Gas phase polymerization process

MYPI1998000292A0Inactive Publication Date: 1998-07-24INEOS SALES (UK) LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1998000292
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1997-01-24
Filing Date
1998-01-23
Publication Date
1998-07-24
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional gas phase polymerization in fluidized-bed reactors face limitations in output efficiency due to heat removal rates and excessive entrainment of polymer particles, leading to reduced production rates and reactor fouling.

Method used

The process involves maintaining a fluidized bed that occupies at least the entire first volume of the reactor, with a disengagement vessel, allowing the bed to extend to the full height of the reactor, which decelerates particles and reduces bubble size, thereby increasing output without excessive particle entrainment and minimizing reactor fouling.

Benefits of technology

This approach significantly increases polymer output rates, reduces reactor fouling, and allows for higher upward gas speeds, enabling more efficient and reliable operation without the need for design changes, while maintaining polymer quality.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

THE PRESENT INVENTION RELATES TO A PROCESS FOR CONTINUOUS GAS PHASE POLYMERIZATION OF OLEFIN(S) IN A REACTOR CONTAINING A FLUIDIZED BED, CONSISTING OF A CYLINDER WITH A VERTICAL SIDE WALL AND OF A DESURGING OR DISENGAGEMENT CHAMBER (3) MOUNTED ABOVE THE SAID CYLINDER1 CHARACTERIZED IN THAT THE ILUIDIZED BED OCCUPIES AT LEAST ALL OF THE CYLINDER WITH A VERTICAL SIDE WALL OF THE REACTOR.
Need to check novelty before this filing date? Find Prior Art

