Anti-Slip Elastic Panel for Civil Engineering and Deck Comprising the Same

A composite laminated structure integrating a protective coating and elastic resin layer on aluminum panels addresses delamination and manufacturing complexity issues, enhancing durability and walkability by improving interfacial bonding strength and stability.

KR103045198B1Active Publication Date: 2026-11-10정호영 +1
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
KR1020260154662
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2026-08-18
Publication Date
2026-11-10
Estimated Expiration
2046-08-18

Smart Images

  • Figure 112026101053473-PAT00003_ABST
    Figure 112026101053473-PAT00003_ABST
Patent Text Reader

Abstract

The present invention relates to an anti-slip elastic panel for civil engineering and a deck including the same, comprising a panel body having connecting fitting portions formed along the longitudinal direction on both sides, an elastic resin layer formed to cover the upper side of the panel body, and a protective coating layer formed to cover the lower side of the panel body, wherein the elastic resin layer is continuously formed on the upper side of the protective coating layer and has a composite laminated structure that is melt-integrated with the protective coating layer, and the anti-slip elastic panel for civil engineering and a deck including the same. As such, the present invention forms a protective coating layer on the surface of a panel body and continuously laminates and bonds an elastic resin layer on the protective coating layer to form an integrated composite laminated structure. In the case of a water-based resin protective coating layer, a stable interfacial bonding structure with the elastic resin layer can be formed through interfacial bonding mediation and interfacial stress relief, and in the case of an HDPE-based protective coating layer, through thermal fusion between polyolefin resins. This suppresses interlayer delamination and lifting caused by repeated temperature changes and external loads, thereby improving long-term durability. Furthermore, by achieving protection of the panel body and stable lamination of the elastic resin layer without a separate primer coating process, the manufacturing process can be simplified and productivity improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] The present invention relates to an anti-slip elastic panel for civil engineering and a deck including the same, and more specifically, to an anti-slip elastic panel for civil engineering and a deck including the same in which a protective coating layer and an elastic resin layer are formed on the surface of a panel body to realize a stable coating and bonding structure for the panel body and secure excellent surface protection, durability, and walkability. Background Technology

[0002] Generally, decks consist of a structure in which multiple panels are connected and are widely used for hiking trails, walking paths, pedestrian walkways, bridges, terraces, and various outdoor facilities, and the panels are composed of wood, synthetic resin, metal, or non-ferrous metal.

[0003] Conventional wooden decks have the advantages of excellent appearance and good walking comfort, but they are prone to decay, cracking, and deformation when exposed to the external environment for a long period, requiring frequent maintenance. Meanwhile, although wood-plastic composites (WPC) offer improved durability, they suffer from issues such as warping due to thermal expansion and contraction, delamination between layers, and a decline in anti-slip performance.

[0004] Accordingly, decks made of metal substrates such as aluminum, which offer excellent lightness, corrosion resistance, and structural strength, are widely used recently, and various surface treatment technologies, such as fluorocarbon coating, powder coating, or polyurea coating, are being applied to the deck surface to improve walking comfort, wear resistance, and aesthetic appeal.

[0005] However, conventional aluminum decks mostly required a separate primer coating process to ensure adhesion between the aluminum substrate and the paint or coating layer; consequently, this not only complicated the manufacturing process but also caused environmental issues due to the use of organic solvents and reduced workability.

[0006] In addition, to resolve the problems associated with such painting and coating, a method was developed to install an elastic material having a certain elastic force on the panel body. However, the aforementioned conventional elastic material is configured such that a groove is formed in the panel body and the elastic material is inserted or bonded into the groove, or a coupling groove is formed in the panel body to allow the panel body and the elastic material to be mutually coupled in a male-female manner. This resulted in the problem of requiring separate processing of the panel body as well as increasing the assembly process.

[0007] In addition, since the elastic material and the panel body are joined as separate components, the elastic material was prone to detachment or looseness due to prolonged repeated walking loads, external impacts, or temperature changes; furthermore, there were issues where moisture or foreign substances penetrated through the joints, degrading durability and appearance quality.

[0008] In addition, a method of directly forming an elastic resin layer on the aluminum-based panel body is being developed; however, even in this case, interfacial delamination, lifting, and cracking were prone to occur during long-term use due to the difference in thermal expansion coefficients between aluminum and the polymer resin and insufficient interfacial bonding strength. Furthermore, even when a primer is used to resolve this, the manufacturing process becomes complex and there are limitations in securing long-term interfacial stability. Prior art literature

[0009] Registered Patent Publication No. 10-2231438 (March 18, 2021) The problem to be solved

[0010] The objective of the present invention is to provide a civil engineering anti-slip elastic panel and a deck including the same, which can protect the panel body from the external environment by forming a protective coating layer on the surface of the panel body, improve interfacial bonding strength and bonding stability between the protective coating layer and the elastic resin layer by continuously integrating an elastic resin layer on the outer side of the protective coating layer, suppress interlayer delamination and cracking due to temperature changes and repeated loads, and simultaneously ensure excellent durability, wear resistance, and walkability.

[0011] The objective of the present invention is to provide a civil engineering anti-slip elastic panel and a deck including the same, which can suppress interlayer delamination and cracking caused by temperature changes and repeated loads by forming a protective coating layer on the surface of a panel body and implementing a composite laminated structure in which an elastic resin layer is continuously laminated and integrated on the outer side of the protective coating layer, thereby protecting the panel body from the external environment by the protective coating layer and simultaneously securing interfacial bonding strength and bonding stability between the protective coating layer and the elastic resin layer.

[0012] The objective of the present invention is to provide a civil engineering anti-slip elastic panel and a deck including the same, which can improve appearance quality, durability, and productivity while ensuring protection of the panel body and bonding stability of the elastic resin layer by directly forming a protective coating layer on the surface of the panel body without forming a separate primer layer, and by continuously melting and integrating the upper elastic part and the side elastic part formed on the outer side of the protective coating layer.

