Metal reduction and melting process

MYPI1997003324A0Inactive Publication Date: 1998-01-25ALLOYSTREAM HLDG (PTY) LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1997003324
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1996-07-25
Filing Date
1997-07-22
Publication Date
1998-01-25
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing metal reduction and melting processes inefficiently utilize combustion gases for preheating the burden before it enters the furnace, leading to higher energy requirements and lower throughput.

Method used

The process involves preheating the burden with gaseous products outside the furnace using a sealed chamber and passage system, where combustion gases are utilized to raise the burden's temperature before it enters, allowing for partial reduction and release of volatile matter, and then these gases are burnt within the furnace to further preheat the burden, optimizing energy use and throughput.

Benefits of technology

This approach reduces energy consumption and increases furnace throughput by preheating the burden before it enters, allowing for earlier reduction reactions and more efficient use of gaseous products, while also minimizing oxidizing gas reactions that could consume carbon-containing compounds.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A METAL REDUCTION AND MELTING PROCESS WHICH INVOLVES THE HEATING OF A BURDEN COMPRISING A METAL CONTAINING COMPONENT AND A CARBON CONTAINING COMPONENT IN A CHANNEL TYPE INDUCTION FURNACE IN ORDER TO REDUCE SUCH METAL CONTAINING COMPONENT, IN WHICH AT LEAST PART OF THE GASEOUS PRODUCTS OF THE PROCESS IS UTILISED FOR PREHEATING THE BURDEN; AND APPARATUS FOR CARRYING OUT SUCH PREHEATING.@@(FIG. 1)
Need to check novelty before this filing date? Find Prior Art

