) or may be manufactured separately and then joined. Thus, such a flange (130) can further increase the bonding strength between the reinforcing plate (120) and the body of the first refractory block (100).
[0052] As illustrated in FIG. 2a, the second refractory block (200) is placed on the inner side of the steel shell (10) with a gap from the first refractory block (100) to form a space (v) for welding the steel shell (10) and the reinforcing plate (120). The lower surface of the second refractory block (200) is in contact with the fourth refractory block (400). The second refractory block (200) may be a shaped refractory. The second refractory block (200) may be formed by stacking multiple shaped refractories of a certain shape in multiple layers, or it may be in the form of an integrated shaped refractory. Although not illustrated in the drawings, it is understood that various modifications are possible for such a second refractory block (200) as long as it wraps around the inner surface of the steel shell (10). When multiple shaped refractories are arranged to form the second refractory block (200), an adhesive may be applied to the contact surfaces between the multiple shaped refractories.
[0053] As illustrated in FIG. 2a, the third refractory block (300) is in contact with the first refractory block (100) and is positioned on the outer side of the steel shell (10). The third refractory block (300) may be in the form of multiple shaped refractories arranged adjacent to each other, or it may be in the form of an integrated shaped refractory. Although not illustrated in the drawings, it is understood that various modifications are possible as long as such a third refractory block (300) wraps around the outer surface of the steel shell (10). When multiple shaped refractories are arranged to form the third refractory block (300), an adhesive may be applied to the contact surfaces between the multiple shaped refractories.
[0054] As illustrated in FIGS. 3a to 4c, the protrusions (110) of the third refractory block (300) and the first refractory block (100) may include at least a portion of inclined surfaces facing each other. When the upper surface of the protrusion (110) has the shape of a flat surface (111) as in FIGS. 2a and FIG. 3a, the lower surface of the third refractory block (300) may have the shape of a flat surface (301) corresponding to the flat surface (111) of the protrusion as in FIG. 4a. When the upper surface of the protrusion (110) has the shape of an inclined surface (112) that becomes lower in height as it moves toward the steel shell (10) as in FIGS. 2b and FIG. 3b, the lower surface of the third refractory block (300) may have an inclined surface (302) corresponding to the inclined surface (112) of the protrusion as in FIG. 4b. In addition, the contact surface with the protrusion (110) of the third refractory block (300) may be formed with a structure in which a flat surface (301) and an inclined surface (302) alternate, as shown in FIG. 4c.
[0055] As a result, since the structure described above increases the bonding strength between the first refractory block (100) and the third refractory block (300), the first refractory block (100) at the bottom of the immersion pipe can be prevented from detaching from the top of the immersion pipe, which is composed of the iron shell (10) and the second to fourth refractory blocks (200, 300, 400).
[0056] As illustrated in FIG. 2a, the third refractory block (300) may include a step (310) on the side facing the outer surface of the first refractory block (100) and the steel shell (10). The first support (600) is coupled to the steel shell (10) so as to protrude from the outer surface of the steel shell (10) and extends outwardly to a length suitable for the step (310) of the third refractory block. The first support (600) may extend in a direction parallel to one side of the step (310). The step (310) of the third refractory block is seated on the first support (600), and the first support (600) supports the load of the third refractory block (300) to reduce the stress applied to the first refractory block (100) and prevent the first refractory block (100) from falling off. The first support member (600) may be formed continuously along the outer circumference of the steel shell (10), or a plurality of support members may be spaced apart at intervals.
[0057] As illustrated in FIG. 2a, the fourth refractory block (400) is placed in a space (v) on the inside of the steel shell (10) to cover at least the welded portion (w) between the steel shell (10) and the reinforcing plate (120). One side of the fourth refractory block (400) is in contact with the first refractory block (100), and the other side is in contact with the second refractory block (200). In this way, the fourth refractory block (400) is placed after the reinforcing plate (120) of the first refractory block (100) and the steel shell (10) are joined on the inside of the immersion pipe, thereby enabling the connection between the steel shell (10) and the first refractory block (100) without machining a separate hole on the outside of the immersion pipe or in the first refractory block (100).
[0058] As illustrated in FIG. 2a, the steel shell (10) may include a second support member (700) protruding from the inner surface of the steel shell. The second support member (700) is positioned between the second refractory block (200) and the fourth refractory block (400), so that one side of the second support member (700) is in contact with the second refractory block (200) and the other side is in contact with the fourth refractory block (400). Since such a second support member (700) supports the load of the second refractory block (200) and reduces the stress applied to the first refractory block (100) and the fourth refractory block (400), the first refractory block (100) can be prevented from falling off. The second support member (700) may be formed continuously along the outer circumference of the steel shell (10), or a plurality of support members may be spaced apart at intervals.