[0013] The objective of the present invention is to provide a civil engineering anti-slip elastic panel and a deck including the same, which suppresses play and impact noise of the elastic panel and maintains a stable fastening state even under repetitive walking loads or temperature changes by forming a protective coating layer up to the inner surface of the connecting fitting part and elastically connecting it with a connecting clip. means of solving the problem

[0014] The anti-slip elastic panel for civil engineering according to the present invention comprises: a panel body (10) having connecting fitting parts (110) formed along the longitudinal direction on both sides and a vertical support part (120) connecting the upper and lower parts; an elastic resin layer (30) formed to cover the upper side of the panel body (10); and a protective covering layer (20) formed to cover the lower side of the panel body (10), wherein the elastic resin layer (30) may be configured to be connected continuously with the protective covering layer (20) to form an integrated structure.

[0015] At this time, the protective coating layer (20) may be formed on the surface of the panel body (10) with a thickness of 0.002 mm to 1.5 mm, and the elastic resin layer (30) may be formed with a thickness of 0.08 mm to 3.0 mm.

[0016] In addition, the anti-slip elastic panel for civil engineering according to the present invention comprises: a panel body (10) having a connecting fitting part (110) formed along the longitudinal direction on both sides and a vertical support part (120) connecting the upper and lower parts; a protective covering layer (20) formed on the upper surface (101), lower surface (102), upper side (103a) and lower side (103b) of both sides (103) of the panel body (10), and the inner surface (110a) of the connecting fitting part (110); and an elastic resin layer (30) formed by laminating on the upper surface (101) and the upper side (103a) of both sides (103) of the panel body (10) on which the protective covering layer (20) is formed. The elastic resin layer (30) is continuously bonded to the outer side of the protective coating layer (20) and integrated with the protective coating layer (20), and the upper surface elastic portion (310) of the elastic resin layer (30) formed on the upper surface (101) of the panel body (10) is characterized by having a natural wood veneer anti-slip pattern (311) formed thereon.

[0017] At this time, the composite laminated structure of the protective coating layer (20) and the elastic resin layer (30) formed to be located on the upper side of the panel body (10) may be formed to have a thickness of 0.082 mm to 4.5 mm on the surface of the panel body (10).

[0018] Additionally, the elastic resin layer (30) comprises an upper elastic portion (310) covering the upper surface (101) of the panel body (10); and a side elastic portion (320) connected to both sides of the upper elastic portion (310) and covering the upper side (103a) of the panel body (10), wherein the upper elastic portion (310) and the side elastic portion (320) are formed as a continuous integral by mutual melt bonding, and an anti-slip pattern (311) may be formed on the surface of the upper elastic portion (310).

[0019] At this time, the anti-slip pattern (311) is made of a natural wood veneer pattern.

[0020] Additionally, the side elastic portion (320) is formed while the upper elastic portion (310) maintains a state where it can be melt-bonded, and is melt-bonded with the upper elastic portion (310).

[0021] Additionally, the elastic resin layer (30) may be formed by an elastic resin composition comprising 55% to 70% by weight of polyolefin elastomer (POE), 15% to 30% by weight of high-density polyethylene (HDPE), 2% to 6% by weight of ultraviolet stabilizer, 7% to 15% by weight of inorganic filler, and 1% to 5% by weight of additive.

[0022] Additionally, the protective coating layer (20) may be formed by an aqueous resin composition comprising 60% to 70% by weight of an aqueous polyurethane-acrylic composite emulsion, 15% to 25% by weight of an aqueous epoxy resin, 1% to 5% by weight of a silane coupling agent, 1% to 6% by weight of an additive, and 5% to 15% by weight of deionized water.

[0023] Additionally, the protective coating layer (20) may be formed by a polyolefin resin composition comprising 65% to 80% by weight of HDPE (high density polyethylene), 5% to 15% by weight of LLDPE (linear low density polyethylene), 5% to 15% by weight of an inorganic filler, 1% to 5% by weight of a UV stabilizer, and 1% to 5% by weight of an additive including an antioxidant and a lubricating agent.

[0024] Furthermore, one or more concave grooves (104) are formed along the longitudinal direction on the upper surface (101) and lower surface (102) of the panel body (10), and the protective coating layer (20) and the elastic resin layer (30) are formed up to the interior of the concave grooves (104), so as to improve the contact area and mechanical bonding strength with the panel body (10).

[0025] Meanwhile, the anti-slip deck (C) for civil engineering according to the present invention is an anti-slip deck for civil engineering in which a plurality of elastic panels (A) are sequentially arranged on a floor surface (B) and adjacent elastic panels (A) are connected so as to be in close contact with each other by one or more connecting clips (80). The connecting clip (80) includes a plate-shaped base plate (810) and an elastic coupling part (820) formed integrally with the base plate (810). The elastic coupling part (820) may be configured to include one or more first elastic support pieces (821) inserted into the connecting fitting part (110) of one elastic panel (A) and one or more second elastic support pieces (822) inserted into the connecting fitting part (110) of the other elastic panel (A).

[0026] At this time, the first elastic support piece (821) and the second elastic support piece (822) can be formed integrally with the base plate (810) by cutting a part of the base plate (810) and then bending it. Effects of the invention

[0027] The present invention forms a protective coating layer on the surface of an aluminum panel body and continuously forms an elastic resin layer in the outer area of ​​the protective coating layer corresponding to the upper surface and upper side of the panel body, thereby protecting the panel body from the external environment while simultaneously providing elasticity, wear resistance, and impact resistance to the area where walking and external loads mainly act.

[0028] In addition, the protective coating layer can continuously cover the surface of the panel body to prevent moisture, contaminants, and corrosive agents from coming into direct contact with the aluminum panel body, thereby preventing surface damage and corrosion of the panel body and improving corrosion resistance and long-term durability. In particular, on the lower surface, lower side, and inner surface of the connecting fitting part of the panel body where the elastic resin layer is not formed, a coating surface is formed in which the protective coating layer itself is exposed to the outside, so that the protective coating layer can perform an independent surface protection function distinct from a simple primer layer for bonding the elastic resin layer.

[0029] When the above protective coating layer is formed from an aqueous resin composition comprising aqueous PU-acrylic, aqueous epoxy, and silane, the aqueous PU-acrylic secures the flexibility of the protective coating layer and interfacial affinity with the upper elastic resin layer, the aqueous epoxy improves the cohesiveness of the protective coating layer itself and adhesion to the aluminum panel body, and the silane assists in interfacial bonding between the aluminum panel body and the organic resin. Accordingly, both the adhesion of the protective coating layer to the panel body and the stability of the protective coating layer itself can be secured.

