Process for the production of cellulose moulded bodies
MYPI1995000405A0Inactive Publication Date: 1995-09-01LENZING AG
View PDF 0 Cites 0 Cited by
Patent Information
- Application Number
- MYPI1995000405
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1994-03-01
- Filing Date
- 1995-02-17
- Publication Date
- 1995-09-01
- Estimated Expiration
- Not applicable · inactive patent
Abstract
THE INVENTION IS CONCERNED WITH A PROCESS FOR THE PRODUCTION OF CELLULOSE MOULDED BODIES, SAID PROCESS COMPRISING THE FOLLOWING STEPS: (A) DISSOLVING CELLULOSE IN AN AQUEOUS SOLUTION OF A TERTIARY AMINE-OXIDE, IN PARTICULAR N-METHYLMORPHOLINE-N-OXIDE (NMMO), TO PRODUCE A MOULDABLE CELLULOSE SOLUTION, (B) MOULDING SAID CELLULOSE SOLUTION AND CONDUCTING THE MOULDED CELLULOSE SOLUTION INTO AN AQUEOUS PRECIPITATION BATH, WHEREIN THE CELLULOSE IS PRECIPITATED, THUS BEING OBTAINED A MOULDED BODY AND A SPENT PRECIPITATION BATH, (C) REGENERATING SAID SPENT PRECIPITATION BATH, THUS BEING OBTAINED A REGENERATED AQUEOUS AMINE-OXIDE SOLUTION WHICH IS USED AGAIN IN STEP (A) FOR DISSOLVING CELLULOSE, CHARACTERIZED IN THAT IN STEP (A) A REGENERATED, AQUEOUS AMINE-OXIDE SOLUTION IS USED WHICH HAS A PH VALUE IN A RANGE WHOSE UPPER AND LOWER LIMITS ARE DEFINED, DEPENDING ON THE CONCENTRATION OF TERTIARY AMINE-OXIDE, BY THE EQUATION PH = -0,0015 X A2 + 0,2816 X A + F, A BEING THE CONCENTRATION OF TERTIARY AMINE-OXIDE IN SAID AQUEOUS SOLUTION, EXPRESSED IN BY WEIGHT OF SAID AQUEOUS SOLUTION, AND FULFILLING THE CONDITION 40< A < 86, PREFERABLY 70< A < 80, AND F HAVING A VALUE OF 1,00 FOR THE UPPER LIMIT AND A VALUE OF -1,80, PREFERABLY -1,00, FOR THE LOWER LIMIT. FIGURE 1
Need to check novelty before this filing date? Find Prior Art