A CEMENT COMPOSITION CONSISTING ESSENTIALLY OF A)FROM 50% TO 97% BY WEIGHT (CALCULATED ON THE TOTAL COMPOSITION) OF A PORTLAND CEMENT CLINKER, THE SULFUR CONTENT OF WHICH IS IN THE RANGE OF 0.5-10% BY WEIGHT EXPRESSED AS SO3, AND THE FLUORINE CONTENT OF WHICH IS IN THE RANGE OF 0.13-1.00% BY WEIGHT EXPRESSED AS F; AND B)FROM 3% TO 50% BY WEIGHT (CALCULATED ON THE TOTAL COMPOSITION) OF AN EXTENDER CONTAINING A CARBONATE SELECTED FROM CALCIUM CARBONATE, MAGNESIUM CARBONATE AND CALCIUM MAGNESIUM CARBONATE, AND MIXTURES THEREOF, AS ITS MAIN CONSTITUENT AND HAVING A MEDIAN PARTICLE SIZE (D50) OF BELOW 14 M.THE CARBONATE-CONTAINING EXTENDER B) HAS BEEN FOUND TO PROVIDE A SURPRISINGLY HIGHER CONTRIBUTION TO THE STRENGTH DEVELOPMENT OF EXTENDED CEMENTS BASED ON THE MINERALISED CLINKER A) THAN TO EXTENDED CEMENTS BASED ON CONVENTIONAL PORTLAND CEMENTS.
Need to check novelty before this filing date? Find Prior Art