Temporary attachment adhesive tape for multilayer ceramic capacitor and method for producing multilayer ceramic capacitor
Patent Information
- Application Number
- MYPI1997001054
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1996-03-15
- Filing Date
- 1997-03-13
- Publication Date
- 1997-09-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing adhesive tapes used in the production of multilayer ceramic capacitors suffer from reduced adhesive strength during cutting due to thermal expansion, leading to lifting and movement of green sheets, and contamination that results in voids or cracks during the baking process, affecting the reliability and yield of the products.
A temporary attachment adhesive tape with a substrate film and an adhesive layer formed from a polymer composition that exhibits a first-order melting transition over a narrow temperature range, allowing for adjustable adhesive strength and easy removal by cooling, preventing contamination and ensuring reliable peeling of the green sheets.
The adhesive tape maintains sufficient strength during the cutting process and allows for residue-free removal of the green sheets, enhancing the reliability and production yield of multilayer ceramic capacitors by adjusting adhesive strength through temperature changes.
Abstract
Description
TEMPORARY ATTACHMENT ADHESIVE TAPE FOR MULTILAYER CERAMIC CAPACITOR AND METHOD FOR PRODUCING MULTILAYER CERAMIC CAPACITORABSTRACT OF THE DISCLOSUREA temporary attachment adhesive tape for a multilayer ceramic capacitor includes a substrate film and an adhesive layer provided on one face or both faces of the substrate film. The adhesive layer is formed of a polymer composition containing a polymer having a first-order melting transition which occurs over a temperature range narrower than about 15 °C. The polymer is a side-chain crystallizable polymer. The side-chain crystallizable polymer is present in the polymer composition in an amount effective to render the polymer composition substantially nontacky at room temperature or lower and tacky at temperatures above room temperature.The side-chain crystallizable polymer is a polymer mainly composed of acrylate and / or methacrylate having a linear alkyl group of 10 or more carbon atoms as a side-chain.-1TEMPORARY ATTACHMENT ADHESIVE TAPE F0R7MULTILAYER CERAMIC CAPACITOR AND METHOD FOR PRODUCING MULTILAYER CERAMIC CAPACITOR.BACKGROUND OF THE INVENTION1. FIELD OF THE INVENTION:The present invention relates to an adhesive tape. In particular, the present invention relates to a temporary attachment adhesive tape used in a process of cutting a multilayer of green sheets into a plurality of chips in the production of a multilayer ceramic capaci10 tor.2. DESCRIPTION OF THE RELATED ARTIn general, a multilayer ceramic capacitor is 15 produced in the following processes: A slurry of ceramic powder is applied onto a carrier tape with a thin thickness using a doctor blade to form a green sheet of ceramic. A plurality of electrodes are printed on the surface of the green sheet. Next, a plurality of green sheets where the electrodes are printed are integrated into a multilayer to form a multilayer of the green sheets. The multilayer which lies along an x-plane is cut in x and y directions to form a plurality of green chips of the ceramic multilayer. The green chips are baked. Thereafter, an external electrode is formed at the end of the obtained chip. The thus obtained chip(s) are also known in the art as works.In the process of forming the multilayer of the green sheets and the process of cutting the multilayer into green chips, the green sheet is temporarily fixed onto a table for sheet fixation using an adhesive tape. Then, after the cutting process, works are peeled from-2 the surface of the table. As the adhesive tape, a tape having a thermal expansion type adhesive layer, as disclosed in Japanese Patent Publication No. 6-79812, is currently used. The adhesive layer of this adhesive tape contains a foaming gent. Thus, when the green chips are cut out and then heated, a contact area between the adhesive layer surface and the work is reduced because the adhesive layer is expanded. As a result, the work is readily released from the adhesive tape surface.However, since this adhesive tape is of the thermal expansion type, gases generated by heating of the adhesive layer contaminated the work. Therefore, when the contaminated work is baked, voids or cracks are generated, thus adversely affecting the reliability and production yield of products.Furthermore, cutting of the green sheet is generally performed in a warmed state to a predetermined temperature in