Flameproof thermoplastic resin compositions

MYPI1997000737A0Inactive Publication Date: 1998-08-26CHEIL INDUSTRIES INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1997000737
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Filing Date
1997-02-26
Publication Date
1998-08-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing flameproof thermoplastic resin compositions face issues with juicing phenomenon, surface cracking, and agglomeration due to incompatibility of styrene-containing copolymers and graft copolymers, leading to compromised heat resistance and flame retardancy, while halogen-based solutions cause mold corrosion and toxic gas release.

Method used

A halogen-free thermoplastic resin composition comprising 80-96% halogen-free polycarbonate, 4-20% core-shell type ABS resin, 5-20 parts by weight of phosphate composition, and 0.1-2.0 parts by weight of perfluoroalkane polymer, with a specific oligomeric arylphosphate formula and core-shell type ABS resin to prevent agglomeration and enhance heat resistance and flame retardancy.

Benefits of technology

The solution provides a flameproof resin with improved heat resistance, no juicing phenomenon, even particle dispersion, and enhanced flame retardancy without agglomeration, preventing toxic gas release and maintaining physical properties.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

THE PRESENT INVENTION RELATES TO FLAMEPROOF THERMOPLASTIC RESIN COMPOSITIONS COMPRISING (A) A BASE RESIN CONSISTING OF (A1) 80 TO 96% BY WEIGHT OF A THERMOPLASTIC, HALOGEN-FREE POLYCARBONATE, AND (A2) 4 TO 20% BY WEIGHT OF A CORE SHELL TYPE ABS RESIN WITH A GRAFT INDEX OF 40 OR ABOVE, WHICH IS OBTAINED BY GRAFTING 25 TO 45% BY WEIGHT OF A STYRENE AND 10 TO 15% BY WEIGHT OF AN ACRYLONITRILE ONTO 45 TO 60% BY WEIGHT OF A BUTADIENE RUBBER, (B) 5 TO 20 PARTS BY WEIGHT, PER 100 PARTS BY WEIGHT OF THE BASE RESIN (A), OF A PHOSPHATE COMPOSITION, AND (C) 0.1 TO 2.0 PARTS BY WEIGHT, PER 100 PARTS BY WEIGHT OF THE BASE RESIN (A), OF A PERFLUOROALKANE POLYMER. THE PHOSPHATE COMPOSITION IS REPRESENTED AS THE GENERAL FORMULA (I): WHEREIN R?, R?, R?, R? AND R5 INDEPENDENTLY OF ONE ANOTHER ARE C6-C20 ARYL OR ALKYL-SUBSTITUTED C8-C20 ARYL AND THE AVERAGE N OF THE PHOSPHATE COMPOSITION IS IN THE RANGE OF 0.3 TO 0.8.