Description

TITLE: METAL REDUCTION AND MELTING PROCESSBACKGROUND TO THE INVENTIONTHIS invention relates to a metal reduction and melting process, such as for example a steelmaking process, in which a metal and carbon containing burden is heated in a channel type induction furnace in order to cause the reduction and melting of the metal containing part of the burden, and apparatus for carrying out such preheating.PRIOR ARTIn a known process in this regard, i.e. that of USA Patent No. 5,411,570, where the metal containing component of the material being fed to the furnace comprises a metal ore, or a partially reduced metal ore (such as sponge iron in the case of an iron containing burden), and the carbon containing component coal; the material is fed substantially vertically into the furnace through one or more feed holes located along the side of the furnace in a manner so that the burden in the furnace forms a continuous longitudinally extending heap along each side of the furnace which floats on the bath of molten metal in the furnace.In the said arrangement the resulting gaseous products, mainly CO, and the volatile matter associated with the coal, are combusted in a cavity located in the furnace above the floating burden by burning them with oxygen, which is introduced into such area from outside the furnace.It is also said that the gases resulting from such combustion, which are typically at a temperature in the order of 1600°C, can be utilised in the furnace for heating the burden or, where the material being fed to the furnace comprises steel scrap or cold iron, the spent carbon monoxide related gas may be discharged through the same opening in the furnace through which they were charged to the furnace, in order to preheat such steel scrap or cold iron by bringing such gases directly into contact with such material.In another process in this regard, i.e. that of USA Patent No. 1,819,238, the 5 ore, carbonaceous material and fluxing materials charged to a induction heated furnace through a charging port in one end of the furnace, forms a pile at the end and is gradually distributed and melted. The gasses that are formed are exhausted through the charging port, and combusted in such manner that direct contact between the gasses and charge materials is ensured.In yet another known process, i.e. that of GB Patent No. 1 572 248, where the melting unit can be a plasma or electric arc type furnace, the gasses formed in the final reduction process are also passed through the material charging ports, allowing direct contact between the gas and charging materials.The same is true for the process disclosed in French Patent No. 1,205,446 where the melting unit can be a channel type furnace comprised of single or multiple vessels. The main reduction reaction according to this invention comprises that between the carbon dissolved in the metal and the iron oxide dissolved in the slag. The gas so formed is said to be passed countercurrently and in contact with the charge material to effect preheating and prereduction.OBJECT OF THE INVENTIONIt is an object of the present invention to provide a metal reduction and melting process in which such combustion gases are better utilised.SUMMARY OF THE INVENTIONAccording to the invention a metal reduction and melting process which involves the heating of a burden comprising a metal containing component and reduce such metal containing component, includes the step of utilising at least part of the gaseous products of such process for preheating the burden, i.e.prior to its introduction to the furnace.It will be appreciated that if as a result of such preheating the temperature of the burden is increased beyond a predetermined value, the metal containing component in the burden will start to be reduced before the burden enters the furnace.This will give rise to at least some gaseous reduction products being formed in the burden prior to its introduction to the furnace.The particular temperature at which such reduction starts to take place in the burden before it enters the furnace, will of course be determined by the nature of the particular metal containing component in the burden.Furthermore, as a result of such preheating of the burden at least some of the volatile matter associated with the carbon containing compound of the burden will also be released in the burden prior to it entering the furnace.The aforesaid gaseous products which enter the furnace may accordingly comprise the aforesaid volatile matter together with the CO and CO2 formed in the said reduction process.It will be appreciated that such preheating of the burden not only gives rise to a reduced energy requirement in the overall process, but also to an increased throughput for the furnace.Further according to the invention at least part of the aforesaid gaseous products are burnt with air and / or oxygen in the furnace and the combustion gases so produced utilised for said preheating of the burden.Further according to the invention the burden is fed to the furnace in an elongated chamber which is provided with one or more passages extending around or through the chamber, through which passages the said combustion gases can pass in order to preheat the burden in the chamber.The chamber and passage(s) are sealed off relative to one another so that no gaseous product can pass between them.In a preferred form of the invention, such a passage may comprise an annular jacket which extends longitudinally around the chamber.Further according to the invention the one or bottom end of said chamber may extend for such a distance into the furnace that it engages the heaps of burden floating on the bath of molten metal in the furnace.In this manner the burden in the chamber is prevented from falling free into the furnace through such end.In one form of the invention a positive pressure may be maintained in said chamber in order to ensure that most of the gaseous products formed in the chamber will pass into the furnace.Such a pressure may, for example, be brought about by introducing the burden to the chamber by means of a suitable lock system.In addition, or alternatively, such positive pressure may be maintained by introducing a pressurised inert gas, such as nitrogen, to the burden prior to passing it into the chamber.In one form of the invention at least some of the aforesaid gaseous products 15 formed in the burden prior to its introduction to the furnace may be removed from the burden prior to the burden entering the furnace.Thus, for example, at least some of the oxidising gases, such as CO2 and H2Ovapour, formed in the burden may so be removed from the burden.The reason for removing such oxidising gases relates to the fact that if the temperature in the burden reaches a predetermined value, such oxidising gases may react with the metal and carbon containing components of the burden thus resulting in the consumption of the carbon containing compound.Further according to the invention