Process of hot briquetting sponge iron
MYPI1996005150A0Inactive Publication Date: 1997-06-09
View PDF 0 Cites 0 Cited by
Patent Information
- Application Number
- MYPI1996005150
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Priority Date
- 1995-12-09
- Filing Date
- 1996-12-07
- Publication Date
- 1997-06-09
- Estimated Expiration
- Not applicable · inactive patent
Abstract
THE GRANULAR SPONGE IRON IS SUPPLIED TO A ROLLER PRESS (2) AT TEMPERATURES OF 600 TO 850?C FOR MOULDING THE HOT BRIQUETS (3A). THERE IS PRODUCED A STRIP STRUCTURE (3) OF SPONGE IRON CONTAINING FORMED HOT BRIQUETS, WHICH ARE ARRANGED AT A DISTANCE FROM EACH OTHER. BY SMASHING THE STRIP STRUCTURE (3), THE HOT BRIQUETS ARE SEPARATED FROM EACH OTHER, SO THAT FRAGMENTS OF THE STRIP STRUCTURE ARE OBTAINED. THE HOT BRIQUETS (3A) AND AT LEAST PART OF THE FRAGMENTS ARE COOLED TO TEMPERATURES IN THE RANGE FROM 20 TO 400?C, AND THE COOLED BRIQUETS AND FRAGMENTS ARE PASSED THROUGH A ROTARY DRUM (12). IN THE ROTARY DRUM, FINE-GRAINED FINES OF THE BRIQUETS AND FRAGMENTS ARE PRODUCED. SUBSEQUENTLY, THESE FINES ARE SEPARATED FROM THE BRIQUETS AND FRAGMENTS, AS THEY EXHIBIT A PYROPHORIC BEHAVIOUR. (FIG.1)
Need to check novelty before this filing date? Find Prior Art