AI Technical Summary
Liquid potting materials for semiconductor packaging face issues such as moisture penetration, residual gas bubbles leading to cracks under thermal stress, and delamination due to mismatched coefficients of linear expansion, particularly in COB and PPGA types, which compromise reliability compared to ceramic-based hermetic potting.
A liquid epoxy resin potting material composition comprising a specific ratio of liquid epoxy resin, alkylated diaminodiphenylmethane, epoxidized polybutadiene, and inorganic filler, optimized for viscosity, molecular weight, and particle size distribution to enhance reliability and reduce thermal stress, ensuring complete filling and uniform distribution.
The composition significantly improves semiconductor reliability by preventing delamination and cracks in accelerated tests, maintaining workability and flow characteristics while reducing filler sedimentation and enhancing thermal stress resistance.
Abstract
Description
LIQUID EPOXY RESIN POTTING MATERIALTECHNICAL FIELD OF THE INVENTIONThe present invention relates to a liquid epoxy resin potting material which is used for potting semiconductors.PRIOR ARTThe lower cost and higher integration trends in semiconductor packaging have changed the packaging form used from the conventional transfer molding DIP (dual inline package) to COB (chip on board), PPGA (plastic pin grid array), and the like. A liquid potting material is used for potting the PPGA-type semiconductor, but it is not satisfactory in reliability compared to a ceramic-based hermetic potting type. The causes for this include, for example, moisture penetrating through the package-fabricated organic printed circuit boards. Moreover, unlike transfer molding DIPs, a liquid potting material under no pressure, when allowed to flow and be molded, results in residual gas bubbles which lead to cracks when subjected to thermal stresses. Furthermore, when the potting material has a different coefficient of linear expansion from that of the semiconductor chip or the organic baseboard, a delamination occurs at the interface when subjected to a thermal stress, which facilitates moisture penetration.OBJECT AND SUMMARY OF THE INVENTIONIntensive study of a way to solve the prior art problems has led to the finding that a composition comprising a specific epoxy resin, aromatic diamine, and elastomer, along with an inoganic filler, provides a potting material with substantially improved semiconductor reliability in an accelerated test such as the PCT (pressure-cooker test) or T / C (cold-heat cycle test), and the like, resulting in the present invention.The present invention provides a liquid epoxy resin potting material mainly comprising (A) a liquid epoxy resin, (B) a liquid alkylated diaminodiphenylmethane, (C) an epoxidized polybutadiene, and (D) an inorganic filler, wherein the ratios of the individual components in weight ratios are:(A) / [(A) + (B)] = 0.65 - 0.80 (C) / [(A)+(B)J = 0.01 - 0.05 and (D) / [(A)+(B)+(C)+(D)] = 0.50 - 0.80.This potting material can substantially improve the reliability of the PPGA-type semiconductor that uses an organic printed circuit board.DETAILED DESCRIPTION OF THE INVENTIONAt least 50% by weight of the liquid epoxy resin component used in this invention preferably has a viscosity at 25°C of not more than 8Pa-s. If at least 50% by weight of the epoxy resin component is not a lowviscosity epoxy, the viscosity of the composition will increase, tending to entrain gas bubbles or to not completely fill to the corner edges when the PPGA package is potted by allowing the liquid potting material to flow, leading to undesirable decreases in reliability. The method for measuring the viscosity of the epoxy resin involves a measurement using an E-type viscometer (manufactured by Toki Sangyo KK) at 25°C if the sample is liquid at room temperature, and a measurement at 150°C using a high temperature cone plate viscometer if the sample is solid at room temperature.Any epoxy resin can be used as long as it meets the above requirements and these are not particularly limited, but they are specifically, for example, bisphenol-A diglycidyl ether-type epoxy resin, bisphenol-F diglycidyl ether-type epoxy resin, bisphenol-S diglycidyl ether-type epoxy resin,3,3’,5,51-tetramethyl-4,4'-dihydroxybiphenyl diglycidyl ether-type epoxy resin, 1,6-dihydroxynaphthalene diglycidyl ether-type epoxy resin, phenol novolak-type