[0030] Furthermore, when an elastic resin composition based on a polyolefin elastomer (POE) is supplied in a molten state to the outer surface of the above-mentioned aqueous protective coating layer to laminate and integrate them, the aqueous protective coating layer can act as a functional intermediate coating layer that mitigates the difference in physical properties between the aluminum panel body and the elastic resin layer. Accordingly, compared to the case where the panel body and the elastic resin layer are directly bonded, interfacial bonding stability is improved, and stress concentration at the interface caused by thermal expansion and contraction due to temperature changes or repetitive walking loads is suppressed, thereby reducing delamination, lifting, and cracking of the elastic resin layer. In particular, the flexibility provided by the aqueous PU-acrylic and the adhesion and cohesiveness provided by the aqueous epoxy act complementarily to improve the bonding reliability and long-term durability of the composite laminated structure.

[0031] Meanwhile, when the above protective coating layer is formed from a polyolefin-based resin composition comprising high-density polyethylene (HDPE) as the main component, linear low-density polyethylene (LLDPE), inorganic fillers, UV stabilizers, and additives, the hardness, wear resistance, water resistance, and corrosion resistance of the protective coating layer can be secured by the HDPE, and the brittleness of the HDPE can be compensated for by the LLDPE to ensure a predetermined toughness and extrusion processability. Furthermore, dimensional stability can be improved by suppressing thermal shrinkage and deformation occurring during the extrusion and cooling processes through the inorganic fillers, and the deterioration of the resin due to outdoor exposure and high-temperature processing can be suppressed through the UV stabilizers and antioxidants. Accordingly, a protective coating structure with excellent durability and dimensional stability can be formed over the entire body of the aluminum panel.

[0032] In addition, when an elastic resin layer based on POE is laminated and integrated on the outer side of the HDPE-based protective coating layer, both the protective coating layer and the elastic resin layer contain polyolefin-based resins, and in particular, since HDPE components can be commonly included in both layers, material compatibility between the two layers can be secured. Accordingly, during the process of supplying the elastic resin layer in a molten state onto the protective coating layer, melt bonding and integration between the two layers are promoted, thereby improving interfacial bonding stability and suppressing delamination or separation between layers due to repeated temperature changes and external loads. Furthermore, the hardness, water resistance, corrosion resistance, and dimensional stability provided by the lower protective coating layer and the elasticity, shock absorption, and wear resistance provided by the upper elastic resin layer work complementarily to improve the durability of the entire composite laminated structure.

[0033] Furthermore, the elastic resin layer described above uses POE as the main component to impart elasticity and shock absorption to the surface of the panel, and by including HDPE to compensate for the excessive softness of POE, surface hardness, abrasion resistance, and scratch resistance can be improved. In addition, shrinkage deformation caused by extrusion and cooling is suppressed by inorganic fillers, and discoloration, powdering, and cracking caused by long-term outdoor exposure are suppressed by UV stabilizers, thereby ensuring the surface durability and weather resistance required for outdoor elastic panels.

[0034] In addition, the elastic resin layer according to the present invention includes an upper elastic portion formed on the upper surface of the panel body and side elastic portions formed on both upper sides of the panel body. Since the upper elastic portion and the side elastic portions are continuously integrated, the upper surface of the panel body can be protected as well as the corners and upper sides. Accordingly, corner damage caused by walking and external impact is suppressed, the impact resistance and wear resistance of the side portions are improved, and the appearance quality is enhanced by preventing discontinuous joints between the upper surface and the side portions from appearing externally.

[0035] In addition, by continuously forming a protective coating layer up to the inner surface of the connecting part of the panel body, direct contact between the connecting clip and the aluminum panel body is prevented, and the surface of the connecting part can be protected. Accordingly, wear, damage, and noise generation at the connecting part caused by repetitive walking loads or temperature changes are reduced, and a stable fastening state can be maintained for a long period.

[0036] Furthermore, the present invention prevents slipping by securing the frictional force required during walking through the formation of an anti-slip pattern on the surface of an elastic resin layer, and can provide an excellent walking sensation along with the elasticity and shock absorption properties of the elastic resin layer itself. Additionally, if the anti-slip pattern is formed as an irregularity or pattern corresponding to the surface shape of natural wood, a texture and appearance similar to natural wood can be realized, thereby improving the aesthetic appeal of the elastic panel and the deck utilizing it.

[0037] Accordingly, the present invention allows for the selective composition of the protective coating layer material as a water-based resin or an HDPE-based polyolefin resin, while simultaneously ensuring surface protection of the panel body and elasticity and wear resistance through the upper elastic resin layer. Furthermore, by forming a stable composite laminated structure with the elastic resin layer in a manner suitable for the material characteristics of each protective coating layer, it is possible to comprehensively improve corrosion resistance, weather resistance, durability, bonding stability, and walkability required in outdoor civil engineering environments. Brief explanation of the drawing

[0038] FIG. 1 is an exemplary diagram showing the configuration of an elastic panel according to the present invention. FIG. 2 is an exemplary diagram showing the front configuration of an elastic panel according to the present invention. FIG. 3 is an exemplary diagram showing the configuration of an embodiment of an elastic panel according to the present invention. FIG. 4 is an example diagram showing the front configuration of an elastic panel according to FIG. 3. FIG. 5 is an example diagram showing the interlayer structure of an elastic panel according to FIG. 3. FIG. 6 is an exemplary diagram showing the configuration of an anti-slip deck according to the present invention. FIG. 7 is an exemplary diagram showing the combined relationship between an elastic panel and a connecting clip according to the present invention. FIG. 8 is an exemplary diagram showing the configuration of a connecting clip according to the present invention. Specific details for implementing the invention

[0039] The main objective of the present invention is to provide a civil engineering anti-slip elastic panel and a deck including the same, which can improve interfacial bonding strength and bonding stability and prevent interlayer delamination due to temperature changes, and secure excellent durability, wear resistance, walkability, and productivity without a separate primer coating process, by implementing a composite laminated structure in which a protective coating layer and an elastic resin layer are continuously laminated and integrated on the surface of a panel body so that the protective coating layer acts as a functional interface layer between the panel body and the elastic resin layer.

[0040] First, referring to FIG. 1, the anti-slip elastic panel (A) for civil engineering according to the present invention includes a composite structure in which an elastic resin layer (30) is formed on the upper part of the panel body (10) and a protective coating layer (20) is formed on the lower part.

