Method of packaging a semiconductor die and a leadframe structure therefor
Patent Information
- Application Number
- MYPI1997004573
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 1997-10-01
- Publication Date
- 1999-04-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing semiconductor packages with fully exposed heat sinks face difficulties in removing mould resin from the bend corners during the deflash process, leading to package integrity issues and increased size due to trapped resin.
A leadframe structure with flag portions featuring V-shaped grooves allows for the bending of side walls to form a base and exposed heat sink, minimizing the inner bend radius and enabling easier resin removal during packaging, while maintaining a high heat sink-to-package ratio.
The solution reduces package size and enhances resin removal efficiency, maintaining high package integrity and maximizing heat sink exposure, thus addressing the challenges of larger die sizes and heat dissipation in high-power semiconductor devices.
Abstract
Description
Method of Packaging a Semiconductor Die and a Leadframe Structure ThereforField of the InventionThis invention relates to a method of packaging a 5 semiconductor die and to leadframe structure on which a semiconductor die can be mounted and which enables a package moulded around the semiconductor die to be reduced in size whilst having an exposed heatsink and minimising package flash.Background of the InventionSemiconductor devices which use high power generally require a heat sink to dissipate the generated heat. The semiconductor die is mounted on a flag portion of the leadframe, which serves as a heat sink. The package is then moulded around the die and the leadframe, such that a lower face of the flag portion is exposed and flush with the outer surface of the packages. In order to accommodate larger die, it is desirable to maximize the heat sink within the same package outline while maintaining high package integrity. The requirements become more and more critical as high power, lower profile, bigger die size packages are needed in some markets, such as the portable radio products market.Various semiconductor packages are known which provide large heat sink-to-moulded package ratios. In one known package, the package structure has a fully exposed heat sink.This package structure maximizes the heat sink while achieving high package integrity by having two side walls of the flag portion bent up, thereby also acting as mould lock. However, the roll over area at the bend corners in this package structure tends to fill up with mould resin during the moulding process, and thus becomes difficult to remove in the subsequent deflash process. FIG. 9 shows the abovementioned known leadframe structure during the package moulding process. The leadframe includes a flag portion 22 on which is mounted the semiconductor die 24, having an electrical connector 25 mounted thereon. Two side walls 29 of the leadframe extend from the flag portion 22 and are bent around the die 24 bend comers 23. The outer surfaces • · · · of the flag portion 22 and the side walls 29 thus serve as a heat sink and are exposed flush with the outer surface of the moulded package. However, during the moulding process, mould resin (flash) 26 is entrapped between the external surface of the bend corners 23 and top and bottom mould cavities 27 and 28, between which the package is moulded. During the following cleaning (deflash) operation, it is difficult to remove all the flash accumulated at these corners. ,Brief Summary of the Invention 10 The present invention therefore seeks to provide a leadframe structure which overcomes, or at least reduces the above-mentioned problems of the prior art.Accordingly, in a first aspect, the invention provides a leadframe for a semiconductor die, the leadframe comprising a first rail having one or more flag portions extending therefrom, each flag portion providing a mounting area for receiving the semiconductor die, a second rail substantially parallel to the first rail and connected thereto by one or more tie bar portions, the second rail having one or more respective lead portions extending therefrom towards the respective flag portion(s) for connection to the respective die(s) when mounted on the respective mounting area(s), wherein at least one of the flag portions is formed with at least two grooves at opposite sides of the mounting area so that opposite sides of the flag portion can be bent along the grooves to provide a base having the mounting area thereon and side walls extending away from the base.According to a second aspect, the invention provides a method of packaging a semiconductor die comprising the steps of:providing a leadframe comprising a first rail having one or more flag portions extending therefrom, each flag portion providing a mounting area for receiving the semiconductor die, a second rail substantially parallel to the first rail and connected thereto by one or more tie bar portions, the second rail having one or more respective