epoxy resin, cresol novolak-type epoxy resin, brominated bisphenol-A diglycidyl ether-type epoxy resin, brominated cresol novolak-type epoxy resin, and the like, which may be used singly or in mixtures thereof.The liquid alkylated diaminodiphenylmethane used in this invention is a diaminodiphenylmethane where 1, 2, or more of the hydrogen atoms of the benzene rings are substituted by an alkyl group such as methyl, ethyl, or the like; having no such alkyl group with 4 or fewer carbon atoms is not preferred because the composition will have a higher viscosity, which tends to entrain gas bubbles or to not completely fill to the corner edges when the package is potted by allowing the liquid potting material to flow in, leading to reduced reliability.Any of alkylated diaminodiphenylmethanes which satisfy the above requirements can be used with no particular limitation and they are specifically, for example, 3,3'-diethyl-4,4'-diaminodiphenylmethane,3,31,5,5'-tetramethyl-4,4'-diaminodiphenylmethane,3,3*,5,5'-tetraethyl-4,4'-diaminodiphenylmethane, and the like, which may be used singly or in mixtures thereof.It is preferred for the compounding ratio of the liquid epoxy resin (A) and liquid alkylated diaminodiphenylmethane (B) by weight to be in the range of (A) / [(A)+(B)] = 0.65 - 0.80. If the ratio (A) / [(A)+(B)] exceeds 0.80, this results in an increased number of unreacted epoxy groups, which decreases the heat resistance such as the glass transition temperature and the like, and which causes an undesirable reduction in reliability in the cold-heat cycle test. On the other hand, a ratio below 0.65 is not preferred due to decreased storage life for the composition.The epoxidized polybutadiene (C) used in this invention preferably has a number average molecular weight of 1,000 to 5,000. It is not preferred for it to be less than 1,000 due to a decreased flexibilizing effect while a level exceeding 5,000 increases the viscosity and decreases the workability, which is not preferable. The epoxy group content (mole% fraction incorporated into the main chain) is preferably 3% to 10%. A mole fraction less than 3% is not preferred because the epoxidized polybutadiene will lack compatibility with the liquid epoxy resin (A), while a level exceeding 10% is not preferred because this will result in epoxy group's cross-linking with a hardening agent, and failing to take on a sea-island structure with no prospect of reducing stress, thereby reducing the flexibilizing effect. Using the epoxidized polybutadiene (C) in the range of a compounding weight ratio of (C) / [(A)+(B)] = 0.01 - 0.05, provides a relaxation effect against thermal stresses, which occur during the cold-heat cycle test. A ratio less than 0.01 is not preferred due to a meager effect of improving stress relaxation, nor is a level exceeding 0.05 preferred, because that will give a cured product with a decreased glass transition temperature, a rise in composition viscosity, and a reduced compatibility, and cause a blooming to the surface of the cured product.The inorganic filler (D) includes fused silica, crystalline silica, and the like. It is available, in general, in spherical form, ruptured form, and the like, but a spherical form filler is most preferred in order to permit incorporating a large amount of filler to reduce the coefficient of linear expansion. It is preferred for the inorganic filler (D) in a weight compounding ratio to be in the range of (D) / [(A)+(B)+(C)+(D)] = 0.50 - 0.80. A level below 0.50 is not preferred because of its small effect of reducing the coefficient of linear expansion, nor is a level exceeding 0.80 preferred, because it will increase the viscosity of the composition, thereby decreasing workability. In general, a small-particle-size filler increases the viscosity of the resin composition, resulting in decreased flow and in gas bubble entrainment and insufficient fillings. On the other hand, a large-particle-size filler tends to undergo a sedimentation, which results in nonuniform filler distribution. The nonuniform filler distribution will give portions of the composition with different coefficients of linear expansion, and top portions having lower amounts of filler tending to experience more crack formation. If the largest particle size is greater than a wire interval, there will be a tendency to insufficiently fill underneath the wires and a short-circuiting problem due to wire distortion.A