[0041] The panel body (10) is preferably formed as a profile of a hollow structure extending in the longitudinal direction, and connecting fitting parts (110) for connecting to adjacent elastic panels (A') may be formed along the longitudinal direction on both sides. Additionally, the panel body (10) is preferably formed as a hollow structure equipped with one or more vertical support parts (120) connecting the upper and lower parts.

[0042] The above panel body (10) may be made of aluminum, aluminum alloy, iron, iron alloy, carbon, or carbon alloy individually or in combination, and preferably may be composed of a hollow profile made of aluminum or aluminum alloy substrate.

[0043] The above connecting fitting part (110) may be formed in a groove shape having a predetermined depth so as to be coupled with a connecting clip (80) described later, and the two sides of the panel body (10) may be divided into an upper side (103a) and a lower side (103b) based on the connecting fitting part (110), as shown in FIG. 3. The upper side (103a) refers to a part located above the connecting fitting part (110) and connected to the upper surface (101) of the panel body (10), and the lower side (103b) refers to a part located below the connecting fitting part (110) and connected to the lower surface (102) of the panel body (10).

[0044] In addition, one or more concave grooves (104) may be formed along the longitudinal direction on the upper surface (101) and lower surface (102) of the panel body (10), as shown in (a) of FIG. 2. The concave grooves (104) can be filled with a resin layer to be described later, thereby increasing the contact area between the panel body (10) and the resin layer (20, 30) and providing a mechanical interlocking effect, which can improve the bonding strength.

[0045] Additionally, the panel body (10) may undergo a pretreatment process including degreasing, chromate treatment, washing, and drying before the protective coating layer (20) or elastic resin layer (30) is formed. In particular, when chromate treatment is performed, the surface of the panel body (10) may be finely roughened (104a) as shown in (b) of FIG. 2, thereby further improving the surface contact area and interfacial bonding strength.

[0046] Referring to FIGS. 1 and 2, the above protective coating layer (20) can be formed on the lower surface (102), lower side (103b) of the panel body (10), and the inner surface (110a) of the connecting fitting part (110), and can form an integrated structure that is continuous with the elastic resin layer (30).

[0047] The above protective coating layer (20) is formed to cover the surface of the panel body (10) to protect the panel body (10) from the external environment, and can be formed by a water-based resin or a polyolefin resin based on HDPE (high density polyethylene).

[0048] The above protective coating layer (20) can be formed by supplying a resin composition for forming the protective coating layer (20) to a corresponding surface of the panel body (10), spreading, pressing, and adjusting the thickness of the resin composition using a roller, or by extruding and supplying the resin composition to a corresponding surface of the panel body (10) using an extrusion head.

[0049] In one embodiment, the protective coating layer (20) may be formed by an aqueous resin composition comprising an aqueous polyurethane-acrylic composite emulsion as the main component.

[0050] For example, the above aqueous resin composition may comprise 60% to 70% by weight of an aqueous polyurethane-acrylic composite emulsion, 15% to 25% by weight of an aqueous epoxy resin, 1% to 5% by weight of a silane coupling agent, 1% to 6% by weight of an additive, and 5% to 15% by weight of deionized water.

[0051] The above water-based polyurethane-acrylic composite emulsion can form a continuous and uniform resin layer on the surface of the panel body (10) as a main film component of the protective coating layer (20), and can impart flexibility and durability to the protective coating layer (20). In addition, when an elastic resin layer (30) is laminated on the protective coating layer (20), the bonding stability of the composite laminated structure can be improved by mediating interfacial bonding between the panel body (10) and the elastic resin layer (30) and relieving interfacial stress caused by the difference in physical properties between the two materials.

[0052] If the above water-based polyurethane-acrylic composite emulsion is included in an amount of less than 60% by weight, it may be difficult to sufficiently secure the continuity, flexibility, and coating properties of the protective coating layer (20) and the panel body (10), and if it is included in an amount exceeding 70% by weight, the relative content of other components decreases, and there is a concern that the adhesion and interfacial bonding properties to the panel body (10) may be reduced, so it is preferable to include it within the above range.

[0053] The above water-based epoxy resin improves the cohesiveness of the protective coating layer (20) and the adhesion to the panel body (10), and improves the bonding stability between the aluminum panel body (10) and the protective coating layer (20), thereby suppressing peeling or lifting of the protective coating layer (20) due to long-term use.

[0054] If the above water-based epoxy resin is included in an amount of less than 15% by weight, it may be difficult to sufficiently secure adhesion and adhesive strength to the panel body (10), and if it is included in an amount exceeding 25% by weight, the protective coating layer (20) may become excessively hard, resulting in reduced flexibility and reduced responsiveness to temperature changes or external forces, so it is preferable to include it within the above range.

[0055] The above silane coupling agent can improve the interfacial affinity and bonding durability of the protective coating layer (20) on the aluminum panel body (10) by modifying the interface between the panel body (10) and the aqueous resin composition.

[0056] If the above silane coupling agent is included in an amount of less than 1 weight%, the interfacial modification effect between the panel body (10) and the aqueous resin composition may not be sufficient, and if it is included in an amount exceeding 5 weight%, the additional interfacial bonding strength enhancement effect may be limited or there is a concern that the storage stability and resin layer formation ability of the aqueous resin composition may be reduced, so it is preferable to include it within the above range.

[0057] The above additive may include a wetting agent, an antifoaming agent, a leveling agent, or a combination thereof, and can improve the fluidity and supply stability of the aqueous resin composition and suppress bubbles, pinholes, and thickness non-uniformity that may occur during the formation process of the protective coating layer (20) by roller or extrusion, thereby forming a uniform protective coating layer (20).

[0058] The above deionized water serves as a dilution medium for controlling the viscosity and fluidity of the aqueous resin composition, allowing the aqueous resin composition to be uniformly supplied and formed on the surface of the panel body (10) by means of a roller or extrusion, and reducing the use of volatile organic solvents.

[0059] The above-described aqueous resin composition allows for the continuity and flexibility of the protective coating layer (20) by the aqueous polyurethane-acrylic composite emulsion, adhesion to the panel body (10) by the aqueous epoxy resin, interfacial bonding by the silane coupling agent, supply and coating formation stability by the additive, and viscosity control effect by the deionized water to work complementarily to form a stable protective coating layer (20) on the surface of the panel body (10) while simultaneously ensuring interfacial bonding stability with the upper elastic resin layer (30).

