Abstract
The present invention relates to a method for manufacturing compressed earth bricks using clay from aggregate quarries as the main component, combined with aggregates and stabilizers. The method includes homogeneous mixing of the materials, pouring them into specific molds, high-pressure compression, careful demolding and natural drying in the open air, thus eliminating any firing process. The resulting bricks have an average mechanical strength of 4.1 MPa, excellent thermal insulation with a conductivity of 0.56 W / m·K.
Need to check novelty before this filing date? Find Prior Art
Citation Information
Patent Citations
Foam concrete building block and preparation method thereof
CN108439887A
Preparation method of foamed ceramic thermal insulation decorative plate and foamed ceramic thermal insulation decorative plate
CN111732425A
High-strength siliceous refractory mortar for hot blast stove and preparation method thereof
CN114057497A