study of the way to solve the above problems has led to the finding that compounding (a) a spherical silica of an average particle size of 0.1 - 3.0 pm and a maximum particle size not more than 10 pm, and (b) a spherical silica of an average particle size of 4 - 10 pm and a maximum particle size not more than 50 pm at a weight ratio of (a) / (a)+(b)] = 0.05 - 0.50 enables suppression of sedimentation without losing flow characteristics. Any silica which satisfies these requirements can be used without limitations. Each of (a) and (b) may be used singly or in blends of two or more kinds.The particle size distribution and average particle size were measured by a laser-type method (Horiba LA-500), where the average particle size was based on a median size.The liquid potting material of this invention, as needed, in addition to the above essential components may contain other resins, a catalyst for promoting the reaction, a diluent, a pigment, a coupler, a leveling agent, a defoamer, or the like. The liquid potting material is prepared by dispersing and kneading each of these components and additives and the like, using a three-roll mill followed by vacuum-defoaming.EXAMPLES OF THIS INVENTIONThe present invention is now specifically described by the following examples of this invention:Example 1The following ingredients were dispersed and kneaded on a three-roll mill and vacuum-defoamed to give a liquid epoxy resin potting material. The resultant epoxy resin potting material was used to pot a PPGA package, followed by oven-curing for three hours at 165°C to give a semiconductor package. The following methods of evaluation were used to confirm the delamination, if any, between the semiconductor chip and print baseboard; the presence, if any, of cracks; and filler sedimentation, and the results are given in Table 1.• Bisphenol-F-type epoxy resin: 100 parts by weight (Epoxy equivalent 161? viscosity at 25°C, 1.5Pa-s) • 3,3'-diethyl-4,4’-diaminodiphenylmethane: 40 parts by weight • Epoxidized polybutadiene: 6 parts by weight (Number average molecular weight: 1800; epoxy equivalent 250) • Spherical fused silica (1): 340 parts by weight (Average particle size 6 ym; maximum particle size 48 ym) • Spherical fused silica (2): 40 parts by weight (Average particle size 0.5 ym; maximum particle size 2 ym) • Composition viscosity:E-type viscometer, 2.5 rpm, 25°C • Ease of filling into packages:The sample was dispensed into a PPGA package at 80°C to confirm the condition of filling in the cavities 5 minutes later.• Confirming of delamination or cracks (1) Normal conditions (after curing) (2) PCT (pressure cooker test) treatment at 125°C / 2.3 atm for 168 hours (3) T / C (cold-heat cycle test) treatment under -65°C / 30 minutes <—► 150°C / 30 minutes, 1,000 cyclesAfter subjecting the above sample to the above conditions (1), (2) or (3) separately, the delamination between the semiconductor chips and print baseboard and crack formation were confirmed using scanning acoustic tomograph (hereinafter abbreviated as SAT).• Filler sedimentation:A cured package was cut across and observed for the cross-section using a scanning electron microscope (hereinafter abbreviated as SEM) to measure the extent of sedimentation from the top of the cured product.The sample of Example 1 showed no delamination or cracks but slight filler sedimentation, which indicates good reliability. The number of packages used for each evaluation were 10. The results are summarized in Table 1.- 10 Examples 2-6Comparative Examples 1-6Liquid epoxy resin potting materials were obtained in a manner similar to that of Example 1, except for using the compounding recipes shown in Table 1 and Table 2, thereby potting the PPGA package to evaluate the reliability of these samples. The results are given in Tables 1 and 2.The following ingredients were used in Example and other examples:• Bisphenol-F-type epoxy resin: (manufactured by Dainippon Ink Kagaku Kogyo KK, EXA-830LVP, epoxy equivalent 161; viscosity at 25°C 1.5 Pa-s) • Bisphenol-A-type epoxy resin: (1): (manufactured by Dainippon Ink Kagaku Kogyo KK, EXA-850CRP, epoxy equivalent 171; viscosity at 25°C 4.5Pa- s) • Bisphenol-A-type epoxy resin: (2): (manufactured by Yuka Shell Epoxy KK; Epikote 1001, epoxy equivalent 470, solid) • 1,6-dihydroxynaphthalene-type resin: (manufacture by Dainippon Ink Kagaku Kogyo KK, HP-4032D, epoxy equivalent 140, viscosity at 25°C 25 Pa-s) • 