A method and an apparatus for forming semiconductor packages on a leadframe
Patent Information
- Application Number
- MYPI1997004529
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 1997-09-27
- Publication Date
- 1999-03-27
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional methods for forming semiconductor packages on a leadframe are limited by the density of packaging sections due to factors like the setting time of the mould compound and the need for minimum separation between sections, which restricts the arrangement and pressure distribution, leading to incomplete filling and premature wear of mould components.
A mould design with elongate cavities having varying cross-sectional areas for packaging sections, allowing for a higher density of packages without increasing pressure, and a unique punch-and-die mechanism for efficient separation of packages without cutting through moulded parts.
Enables a higher density of semiconductor packages on a leadframe without damaging the interconnecting wires or dies, while maintaining consistent pressure and reducing wear on mould components, and provides an efficient method for separating packages without damaging the punch.
Abstract
Description
A METHOD AND AN APPARATUS FOR FORMING SEMICONDUCTOR PACKAGES ON A LEADFRAMEField of the InventionThis invention relates to a method and apparatus for forming semiconductor packages on a leadframe and particularly to forming a high density of semiconductor packages on the leadframe.Background of the InventionA semiconductor die mounted on a leadframe, portions of the leadframe, and wires connecting the die to the leadframe, are encapsulated in moulding compound to form a semiconductor package.Conventionally, the leadframe is clamped between moulding surfaces of two mould pieces. Cavities or packaging sections in the moulding surfaces enclose corresponding semiconductor dies, portions of the leadframe, and the wires connecting the dies to the leadframe. Distribution channels in the moulding surfaces guide the flow of molten mould compound from a reservoir into the packaging sections. It is important that the molten mould compound enters the packaging sections at a predetermined pressure. A pressure higher than the predetermined pressure can damage the interconnecting wires and / or the dies enclosed in the packaging sections, and a pressure lower than the predetermined pressure can result in incompletely filled packaging sections.Various factors limit the density of packaging sections in the moulding surfaces. A first factor is the setting time of the mould compound. Setting time is the time during which the mould compound remains in a molten state and can, under pressure, be made to flow through the distribution channels and into the packaging sections. Consequently, the arrangement of the distribution channels and the packaging sections in the mould surfaces must ensure that the molten mould compound can be made to flow from the reservoir, through the distribution channels and into the packaging sections at the predetermined pressure, within the setting time.Conventionally, this is accomplished by having many short lengths of distribution channels with each one having no more than two packaging sections theraon. A disadvantage of this method is that a significant portion of the moulding surfaces is taken up by the distribution channels, thus reducing the portion of the moulding surfaces that is available for the packaging sections.One way of overcoming this limitation is to have fewer distribution channels with more than two packaging sections on each distribution channel. However, the greater the number of packaging sections, the greater the volume of molten mould compound that has to be transported from the reservoir into the packaging sections within the same setting time, and the greater the difficulty of ensuring the molten mould compound enters each of the packaging sections at the predetermined pressure.A higher pressure may be applied to the molten compound to speed up its delivery into the packaging sections. However, this does not ensure that the molten mould compound enters each of the packaging sections at the predetermined pressure. In addition, an increased pressure on the mould compound has been known to cause premature wear of inlets of the packaging sections.A second factor that limits the density of packaging sections in the moulding surfaces is the need to separate the packaging sections by a predetermined minimum distance. This separation is required to allow a punch to pass between the packages formed an the leadframe and cut through, and remove, a moulded portion formed in the distribution channel that connects the packaging sections.The greater the number of packaging sections on the moulding surfaces the smaller the distance between the packaging sections, Consequently, the reduced separation leaves little room to manoeuvre a punch. A smaller punch may be used, however, reducing the size of the punch reduces the strength of the punch, and this results in a punch that can be easily damaged.Brief Summary of the InventionThe present invention therefore seeks to provide a mould that allows a higher density of semiconductor packages to be formed on a leadframe.Accordingly, in one aspect the invention provides a mould for forming packages on a leadframe, the mould comprising: mould pieces having moulding surfaces that come together to form an elongate cavity therebetween having a first end and a second end, wherein the first end is tor coupling to a reservoir ot mould compound, the elongate cavity including: a first packaging section adjacent to the first end for