Adhesive composition for metal foil, adhesive-applied copper foil with the adhesive composition applied and dried, and copper-clad laminate manufactured by laminating the copper foil and prepreg sheets

MYPI1995001167A0Inactive Publication Date: 1995-11-24MITSUI MINING & SMELTING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1995001167
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1994-05-24
Filing Date
1995-05-03
Publication Date
1995-11-24
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing adhesive compositions for copper-clad laminates used in printed circuit boards face issues with storage stability, leading to reduced soldering heat resistance and potential gelling, especially when using block isocyanate resins, and carboxylic acids offer limited solubility and reactivity with non-melamine resin-based adhesives.

Method used

An adhesive composition comprising 0.5 to 60 parts by weight of a high-molecular compound with carboxylic acid, 10 to 40 parts by weight of block isocyanate resin, and 5 to 50 parts by weight of epoxy resin, which improves storage stability by trapping impurities and ensuring the carboxylic acid is integrated as side chains, preventing sublimation and enhancing soldering heat resistance.

Benefits of technology

The proposed adhesive composition achieves improved storage stability and high resistance to soldering heat, preventing gelling and maintaining adhesive properties, as evident from the copper-clad laminate samples tested.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

AN ADHESIVE COMPOSITION FOR METAL FOIL CHARACTERIZED BY COMPRISING 0.5 TO 60 PARTS BY WEIGHT OF A HIGH-MOLECULAR COMPOUND WHICH CONTAINS A CARBOXYLIC ACID, 10 TO 40 PARTS BY WEIGHT OF A BLOCK ISOCYANATE RESIN, AND 5 TO 50 PARTS BY WEIGHT OF AN EPOXY RESIN. THE ADHESIVE COMPOSITION HAS AN IMPROVED STORAGE STABILITY, ALONG WITH GOOD PROPERTIES FOR THE ADHESIVE PRESENT IN PRINTED CIRCUIT BOARDS RETAINED.
Need to check novelty before this filing date? Find Prior Art

