Fire resistant pipe

MYPI1996004314A0Inactive Publication Date: 1997-04-25AMERON INTERNATIONAL CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1996004314
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1996-05-06
Filing Date
1996-10-17
Publication Date
1997-04-25
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional fiber-reinforced plastic pipes and pipe fittings, made from epoxy, polyester, and phenolic resins, fail to pass rigorous fire testing due to temperature-induced deterioration, lack of impact resistance, and production of toxic smoke when exposed to flames, limiting their use in fire fighting applications.

Method used

The development of fire-resistant pipes with a structural pipe wall formed from helically wound reinforcing fibers bonded with a thermoset polymer resin, featuring a fire-resistant layer, energy-absorbing material layers, or a jacket with release layers to enhance heat resistance, impact resistance, and prevent toxic smoke production.

Benefits of technology

The solution provides pipes that are lightweight, corrosion-resistant, and capable of withstanding high temperatures and impacts without structural damage or toxic smoke production, meeting the requirements for fire fighting applications by maintaining hoop strength and preventing heat-induced degradation.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

FIRE RESISTANT PIPES AND PIPE FITTINGS INCLUDE A STRUCTURAL PIPE WALL FORMED FROM HELICALLY WOUND REINFORCING FIBER THAT IS BONDED TOGETHER WITH A THERMOSET POLYMER RESIN. FIRST EMBODIMENT PIPES INCLUDE A FIRE RESISTANT LAYER IN THE FORM OF A RESIN RICH CARRIER THAT IS APPLIED TO THE SURFACE OF THE STRUCTURAL PIPE WALL. THE RESIN USED TO IMPREGNATE THE CARRIER IS SELECTED FROM THE SAME GROUP OF RESINS USED TO FORM THE STRUCTURAL PIPE WALL. SECOND EMBODIMENT PIPES INCLUDE A NUMBER OF ENERGY ABSORBING MATERIAL LAYERS DISPOSED AROUND THE STRUCTURAL PIPE WALL, AND ARE FORMED FROM A MATERIAL CAPABLE OF ABSORBING HEAT ENERGY FROM A SURROUNDING OUTSIDE LAYER TO PRODUCE A THERMALLY INSULATING GAS THEREBETWEEN. A NUMBER OF FIBER-REINFORCED RESIN LAYERS ARE DISPOSED AROUND THE ABSORBING MATERIAL LAYERS. THIRD EMBODIMENT PIPES INCLUDE A JACKET DISPOSED AROUND THE STRUCTURAL PIPE WALL THAT IS FORMED FROM AN IMPACT ABSORBING CONFIGURATION OF ALTERNATING RELEASE LAYERS AND FIBERRETHFORCED RESIN LAYERS. FIRE RESISTANT PIPE EMBODIMENTS OF THIS INVENTION ARE CONFIGURED TO PROTECT THE STRUCTURAL WALL FROM HEAT INDUCED FAILURE PRODUCED BY EXPOSING THE OUTERMOST PIPE WALL TO A 1 ,000?C FLAME FOR AT LEAST FIVE MINUTES IN A DRY CONDITION.
Need to check novelty before this filing date? Find Prior Art

