Metal surface protected against metal-dusting corrosion, which has a thermal insulating layer

MYPI1996005557A0Inactive Publication Date: 1997-10-06MG TECH AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1996005557
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1996-04-06
Filing Date
1996-12-31
Publication Date
1997-10-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Metal-dusting corrosion, caused by the decomposition of CO in hot, CO-containing gases, poses a significant threat to metal structures, particularly steels and nickel-based materials, as it leads to the formation of carbides that destroy the material's structure, and existing methods require external protective gas supplies, which are costly and inefficient.

Method used

A catalyst is introduced between the metal surface and the hotter side of a thermally insulating layer to promote reactions that reduce CO concentration, preventing the Boudouard reaction and thereby mitigating metal-dusting corrosion, using transition metals like nickel, copper, or platinum, which can be impregnated into the insulation or added to the material.

Benefits of technology

This approach effectively reduces the CO concentration locally, lowering the Boudouard temperature and preventing CO decomposition, thus protecting metal surfaces from corrosion without the need for external protective gases, even with small catalyst amounts, and is applicable to plant components exposed to high temperatures and pressures.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

THE METAL SURFACE PROTECTED AGAINST METAL-DUSTING CORROSION HAS AN INSULATING LAYER OF A GAS-PERMEABLE, THERMALLY INSULATING MATERIAL. THE SIDE OF THE THERMAL INSULATING LAYER THAT IS COLDER DURING OPERATION IS IN DIRECT VICINITY OF THE METAL SURFACE, AND THE SIDE OF THE INSULATING LAYER THAT IS HOTTER DURING OPERATION IS HEATED BY A GAS STREAM CONTAINING CARBON MONOXIDE, WHICH IN ADDITION CONTAINS HYDROGEN AND / OR STEAM AND HAS A TEMPERATURE IN THE RANGE FROM 300 TO 1700?C. IN THE REGION BETWEEN THE METAL SURFACE TO BE PROTECTED AND THE HOT SIDE OF THE INSULATING LAYER A CATALYST IS PROVIDED FOR REACTING CARBON MONOXIDE WITH HYDROGEN AND / OR STEAM.(FIGURE 1)
Need to check novelty before this filing date? Find Prior Art