order to prevent the green sheet from cracking by the insertion of a cutter. However, since the adhesive tape is of the thermal expansion type, it is likely that the adhesive layer of the adhesive tape is expanded at such a temperature at the time of cutting the green sheet. Therefore, since the adhesive strength of the adhesive layer deteriorates, works cut out by the operation of the cutter may peel from the adhesive layer, resulting in lifting. Moreover, the work may disadvantageously move to an uncut green sheet.SUMMARY OF THE INVENTIONA temporary adhesive tape for producing a multilayer ceramic capacitor of the present invention includes a substrate film and an adhesive layer provided on one face or both faces of the substrate film. The adhesive layer is formed of a polymer composition containing a polymer having a first-order melting transition which occurs over a temperature range narrower than 15°C.The polymer is a side-chain crystallizable polymer, the side-chain crystallizable polymer being a copolymer composed of 60 to 90 parts weight of stearylacrylate, 10 to 30 parts by weight of methylacrylate and 2 to 10 parts by weight of acrylic acid.According to another aspect of the invention, a temporary attachment adhesive tape for producing a multilayer ceramic capacitor includes a substrate film and an adhesive layer provided on one face or both faces of a substrate film.The adhesive tape layer is formed of polymer composition containing a polymer having first-order melt transition which occurs over a temperature range narrower than 15°C.The polymer is a side-chain crystallizable polymer, the side chain crystallizable polymer being a copolymer composed of 20 to 40 parts by weight of dococylacrylate, 60 to 80 parts by weight of hexadecylacrylate and 2 to 10 parts by weight of acrylic acid.In stacking green ceramic sheets provided with printed electrodes on a table, the green sheets are ft temporarily fixed onto the table using the adhesive tape. Then, maintaining this state, the multilayer of the green sheets is subjected to heat-application and cutting. Thereafter, in order to release works from the table, the adhesive tape is subjected to natural cooling or forced cooling to a predetermined temperature or less so that the works can be readily peeled off from the adhesive tape.Thus, the adhesive strength of the temporary attachment adhesive tape to the multilayer made of ceramic can be adjusted simply by changing the temperature of the temporary attachment adhesive tape. Thus, the adhesive strength of the adhesive tape can be large during a period of temporary attachment to the multilayer. On the other hand, the adhesive tape can be readily peeled at the time of removing the work, simply by cooling the adhesive tape. Furthermore, since the work is not contaminated, the reliability of the multilayer capacitor can be enhanced.Thus, the invention described herein makes possible the advantages of (1) providing a temporary attachment adhesive tape for a multilayer ceramic capacitor having an adhesive strength sufficient to prevent lifting or movement of works from occurring at a temperature during the process of cutting green sheets and the previous processes, and capable of releasing the works without leaving residues on the works by cooling to a predetermined temperature; and (2) providing a method for producing a multilayer ceramic capacitor using such an adhesive tape.These and other advantages of the present invention will become apparent to those skilled in the art upon reading and understanding the following detailed description with reference to the accompanying figures.BRIEF DESCRIPTION OF THE DRAWINGSFigures 1A to IG are views illustrating a production process of a multilayer ceramic capacitor according to the present invention.DESCRIPTION OF THE PREFERRED EMBODIMENTSExamples of a substrate film used in the present invention include a single layer of a synthetic resin film such as a polypropylene film, a polyester film, a polyamide film, a polycarbonate film, an ethylene vinyl acetate copolymer film, an ethylene ethyl acrylate copolymer film, an ethylene polypropylene copolymer film, a polyvinyl chloride film, or a multilayer thereof. The thickness of the substrate film is preferably 5 to 500 pm. A corona discharge treatment or the like may be performed to the surface of the substrate film in order to improve its adhesive strength to an adhesive layer.Adhesive layers formed of a polymer composition described in detail later are provided on one face or both faces of the substrate film.The polymer composition containing a polymer having a first-order melting transition which