Description

FIRE RESISTANT PIPEField of the InventionThe present invention relates generally to fire resistant pipe and pipe fittings and, more particularly, to a filament wound fiber-reinforced pipe and pipe fittings having one or more surrounding fiber-reinforced resin impregnated layers, which display enhanced fire resistance, burst strength, and impact resistance when compared with conventional fiber-reinforced pipes and pipe fittings.Background of the InventionPipes and pipe fittings formed from fiber-reinforced plastics have gained widespread acceptance as viable alternatives to their steel counterparts in such applications where cost, weight, and / or chemical resistance is a concern. Conventional fiber-reinforced plastic pipes include a filament component that is wound on a mandrel, and a resin component that is used to bond the filament windings together. The filament winding acts to structurally reinforce the otherwise resin pipe by providing a desired degree of hoop and longitudinal strength to the pipe The fiber and resin components are selected for one or more desired physical properties, makiing the pipe particularly adapted to a specific application. Polyester and epoxy resins are typically favored for use in forming such pipes and pipe fittings because of their good weatherability, corrosion, and chemical resistance.Fiber-reinforced plastic pipes and pipe fittings are used in applications where some degree of temperature resistance is desired as well as weather, corrosion and chemical resistance. An example of one such application is fire fighting piping that is used in industrial plants, offshore platforms and the like. Typically, pipes and pipe fittings used in fire fighting piping must be designed to accommodate and deliver a desired pressure of water, or other fire fighting liquid, foam, or foam / liquid mixture, when subjected to high temperature conditions or when placed in close flame vicinity. Fiber-reinforced plastic pipes are favored for use as Fire fighting piping on off-shore oil platforms and are typically maintained in an empty or uncliarged state until a fire is detected. Once a fire is detected, water is routed to the pipes at pressures that can be as high as 225 psig (16 Kgf / cm ), depending on the rated pressure for the pipe. Accordingly, fiber-reinforced pipes that are used in such applications must be able to w ithstand an elevated temperature and / or close flame contact for a brief period of time when empty, i.e., without the benefit of being charged with water and having the water act as a heat transfer medium to minimize detrimental temperature effects.Fiber-reinforced plastic pipes used in such fire fighting pipe applications include those made from epoxy resin because of their enhanced corrosion resistance. A rigorous test has been devised to qualify fiber-reinforced pipes for use in such fire fighting pipe applications. The test requires placing the pipe and pipe fitting assembly in close vicinity to a 1,000°C flamewith title pipe dry for a period of five minutes, and then filling the pipe with water at a rated pressure for approximately twenty minutes. To pass the test, the pipe and pipe fittings assembly must not show any signs of structural damage and only minor leakage. Fiber-reinforced plastic pipes and pipe fittings formed from epoxy resin have been shown to display significant temperature induced deterioration at temperatures as low as 120°C and, therefore, have proven incapable of passing the test. Fiber-reinforced pipes and pipe fittings formed from polyester resin are equally incapable of passing the test, as these pipes have been demonstrated significant temperature induced deterioration at temperatures as low as 94°C.In order to pass the test, fiber-reinforced plastic pipes formed from epoxy resin can be coated with an intumescent coating, or formed from an intumescent containing epoxy resin. When exposed to high-temperature conditions or flame contact, the intumescent coating foams, forming a temperature insulating barrier that serves to protect the underlying pipe surface. However, a disadvantage of using an intumescent coating is that it increases the expense of the fiber-reinforced plastic pipe, thereby reducing the cost incentive for using the pipe, and generates toxic smoke when subjected to flame contact.An alternative for using intumescent coated fiber-reinforced epoxy pipes in fire fighting pipe applications is to construct the pipe from phenolic rather than epoxy resin, which is known to provide enhanced temperature resistance. However, fire fighting pipes and pipe fittings made from fiber-reinforced phenolic resin have also been found to be incapable of passing the test, displaying fiber rupture induced side wall failures when exposed to rated pressures.Fiber-reinforced plastic pipes formed from epoxy, polyester and phenolic resins are knov / n to display a limited amount of impact resistance and flexibility. Physical properties of impact resistance and flexibility are desired in applications such as fire fighting piping and pipe fittings because it is desired that such piping remain capable of retaining a rated water pressure even when subjected to some amount of movement, possibly created by falling, failing or distorting adjacent structures during a fire.It is, therefore, desired that fiber-reinforced resin pipe and pipe fittings be constructed that are lightweight, weatherable, corrosion resistant, chemical resistant, and have sufficient burst strength and temperature resistance to pass the above-described test for use in fire fighting pipe applications. It is desired that the fiber-reinforced resin pipe not produce toxic smoke when exposed to flame contact, and provide a desired degree of both impact resistance and flexibility. It is also desired that the fiber-reinforced resin pipe be formed from available materials using conventional manufacturing techniques.Summary of the Invention:There is, therefore, provided in the practice of this invention fire resistant pipes and pipe fittings that are constructed having sufficient temperature and flame contact resistant to permit their use in such high-temperature applications as fire fighting piping. Fire resistant pipes prepared according to principles of this invention include a structural pipe wall formed from helically wound reinforcing fiber that is bonded together with a thermoset polymer resin. The polymer resin is selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, fiiran resins, and mixtures thereof. The helically wound reinforcing fiber is wetted by the resin so that it comprises in the range of from about 10 to 40 percent by weight resin. The structural wall is formed from multiple layers of the windings, wherein the number of layers depend on such factors as the desired hoop and longitudinal strength, and temperature resistance desired for a particular pipe application.In a first embodiment, a fire resistant layer is applied to the surface of the structural pipe wall. The fire resistant layer is a resin rich layer that acts as a heat ablative shield. The fire resistant layer includes a carrier adapted to accommodate a large amount of a thermosetting polymer resin. The carrier is selected from the group of fibrous mat-like materials that include glass fiber, carbon fiber, nylon fiber, polyester fiber, similar fiber felts, chopped fibers, and combinations thereof. The resin component is selected from the same group of resins previously described for forming the structural pipe wall. It is desired that both resins be compatible, and preferably be the same, to facilitate forming a chemical bond between the structural pipe wall and the fire resistant layer during cure. The fire resistant layer comprises abouit three times the resin content of the helically wound reinforcing fiber layer.In a second embodiment, a number of energy absorbing material layers are disposed around a surface of the structural wall. The energy absorbing material used to form the layers is selected from the group of materials capable of absorbing heat energy from an outside surrounding layer by phase transformation, e.g., to produce a gas, below a degradation temperature of the structural wall. The gas formed by such phase transformation produces a thermally insulating air pocket therebetween.A number of fiber-reinforced resin layers are disposed over the energy absorbing layers. The fiber-reinforced layers can be made from the same or different fiber and resin components used to form the structural wall.In a third embodiment, a jacket is disposed around a surface of the structural wall. The jacke t is made up of alternating release layers and fiber-reinforced resin layers. The release layers are formed from a material that is incapable of forming a bond with the resin component of the surrounding fiber-reinforced resin layers and / or structural wall to form a disbondment layer therebetween. Such a disbondment layer improves the impact resistance of the pipe because it is energy absorbing to improve impact resistance and reduce thermal stress be preventing the transfer of an impact shock wave from an outside pipe surface to the structural wall.The fire resistant layer in the first embodiment, the energy absorbing material layers in the second embodiment, and the jacket in the third embodiment are each formed having a sufficient wall thickness to protect the structural wall of the pipe or pipe fitting from heat induced degradation caused by exposing the outermost pipe wall to a 1,000°C flame for at least five minutes when the pipe is in a dry condition, i.e., when the pipe is not charged with water.Fire resistant pipes and pipe fittings prepared according to principles of this invention are lightweight, weatherable, corrosion resistant, chemical resistant, and have sufficient temperature resistance to be used in fire fighting pipe applications without suffering temperature or flame contact related failure. Fire resistant pipes of this invention, when exposed to flame contact, do not produce toxic smoke and have enhanced impact resistance and flexibility when compared to conventional fiber reinforced plastic pipes formed from epoxy and polyester resin ingredients.Brief Description of the Drawings:These and other features and advantages of the present invention will become appreciated as the same becomes better understood with reference to the specification, claims, and drawings wherein:FIG. 1 is a side elevational view of a first fire resistant pipe embodiment constructed according to principles of this invention prior to application of one or more fire resistant layer(s);FIG. 2 is a side elevational view of the fire resistant pipe of FIG. 1 after application of one or more fire resistant layer(s);FIG. 3 is a cross sectional view of the fire resistant pipe of FIG. 2 taken across section3-3;FIG. 4 is a cross sectional view of a second fire resistant pipe embodiment comprising an energy absorbing material layer interposed between a structural pipe wall and an outside fiber-reinforced resin layer;FIG. 5 is a cross sectional view of an alternative second fire resistant pipe embodiment comprising successive energy absorbing material layers interposed between a structural pipe wall and an outside fiber-reinforced resin layer;FIG. 6 is a perspective view of a third fire resistant pipe embodiment comprising a jacket of repeating release layers and fiber-reinforced resin layers interposed between a structural pipe wall and an outside fiber-reinforced resin layer; andFIGS. 