3,31-diethyl-4,41-diaminodiphenylmethane; (manufactured by Nippon Kayaku KK, Kayahard A-A) • 3,3'-5,5'-tetramethyl-4,4'-diaminodiphenylmethane; (manufactured by Nippon Kayaku K.K., Kayabond C-200) • Epoxidized polybutadiene: (manufactured by Nippon Sekiyu Kagaku KK, E-1800-6.5, number average molecular weight 1800, epoxy equivalent 250) • Spherical fused silica (1): {manufactured by Denki Kgaku Kogyo KK, FB-30, average particle size 6 pm, maximum particle size 48 pm) · Spherical fused silica (2)s (manufactured by AdmatexKK, SO-25R, average particle size 0.5 pm, maximum particle size 2 pm) • Spherical fused silica (3): (manufactured by Admatex KK, SO-32R, average particle size 2.0 pm, maximum particle size 8 pm) • Spherical fused silica (4): (a blend [weight ratio 1:1] of the above spherical fused silicas (2) and (3)? average particle size 1.0 pm, maximum particle size 8 pm) · Spherical fused silica {5): {manufactured by DenkiKagaku Kogyo KK, FB-25S, average particle size 17.0 pm, maximum particle size 75 pm)TABLE 1Examples 1 2 3 4 5 6 Compounding (parts by weight) Bisphenol- resin •F-type epoxy 100 100 100 100 50 Bisphenolresin (1) •A-type epoxy 100 1,6-dihydroxynaphthalene-type epoxy resin 50 3,3'-diethyl-4,4'diaminodiphenyImethane 40 40 40 37 32 43 3,3'-5,5'-tetramethyl4, 4 ’ -diaminodiphenylmethane 5 Epoxidized polybutadiene 6 6 6 6 6 6 Spherical (1) fused silica 340 230 230 340 300 260 Spherical (2) fused silica 40 160 40 110 Spherical (3) fused silica 80 Spherical (4) fused silica 160 Physical Properties Composition viscosity (Pa-s) 20 17 18 30 19 35 Ease of package filling good good good good good good Delamina- After Curing 0 0 0 0 0 0 tion After PCT 0 0 0 0 0 0 After T / C 0 0 0 0 0 0 Cracks After Curing After PCT 0 0 0 0 0 0 0 0 0 0 0 0 After T / C 0 0 0 0 0 0 Filler sedimentation (pm) 24 Not more than 3 Not more than 3 20 10 5TABLE 2Comparative Examples 1 2 3 4 5 6 Compounding (parts by weight) Bisphenol- resin F-type epoxy 100 100 100 100 100 30 Bisphenolresin (2) •A-type epoxy 70 3,3’-diethyl-4, 4 ' diaminodiphenylmethane 40 40 40 40 40 40 Epoxidized polybutadiene 6 6 6 6 6 Spherical (1) fused silica 380 420 230 110 340 Spherical (2) fused silica 280 160 260 40 Spherical (5) fused silica 380 ! Physical Properties Composition viscosity (Pa-s) 30 120 17 130 27 125 Ease of package filling good poor good poor good poor Delamina- After Curing 0 - 0 - 0 - tion After PCT 0 - 8 - 0 - After T / C 3 - 0 - 4 - Cracks After Curing After PCT 0 0 — 0 3 0 0 After T / C 5 - 0 - 8 - Filler sedimentation (pm) 80 - Not more than 3 - 100 -As illustrated in the above Examples 1-6, potting a semiconductor package with a liquid potting material of this invention can provide a highly reliable semiconductor package free of delamination or cracks in a pressure cooker test or cold-heat cycle test without adversely affecting flow or workability, thereby providing much industrial advantage.
Claims
Claims:
1. A liquid epoxy resin potting material comprising (A) one or more liquid epoxy resins, (B) a liquid alkylated diaminodiphenylmethane, (C) an epoxidized polybutadiene, and (D) an inorganic filler, wherein the ratios of the 5 individual components in weight ratios are: (A) / [(A) + (B) = 0.65-0.80 and (D) / [(A) + (B) + (C) + (D)] = 0.50-0.80 characterized in that 10 (C) / [(A) + (B)] = 0.01-0.05, whereby a relaxation effect against thermal stresses is produced.
2. A liquid epoxy resin potting material, as claimed in claim 1, wherein at least 50% by weight of component (A) comprises a liquid epoxy resin having a viscosity not higher than 8Pa-s / 25°C.
153. A liquid epoxy resin potting material, as claimed in claim 1, wherein the (D) inorganic filler comprises (a) a spherical silica having an average particle size of 0.1 pm to 3.0 pm and a maximum particle size not more than 10 pm and (b) a spherical silica of an average particle size of 4 pm to 10 pm and a maximum particle size of not more than 50 pm, with the compounding ratio in 20 weight being (a) / [(a) + (b) = 0.05-0.50.
4. A liquid epoxy resin potting material, as set forth in claim 2, wherein the (D) inorganic filler comprises (a) a spherical silica having an average particle size of 0.1 pm to 3.0 pm and a maximum particle size not more than 10 pm and (b) a spherical silica of an average particle size of 4 pm to 10 pm and a 25 maximum particle size of not more than 50 pm, with the compounding ratio in weight being (a) / [(a) = (b)] = 0.05-0.50.