Method of treating waste.
Patent Information
- Application Number
- MYPI1997002167
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1996-05-20
- Filing Date
- 1997-05-19
- Publication Date
- 1997-11-20
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Current methods for stabilizing harmful heavy metals in waste, particularly lead in high-alkalinity ash from incinerator plants, are ineffective and costly, as cement fails to stabilize lead and do not comply with regulations.
A method involving the addition of water glass and water to waste, with optional cement, kneading, and aging to solidness, which stabilizes heavy metals by forming precipitates like lead silicate, reducing lead elution.
The method effectively stabilizes lead and other heavy metals, meeting regulatory standards with a lower cost compared to conventional chelating agents, as demonstrated by significant reductions in lead concentration in leach tests.
Abstract
Description
METHOD OF TREATING WASTEFIELD OF THE INVENTIONThe present invention relates to a waste treating method useful for stabilizing waste containing harmful heavy metals such as lead, cadmium, chromium, silver, copper, zinc, and the like.PRIOR ARTFor disposing of waste containing harmful metals, there is currently employed a method in which the waste is mixed with cement, water is added, the mixture is kneaded and aged to solidness to prevent the elution of harmful metal ions and stabilize the harmful metals. However, not all of harmful metals can be stabilized by the above conventional method of solidifying them with cement. The use of the above method is therefore inevitably limited. In some fields, the above method is not competent to laws and regulations.In an incinerator plant, for example, there is employed a method in which slaked lime or burnt lime is blown in for trapping hydrochloric acid gas formed in the incinerator before the introduction into a dust collector. Since, however, flying ash contains slaked lime, etc., in an unreacted state, the flying ash has a pH of 12 or higher, or a high alkalinity. The flying ash often contains a high concentration of lead, and the lead has the property of becoming water-soluble in the form of plumbate. When the ash is disposed without any treatment, lead is finally eluted. In the incinerator plant, therefore, the ash is mixed with cement, water is added and the mixture is aged to solidness for preventing the elution of the harmful metal. However, cement is not effective for stabilizing lead contained in flying ash since it is alkaline.PI 97002167As described above, the currently employed wast treating method has a problem, and it is therefore desired to develop a method of stabilizing harmful metals, lead in particular, contained in the ash of waste with a small amount of treating agents at a low cost.SUMMARY OF THE INVENTIONIt is an object of the present invention to provide a waste treating method useful for stabilizing waste containing harmful heavy metals. In particular, it is an object of the present invention to provide a waste treating method for preventing the re-elution of harmful metals contained in high-alkalinity ash exhausted from a waste incinerator plant and stabilizing harmful heavy metals.According to the present invention, there is provided a method of treating waste, which comprises adding water glass and water to waste containing harmful metal or metals, and kneading them.DETAILED DESCRIPTION OF THE INVENTIONThe present inventors have made diligent studies and have found that harmful metal(s) contained in waste can be stabilized by adding water glass and water to the waste. That is, the present invention is directed to a method of treating waste, which comprises adding water glass and water to waste, kneading them, and aging the kneaded mixture to solidness. The above method may be a method in which cement is added in addition to the water glass and water and the mixture is kneaded and aged to solidness. It is preferred to add cement since the cement enhances the effect of stabilizing heavy metals and at the same increases the strength of a solid substance obtained by aging the kneaded mixture.Pl 97002167The method of the present invention includes three embodiments, one in which water glass is directly added to ash, then water is added and the mixture is kneaded, a second embodiment in which water is added to ash, the mixture is kneaded to form an emulsion-like substance, water glass is added thereto and the mixture is kneaded, and a third embodiment in which water glass which is diluted with water in advance is added to ash and the mixture is kneaded.It is not necessary to impose the upper limitation on the amount of the water glass, since the larger the amount of the water glass is, the better. However, it is not good for economic performance to use water glass in too large an amount. Generally, the amount of the water glass per 100 parts by weight of waste is therefore 10 to 30 parts by weight, preferably 10 to 20 parts by weight.The