7A to 7C are elevational side views of fire-resistant pipe fittings constructed according to principles of this invention.Detailed Description:Referring to FIG. 1, a fire resistant pipe 10 constructed according to principles of this invention includes a structural pipe wall 12 formed from multiple layers of helically wound reinforcing fiber 14 bonded together with a resin 16. The structural pipe wall 12 can be formed by using conventional techniques well known in the art for forming fiber-reinforced plastic (FRP) pipe, such as by winding the reinforcing fiber around a mandrel at one or more specific wind angles, and in one or more directions, to obtain a particular degree of hoop and longitudinal strength. In a preferred embodiment, the fiber windings are wound under tension at an angle of approximately 54 degrees around the mandrel in one directions and then in an opposite direction, as this wind angle is known to produce a pipe having an optimum degree of both hoop and longitudinal strength. The number of fiber windings that are used to construct the structural pipe wall depends on the particular size of and application for the pipe. While the above-described technique has been directed toward the construction of pipe, it is to be understood that the same technique can be used to construct pipe fittings such as tees, elbows and the like as well.The reinforcing fiber component may be selected from conventional filament materials used for forming FRP pipe that do not melt when exposed to fire such as glass, carbon, and the Hike, and combinations thereof. In a preferred embodiment, the reinforcing fiber is glass. The structural pipe wall is constructed so that a sufficient amount of the resin component is used to wet and bond together the fiber windings. The structural pipe wall may comprise in the range of from about 10 to 40 percent by weight of the resin component. In a preferred embodiment, the structural pipe wall comprises approximately 25 percent by weight resin. The resin, is applied to the fiber windings by a conventional application technique, such as by running the windings through a resin bath.The resin component may be selected from the group of resins consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof. Any type of phenolic resin can be used as the resin component and is ultimately selected based on the desired physical properties for the intended end use application. Preferred phenolic resins suitable for use in forming the structural pipe wall include phenolic resole and phenolic novolac resins. Suitable phenolic resins can include those based on phenol, substituted phenols like para-cresol, xylenol, bisphenol A, paraphenylphenol, para-tert-butyl phenol, para-t-octyl phenol and resorcinol. The phenolic resin can be prepared by combining a suitable phenol with an aldehyde, such as formaldehyde, acetaldehyde, paraldehyde, glyoxal, hexamethylene-tetra<imine, and furfural.Preferred phenolic resins are low viscosity phenolic resole resins because of their optimal wetting of the fiber-reinforcing material and their contribution to producing a fiber-reinforced pipe having a high glass content. Preferred phenolic novolacs found most useful in this invention are prepared from any of the phenols and aldehydes previously described andhave molecular weights in the range of from about 400 to 5,000 with glass transition temperatures in the range of from about 40°C to 90°C. Phenolic resoles found most useful in this invention have molecular weights in the range of from about 300 to 3,000, solids contents from 50 to 90% by weight, and may contain from 2 to 20% by weight free phenol or substituted phenol and from 1 to 10% by weight water.Manufacturers of suitable phenolic resins include: B.P. Chemical Division of British Petroleum of Barry U.K.; the Packaging and Industrial Products Division of Borden, Inc., of Columbus, Ohio; the Durez Division of Occidental Petroleum of Dallas, Texas; Georgia-Pacific Corporation of Atlanta, Georgia; Neste Resins Corporation of Eugene, Oregon, as well as a number of other small producers. Some preferred phenolic resins include B.P. Chemical's Cellobond J1996L, J2018L and J2027L, Borden's SL-898 phenolic resole, and Georgia-Pacific's GP5018 phenolic resole.Particularly preferred siloxane-modified phenolic resins useful in forming the structural pipe wall include those prepared by combining, in a first embodiment, a silicone intermediate, a phenol or substituted phenol, and an aldehyde donor, by combining, in a second embodiment, one of the above-described phenolic novolac resins with a silicone intermediate, or by combining, in a third embodiment one of the above-described phenolic resole resins with a silicone intermediate.In a first embodiment, a siloxane-modified phenolic resin is prepared by combining phenol or a substituted phenol described above, with an aldehyde described above, and a silicone intermediate. The amount of aldehyde present and the type of catalyst used will determine whether a siloxane-modified phenolic novolac or resole resin is formed.With respect to the silicone intermediate, alkoxy-functional and silanol-functional silicone intermediates may be used. Silicone intermediates as referred to in this invention are chemical polymer structures that have an -Si-O- backbone and that are capable of undergoing further reaction, e.g., hydrolysis and / or condensation, to form a cured polymer structure, and that have a molecular weight of in the range of from about 150 to about 10,000.Another group of silicone intermediate can be represented by an hydroxyl (OH) containing silicone material, including those materials wherein the OH group or groups are attached directly to the silicon atom such as the silanol materials.Still another group of OH containing silicone materials are materials that comprise two or more OH groups attached to a silicon atom, and that have two or more silicon atoms attached through divalent organic radicals.Methoxy-functional silicone intermediates useful in this invention include, but are not limited to: DC-3074, DC-3037 from Dow Corning Corporation of Midland, Michigan; SY-231 (molecular weight approximately 1,000) and MSE-100 from Wacker Silicone Corporation; and SR-191 from General Electric. Silanol-functional silicone intermediates generally have in the range of from about 0.5% to 6% by weight Si-OH. Commercially available silanol-functionalsilicone intermediates useful in this invention include, >ut are not limited to: Diphenylsilandiol (mollecular weight approximately 216), Wacker Silicones SY-409 (molecular weight approximately 10,000) and SY-430; and the following materials from Dow Corning: DC804, DC805, DC806A, DC840, Z-6018, DC-1-2530, D< !-6-2230, DC-1-0409, DC-1-0410 and laminating resins 2103, 2104 and 2106.A preferred first embodiment of a siloxane-i lodified phenolic resin is prepared by combining phenol, or substituted phenol, an aldehyc ; such as formaldehyde, and a silicone intermediate. On the basis of a charge weight c ' one mole of phenol, the weight of formaldehyde will vary between 0.75 and 0.90 moles, and the weight of silicone intermediate will vary between 0.01 and 0.3 moles. The mola: ratio of phenol to formaldehyde in a phenolic novolac resin is typically 1:0.75-0.90.A first preferred embodiment of a siloxane-mt lified phenolic resole resin is prepared by combining phenol, or substituted phenol, an aldehj le such as formaldehyde, and a silicone intermediate. On the basis of a charge weight o one mole of phenol, the weight of formaldehyde will vary between 1.2 and 3 moles, and be weight of silicone intermediate will vary between 0.01 and 0.7 moles. The molar ratio c t phenol to formaldehyde in a phenolic resole resin is typically 1:1.2-3.For each of the above-described first embodir ents of the siloxane-modified phenolic novolac and resole resins, it is desired that in the ra ige of from about 0.5 to 35 percent by weight of the silicone intermediate be used.In preparing first embodiments of the siloxane modified phenolic resins, catalysts are used to form either a desired phenolic novolac or i lenolic resole resin prepolymer. For example, when forming the siloxane-modified pheno ic resin, a strong acid such as sulfuric acid, sulfonic acid, oxalic acid, or phosphoric acic is used to facilitate formation of the phenolic novolac resin prepolymer. When forming tie siloxane-modified phenolic resin, a strong base such as sodium hydroxide, calcium hyd oxide or barium hydroxide is used to facilitate formation of the phenolic resole prepolym :r. In preferred first embodiments, a siloxane-modified phenolic novolac resin may be pre ared by using up to about five percent by weight acid catalyst, and a siloxane-modified ph< nolic resole resin may be prepared by using; up about five percent by weight base catalyst.Catalysts other than, and in addition to, those [escribed above can optionally be used in preparing first embodiments of the siloxane- lodified phenolic resin to facilitate condensation of the phenolic resin and silicone int< rmediate by reducing the time and / or temperature associated with such reactions. Catalyst useful for facilitating condensation of the phenolic resin and silicone intermediate are th< same, and can be used in the