such oxidising gases may be removed from the burden by means of a elongated open ended conduit which extends longitudinally through said elongated chamber, so that its one or bottom end is located towards the bottom end of the chamber and its other or upper end communicates with a suitable gas withdrawal system, the conduit including over its length at least one gas outlet which is located at a predetermined level in the chamber.In use, the conduit will accordingly be surrounded by the burden and its said gas outlet located at a predetermined level in the burden.Further according to the invention said gas outlet of the conduit is located at a level in the chamber where the burden is at that temperature just before which said oxidising gases will start to react with the metal and carbon containing components of the burden.Such preferred level may, for example, be determined experimentally by, for example, analysing the gas withdrawn from the conduit.In addition, or alternatively, the temperature at the gas outlet of the conduit may be measured such as, for example, by means of a thermocouple or the like.In practice, once the preferred level of said gas outlet of the conduit has been determined, its position will remain fixed and the temperature of the burden in said location controlled by, for example, controlling the rate at which the oxidising gases is removed from the conduit, and / or the rate of the preheating, and / or the rate at which the burden is fed through the chamber.In the case where the metal containing compound comprises iron, and the carbon containing component coal, the aforesaid temperature will be in the order of 600°C.The oxidising gases which are so removed may, for example, be utilised elsewhere or they may be passed to the said passage(s) utilised for preheating the burden.Further according to the invention preheated oxygen and / or air are / is introduced to the conduit towards its said bottom end in order to combust any CO present in that part of the burden to CO2, which is then also withdrawn through said gas outlet.In order to ensure that substantially all the CO is converted to CO2 before the gas reaches the said gas outlet, the wall of the chamber immediately below the gas outlet is maintained at a lower temperature relative to the rest of the chamber.Such lower temperature may be obtained through suitable heat insulation, and / or by delaying the rate at which the burden in the chamber moves past such part of the conduit's wall. This latter operation could, for example, be effected by increasing the cross sectional width of the chamber in such areas.Still further according to the invention at least some of the volatile matter associated with the carbon containing components of the burden is circulated from the said upper end of the conduit towards its said bottom end, where it can be combusted simultaneously with the CO by oxygen and / or preheated air.As will be appreciated the heat supplied through such conversion and combustion will assist in the preheating of the burden.Said circulation of the volatile matter may be brought about by means of an elongated open ended pipe of which the one end is located at a predetermined level towards said upper end of the conduit, and the other end towards said bottom end of the conduit.Still further according to the invention, the carbon containing component of the burden may be charged to the chamber in such a manner that it is distributed towards the outer wall of the chamber, while the metal containing component of the burden is distributed towards the outer wall of said conduit.In this way the carbon containing component (which provides the carbon which is required for the endothermic Boudouard reaction which in turn is required to convert carbon dioxide into carbon monoxide, which is ultimately required for reducing the metal in the metal containing component of the burden), is closer to the preheating source than the metal containing component, which in some cases reacts exothermically with carbon monoxide. ,Further according to the invention the iron containing compound of the burden comprises an iron ore, and the carbon containing component, coal.The invention will now be described further by way of example with reference to the enclosed drawings, in which:BRIEF DESCRIPTION OF THE DRAWINGSFigure 1 is a diagrammatic cross sectional view of one embodiment of a furnace provided with preheating apparatus according to the invention; andFigure 2 is a similar view as that of figure 1 with parts shown broken away, of another embodiment of said apparatus.DETAILED DESCRIPTION OF EMBODIMENTS OF THE INVENTIONIn both embodiments of the invention a burden preheating arrangement 10 according to the invention is shown as being utilised with a channel type induction furnace 11.Furnace 11 comprises an elongated tubular vessel 12 which is of circular configuration in cross section and which includes at least two parallel spaced rows of burden feed holes which each extends through the wall· of vessel 12 along opposite sides thereof and of which only one, 13, is shown in detail in the drawings.IQ Vessel 12 is heated from below by means of two parallel spaced rows of electric induction heaters 14.When used in a steelmaking process, vessel 12 is charged with a quantity of molten steel to form a bath 16, and a burden 15, comprising-a mixture of coal and iron ore, is introduced to vessel 12 through feed holes 13 to float on the 15 bath of molten steel 16 in the form of two spaced apart heaps 17 which each extends along a longitudinal side of vessel 12, and above which a cavity 18 is formed in vessel 12.Vessel 12 is also provided with a plurality of oxygen burners 19, and at least one port (not shown) for removing the reduced and molten steel from vessel 12.In the embodiment shown in figure 1, arrangement 10 includes an elongated chamber 20 of which the one end extends through feed hole 13 into the interior of furnace 11 to such a depth that it engages the upper end of heap 17.Burden 15 is fed to chamber 20 via a burden feed bunker 21 and a series of lock systems 22.Chamber 20 is surrounded by an elongated annular passage in the form of a jacket 23 which has a bottom inlet 24 provided with a nozzle 25 which passes through the wall of vessel 12 to communicate with area 18 of furnace 11.Jacket 23 also includes a top outlet 26 which is connected via a pipe 27 to the duct 28 of a gas exhaust system (not shown).Chamber 20 and jacket 23 are suitably sealed off with respect to each other to prevent any gas from passing from the one to the other.In operation, vessel 12 is charged with a supply of molten steel 16, and induction heaters 14 switched on. A burden 15, comprising a mixture of coal and iron ore, is fed from bunker 21 via lock systems 22 and feed holes 13 into vessel 12, to form heaps 17 which float on top of liquid metal bath 16. The upper end of a heap 17 is engaged by the bottom end of chamber 20 so that the burden at the