Description

GAS PHASE POLYMERIZATION PROCESSThe present invention relates to a process for gas phase polymerization in a fluidized-bed reactorIt is known to polymerize one or more monomers in the gas phase at a pressure higher than atmospheric pressure in a fluidized-bed reactor where panicles of polymer being formed are maintained in the fluidized state by virtue of a reaction gas mixture containing the monomer(s) to be polymerized travelling in a rising stream. The polymer thus manufactured in powder form is generally drained from the reactor in order to keep the bed at a more or less constant volume. A process which is preferred on the industrial scale employs a fluidization grid which distributes the reaction gas mixture through the bed and which acts as a support for the bed in the event of a cut in the flow ofthe rising gas The reaction gas mixture leaving at the top of the tluidized-bed reactor is recycled to the base of the latter under the fluidization grid by means of an external circulation conduit provided with a compressoiThe polymerization ofthe monomers is an exothermic reaction. It is therefore necessary to provide a suitable means for cooling the bed in order to extract the heat of polymerization theiefrom. The preferred method for the polymerization of olefins in a fluidized bed consists in cooling the reaction gas mixture below the polymerization temperature, and, when this fluidization gas passes through the bed, this makes it possible to compensate for the excess heat generated by the polymei ization. Thus, as it is being returned, the reaction gas mixture is geneially cooled with the aid ol at least one heat exchanger arranged on the outer circulation conduit so as to lemove the heat produced by the polymei ization leaction and io keep the polymei ization temperature al the desired5 levelAttempts have been made, very pailicularly in recent years, to optimize the gas phase polymerization process so as to increase the output of polymer in existing plants The thinking has accordingly been in terms of rate of production of polymer, namely in terms of weight yield of polymer produced per unit volume of the reactor and per unit of lime (kg / li / m*'). In commercial fluidized-bed reactors of the abovementioned type it is known that the output rate depends directly on the rate of removal of heat generated in the reactor This rate of removal can be increased, for example by increasing the speed of the fluidizing gas and / or by reducing the temperature of the fluidizing gas and / or by increasing the heat capacity of the fluidizing gasFor example, in its patent application WO 94 / 28032 BP Chemicals Limited has proposed a process for gas phase polymerization of olefin(s), in which the recycle gas stream is cooled to a sufficient temperature to form a liquid and a gas. By separating the liquid from the gas and bv introducing the liquid directly into the fluidized bed it is possible to increase the total quantity of liquid introduced into the fluidized-bed reactor, and this makes it possible to cool the bed better by evaporation and hence to ι each higher output efficiency levelsIn general, fluidized-bed reactors according to the present invention can be represented by a first volume, the enclosure (wall) of which consists of at least one surface of revolution generated by the rotation about a vertical axis known as axis of revolution, of a rectilinear and / or curved segment, above which is mounted a second volume, commonly called a disengagement vessel, the enclosure (wall) of which also consists of at least one surface of revolution generated by the rotation, about the same vertical axis known as axis of revolution, of a rectilinear and / or curved segment According to its definition of disengagement vessel, the orthogonal section of the second volume (at the location situated just above the junction between the twii volumes} is higher than the orthogonal section of the first volume (at the location situated at its upper point).Conventional fluidized-bed reactors employed for the gas phase polymerization of olefin(s) usually consist of a cylinder (I) with a vertical axis above which is mounted a disengagement vessel (3) in accordance with Figure 1, which shows diagrammatically a preferred apparatus for the gas phase polymerization according to the present invention.The known essential function of the disengagement vessel is to slow down the rising gas stream which, aftei having passed through the fluidized bed, can entrain relatively large quanlilies of solid panicles As a result, most of the entrained solid particles return directly into the fluidized bed. Only the finest particles can be entrained out of the rectorIn principle, the fluidized bed could occupy all of the cylindrical part of the reactor, a part which rises over a height H starting from the base of the fluidized bed, which generally coincides with the fluidization grid (4). In practice the fluidized bed generally occupies only a portion of the cylindrical part of the fluidized-bed reactor, with the result that the real height of the fluidized bed (h) is equivalent to 0.95 x H, preferably 0 90 x H, and in particular 0.85 x H This height limit of the fluidized bed has been dictated bv the person skilled in the art in order to avoid excessive entrainment of polymer panicles out of the reactor Studies of fluidization have shown the formation of bubbles within the fluidized bed. Coalescence of the bubbles takes place as they use within the bed until they burst when they reach the upper pan of the fluidized bed. This bursting considerably accelerates the entrainment of the panicles out of the reactor. All this has therefore naturally led the person skilled in the an to limit the height of the fluidized bed in a practical manner during the polymerization.Within the context of research related to the increase in the output efficiency of its industrial plants foi gas phase polymerization of olefins, the Applicant Company has succeeded, despite existing prejudices, in developing a simple and reliable process which makes it possible to increase considerably the output of polymers In addition, the Applicant Company has completely unexpectedly discovered that the use of its new process offers many advantages as disclosed in the description