same proportion, as those described below that can optionall be used for preparing second and third embodiments of the siloxane-modified phenolic resinFirst embodiments of the siloxane-modified phenolic novolac and resole resins are prepared by first combining the phenol and silicone : itermediate ingredients and then adding the aldehyde ingredient to form a mixture of phei olic polymers, siloxane polymers, and phenolic-siloxane polymers. Elevating the temperat re of the combined mixture is desirable to reduce reaction times associated with forming the siloxane-modified phenolic resin.For example, a first embodiment of the silox ne-modified phenolic novolac resin can be prepared by a batch process using a jacketed stai Jess-steel reaction vessel equipped with a turbine blade or anchor-type agitator, a vapor c< ndenser, and a temperature controller. Typically, molten phenol is charged to the reaction \ ;ssel, the agitator is started and silicone inteimediate is added. An acid catalyst can be added it this point to facilitate formation of the phenolic novolac polymer. Formalin (37-40 percem aqueous formaldehyde) is then charged to die reaction vessel, either before raising the tei iperature, or by controlled addition at elevated temperature. A vigorous condensation reac ion ensues which is highly exothermic. The condensation step is continued until the desired molecular weight distribution has been achieved, During this time the mixture may become t vo phases with separation of the resinous component. The actual reaction time will vary dep :nding on the desired molecular weight distribution, the use of one or more catalysts, p] I, and aldehyde to phenol to silicone inteimediate mole ratios.The ingredients are mixed together, during whi :h time the phenol, aldehyde and silicone intermediate undergo polycondensation, which polycc ndensation can optionally be accelerated by action of a catalyst, as described below. Duri tg this time, alkoxy-functional silicone intermediates also undergo hydrolysis to form silanol- functional silicone intermediates, which polymerize to form a siloxane polymer and also copo ymerize with the newly-formed phenolic novolac resin prepolymer to form a siloxane-mod: fied phenolic resin. Accordingly, the resulting resin comprises an IPN of phenolic novok : polymer and siloxane polymer, and a continuous phase formed from the phenolic polymer 1 aving one or more siloxane groups in its backbone. Hydrolysis of the alkoxy-functional si icone intermediates can optionally be accelerated by action of a catalyst, as described b slow. Alternatively, silanol-functional silicone intermediates can be used in the process which can copolymerize directly with newly-formed phenolic novolac resin prepolymer.At the end of the condensation period, water, esidual moisture, unreacted phenol and low molecular weight species may be removed by ati Lospheric, vacuum or steam distillation. The point at which distillation is stopped is usually de ermined by taking a sample of the resin and measuring its melt viscosity. After the resin has ooled, it can be treated in several ways. It can be sold in lump or flake form, compounded :o form molding powders, or it can be ground and blended with hexamine and other fillers.As another example, a first embodiment of the siloxane-modified phenolic resole resin can be prepared by a batch process using the sar le equipment previously described forpreparing a first embodiment of the siloxane-modified phenolic novolac resin. Typically, molten phenol is charged to the reaction vessel, the agitator is started and silicone intermediate is added. Alkaline catalysts may be added at this time to facilitate formation of the phenolic resole polymer. Formalin is added and the batch is heated. The initial reaction is exothermic. Condensation is usually carried out at atmospheric pressure and at temperatures in the range of from 60 to 100°C or at reflux. Because siloxane-modified phenolic resole siloxane resins are themselves thermosetting, dehydration is carried out quickly and at low temperatures so as to prevent over-reaction or gelation. The end point is found by manual determination of a specific hot-plate gel time, which decreases as resinification advances. Siloxane-modified phenolic resole resins can be refrigerated to prolong their storage stability.Second and third embodiments of a siloxane-modified phenolic novolac resin and a siloxane-modified phenolic resole resin, respectively, are prepared by using a phenolic novolac resin and phenolic resole resin, respectively, as starting materials. Suitable phenolic resole and phenolic novolac resins include those previously described above. The second embodiment of the siloxane-modified phenolic novolac resin is prepared by combining in the range of from 75 to 95 percent by weight of the phenolic novolac resin. The third embodiment of the siloxane-modified phenolic resole resin is prepared by combining in the range of from 65 to 99.5 percent by weight of the phenolic resole resin.With respect to the silicone intermediate, those silicone intermediates previously described for preparing the first embodiments of the siloxane-modified phenolic resin are also used to prepare the second and third embodiments of the siloxane-modified phenolic resins. Second and third embodiments of the siloxane-modified phenolic resins may each comprise in the range of from 0.5 to 35 percent by weight of the alkoxy-functional or silanol-functional silicone intermediate.In the second embodiment, the siloxane-modified phenolic novolac resin is prepared by combining a phenolic novolac resin with a formaldehyde donor and a silicone intermediate. Suitable formaldehyde donors include aqueous formaldehyde solutions, paraform, trioxane, hexamethylenetetraamine and the like, a preferred material is hexamethylenetetraamine. The second embodiment of the siloxane-modified phenolic novolac resin may comprise in the range of from about 3 to 15 percent by weight of the formaldehyde donor.The third embodiment of a siloxane-modified phenolic resole resin is prepared by combining a phenolic resole resin with a silicone intermediate. If desired, either an acid or base catalyst can optionally be used to reduce reaction time associated with finally curing the resin. Suitable inorganic acid catalysts that can optionally be used in the third embodiment include phosphoric, hydrochloric, and sulfuric acids. Suitable organic acids that can optionally be used in the third embodiment include paratoluene sulfonic and phenyl sulfonic acids. Latent acid catalysts can also be used in to improve pot life and to increase the application window without gel formation. Suitable base catalysts for curing phenolic resoles include variousforms of barium and magnesium oxide, and the like. Commercially available proprietary latent acid type catalysts useful in this invention are avai ible from British Petroleum Chemicals under the trade name Phencat 381 and Phencat 382. ( ther proprietary catalysts include Borden RC-901, a diphenyl phosphoric acid ester supplied frc n Dover Corp., having the product name Doverphos 231L, and Georgia-Pacific's GP3839 an GP308D50. The third embodiment of the siloxane-modified phenolic resole resin may comj rise up to about 15 percent by weight of the optional acid or base catalyst or curing agent.If desired, the first, second and third embodi aents of the siloxane-modified phenolic resins may each optionally comprise a sufficient amoi nt of catalyst to reduce the reaction time and reduce the reaction temperatures associated with ondensing the silicone intermediate and copolymerizing it with the phenolic polymer duri lg formation of the siloxane-modified phenolic resin.Suitable catalysts are selected from the group < insisting of organometallic compounds, amine compounds, and mixtures thereof. Combinati< ns of an organometallic compound with an amine compound are preferred, when desired, for < italyzing hydrolysis and / or condensation of the silicone intermediate. Useful organometalli : compounds include metal driers well known in the paint industry such as zinc, mangar :se, cobalt, iron, lead and tin octoate, neodecanates and naphthenates, and the like. Organoi tanates such as butyl titanate and the like are also useful in the current invention. Organotii compounds useful as catalysts include tetramethyltin, tetrabutyltin, tetraoctyltin, tributy in chloride, tributyltin methacrylate, dibutyltin dichloride, dibutyltin oxide, dibutyltin sulfi< e, dibutyltin acetate, dibutyltin dilaurate, dibutyltin maleate polymer, dibutyltin dilauryhr : reap tide, tin octoate, dibutyltin bis (isooctylthioglycolate), butyltin trichloride, butylstani oic acid, dioctyltin dichloride, dioctyltin oxide, dioctyltin dilaurate, dioctyltin oxide, dioctylt ri dilaurate, dioctyltin maleate polymer, dioctyltin bis (isooctylthioglycolate), dioctyltin sulfid , and dibutyltin 3-mercapto propionate. The first, second and third embodiments of the siloxa le-modified phenolic resin may comprise up to about five percent by weight of the organomet llic catalyst.With respect to the amine compound, pref rred amine compounds for optionally catalyzing the hydrolysis and / or condensation reactioi s of the silicone intermediate are tertiary amines. Suitable amine compounds useful as cat lysts include dimethyl methanolamine, ethylamino ethanol, dimethyl ethanolamine, dimethyl propanolamine, dimethyl butanolamine, dimethyl pentanolamine, dimethyl hexanolamine, m thylethyl methanolamine, methylpropyl methanolamine, methylethyl ethanolamin methylethyl propanolamine, monoisopropanolamine, methyldiethanolamine, i iethanolamine, diethanolamine, and ethanolamine. Preferred amine compounds incl ide dimethyl ethanolamine and ethyl aminoethanol. The first, second and third embodimei s of the siloxane-modified phenolic resin may comprise up to about five percent by weight of the amine catalyst.If desired, the organometallic compound and amine compound can each be used independently to form a siloxane-modified phenolic resin. However, it has been discovered that when combined, the organometallic compound and amine compound act synergistically to catalyze the curing process, thereby reducing the curing time further and / or reaction temperatures greater than that observed by using either the organometallic or amine catalyst alone. Accordingly, if desired under the