Need to check novelty before this filing date? Find Prior Art

Description

FLAMEPROOF THERMOPLASTIC RESIN COMPOSITIONSField of the InventionThe present invention relates to flameproof thermoplastic resin compositions, and specifically to those for molding, comprising a base resin consisting of a halogen-free polycarbonate and a core-shell type ABS(acrylonitrile / butadiene / styrene), a phosphate composition and a perfluoroalkane polymer. The thermoplastic resin compositions of the present invention may further contain additives such as inorganic fillers, heat stabilizers, dyes, or pigments in fractions as needed.Background of the InventionA polycarbonate molding composition is widely used for parts of automobiles and electrical appliances, which has a good combination of transparency, high impact strength and heat resistance. However, the polycarbonate molding composition does not have a good processability during molding process, so other resins are used with a polycarbonate resin. For example, a molding composition comprising a polycarbonate resin and a styrenic resin has a good processability as well as a high notched impact strength.Furthermore, the polycarbonate molding composition used for housing materials of home appliances and computers should be flame resistant to prevent fires. For this purpose, halogen and / or antimony containing-compounds have been used to render flame retardency to a thermoplastic molding composition. In U.S. Patent Nos. 4,983,658 and 4,883,835, a halogen-containing compound is used as flame-retardant. The halogen-containing compound, however, results in the corrosion of the mold itself by the hydrogen halide gases released during a molding process and is fatally harmful due to the toxic gases liberated in the case of fire.- 2 U.S. Patent No. 4,692,488 discloses a thermoplastic molding composition comprising a halogen-free aromatic polycarbonate, a halogen-free thermoplastic copolymer of styrene and acrylonitrile, a halogen-free phosphorus compound, a tetrafluoroethylene polymer and graft polymers of ABS. The use of a phosphorus compound and a perfluoroalkane polymer to render flame retardency to a polycarbonate / ABS resin composition, as disclosed in U.S. Patent No. 4,692,488, prevents the dripping of flaming -particles during combustion. Though the resin composition results in satisfactory flame retardency, unsatisfactory surface crack due to the flame retardant migration during a molding process, called juicing, might occur, thus degrading the physical properties of the resin composition. In order to prevent the juicing phenomenon, an oligomeric phosphate is used in the preparation of a polycarbonate / ABS resin composition, as disclosed in U.S. Patent No. 5,204,394. U.S. Patent No. 5,204,394 discloses a polymer mixture comprising an aromatic polycarbonate, a styrene-containing copolymer and / or styrene-containing graft copolymer and an oligomeric phosphate or a blend of oligomeric phosphates as flame retardant.In the U.S. Patents mentioned above, representative examples of the phosphorus compound are triarylphosphates and oligomeric phosphates. In the process of using triarylphosphates, a juicing phenomenon occurs during a molding process because the triarylphosphates form laminae on the surface to which a strong stress is applied, and the heat resistance of the resin composition deteriorates. On the other hand, in the process of using oligomeric phosphates, a juicing phenomenon may not occur, but the appearance of molded articles is not good (i.e., the articles have color stripes). In addition, when oligomeric phosphates add to a resin with the same content as triarylphosphate, the flame retardency of oligomeric phosphates is-- 3 inferior to that of triarylphosphate.In case of using a base resin comprising a polycarbonate, a styrene-containing graft copolymer and a styrene-containing copolymer in the resin composition, the present inventors have found that the particles of the styrene-containing copolymer agglomerate with the particles of the styrene-containing graft copolymer. It is believed that the styrene-containing copolymer does not have a good compatibility with the styrene-containing graft copolymer. In the resin composition, the