[0060] In another embodiment, the protective coating layer (20) may be formed by a polyolefin-based resin composition based on HDPE (high density polyethylene).

[0061] Specifically, the polyolefin resin composition may comprise, based on 100% by weight of the total, 65% to 80% by weight of HDPE, 5% to 15% by weight of LLDPE (linear low density polyethylene), 5% to 15% by weight of an inorganic filler, 1% to 5% by weight of a UV stabilizer, and 1% to 5% by weight of an additive including an antioxidant and a lubricating agent. The inorganic filler may include calcium carbonate, talc powder, or a mixture thereof.

[0062] The above HDPE is a component that forms the main resin matrix of the protective coating layer (20), thereby imparting a certain hardness and mechanical strength to the protective coating layer (20) and preventing moisture or external contaminants from coming into direct contact with the panel body (10), thus protecting the aluminum panel body (10) from the external environment. In addition, HDPE has excellent water resistance, chemical resistance, and abrasion resistance, which can improve the surface protection and long-term durability of the panel body (10) exposed to the outdoor environment.

[0063] If the above HDPE is included in an amount of less than 65 weight%, the continuity of the resin matrix is ​​relatively reduced, making it difficult to sufficiently secure the hardness, wear resistance, and dimensional stability required for the protective coating layer (20); if it is included in an amount exceeding 80 weight%, the flexibility and toughness of the protective coating layer (20) are relatively reduced, and the possibility of cracking or brittle fracture occurring during the deformation process due to thermal shrinkage or external force may increase, so it is added within an appropriate range.

[0064] The above LLDPE is mixed with HDPE to impart toughness and flexibility to the protective coating layer (20) and to suppress brittle fracture or cracking that may occur due to the high crystallinity and hardness of HDPE, thereby supplementing fluidity and processability in the molten state so that the polyolefin resin composition can be stably supplied and molded along the surface of the panel body (10).

[0065] If the above LLDPE is included in an amount of less than 5 weight%, it is difficult to sufficiently compensate for the hardness of HDPE, and the possibility of cracking or brittle failure occurring during the bending or thermal deformation process of the protective coating layer (20) may increase, and if it exceeds 15 weight%, the hardness and wear resistance of the protective coating layer (20) are relatively reduced, and the dimensional stability and surface protection required for the protective coating layer (20) based on HDPE may be reduced.

[0066] The above-mentioned inorganic filler may consist of calcium carbonate, talc powder, or a mixture thereof, and can improve the dimensional stability of the protective coating layer (20) by suppressing thermal shrinkage of the polyolefin resin composition and reducing shrinkage deformation or warping that may occur during the extrusion and cooling process. In particular, talc powder is advantageous for suppressing thermal deformation and shrinkage of the resin matrix due to its plate-like structure, and calcium carbonate can reduce raw material costs while supplementing the rigidity and dimensional stability of the protective coating layer (20).

[0067] In addition, when the calcium carbonate and talc powder are mixed and used, the effect of improving rigidity and dimensional stability due to the calcium carbonate and the effect of suppressing thermal shrinkage and deformation due to the talc powder can act complementarily. At this time, the mixing ratio of the calcium carbonate and talc powder is not specifically limited, and can be adjusted and mixed in an appropriate ratio so that the effects of each component can be realized in a balanced manner, taking into account the mechanical strength, dimensional stability, thermal shrinkage suppression, and extrusion processability required for the protective coating layer (20).

[0068] If the above inorganic filler is included in an amount of less than 5% by weight, the effect of suppressing thermal shrinkage and improving dimensional stability may not be sufficient, and if it exceeds 15% by weight, the melt flowability of the resin composition may decrease, resulting in reduced extrusion processability, and the toughness and bending properties of the protective coating layer (20) may decrease or the surface may become rough due to an increase in the interface between the resin and the inorganic filler.

[0069] The above UV stabilizer is intended to improve the weather resistance of the protective coating layer (20) by suppressing photo-oxidation deterioration, discoloration, powdering, and cracking that may occur in the protective coating layer (20) due to long-term exposure to sunlight in an outdoor environment.

[0070] If the above UV stabilizer is included in an amount of less than 1 weight%, it may be difficult to sufficiently suppress UV degradation due to long-term outdoor exposure, and if it exceeds 5 weight%, it is difficult to expect an improvement in weather resistance proportional to the increase in the amount added, and since an excessive amount of additive may affect the dispersibility or physical properties of the resin matrix, it is desirable to include it within the above range.

[0071] The above additives may include an antioxidant and a lubricating processing aid. The antioxidant can suppress the degradation of physical properties caused by thermal oxidation of HDPE and LLDPE during the process of melting and extruding the polyolefin-based resin composition at high temperatures. The lubricating processing aid improves the melt flowability of the resin composition and reduces friction and adhesion between the extruder, mold, and the resin composition, thereby ensuring that the resin composition is discharged uniformly and preventing the accumulation of resin in the discharge portion of the mold.

[0072] If the above additive is included in an amount of less than 1 weight%, the effects of inhibiting thermal oxidation during the high-temperature extrusion process, improving melt flowability, and inhibiting mold adhesion may not be sufficient, and if it exceeds 5 weight%, the excess additive may affect the mechanical properties or surface characteristics of the protective coating layer (20) and the additional effect of improving processability may be limited, so it is preferable to include it within the above range.

[0073] Such a polyolefin-based resin composition can secure the hardness, wear resistance, water resistance, and corrosion resistance required for the protective coating layer (20) by means of HDPE, while compensating for the brittleness of HDPE by means of LLDPE to secure the specified toughness and processability. In addition, shrinkage and deformation occurring during the extrusion and cooling process can be suppressed by means of inorganic fillers, and deterioration of the resin due to outdoor environments and high-temperature processing can be suppressed by means of UV stabilizers and antioxidants.

[0074] Accordingly, the protective coating layer (20) made of the above polyolefin resin composition can cover the surface of the aluminum panel body (10) to protect the panel body (10) from external moisture, contaminants, and corrosive environments, and at the same time maintain a stable shape even after extrusion and cooling, thereby forming a protective coating structure with excellent durability and dimensional stability on the surface of the panel body (10).