top of the heap blocks the open end of chamber 20, thus preventing burden 15 from falling freely from the open end of chamber 20.Lock systems 22 ensure that a positive pressure is maintained in chamber 20 so that substantially no gas can escape from the cold upper surface of burden15 to the outside of chamber 20.The gases, mainly CO, O^and volatile matter resulting from the heating and consequential reduction of the iron containing component of burden 15 are burnt in cavity 18 by the oxygen supplied by burners 19.The resulting combustion products are fed from area 18 via nozzle 25 and inlet 15 24 into jacket 23 where they serve to preheat the burden 15 located in the bore of chamber 20.As a result of such preheating of burden 15, the throughput of furnace 11 is increased significantly.The spent combustion gasses passing from jacket 23 via outlet 26 and pipe 27 to duct 28, can be used elsewhere in the process in order to utilise their chemical and / or thermal properties.At the same time the coal associated volatile matter located in chamber 20 can as a result of such preheating of burden 14, be cracked to carbon, CO andH2 which can then directly participate in the reduction of burden 15 in pipe 20.As a result of this, the coal and oxygen consumption per ton of product in the process can also be reduced significantly.In the embodiment shown in figure 2, wherein parts corresponding to those shown in figure 1 are indicated by the same number, a burden 15 is fed from feed bunker 21 to the upper end of an elongated chamber 29 of which the bottom end communicates with an inlet 13 in vessel 12 of furnace 11.Chamber 29 is annularly surrounded by an elongated jacket 30 of which the bottom end has an outlet 24 which communicates via nozzle 25 with area 18 of vessel 12.The upper end of jacket 30 has an outlet 26 which communicates via a pipe 27 with the duct 28 of a gas withdrawal system (not shown).The outlet of feed bunker 21 is provided with a gas inlet pipe 30.1 by means of which an inert gas such as nitrogen can be passed into burden 15 and so into chamber 29 in order to put the latter under a positive pressure.Chamber 29 is provided with an elongated open ended conduit 31 of which the upper end 32 communicates via a pipe 33 and pipe 27 with duct 28.The lower end 34 of conduit 31 extends a predetermined depth into chamber29. More details of this are given later.When burden 15 is fed through chamber 29 into vessel 12, the burden in chamber 29 will annularly surround conduit 31 and engage its bottom open end34.Conduit 31 is provided towards the middle of its length with a series of apertures 35 which are of such size that gas, but not solid burden 15, can pass through them.Conduit 31 is also provided with an elongated open ended pipe 36 of which the upper end 37 is located towards the upper end 32 of conduit 31 and its lower end 38 towards the lower end 34 of conduit 31.Conduit 31 is also provided at its open end 34 with the inlet 39 of an oxygen 5 preheated / air burner (not shown).Cohduit 31 is so positioned in chamber 29 that its apertures 35 are located in that part of burden 15 where its temperature is in the order of 600°C. Conduit 31 is furthermore of such a length that its upper end 32 is located in that part of burden 15 where its temperature is in the order of 200°C, and its lower end 10 34 in that part of burden 15 where its temperature is in excess of 800°C.Furnace 12 is operated in the same manner as that described above in respect of the embodiment of figure 1.During such operation, preheating of the lower end of chamber 29 by jacket 30 to a temperature in the order of 850° C causes the Boudoard reaction to take place, in this part of burden 15, i.e. C + CO2-> 2CO.Part of such CO will react with the iron component of burden 15 to form CC>2, thus causing the partial reduction of the iron component, i.e. 3Ρε2θ3 + CO -> 2 FegQj + CO2.The formed CO2 will flow upwardly in burden 15 until it reaches apertures 35 5 of conduit 31 through which it is then withdrawn via the bore of conduit 31 and pipes 33 and 27 to duct 28 of the gas exhaust system (not shown).Another part of the CO will flow upwardly in the bore of conduit 31 where it will be burnt to 0¾ by oxygen / preheated air burner 39, i.e. 2C0 + O2 C02» which CO2 will then, with the CO2 passing from apertures 35, pass via pipes 33 and 27 to duct 28.At the same time any volatile matter and water vapour present in the upper part in chamber 29 will pass from the upper end 37 of pipe 36 through its bottom end 38 into the bore of conduit 31 where the volatile matter will be combusted by oxygen / preheated air burner 39.It will be appreciated that the heat developed in the conversion of the CO toCO2, and the combustion of the volatile matter, will assist in heating up burden in chamber 29.It will be appreciated further that by locating conduit 31 in the said position in chamber 29 where its apertures 35 are located at that position where the temperature of the burden 15 is in the order of 600°C, the said CO2 will be removed from burden 15 before it can react with the metal and / or carbon containing components of burden 15.In order to further prevent such reaction from taking place, those parts of theIQ wall of conduit 31 located immediately below apertures 35 may be maintained at a lower temperature relative to the rest of the wall. This, may, for example be effected through proper heat insulation of the wall and / or by reducing the flow rate of burden 15 through chamber 29 in such area. The latter operation may, for example, be effected by increasing the cross sectional width of chamber 29 in such area.It will be appreciated further that the temperature of the burden at the lower end 34 of conduit 31 can be controlled by controlling any one or more of the following integers: (1) the rate at which burden 15 is fed through chamber 29;(2) the nature of the combustion in conduit 31, and (3) the rate at which the combustion gases are passed through jacket 30.It will be appreciated still further that, if required, at least part of the gases formed in vessel 12 during the reduction of burden 15 can be sucked back via inlet 13 into chamber 29 in order for them to be utilised in the reduction and / or preheating of burden 15. The molten metal product of furnace 12 can further be treated and collected in the conventional manner.It will be appreciated that the invention also includes within its scope apparatus for carrying out the process of the invention substantially as herein IQ described. It will be appreciated further that there are no doubt many variations in detail possible with a process and apparatus according to the invention without departing from the scope of the claims.Thus, for example, burden 15 may be charged to chamber 29 in such a manner that its carbon containing component is distributed towards the wall of chamber 29 and its metal containing component towards the outer wall of conduit 31 for the reasons set out above.