moulding a package therein having an inlet with a first cross sectional area and an outlet; and a second packaging section adjacent to the second end for moulding another package therein having an inlet with a second cross sectional area which is less than the first cross sectional area.in another aspect the invention provides a method for forming packages on a leadframe, the method comprising the steps of: providing the leadframe and mould compound; clamping the leadframe between moulding surfaces on mould pieces, wherein the moulding surfaces form an elongate cavity having a first end and a second end, and wherein portions of the leadframe are enclosed within the elongate cavity; forcing the mould compound into the first end of the elongate cavity; filling a first packaging section ot the elongate cavity with mould compound, wherein the first packaging section has an inlet with a first cross sectional area and an outlet, and wherein the mould compound passes through the inlet of the first packaging section at a first predetermined pressure; filling a second packaging section of the elongate cavity with mould compound, wherein the second packaging section has an inlet with a second cross sectional area which is less than the first cross sectional area, and wherein the mould compound passes through the inlet of the second packaging section at a second predetermined pressure which is substantially equal to the first predetermined pressure; hardening mould compound in the elongate cavity: and removing the leadframe from between the moulding surfaces.Brief Description of the DrawingsAn embodiment of the invention will now be more fully described, by way of example, with reference to the drawings, of which:FIG. 1 shows a portion of a prior art mould piece;FIG. 2 shows a portion of a leadframe with semiconductor packages formed thereon by the mould piece in FIG. 1;FIG. 3 shows a side sectional view of mould pieces in accordance with the present invention;FIG. 4 shows a portion of one of the mould pieces in FIG. 3 as viewed along plane A-A;FIG. 5 shows a side view of a leadframe with semiconductor packages formed thereon by the mould pieces in FIG. 3;FIG. 6 shows a front view of a portion of the leadframe in FIG. 5; andFIG. 7 shows a sectional view of an apparatus for separating the semiconductor packages formed on the leadframe shown in FIG. 6.Detailed Description of the DrawingsFIG. 1 shows a prior art mould piece 5 with a moulding surface 8. Typically a mould has two complementary mould pieces, however, for illustrative purposes only one 5 of the two mould pieces is shown.The moulding surface 8 and a moulding surface of a complementary mould piece come together to form a mould cavity having various sections. Parts of the sections of the mould cavity in the moulding surface 8 includes: a main distribution channel 10, which is coupled to a reservoir (not shown) of mould compound; a distribution channel 15 which branches out from the main distribution channel 10; sub-distribution channels 20 that branch out from the distribution channel 15, each sub-distribution channel 20 feeding one of a first group of packaging sections 25. In addition, a predetermined length of interconnecting distribution channels or sections 30 connects each of the first group of packaging sections 25 to each of a second group of packaging sections 35.Each one of the first group of packaging sections 25 has an inlet 21 and an outlet 22, and each one of the second group of packaging sections 35 has an inlet 31. The cross sectional areas of the main distribution channel 10 and the distribution channel 15 are approximately equal. Similarly, the cross sectional areas ol the subdistribution channels 20 and the interconnecting distribution channels 30 are approximately equal.In operation, a leadframe (70 in FIG. 2) is clamped in a predetermined position between the mould surface 8 and the mould surface of the complementary mould piece. Corresponding packaging sections on the two moulding surfaces (8 and the other not shown) encloses a semiconductor die, portions of the leadframe, and interconnecting wires. The two mould pieces 5 and that of the complementary mould piece (not shown), and the mould compound in the reservoir are then heated to a predetermined temperature, and a pressure is exerted on the heated mould compound to force the mould compound into the main distribution channel 10. The cumulative effect of the heat and pressure causes the mould compound in the reservoir to melt, and the molten mould compound to flow through the main distribution channel 10, the distribution channel 15 and the subdistribution channels 20, and through the inlets 21 at a predetermined pressure into the first group of packaging sections 25. As the first group of packaging sections 25 is filled, the molten mould compound flows through the outlets 22, the interconnecting distribution channels 30, and the inlets 31, into the second group of packaging sections 35.The pressure applied on the mould compound is such that it enters the packaging sections in the first and second group of packaging sections 25 and 35 at approximately the same predetermined pressure. The pressure on the mould compound is applied for a predetermined time to allow the molten mould compound to flow into, and completely fill, the first and second group of packaging sections 25 and 35 at approximately the same predetermined pressure. After the mould compound has set or hardened, the two mould pieces 5 and the mould surface of the complementary mould piece (not shown) are separated, and the leadframe 70 with semiconductor packages formed on it can be removed. Typically, a