[0075] The protective coating layer (20) can be formed on the surface of the panel body (10) with a thickness of 0.002 mm to 1.5 mm, and preferably with a thickness of about 0.2 mm to 1.2 mm.

[0076] If the thickness of the protective coating layer (20) is less than 0.002 mm, it is difficult to continuously cover the surface of the panel body (10), so localized non-uniformity of coverage or uncovered areas may occur, and it may be difficult to sufficiently secure surface protection and coverage stability for the panel body (10). If it exceeds 1.5 mm, the effect of improving protection with increasing thickness is limited, while the amount of raw material used increases, and there is a risk of deformation or internal stress increasing during the formation of the protective coating layer (20) and subsequent processes.

[0077] In particular, when the thickness of the protective coating layer (20) is 0.2 mm or more, a relatively uniform and continuous coating thickness can be secured despite surface irregularities or fine shape deviations of the panel body (10), thereby ensuring surface protection and coating stability more stably, and in the area where the elastic resin layer (30) is laminated, it is advantageous to secure a sufficient coating thickness to support the elastic resin layer (30).

[0078] The protective coating layer (20) configured as described above is distinguished from a primer layer that merely improves the adhesion of a metal substrate, and is formed independently on the surface of the panel body (10) with a predetermined thickness to perform the function of protecting the panel body (10) from the external environment. In particular, the protective coating layer (20) can act as an intermediate coating layer that improves the interfacial bonding stability between the two layers by being located between the panel body (10) and the elastic resin layer (30) in the area where the elastic resin layer (30) is laminated. By being continuously laminated and bonded with the elastic resin layer (30) to form a composite laminated structure, interlayer delamination and lifting can be suppressed, and a long-term stable bonding state and excellent durability can be secured.

[0079] The above elastic resin layer (30) includes an upper elastic portion (310) covering the upper surface of the panel body (10) as in FIG. 1 and a side elastic portion (320) covering the upper side (103a) of the panel body (10), and the upper elastic portion (310) and the side elastic portion (320) can be formed as a continuous integral by mutually melting and bonding.

[0080] At this time, the upper surface elastic part (310) can be formed to have a predetermined thickness by extruding a molten elastic resin composition onto the upper surface of the panel body (10) and then applying pressure by a roller.

[0081] Additionally, the side elastic member (320) may be formed by extruding a molten elastic resin composition onto the upper side (103a) of the panel body (10) and, if necessary, by applying pressure with a roller. Furthermore, the side elastic member (320) may be formed as a continuous integral by melt-bonding with the upper elastic member (310) before the upper elastic member (310) is completely solidified, that is, while the upper elastic member (310) maintains a state where melt-bonding is possible.

[0082] The above elastic resin layer (30) can be formed by an elastic resin composition comprising polyolefin elastomer (POE) as the main component and high-density polyethylene (HDPE).

[0083] For example, the elastic resin composition may comprise 55% to 70% by weight of polyolefin elastomer (POE), 15% to 30% by weight of high-density polyethylene (HDPE), 2% to 6% by weight of UV stabilizer, 7% to 15% by weight of inorganic filler, and 1% to 5% by weight of additive.

[0084] The above polyolefin elastomer (POE) is a thermoplastic elastic resin that forms the main component of the elastic resin layer (30), and provides excellent elasticity and resilience, thereby mitigating impact during walking and providing an excellent walking sensation. In addition, it maintains excellent ductility even in low-temperature environments to prevent cracking, and can achieve a soft touch similar to wood.

[0085] If the above polyolefin elastomer (POE) is included in an amount of less than 55% by weight, it may be difficult to sufficiently secure the elasticity, resilience, and low-temperature ductility required for the elastic resin layer (30), and if it exceeds 70% by weight, the elastic resin layer (30) may become excessively soft, and there is a risk that the surface hardness, wear resistance, and dimensional stability may be reduced, so it is preferable to include it within the above range.

[0086] The above high-density polyethylene (HDPE) can improve the surface hardness and wear resistance of the elastic resin layer (30), thereby suppressing wear and scratching caused by walking for a long time or external impact and improving the durability of the surface.

[0087] If the above high-density polyethylene (HDPE) is included in an amount of less than 15% by weight, the surface hardness and wear resistance are not sufficiently secured, so wear and scratching may occur due to long-term use, and if it exceeds 30% by weight, the elastic resin layer (30) becomes excessively hard, and there is a risk that elasticity, resilience and walking feel will be reduced, so it is desirable to include it within the above range.

[0088] The above UV stabilizer inhibits the decomposition of polymer chains by ultraviolet rays, thereby preventing discoloration, powdering, and deterioration of physical properties of the elastic resin layer (30), and thus can maintain excellent weather resistance even in an outdoor environment for a long period of time.

[0089] If the above UV stabilizer is included in an amount of less than 2 weight%, it may be difficult to sufficiently suppress discoloration, powdering, and deterioration of physical properties caused by UV rays, and if it exceeds 6 weight%, while the additional effect of improving weather resistance is limited, there is a concern that the economic efficiency and balance of physical properties of the composition may be reduced, so it is desirable to include it within the above range.

[0090] The above-mentioned inorganic filler may include talc, calcium carbonate, silica, mica, kaolin, barium sulfate, or a combination thereof, and preferably may include talc.

[0091] The above-mentioned inorganic filler improves the thermal stability and dimensional stability of the upper elastic resin layer (30) to suppress thermal shrinkage and warping after molding, improves mechanical strength and surface rigidity to suppress deformation and wear caused by external forces, and can reduce manufacturing costs by including an appropriate amount.

[0092] In one embodiment, when the inorganic filler includes talc powder, the rigidity and dimensional stability of the elastic resin layer (30) are further improved, thereby improving the shape retention of the anti-slip pattern (311) formed by the heat pressing of the pattern roller described later, and suppressing wear and deformation of the anti-slip pattern (311) even during long-term use.

[0093] If the above-mentioned inorganic filler is included in an amount of less than 7% by weight, it may be difficult to sufficiently express thermal stability, dimensional stability, and thermal shrinkage inhibition effects, and if it exceeds 15% by weight, there is a risk that the melt fluidity of the elastic resin composition may decrease or the elasticity and surface tactile sensation of the elastic resin layer (30) may decrease, so it is preferable to include it within the above range.