particles of the styrene-containing graft copolymer are not evenly distributed, thereby causing an agglomeration. This phenomenon cannot provide a resin composition with favorable physical properties, in particular, the physical properties of the resin composition deteriorate during a molding process.Accordingly, the present inventors developed a new thermoplastic resin composition with a good combination of heat resistance, no juicing phenomenon, good processability, appearance and flame retardency, by comprising a base resin consisting of a polycarbonate and a styrene-containing graft copolymer, a phosphate composition and a perfluoroalkane polymer, and filed a patent application (Korean Patent Application No. 95-4542: Corresponding U.S. Serial No. 08 / 449,521).The present inventors also developed another new thermoplastic resin composition comprising a base resin consisting of a polycarbonate and a styrene-containing graft copolymer, a phosphate composition, and a perfluoroalkane polymer. The styrene-containing graft copolymer is obtained by grafting methyl methacrylate, butyl acrylate and styrene onto butadiene rubber. The new thermoplastic resin composition was filed as a Korean Patent Application No. 95-24618.For the same purposes as in the above Korean Patent Applications, the present inventors have further developed a new resin- 4 composition comprising a base resin consisting of a halogen- free polycarbonate and a core-shell type ABS(acrylonitrile / butadiene / styrene) resin, a phosphate composition and a perfluoro alkane polymer.Objects of the InventionAn object of the, present invention is to provide a flameproof thermoplastic resin composition with -a good combination of heat resistance, no juicing phenomenon, processability, appearance, and flame retardancy which comprises a base resin consisting of a halogen-free polycarbonate and a core-shell type ABS resin, a phosphate composition, and a perfluoroalkane polymer.Another object of the invention is to provide a flameproof thermoplastic resin composition whose particles are evenly dispersed without causing agglomeration with the change of processing conditions, which comprises a base resin consisting of a halogen-free polycarbonate and a core-shell type ABS resin, a phosphate composition and a perfluoroalkane polymer.A further object of the present invention is to provide a flameproof thermoplastic resin composition whose molded articles have a good impact strength independently of thickness of the articles.Summary of the InventionThe present invention relates to flameproof thermoplastic resin compositions comprising (A) a base resin consisting of (1) 80 to 96 % by weight of a thermoplastic, halogen-free polycarbonate, and (2) 4 to 20 % by weight of a core-shell type ABS resin with a graft index of 40 or above, which is obtained by grafting 25 to 45 % by weight of a styrene and 10 to 15 % by weight of an acrylonitrile onto 45 to 60 % by weight of a butadiene rubber, (B) 5 to 20 parts by weight, per 100- 5 parts by weight of the base resin(A), of a phosphate composition, and (C) 0.1 to 2.0 parts by weight, per 100 parts by weight of the base resin(A), of a perfluoroalkane polymer. The oligomeric arylphosphate is represented as the general formula (I):IIIIRi~0 — P-O-(R3-O- P —O)n—R5I I(I)O0IIR2R4 wherein Ri, R2, R3, R4 and R5 independently of one another are Ce-Czo aryl or alkyl-substituted C6-C20 aryl and the average n of the phosphorus compound is in the range of 0.3 to 0.8.Brief Description of the DrawingsThe photomicrographs depicted in Figs. 1-6 were taken for the 1 / 4 specimens.Fig. 1 represents a transmission electron microphotograph of a resin composition of Example 1 according to this invention.Fig. 2 represents a transmission electron microphotograph of a resin composition of Example 2 according to this invention.Fig. 3 represents a transmission electron microphotograph of a resin composition of Comparative Example 1 according to this invention.Fig. 4 represents a transmission electron microphotograph of a resin composition of Comparative Example 2 according to this invention.Fig. 5 represents a transmission electron microphotograph of a resin composition of Comparative Example 3 according to this- 6 invention.Fig. 6 represents a transmission electron microphotograph of a resin composition of Comparative Example 4 according to this invention.Detailed Description of the InventionThe flameproof thermoplastic resin compositions according to the invention comprise a base resin(A), a phosphate composition(B) and a perfluoroalkane polymer(C). The detailed descriptions of each component are as follows.