Method for reusing paint waste

MYPI1997002654A0Inactive Publication Date: 1997-12-18HONDA MOTOR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1997002654
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1996-06-18
Filing Date
1997-06-13
Publication Date
1997-12-18
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Current methods for reusing paint waste are economically inefficient and environmentally harmful, as they require large and expensive equipment, and the treatment of paint waste can lead to destruction of natural components due to slow decomposition.

Method used

The method involves torrefying paint waste to produce a lightweight, porous paint residue with a high specific surface area, which is then impregnated with fertilizer components or microorganisms for use as a fertilizer or in water purification, utilizing a convenient apparatus and controlled torrefaction temperature between 600 °C to 900 °C.

Benefits of technology

This approach allows for the efficient reuse of paint waste as a fertilizer or for water purification, reducing equipment costs and environmental impact by creating a residue with a large specific surface area and controlled pH, leading to improved fertilizer retention and water-purifying capabilities.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

THE PRESENT INVENTION RELATES TO A METHOD FOR REUSING PAINT WASTE,CONTAINING WATER DISCHARGED DURING PAINTING OPERATIONS IS TORREFIED TO ORBAIN A POROUS PAINT RESIDUE.THEN,THE PAINT RESIDUE IS IMPREGNATED WITH A FERTILIZER COMPONENT CONTAINING NITROGEN,PHOSPHATE,AND POTASSIUM. ACCORDINGLY, THE PAINT WASTE IS REUSED, AND AN EXCELLANT FERTILIZER CAN BE EASILY OBTAINED. THUS IT IS POSSIBLE TO REUSE THE PAINT WASTE BY USING SIMPLE STEPS AND EQUIPMENT.
Need to check novelty before this filing date? Find Prior Art