portion of a long length of leadframe is moulded at a time. A next portion of the leadframe is then moved between the mould pieces as the moulded portion is moved out.FIG. 2 shows the leadframe 70 with packages 55 formed by the first group of packaging sections 25, packages 65 formed by the second group of packaging sections 35, and moulded parts 40, 45, 50 and 60 that were formed by the mould compound setting in the main distribution channel 10, the distribution channel 15, the sub-distribution channel 20, and the interconnecting distribution channel 30, respectively. The moulded part 60 is removed by a punch (not shown), which punches it 5 out to separate the packages 55 and 65.With the prior art mould pieces, increasing the density of packaging sections in the mould surfaces can result in incompletely filled packaging sections. The pressure on the mould compound could be increased to fill the increased number of packaging sections, however, 10 increasing the pressure can cause the increased flow rate of the molten mould compound to damage the die and interconnecting wires enclosed in the packaging sections. In addition, the increased pressure on the mould compound has been known to cause the inlets 21 and 31 of the packaging sections in the first and second groups 25 and 35 to suffer premature wear and tear, thus shortening the life of the mould pieces (5 and the other not shown).Also, for a given area of mould surface, increasing the density of packaging sections reduces the distance between the packaging sections. Consequently, a narrower punch will be required to punch out 20 the moulded parts between the moulded packages 60. However, a narrower punch will tend to break more easily.The present invention advantageously allows a higher density of packages to be formed on a leadframe without the need to increase the pressure on the molten mould compound. In addition, the present invention also provides a means of separating the moulded packages that does not require a punch to cut through moulded parts.FIG. 3 shows a mould 100 in accordance with the present invention having a first mould piece 101 and a second mould piece 102 that form a mould cavity having various sections. With reference to FIGS.3 and 4, parts of the sections of the mould cavity will be described. The first mould piece 101 has a moulding surface 103 which has a main distribution channel 104 formed therein which is coupled to a reservoir (not shown) of mould compound. A number of distribution channels 105 are formed in the surface 103 and branches out from the main distribution channel 104. The distribution channel 103 has its largest cross sectional area at the end that is coupled to the main distribution channel 104, and the smallest cross sectional area at the end furthest away from the main distribution channel 104.The distribution channel 105 has three packaging sections 107,111 and 115 formed on it, each packaging section having an inlet 106, 110 and 114 and an outlet 108 and 112. The cross sectional area of the inlets 106, 110 and 114, and the outlets 106 and 112, of the packaging sections 107, 111 and 115 respectively, are determined by the cross sectional area of a tapered channel formed by the interconnecting sections 109 and 113 of the distribution channel 105, and imaginary sections that run through the packaging section 111. The interconnecting section 109 of the distribution channel 105 tapers from the outlet 106 to the inlet 110, and the interconnecting section 113 tapers from the outlet112 and the inlet 114. It should be noted that the interconnecting sections 109 and 113 of the distribution channel 105 are shown exaggerated in size for illustrative purposes.In accordance with the described embodiment, the further the location of a packaging section on the distribution channel 105, the smaller the cross sectional area of its inlet. Consequently, the greater the compensation for the loss of pressure along the length of the distribution channel 105. For example, after the packaging section 107 is filled with mould compound, the pressure on the mould compound entering the inlet 106 and the pressure on the mould compound that flows from the outlet 108 are not equal. There is a loss in pressure, and the reduced cross sectional area of the distribution channel 105 at the inlet 110 of the next packaging section 111 on the distribution channel 105, compensates or raises ths pressure on the mould compound entering the next packaging section 111, to come closer to the predetermined pressure. With this arrangement, the pressure on the molten mould compound at the inlets 106, 110 and 114 of the mould packaging sections 107, 111 and 115, respectively, is maintained at approximately the predetermined pressure.The reducing cross sectional area of a distribution channel advantageously increases and equalises the pressure on the mould compound at the inlets of the packaging sections on the distribution channel. This enables each of the packaging sections on the distribution channel to be filled with mould compound at approximately tha same rate. Consequently, this allows a distribution channel in the moulding surfaces to have a greater number of packaging sections on it, which reduces the portion of the moulding surfaces used for distribution channels, and increases the portion of the moulding surfaces available for packaging sections.On the mould piece 101 there are ridges 120 and 122 within the interconnecting sections 109 and 113, respectively, of the distribution channel 105. The ridges 120 and 122 are formed on the inner surfaces of the respective interconnecting sections 109 and 113 and are transverse