lead portions extending therefrom towards the respective flag portion(s) for connection to the• ·- 7 respective die(s) when mounted on the respective mounting area(s);forming at least two, substantially parallel grooves at opposite sides of the flag portion;bending opposite sides of the flag portion along the grooves to provide a base having the mounting area thereon and side walls extending away from the base;mounting the semiconductor die(s) on the respective mounting area(s); ' connecting the semiconductor die(s) to the respective lead portion(s); and moulding a package around the leadframe and semiconductor die such that outer surfaces of the base and side walls are exposed and flush with outer surfaces of the moulded package.In one embodiment, the grooves have a “V” shape. Preferably, the two side walls extend at an angle slightly less than 90° to the base. The grooves preferably extend to a depth of approximately 0.6 times the thickness of the flag portion.Brief Description of the DrawingsOne embodiment of the invention will now be more fully described, by way of example, with reference to the drawings, of which;FIG. 1 shows a plan view of one embodiment of a 25 leadframe structure according to the invention having semiconductor dies mounted thereon;FIG. 2 shows a side view of the leadframe structure of FIG.1;FIG. 3 shows a plan view of the leadframe structure of FIG. 30 1, at an initial stage in the packaging process;FIG. 4 shows a cross-sectional view along line A-A of FIG. 3 and illustrating the grooves being formed therein;FIG. 5 shows a plan view of the leadframe structure of FIG. 3, after the next stage in the packaging process;FIG. 6 shows a cross-sectional view along line B-B of FIG. 5 and illustrating the side walls being bent;• ·FIGS. 7 and 8 show a comparison between a typical known bending process and the bending radius of the corners of the embodiment illustrated in FIGS. 1 to 6; andFIG. 9 shows a part cross-sectional view through a known leadframe structure with fully exposed heat sink during the package moulding process.Detailed Description of the DrawingsReferring first to FIGS. 1 and 2, a leadframe structure having three (3) units per section is shown. Each unit is formed by a flag portion 2, on which a semiconductor die 3 is mounted. The flag portion 2 is connected to a rail 1, which connects several flag portions together, and to other sections of the leadframe. Opposite sides of the flag portion 2, on either side of the semiconductor die 3 are bent upwards to form side walls 6. FIG.also shows a set of three lead portions 4 of the leadframe extending towards each of the semiconductor die 3. These lead portions 4 may be bent up and over the semiconductor die 3 to facilitate electrical connection thereto and the connection may be made either by means of wire bonds or soldered clips (not shown). As shown in FIG. 2, in this embodiment of the invention, the bends to form the side walls 6 are facilitated by the provision of V-shaped grooves 5, which are stamped into the flag portion.To further illustrate this embodiment, FIG. 2 shows a leadframe structure (only showing two units) after the V-groove stamping stage. Each V-groove 5 defines an axis along which an outer portion 10 of the flag portion 2 can be bent to produce the upstanding side walls 6. As best shown in FIG. 4, the V-groove 5 is made by using a punch 11 having a ridge 7 on its end and moving the punch 11 in the direction of arrow 12 onto the surface of the flag portion 2. The stamping process actually produces a groove 5 with sloping side walls 8 meeting together at an apex 9. Thus, since material is removed from the groove 5, the actual material thickness along the bend axis is reduced; this enables a smaller inner bend radius to be produced at the bend, with a correspondingly smaller external bend radius beingproduced during the subsequent side wall forming stage to be described below.Thus, FIG. 5 illustrates the final lead frame structure, after the side wall forming process illustrated in FIG. 6. As best shown in FIG. 6, the leadframe is clamped at its flag portion 2 between a top anvil 14 and a bottom pressure pad 15, with the V-grooves 5 arranged along the bottom side edges of the top anvil 14. A bending punch 16 then presses upwards, in the direction of arrow 17, so as to bend the outer portions 10 of the flag portion 2 along the grooves 5 and against the side walls of the top anvil 14 to form the side walls 6. In this way, an inner bend corner 20 will be formed around the top anvil 14, corresponding to the radius R 19 of the top anvil 14 along its bottom side edges. Since material in the V-groove region has been removed, a top anvil 14 with smaller radii can be used than hitherto, thereby producing bends with smaller inner radii. As a result of this wall forming process, the side walls 6 extend in a plane 21, which is slightly less than 90° to the plane of the flag portion 2. The finished leadframe is illustrated in FIG. 5, showing the same view as FIG. 3, but with the outer portions 10 of the