circumstances, it is preferred that an organometallic compound be used in combination with an amine compound to catalyze both the formation of hydroxide by hydrolysis of the silicone intermediate, in the event that an alkoxy-functional silicone intermediate is used, and polymerization by condensation of both the alkoxy and silanol-functional silicone intermediate. An exemplary organometallic and amine compound combination is dibutyltin diacetate and ethyl aminoethanol. Dibutyltin diacetate, when combined with the amine, reacts synergistically to catalyze the curing process. Although it is believed that the synergistic effect of the organotin compound and the amine compound is mecltianistic in character, the exact mechanism is not known.A preferred ratio of organometallic compound to amine compound, when used together as the catalyst, is approximately one to one. Therefore, the first, second and third siloxane-modified phenolic resins may comprise up to about 10 percent by weight combined organometallic and amine catalyst. Accordingly, siloxane-modified phenolic resins prepared by combining an organometallic and amine catalyst, and an optional acid or base catalyst may comprise up to about 25 percent by weight catalyst. Preferred first, second and third siloxane-modified phenolic resins comprise in the range of from 5 to 25 percent by weight of the combined catalysts.Water may be present in the form of an aqueous phenolic resole or in the form of an aqueous formaldehyde. For example, the phenolic resole may comprise in the range of from 3 to 12 percent by weight water, and the formaldehyde may comprise formalin, which is approximately 37-40 percent aqueous formaldehyde. The first, second and third embodiments of the siloxane-modified phenolic resin can result in the formation of phenolic resins having very low or zero water content, which provides improved fire stability and processing characteristics. The silicone intermediate functions as a reactive diluent to give a stable product with generally low viscosity.Second and third embodiments of the siloxane-modified phenolic resin are prepared by combining in the above-described proportions a phenolic novolac or resole resin with a methoxy or silanol-functional silicone intermediate. A formaldehyde donor is added in the second embodiment. If desired, the catalyst for the phenolic resin, and the catalyst for the silicone intermediate, i.e., the organometallic compound and / or the amine compound, can optionally be added to reduce reaction and cure time and reduce reaction temperature.Fire resistant pipes having the structural pipe wall and fire resistant layer formed from siloxane-modified phenolic resins display improved physical properties of hoop strength,chemical resistance, flexibility, impact resistance, and flexural modulus when compared to pipes otherwise formed from non-modified phenolic resins, without affecting the physical projperties of heat, flame and chemical resistance inherent in the phenolic resin. Additionally, fire resistant pipes formed from such siloxane-modified phenolic resins have reduced microvoid formation and, therefore, densities closer to theoretical density when compared to conventional non-modified phenolic resins. Less microvoid formation also prevents possible water entrapment that would adversely affect the resin's temperature resistant properties due to steam generation and related resin matrix failure.Furan resins can be selected for use in forming the structural pipe wall because of their entoinced temperature resistance when compared with conventional epoxy and polyester FRP resins. Furan resins, however, display a lower degree of temperature resistance and are more expensive than either the phenolic or siloxane-modified phenolic resins.The structural pipe wall of the fire resistant pipe is constructed having one or more layers of fiber windings. For example, for an approximately two inch inside diameter pipe, rated at 225 psig for fire fighting pipe service, it is desired that the structural wall comprise in the range of from 2 to 20 layers of fiber winding, and optimally 6 to 16 layers of fiber winding. A structural pipe wall having less than about 2 layers of fiber winding will have a degree of hoop and longitudinal strength, and temperature resistance less than that desired for use in a fire fighting pipe application. A structural pipe wall constructed having more than about 20 layers of fiber winding is more than that necessary to provide a sufficient degree of hoop and longitudinal strength, and temperature resistance for use in a fire fighting pipe application and, therefore adds unnecessary weight and expense to the pipe.Referring now to FIG. 2, in a first embodiment, a fire resistant layer 18 is disposed around the outside surface of the structural pipe wall 12. The fire resistant layer 18 is generally a resin rich heat-ablative shield that is used to surround the structural pipe wall 12 and protect it from exposure to high temperature or direct flame contact. The fire resistant layer 18 comprises a carrier component 20 that is impregnated with a resin component 22. Typically, fire resistant layer 18 is wound circumferentially around the outside surface of the structural pipe wall 12 until a desired number of layers, i.e., heat shield wall thickness, is obtained. The fire resistant layer can, however, be applied by a spray application technique.FIG. 3 illustrates a first embodiment of a fire resistant pipe 10 constructed according to principles of this inyention comprising a structural wall 12 formed from multiple fiber windings 14, and multiple fire resistant layers 18. The number of fire resistant layers that are used to form the fire resistant pipe or pipe fitting varies, depending such factors as the size of the pipe, the potential temperature or flame exposure by the pipe, the type of fiber and / or resin comiponent selected to form the structural pipe wall, the type of carrier and / or resin component selected to form the fire resistant layer, and the like. Preferred embodiments of the first fire resistant pipe embodiment may include in the range of from 1 to 15 fire resistant layers,depending on the above-mentioned factors. In one example, for an approximately two inch inside diameter pipe, the fire resistant pipe comprises in the range of from 2 to 15 fire resistant layers.The fire resistant layer 18 can be wound around the structural pipe wall 12 by conventional winding techniques, such as those described above for constructing the structural pipe wall. It is desired that the fire resistant layer be wound at a sufficient tension to provide a good interface between the adjoining pipe wall and fire resistant layer surfaces. In a preferred first embodiment, the fire resistant layer 18 is applied shortly after forming the structural pipe wall, and before the resin component of the pipe wall has cured, to provide good interlayer bonding during cure between the interfacing resin components of the pipe wall and fire resistant layer. Accordingly, as described below, it is desired that the resin component of the fire resistant layer be compatible with the resin used to form the structural pipe wall.The carrier component 20 used to form the fire resistant layer 18 can be formed from any type of material capable of both accommodating a large amount of the resin component and providing a support structure for the resin in both a wet and cured state. Additionally, it is desired that the carrier be capable of supporting the resin and not crumbling or flaking away from, the structural pipe wall when subjected to high temperature or direct flame. It is desired that tthe carrier be capable of accommodating in the range of from 75 to 95 percent by weight of the resin component, or roughly three times the resin content of the fiber-reinforced windings. In a preferred first embodiment, the fire resistant layer comprises approximately 90 percent by weight resin.Suitable carrier materials include fibrous mat-like structures comprising glass fiber, carbon fiber, mixtures of polyester fiber or nylon fibers with other high-temperature fibers, similar fiber felts, chopped fibers, and the like, and combinations thereof. A preferred glass fiber containing carrier material is one manufactured by Owens Corning of Toledo, Ohio under the product name C-Veil, product code number GC 70E, which is a thin mat of randomly oriented chopped C-glass fibers that are bound together by a binder dispersion. A preferred polyester fiber containing material is one manufactured by Precision Fabrics Group of Greensboro, North Carolina under the product name Nexus, product code number 111-00005, which is formed from stretched and heat set 100 Dacron® polyester, and that does not contain any glass fibers.Although the carrier component has been described and illustrated as being a mat-like structure applied by conventional winding technique, it is to be understood that the carrier can alternatively be in the form of a spray applicable material containing chopped fibers and resin. Suitable spray applicable carriers include those capable of being loaded with the above-described amount of the resin component for spray application onto the surface of the structural pipe wall using conventional spray application techniques.The carrier component provides a fibrous reinforcement in the resin matrix of the fire resistant layer. The fibers provide mechanical strength for the resin which may be somewhat brittle. Thermal decomposition of the resin makes it brittle even when relatively impact resistant before exposure. The effect is that the fire resistant layer at most ablates in fine panicles instead of spalling in large flakes that would rapidly deplete the resin rich protective layer and expose the underlying structural wall of the pipe to thermal degradation. Surprisingly, some thermoplastic resin fibers may be used even though they would seem to be subject to significant degradation in a flame test. Such fibers work best, however, when mixed with high-temperature fibers. Glass fibers are, however, preferred for strength and temperature resistance.The resin component 22 used to impregnate the carrier component to form the fire resistant layer 18 is selected from the same group of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof described above for the resin used to form the structural pipe wall. The resin