(A) Base ResinThe base resin used in this invention is a blend of a thermoplastic, halogen-free polycarbonate and a core-shell type ABS resin. More particularly, the base resin consists of 80 to 96 % by weight of a thermoplastic, halogen-free polycarbonate and 4 to 20 % by weight of a core-shell type ABS resin.According to substituted groups of the polycarbonate, there are aromatic polycarbonates, aliphatic polycarbonates, and aromatic / aliphatic polycarbonates, and a polycarbonate or a blend of the polycarbonates may be used in this invention. Aromatic polycarbonates are preferable, and aromatic polycarbonates synthesized from 2, 2'-bis(4-hydroxylphenyl)propane, called Bisphenol A, are preferred.There are two types of a styrene-containing graft copolymer, a hemisphere type copolymer and a core-shell type copolymer, depending on the shell structure of the copolymer. In this invention, the present inventors have discovered that the resin composition containing a core-shell type ABS resin has superior properties to the resin composition containing a hemisphere type ABS resin in heat stability, juicing phenomenon, processability, appearance, flame retardancy, and- 7 agglomeration of particles.In a process for preparing a hemisphere type or core-shell type styrene-containing graft copolymer including an ABS, a conventional polymerization process may be employed by an ordinary skilled person in the art. An emulsion polymerization process may be preferably employed to prepare a core-shell type ABS resin in this invention.The core-shell type ABS resin is obtained by grafting 25 to _45 % by weight of a styrene and 10 to 15 % by weight of an acrylonitrile onto 45 to 60 % by weight of a butadiene rubber. In this invention, it is preferable that the core-shell type ABS resin has a graft index of 40 or above, and a gel content of 70 % by weight or above, when the ABS resin is dissolved in acetone. In order to avoid agglomeration of particles, the base resin of the present invention should not contain a SAN (styrene / acrylonitrile) resin.The base resin of the invention consists of 80 to 96 % by weight of a thermoplastic, halogen-free polycarbonate and 4 to 20 % by weight of a core-shell type ABS resin. If the amount of the polycarbonate is less than 80 % by weight, the resin composition has a poor flame-retardency. On the other hand, if the amount of the polycarbonate is in excess of 96 % by weight, the resin composition has a poor impact strength.(B) Phosphate CompositionThe phosphate composition used in this invention is represented as the general formula (I):IIIIRi~0 — P —0 —(R3—0 — P —O)n—R5I I(i) r2r4- 8 wherein Ri, R2, R3, R4 and Rs independently of one another are Cs-Czo aryl or alkyl-substituted C6-C20 aryl and n is 0 to 5.The average n of the phosphate composition should be in the range of 0.3 to 0.8. Thus, the phosphate composition is a blend of the phosphates represented by the general formula(I), wherein n is 0, 1, 2, 3, 4 or 5. Where n is 0, the phosphate compositions are monomeric triarylphosphate, and where n is 1, 2, 3, 4 or 5, the phosphate compositions are oligomeric triarylphosphates.The monomeric triarylphosphates are phosphates where n is 0 in the general formula (I). The examples of the triarylphosphates are triphenylphosphate, tri(2,6-dimethylphenyl)phosphate, tri(4-methyl~phenyl)phosphate, tricresylphosphate, diphenyl 2-ethylcresylphosphate, diphenylcresylphosphate, tri(isopropylphenyl)phosphate, trixylenylphosphate, xylenyldiphenylphosphate, etc.When only monomeric triarylphosphates with n=0 are only used in a resin composition, a juicing problem might appear during a molding processes, because the monomeric triarylphosphates are volatile at about 200 °C or above. If a blend of phosphates with the average n of 1.2 or above is used in a resin composition, a juicing problem can be