Description

METHOD FOR REUSING PAINT WASTEBACKGROUND OF THE INVENTIONField of the Invention:The present invention relates to a method for reusing paint waste, in which it is intended to reuse waste of paint that has been used for painting operations.Description of the Related Art:When automobile bodies are painted, for example, a large amount of so-called paint waste is produced, including, for example, discharged paint without being practically deposited on the bodies, and remaining paintΙθ discharged when paint passages or the like disposed in painting equipment are washed in order to change the color of paint and perform painting with another color.At present, how to process paint waste is a topic in view of, for example, protection of the natural environment.The paint waste is usually recovered in a state in which it is mixed with water, and then it is treated to be buried in the ground, or it is discarded after burning. However, a problem arises in that disposal of a large amount of paint waste is uneconomic. Further, it is feared that the treatment to bury paint waste in the ground may cause a factor of destruction of nature since components contained in paint are decomposed at slow velocities in the nature.In such circumstances, for example, as disclosed in Japanese Laid-Open Patent Publication No. 7-275760, an apparatus for reusing paint discarded from painting process is known, which comprises a capturing means for capturing, with liquid, paint floating in air produced in a paint booth, a recovering means for recovering the paint from the liquid containing the captured paint, and a liquid-removing means for removing liquid from recovered and aggregated paint, in order to make reuse as paint.However, the apparatus concerning the foregoing conventional technique includes a paint filter which is provided, in the paint booth, as the capturing means for jetting water, and a means for removing water such as a centrifuge which is arranged, via the recovering means, with an external water tank for introducing paint waste (waste liquid) collected in a water tank in the paint booth to the outside of the paint booth. Therefore, problems are pointed out in that the whole painting apparatus has a considerably large size, and the equipment cost becomes extremely expensive. A problem is further pointed out concerning use or application of regenerated paint.SUMMARY OF THE INVENTIONA principal object of the present invention is to provide a method for reusing paint waste, which makes it possible to reuse paint waste by using simple steps and equipment.According to one aspect of the present invention, as shown in FIG. 1, paint waste containing water, which is discharged during painting operations, is recovered (step A), and the paint waste is torrefied (step B). Thus the water is evaporated, and the weight is reduced, by using a convenient apparatus to obtain an ashen lightweight paint residue (step C).Inorganic particles used for paint are extremely fine, and they are sintered at a temperature during the torrefaction. Upon the sintering, sintered particles are produced, which have many cracks and include internal voids, because the paint waste itself contains many liquid components. Accordingly, the sintered particles have a porous form having an extremely light specific gravity and an extremely large specific surface area. Specifically, when the obtained paint residue is allowed to have a dimension of not more than 1 mm, the specific surface area is not less than 100 to 200 m2 / g which is an extremely large value as compared with ordinary sand having a specific surface area of not more than 1 m2 / g. The value of the specific surface area obtained in the present invention is equivalent to or superior to those obtained after performing an acid treatment for clay mineral to increase the interatomic distance between oriented atoms thereof.During the torrefaction described above, a basic component such as calcium carbonate and slaked lime is added in order to improve the decomposition efficiency and control the torrefaction temperature. In general, when the paint waste is subjected to a torrefaction treatment, an obtained paint residue tends to have acidity due to formation of acidic oxides such as iron oxide, alumina, titanium oxide, and silica. However, in the present invention, the addition of the basic component allows the paint residue to be neutral or basic. Therefore, it is possible to obtain a preferred environment for growth of plants.The torrefaction temperature is set to be within a range of 600 °C to 900 °C. If the torrefaction temperature is less than 600 °C, sintering for the inorganic particles does not proceed. As a result, an obtained paint residue tends to be powdery and dusty, and it cannot be practically used because the liquid-holding ratio per unit mass is decreased. On the other hand, if the torrefaction temperature exceeds 900 °C, sintering for the particles excessively proceeds. As a result, although the particle strength is increased, the specific surface area and the liquid-holding ratio per unit mass are greatly decreased, and an obtained paint residue is unsuitable for use.In the next step of the present invention, the obtained paint residue is added with a fertilizer component such as those containing nitrogen, phosphate, and potassium (step D). The paint residue is impregnated with the fertilizer component which is not in a state of solid powder but in a state of aqueous solution obtained by dissolving the fertilizer component in water, because of the following reason. Namely, if the fertilizer component is added in a state of solid powder, the fertilizer component is not incorporated into the inside of the particles of the paint residue. As a result, the effect of the fertilizer is deteriorated, and the fertilizer component-carrying amount per unit mass is decreased.The paint residue impregnated with the liquid fertilizer component is subjected to a drying treatment to obtain a granular or powdery fertilizer which may be scattered over an agricultural land (step E). After the scattering, the fertilizer component is gradually eluted to the outside by the aid of rain and dew or water for irrigation or the like. The fertilizer component is in a state as if it is adsorbed and held on the surfaces of the paint residue particles. Accordingly, the elution speed is slow owing to the action of intermolecular force. Namely, the property of difficult elution (property to make elution difficult) can be improved.According to another aspect of the present invention, as shown in FIG. 2, paint waste containing water, which is discharged during painting operations, is recovered (step Ax), and the paint waste is torrefied (step B2). Thus the water is evaporated, and the weight is reduced, by