Description

Metal Surface Protected Against Metal-Dusting Corrosion, Which Has a Thermal Insulating LayerThis invention relates to a metal surface protected against metal-dusting corrosion, which has an insulating layer of a gas-permeable, thermally insulating material, where the side of the thermal insulating layer that is colder during operation is in direct vicinity of the metal surface, and the side of the insulating layer that is hotter during operation is heated by a gas stream containing carbon monoxide, which additionally contains hydrogen and / or steam and has a temperature in the range from 300 to 1700°C.From DE-C-4327176 (to which corresponds US-Patent 5,490,974) it is known to protect metal surfaces against metal-dusting corrosion by introducing a largely CO-free, gaseous or vaporous protective medium into a region between the metal surface and the thermal insulating layer. The object underlying the invention is to perform the protection against metal-dusting corrosion in a simple and inexpensive way without supplying a protective gas from the outside. In accordance with the invention this is achieved in that in the region between the metal surface to be protected and the hot side of the insulating layer a catalyst is provided for reacting carbon monoxide with hydrogen and / or steam.Metal-dusting corrosion occurs under the influence of a hot, CO-containing gas when the gas cools on the metal surface, and the CO is decomposed to form C + CO2 due to the Boudouard reaction. In the metal structure, carbides are formed which lead to the destruction of the structure of the material. Metal-dusting corrosion not only attacks steels, but for instance also nickel-based materials.The intensity of the corrosive attack increases with increasing partial pressure of CO and with increasing molar ratio between CO and CO2 on the metal surface. The phenomenon of the metal-dusting corrosion has not yet been clarified scientifically in all details, but it is known that the potential for the formation of free carbon from the decomposition of CO plays an important role. This decomposition of CO takes place below the Boudouard equilibrium temperature, with this temperature limit being briefly referred to as Boudouard temperature. The Boudouard temperature increases with increasing partial pressure of CO and with increasing molar ratio between CO and CO2.In accordance with the invention, the protection of the metal surface against metal-dusting corrosion is effected by the presence of a catalyst. This catalyst is disposed on the metal surface to be protected or in the region between the metal surface and the side of the insulating layer that is hotter during operation, and in particular in the region of the cold side of the insulating layer. By means of the catalyst, at least one of the reactions A or B (A) CO + 3 H2—> CH4+ H2O (B) CO und H2O —> CO2+ H2is promoted. Due to the local reduction of the CO concentration, the Boudouard temperature is reduced in the susceptible region, so that the decomposition of CO is wholly or largely prevented.In the susceptible region, even small amounts of catalyst may be sufficient for protecting the metal surface, because usually only relatively small amounts of CO must be reacted. Usually, the thermal insulation consists of porous insulating concrete, porous bricks or a layer of ceramic fibers. Such thermal insulation can easily be provided with the required concentration of catalyst, e.g. through impregnation with a catalyst solution and subsequent drying. It is also possible to admix catalyst to the insulating concrete before the processing, or to the material for manufacturing the bricks.For promoting at least one of the above-mentioned reactions A or B, catalysts known per se may be used. These catalysts usually contain transition elements of the groups VIII, lb and IVa of the Periodic Table. In particular, one or several of the metals nickel, copper, iron, cobalt, molybdenum, tungsten, chromium, platinum, palladium, rhodium or ruthenium are suited as catalyst components.Plant components susceptible to metal-dusting corrosion are, for instance, lines or conduits through which flows synthesis gas, whose main components are CO and H2· Heat exchangers for cooling CO-containing gas, e.g. synthesis gas, must also be considered. The temperatures on the susceptible metal surface usually lie in the range from 300 to 1200°C, and the metal parts are exposed to pressures from 1 to 150 bar. The hot gas, which causes the corrosion, mostly has a CO content in the range from 2 to 80 vol-%.Embodiments for the protection against corrosion will now be explained with reference to the drawing. It represents a longitudinal section through lines carrying hot, CO-containing gas.A collecting line 1 has an outer steel shell 2, which on the inside is lined with a porous, thermal insulating layer 3. In the interior of line 1 a hot, CO-containing gas flows, as is indicated by the arrows 5.Several individual lines 8, of which only one is represented in the drawing, open into the collecting line 1. The individual lines come, for instance, from a not represented tubular furnace for cracking hydrocarbons, in order to produce raw synthesis gas having a temperature in the range from e.g. 800 to 1000°C.In the orifice portion 8a of the individual line 8 the steel shell 2 has been shaped into a bell 9, whose upper portion 9a is welded with line 8. Between the bell 9 and the outside of line 8 there is likewise provided the porous thermal insulation, which fills this area. Since in particular the inside of the bell 9 is susceptible to metal-dusting corrosion, the insulating material has dispersed therein a catalytically active metal. The content of catalyst in the thermal insulation is indicated in the drawing by cross-hatched lines 4. As is furthermore shown in the drawing, not the entire thermal insulation is provided with catalyst, but only the susceptible portion inside the bell 9 and the portion directly adjacent thereto. Of course, the thermal insulation is only provided with a catalyst at those regions, of which it is known through calculation or from experience that the metal is attacked by metal-dusting corrosion. The type and concentration of the catalyst to be used is best found out by means of experiments. It was found out that the catalyst need only be present in relatively small concentrations in the vicinity of the susceptible points, in order to achieve the required reduction of the CO concentration in the gas produced there.In an example, an arrangement corresponding to the drawing was examined. The raw synthesis gas supplied through lines 1 and 8 had a temperature of 870°C and the following composition:co2 5.0 vol-% co 9.9 vol-% H2 50.1 vol-% ch4 5.0 vol-% h20 30.0 vol-%The insulating layer 3 consisted of porous alumina, and within the area of the bell 9 it was impregnated with an agueous nickel nitrate solution. The concentration of the Ni catalyst was 30 mg Ni per cm3. The gas composition directly on the inside of the bell 9 was determined by means of probes, and it was noted that the CO content of the synthesis gas was decreased to a residual content below 1 vol-% corresponding to reactions (A) and (B). At temperatures in this range of 400 - 600°C the risk of a metal-dusting corrosion did therefore not exist. Without the catalyst, the CO concentration on the inside of the bell virtually corresponded to the composition of the synthesis gas, so that a Boudouard equilibrium temperature of 785°C is obtained. In this case, metal-dusting corrosion therefore had to be anticipated.

Claims

Claims:

1. A metal surface which is protected against metal-dusting corrosion, which has an insulating layer of gas-permeable, thermally insulating material, with that side of the thermal insulating layer (3) which is colder in operation being located in the immediate vicinity of the metal surface and that side of the insulating surface which is hotter in operation being heated by a gas stream which is at a temperature in the range from 300 to 1700°C, characterised in that a catalyst for reacting carbon monoxide with hydrogen and / or steam is located in the region between the metal surface to be protected and the hot side of the insulating layer.

2. A metal surface having a thermal insulating layer (3) according to Claim 1, characterised in that the catalyst contains one or more of the metals nickel, copper, iron, cobalt, molybdenum, tungsten, chromium, platinum, palladium, rhodium or ruthenium.

3. A metal surface having a thermal insulating layer (3) according to Claim 1 or 2, characterised in that the thermal insulating layer consists of porous insulating concrete, porous bricks or a layer of ceramic fibres.

4. A metal surface having a thermal insulating layer (3) according to one of Claims 1 to 3, characterised in that the thermal insulating layer is provided with the catalyst close to the metal surface to be protected.

5. A metal surface having a thermal insulating layer (3) according to Claim 1 or one of the following claims, characterised in that the metal surface is designed for temperatures in the range from 300 to 1200°C.