improved, but the flame retardency and physical properties deteriorate. The phosphates with an average n from 0.3 to 0.8 may be preferably used in this invention so as to improve the physical properties as well as flame retardency of the resin compositions.For the phosphate compositions to have an average n from 0.3 to 0.8, the phosphate compositions consist of 30 to 60 % by weight of monomeric triarylphosphates and 40 to 70 % by weight of triarylphosphates.Synthetic oligomeric triarylphosphates which may also be used in this invention, in which the average n of the synthetic oligomeric- 9 triarylphosphate is 0.3 to 0.8. Synthetic oligomeric triarylphosphates are prepared by adding phenol, resorcinol and dichloromagnesium to benzene, heating the solution, and dropping trichlorophosphinoxide in the solution. The synthetic oligomeric triarylphosphate with the average n of 0.3 to 0.8 is extracted from the resultant solution. The phosphate composition is used in an amount of 5 to 20 parts by weight per 100 parts by weight of the base resin.(C) Perfluoro alkane PolymerThe flameproof thermoplastic resin compositions according to the present invention include a perfluoroalkane polymer. Examples of the perfluoroalkane polymers are polytetrafluoroethylene, polyvinylidene fluoride, copolymer of polytetrafluoroethylene and polyvinylidene fluoride, copolymer of tetrafluoroethylene and fluoroalkylvinylether, and copolymer of tetrafluoroethylene and hexafluoropropylene. At least one of the perfluoroalkane polymers may be used in the flameproof thermoplastic resin compositions. The perfluoroalkane polymer decreases the melting flow of the flameproof thermoplastic resin during combustion by forming a fibrillar network in the resin and increases the shrinkage of the resin, thereby preventing the dripping of the melting resin during combustion. The perfluoroalkane polymer may be preferably used in a form of powder so as to disperse and blend evenly in a flameproof thermoplastic resin composition. Polytetrafluoroethylene with a particle size of 20 to 500 μ is conventionally available for this invention. 0.1 to 2.0 parts by weight of a perfluoroalkane polymer per 100 parts by weight of the base resin is blended.The flameproof thermoplastic resin compositions may further include additives such as inorganic fillers, heat stabilizers, oxidation inhibitors, light stabilizers, pigments and / or dyes depending on specific- 10 applications. The examples of the inorganic fillers are asbestos, glass fiber, talc or ceramic. The other additives are conventionally available to a skilled person in this technical field. The additives may be blended in a resin composition with an amount up to 30 parts by weight per 100 parts by weight of the base resin.The flameproof thermoplastic resin compositions are prepared by . blending a base resin, a phosphate composition and a perfluoroalkane polymer with a conventional mixer. An additive may be included in the blend. The flameproof thermoplastic resin compositions are prepared in a form of pellet by extruding the blend with a conventional extruder.The flameproof thermoplastic resin compositions have effects that the compositions prevent toxic gases during combustion, and have a good combination of heat resistance, no juicing phenomenon, processability, appearance, flame retardency and good agglomeration properties.According to transmission electron microphotographs, the resin compositions of the present invention show even dispersion of particles without causing agglomeration.The invention may be better understood by reference to the following examples which are intended for the purpose of illustration and are not to be construed as in any way limiting the scope of the present invention, which is defined in the claims appended hereto.EXAMPLESThe components to prepare flameproof thermoplastic resin compositions in Examples 1-3 and Comparative Examples 1-4 are as follow:(A) Base Resin- 11 (ai) Polycarbonate: L-1225L Grade of Teijin, Inc. of Japan was used.