using a convenient apparatus to obtain an ashen lightweight paint residue (step C1).During the torrefaction described above, a basic component such as calcium carbonate and slaked lime is added in order to improve the decomposition efficiency and control the torrefaction temperature. In general, when the paint waste is subjected to a torrefaction treatment, an obtained paint residue tends to have acidity due to formation of acidic oxides such as iron oxide, alumina, titanium oxide, and silica. However, in the present invention, the addition of the basic component allows the paint residue to be neutral or basic. Therefore, it is possible to obtain a preferred environment for growth of microorganisms or the like.The torrefaction temperature is set to be within a range of 600 °C to 900 °C. If the torrefaction temperature is less than 600 °C, decomposition residues of contained organic matters tend to remain. In this state, if an obtained paint residue contacts with water for a long period of time, it is feared that harmful substances such as formaldehyde and acetoaldehyde may be produced. Moreover, decomposition residues of organic matters also remain on the surfaces of inorganic particles, resulting in decrease in specific surface area. On the other hand, if the torrefaction temperature exceeds 900 °C, although decomposition of organic matters is achieved at approximately 100 %, sintering for inorganic particles excessively proceeds. As a result, the specific surface area is decreased, and the carrying ability is greatly decreased.When the paint waste is torrefied within the range of 600 °C to 900 °C, few components remain as organic matters. However, organic matters may remain as free carbon in a degree of 2 % or less at maximum. Such carbon serves in the same manner as activated carbon, which functions in an appropriate manner upon the use for the water purification process or the like. When the treatment is performed within the range of 600 °C to 900 °C, the specific surface area of the obtained paint residue is maximized, which reaches a value of not less than 100 to 200 m2 / g.In the next step, the paint residue after the torrefaction is allowed to carry microorganisms and / or fungi such as Lactobacillus bifidus, lactic acid bacteria, yeasts, photosynthetic bacteria, actinomycetes, and filamentous fungi for performing water-purifying action to clean and process dirty water and sludge (step Dx).The paint residue is added with a moisture component and / or a nutrient, if necessary, in addition to the microorganisms and / or fungi, and an obtained product is scattered for processing dirty water and sludge (step Ex). The microorganisms, for example, act in dirty water and sludge and serve to consume, decompose, and remove organic matters, which may be aerobic or anaerobic. Alternatively, aerobic and anaerobic microorganisms may exist in a mixed manner. When microorganisms grow previously, or when a water-purifying process is previously performed, the paint residue may be scattered as it is.When the water-purifying process proceeds with a high flow rate, and it is feared that the process fluid may become turbid if an ashen paint residue is used, for example, then the paint residue after the torrefaction is added with a binder containing, for example, sodium phosphate or sodium silicate to form a molded product having a predetermined shape, for example, a block-shaped molded product. After that, the molded product is fired at a temperature of 600 °C to 1200 °C to obtain a fired product. Subsequently, the fired product is allowed to carry microorganisms and / or fungi.According to this procedure, the inorganic porous structure of the paint residue is slightly glassified. Thus a pumiceous block, which includes continuous pores communicating with the inside, is obtained. The pumiceous block is preferably used as a medium for microorganisms and / or fungi. The pumiceous block is especially preferred for aerobic microorganisms, in which air is easily carried, the action of the microorganisms is activated by means of simple aeration, and the process ability of water purification or the like is improved.The above and other objects, features and advantages of the present invention will become more apparent from the following description when taken in conjunction with the accompanying drawings in which a preferred embodiment of the present invention is shown by way of illustrative example.BRIEF DESCRIPTION OF THE DRAWINGSFIG. 1 illustratively shows a diagram of steps of a method for reusing paint waste according to a first embodiment of the present invention.FIG. 2 illustratively shows a diagram of steps of a method for reusing paint waste according to a second embodiment of the present invention.FIG. 3 illustratively shows a paint residue particle produced in accordance with the steps of any one of the foregoing reusing methods.FIG. 4 illustratively shows a vertical cross-sectional view of the paint residue particle.FIG. 5 illustratively shows comparison concerning the time required to process dirty water between the microorganism-carrying paint residue of the present invention and a commercially available agent.DESCRIPTION OF THE PREFERRED EMBODIMENTSA method for reusing paint waste according to a first embodiment of the present invention will be explained below.At first, waste of undercoat paint, for example, paint waste containing red iron oxide, white components, or mica, which was discharged from painting steps for automobile bodies, was recovered. The paint waste was dehydrated, and then it was added with slaked lime, followed by torrefaction at 800 °C. Table 1 shows analytical values obtained by analyzing paint residue components after the torrefaction.Table 1COMPONENTS OF RESIDUE Fe2O3 T i 02 S Ϊ02 A 1 203 CaO Na20 KzO FC CONTENT (X BY WEIGHT) 13 41 20 12 8. 5 1.5 2. 5 1. 