Method for reusing paint waste
Patent Information
- Application Number
- MYPI1997002462
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1996-06-20
- Filing Date
- 1997-06-03
- Publication Date
- 1997-12-07
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Current methods for reusing paint waste are economically inefficient and environmentally harmful, as they require large and expensive equipment, and the treatment of paint waste can lead to destruction of the natural environment due to slow decomposition of paint components.
A method involving the torrefaction of paint waste to produce a porous, lightweight residue, which is then mixed with a phosphate compound and an alkali earth metal to create a slurry that is molded and fired in a nitrogen atmosphere, resulting in a high-strength, lightweight material suitable for various applications such as tiles and heat insulating materials.
This method effectively reuses paint waste by producing a stable, high-strength material that is environmentally friendly, reducing waste volume, and simplifying the equipment and process, while providing improved workability and strength compared to traditional materials like Portland cement.
Abstract
Description
METHOD FOR REUSING PAINT WASTEBACKGROUND OF THE INVENTIONField of the Invention:The present invention relates to a method for reusing paint waste, in which it is intended to reuse waste of paint that has been used for painting operations.Description of the Related Art:When automobile bodies are painted, for example, a large amount of so-called paint waste is produced, including, for example, discharged paint without being practically deposited on the bodies, and remaining paint discharged when paint passages or the like disposed in painting equipment are washed in order to change the color of paint and perform painting with another color.At present, how to process paint waste is a topic in view of, for example, protection of the natural environment. The paint waste is usually recovered in a state in which it is mixed with water, and then it is treated to be buried in the ground, or it is discarded after burning. However, a problem arises in that disposal of a large amount of paint waste is uneconomic. Further, it is feared that the treatment to bury paint waste in the ground may cause a factor of destruction of nature since components contained in paint are decomposed at slow velocities in the nature.In such circumstances, for example, as disclosed in Japanese Laid-Open Patent Publication No. 7-275760, an-2apparatus for reusing paint discarded from painting process is known, which comprises a capturing means for capturing, with liquid, paint floating in air produced in a paint booth, a recovering means for recovering the paint from the liquid containing the captured paint, and a liquid-removing means for removing liquid from recovered and aggregated paint, in order to make reuse as paint.However, the apparatus concerning the foregoing conventional technique includes a paint filter which is provided, in the paint booth, as the capturing means for jetting water, and a means for removing water such as centrifuge which is arranged, via the recovering means, with an external water tank for introducing paint waste (waste liquid) collected in a water tank in the paint booth to the outside of the paint booth. Therefore, problems are pointed out in that the whole painting apparatus has a considerably large size, and the equipment cost becomes extremely expensive. A problem is further pointed out concerning use or application of regenerated paint.SUMMARY OF THE INVENTIONA principal object of the present invention is to provide a method for reusing paint waste, which makes it possible to effectively reuse paint waste by using simple steps and equipment.According to one aspect of the present invention, there is provided a method for reusing paint waste, wherein paint-3waste containing water, which is discharged during painting operations, is recovered (step A), and the paint waste is torrefied (step B) as shown in FIG, 1. Thus the water is evaporated, and the weight is reduced, by using a convenient apparatus to obtain an ashen paint residue (step C). The paint residue comprises components of, for example, TiO2, A12O3, and Fe2O3which are aggregated and sintered by torrefaction to provide a coarse and bulky structure. Thus the constructed paint residue is porous.Next, the porous paint residue is mixed with a phosphate compound and an alkali earth metal to obtain a slurry (step D). The slurry is subjected to a molding process to obtain a molded product (step E). After that, the molded product is fired in a nitrogen atmosphere (step F). Thus a fired product is obtained (step G), which is a carbonized, nitrided, or carbo-nitrided structural material having a high strength and a light weight. The fired product is reused for various applications such as waterpermeative tiles, water-permeative blocks, and heat insulating materials.The color of the fired product is deep indigo in the case of carbonization, or beautiful gold