occurs over a temperature range narrower than about 15°C, which is used in the present invention, is disclosed in Japanese .nPatent Publication No. 4-507425. In this polymer composition, a side-chain crystallizable polymer can be present in an amount effective to render the adhesive layer formed of the polymer composition substantially nontacky at room temperature or lower and tacky at temperatures above room temperature. The temperature can be changed depending on the temperature in the process of cutting the multilayer of green sheets made of ceramic. For example, the temperature may be changed so as to render the adhesive layer (i) substantially nontacky at about 20°C or lower and tacky at temperatures above that temperature; (ii) substantially nontacky at about 30°C or lower and tacky at temperatures above that temperature; or (iii) substantially nontacky at about 40°C or lower and tacky at temperatures above that temperature. The change of the temperature can be arbitrarily performed by changing the polymer structure, the formulation of the polymer composition or the like.As embodiments of the polymer composition constituting the adhesive layer, it is preferable to use a side-chain crystallizable polymer or a main-chain crystallizable polymer commercially available from Landec Labs, Inc. US. These polymers include a polymer which exhibits the temperature-dependent adhesion properties. The crystallizable polymer usable for the polymer composition can include both of the side-chain crystallizable polymer and a main-chain crystallizable polymer. A difference therebetween lies in that a compound of the former class includes a crystallizable side-chain portion, and the latter class is crystallizable in its backbone structure.By the terms melting point or first-order transition, as used herein is meant the temperature at which an equilibrium process causes certain portions of the polymer, initially aligned in an ordered array, to become, disordered. By the term freezing point, is meant the temperature at which an equilibrium process causes those certain portions of the polymer, initially, disordered, to become aligned in an ordered array. In one embodiment, preferably, the first-order transition temperature or melting point will be in the range of about 20°C to 35°C, more preferably in the range of about 25°C to 30°C. It is preferred that melting occur rapidly, i.e., over a relatively narrow temperature range, less than about 10°C, preferably less than about 5°C. The polymer composition comprises a polymer which provides for loss of adhesion upon simple chilling, e.g., by application of ice, a cold pack, cold air or the like. In another embodiment, the polymer has a freezing (or crystallization) point, preferably in the range of about 10°C to 28°C, more preferably in the range of about 15°C to 25°C. It is also preferable that the polymer crystallize rapidly. To this end, seeding agents, or crystallization catalysts can be incorporated into the polymer which provide for rapid crystallization kinetics. In this embodiment, removal of the adhesive layer from the multilayer ceramic capacitor is greatly facilitated; after use, the adhesive layer may be readily removed by simple chilling, only slightly below its use temperature, without imparting undue trauma to the surface of the multilayer ceramic capacitor.The polymer is preferably a crystallizable polymer or a functional equivalent of a crystallizable polymer having a weight average molecular weight in the range of about 20,000 to 2,300,000 Daltons, typically 100,00 to 1,300,000 Daltons, most typically 250,000 to 1,000,000 Daltons. The polymer which exhibits the temperature-dependent adhesion properties described above is included in polymers which are functionally equivalent to crystallizable polymers. Depending on the embodiment, the polymer selected for incorporation into the polymer composition will comprise different monomers which provide the composition with the desired phasetransition temperature, bond strength and tack. The polymer composition may also be formulated so as to contain blends of two or more different polymers as described herein.Side-chain crystallizable polymers, sometimes called comb-like polymers, are well-known and available commercially. These polymers are reviewed in J. Polymer Sci.: Macromol. Rev. 8:117-253 (1974), the disclosure of which is hereby incorporated by reference.In general, there polymers contain monomer units X of the formula:-ΜΙSI cwherein M is a backbone atom, S is a spacer unit and C is a crystallizable group. These polymers generally have a heat of fusion (Δη£) of at least about 20 Joules / g, preferably at least about 40 Joules / g. The polymers will contain 50 to 100 wt.