Claims

CLAIMS 1. A metal reduction and melting process which involves the heating of a burden (15) comprising a metal containing component and a carbon containing component in a channel type induction furnace (11) in 5 order to reduce such metal containing component, and which utilizes at least part of the gaseous products of such process produced in the furnace (11) for preheating the burden (15), characterized in that the burden (15) is fed to the furnace (11) in at least one chamber (20,29) which is provided with one or more passages (23,30) extending around or 10 through the chamber (20,29), through which the or each passage (23,30) the said gaseous products pass to preheat the burden (15) in the chamber (20,29) the or each chamber (20,29) and the or each passage (23,30) being sealed off relative to one another so that no gaseous product can pass between them.

152. The process of claim 1, characterized in that at least part of such gaseous products comprises gases produced by burning the gases resulting from the process with air and / or oxygen in the furnace (11).

3. The process of claims 1 or 2, characterized in that the or each passage (23,30) comprises an annular jacket which extends 20 longitudinally around the or each chamber (20,29).

4. The process of any one of claims 1 to 3, which is carried out in such a manner that at least one heap (17) of burden material (15) is formed which floats on a bath (16) of molten metal in the furnace (11), characterized in that the one or bottom end of the or each chamber (20.29) extends for such a distance into the furnace (11) that it engages a heap (17) of burden (15) in the furnace (11).