in the case of nitriding. In the case of carbo-nitriding, the foregoing colors co-exist, and the depth of the colors is enhanced.The fired product is stabilized by carbonization, nitriding, or carbo-nitriding. Accordingly, if the fired product itself is pulverized, the natural environment is not-4polluted.The phosphate compound is effective on change in composition caused by variation of components of the paint waste. Namely, the working operation and the processed product are not affected even when the variation of components of the paint waste is large to some extent, owing to the molecular chain-forming behavior and the chemical reaction-associated behavior of the phosphate compound. Further, the phosphate compound effects a catalytic function upon carbonization, nitriding, or carbo-nitriding, which is effective to lower the temperature required for carbonization, nitriding, or carbo-nitriding.The phosphate compound also serves like a binder which causes solidification and exhibits large binding force, in accordance with the acid-base reaction involving solid acid. Those usable as the phosphate compound preferably includes polyphosphates because polyphosphates have large molecules, and they express high strength. More preferably, those usable as the phosphate compound include, for example, metaphosphate compounds, triphosphate compounds, or tetraphosphate compounds.The polyphosphate makes a reaction with an aggregate of the torrefied residue, or it makes a reaction to surround the aggregate. A concept concerning solid acid-base may be applied, in which the aggregate serves as acid or base with respect to the polyphosphate. In this case, those principally comprising TiO2are considered to be solid acid.-5Therefore, the polyphosphate is considered to be base. On this assumption, sodium salts or potassium salts thereof are preferred.The reaction velocity is slow when the polyphosphate is used. Accordingly, the reaction velocity is controlled, i.e., the solidification time is controlled. For this purpose, the torrefied residue is added with orthophosphate such as sodium compounds of primary phosphate, potassium compounds of primary phosphate, sodium compounds of secondary phosphate, or potassium compounds of secondary phosphate within a range of 1 g to 12 g with respect to 100 g of the torrefied residue.If the orthophosphate is added in an amount less than 1 g, the molded product after drying has a low strength, and the handing workability is lowered, even when the type of phosphate compound is changed, or even when the type or the amount of alkali earth metal is changed. Further, under such a condition, a high temperature is required for carbonization or the like, which is not practical. On the other hand, if the orthophosphate is added in an amount exceeding 12 g, no change occurs in strength of an obtained molded product in a semidry state, easiness to perform construction work, and handling workability. The obtained molded product behaves as flux during the firing step, resulting in decrease in melting point. Therefore, melting occurs before sufficient carbonization or the like, making it impossible to maintain any shape. Moreover,-6carbonization or the like occurs only locally, and an obtained fired product has an extremely low strength, which cannot be practically used.The alkali earth metal has a function to shorten the solidification time. The alkali earth metal reacts with TiO2as a major component of the paint residue after torrefaction, providing an effect to express the strength and other significant properties. The alkali earth metal greatly contributes to lower the temperature for carbonization, nitriding, or carbo-nitriding. Those conveniently handled as the alkali earth metal include, for example, Mg, Ca, and Ba. Those preferably used as compounds of the alkali earth metal include oxides, carbonates, and hydroxides. They directly relate to setting of the solidification time for the molded product or the like. For example, when one or more calcium salts are added, it is possible to control the solidification time, the semidry strength upon solidification, and the dry strength, by using both of calcium carbonate and calcium hydroxide.The amount of addition of the alkali earth metal increases or decreases in conformity with the phosphate compound to be added. However, the ratio of addition of the alkali earth metal to the phosphate compound is set to be within a range of 0.3 to 1.5. If the ratio of addition is less than 0.3, it takes not less than 24 hours until solidification is achieved regardless of the amount of the phosphate compound, causing a problem from a viewpoint of-7construction work. On the other hand, if the ratio of addition exceeds 1.5, the time required to achieve solidification is several tens of seconds, making it substantially impossible to perform any construction work.Accordingly, the amount of addition of the alkali earth metal salt or compound is set to be within a range of 0.3 g to 18 g when the phosphate compound is added in an amount of 1 g to 12 g to 100 g of the