% monomer units represented by X. If the polymer contains less than 100% X, it will in addition contain monomer units which may be represented by Y or Z, or both, wherein Y is any polar or nonpolar monomer or mixture of polar or nonpolar monomers capable of polymerizing with X and / or Z, and wherein Z is a polar monomer or mixture of polar monomers. These polar monomers, e.g., polyoxyalkylenes, acrylates including hydroxyethylaery1ate , acrylamides and methacrylamides, will typically increase adhesion to most substrates.The backbone of the polymer (defined by M) may be any organic structure (aliphatic or aromatic hydrocarbon, ester, ether, amide, etc.) or an inorganic structure (sulfide, phosphazine, silicone, etc.), and may include spacer linkages which can be any- suitable organic or inorganic unit, for example ester, amide, hydrocarbon, phenyl, ether, or ionic salt (e.g., a carboxyl-alkyl ammonium or sulfonium or phosphonium ion pair or other known ionic salt pair).The side-chain (defined by S and C ) may be aliphatic or aromatic or a combination of aliphatic and aromatic, but should generally be capable of entering into a crystalline state. Common examples are: linear aliphatic side-chains of at least 10 carbon atoms, e.g., Ci4-C22acrylates or methacrylates, acrylamides or methacrylamides, vinyl ethers or esters, siloxanes or alpha olefins; fluorinated aliphatic side-chains of at least 6 carbons; and p-alkyl styrene side-chains wherein the alkyl is of 8 to 24 carbon atoms.-ftThe length of the side-chain moiety is usually greater than 5 times the distance between side-chains in the case of acrylates, methacrylates, vinyl esters, acrylamides, methacrylamides, vinyl ethers and alpha olefins. In the extreme case of a fluoroacrylate alternate copolymer with butadiene, the side-chain can have as little as two times the length as the distance between the branches. In any case, the side-chain units make up greater than 50% of the volume of the polymer, preferably greater than 65% of the volume.Specific examples of side-chain crystallizable monomers are the acrylate, fluoroacrylate, methacrylate and vinyl ester polymers described in J. Poly. Sci. 10: 3347 (1972); J. Poly. Sci. 10: 1657 (1972); J. Poly. Sci. 9: 3367 (1971); J. Poly. Sci. 9: 3349 (1971); J. Poly. Sci. 9: 1835 (1971); J.A.C.S. 76: 6280 (1954); J. Poly. Sci. 7: 3053 (1969); Polymer J. 17: 991 (1985), corresponding acrylamides, substituted acrylamide and maleimide polymers (J. Poly. Sci.: Poly. Physics Ed. 18: 2197 (1980); poly(α-olefin polymers such as those described in J. Poly. Sci.: Macromol. Rev. 8: 117-253 (1974) and Macromolecules 13: 12 (1980), polyalkylvinylethers, polyalkylethylene oxides such as those described in Macromolecules 13: 15 (1980), alkylphosphazene polymers, polyamino acids such as those described in J. Poly. Sci. USSR 21: 241, Macromolecules 18: 2141, polyisocyanates such as those described in Macromolecules 12: 94 (1979), polyurethanes made by reacting amine- or alcohol-containing monomers with long11 chain alkyl isocyanates, polyesters and polyethers, polysiloxanes and polysilanes such as those described in Macromolecules 19: 611 (1986), and p-alkylstyrene polymers such as those described in J.A.C.S. 75: 3326 (1953) and J. Poly. Sci. 60: 19 (1962).Of specific utility are polymers which are both relatively polar and capable of crystallization, but wherein the crystallizing portion is not affected by moisture. For example, incorporation of polyoxyethylene, polyoxypropylene, polyoxybutylene or copolyoxyalkylene units in the polymer will make the polymer more polar, improving adhesion to a moist multilayer ceramic capacitor.In a particular preferred embodiment herein, in the above structure, -C is selected from the group consisting of - (CH2)n-CH3and - (CF2)n-CF2H, where n is an integer in the range of 8 to 20 inclusive, -S- is selected from the group consisting of -0-, -CH2-, -(CO)-, 0( CO)- and -NR- where R is hydrogen or lower alkyl (16C), and -M- is -[(CH2)m-CH]- where m is 0 to 2.Typical Y units include linear or branched alkyl or aryl acrylates or methacrylates, alpha olefins, linear or branched alkyl vinyl ether or vinyl esters, maleic esters or itaconic acid esters, acrylamides, styrenes or substituted styrenes, acrylic acid, methacrylic acid and hydrophilic monomers as detailed in W084 / 0387.In addition to the above-described monomer units M-S-C, monomer structures given by-ΜI sID may in addition, or in the alternative, be present in the polymer.”D is a hydrophilic polyether chain such as a polyoxyalkylene chain (e.g., polyoxyethylene) which, in contrast to C, may or may not be crystallizable. D preferably has a molecular weight higher than about 100 Daltons.It is important in the case of polyolefins, which can exist in a plurality of tactic forms, that in order to effect the sharpness of transition between tacky and nontacky states the tacticity of the polymer must be carefully selected. The polymer can be present in a singular configuration, i.e., either atactic, syndiotactic or isotactic, but not in a mixture of tacticities unless their melting points opportunistically coincide. Having a mixture of various tactic polymers with different melting points will broaden the transition and cause the resultant polymer to exhibit sluggish adhesive property changes over a narrow temperature range.Preferred main-chain crystallizable polymers include water-insoluble polyalkylene oxides, lower alkyl polyesters and polytetrahydrofuran.The crystallizable polymer, where side-chain or main-chain crystallizable, may or may not be crosslinked. Cross-linking the adhesive composition as well as employing high molecular weight polymers will, in general, result in a material that exhibits decreased melt flow and greater cohesive strength than noncrosslinked and low molecular weight materials. Because the adhesive composition may be used at temperatures above the melting point of the polymer, low melt flow is desirable so that the adhesive will not migrate, flow or transfer to the surface of the multilayer ceramic capacitor (i.e., in contrast to conventional hot-melt adhesives). Adhesive compositions with sufficient cohesive strength to prevent cohesive failure is thus desirable. Low melt flow and suitable cohesive strength may be achieved by other means such as the addition of suitable co-monomers (e.g., high Tg monomers), by the use of block copolymerization or other art-known methods, or the inducement of cross-linking before, during or after preparation of the adhesive layer.·A variety of methods are available to produce cross-linked crystallizable materials. A network copolymer can be prepared by polymerizing a crystallizable monomer and a multifunctional monomer either in one or two steps. A one-step process may be used to form an adhesive in place, while a two-step process is useful where an intermediate processing step is necessary. A variety of multifunctional monomers (di-, tri- or multifunctional acrylic or methacrylic esters, vinyl ethers, esters or amides, isocyanates, aldehydes, epoxies and the like) are known in the art. These multifunctional monomers can be used in a one- or two14 step process depending on the desired result. Ionizing radiation, for example beta or gamma radiation, peroxides, silanes, or similar cure agents, can be used to cross-link a preformed crystallizable polymer with or without added comonomers. Ionic cross-links can be formed by, for example, reacting an acidic polymer site with a di- or trivalent metal salt or oxide to produce a complex which serves as a cross-link site. Likewise, organic salts or complexes can be prepared by methods known in the art.If the material is cross-linked to too great an extent, crystallinity and / or tack may be decreased to the point that the desirable temperature-activated properties are lost. To optimize the aforementioned factors, crosslinking should be in the range of about 0.01 percent to 5 mole percent and preferably 0.05 to 1 mole percent. The cross-linked polymers will normally have a heat of fusion of at least about 20 Joules / g, and preferably at least 30 Joules / g.Effective cross-linking may also be obtained by physical methods. For example, a block copolymer containing a crystallizable portion and a second portion which exhibits a glass transition or melting point higher than the crystallizable polymer may be prepared wherein the entire mass exhibits mechanical stability above the melting point of the crystallizable polymer but below the transition of the second polymer.As noted earlier, it is also desirable that the adhesive composition be formulated with a polymer or mixture of polymers selected such that the first-order melting transition of the composition occurs over a range narrower than about 15°C, preferably narrower than about 10°C. It is also preferred that the melting transition occur between about 5°C and about 50°C. In addition, the tack of the composition must develop within less than a minute when it is raised above the melting range and then, without contacting any substrate, revert to the nontacky state when the temperature is lowered a few degrees below the melting range. This reversal should take less than about 5 minutes. The latter tack value (PKI) is preferably less than about 25 g«cm / sec or the minimum limit of the tack measuring instrument.The adhesive compositions useful herein may include, in addition to one or more polymers as described above, conventional additives such as tackifiers (wood rosin, polyesters, etc.), antioxidants, fibrous or nonfibrous fillers, colorants, and the like. It is also possible to include additional adhesives, providing that the overall temperature sensitivity profile is not significantly affected. It is preferred that the amount of crystallizable polymer in the adhesive composition be in the range of about 40 wt.