activity or function of water glass stabilizing a harmful heavy metal has not yet been clarified. However, it is assumed that the heavy metal is stabilized by the following activity. For example, sodium aluminate and water glass are both in the state of a solution when each is taken alone. However, when these are mixed, a precipitate of silica-alumina is formed, and when the mixture containing the precipitate is hydrothermally treated, a synthetic zeolite is obtained. Similarly, lead ion is in a dissolved state in the form of a plumbate at the time of a high alkalinity (pH 12 or higher). However, it is assumed that when lead ion is brought into contact with water glass, it precipitates in the form of lead silicate.The water glass includes sodium silicates Nos. 1, 2, 3 and 4 and sodium metasilicate. Table 1 shows the compositions of these.PI 97002167Table 1SiOj I*) Na2O I*) Molar ratio SiO2 / Na2O Form Na silicate No. 1 36 - 38 17 ~ IB 2.00 - 2.30 liquid Na silicate No. 2 30 ~ 32 11.7 - 12.7 2.40 - 2.70 1iquid Na silicate No. 3 28 - 30 9 - 10 3.00 - 3.90 liquid Na silicate No. 4 23 - 25 6-7 3.70 - 3.90 liquid Na metasilicate 28 - 29 29 ~ 30 0.92 - 1.05 liquidReferential ExamplesLead was dissolved in a 0.1 N NaOH aqueous solution to obtain a solution containing 125,0 mg / f of lead, and the solution was separated into four portions in an amount of 300 ml each. Then, water glass No. 1, water glass No. 3 and sodium metasilicate in an amount of 2.0 g each were respectively added to 300 ml each of the above-prepared high-alkalinity aqueous solutions containing Pb ion. Each mixture was shaken at 25°C for 1 hour. Then, the shaken mixtures were centrifugally separated, and each supernatant was measured for a lead concentration. Table 2 shows the results. Further, the untreated high-alkalinity aqueous solution was measured for a lead concentration, and Table 2 also shows the result.Table 2Referential Example Sodium silicate Lead concentration (mg / f) 1-1 Water glass No. 1 5.0 1-2 Water glass No. 3 34.5 1-3 Sodium metasilicate 4.4 Control Not treated 125.0PI 97002167Table 2 clearly shows that the lead concentration in the supernatant (filtrate) is remarkably decreased according to the method of the present invention. In particular, as silica in sodium silicate comes closer to a monomer, the sodium silicate exhibits a higher effect on the stabilization of lead.EXAMPLESExamples and Comparative Example 1 (Control)Water glass No. 1 and water in amounts (part by weight) shown in Table 3 were added to 100 parts by weight of lead-containing alkaline ash from a civic garbage and waste incinerator plant, and the mixture was kneaded. The kneaded mixture was dried and aged at 80°C for 20 hours to solidify the mixture. Then, the solidified mixture was pulverized and passed through a sieve of 100 mesh, and pieces which passed through the sieve were used as a sample. 10 Grams of the sample and 100 ml of pure water were placed in an Erlenmeyer flask having a volume of 200 ml, and the flask was shaken at 37°C for 2 hours. Then, the mixture was centrifugally separated and a supernatant was sampled. Concentrated hydrochloric acid and concentrated nitric acid in an amount of 5 ml each were added to the sampled supernatant, and the mixture was boiled for 10 minutes and then measured for a concentration of lead by atomic absorption spectrometry. Table 3 shows the measurement results together with the result of measurement of a sample (Control) containing no water glass.PI 97002167Table 3Ash Water glass No. 1 Water 1 Amount lead of eluted (mg / 1) Ex.1-1 100 2.0 60.0 2.50 Ex.1-2 100 4.0 60.0 1.64 Ex,1-3 100 8.0 60.0 1.04 Ex.1-4 100 12.0 60.0 0.72 Ex.1-5 100 15.0 60.0 0.68 Ex.1-6 100 20.0 60.0 <0.1 Ex.1-7 100 30.0 | 60.0 <0.1 Control 100 - 60.0 7.48 Value under legal control - - - <0.3Ex. = ExampleTable 3 shows the following. The method of the present invention is excellent in the stabilization of lead, and it is sufficient to add 20 parts by weight, per 100 parts by weight of ash, of water glass No. 1 for meeting with the legal regulation. The above amount, 20 parts by weight, is economically advantageous when compared with the amount of a conventional chelating agent.The waste treating method of the present invention is useful for stabilizing industrial waste containing harmful heavy metals and ashes containing harmful heavy metals, exhausted from civic waste and garbage incinerator plants and trapped with an electric dust collector or a bag filter, particularly for stabilizing ashes from waste which is incinerated by blowing in slaked lime or burnt lime.
Claims
WHAT IS CLAIMED IS:
1. A method of treating waste, which comprises adding water glass and water to waste containing harmful metal or 5 metals, and kneading them.
2. A method according to claim 1, wherein the waste is an incineration ash or an incineration flying ash.
3. A method according to claim 1, wherein the water glass is added in an amount of 10 to 30 parts by weight per 10 100 parts by weight of the waste.