Strip shaped composite material and process for making it

MYPI1997005740A0Inactive Publication Date: 1998-06-19WIELAND WERKE AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1997005740
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Filing Date
1997-11-28
Publication Date
1998-06-19
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Strip composite materials with tin coatings suffer from surface oxidation, leading to inadequate contact resistance under mechanical stress and poor wear and corrosion resistance, especially in applications like plug connectors.

Method used

Embedding 1 to 50 atomic percent carbon into the tin coating's outer surface region to a thickness of approximately 2 μm, followed by a hot oil bath treatment and subsequent quenching in a cold oil bath, enhances friction behavior, corrosion resistance, and maintains constant contact transfer resistance.

Benefits of technology

The carbon-embedded tin coating reduces plugging and pulling forces by 20% to 75%, significantly improves corrosion resistance, and ensures a stable contact resistance over the lifespan of components like plug connectors.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

THE INVENTION RELATES TO A STRIP COMPOSITE MATERIAL (1) WITH A BASE MATERIAL OF A METAL OR A METAL ALLOY AND A TIN COATING ON THE SURFACE, WHEREBY AN INTERMETALLIC PHASE (IMP) IS CONSTRUCTED BETWEEN BOTH MATERIALS. IN PARTICULAR FOR ACHIEVING GOOD WEAR AND CORROSION RESISTANCE OF THE COMPOSITE MATERIAL (1) WITH A SIMULTANEOUSLY OXIDE-FREE SURFACE, 1 TO 50 AT.-%, PREFERABLY 6 TO 30 AT.-%, CARBON (C) ARE EMBEDDED IN AN OUTER SURFACE REGION OF THE TIN COATING UP TO A THICKNESS D OF APPROXIMATELY 2 ?M.A METHOD (OIL TREATMENT) AND APPARATUS FOR THE MANUFACTURE OF THE COMPOSITE MATERIAL OF THE INVENTION ARE ALSO DISCLOSED.(FIG 1)
Need to check novelty before this filing date? Find Prior Art