[0059] In addition to the second support member (700), a plurality of additional support members may protrude from the inner surface of the steel shell (10) and be coupled to the steel shell (10). When a plurality of additional support members are coupled, a step may be formed on the surface where the second refractory block (200) contacts the inner surface of the steel shell (10) or on the surface where the fourth refractory block (400) contacts the inner surface of the steel shell (10). Accordingly, by having each of these steps seated on each support member, the load of the second refractory block (200) and the fourth refractory block (400) can be stably supported.
[0060] In the process of arranging the first refractory block (100), the second refractory block (200), the third refractory block (300), and the fourth refractory block (400) around the iron shell (10), an irregular refractory material (500) may be filled into the space formed between the iron shell (10), the first refractory block (100), the second refractory block (200), the third refractory block (300), and the fourth refractory block (400). Through this, the first refractory block (100) can maintain a connection with the second refractory block (200), the third refractory block (300), and the fourth refractory block (400) at least firmly.
[0061] Accordingly, as described above, the immersion tube according to the present invention will enable the provision of an immersion tube that is easy to use and maintain, and has improved durability.
[0062] Next, a preferred embodiment of the method for constructing a immersion pipe according to the present invention will be described in detail below. FIG. 5 is a flowchart of the method for constructing a immersion pipe according to one embodiment of the present invention, and FIG. 6 is a diagram showing a partial sequence of the method for constructing a immersion pipe according to one embodiment of the present invention.
[0063] Referring to FIGS. 5 and 6, a method for constructing a immersion pipe according to one embodiment of the present invention may include the steps of preparing a pipe-shaped steel shell (S100), preparing a first refractory block (S200), arranging a second refractory block and a third refractory block (S300), arranging the first refractory block (S400), connecting the steel shell and a reinforcing plate (S500), arranging a fourth refractory block (S600), and filling the space between each refractory block and the steel shell with an irregular refractory material (S700).
[0064] As illustrated in FIGS. 5 and 6, in step S200 of preparing the first refractory material, a first refractory block (100) is prepared. The first refractory block (100) may be formed in an annular shape, or may have a shape that matches the outer surface of the steel shell (10) to surround the steel shell (10).
[0065] In step S200, the first refractory block (100) is formed to include a reinforcing plate (120) for welding with the steel shell (10). The reinforcing plate (120) may be placed in a mold in advance when manufacturing the first refractory block (100) and then fixed inside the first refractory block (100) by filling in irregular refractory material, or the reinforcing plate (120) may be placed after manufacturing the first refractory block (100) and then fixed by filling in irregular refractory material.
[0066] The reinforcing plate (120) may be an annular metal plate that is continuously welded along the circumferential direction to one end (p1) of the steel shell (10). In addition, the reinforcing plate (120) may have a shape that matches the outer shape of the steel shell (10) so that welding with the steel shell (10) is possible, and the circumference of the reinforcing plate (120) may be greater than or equal to the circumference of the steel shell (10). The circumference of the reinforcing plate (120) may be formed larger than the circumference of the steel shell (10) so that a gap is formed between the reinforcing plate (120) and the steel shell (10) to fill with irregular refractory materials such as insulation. Furthermore, the reinforcing plate (120) may be made of the same or different type of metal so that welding with the steel shell (10) is possible.
[0067] In step S200 of preparing the first refractory material, the first refractory block (100) may be formed to further include a protrusion (110) that protrudes in the longitudinal direction of the steel shell (10) to support the reinforcing plate (120) from the outside of the reinforcing plate (120). To support the reinforcing plate (120) from the outside of the reinforcing plate (120), the protrusion (110) may be formed to have a shape that matches the outer shape of the reinforcing plate (120), and the circumference of the protrusion (110) may be formed to be greater than or equal to the circumference of the reinforcing plate (120). The protrusion (110) serves to support the reinforcing plate from the outside of the reinforcing plate (120) while the steel shell (10) and the reinforcing plate (120) are welded. In addition, the immersion pipe of the existing RH facility often experiences problems where the lower part of the steel shell bends outward due to thermal deformation while operating at high temperatures. However, in the present invention, the reinforcing plate (120) and the protrusion (110) surround the steel shell (10) on the outer side of the lower part of the steel shell (10), thereby preventing deformation and damage to the steel shell (10) that occurs during the operation of the immersion pipe.