5The amount of each element shown in Table 1 is an amount calculated as oxide after conversion. The paint residue had an average particle diameter of about 0.1 mm or less and a maximum particle diameter of about 3 mm.The fine structure of the particle was observed by using an electron microscope and other instruments. As a result, as illustratively shown in FIGs. 3 and 4, the particle 10 of the paint residue was composed of a large number of weakly sintered primary particles 12 each having a size of about 0.1 pm or less (submicron). A large number of cracks 14 were observed, and a hollow cavity 16 was formed at the inside.Next, the paint residue was added with fertilizer components, i.e., ammonium phosphate, potassium phosphate, and calcium hydroxide as a solution or an emulsion respectively so that the fertilizer components were allowed to make penetration and impregnation into the inside of the respective particles 10. After that, the water content was adjusted to contain water in an amount of 7 to 9 %. Thus a fertilizer product was obtained. In order to easily scatter the product as a fertilizer, it is allowable to perform simplified granulation so that the particle 10 has a size of about 3 mm or less during the drying step or the water content-adjusting step.The purpose of the addition of calcium hydroxide is to exhibit the function as a binder and adjust pH. When the paint residue has a large content of calcium hydroxide, and elution occurs in the presence of water, it is unnecessary to add calcium hydroxide.The fertilizer thus produced was compared with a conventional agent composed of clay mineral impregnated with fertilizer components. The amounts of phosphorus, potassium, and nitrogen contained in 100 g of the paint residue were set to be identical with the amounts of impregnation in the commercially available clay mineral agent. A comparative test was performed to confirm the property of difficult elution by measuring the index of difficult elution. As a result, the conventional agent had an index of difficult elution of 99.0 to 99.8, while the fertilizer product obtained in the first embodiment had an index of difficult elution of 99.6 to 99.8. Thus a difference was scarcely found between the both.The conventional agent and the fertilizer obtained in the first embodiment were scattered, and the elution speeds of the fertilizer components of the both were compared with each other by detecting elution speeds of the phosphorus component. As a result, the fertilizer obtained in the first embodiment had an elution speed of the phosphorus component which was about 1 / 2 as compared with the elution speed of the conventional agent. Accordingly, the fertilizer obtained in the first embodiment was advantageous in that the effect of the fertilizer continued over a considerably long period of time.A method for reusing paint waste according to a second embodiment of the present invention will be explained below.In general, the paints used in painting steps for automobile bodies are mostly aqueous paints, and the paint waste discharged therefrom contains water in an amount of 50 to 70 % by weight or more. Accordingly, in this embodiment, the water content of the paint waste was firstly decreased to be not more than 30 % by weight by means of a dehydration treatment. After that, an obtained material was added with slaked lime, and it was torrefied at 800 °C.An ashen paint residue thus obtained (hereinafter referred to as first residue) contained coarse particles having a maximum particle diameter of about 3 mm, which had a broad particle size distribution ranging to a minimum particle diameter of submicron. In this embodiment, as illustratively shown in FIGs. 3 and 4, the particle 10 of the paint residue was composed of a large number of weakly sintered primary particles 12 each having a size of about 0.1 pm or less. A large number of cracks 14 were observed, and a hollow cavity 16 was formed at the inside. Therefore, for example, the microorganisms may inhabit irregular surfaces of the particle 10, the cracks 14, and the hollow cavity 16.The paint waste contained painting components of the undercoat, intermediate coat, finish coat, and overcoat in a mixed manner. The first residue obtained by torrefaction contained components as shown in Table 1 (see the first embodiment).In Table 1, FC represents free carbon. The variation of each of the components was large in iron oxide, titanium oxide, and alumina, which varied with fluctuations of about ±5, ±7, and ±4 respectively.The paint waste after dehydration was added with a sludge (so-called Bonderlte sludge) of the zinc phosphate treatment, produced in pre-painting steps or pre-steps for forging lubrication, in an amount of 30 %, followed by torrefaction. An ashen paint residue thus obtained (hereinafter referred to as second residue) contained newly added components of P2O5and ZnO which had contents of about 4 % and about 2 % respectively. As for the particles, the maximum particle diameter and the minimum particle diameter were not changed so much. However, the particle size distribution was slightly changed.The first and second residues had specific surface areas of 108 mz / g and 132 m2 / g respectively, and they had water absorption indexes per unit mass of 18 g and 24 g respectively.The first and second residues were added with microorganisms for water purification together with their culture liquid respectively, followed by being stationarily left to stand. After that, 1 kg of each of obtained samples was picked, in the same manner as a sample of a commercially available water-purifying agent used in the water purification plant. Each of the samples was added with 1 liter of domestic sewage to perform an experiment in order to compare the processing ability. Specifically, BOD (biochemical oxygen demand) was measured. A period of time required to perform the treatment by using the sample of the present invention was compared with that obtained by using the commercially available agent. Results are shown in FIG.5.Assuming that the treatment time obtained by using the commercially available agent was 1, the treatment times obtained by using the first and second residues were greatly decreased to be 0.5 and 0.3 respectively. Thus an effect was obtained in that the time was considerably shortened.The paint residue obtained by torrefaction may be mixed • with, for example, sodium phosphate, soda ash, or slaked lime, to which water may be added to perform molding, followed by firing to obtain, for example, a block-shaped product. The block-shaped product is porous and excellent in shape-retaining property, and it allows liquid to pass therethrough well. The block-shaped product has a communicating honeycomb-shaped three-dimensional network structure. The additive ensures the shape-retaining property and it functions to introduce large voids owing to the foaming action.According to the method for reusing paint waste of the present invention, the paint waste containing water discharged during painting operations is torrefied to obtain the porous paint residue, and then the paint residue is impregnated with the fertilizer components to obtain the fertilizer. Therefore, it is possible to reuse the paint waste as an excellent fertilizer by using simple steps and equipment.According to the method for reusing paint waste of the present invention, the paint waste containing water discharged during painting operations is torrefied to obtain the ashen paint residue, and then the paint residue is allowed to carry microorganisms and / or fungi. Therefore, it is possible to reuse the paint waste for the process for cleaning dirty water, sludge or the like, by using simple steps and equipment.