to the length of the interconnecting sections 109 and 113, With additional reference to FIGS. 5 and 6, a leadframe 202 is shown after the moulding process with packages 212, 216 and 220 formed thereon, and moulded parts 210, 214 and 218 being the mould compound that has hardened or set in the main distribution channel 104, and the interconnecting sections 109 and 113, respectively. The moulded part 214 has a notch 230 formed therein by the ridge 120. Similarly, the moulded part 218 has a notch 232 formed therein by the ridge 122. The notches 230 and 232 provide stress concentration points for subsequent punching and shearing processes.FIG. 7 shows packages 212 and 216 having dies 330, and interconnecting wires 340 moulded therein on the leadframe 202. A punch 410 and a die 430 are used to separate the packages 212 and 216 formed on the lead frame 202. An arrow indicates the direction of travel of the punch 410 towards the die 430 and into an opening 435 in the die 430. In operation, the moulded part 214 is located between the punch 410 and die 430. The moulded part 214 is aligned with the punch 410 so that the punch 410 impacts upon the side of the moulded section 214 that is opposite the notch 216.The upward force of the punch 410 on the moulded part 214 pushes the moulded part 214 upwards. However, the die 430 prevents the upward movement of the two packages 212 and 216. This results in the moulded part 214 being moved further upward by the punch 410 causing a bending force on the moulded part 214. The notch 230 is a stress concentration point that focuses the bending force on the moulded part 214 adjacent to the notch 230. This causes the moulded compound at of the moulded part 214 to stretch and tear or break, thus, separating the packages 212 and 216. The same process is then repeated to separate the packages 216 and 220. It should be noted that the interconnecting parts 214 and 218 are shown exaggerated in size for illustrative purposes.Hence, the described mould advantageously allows a higher density.of packages to be formed on a leadframe without increasing the pressure on the mould compound. This is accomplished by reducing the cross sectional area of a distribution channel that guides the mould compound into packaging sections thereon, such that the packaging sections on the distribution channel that are located further away from the supply of mould compound have a smaller cross sectional area. This arrangement equalises the pressure on the mould compound at the inlets to the packaging sections on the distribution channel to become approximately equal to a desired pressure, irrespective of the location of the packaging sections on the distribution channel.In addition, the described mould and punch and die together provide a means for separating a higher density of moulded semiconductor packages that are formed on a leadframe. This is accomplished by the mould forming a notch on one side of a moulded part that interconnects the packages, and punching the moulded part on the opposite side to where the notch is located. This causes the moulded part to tear at the point adjacent to the notch and separates the packages.Hence, the described mould and punch and die set allows a higher density of semiconductor packages to be formed on a leadframe, and in addition, provides a means of separating the packages formed on the leadframe.
Claims
1. A mould for forming packages on a leadframe, the mould comprising: mould pieces (101,102) having moulding surfaces (103) that come together to form an elongate cavity therebetween having a first end and a second end, wherein the first end is for coupling to a reservoir of mould compound, the elongate cavity including: a first packaging section (107) adjacent to the first end for moulding a package therein having an inlet (106) with a first cross sectional area and an outlet (108); and a second packaging section (111) adjacent to the second end for moulding another package therein having an inlet (110) with a second cross sectional area which is less than the first cross sectional area.
2. A mould in accordance with claim 1 wherein the outlet has a third cross sectional area which is less than the first and greater than the second cross sectional area.
3. A mould in accordance with any one of the preceding claims wherein the elongate cavity further comprises a first tapered interconnecting section (109) that tapers from the outlet (108) of the first packaging section (107) to the inlet (110) of the second packaging section (111).
4. A mould in accordance with claim 1 wherein the elongate cavity further comprises at least one packaging section located between the first and second packaging sections for moulding a further package therein having an inlet with a fourth cross sectional area which is greater than the second cross sectional area.
5. A mould in accordance with claim 4 wherein the cross sectional area of the inlet of the at least one packaging section is less than the first cross sectional area6. A mould in accordance with either claim 4 or 5 wherein the cross sectional area of the outlet of the at least one packaging section is greater than the second cross sectional area.
7. A mould in accordance with any one of claims 4, 5 or 6 wherein the cross sectional area of the outlet of the at least one packaging section is less than the fourth cross sectional area.
8. A mould in accordance with any one of claims 4-7 wherein the elongate cavity further comprises a second tapered interconnecting section (113) that tapers from the outlet (108) of the first packaging section (107) to the inlet (110) of the at least one packaging section.