(a2) Core-shell Type ABS Resin parts by weight of butadiene latex powder, 12 parts by weight of styrene, 4 parts by weight of acrylonitrile, and 150 parts by weight of deionized water were blended, and 1.0 parts by weight of rosin soap, 0.2 parts by weight of tetrasodium pyrophosphate, 0.4 parts by weight of glucose, 0.006 parts by weight of ferrous sulfate, 0.25 parts by weight of cumenhydroperoxide and 0.2 parts by weight of tertiarydodecylmercaptan were added to the blended solution. The resultant solution was kept at 75 °C for 1 hour. 26 parts by weight of styrene, 8 parts by weight of acrylonitile, 0.25 parts by weight of peroxide and 0.2 parts by weight of tertiarydodecylmercaptan were added to the blended solution over 3 hours to prepare core-shell type ABS graft polymer. 1 % H2SO4 to the core-shell type ABS graft polymer latex to yield a core-shell type ABS resin in powder form.(as) Hemisphere Type ABS Resin parts by weight of butadiene latex in powder, 36 parts by weight of styrene, 14 parts by weight of acrylonitrile, and 150 parts by weight of deionized water were blended, and 1.0 parts by weight of potassium oleate, 0.4 parts by weight of cumenhydroperoxide and 0.3 parts by weight of a grafting reagent were added to the blended solution. The resultant solution was kept at 75 °C for 5 hours to prepare styrene-containing graft copolymer. To the styrene-containing graft copolymer 0.3 parts by weight of H2SO4 was added to prepare hemisphere type ABS resin in powder form.(a4) SAN Copolymer parts by weight of styrene, 30 parts by weight of acrylonitrile and 120 parts by weight of deionized water were blended, and 0.2 parts by weight of azobisisobutylonitrile and 0.5 parts by- 12 weight of tricalciumphosphate were added to the blended solution. Styrene-containing copolymer was prepared by suspension polymerization by washing, dehydrating and drying the resultant. Styrene-containing copolymer in powder form was obtained.(B) Phosphate CompositionTriphenylphosphate(n=0): a triphenylphosphate of Daihachi Co., of Japan- was used.Oligomeric phosphate(n=1.4): CR-733S of Daihachi Co., of Japan was used.Synthetic oligomeric phosphate: 114.7 g of phenol, 220 g of resorcinol and 0.2 g of dichloromagnesium were added to 100 m£ of benzene. The solution was heated to 70 °C. 82.8 g of trichlorophosphinoxide was dropped in the solution over 2 hours at the temperature of 70 °C. The resultant solution was stirred at 120 °C over 3 hours not to release hydrogen chloride gas any more. The solvent and impurities were extracted from the solution so as to prepare synthetic oligomeric phosphate in liquid at room temperature with a melting point of -10 °C and with n of 0.6 in the general formula (I).(C) Perfluoroalkane PolymerTeflon (trademark) 7AJ of Dupont, Inc. of U.S.A, was used.Examples 1-2 and Comparative Examples 1-6The compositions of each component used in Examples 1-2 and Comparative Examples 1-6 are shown in Table 1. Neither a hemisphere type ABS nor a SAN was used in Examples 1-2, but a hemisphere type ABS only was used in Comparative Examples 1-2, and both a hemisphere type ABS and a SAN were used inComparative Examples 3-6.In the Examples and Comparative Examples, the flameproof thermoplastic resin compositions were extruded in a form of pellet. And the resin pellets were molded into test specimens.TABLE 1-—_________ Examples Comparative Examples 1 2 1 2 3 4 5 6 (A) (ai )polycarbonate 90 90 90 90 90 90 90 90 (ajjcore-shel1 type ABS 10 10 - - - - - - (aajhemisphere type ABS - - 10 10 6 6 6 6 (a«)SAN copolymer - - - 4 4 4 4 (B) triphenylphosphate(n=0) - - - - - - 9 9 oligomeric phosphate!n=l. 4) - - - - 9 9 - oligomeric phosphate(n=0. 6) 9 9 9 9 - - - - (c) perfluoroalkane polymer 0.7 0.7 0.7 0.7 0.7 0.7 0.7 0.7 Molding Temperature! °C) 240 270 240 270 240 270 240 270All numerals except the molding temperatures are in grams.For the test specimens according to the Examples and Comparative Examples, flame retardency, impact strength, and heat resistance were measured, and juicing phenomenon and agglomeration were observed. The test results are shown in Table 2. Fig. 1-6 represent transmission electron microphotographs of resin compositions of Examples 1-2 and Comparative Examples 1-4. Examples 1-2 do not show agglomeration of the particles of the resin composition. Comparative Examples 3-4 show agglomeration. It is believed that the ABS resin agglomerates with the SAN resin. Comparative Example 1 shows even