[0094] The above additive may include an antioxidant, a processing aid, or a combination thereof, and can prevent thermal decomposition of the elastic resin during high-temperature extrusion and thermal composite processes and improve melt fluidity, thereby improving extrusion stability and moldability. Accordingly, the thickness and surface condition of the elastic resin layer (30) can be formed more uniformly. Since known additives may be used, a detailed description thereof is omitted.

[0095] The elastic resin composition described above can prevent the elastic resin layer (30) from becoming excessively soft or hard by ensuring excellent walking comfort and surface durability at the same time, as the elasticity and resilience provided by the polyolefin elastomer (POE) and the surface hardness and wear resistance provided by the high-density polyethylene (HDPE) work complementarily.

[0096] In addition, the elastic resin layer (30) can be formed with a thickness of about 0.08 mm to 3.0 mm, and while providing excellent walking comfort and wear resistance by securing sufficient elasticity and resilience, it can maintain a stable surface condition for a long period of time by suppressing thermal shrinkage and deformation caused by excessive thickness increase.

[0097] If the thickness of the elastic resin layer (30) is less than 0.08 mm, it may be difficult to secure sufficient elasticity and resilience to absorb and mitigate repeated walking loads or external impacts, and the elastic resin layer (30) may wear out prematurely due to repeated friction, thereby reducing surface protection and durability for the panel body (10). Additionally, if the thickness of the elastic resin layer (30) exceeds 3.0 mm, the additional improvement effect of elasticity and shock absorption due to the increase in the thickness of the elastic resin layer (30) is limited, while the amount of elastic deformation due to walking load increases, which may reduce the dimensional stability of the surface. In particular, during the cooling process after extrusion, the difference in cooling speed between the inside and outside of the elastic resin layer (30) increases, which may cause shrinkage deviation, warping, or local deformation, and the amount of raw material used and cooling time may increase, thereby reducing manufacturing efficiency and economic feasibility.

[0098] Meanwhile, the anti-slip elastic panel (A) for civil engineering according to the present invention may include a composite laminated structure in which a protective coating layer (20) is formed over the entire surface of the panel body (10) as shown in FIGS. 3 to 5, and the upper side of the panel body (10) has a protective coating layer (20) and an elastic resin layer (30) laminated thereon.

[0099] Specifically, the present invention may include a panel body (10) having connecting fitting portions (110) formed along the longitudinal direction on both sides; a protective covering layer (20) formed to cover the entire surface of the panel body (10); and an elastic resin layer (30) formed on the protective covering layer (20) to cover the upper side of the panel body (10).

[0100] More specifically, the protective coating layer (20) is formed on the upper surface (101), lower surface (102), upper side (103a) and lower side (103b) of the two sides (103) of the panel body (10) and the U-shaped inner surface (110a) of the connecting fitting part (110), and the elastic resin layer (30) is formed by laminating on the upper surface (101) and upper side (103a) of the two sides (103) of the panel body (10) where the protective coating layer (20) is formed, and the elastic resin layer (30) is formed as a composite laminated structure that is continuously bonded to the outside of the protective coating layer (20) and integrated with the protective coating layer (20).

[0101] In addition, the composite laminated structure of the protective coating layer (20) and the elastic resin layer (30), which is formed to be located on the upper side of the panel body (10), can be formed to have a thickness of about 0.082 mm to 4.5 mm from the surface of the aluminum panel body (10), and preferably can be formed to have a thickness of about 0.58 mm to 3.0 mm.

[0102] The above protective coating layer (20) and elastic resin layer (30) can each be continuously formed along the longitudinal direction of the panel body (10), and the elastic resin layer (30) can be continuously bonded to the outer side of the protective coating layer (20) by extruding and supplying a molten elastic resin composition to the outer side of the protective coating layer (20) and then pressurizing and molding it by a roller. Accordingly, a continuous composite laminated structure can be formed on the upper surface (101) and both upper sides (103a) of the panel body (10) in which the panel body (10), the protective coating layer (20), and the elastic resin layer (30) are sequentially laminated and bonded to each other.

[0103] In one embodiment, when the protective coating layer (20) is formed from an aqueous resin composition, the protective coating layer (20) can mediate interfacial bonding between the panel body (10) and the elastic resin layer (30) and alleviate interfacial stress caused by differences in physical properties and thermal expansion characteristics. Accordingly, by continuously laminating and bonding the elastic resin layer (30), which is supplied in a molten state, to the outside of the protective coating layer (20), interfacial bonding stability can be improved compared to the case where the panel body (10) and the elastic resin layer (30) are directly bonded, and interlayer delamination, lifting, and cracking caused by repeated temperature changes, walking loads, and external impacts can be suppressed.

[0104] In another embodiment, when the protective coating layer (20) is formed from a polyolefin-based resin composition based on HDPE, both the protective coating layer (20) and the elastic resin layer (30) contain polyolefin-based resin and include HDPE as a common component. Therefore, during the process of extruding and pressing the molten elastic resin layer (30) to the outside of the protective coating layer (20), thermal fusion and integration between the two layers can be smoothly achieved, thereby improving the interfacial bonding stability between the two layers and suppressing interlayer delamination or lifting due to repeated temperature changes and external loads.

[0105] In this way, by continuously laminating an elastic resin layer (30) on the outer side of the protective coating layer (20) to form a composite laminated structure, even when repeated walking loads, external impacts, and temperature changes are applied to the upper surface (101) and both upper sides (103a) of the panel body (10), a stable bonded state can be maintained while suppressing interlayer delamination and lifting, and the long-term durability of the composite laminated structure can be improved.

[0106] In addition, as shown in FIG. 4 (b), the present invention may form an anti-slip pattern (311) of natural wood veneer on the upper surface elastic portion (310) of the elastic resin layer (30) formed on the upper surface (101) of the panel body (10).

[0107] Meanwhile, the anti-slip deck (C) for civil engineering according to the present invention has a structure in which adjacent elastic panels (A) are connected by one or more connecting clips (80).

[0108] That is, with reference to FIGS. 6 to 8, the present invention can sequentially arrange a plurality of elastic panels (A) on a bottom surface (B) and connect and fix adjacent elastic panels (A) so that they are in close contact with each other using one or more connecting clips (80).