torrefied residue obtained from the paint waste.The temperature for carbonization, nitriding, or carbonitriding of TiO2is usually at least not less than 1650 °C. However, it has been found that carbonization, nitriding, or carbo-nitriding effectively proceeds within a temperature range of 1200 °C to 1400 °C, by adding the phosphate compound (see FIG. 2). Therefore, the firing temperature is set to be within a range of 1200 °C to 1400 °C.If the firing temperature is less than 1200 °C, carbonization, nitriding, or carbo-nitriding does not proceeds even when the amounts of the phosphate compound and the alkali earth metal are changed. Therefore, such a temperature is not suitable for practical use. On the other hand, if the firing temperature exceeds 1400 °C, carbonization or the like sufficiently proceeds. However, the cost for processing equipment becomes expensive, and thus such a temperature is not practical. As shown in FIG.2, when the firing temperature exceeds 1250 °C, the ratio of carbonization or the like is quickly raised. Therefore, the-8firing temperature is more preferably set to be within a range of 1250 °C to 1400eC.The porosity of the fired product is set to be within a range of 10 % to 60 % in which continuous pores are obtained. The compressive strength is quickly decreased in proportion to the increase in porosity. When the porosity is increased to be 10 %, 20 %, 30 %, 40 %, and 50 %, the compressive strength is decreased to be 1400 Mpa, 1150 Mpa, 900 Mpa, 650 Mpa, and 400 Mpa respectively. However, the compressive strength of Portland cement is usually about 30 Mpa, while it varies a little depending on the aggregate to be contained. The fired product has a strength which is not less than 10 times that of Portland cement. Accordingly, it is possible for the fired product to obtain a strength sufficient to be used as laying tiles or the like.If the porosity is less than 10 %, pores are substantially independent. Therefore, it is impossible to achieve a light weight. On the other hand, if the porosity exceeds 60 %, it becomes difficult to introduce any additional pores. An obtained product is unstable even when an additive such as a foaming agent is added, and its practical strength is deteriorated to be approximately the same as Portland cement. According to the present invention, the fired product has continuous pores, and hence the following effects are provided. Namely, the product of the present invention is friendly to the global environment in that rainwater or the like is smoothly permeated to avoid-9flood damage, and it is possible to allow plants to smoothly perform their respiration.According to another aspect of the present invention, there is provided a method for reusing paint waste, wherein paint waste containing water, which is discharged during painting operations, is recovered (step A), and the paint waste is torrefied (step B). Thus the water is evaporated, and the weight is reduced by using a convenient apparatus to obtain a porous paint residue having a light weight (step C). Inorganic particles used for the paint are extremely fine. When the particles are torrefied, the particles are sintered and joined to one another even at a relatively low temperature to form a light-weight aggregate like vermiculite.The paint residue principally comprises components of TiO2and A12O3, containing mica, iron oxides and so on. The components are aggregated and sintered by torrefaction to be coarse and bulky, and thus a porous structure is constructed. The components differ depending on the color of the paint. Therefore, it is difficult to specify the components, and the range of the components is broad. For this reason, it is necessary to use a binder having an extremely strong binding force without being affected by the type of particles.According to such a viewpoint, those usable as the binder include clay minerals containing clay, such as kaolin, talc, and bentonite; phosphates; silicates; and-10alkali earth metal compounds. In particular, the phosphates and the silicates are exemplified by alkali phosphates and alkali silicates, specifically including, for example, sodium phosphate, sodium metaphosphate, sodium tripolyphosphate, potassium tripolyphosphate, sodium tetraphosphate, sodium hydrogenphosphate, potassium hydrogenphosphate, sodium metasilicate, potassium metasilicate, potassium orthosilicate, sodium orthosilicate, sodium primary silicate, sodium secondary silicate, sodium tertiary silicate, potassium primary silicate, potassium secondary silicate, and potassium tertiary silicate.The binder is added in an appropriate amount. However, it is desirable to mix 100 g of the paint residue obtained after torrefaction with the binder within a range of 0.3 to 10 g in the case of the clay mineral, 3 g to 20 g in the case of the phosphate, 2 g to 10 g in the case of the silicate, and 0.3 g to 8 g in the case of the alkali earth metal compound. If the binder is added in an amount less than the foregoing amount of addition, the strength after molding and torrefaction is low, and an