[0068] In step S200 of preparing the first refractory material, the first refractory block (100) may be manufactured as a shaped refractory material or a pre-cast refractory material having a specific shape. Here, a pre-cast refractory material is a castable material that is filled into a mold and processed to have a specific shape, and may have the characteristic of being assembled into a steel shell while having a specific shape. When the first refractory block (100) is molded as a pre-cast refractory material, the first refractory block (100) may be molded by loading raw materials containing irregular refractory material into a mold and undergoing a curing process. Unlike shaped refractory material, pre-cast refractory material may not require a pressurization process by a press to have a specific shape, so it can be manufactured more easily compared to manufacturing shaped refractory material. Furthermore, since the performance of shaped refractory material can be induced through the production of pre-cast refractory material, problems such as reduced durability during use, erosion of the steel shell, and subsequent detachment of internal refractory bricks that occur when using irregular refractory material for construction will be mitigated.
[0069] In step S200 of preparing the first refractory material, the first refractory block (100) may be formed to further include a flange (130). The flange (130) is connected to one end of the reinforcing plate (120) and may be formed integrally with the reinforcing plate (120) inside the first refractory block (100). The flange (130) may be manufactured integrally with the reinforcing plate (120) or may be manufactured separately and then joined. Thus, such a flange (130) can further increase the bonding strength between the reinforcing plate (120) and the body of the first refractory block (100).
[0070] In step S200 of preparing the first refractory material, the upper surface of the protrusion (110) of the first refractory block (100) may be formed to have a flat surface (111) as in FIG. 2a, or it may be formed to have an inclined surface (112) that becomes lower in height toward the steel shell (10) as in FIG. 2b. When the upper surface of the protrusion (110) is a flat surface (111) as in FIG. 2a, the lower surface of the third refractory block (300) may be formed to have a flat surface (301) as in FIG. 3a, and when the upper surface of the protrusion (110) has an inclined surface (112) as in FIG. 2b, the lower surface of the third refractory block (300) may be formed to have an inclined surface (302) corresponding to the inclined surface (112) of the protrusion as in FIG. 3b.
[0071] Additionally, the contact surface with the protrusion (110) of the third refractory block (300) may be molded to have a structure in which a flat surface (301) and an inclined surface (302) alternate, as shown in FIG. 3C. Since such a structure increases the bonding strength between the first refractory block (100) and the third refractory block (300), it can prevent the first refractory block (100) at the bottom of the immersion pipe from detaching from the top of the immersion pipe, which is composed of the iron shell (10) and the second to fourth refractory blocks (200, 300, 400).
[0072] As illustrated in FIGS. 5 and 6, in step S300 of arranging the second refractory block and the third refractory block, the refractory blocks are arranged around the steel shell (10). The third refractory block (300) is arranged on the outside of the steel shell (10), and one side of the third refractory block (300) is in contact with the first refractory block (100). The second refractory block (200) is arranged in a part of the inside of the steel shell (10) to form a space (v) for welding the steel shell (10) and the reinforcing plate (120).
[0073] In step S300, the second refractory block (200) may be a shaped refractory. The second refractory block (200) may be formed by stacking multiple shaped refractories of a certain shape in multiple layers, or it may be in the form of a single shaped refractory. Although not shown in the drawing, it is understood that various modifications are possible for such a second refractory block (200) as long as it wraps around the inner surface of the steel shell (10). When multiple shaped refractories are arranged to form the second refractory block (200), an adhesive may be applied to the contact surfaces between the multiple shaped refractories.
[0074] In step S300, the third refractory block (300) may be a shaped refractory. The third refractory block (300) may be in the form of multiple shaped refractories arranged adjacent to each other, or it may be in the form of a single shaped refractory. Although not shown in the drawing, it is understood that various modifications are possible for such a third refractory block (300) as long as it wraps around the outer surface of the steel shell (10). When multiple shaped refractories are arranged to form the third refractory block (300), an adhesive may be applied to the contact surfaces between the multiple shaped refractories.
[0075] In step S300, the third refractory block (300) may be formed to include a step (310) on the side facing the outer surface of the first refractory block (100) and the steel shell (10). The first support (600) may be attached to the steel shell (10) so as to protrude from the outer surface of the steel shell (10) and may be extended outwardly to a length suitable for the step (310) of the third refractory block. The first support (600) may be extended in a direction parallel to one side of the step (310). The step (310) of the third refractory block is seated on the first support (600), and the first support (600) may support the load of the third refractory block (300) to reduce the stress applied to the first refractory block (100) and prevent the first refractory block (100) from falling off. The first support member (600) may be formed continuously along the outer circumference of the steel shell (10), or a plurality of support members may be spaced apart at intervals.