Description

Strip shaped composite material and process for making itThe invention relates to a strip composite material according to the preamble of Claim 1.A specific adjustment of the thickness of the intermetallic phase (IMP) occurs in hot-tinned strips through a subsequent heat treatment in hood-type, through-type, or suspended-conveyor furnaces at temperatures between 150°C to 180°C and annealing times, for example, in hood-type furnaces of about 16 h. In galvanically tinned strips there takes place an additional reflow treatment with IR-radiation or hot air in order to achieve through a remelting of the tin a better soldering ability and / or a better adhesive ability of the tin on the base material. However, the surface is in both cases lightly oxidized or not protected against further oxidation so that a permanent low contact resistance even under mechanical stress is not guaranteed.The basic purpose of the invention is to provide a strip composite material of the mentioned type with an oxide-free surface and which has a good wear and corrosion resistance.This purpose is surprisingly attained by embedding 1 to 50 At.-% carbon (C), preferably 6 to 30 At.-% C, in an outer surface region of the tin coating up to a thickness D of approximately 2 μτη (At.-% = atomic weight-%) .The embedding of carbon into the Sn layer results; in an improvement of the friction behavior, namely, in plug connectors, in the reduction of the plugging and pulling force, in the improvement of the corrosion resistance, in particular the resistance to fretting corrosion, and thus in the guarantee of a constant contact transfer resistance during the life of, for example, plug connectors. The oil csrmot be removed, for example, through an ultrasound treatment in acetone. However,Miu u .HlI'm ii-7i n —πττητ·I2ithers exist no cxidic binding atructurcs cf cha main elements.The base material consists preferably of copper cr a coppery alloy, of iron cr ar. iron alloy, of nickel or a ''nickel? alloy, of zinc or a zinc alloy.A,method for the manufacture of the composite material of the invention is characterized in such a manner.that the tinned base material is pulled through a hot oil bath for a duration of 1 rain, to 130 min., which oil bath contains an oil on a paraffin and / or ester and / or^fatty acid base, both of a natural and also synthetic origin vith common additives, a-d the temperature T of which oil bath lias above the r.eiting point of the respective tinning. The hot oil bath contains preferably a paraffin oil or paraffir.-basad solvent raffinates and ia free of chlorine or ?C3, The temperature lies above the melting point of the respective tinning: in the caee of pure tin thus preferably at 24C“C, in the case cf Snib at 200°C, in the case of' SnAgO, 5Sbl at 25C*C. The duration is preferably 2 min. to 4 siln.The Intermetallic phase (1WP) is adjusted depending on the layer thickness and temperature / time treatment to 104 to 100% of the entire tin layer thickness. The Sn surface: shows then a high-gloss surface, which is corrosion-resistant, in particular, however, xrictioncorroeiba-resistant. The static contact resistance does not change with the oil treatment, The friction forces are reduced through this by 20% to 75%.It!is furthermore advisable to quench the composite material immediately after the oil treatment in a cold oil bath on a paraffin, and / or ester ar.d / or fatty acid base, both of * natural and also synthetic origin with the usual additives, at a temperature of SeC to 5CeC, in particular at 30eC to 30aC. The C content in the Sn layer is furthermore increased by this quenching. The duration of the composite material in the cold oil bath is preferably 2 min. to 10 min.According to a further modification of the invention, oil on a paraffin and / or ester and / or fatty acid base, both of a natural and also synthetic origin with the usual additives, is sprayed directly after the tinning of the base material onto the still hot tin coating. The oil is hereby not too tightly bound” to the tinning, however, compared with the non-treated tinning positive influences, in particular with respect to the friction corrosion, can be measured.The invention will be discussed in greater detail in connection with the following exemplary embodiment:The figure (Figure 1) shows schematically the sequence of the 15 heat treatment of tinned strips 1 in a hot oil 2 of a hot-oil part 3 with a subsequent quenching in cold oil 4 of a cold-oil part 5, whereby the strip 1 is guided cold from an unwinding device 6 (not illustrated in detail) through guide rollers 7 and a lock 8 into the hot oil.bath 2 heated to 190°C to 270°C. The oil-bath temperature must thereby lie above the melting point of the respective tinning. When the strip 1 is inductively brought up to temperature and moves then into the oil bath 2, there exists the danger of the formation of decrosslinkings and of the bone-shaped effect.A smoke exhaust 9 is integrated at the highest point of the hot-oil part 3.The strip 1 moves through a thermal lock 10 and around a guide roller 11 into a cooled oil bath 4 with a temperature of 5°C to 50°C, preferably 10°C to 30°C, for quenching without air supply. When emerging from the oil bath 4, the excessive oil is wiped off by exhaust nozzles 12 or squeezing rollers, and the strip 1, guided by a guide roller 13, is wound up (onto a winding-up device 14PI 9705740 not ..illustrated in detail) . The hot oil 2 is circulated by a circulation system having an integrated heating device. The cold .oil 4 is circulated by a further circulation system having an integrated return-cooling device. The drain 15 is used only for servicing purposes .Numerical Example:A CuSn6-bronze strip with the dimension 0.63 mm x 80 mm was hot-tinned with pure tin (layer thickness approximately 1.8 mm) and subsequently oil-treated in a bath of commercially available, paraffin-based solvent raffinate (the respective treatment parameters are listed in Column I of the following table).1 II III IV Treatment (A11 = Quenching) Layer Thickness RFA Lum] Coul (VS / RS) (VS / RS) C-content in At.-% 0 —* 2 pm Depth Fretting Corrosion [mO / cycles] Initial State 1.5 / 1.7 1.1 / 1.5 0.7% - 0% 1000 / 1250 195°C / 1 min 195°C / 4 min A'·’ 1.5 / 1.7 0.8 / 1.3 1.5 / 1.8 0.8 / 0.7 6% - 0.8% 1 % - 0.6% 1000 / 2080 1000 / 1850 250°C / 4 min 250°C / 4 min A'·’ 1.4 / 1.8 n.n.2’ / 0.2 1.4 / 1.8 π.πΛ' / η.π.’·’ 10% - 0.1 % 25.8% - 0.1% 3.8 / 5000 2.6 / 5000 n.n.2'1 = Cannot be proven ..PI 97057404, .... □ ........................Column IX of tie table lists the *«yex ckr*?s on <&eh of the front side (vs) and the beck side £XS) of c*ic strip. The layer thickness, which is measured by means, of ^adiograph-fl-corescance-analysis CRPA), is thereby the entire thickness of the free SU layer and of the intermetallic phase (ZM?), whereas the coulcmetricaily measured layer thicfeess relates only to the free Sr. layer- Th· difference thus results in the thicJcteee of the 1X5.Column XIX of the table lists the C content, which is measured by meaa* of .auger-siectron-spectrcsccpy ·.(ABS) )&nd eeccndary-ion-ajass-flpectroscopY (sires) .Column IV of the table lists the fretting corrosion tendency, measured in accordance with the so-called ’ridef-ca-flat’' oethod (contact resistance ir. after n cycles' at 1 N contact force and 25 μχ amplitude) .Either the number of cycles is thereby disclosed, after which a contact resistance of 1000 mn ie reached, or if 100D m3 is not reached - the measuring is stepped after 5000 cycles.Using the table, it is stated that through an oil treatment at 195°C compared with the initial, state indeed^ a slight improvement with respect to the construction of the IMP and the fretting corrosion tendency is achieved, however, a significant shortening of the j up to now ccrrroon times for adjusting the IM? is achieved only through the oil treatment of the invention at 250*C (a free Sn layer can co longer be detected according to Column ΣΣ).The fretting corrosion tendency is at the same time considerably reduced with an increasing carbon content.