obtained product is unsuitable for use. On the other hand, if the binder is added in an amount exceeding the foregoing amount, no effect is obtained, and physical properties are lowered.In the next step, after the porous paint residue is added with at least one or more materials of the clay mineral, the phosphate, the silicate, or the alkali earth metal compound within the foregoing range, water is added-11and incorporated to obtain a slurry (step D). The slurry is poured into, for example, a mold to mold a molded product (step E). In this process, solidification is achieved after the working operation within several tens of seconds to several hours by selecting additives such that the relation of solid base and solid acid is utilized. By doing so, good workability is obtained. Such selection is exemplified by a combination of sodium hexametaphosphate, potassium hydrogenphosphate, and calcium hydroxide.In order to improve the workability and avoid any crack in the molded product during the processes of, for example, solidification, drying, and temperature raising during firing, it is desirable to add a small amount of CMC (carboxymethyl cellulose), MC (methyl cellulose), PVA (polyvinyl alcohol) or the like.The molded product is fired in the atmospheric air within a temperature range of 200 °C to 500 °C or 700 °C to 1200 °C (step F) to obtain a fired product as a light-weight aggregate ( step G).The silicates and the phosphates used as the binder undergo transformation at a temperature less than 600 °C to 700 °C, or their binding network is changed at that temperature, and thus the strength, for example, the transverse rupture strength is minimized to be approximately zero in some cases. For this reason, it is necessary for the firing temperature to avoid a temperature range of less than 600 °C to 700 °C. If the firing temperature is less-12than 200 °C, water remains, and decrease in strength is caused. On the other hand, if the firing temperature exceeds 1200 °C, an obtained product is conspicuously glassified excessively, and such a product is easily destroyed. Therefore, the firing temperature is set to be within the temperature range of 200 °C to 500 °C or 700 °C to 1200 °C.The obtained fired product has an extremely light specific gravity and an extremely large void volume, owing to a low bulk density of the torrefied residue and other factors. In fact, the void volume is not less than 30 % to%.When the fired product is used, for example, as a heat insulating material for building, the effect of air conditioning is improved. The fired product may be also used as a fireproof heat insulating material such as those for ladles and ladle furnaces for steel manufacture. The use of the fired product is not limited to steel manufacture. The fired product can be widely applied to various furnaces and holding furnaces as applications concerning heat insulating materials based on the property of a large number of voids. A part or all of heat insulating materials based on carbon principally used for vacuum furnaces may be replaced with the fired product of the present invention.On the other hand, in the case of applications concerning fireproof heat insulating materials, the product-13of the present invention may be also used as an amorphous fireproof material without being subjected to the step of firing. Such an amorphous fireproof material can be directly applied to ladles or the like. Namely, paint waste is added with the additive to obtain a mixture which is transferred to a place of construction work, followed by being mixed and incorporated with water to be directly subjected to construction work so that firing is performed by utilizing accumulated heat of a ladle or the like or by utilizing heat of molten metal. Accordingly, it is unnecessary to provide any firing equipment, and the construction work is simplified.The fireproof heat insulating material thus obtained has more excellent properties than conventional alumina balloon, volcanic ash and sand deposit balloon, and vermiculite used as a fireproof heat insulating material.The above and other objects, features and advantages of the present invention will become more apparent from the following description when taken in conjunction with the accompanying drawings in which a preferred embodiment of the present invention is shown by way of illustrative example.BRIEF DESCRIPTION OF THE DRAWINGSFIG. 