which followsThe present invention consists therefore of a process for gas phase polymerization in a fluidized-bed reactor consisting of a first volume, the enclosure (wall) of which consists of at least one surface of revolution generated by the rotation, about a vertical axis known as axis of revolution, of a rectilinear and / or curved segment, above which is mounted a second volume, commonly called a disengagement vessel, adjoining the first volume, the enclosure (wall) of which also consists of at least one surface of evolution generated by the rotation, about the same vertical axis known as axis of (evolution, of a rectilinear and / or curved segmenr, characterized in that (tic fluidized bed occupies at least ail of the first volume of die reactoi Thus, according to the piesent invention the height of the fluidized bed (h) is al least equal to the height H of ihe polymerization teactoi The fluidized bed preferably occupies at least partially the second volume known as a disengagement vessel.Unexpectedly, the Applicant Company has discovered that the process according to the present invention does not in any way lead to excessive entrainment of polymer particles out of the reactor. Although not wishing to be bound to the following explanation, the Applicant Company thinks that this finding originates, on the one hand, from the fact that the particles undergo a deceleration when they reach the disengagement vessel and, on the other hand, because the bubbles are limited and / or reduced in size when they enter the disengagement vesselAlthough not wishing to be limited to one type of polymerization in pamculai, the present invention is particularly appropriate for reactions of polymerization of one or more monomers such as olefins, polar vinyl monomers, dienes, acetylenes and aldehydesThe process according to the present invention preferably applies to the polymerization of one oi more olefmic monomeis such as ethylene, propylene. 1butene. 1-pentene, 4-methyl-1-pentene. I-hexene and I-octeneAccording to the present invention it is possible to decide to polymerize intermittently with a bed height in accordance with the present invention and with a bed height lower than that of the invention However, it is preferable to perform the polymerization with a hed height constantly within the range of the present inventionAs indicated above, the height H of the polymei ization reactor is defined as being the distance separating the base of the fluidized bed, a base which generally coincides with the fluidization grid, and the junction between the first volume or lower volume and the second volume called a disengagement vessel. In the preferred case of the cylinder with a vertical axis, H therefore represents the length of the vertical side wall of tile cylinder rising above the base of the fluidized bed.According to a preferred embodiment of the present invention the height of the fluidized bed (h) is greater than the height H of the reactor, preferably greater than 1.05 χ H and in particular gieatei than I I x HThe disengagement vessel mounted above the cylinder liable to contain the fluidized bed has, in principle a cross-section which is greater than that of the cylinder It is preferably in the shape of a bulb consisting essentially of a conical frustum of revolution with a veiiical axis coinciding with the axis of the cylindei.with apex pointing downwards with preferably an angle of between 10° and 60° and with a dome of substantially hemispherical shape mounted above it. The small base of this conical frustum coincides with the upper end of the cylinder of the reactor, and its large base coincides with the base ofthe dome. It can also consist of a vertical cylinder which is joined to the cylinder liable to contain the fluidized bed by a joining surface in the shape of a widened conduit. In this case this cylinder has a vertical axis coinciding with the axis ofthe cylinder liable to contain the fluidized bed and a roof generally of substantially hemispherical shape.According to a preferred embodiment of the present invention the height of the fluidized bed (h) is such that the volume ofthe disengagement vessel occupied by the fluidized bed represents more than 5% of the total volume of the vessel, preferably more than 10%, more preferably more than 15%.According to a preferred embodiment ofthe present invention the height of the fluidized bed (h) is such that the volume ofthe disengagement vessel occupied by the fluidized bed represents less than 70% ofthe total volume of the vessel, preferably less than 50%, moie preferably less than 30%.In the case ofthe vessel consisting ofthe conical frustum of revolution with a dome mounted above ii, the upper limit ofthe fluidized bed (h) preferably does not reach the height which corresponds to the largest orthogonal section of the said vessel. This limiting height which it is preferable not to exceed is identified by Lrin Figure 2The presence of the fines m the reactor can affect the properties of the polymer by increasing the gel content ofthe finished product such as the films and receptacles made of plastic In addition, during the polymerization, agglomerates can form on the internal wall of the reactor, in particular on the wall of the disengagement vessel. The accumulation ofthe fines and agglomerates on the wall ofthe reactor constitute the fouling of the reactorTo prevent the fouling of the reactor from affecting the operation of the polymerization system and the quality ofthe polymer produced, the reactor is stopped at regular intervals in order to clean its wall and to remove the agglomerates from it This can be done bv means of water or nitrogen under pressure Cleaning of this type causes entries of poison into the reactor, and this automatically involves a purge ofthe i eactor and drying in order to remove these poisons This procedure takes time and is not very economicalUnexpectedly. the Applicant Company has also discovered that the process according to the present invention makes it possible to reduce and / or to eliminate the problems linked with the fouling ofthe reactor wall, in particular ofthe wall of the disengagement vesselFigure 2 shows diagrammatically an illustration of a plant for gas phase polymerization of olefm(s) according to the present