flag portions 2 having been bent up to form the side walls 6 on either side of a mounting area onto which the semiconductor die will be mounted.FIGS. 7 and 8 illustrate the important dimensions of the leadframe structures of the prior art (FIG. 7) and of the embodiment of the invention described above (FIG. 8). In these two FIGS, the leadframe has a thickness t, at least of the flag portion 2, so that, for the prior art bending shown in FIG. 7, the inner radius Rl is 0.5t, whereas the outer radius R2 is Rl + t = 1.5t. In the case of the present embodiment, as shown in FIG. 8, for a groove having a height h, the minimum inner radius, R3 is given by:R3 = 0.5 x (t - h) so that, for a height h = 0.4t, the inner radius is 0.3t. Then:R4 = R3 + (t - h) - 0.9t.Thus, R4 is substantially smaller than R2.Some values found to be useful in the implementation of this embodiment are give below, with reference to the general bending formula;a = (q / 180)x (Kt + R) where a = length of arc (neutral bending line)R = internal bending radius t = thickness of material q 4= bend angleK = constantThus, a first beneficial value is for the depth h of the V-groove given by;h < 0.6 t indicating that the depth of the V-groove punch is preferably 15 less than 60% of the material thickness.Secondly, the opening angle φ of the V-groove is given by: φ> 90° indicating that the opening angle of the V-groove is preferably greater than 90 degrees.Thirdly, the opening width of the V-groove is given by:w = t + / - 0.2 t indicating that the opening width of the V-groove is preferably not less than 80% of the material thickness, and not more than 120% of the material thickness.In a preferred embodiment, the radius R5 of the bottom side edge of the top anvil 14 is given by:R5 < 0.2 t indicating that the top anvil bottom side edge radius is preferably less than 20% of the material thickness.Finally, the bend angle Θ is given by:90° < Θ < 100° indicating that the bend angle is preferably more than 90 degrees but less than 100 degrees.It will be appreciated that although only one particular 35 embodiment of the invention has been described in detail, various modifications and improvements can be made by a >··· ···· · « person skilled in the art without departing from the scope of the present invention.
Claims
Claims 1. A leadframe for a semiconductor die, the leadframe comprising a first rail having one or more flag portions extending 5 therefrom, each flag portion providing a mounting area for receiving the semiconductor die, a second rail substantially parallel to the First rail and connected thereto by one or more tie ' bar portions, the second rail having one or more respective lead portions extending therefrom towards the respective flag 10 portion(s) for connection to the respective die(s) when mounted on the respective mounting area(s), wherein at least one of the flag portions is formed with at least two grooves at opposite sides of the mounting area so that opposite sides of the flag portion can be bent along the grooves to provide a base having the mounting 15 area thereon and side walls extending away from the base.
2. A leadframe according to claim 1, wherein the grooves have a “V” shape.
203. A leadframe according to either claim 1 or claim 2, wherein the two side walls extend at an angle slightly less than 90° to the base.
4. A leadframe according to any one of claims 1, 2 or 3, 25 wherein the grooves extend to a depth of approximately 0.6 times the thickness of the flag portion.
5. A method of packaging a semiconductor die comprising the steps of: 30 providing a leadframe comprising a first rail having one or more flag portions extending therefrom, each flag portion providing a mounting area for receiving the semiconductor die, a second rail substantially parallel to the first rail and connected thereto by one or more tie bar portions, the second rail having 35 one or more respective lead portions extending therefrom towards the respective flag portion(s) for connection to the • ············ • · · · · ······ · • · · · · ·· . 9 respective die(s) when mounted on the respective mounting area(s); forming at least two, substantially parallel grooves at opposite sides of the flag portion; bending opposite sides of the flag portion along the grooves to provide a base having the mounting area thereon and side walls extending away from the base; mounting the semiconductor die(s) on the respective mounting area(s); connecting the semiconductor die(s) to the respective lead portion(s); and moulding a package around the leadframe and semiconductor die such that outer surfaces of the base and side walls are exposed and flush with outer surfaces of the moulded package.
6. A method according to claim 5, wherein the the grooves have a “V” shape.
7. A method according to either claim 5 or claim 6, wherein the two side walls extend at an angle slightly less than 90° to the base.
8. A method according to any one of claims 5, 6 or 7, wherein the grooves extend to a depth of approximately 0.6 times the thickness of the flag portion.