5. The process of any one of claims 1 to 4, characterized in that 5 a positive pressure is maintained in the or each chamber (20,29) so that most of the gaseous products formed in the or each chamber (20,29) pass into the furnace (11).

6. The process of claim 5, characterized in that the said pressure is brought about by introducing the burden (15) to the chamber 10 (20) by means of a lock system (22).

7. The process of claims 5 or 6, characterized in that the said pressure is maintained by introducing a pressurized inert gas, such as nitrogen, to the burden (15) prior to passing it into the or each chamber (20.29) .

158. The process of any one of the preceding claims, characterized in that at least some of the gaseous products formed in the burden (15) in the or each chamber (29) prior to the introduction of the burden (15) to the furnace (11) is removed from the burden (15) prior to the burden (15) entering the furnace (11).

209. The process of claim 8, characterized in that at least some of the oxidising gases, such as CO2 and H2O vapour, formed in the burden (15) are so removed from the burden (15).

10. The process of claims 8 or 9, characterized in that the said gaseous products formed in the burden (15) are removed from the burden (15) by means of an elongated open ended conduit (31) which extends longitudinally through the chamber (29), so that the one or bottom end (34) 5 of the conduit (31) is located towards the bottom end of the chamber (29) and the other or upper end (32) of the conduit (31) communicates with a suitable gas exhaust system (33,27,28) the conduit (31) including over its length at least one gas aperture (35) which is located at a predetermined level in the chamber (29). 1011. The process of claim 10, characterized in that said gas aperture (35) in the conduit (31) is located at a level in the chamber (29) where the burden (15) is at that temperature just before which oxidising gases in the burden (15) will start to react with the metal and carbon containing components of the burden (15). 1512. The process of claim 11 characterized in that the preferred level of the gas aperture (35) in the conduit (31) is determined by analysing the gas withdrawn from the conduit (31) for its CO and CO2 content.

13. The process of claims 11 or 12, characterized in that the temperature of the gas aperture (35) in the conduit (31) is measured by 20 means of a thermocouple or the like.

14. The process of any one of claims 11 to 13, characterized in that once the preferred level of the gas aperture (35) of the conduit (31) has been determined, its position remains fixed, and the temperature of the burden (15) in said location is controlled by controlling at least one of the following: the rate at which the oxidising gases is removed from the conduit (31), 5 - the rate of the preheating, the rate at which the burden (15) is fed through the chamber (29).

15. The process of any one of claims 10 to 14, characterized in that the gaseous products so removed are utilized elsewhere or passed to 10 the said passage(s) utilized for preheating the burden (15).

16. The process of any one of claims 10 to 15, characterized in that preheated oxygen and / or air are / is introduced to the conduit (31) towards its said bottom end (34) in order to combust any CO present to CO2. 1517. The process of claim 16, characterized in that the wall of the chamber (29) immediately below the gas aperture (35) is maintained at a lower temperature relative to the rest of the chamber so that substantially all the CO is converted to CO2 before the gas reaches said gas aperture (35). 2018. The process of claim 17, characterized in that the lower temperature is effected through suitable heat insulation of the chamber (29), and / or by delaying the rate at which the burden (15) in the chamber (29) moves past such part of the chamber’s wall by, for example, increasing the cross-sectional width of the chamber in such area.

19. The process of any one of claims 10 to 18, characterized in that at least some of the volatile matter associated with the carbon 5 containing component of the burden (15) is circulated from the burden (15) via at least one aperture (35) at the said other end (32) of the conduit (31) and further, towards the said one end (34) of the conduit (31), where it is combusted, simultaneously with any CO present, by means (39) of oxygen and / or preheated air. 10 20. The process of claim 19, characterized in that said circulation of the volatile matter is brought about by means of an elongated open ended pipe (36) of which the one end (37) is located at a predetermined level towards said upper end (32) of the conduit (31) in a manner so that it communicates with the burden (15), and the other end (38) is located 15 towards said bottom end (34) of the conduit (31).