[0076] As illustrated in FIGS. 5 and 6, in step S400 of placing the first refractory block, the first refractory block (100) is placed in a structure in which the steel shell (10), the second refractory block (200), and the third refractory block (300) are placed. The first refractory block (100) is placed on the inner side of the steel shell (10) to form a space (v) for welding the steel shell (10) and the reinforcing plate (120) between the second refractory block (200). Preferably, prior to step S400, an additional step may be included in which an irregular refractory material (500) is filled into the space between the steel shell (10), the third refractory block (310), and the first refractory block (100).
[0077] In step S400, a predetermined gap may be provided between the end (p1) of the steel shell (10) and the first refractory block (100) for welding the steel shell (10) and the reinforcing plate (120). Additionally, at least a portion of the gap between the reinforcing plate (120) and the steel shell (10) may be filled with an amorphous refractory material, such as a refractory material and an insulating material, to prevent deformation of the steel shell (10). The amorphous refractory material may be mixed with a solvent in the form of a powder and installed to fill the space between the reinforcing plate (120) and the steel shell (10). Thus, it is possible to prevent the steel shell (10) from expanding or deforming due to high heat.
[0078] As illustrated in FIGS. 5 and 6, in step S500 of connecting the steel shell (10) and the reinforcing plate (120), a welding device enters through a space (v) from the inner direction of the steel shell (10), and the steel shell (10) and the reinforcing plate (120) are welded in the space between the end (p1) of the steel shell and the first refractory block (100) to form a welded portion (w). The steel shell (10) and the reinforcing plate (120) can be welded continuously along the circumferential direction with one end (p1) of the steel shell (10). Additionally, it may be possible to spot weld the steel shell (10) and the reinforcing plate (120) densely at regular intervals. However, in terms of rigidity, continuous welding is preferable. In this case, since welding of the reinforcing plate (120) and the steel shell (10) is possible along the circumference of the steel shell (10) and over the entire perimeter of the steel shell (10), the bonding strength between the steel shell (10) and the first refractory block (100) is increased, and thus the durability of the immersion pipe can be improved. Other fastening means, such as bolts and nuts, may be added to increase the bonding strength between the steel shell (10) and the first refractory block (100).
[0079] As illustrated in FIGS. 5 and 6, in step S600 where the fourth refractory block (400) is placed, the fourth refractory block (400) is placed in the space (v) formed between the first refractory block (100) and the second refractory block (200) to cover the welded portion (w) of the steel shell (10) and the reinforcing plate (120). One side of the fourth refractory block (400) is in contact with the steel shell (10), another side is in contact with the first refractory block (100), and yet another side is in contact with the second refractory block (200). Through this, the steel shell (10) is protected by refractory material on its entire surface so as not to be exposed to the outside. An adhesive may be applied to the contact surface between the first refractory block (100), the second refractory block (200), and the fourth refractory block (400).
[0080] Accordingly, as described above, by placing the fourth refractory block (400) after the reinforcing plate (120) of the first refractory block (100) and the steel shell (10) are combined, the reinforcing plate (120) and the steel shell (10) can be combined without drilling a separate fastening hole in the first refractory block or the third refractory block (300), and since welding is possible along the circumference of the steel shell (10), the bonding strength between the reinforcing plate (120) and the steel shell (10) can be increased and the durability of the immersion pipe can be improved.
[0081] In step S600, a second support member (700) may be provided between the second refractory block (200) and the fourth refractory block (400). The second support member (700) is coupled to the steel shell (10) so as to protrude from the inner surface of the steel shell (10) and is extended to a length suitable for positioning between the second refractory block (200) and the fourth refractory block (400). The second support member (700) is positioned between the second refractory block (200) and the fourth refractory block (400), such that one side of the second support member (700) is in contact with the second refractory block (200) and the other side is in contact with the fourth refractory block (400). Accordingly, the second support (700) supports the load of the second refractory block (200) and reduces the stress applied to the first refractory block (100) and the fourth refractory block (400), thereby preventing the first refractory block (100) from falling off.
[0082] The second support member (700) may be formed continuously along the outer circumference of the steel shell (10), or a plurality of support members may be spaced apart. In addition to the second support member (700), a plurality of support members may additionally protrude from the inner surface of the steel shell (10) and be attached to the steel shell (10). When a plurality of support members are additionally attached, a step is formed on the side facing the inner surface of the second refractory block (200) and the steel shell (10), or on the side where the inner surface of the fourth refractory block (400) and the steel shell (10) come into contact. Accordingly, by having each of these steps rest on each support member, the load of the second refractory block (200) and the fourth refractory block (400) can be stably supported.