[0109] As shown in FIG. 8, the above connecting clip (80) includes a plate-shaped base plate (810) and an elastic coupling part (820) formed integrally with the base plate (810), and the elastic coupling part (820) may include one or more first elastic support pieces (821) inserted into the connecting fitting part (110) of one elastic panel (A) and one or more second elastic support pieces (822) inserted into the connecting fitting part (110) of the other elastic panel (A').

[0110] At this time, it is preferable that the elastic coupling part (820) be formed integrally with the base plate (810) by cutting a part of the base plate (810) and then bending it.

[0111] The connecting clip (80) configured in this manner can fix the pair of elastic panels (A) to the bottom surface (B) by fixing the base plate (810) to the bottom surface (B) by means of a fastening screw or an equivalent fastening means (830), and by fitting one or more first elastic support pieces (821) and one or more second elastic support pieces (822) to each of the connecting fitting parts (110) formed on the adjacent pair of elastic panels (A).

[0112] At this time, the elastic coupling part (820) provides continuous elastic restoring force while elastically contacting and supporting the protective coating layer (20) formed on the inner surface of the connecting fitting part (110), thereby suppressing the occurrence of play in the elastic panel (A) and maintaining a stable fastening state. In addition, the protective coating layer (20) acts as a functional interface layer that protects the inner surface of the connecting fitting part (110), and at the same time, relieves contact stress with the elastic coupling part (820), thereby suppressing wear caused by repeated fastening and vibration.

[0113] In addition, the connecting clip (80) simultaneously elastically supports two adjacent elastic panels (A) through an elastic coupling part (820) integrally formed on a base plate (810), thereby improving constructability and stably supporting the elastic panels (A) while suppressing the occurrence of gaps even when thermal expansion and contraction occur due to repeated walking loads or temperature changes.

[0114] The present invention is not limited to the specific preferred embodiments described above, and anyone with ordinary knowledge in the art to which the invention pertains can make various modifications without departing from the essence of the invention as claimed in the claims, and such modifications will be within the scope of the claims.

[0115] Furthermore, the terms described in this invention are intended to distinguish one component from another and to aid in understanding the invention; therefore, the components of the invention are not limited by the described terms.

[0116] In addition, the components in each drawing may be depicted with exaggerated or simplified sizes or thicknesses for the sake of ease of understanding, but the scope of protection of the present invention should not be interpreted as being limited by this. Explanation of the symbols

[0117] 10 : Panel body 110 : Connecting part 120 : Vertical support 20 : Protective coating layer 30 : Elastic resin layer 310 : Upper surface elastic part 320 : Side elastic part 80 : Connecting clip 810: Base plate 820: Elastic connecting part

Claims

Claim 1 A panel body (10) having a connecting fitting part (110) formed along the longitudinal direction on both sides and a vertical support part (120) connecting the upper and lower parts; a protective covering layer (20) formed on the upper surface (101), lower surface (102), upper side (103a) and lower side (103b) of both sides (103) of the panel body (10), and the inner surface (110a) of the connecting fitting part (110); and an elastic resin layer (30) formed by laminating on the upper surface (101) and the upper side (103a) of both sides (103) of the panel body (10) on which the protective covering layer (20) is formed. A civil engineering anti-slip elastic panel characterized in that the elastic resin layer (30) is continuously bonded to the outer side of the protective covering layer (20) and integrated with the protective covering layer (20), and an anti-slip pattern (311) of natural wood veneer is formed on the upper surface elastic portion (310) of the elastic resin layer (30) formed on the upper surface (101) of the panel body (10). Claim 2 delete Claim 3 A civil engineering anti-slip elastic panel according to claim 1, wherein the protective coating layer (20) is formed by an aqueous resin composition comprising 60% to 70% by weight of an aqueous polyurethane-acrylic composite emulsion, 15% to 25% by weight of an aqueous epoxy resin, 1% to 5% by weight of a silane coupling agent, 1% to 6% by weight of an additive, and 5% to 15% by weight of deionized water, or a polyolefin-based resin composition comprising 65% to 80% by weight of HDPE (high density polyethylene), 5% to 15% by weight of LLDPE (linear low density polyethylene), 5% to 15% by weight of an inorganic filler, 1% to 5% by weight of a UV stabilizer, and 1% to 5% by weight of an additive including an antioxidant and a lubricating agent. Claim 4 A civil engineering anti-slip elastic panel according to claim 1, wherein the elastic resin layer (30) is formed by an elastic resin composition comprising 55% to 70% by weight of polyolefin elastomer (POE), 15% to 30% by weight of high-density polyethylene (HDPE), 2% to 6% by weight of ultraviolet stabilizer, 7% to 15% by weight of inorganic filler, and 1% to 5% by weight of additive. Claim 5 A civil engineering anti-slip elastic panel characterized in that, in claim 1, one or more concave grooves (104) are formed along the longitudinal direction on the upper surface (101) and lower surface (102) of the panel body (10), and the protective coating layer (20) and elastic resin layer (30) are formed up to the interior of the concave grooves (104), thereby improving the contact area and mechanical bonding strength with the panel body (10). Claim 6 A civil engineering anti-slip deck (C) wherein a plurality of elastic panels (A) according to any one of claims 1, 3 to 5 are sequentially arranged on a floor surface (B), and adjacent elastic panels (A) are connected so as to be in close contact with each other by one or more connecting clips (80), wherein the connecting clip (80) comprises a plate-shaped base plate (810) and an elastic coupling part (820) formed integrally with the base plate (810), and the elastic coupling part (820) comprises one or more first elastic support pieces (821) inserted into the connecting fitting part (110) of one elastic panel (A) and one or more second elastic support pieces (822) inserted into the connecting fitting part (110) of the other elastic panel (A). Claim 7 In claim 6, the first elastic support member (821) and the second elastic support member (822) are formed integrally with the base plate (810) by cutting a part of the base plate (810) and then bending it.

Citation Information

Patent Citations

  • Surface coating composition for bicycle road

    KR101336740B1

  • Clip for Upper Plate Coupling of Wood Deck

    KR101754110B1

  • Waterborne top coating composition and method for manufacturing same

    KR1020140141741A

  • Polypropylene resin composition for insulating material of power cable

    KR1020190079535A

  • Floor panel assembly clips with improved tightening

    KR102856538B1