Description

ADHESIVE-APPLIED COPPER FOIL WITH THE ADHESIVECOMPOSITION APPLIED AND DRIED, AND COPPER-CLAD LAMINATE MANUFACTURED BY LAMINATINGTHE COPPER FOIL AND PREPREG SHEETSBACKGROUND OF THE INVENTIONa) Field of the InventionThis invention relates to an adhesive composition applied to the metal foil which is used for the manufacture of copper-clad laminate used to make printed circuit5boards, adhesive-applied copper foil with the adhesive composition applied and dried, and copper-clad laminate manufactured by laminating prepreg sheets and the adhesive-applied copper foil.b) Description of the Prior ArtPaper base copper-clad laminate, which is commonly used to make printed io circuit boards for commercial electric and electronic devices, is manufactured by superposing a predetermined number of prepreg sheets, prepared by impregnating paper sheets with a resin composition such as a phenolic resin and / or melamine base resin composition or a resin such as an epoxy resin, and adhesive-applied copper foil on either side or both sides of the superposed prepreg sheets and15applying heat and pressure to them.The aforementioned adhesive applied to copper foil conventionally used is poly(vinyl acetal) resin, an epoxy resin, a phenolic resin or melamine resin base adhesive. These adhesives are dissolved in an organic solvent such as toluene and methyl ethyl ketone, and used in a varnish. The adhesive varnish is applied to metal o foil such as copper foil and dried and partially cured in a heating furnace to produce adhesive-applied metal foil with no stickiness at ordinary temperatures. The widening range of use and the miniaturization of electronic circuits in recent years require higher heat resistance, water resistance and tracking resistance of the adhesive. To meet this request, the adhesive is often metamorphosed with a block isocyanate resin.• ••••••a · a ·· • ·· a ··· a a a • a · a a a a a a a a a a a a a a a a ·· kAlthough the properties of the adhesive are improved by the metamorphism of the adhesive with a block isocyanate resin, the storage stability of the adhesive substantially deteriorates, sometimes resulting in the lowered resistance to soldering heat or the occurrence of gelling. Adhesive compositions for metal foil5with an improved storage stability are disclosed in Japanese ProvisionalPublication 1992-154885 and Japanese Provisional Publication 1991-177478, which contain carboxylic acids used to improve the storage stability. With carboxylic acids, however, there are problems of the low solubility in organic solvents such as toluene and methyl ethyl ketone commonly used for preparation ° of the adhesive for metal foil and the contamination of the adhesive and metal foil in a heating furnace by sublimation in the furnace due to their being a low-molecular compound. Although carboxylic acids are known to act on melamine resin as an accelerator and may be effective for adhesive compositions which contain melamine resin, they cannot be used for adhesive compositions which do not 15 contain melamine resin because they remain unreacted in the adhesives and deteriorate the soldering heat resistance and other properties.SUMMARY OF THE INVENTIONThe object of this invention is to provide an adhesive composition for metal foil with a high storage stability which is used for the manufacture of copper-clad20laminate used to make printed circuit boards, adhesive-applied copper foil with the adhesive composition applied and dried, and copper-clad laminate manufactured by laminating the adhesive-applied copper foil and prepreg sheets «To achieve the object, this invention provides an adhesive composition for metal foil characterized by comprising 0.5 to 60 parts by weight of a high-molecular compound which contains a carboxylic acid, 10 to 40 parts by weight of a block isocyanate resin and 5 to 50 parts by weight of an epoxy resin, and characterized by preferably comprising 10 to 50 parts by weight of a high-molecular compound which contains a carboxylic acid, 15 to 30 parts by weight of a block isocyanate resin, and 15 to 40 parts by weight of an epoxy resin.30The adhesive-applied copper foil of this invention is obtained by dissolving the above adhesive composition in an organic solvent to prepare a varnish andPI 95001167 applying the varnish to the surface of copper foil and drying it.The copper-clad laminate of this invention is obtained by superposing paper prepreg sheets impregnated with a phenolic resin and the adhesive-applied copper foil on either side or both sides ofthe superposed prepreg sheets and applying heat and pressure to them.It is generally known that a block isocyanate resin is a bridging agent for poly(vinyl acetal) resin and that dissociation of a block agent is substantially accerelated by addition of basic ion. Since a block isocyanate and a high-molecular compound containing a carboxylic acid are made to be present together in the adhesive composition of this invention, the carboxylic acid in the high-molecular compound is considered to trap the impurities such as sodium ions in the resins used, thereby improving the storage stability. In addition, the carboxylic acid is contained as side chains of a polymerized resin and therefore does not sublimate in a heating furnace. Further, since the adhesive composition of this invention also contains an epoxy resin added and an epoxy resin easily bridges the molecules of the high-molecular compound containing a carboxylic acid, the high-molecular compound does not remain alone in the adhesive and hence does not cause the resistance to soldering heat and other properties to deteriorate.DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTSFor the high molecular compound containing a carboxylic acid for the composition of this invention, acrylic resin, a polyester resin, a poly(vinyl acetal) resin and acrylnoitrile-butadiana copolymer which contain a carboxyl groups such as acrylic acid, methacrylic acid and maleic acid as side branches can be used, for example. There are no limitations imposed on the amount and the molecular weight of carboxyl groups contained. These high molecular compounds containing a carboxylic acid may be used singly or in a mixture of two or more of them.For the block isocyanate resin, those obtained by blocking polyisocyanate with a phenol, an oxime or an alcohol can be used. They may be used singly or in a mixture of two or more of them.For the epoxy resin, bisphenol A epoxy resin, bisphenol F epoxy resin, novolac type epoxy resin, o-cresol novolac type epoxy resin, glycidylamine compounds ·· ···· • · · • · · · · • · · • · · ·I · · · · · · • · · · · · « • · · « such as triglycidylisocyanurate, tetrakis(glycidyloxyphenyl)ethane, epoxidized polybutadiene and N,N glycidyl aniline, and tetrahydrophthaiic acid-diglycidyl ester can be used, for example. There are no limitations imposed on the degree of polymerization as epoxy resin and the epoxy equivalent. These epoxy resins may5be used singly or in a mixture of two or more of them.The proportion of each resin ofthe adhesive composition of this invention is 0.5 to 60 parts by weight for a high molecular compound containing a carboxylic acid, 10 to 40 parts by weight for a block isocyanate resin and 5 to 50 parts by weight for an epoxy resin, and preferably 10 to 50 parts by