component is applied to the carrier, when embodied as a mat-like structure, by the same technique described above for applying resin to the fiber-reinforced windings. It is preferred that the resin component selected for the fire resistant layer be the same as that selected to form the underlying structural pipe wall to ensure chemical compatibility and, thereby provide a good chemical bond between interfacing structural pipe wall! and fire resistant layer surfaces during cure. Furthermore, by using the same resin, a single cure cycle is used for the entire pipe.The first fire resistant pipe embodiment may be constructed having one or more layer(s) of the same type of fire resistant material, or may be constructed having one or more layers of different types of the fire resistant material. It is desired that the resin component of each different type of fire resistant material be compatible with the resin component of the adjacent structural pipe wall or fire resistant layer surface to promote good interlayer bonding. For example, the fire resistant pipe or pipe fitting may include, moving outwardly from the surface of the pipe wall, one or more layer(s) of the C-Veil-type material, one or more layer(s) of the Nexus type material, and one or more layer(s) of the C-Veil type material, each impregnated with the same resin component as that used to form the structural pipe wall. The use of different types of fire resistant layers may be desired to reduce raw material costs, optimize temperature resistance, minimize weight, or the like. In a preferred first fire resistant pipe embodiment, the fire resistant layer is formed from alternating layers of C-glass fiber (C-Veil) and polyester material (Nexus) impregnated with a siloxane-modified phenolic resin composition.After the structural pipe wall has been formed, and the fiber resistant layer has been applied, the resin components of the first fire resistant pipe embodiment are cured simu ltaneously by exposing the pipe to a temperature in the range of from about 140 to 190°F (60 to 88°C) for a period of about 30 minutes. It is desired that the resins used to form thestructural pipe wall and the fire resistant pipe comprise sufficient catalyst to effect cure at a temperature below about 212°F (100°C). It is to be understood that the cure conditions for the pipe may vary depending on the amount and / or type of catalyst used, the type of resin selected, the number of fiber-reinforced windings, the number of fire resistant layers, and the like.The cured fire resistant layer acts as a heat ablative coating that forms a porous outer layer when exposed to conditions of high-temperature or direct flame. The porous outer layer does ablate away from the pipe but, remains intact to form a heat insulating layer that protects the underlying structural pipe wall from potentially damaging effects of such high-temperature or direct flame conditions.Referring now to FIG. 4, a second fire resistant pipe embodiment constructed according to principles of this invention includes a structural wall 24, constructed as described above for the first fire resistant pipe embodiment, and one or more layers of an energy absorbing material 26 disposed onto the surface of the structural pipe wall. The energy absorbing material used to form the layer is preferably one capable of absorbing a large degree of heat from an outside surrounding layer and using such energy, e.g., via an endothermic reaction, to effect a phase change, e.g., from solid to gas, below the degradation temperature of the structural wall. The gas formed from the layers produce a thermally insulating air gap between the outside surrounding layer and the structural pipe wall.Suitable energy absorbing materials include polymeric materials, solid hydrate or hydrite materials and the like that are capable of undergoing an endothermic phase transformation to vaporize, or liberate a gas, at a temperature below the degradation temperature of the resin selected to form the underlying structural wall, i.e., below about 300°C. Examples of preferred energy absorbing materials include polyethylene, hydrated calcium sulfate (gypsum), aluminum trihydroxide, and other hydrated or hydroxide containing compounds capable of vaporizing or producing a gas constituent below about 300°C. Polymeric materials, such as polyethylene and the like, filled with a powder component are also desired, as the combination of gsis and powder produced during vaporization produces a gas and powder layer between the outside surrounding layer and the structural pipe wall having enhanced thermal insulating properties.When polyethylene is used as the energy absorbing material to form a second fire resistant pipe embodiment, it can be wound in sheet form around the structural pipe wall 24 a number of times to form a desired number of layers or layer thickness. When polyethylene in the form of 0.15 millimeter thick sheet is used, it is desired that in the range of from 4 to 20 layers be used, thereby providing a total energy absorbing material wall thickness in the range of from about 0.6 to 3 millimeters. The polyethylene sheet is applied by the same wind ing technique described above for the structural pipe wall and fire resistant layer of the first fire resistant pipe embodiment. It is not necessary that the polyethylene layer be appliedat a specific wind angle, since it is intended to be saci ificial and not contribute to the hoop or longitudinal strength of the pipe. Where the en;rgy absorbing material is other than polyethylene, it can be applied in sheet form, in spray form, or in the form of solid half sheets configured to fit over part of the structural pipe wallLayers of fiber-reinforced resin 28 are wound around an outside surface of the energy absorbing material layer 26. The fiber-reinforced r :sin can be the same as that selected to form the structural pipe wall 24, or can be different. In a preferred second fire resistant pipe embodiment, the fiber-reinforced resin is the same, ar d is applied in the same manner, as that selected to form the structural pipe wall. The numb :r of layers of the fiber-reinforced resin that is applied depends on the particular pipe appli :ation and the degree of heat or flame resistance desired. Preferred second fire resistant pip: embodiments may include in the range of from 2 to 20 layers of the fiber-reinforced resin 21.Alternatively, a second fire resistant pipe enbodiment may comprise a number of repeating fiber-reinforced resin layers and energy absorbing material layers. For example, a fire resistant pipe can include first energy absorbing m iterial layers disposed onto the structural pipe wall, first fiber-reinforced resin layers disposed c nto an outside surface of the first energy absorbing material layers, second energy absorbing la yers disposed onto a surface of the first fiber-reinforced resin layers, and second fiber-reinfor< ed resin layers disposed onto an outside surface of the second energy absorbing material laye rs. In such an embodiment, the energy absorbing materials selected to form the first and seco id energy absorbing material layers can be the same or can be different, and can be selecte i so that an energy absorbing material having a relatively higher vaporization temperature b :low the degradation temperature of the fiber-reinforced resin layers is used to form the oute rmost energy absorbing material layer. In such an embodiment, the number of each energy at sorbing material layers can be the same as or less than that disclosed above for an embodi: nent having a single energy absorbing material layer.Referring to FIG. 5, an alternative second fir< resistant pipe embodiment can include two different types of energy absorbing material la; ers positioned adjacent one another to provide a desired degree of energy absorption and the mal insulation. For example, a number of fu st energy absorbing material layers 30, of a firs type of energy absorbing material, are disposed onto a surface of the structural pipe wall 32. A number of second energy absorbing material layers 34, of a second type of energy absorbi lg material, are disposed onto a surface of the first energy absorbing material layers. Preferal ly, the second type of energy absorbing material has a relatively higher vaporization temperatu re than the first type of energy absorbing material so that the two layers act as a sequential th ;rmal insulator to prevent harmful heat energy from reaching the structural pipe wall.A number of fiber-reinforced resin layers 36 an: wound around an outside surface of the second energy absorbing material layer. The numbei of fiber-reinforced resin layers 36 thatare used can be the same as or less than that used to form the structural pipe wall. Additionally, the type of fiber reinforcing material ar d resin used to form the fiber-reinforced resin layer 36 can be the same as or different than tl tat used to form the structural pipe wall. The: number of energy absorbing material layers u ;ed to form the first and second energy absorbing material layer can be the same as or dif ferent than that used to form the single energy absorbing material layer embodiment disclos :d above.If desired, the second alternative fire resistant pipe embodiment can be formed having more than one set of energy absorbing material laj ers to provide a desired degree of heat and / or flame protection to the structural pipe wall. F or example, the fire resistant pipe can be formed having a structural pipe wall, a first set of dil ferent energy absorbing material layers, a fu st fiber-reinforced resin layer, a second set of dil ferent energy absorbing material layers, and a second fiber-reinforced resin layer. In such em bodiment, the types of energy absorbing materials that are used to form the first set of energy ; ibsorbing material layers can be the same as or different than that used to form the second set of energy absorbing material layers.Alternatively, the first fire resistant pipe embo liment can be constructed having one or more layers of an energy absorbing material describe* I above interposed between the structural pipe wall and the fire resistant layers to provide an en lanced degree of heat or flame protection to the structural pipe wall. In such an embodiment, t le resin component used to form the heat shield can be different than the resin component usei I