Claims

CLAIMS 1. A method for reusing paint waste comprising the steps of: torrefying said paint waste discharged during painting operations; and impregnating a paint residue obtained after said torrefying step with a fertilizer component comprising at least one of nitrogen, phosphate, and potassium.

2. The method according to claim 1, wherein said torrefying step is performed at a temperature within a range of 600 °C to 900 °C.

3. The method according to claim 1 or 2, wherein a basic component is added when said paint waste is torrefied.

4. The method according to claim 1, wherein said paint residue is impregnated with said fertilizer component which is in a state of an aqueous solution obtained by dissolving said fertilizer component in water.

5. The method according to claim 4, further comprising the step of performing a drying treatment for said paint residue impregnated with said fertilizer component which is in said state of said aqueous solution, to obtain a granular or powdery fertilizer.

6. A method for reusing paint waste comprising the steps of: torrefying said paint waste discharged during painting operations; and 5 allowing a paint residue obtained after said torrefying step to carry microorganisms or fungi.

7. The method according to claim 6, wherein said torrefying step is performed at a temperature within a range of 600 °C to 900 °C.

108. The method according to claim 6 or 7, wherein a basic component is added when said paint waste is torrefied.

9. The method according to any one of claims 6 to 8, further comprising the steps of: adding a binder containing a phosphate and / or a 15 silicate to said paint residue obtained by said torrefying step to form a molded product; firing said molded product at 600 °C to 1200 °C to obtain a fired product; and allowing said fired product to carry said 20 microorganisms or said fungi.

10. The method according to claim 6, wherein said paint residue is added with a moisture component and / or a nutrient.

11. The method according to claim 6, wherein said paint waste is added with a sludge of a zinc phosphate treatment, and then it is torrefied.