% to about 100 wt.%.Herein, preferred examples of a polymer contained in the polymer composition are as follows:(1) a copolymer of 40 to 60 parts by weight of hexadecylacrylate, 30 to 50 parts by weight of tetradecylacrylate and 2 to 10 parts by weight of acrylic acid;(2) a copolymer of 60 to 90 parts by weight of stearylacrylate, 10 to 30 parts by weight of methylacrylate and 2 to 10 parts by weight of ^acrylic acid; and (3) a copolymer of 20 to 40 parts by weight of dococylacrylate, 60 to 80 parts by weight of hexadecylacrylate and 2 to 10 parts by weight of acrylic acid.A temperature-activated polymer composition can be provided on a substrate film in any number of methods, e.g., by spray deposition, painting, dipping, gravure printing, rolling or the like. The polymer composition may also be applied by transfer from a release sheet, i.e., in a manner similar to that involved in transfer printing. The composition may be applied neat (i.e., without anything else), or in a suitable solvent or as an emulsion or latex. Alternatively, a mixture of the appropriate monomers and additives may be applied directly to a substrate and cured in place by heat, irradiation, or other suitable art-known processes.It is preferable that the adhesive layer is protected by a separator until it adheres to the surface of the multilayer of green sheets. The separator is formed of a flexible thin member made of a paper, a plastic film such as polypropylene, a metal foil or the like, and is subjected to a surface treatment with a peeling agent to provide an easy peeling property, if necessary.Next, a method for producing a multilayer ceramic capacitor will be described with reference to the accom17 panying drawings below.First, as shown in Figure IA, a slurry of ceramic powder is applied onto a carrier tape 10 with a thin thickness using a doctor blade to form a green sheet 1 of ceramic, and electrodes 2 are printed on the surface of the green sheet 1 (Figure IB). Next, a plurality of green sheets 1 are integrated into a multilayer to form a multilayer 3 of the green sheets. Herein, when integrating the green sheets into the multilayer 3, the green sheet is temporarily fixed onto a table 5 made of aluminum or the like via an adhesive tape 4 of the present invention. Since the temperature in this process is relatively high (e.g., 30°C to 80°C), the multilayer 3 satisfactorily adheres to the adhesive layer of the adhesive tape 4. Next, the multilayer 3 is subjected to heat-application and cutting (Figures 1C to IE). Reference numeral 5 in Figure ID denotes a cutter. In the process of heat-application and cutting of the multilayer, a work 7 does not peel from the adhesive layer, nor move to an uncut green sheet 1. In this manner, a plurality of green chips 7 of the ceramic multilayer are formed, and then the obtained work (green chip) 7 is removed from the adhesive tape 4. Then, the green chip 7 is transported to a preliminary baking process and then a main baking process. At this time, the adhesive tape 4 is cooled to a predetermined temperature so that the work 7 can be easily peeled off from the adhesive tape 4, as described above (Figure IF). In cooling the adhesive tape, cooling can be performed via the table, or the multilayer 3 can be placed in a freezer or the like. Thereafter, the work is baked, and an external electrode 8 is formed at the end of the work 7 to obtain a multilayer ceramic capacitor in the form of a chip (Figure 1G).ExamplesHereinafter, the present invention will be described by way of examples.A. Preparation of the polymer (Synthesization Example 1)First, 54 parts by weight of hexadecylacrylate, parts of tetradecylacrylate, 3 parts by weight of acrylic acid and 0.3 parts by weight of azobisisobutyronitrile (hereinafter, referred to as AIBN) were mixed in 200 parts by weight of toluene. The mixture was stirred at 70 °C for 20 hours to polymerize these monomers. The molecular weight of the obtained polymer was 200,000.