to form the structural pipe wall.Additionally, if desired, the first fire resista it pipe embodiment can be constructed having one or more energy absorbing layers interpose 1 between different types of fire resistant layers. Accordingly, it is to be understood within the scope of this invention that one or more energy absorbing material layers can be placed be:ween the structural pipe wall and fire resistant layers and / or between different types of fire resistant layers as desired, depending on the particular application, to provide an optimum de gree of heat and flame protection to the structural pipe wall.Referring now to FIG. 6, a third embodiment fire resistant pipe 38 constructed according to principles of this invention includes a r:lease layer 40 disposed onto an outside surface of the structural pipe wall 42, and a fiber-n inforced resin layer 44 disposed onto a surface of the release layer 40. In such third embod ment, the structural pipe wall is formed in title same manner previously described for th: first and second fire resistant pipe embodiments. In an exemplary embodiment, the third embodiment fire resistant pipe comprises a jacket 46 of alternating release layers 40 and fiber-reinforced resin layers 44 disposed around the outside surface of the structural pipe wall 42.Materials useful for forming the release layer u 0 are preferably those that neither bond with the resin used to form the adjacent structural pip; wall or with the resin used to form the fiber-reinforced resin layer. It is desired that the release layer not form a bond with an adjacent structural pipe wall or fiber-reinforced resin .vail to permit the release layer to act asa disbondment layer between the resin-containing layers. The disbonding action of the release layer serves to improve the impact of the fire resistant pipe by attenuating the travel of any shock waves through the pipe caused by contact made to the outside surface. Functioning in this manner, the release layers act to deaden or prevent potentially damaging impact shock waves from traveling completely through the pipe to the structural wall, thereby preventing possible fracture or rupture.Suitable materials for forming the release layers include films formed from polymeric materials that are chemically incompatible with the particular resin used to form the structural pipe wall and fiber-reinforced resin layers. Examples of such polymeric materials include poly olefins such as polypropylene, polyethylene and the like. A particularly preferred release layer is formed from polypropylene.It is also desired that the material selected to form the release layer be capable of absorbing heat energy applied from the pipe surface, and preferably be a material capable of absorbing a large degree of heat from an outside surrounding layer and using such energy, e.g., via an endothermic reaction, to effect a phase change, e.g., from solid to gas, below the degradation temperature of the structural wall. The gas formed from the release layer(s) acts to form a thermally insulating air gap between the adjacent fiber-reinforced resin layer, and between the fiber reinforcing layers and the structural pipe wall. The air gap allows each of the independent fiber-reinforced resin layers to act as a radiation shield to increase the thermal resistance of the pipe by requiring that radiant heat be progressively transferred through each fiber-reinforced resin layer before reaching the structural pipe wall. The multi-radiation shield function of the air gaps avoids the potentially high wall stresses in the pipe caused by the steep thermal gradient on the outside of the pipe during a fire.The materials noted above for forming the release layers are also heat absorbing and, therefore, useful in forming a release layer that is both disbonding and energy absorbing. Other suitable release layer materials include solid hydrate or hydrite materials and the like, as discussed above for forming the layers of energy absorbing materials, that are capable of undergoing an endothermic phase transformation to vaporize, or liberate a gas, at a temperature below the degradation temperature of the resin selected to form the underlying structural wall, i.e., below about 300°C. Examples of preferred energy absorbing materials include polypropylene, polyethylene, hydrated calcium sulfate (gypsum), aluminum trihydroxide, and other hydrated or hydroxide containing compounds capable of vaporizing or producing a gas constituent below about 300°C.Polymeric materials, such as polypropylene, polyethylene and the like, filled with a powder component are also desired, as the combination of gas and powder produced during vaporization produces a gas and powder layer between the outside surrounding layer and the structural pipe wall having enhanced thermal insulating properties.The number of alternating release and fiber-reinforced resin layers used to form the jacket that surrounds the structural pipe wall depends on the particular fire pipe application andthe degree of heat or flame resistance desired. In an exemplary embodiment, for a pipe havingia structural pipe wall diameter of approximately two inches (51 millimeters), a minimum jacket thickness is approximately 1 / 8 inches (3 millimeters) comprising four each alternating release and fiber-reinforced resin layers, as shown in FIG. 6. In forming pipe fittings, such as elbows, Y-connections, T-connections and the like, a minimum jacket thickness of approximately 1 / 8 inches (3 millimeters) is desired. It is to be understood that the exact number of release and fiber-reinforced resin layers that are used to make up a jacket of any designated thickness depends on the thickness of both the release layer material and the fiber-reinforcing material.When the release layer of the jacket is polypropylene tape, it is applied to the structural pipe: wall by the same winding technique described above for the structural pipe wall. Where the release layer is other than polypropylene or other material in tape form, it can be applied in sheet form, in spray form, or in the form of solid half sheets configured to fit over part of the structural pipe wall.Each fiber-reinforced resin layer is wound around an outside surface of a respective release layer. The material use to form the fiber-reinforced resin layers can be the same as that selected to form the structural pipe wall, or can be different. In a preferred embodiment, the fiber-reinforced resin layers are formed from the same materials as the structural pipe wall and is applied in the same manner as that selected to form the structural pipe wall. Like the release layers, the number of fiber-reinforced resin layers that are applied depends on the particular fire pipe application and the degree of heat or flame resistance desired.The jacket surrounding the structural pipe wall may comprise repeating release layers that are each formed from the same or different materials. For example, a fire resistant pipe may have a jacket comprising release layers the are formed from progressively more energy absorbing materials moving from the structural pipe wall to the outermost fiber-reinforced resin layer, to thereby provide a graduated degree of heat protection with the highest protection located where it is needed most, i.e., nearest the outermost surface of the pipe. In such an embodiment, it is desired that the material selected to form an outermost release layer have a relatively higher vaporization temperature than the remaining release layers that would be below the degradation temperature of the adjacent fiber-reinforced resin layers.Additionally, the jacket surrounding the structural pipe wall may comprise an outermost fiber-reinforced resin layer having, as a filament component, at least one carbon fiber winding for purposes of holding the jacket together during pipe exposure to fire temperatures that exceed the melting temperature of glass filament.Although the construction of fire resistant pipe embodiments have been specifically described and illustrated above, it is to be understood that this invention also includes the construction of fire resistant pipe fittings. Referring to FIGS. 7A to 7C, fire resistant pipefittings, such as elbows 48, tees 50, Y-shaped fittings 52, and the like are also prepared according to principles of this invention.Fire resistant pipes and pipe fittings of this invention can be used alone or combined to form a pipe assembly well suited for use in fire fighting pipe applications, such as fire fighting pipe assemblies that are used on offshore platforms and the like. Pipes and pipe fittings used in such applications must be able to function under conditions of high temperature and close flame vicinity without suffering significant reductions in hoop strength and longitudinal strength.Fire resistant pipes and pipe fittings constructed according to principles of this invention were subjected to a rigorous high-temperature to qualify for use in fire fighting piping applications. The test involved placing the pipe and / or pipe fittings approximately four inches from a 1,000°C flame with the pipe dry, i.e., with no water contained therein, for a period of approximately five minutes. After five minutes, the pipe and / or })ipe fittings were filled with water at a rated pressure of approximately 300 psig (21 Kgf / cm ) for approximately fifteen minutes while still subjected to the flame.To qualify for use in a fire fighting pipe application, the pipe and / or pipe fittings must rema in structurally sound when subjected to rated pressure and not show signs of leakage in excess of ten percent of the rated pipe flow. In order to determine the total pressure withstanding ability of pipes subjected to such extreme temperature conditions, and to better understand the mechanism for heat related failure, the pressure was increased on pipe and pipe fitting samples that showed no signs of pipe leakage or structural damage beyond the rated pressure until pipe failure.Although specific embodiments of fire resistant pipes and pipe fittings have been described and illustrated, many modifications and variations will be apparent to those skilled in the art. It is, therefore, to be understood that, within the scope of the appended claims, fire resis tant pipe and pipe fittings of this invention can be constructed other than as specifically described herein.