9. A mould in accordance with any one of claims 4-8 wherein the elongate cavity further comprises a third tapered interconnecting section that tapers from the outlet of the at least one packaging section and the inlet of the second packaging section (111).
10. A mould in accordance with claim 3 wherein the first tapered interconnecting section (109) has an internal surface with a first ridge (120) that extends therefrom and being arranged transverse to the length of the first tapered interconnecting section (109).
11. A mould in accordance with either claim 8 or 9 wherein the second tapered interconnecting section (113) has an internal surface with a second ridge (122) that extends therefrom and being arranged transverse to the length of the second tapered interconnecting section.
12. A mould in accordance with any one of claims 8, 9 or 11 wherein the third tapered interconnecting section has an internal surface with a third ridge that extends therefrom and being arranged transverse to the length of the third tapered interconnecting section.
13. A mould in accordance with any one of the preceding claims wherein the mould pieces (101,102) are made of high speed hardened steel.
14. A mould in accordance with any one of the preceding claims wherein the mould pieces (101,102) are made of ASP 23.
15. A mould in accordance with any one of the preceding claims wherein the lead frame has device locations thereon, and wherein the packaging sections in the mould surfaces are arranged to enclose the device locations therein when the leadframe (202) is clamped between the moulding surfaces.
16. A mould in accordance with any one of the preceding claims wherein the mould pieces comprise at least two mould pieces (101,102).
17. A method for forming packages on a leadframe (202), the method comprising the steps of: a) providing the leadframe (202) and mould compound; b) clamping the leadframe (202) between moulding surfaces on mould pieces (101,102), wherein the moulding surfaces form an elongate cavity having a first end and a second end, and wherein portions of the leadframe (202) are enclosed within the elongate cavity; c) forcing the mould compound into the first end of the elongate cavity; d) filling a first packaging section (107) of the elongate cavity with mould compound, wherein the first packaging section has an inlet (106) with a first cross sectional area and an outlet (108), and wherein the mould compound passes through the inlet of the first packaging section at a first predetermined pressure; e) filling a second packaging section (111) of the elongate cavity with mould compound, wherein the second packaging section has an inlet (110) with a second cross sectional area which is less than the first cross sectional area, and wherein the mould compound passes through the inlet of the second packaging section at a second predetermined pressure which is substantially equal to the first predetermined pressure; f) hardening mould compound in the elongate cavity; and g) removing the leadframe (202) from between the moulding surfaces.
18. A method in accordance with claim 17 further comprising after step (d) the steps of: h) guiding mould compound into at least one packaging section located between the first and second packaging sections having an inlet with a third cross sectional area which is less than the first and greater than the second cross sectional area and an outlet; and i) filling the at least one packaging section with mould compound.
19. A method in accordance with claim 17 further comprising after step (d) but before step (e) the step of guiding mould compound through a first tapered interconnecting section (109) of the elongate cavity which tapers from the outlet of the first packaging section to the inlet of the second packaging section (111).
20. A method in accordance with claim 18 wherein step (h) further comprises the step of guiding mould compound through a second tapered interconnecting section (113) of the elongate cavity which tapers from the outlet of the first packaging section and the inlet of the at least one packaging section.
21. A method in accordance with claim 18 after step (i) further comprises guiding mould compound through a third tapered interconnecting section of the elongate cavity which tapers from the outlet of the at least one packaging section and the inlet of the second packaging section (111).
22. A method in accordance with claim 19 further comprising the step of forming a first notch on mould compound in the first tapered interconnecting section (109) with a first ridge (120) extending from an inner surface of the first tapered interconnecting section, wherein the first ridge is arranged transverse to the length of the first tapered interconnecting section.
23. A method in accordance with claim 20 further comprising the step of forming a second notch on mould compound in the second tapered 5 interconnecting section (113) with a second ridge (122) extending from an inner surface of the second tapered interconnecting section, wherein the second ridge is arranged transverse to the length of the second tapered interconnecting section.
24. A method in accordance with either claim 21 or 23 further comprising the step of forming a third notch on mould compound in the third 10 tapered interconnecting section with a third ridge extending from an inner surface of the third tapered interconnecting section, wherein the third ridge is arranged transverse to the length of the second tapered interconnecting section (113).
25. A method in accordance with any one of claims 17-25 further comprising the step of clamping the leadframe (202) in a predetermined position 15 between the moulding surfaces of the mould pieces (101,102).