1 illustratively shows a diagram of steps of the method for reusing paint waste according to the present invention.FIG. 2 shows a relationship between the firing-14tempe:?ature and the nitriding ratio.DESCRIPTION OF THE PREFERRED EMBODIMENTSA method for reusing paint waste according to a first embodiment of the present invention will be described.At first, paint waste discharged from painting steps for automobile bodies was recovered from final coating, intermediate coating, and undercoating steps. After that the paint waste was torrefied. Subsequently, a paint residue produced by torrefaction was collected. The paint residue (100 g) was added with 1 g, 5 g, or 12 g of sodium hexametaphosphate, 0.5 g, 4 g, or 7 g of calcium hydroxide, and Og, 0.3g, orlgof potassium primary phosphate to obtain mixed powders respectively. Each of the mixed powders (100 g) was added, mixed, and incorporated with 12 g, 27 g, or 40 g of water to obtain slurries respectively. The print residue had a maximum particle size of about 2 mm, and a minimum particle size of submicrons. The paint residue contained unburned carbon in an amount of about 3 %.I ach of the slurries was subjected to a molding process to obtain a molded product having a size of 30 x 30 x 70 mm. The time passed from addition of water to solidification of each cf the molded products was 10 minutes, 2 minutes, and 5 minutes respectively. The respective molded products were subjected to a drying treatment at 110 °C for 4 hours after solidification, which were held at 1250 “C for 50 minutes in a nitiogen atmosphere to apply a firing treatment. During-15this process, the nitrogen pressure was 0.001 bar until the holding temperature, and it was 0.05 bar at the holding temperature.Each of fired products obtained by the firing treatment 05 was porous having a deep indigo color. However, portions having a gold color were present at parts of the fired products. The fired products had porosities of about 25 %, 40 %, and 50 % respectively, and they had strengths which could not be obtained by using ordinary oxide (A12O3) as shown in Table 1.Table 1Poros ity (« Bending strength (MPa) Example Comparative Example (AI;Oj) 25 400 100 40 ZOO SO 50 120 30Next, a method for reusing paint waste according to a second embodiment of the present invention will be described.At first, paint waste discharged from painting steps 15 for automobile bodies, which was obtained from final coating, intermediate coating, and undercoating steps, was torrefied in a fluidized bed furnace to obtain a torrefied-16residue (hereinafter referred to as paint residue) to be used as a raw material. Next, the paint residue (100 g) produced by torrefaction was added with sodium hexametaphosphate and potassium dihydrogenphosphate as the 05 phosphate compound; bentonite, talc, and kibushi clay obtained in Japan as the clay mineral; sodium metasilicate and sodium orthosilicate as the silicate compound; calcium carbonate; and calcium hydroxide in proportions shown in Table 2 respectively.Table 2List of Blending Composition (unit: g)A B C D E Sodium hexametaphosphate 5 7 4 3 Potassium dihydrogenphosphate 2 1 1 Bentonite 1 2 Kaolin 1 1 Talc 1 1 Kibushi clay 3 5 2 Calcium carbonate 1 1 Calcium hydroxide 3 4 2 1 Sodium metasi 1icate 3 1 1 Sodi urn orthos i 1 i cate 2 1-17The respective mixed powders were incorporated with water to obtain slurries. Each of the slurries was poured into a mold, followed by solidification to obtain a molded product having a size of 70 x 70 x 40 (thickness). The respective molded products were subjected to a drying treatment at 110 °C after solidification, and they were held at 350 °C and 850 °C for 60 minutes respectively to produce test pieces.During the process, the contraction ratio was not more 10 than about 1 %. Accordingly, a result was obtained, i.e., the dimensional accuracy was excellent. The products had values of their bulk densities and void volumes as shown inTable 3. A result was obtained for any of the test pieces, i.e., an extremely high void volume was obtained, making it possible to be effectively utilized as a heat insulating material.Table 3List of Physical Properties— A B C D E Calcination at 350 °C Bulk densi ty (g / cmJ) 0. 8 1. 2 1. 0 1. 6 1. 4 Void volume (X) 70 55 60 45 50 Calcination at 350 °C Bulk densi ty (g / cm1) 0. 8 1. 2 1. 0 1. 6 1. 4 Void volume (X) 70 55 60 45 50-18In the method for reusing paint waste according to the present invention, the paint waste containing water discharged during painting operations is torrefied to obtain the paint residue. After that, the paint residue is mixed with the phosphate compound and the alkali earth metal to obtain the slurry from which the molded product is formed. The molded product is fired in the nitrogen atmosphere to obtain the fired product which is a light-weight .structural material having a high strength having been carbonized, nitrided, or carbo-nitrided. Accordingly, the paint waste can be reused for various applications such as waterpermeative tiles, water-permeative blocks, and heat insulating materials, by using simple steps and equipment.In the method for reusing paint waste according to the present invention, the paint waste containing water discharged during painting operations is torrefied to obtain the porous paint residue. After that, the paint residue is mixed with the binder to obtain the slurry from which the molded product is formed. The molded product is fired in the atmospheric air to obtain the fired product as a lightweight aggregate. Accordingly, the paint waste can be reused for various applications such as light-weight heat insulating materials and light-weight fireproof heat insulating materials, by using simple steps and equipment.