(Synthesization Example 2)First, 75 parts by weight of stearylacrylate, 20 parts by weight of methylacrylate, 5 parts by weight of acrylic acid and 0.3 parts by weight of AIBN were mixed in 200 parts by weight of toluene. The mixture was stirred at 60°C for 20 hours to polymerize these monomers. The molecular weight of the obtained polymer was 500,000.(Synthesization Example 3)First, 30 parts by weight of dococylacrylate, 65 parts by weight of hexadecylacrylate, 5 parts by weight of acrylic acid and 0.3 parts by weight of AIBN were mixed in 200 parts by weight of toluene. The mixture was stirred at 60°C for 20 hours to polymerize these mono19 mers. The molecular weight of the obtained polymer was 400,000.B. Preparation of a temporary attachment adhesive tape for a multilayer ceramic capacitor (Example 1)A solvent (heptane / ethyl acetate = 90 parts by weight / 10 parts by weight) was added to the polymer obtained in Synthesization Example 1 so as to prepare a polymer solution having a solid % of 30%. To the polymer solution was added 0.1 parts by weight of Chemitight PZ33 as a crosslinking agent on the basis of 100 parts by weight of the polymer. Then, the resultant solution was applied to the face having been subjected to a corona discharge treatment of a PET film 100 pm thick using a roll coater so as to obtain a temporary attachment adhesive tape with a release sheet having an acrylic adhesive layer.An adhesive strength of the obtained adhesive tape was measured using an SUS as an adherend in accordance with JIS C 2107. Furthermore, the adhesive tape was peeled from the surface of the SUS, and the level of contamination of the surface of the SUS was measured by a TDS (Thermal Desorption Spectroscopy) method. The results are shown in Table 1 below.(Example 2)An adhesive tape was obtained in the same manner as in Example 1, except that the polymer obtained in Synthesization Example 2 was used. The adhesive strength and the level of contamination of the obtained adhesive tape were evaluated in the same manner as in Example 1. The results are shown in Table 1 below.(Example 3 )An adhesive tape was obtained in the same manner as in Example 1, except that the polymer obtained in Synthesization Example 3 was used. The adhesive strength and the level of contamination of the obtained adhesive tape were evaluated in the same manner as in Example 1.The results are shown in Table 1 below.(Comparative Example 1)For comparison, a thermal expansion type adhesive sheet (an expansion peel sheet (3194M-S) manufactured byNitto Denko Corporation) was used, and the adhesive strength and the level of contamination thereof were evaluated in the same manner as in Example 1. The results are shown in Table 1 below.Table 1Peel strength (gf / cm) Residue after peeling 20°C 30°C 40 °C 60°C 80°C Example 1 0 150 130 140 150 Absence ( after peeling at 20°C) Example 2 0 0 120 130 130 Absence ( after peeling at 30°C) Example 3 0 0 0 0 110 Absence ( after peeling at 30°C) Compar- a t i v e Example 1 25 20 20 30 10 Presence ( after peeling at 80°C)Various other modifications will be apparent to and can be readily made by those skilled in the art without departing from the scope and spirit of this invention. Accordingly, it is not intended that the scope of the claims appended hereto be limited to the description as set forth herein, but rather that the claims be broadly construed.
Claims
CLAIMS 1. A temporary attachment adhesive tape (4) for producing a multilayer ceramic capacitor comprising a substrate film and an adhesive layer provided on one face or both faces of the substrate film, wherein the adhesive layer is formed of a polymer composition containing a polymer having a first order melt transition which occurs over a temperature range narrower than 15°C; wherein the polymer is a side-chain crystallizable polymer, the side-chain crystallizable polymer being a copolymer composed of 60 to 90 parts by weight of stearylacrylate, 10 to 30 parts by weight of methylacrylate and 2 to 10 parts by weight of acrylic acid.
2. A temporary attachment adhesive tape (4) for producing a multilayer ceramic capacitor comprising a substrate film and an adhesive layer provided on one face or both faces of the substrate film, wherein the adhesive layer is formed of a polymer composition containing a polymer having a first-order melt transition which occurs over a temperature range narrower than 15°C; wherein the polymer is a side-chain crystallizable polymer, the side chain crystallizable polymer being a copolymer composed of 20 to 40 parts by weight of dococylacrylate, 60 to 80 parts by weight of hexadecylacrylate and 2 to 10 parts by weight of acrylic acid.