21. The process of any one of the preceding claims, characterized in that the carbon containing component of the burden (15) is charged to the or each chamber (20,29) in such a manner that it is distributed towards the wall of the chamber (20,29).20 22. The process of any one of the preceding claims, characterized in that the iron containing compound of the burden (15) comprises iron ore, and the carbon containing component, coal.

23. Apparatus for preheating the burden (15) of a metal reduction and melting process which involves the heating of a burden (15) comprising a metal containing component and a carbon containing component in a channel type induction furnace (11) in order to reduce such metal 5 containing component, and which involves utilizing at least part of the gaseous products so formed in the furnace (11) for preheating the burden (15) , characterized in that the apparatus comprises at least one chamber (20.29) through which the burden (15) is fed to the furnace (11), and one or more passages (23,30) extending around or through the chamber (20,29), 10 through which passages (23,30) gaseous products formed in the furnace during the process pass in order to preheat the burden (15) in the or each chamber (20,29), the or each chamber (20,29) and the or each passage (23.30) being sealed off relative to one another so that no gaseous product can pass between them. 1524. The apparatus of claim 23, characterized in that the or each passage (23,30) comprises an annular jacket (23,30) which extends longitudinally around the chamber (20,29).

25. The apparatus of claims 23 or 24, characterized in that the one end of the or each chamber (20,29) extends for such a distance into the 20 furnace (11) that it engages a heap (17) of burden (15) floating on the bath (16) of molten metal in the furnace (11).

26. The apparatus of any one of claims 23 to 25, characterized in that the or each chamber (20) includes a lock system (22) which feeds the burden (15) to the chamber so that a positive pressure is maintained in the chamber (20) and so that most of the gaseous products formed in the chamber (20) pass into the furnace (11).

27. The apparatus of any one of claims 23 to 25, characterized in 5 that the or each chamber includes means (30.1) for introducing a pressurized inert gas, such as nitrogen, to the burden (15) prior to passing it into the chamber (29) in order to maintain a positive pressure in the chamber.

28. The apparatus of any one of claims 23 to 27 characterized in 10 that the or each chamber includes an elongated open ended conduit (31) which extends longitudinally through said chamber (29), so that its one or bottom end (34) is located towards the bottom end of the chamber (29) and its other or upper end (32) communicates with a suitable gas withdrawal system (33,27,28), the conduit (31) including over its length at least one 15 gas aperture (35) which is located at a predetermined level in the chamber (29) and through which at least some of the gaseous products formed in the burden (15) prior to its introduction to the furnace (11) is removed from the burden (15) prior to it entering the furnace (11).

29. The apparatus of claim 28, characterized in that said gas 20 aperture (35) in the conduit (31) is located at a level in the chamber (29) where the burden (15) is at that temperature just before which oxidizing gases in the burden (15) will start to react with the metal and carbon containing components of the burden (15).

30. The apparatus of any one of claims 28 or 29, characterized in that the or each chamber (29) includes means (39) for introducing oxygen and / or preheated air to the conduit (31) towards its bottom end (34) to combust any CO present to CO2. 5 31. The apparatus of claim 30, characterized in that the wall of the or each chamber (29) immediately below the gas aperture (35) is maintained at a lower temperature relative to the rest of the chamber (29) so that substantially all the CO is converted to CO2 before the gas reaches the said gas aperture (35). 1032. The apparatus of claim 31, characterized in that the said lower temperature is effected through suitable heat insulation applied to the chamber’s wall.

33. The apparatus of any one of claims 23 to 32, characterized in that the or each chamber (29) includes an elongated open ended pipe (36) 15 of which the one end (37) is located at a predetermined level towards said upper end (32) of the conduit (31), and its other end (38) is located towards said bottom end (34) of the conduit (31), the pipe (36) serving to circulate at least some of the volatile matter associated with the carbon containing component of the burden (15) said volatile matter circulates into the conduit 20 (31) from the burden (15) via at least one gas aperture (35) at said upper end (32) of the conduit (31) towards said bottom end (34) of the conduit (31), where it is simultaneously with any CO present, combusted by means (39) of oxygen and / or preheated air.