[0083] As illustrated in FIGS. 5 and 6, in step S700 of filling the space between the refractory blocks and the steel shell, an irregular refractory material (500) may be filled in the space formed between the steel shell (10), the first refractory block (100), the second refractory block (200), the third refractory block (300), and the fourth refractory block (400). Through this, the first refractory block (100) can maintain a connection with the second refractory block (200), the third refractory block (300), and the fourth refractory block (400) at least firmly.
[0084] Accordingly, according to the method of constructing a immersion pipe according to the present invention described above based on FIGS. 5 and FIGS. 6, by efficiently arranging refractory materials having a certain shape on the outside and bottom of the immersion pipe around the iron shell (10), not only is the durability of the immersion pipe improved, but the construction time of the immersion pipe can also be shortened. Explanation of the symbols
[0085] 10: Iron skin 100: 1st refractory block 110: Protrusion 120: Metal strip 130: Flange 200: 2nd refractory block 300: 3rd refractory block 400: 4th refractory block 500: Amorphous refractory material 600: First support 700: Second support v: Space for welding the steel shell and reinforcing plate w: Welded joint between steel shell and reinforcing plate
Claims
Claim 1 Tube-shaped iron shell; A first refractory block disposed to face at least one end of the steel shell and including a reinforcing plate for welding with the steel shell; a second refractory block disposed inside the steel shell with a gap from the first refractory block to form a space for welding the steel shell and the reinforcing plate; An immersion tube comprising: a third refractory block in contact with the first refractory block and disposed on the outer side of the steel shell; and a fourth refractory block disposed in the space on the inner side of the steel shell to cover at least the welded portion of the steel shell and the reinforcing plate. Claim 2 The above reinforcing plate is an annular metal plate welded continuously or spacedly along the circumferential direction to one end of the steel shell through the above space, forming an immersion tube. Claim 3 In claim 1, the first refractory block further comprises a protrusion that protrudes in the longitudinal direction of the steel shell to support at least the reinforcing plate from the outer side of the reinforcing plate. Claim 4 In any one of paragraphs 1 through 3, The first refractory block above is a immersion tube made of shaped refractory or pre-cast refractory manufactured into a specific shape. Claim 5 In paragraph 3, the immersion tube comprising at least a portion of an inclined surface in contact with each other between the third refractory block and the protrusion. Claim 6 A immersion pipe according to claim 1, wherein the first refractory block is connected to one end of the reinforcing plate and further comprises a flange formed integrally with the reinforcing plate inside the first refractory block. Claim 7 In claim 1, the steel shell includes a first support protruding from the outer surface, and The third refractory block includes a step formed on the side facing the first refractory block and the outer surface of the steel shell, and The first support above is a immersion tube disposed on one side of the step. Claim 8 In paragraph 1, The above iron shell includes a second support protruding from the inner surface, and The above second support is a immersion tube disposed between the second refractory block and the fourth refractory block. Claim 9 In claim 1, the reinforcing plate is spaced apart from the outer surface of the steel shell at a predetermined distance, and at least a portion of the gap is filled with irregular refractory material to prevent deformation of the steel shell. Claim 10 A method for constructing a immersion pipe, comprising: a step of preparing a pipe-shaped steel shell; a step of preparing a first refractory block including a reinforcing plate for welding with the steel shell; a step of placing a third refractory block on the outer side of the steel shell and placing a second refractory block on a part of the inner side of the steel shell to form a space for welding the steel shell and the reinforcing plate; a step of placing a first refractory block to form the space with the second refractory block and to face at least one end of the steel shell; a step of welding the steel shell and the reinforcing plate through the space; and a step of placing a fourth refractory block in the space to seal at least the welded portion of the steel shell and the reinforcing plate on the inner side of the steel shell. Claim 11 A method for constructing a immersion pipe according to claim 10, wherein, in the step of welding the steel shell and the reinforcing plate, the reinforcing plate is welded continuously or spaced apart along the circumferential direction to one end of the steel shell through a welding device that moves in and out through the space. Claim 12 A method for constructing a immersion pipe according to claim 10, wherein the first refractory block further comprises a protrusion protruding in the longitudinal direction of the steel shell, configured to support the reinforcing plate from the outside of the reinforcing plate during welding of the steel shell and the reinforcing plate. Claim 13 A method for constructing an immersion pipe according to claim 10, further comprising the step of filling the space between the steel shell, the first refractory block, the second refractory block, the third refractory block, and the fourth refractory block with irregular refractory material. Claim 14 A method for constructing an immersion pipe according to any one of claims 10 to 12, wherein, in the step of preparing the first refractory block, the first refractory block is manufactured as a shaped refractory or a pre-cast refractory having a certain shape.