Claims

What is Claimed is:

1. A fire resistant pipe comprising: a structural wall comprising layers of helical resin selected from the group consisting of phenolic furam resins, and mixtures thereof; and at least one fire resistant layer overlying the layer includes a fibrous carrier component impregn consisting of phenolic resins, siloxane-modified ph thereof, and wherein the resin selected to form the resin selected to form the structural wall.

2. A fire resistant pipe as recited in claim structural wall and the fire resistant layer are the sa3. A fire resistant pipe as recited in c comprises at least 75 percent by weight resin.

4. A fire resistant pipe as recited in cla structural wall and the fire resistant layer are boti wherein the fire resistant layer comprises at least thr wound reinforcing fiber forming the structural wall5. A fire resistant pipe as recited in c absorbing material layers interposed between the st6. A fire resistant pipe comprising: a structural wall comprising layers of helical] resin selected from the group consisting of phenolic furan resins, and mixtures thereof; a number of energy absorbing material layer the energy absorbing material is selected from the absorbing energy by phase transformation at a temi of the structural wall; and a number of fiber-reinforced resin layers dispabsorbing material layers, wherein resin component used to form the structural wall. wound reinforcing fiber bonded with a :sins, siloxane-modified phenolic resins, tructural wall, wherein the fire resistant ted with a resin selected from the group nolic resins, furan resins, and mixtures re resistant layer is compatible with the wherein the resins selected to form the ie. lim 1 wherein the fire resistant layer η 1 wherein the resin used to form the siloxane-modified phenolic resins, and ; times the resin content as the helically im 1 comprising a number of energy ictural wall and the fire resistant layer. wound reinforcing fiber bonded with a sins, siloxane-modified phenolic resins, overlaying the structural wall, wherein roup consisting of materials capable of rature below a degradation temperature ied over an outside surface of the energy selected from the same group of resins -227. A fire resistant pipe as recited in claim 6 wherein the resin is a siloxane-modified phenolic resin prepared by combining: a major proportion of phenolic resole or phenolic novolac resin; a minor proportion of silicone intermediate; and a sufficient amount of catalyst to facilitate processing and effect cure.

8. A fire resistant pipe comprising; a structural wall comprising layers of helically wound reinforcing fiber bonded with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof; and a jacket disposed around the structural wall, the jacket comprising: at least one release layer of material that is chemically incompatible with the resin used to form the structural wall; and at least one fiber-reinforced resin layer disposed around a surface of the release layer.

9. The fire resistant pipe as recited in claim 8 wherein the jacket comprises a number of alternating release and fiber-reinforced resin layers.

10. The fire resistant pipe as recited in claim 8 wherein the fiber-reinforced resin layer comprises helically wound reinforcing fibers bonded with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof.

11. The fire resistant pipe as recited in claim 8 wherein the release layer is formed from a polyolefinic material.

12. A fire resistant pipe as recited in claim 8 wherein the resin used to form the structural wall and the fire resistant layer are both siloxane-modified phenolic resins.

13. A fire resistant pipe comprising: a structural wall comprising layers of helically wound reinforcing fiber bonded with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof; a jacket disposed around the structural wall, wherein the jacket comprises a number of alternating release layers and fiber-reinforced resin layers, wherein a fiber-reinforced resin layer forms an outermost pipe layer, and wherein the release layers are formed from a material -23that in incapable of forming a bond with the resin component of the structural wall and the fiber-reinforced layers.

14. The fire resistant pipe as recited in claim 13 wherein the fiber-reinforced resin layer comprises layers of helically wound reinforcing fiber bonded with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof.

15. A fire resistant pipe comprising: a structural wall comprising layers of helically wound reinforcing fiber bonded with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof; and a jacket disposed around the structural wall, the jacket comprising: at least one release layer of material that is chemically incompatible with the resin used to form the structural wall; and at least one fiber-reinforced resin layer disposed around a surface of the release layer, wherein the fiber-reinforced resin layer comprises helically wound reinforcing fiber bonded with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof, and wherein the release layer is formed from a material that is chemically incompatible with the resin used to form the fiber-reinforced resin layer.

16. A fire resistant pipe comprising: a structural wall comprising layers of helically wound reinforcing fiber bonded with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof; a jacket disposed around the structural wall, wherein the jacket comprises a number of alternating release layers and fiber-reinforced resin layers, wherein a release layer is disposed around an outside surface of the structural wall, wherein a fiber-reinforced resin layer forms an outermost pipe layer, wherein each fiber-reinforced resin layer comprises a reinforcing fiber bonded with the same resin used to form the structural wall, and wherein each release layer is fo rmed from a material that in incapable of forming a bond with the resin component of the structural wall and the fiber-reinforced layers.

17. The pipe as recited in claim 16 wherein the material used to form the release layer is selected from the group consisting of materials capable of absorbing energy by phase transformation at a temperature below a degradation temperature of the structural wall. o · -2418. A method for forming a fire resistant pipe comprising the steps of: helically winding reinforcing fiber wetted with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof, for forming a structural pipe wall; placing a fibrous carrier wetted with the same resin over the structural pipe wall, for forming a fire resistant layer; and curing the resin in both the structural pipe wall and the fire resistant layer to form a bond therebetween.

19. A method for forming a fire resistant pipe comprising the steps of: helically winding a reinforcing fiber wetted with a first resin for forming a structural pipe wall, wherein the first resin is selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof; and winding a fibrous carrier wetted with a second resin around the structural pipe wall for forming a fire resistant layer, wherein the second resin is selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof, wherein the second resin is compatible with the first resin, and wherein the carrier comprises at least 75 percent by weight of the second resin.

20. A method for forming a fire resistant pipe comprising the steps of: helically winding reinforcing fiber wetted with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof, for forming a structural pipe wall; placing a number of energy absorbing layers over the structural pipe wall, wherein the energy absorbing layers are formed from materials selected from the group consisting of materials capable of absorbing energy by phase transformation at a temperature below a degradation temperature of the structural pipe wall; and helically winding a number of fiber-reinforced resin layers over the energy absorbing layers, wherein the resin component used to form the fiber-reinforcing layers is selected from the same group of resins used to form the structural pipe wall.

21. A method for forming a fire resistant pipe comprising the steps of: helically winding reinforcing fiber wetted with a resin selected from the group consisting of phenolic resins, siloxane-modified phenolic resins, furan resins, and mixtures thereof, for forming a structural pipe wall; forming a jacket around an outside surface of the structural pipe wall by placing a release material around the outside surface of the structural pipe wall, and placing a fibero · • · -25reinforced resin layer over the release material, wherein the release material is formed from a material that is incapable of forming a bond with resins used to form both the structural pipe wall and the fiber-reinforcer resins layer; and curing the resin in both the structural pipe wall and the fiber-reinforced resin layer.