weight for a high molecular ι o compound containing a carboxylic acid, 15 to 30 parts by weight for a block isocyanate resin and 15 to 40 parts by weight for an epoxy resin.If the amount of a high molecular compound containing a carboxylic acid is less than 0.5 parts by weight, the effect of improving the storage stability is not noticeable. If greater than 60 parts by weight, the composition is difficult to dissolve15into an adhesive varnish.If the amount of a block isocyanate resin is less than 10 parts by weight, the resistance to soldering heat of the adhesive is too low. If greater than 40 parts by weight, a long time of heating is required to dissociate the block agent when drying the adhesive, and the application process is too slow to be practical.20If the amount of an epoxy resin is less than 5 parts by weight, the resistance to soldering heat is considerably low. If greater than 50 parts by weight, the adhesive layer is too brittle, and the adhesive-applied copper foil is difficult to handle.One or more resins which do not contain carboxyl groups such as acrylic resin, a poly(vinyl acetal) resin, a polyester resin, a phenolic resin, melamine resin and5 urethane resin, additives such as a curing agent for an epoxy resin, a curing accelerator, a defoaming agent, a leveling agent and a silane coupling agent, and even an inorganic filler may be added to the composition of this invention within limits not injurious to the object of this invention. These resins and additives have effects of increasing the peeling-off strength and decreasing the cost of the adhesive.The above composition is dissolved in an organic solvent to prepare an adhesive varnish. Any organic solvent capable of dissolving every resin of the composition • · • ·· ·· · · · · • · · · · · · • · ·· ···· • ··· ··· · • · · · · • · · may be used for the solvent, but comparatively inexpensive ones such as methanol, acetone, methyl ethyl ketone and toluene are preferable.The varnish is then applied to the surface of copper foil and dried to obtain the adhesive-applied copper foil of this invention.5The adhesive-applied copper foil and a predetermined number of paper prepreg sheets impregnated with a resin such as an epoxy resin are superposed and heat and pressure are applied to them to obtain paper prepreg laminate clad with copper foil.By this invention as described above, an adhesive composition suited for use as10an adhesive for the manufacture of copper-clad laminate used for making printed circuit boards, adhesive-applied copper foil with the adhesive composition applied to the surface and dried, and copper-clad laminate manufactured by superposing paper prepreg sheets and the adhesive-applied copper foil and applying heat and pressure to them.15Hereinafter shown are some examples.[Example 1] parts by weight of a polyester resin containing carboxyl groups FINEDIC M8630 (from Dainippon Ink and Chemicals Inc., Trademark), 40 parts by weight of a poly(vinyl acetal) resin DENKA BUTYRAL #5000 (from Dankikagakukogyo,20Trademark), 20 parts by weight of a block isocyanate resin MILLIONATE MS-50 (from Nippon Polyurethane Co., Ltd., Trademark) and 30 parts by weight of an epoxy resin EPOTOHTO YDCN701 (from Tohto Kasei, Trademark) were uniformly dissolved in a mixed solvent of methyl ethyl ketone and methanol of the mixture ratio of 1 to 1 to prepare an adhesive varnish.[Example 2]An adhesive varnish was prepared in the same manner as Example 1 except that the same amount of DENKA BUTYRAL 6000AP (from Dankikagakukogyo, Trademark) (Proportion of carboxyl groups: 1.6%) was used in place of FINEDIC M-8630, a polyester resin containing carboxyl groups.·· ···· » · · • ·· · ········ · · ·· • · · · · ·· ·· · • · ··· · · · · ··· ··· · · · · · · · » · · • · · · · • · · · • · • · · [Example 3]An adhesive varnish was prepared in the same manner as Example 1 except that the same amount of acrylonitrile-butadiene copolymer Nipol 1072 (from Nippon Zeon Co., Ltd., Trademark) containing carboxyl groups was used in place of FINEDIC M-8630, a polyester resin containing carboxyl groups.[Example 4] parts by weight of DENKA BUTYRAL 6000AP (from Denkikagakukogyo, Trademark) containing 1.6% of carboxyl groups used in Example 2, 20 parts by weight of a block isocyanate resin MILLIONATE MS-50 (from Nippon ι o Polyurethane Co., LTD., Trademark), 10 parts by weight of an epoxy resin EPYCOATE 1001 (from Yukashell Epoxy, Trademark) and phenolic resin SHONOL BLS-364 (from Shows Highpolymer, Trademark) were prepared into a varnish in the same manner as Example 1.[Example 5]15An adhesive varnish was prepared in the same manner as Example 1 except that the same amount of acrylonitrile-butadiene copolymer containing carboxyl groups Hycarl 1300X8 (Ube industries Co., Ltd., Trademark) was used in place of FINEDIC M-8630, a polyester resin containing carboxyl groups used in Example 1.[Comparative Example 1]An adhesive varnish was prepared in the same manner as Example 1 except that FINEDIC M-8630, a polyester resin containing carboxyl groups used in Example 1, was not used and that the amount of DENKA BUTYRAL #5000 (from Denkikagakukogyo, Trademark) was changed to 50 parts by weight.5 [Comparative Example 2]An adhesive varnish was prepared in the same manner as Example 1 except that Nipol 1072 (from Nippon Zeon Co., Ltd., Trademark), acrylonitrile-butadiene copolymer containing carboxyl groups used in Example 3, was changed to • · ··· ·· ···· ·· · · · · • · · · · • · · · · · · • · · · · • · · · · · · • · » · » · • · · • · · · • · · 4 acrylonitrile-butadiene copolymer which does not contain carboxyl groups.[Comparative Example 3]An adhesive varnish was prepared in the same manner as Example 1 except that FINEDIC M-8630 used in Example 1 was not used, that the amount of DENKA BUTYRAL #5000 (from Denkikagakukogyo, Trademark), a poly(vinyl acetal) resin, was changed to 50 parts by weight, and that 1 parts by weight of ptoluene sulfonic acid was used.The adhesive varnishes prepared by Examples 1 to 5 and Comparative Examples 1 to 3 were applied to the roughened surface of electrolytic copper foil so that the thickness of the adhesive layer dried was 30 to 40 pm, air-dried, then dried at 130 °C for 5 minutes to obtain copper foil samples with an adhesive layer. The same adhesives were put in tightly closed containers and heat-treated at 60 °C for 3 days. After the treatment, the state of the adhesives were inspected, and adhesive-applied copper foil samples were made in the same manner as the samples above. Each of the copper foil samples with an adhesive layer and a predetermined number of paper prepreg sheets were superposed, and heated and pressed by a hot press at 150 °C with 100 kgf / cm2for one hour to make copperclad laminate samples. Then, the resistance to soldering heat of these copper-clad laminate samples were measured according to the JIS-C6481 standards. The results are shown in Table 1. The evaluation of the storage stability of the adhesive varnishes was made on whether gelling was occurred after the heat treatment and on the resistance to soldering heat of the copper-clad laminate samples.As apparent from Table 1, the adhesive composition of this invention has an improved storage stability, and the copper-clad laminate of this invention has a high resistance to soldering heat.