Claims
WHAT IS CLAIMED IS:
1. A method for reusing paint waste, comprising the steps of: torrefying said paint waste discharged during painting 05 operations; mixing a paint residue obtained after said torrefaction with a phosphate compound and an alkali earth metal to obtain a slurry; allowing said slurry to be subjected to a molding 10 process to obtain a molded product; and firing said molded product in a nitrogen atmosphere to obtain a fired product.
2. The method according to claim 1, wherein said fired product contains, as a major component, any one of 15 titanium carbonate, titanium nitride, and titanium carbonitride .
3. The method according to claim 1, wherein said phosphate compound is at least any one of a sodium compound of polyphosphate, a potassium compound of polyphosphate, a 20 sodium compound of primary phosphate, a potassium compound of primary phosphate, a sodium compound of secondary phosphate, and a potassium compound of secondary phosphate.
4. The method according to claim 3, wherein said -20polyphosphate is a metaphosphate compound, a triphosphate compound, or a tetraphosphate compound.
5. The method according to claim 1, wherein said phosphate compound and said alkali earth metal are added 05 within ranges of 1 g to 12 g and 0.3 g to 18 g respectively with respect to 100 g of said paint residue.
6. The method according to claim 1, wherein said alkali earth metal is any one of magnesium, calcium, barium, an oxide thereof, a carbonate thereof, and a hydroxide 10 thereof.
7. The method according to claim 1, wherein said molded product is fired at a temperature within a range of 1200 °C to 1400 °C.
8. The method according to claim 7, wherein said 15 firing temperature is within a range of 1250 °C to 1400 ’C.
9. The method according to claim 1, wherein said fired product has a porosity which is set to be within a range of 10 % to 60 % to provide continuous pores.
10. A method for reusing paint waste, comprising the 20 steps of: torrefying said paint waste discharged during painting -21operations; mixing a paint residue obtained after said torrefaction with at least one compound selected from a clay mineral, a phosphate, a silicate, and an alkali earth metal to obtain a slurry; allowing said slurry to be subjected to a molding process to obtain a molded product; and firing said molded product in atmospheric air to obtain a fired product.
11. The method according to claim 10, wherein said clay mineral is added within a range of 0.3 g to 10 g, said phosphate is added within a range of 3 g to 20 g, said silicate is added within a range of 2 g to 10 g, or said alkali earth metal is added within a range of 0.3 to 8 g, with respect to 100 g of said paint residue.
12. The method according to claim 10, wherein said phosphate is selected from sodium phosphate, sodium metaphosphate, sodium tripolyphosphate, potassium tripolyphosphate, sodium tetraphosphate, sodium hydrogenphosphate, potassium hydrogenphosphate, and potassium metaphosphate, and said silicate is selected from sodium metasilicate, potassium orthosilicate, sodium orthosilicate, sodium primary silicate, sodium secondary silicate, sodium tertiary silicate, potassium primary silicate, potassium secondary silicate, and potassium -2205 tertiary silicate.
13. The method according to claim 10, wherein said molded product is fired at a temperature within a range of 200 °C to 500 °C or 700 °C to 1200 °C.
14. The method according to claim 10, wherein carboxymethyl cellulose, methyl cellulose, or polyvinyl alcohol is added in order to obtain said molded product.