distribution not agglomerating grafted rubber particles, but Comparative Example 2 shows agglomeration of the rubber particles. It is believed that the agglomeration depends on the conditions of a molding process, for example, molding temperature. In this application, transmission electron microphotographs for Comparative Examples 5-6- 14 are not attached. However, it appeared that the agglomeration for Comparative Examples 5-6 depended on the thickness of a molded article and the molding condition.TABLE 2Examples Comparative Examples 1 2 1 2 3 4 5 6 UL.94(1 / 16 )1 V-0 V-0 V-0 V-0 V-l V-l V-0 V-0 Impact Strength(l / 4 )2 33 34 34 16 12 11 36 19 Impact Strength(l / 8 )2 62 60 60 55 47 19 62 54 Heat Stability(VST)3 105 - 104 - 108 - 102 - 4 Juicing X X X X X X o o Agglomeration5 X Fig.l X Fig. 2 X Fig. 3 Δ Fig. 4 Δ Fig. 5 O Fig.6 X ΔNotes) 1: UL94(1 / 16) was tested according to UL 94 VB.2·’ Impact strength (kgf · cm / cm) was tested according toASTM D256.3·’ Heat stability was tested according to ASTM D306,4: Juicing was observed with an optical microscope, after the specimens were kept at 80 °C for 24 hours.(x: Juicing was not observed, O·’ Juicing was observed,Δ: Juicing was observed depending on the molding condition) 5: Agglomeration was observed with a transmission electron microscope, (x: Agglomeration was not observed, O:Agglomeration was observed, Δ: Agglomeration was observed depending on the molding condition and thickness of an molded article)

Claims

1. A flameproof thermoplastic resin composition consisting of: (A) a base resin consisting of (1) 80 to 96% by weight of a thermoplastic, halogenfree polycarbonate, and (2) 20 to 4% by weight of a core-shell acryionitriie / butadiene / styrene graft copolymer having a graft index of at least 40, wherein said acrylonitrile / butadiene / styrene graft copolymer is made by grafting 25 to 45% by weight of a styrene and 10 to 15% by weight of an acrylonitrile onto 45 to 60% by weight of a butadiene rubber; (6) 5 to 20 parts by weight, per 100 parts oy weight of tne case resin (A), of a phosphate composition consisting of 30 to 60% by weight of monomeric triaylphosphates and 70 to 40% by weight of oligomeric triarylphosphates of the general formula: oo IIII R1—Ο—P—O—(Rj—Ο—P—O)„—Rs OO II RjR< wherein R<, R2, Ra, R4 and R5 independently of one anotner are Ce-C2o aryl or alkyl-substituted C6-C2o aryl, and n is 0 to 5, and wherein the average n of the phospate composition is about 0.3 to 0.8; and (c)0.1 to 2.0 parts by weight, per 100 parts by weight of the base resin (A), of a perfiuoroalkane polymer.

2. The thermoplastic resin composition of claim 1 wherein said perfluoroalkane polymer is selected from the group consisting of polytetrafluoroethylene, polyvinylidenefluoride, copoiymer of tetrafluoroethylene and vinyiidenefluoride, copolymer of tetrafluoroethylene and fluoroalkylvinylether, and copolymer of tetrafluoroethylene and hexafluoropropoylene.

3. A flameproof thermoplastic resin composition consisting of: (a) a base resin consisting of (1) 80 to 9.6% by weight of a thermoplastic, halogen-free polyccarbonate, and (2) 20 to4% by weight of a core-shell acrylonitriie / butadiene / styrene graft copolymer having a graft index of at least 40,5 wherein said acrylonithie / butadiene / styrene graft copolymer is made by grafting 25 to 45% by weight of a styrene and 10 to 15% by weight of an acrylonitrile onto 45 to 60% by weight of a butadiene rubber; (b) 5 to 20 parts by weight, per 100 parts by weight of the base resin (A), of a phosphate composition consisting of 30 to 60% by weight of monomeric 10 triarylphosphates and 70 to 40% by weight of oligomeric triarylphosphates of the general formula: O0 IIII Ri—Ο — P — O-(Rj —O-P-O)„ — Rj OO II R:R. wherein R1( R2, R3, R4 and R5 independently of one another are Ce-C2o aryl or aikyi-substituted Cfl-C20 aryi, and n is 0 to 5, and wherein the average n of the phosphate composition is about 0.3 to 0.8; 15 (c) 0.1 to 2.0 parts by weight, per 100 parts by weight of the base resin (A), of a perfluoroaikane polymer; and (d) an additive selected from the group consisting of inorganic fillers, heat stabilizers, oxidation inhibitors, light stabilizers, pigments, dyes, and combinations thereof.