Claims

Claims 1. Strip-shaped composite material (1) having a base material of metal or a metal alloy and having a surface coating of pure tin or a tin alloy which is applied by electroplating or by melt tin-plating, an intermetallic phase (IMP) 5 being formed between the two materials, characterised in that from 1 to 50 atomic weight % of carbon (C) is incorporated in an outer edge portion of the tin coating up to a thickness D of approximately 2 pm.

2. Composite material (1) according to claim 1, characterised in that from 6 to 30 atomic weight % of C is incorporated.

103. Composite material (1) according to claim 1 or 2, characterised in that the base material comprises copper or a copper alloy, iron or an iron alloy, nickel or a nickel alloy, zinc or a zinc alloy.

4. Process for the manufacture of the composite material (1) according to one or more of claims 1 to 3, characterised in that the tin-plated base material 15 is pulled, with a residence time of from 1 to 130 minutes, through a hot oil bath (3) which contains an oil based on paraffin and / or ester and / or fatty acid, of both natural and synthetic origin with conventional additives, and the temperature T of which is above the melting point of the tin plating. PI 970057405. Process according to claim 4, characterised in that the residence time is from 2 to 4 minutes.

6. Process according to claim 4 or 5, characterised in that the composite material (1), immediately after the oil treatment, is quenched at a temperature 5 of from 5 to 50°C in a cold oil bath (5) based on paraffin and / or ester and / or fatty acid, of both natural and synthetic origin with conventional additives.

7. Process according to claim 6, characterised in that quenching is carried out at a temperature of from 10 to 30°C.

8. Process according to claim 6 or 7, characterised in that the residence 10 time of the composite material (1) in the cold oil bath (5) is from 2 to 10 minutes. PI 970057409. Process for the manufacture of the composite profile according to one: or more of claims 1 to 3, characterised in that oil based on paraffin and / or ester and / or fatty acid, of both natural and synthetic origin with conventional additives, is sprayed onto the still-hot tin coating directly after the tin-plating 5 of the base material.