Claims

1. An adhesive composition for metal foil characterized by comprising 0.5 to 60 parts by weight of a high-molecular compound which contains a carboxylic acid, 10 to 40 parts by weight of a block isocyanate resin, and 5 to 50 parts by weight 5 of an epoxy resin.

2. An adhesive composition for metal foil characterized by comprising 10 to 50 parts by weight of a high-molecular compound which contains a carboxylic acid, 15 to 30 parts by weight of a block isocyanate resin, and 15 to 40 parts by weight of an epoxy resin.

103. The adhesive composition for metal foil of claim 1 or 2 wherein the highmolecular compound which contains a carboxylic acid is acrylic resin, a polyester resin, a poly(vinyl acetal) resin, acrylnoitrile-butadiene copolymer, or a mixture of two or more of them.

4. The adhesive composition for metal foil of any one of claims 1 to 3 wherein the 15 block isocyanate resin is the one Obtained by blocking a phenol, an oxime or an alcohol.

5. Adhesive-applied copper foil obtained by applying the adhesive varnish which is prepared by dissolving the adhesive composition of any one of claims 1 to 4 in an organic compound. 20 6. Copper-clad laminate made by superposing paper prepreg sheets impregnated with an appropriate resin and the adhesive-applied copper foil of claim 5 on either side or both sides of the superposed prepreg sheets and applying heat and pressure to the superposed paper prepreg sheets and adhesive-applied copper foil.