invention. The apparatus includes (i) a fluidized-bed reactor (1) provided with a dome (2) and with a base comprising a fluidization grid (4) and consisting of a cylinder with a vertical side wall above which is mounted a desurging or disengagement chamber (3) mounted above the said cylinder, the top of the chamber (3) forming the dome (2) ofthe leactoi, (ii) an entry chamber (9) for a reaction gas mixture, situated under the grid (4) and communicating with the cylindrical part of the reactor (I) through the grid (4), and (iii) an outer conduit (5) for circulation ofthe reaction gas mixture, joining the dome (2) ofthe reactor to the entry chamber (9) for the reaction gas mixture, and including a compressor (8) and at least one heat exchanger (6,7)One or more feed conduits (10) for constituents ofthe reaction gas mixture, such as one or more olefins, for example ethylene or propylene or C4-C10 alpha-olefins, one or more, preferably unconjugated, dienes, hydrogen, one or several inert gases such as nitiogen or (d-C,,, preferably C2-C5 alkanes, can emerge into the outer circulation conduit (5), in one or more places along this conduit.Another subject ofthe present invention is a process for continuous gas phase polymerization of oletin(s) in a reactor containing a fluidized and optionally mechanically stirred bed, consisting of a cy lindei with a vertical side wall and of a desurging 01 disengagement chamber (3) mounted above the said cylinder, at an absolute pressure higliei than the atmospheric pressure, by continuous or intermittent introduction of a catalyst into the reactor, continuous introduction of olefin(s) into a reaction gas mixture passing through the reactor in an upward stream, removal ofthe heat of polymerization by cooling the recycled reaction gas mixture, draining the polymer manufactured, a process characterized in that the fluidized bed occupies at least all of the cylindei with a vertical side wall ofthe react 01 The Hindi zed bed accoidingly pieteiablv occupies at least partially the said disengagement vessel.The process of the invention is very particularly suitable for polyolefin powders, especially of high or low linear density polyethylene, for example of relative density ranging from 0 87 to 0.97, or of polypropylene. The polymers manufactured according to the present process may especially be powders corresponding essentially to type B and sometimes to types A and B, according to the classification given by D Geldart “Gas Fluidization Technology” published intLA. Wiley-lnterscience Publication” by John-Wiley & Sons (1986), pages 33 to 46. The polymers may consist of particles which have a mass-average diameter ranging from 300 to 2000, preferably from 500 to 1500 μ in.The process for continuous gas phase polymerization of olefm(s) is usually carried out in a reactoi containing a fluidized and optionally mechanically stirred bed, kept at an absolute pressure Pj which can range from 0.5 to 6, preferably from I to 4 MPa The temperature of the fluidized bed may be maintained at a value lower than the melting point of the polymer, for example at a temperature ranging from 30 to 13O°C, preferably from 50 to I IO°C. A reaction gas mixture passes through the reactor with an upward speed which can range from 0 3 to I m / s, preferably from 0.4 to 0 8 m / s. The reaction gas mixture may contain one or more olefins, especially from C2to pjii, preferably from C2to C8, for example ethylene or propylene, oi a mixture of ethylene with at least one (\-Cm, preferably C\-Cs olefin, for example propylene, I-butene, I-hexene, 4-methyl-1-pentene or 1octene, and / or also with at least one diene, for example an unconjugated diene It may also contain hydrogen and An an inert gas such as nitrogen or an alkane, for example from C] to C(l. preferably from C2to Cs, foi example pentane and / or isopentane. The polymerization piocess may in particular be carried out according to the process described in PCT Patent Application No 94 / 28032. It may be carried out in the presence of a catalyst comprising at least one transition metal belonging to groups 4, 5 or 6 of the Periodic Classification of the Elements (approved by the Nomenclature Committee of the American Chemical Society, see “Encyclopaedia of Inoiganie Chemistry, editor R Bruce King, published bv John Wiley & Sons (1904)) In paiticular, it is possible to employ a catalyst system of the Ziegler-Nalta type including a solid catalyst comprising a compound of a transition metal such as those mentioned above and a cocatalyst comprising an organometallic compound of a metal belonging ro groups 1, 2 or 3 of the Periodic Classification of the Elements, for example an organoaluminiuiri compound High7S activity catalyst systems have already been known for many years and are capable of producing large quantities of polymer in a relatively short time, with the result that it is possible to avoid the stage of removal of the catalyst residues present in the polymer These high-activity catalyst systems generally include a solid catalyst comprising essentially transition metal, magnesium and halogen atoms. It is also possible to employ a high-activity catalyst essentially comprising a chromium oxide activated by a heat treatment and associated with a granular support based on refractory oxide. The polymerization process is very particularly suitable for being employed with metallocene catalysts such as zirconocene, hafnocene, titanocene or chromocene, or silica-supported Ziegler catalysts based, for example, on titanium or vanadium For example, the metallocene catalysts can be represented by the general formula (Cp)mMRxR ly in which Cp denotes a substituted or unsubstituted eyclopentadienyl ring, M denotes a transition metal of group IV, V or VI of the Periodic Classification of the Elements, such as zirconium, titanium or hafnium, R and R I being identical or different. denote a hydrocarbon radical containing from 1 to 20 carbon atoms, a halogen atom or another monovalent ligand, m = 1 to 3, x = 0 to 3 and y ' 0 to 3, on condition that the sum of m, x and y is equal to the oxidation state of M. Examples of catalyst of metallocene type are found in EP0129368, US5324800 and EP-0206794. The catalyst may also be a catalyst represented by a compound containing a monocyclopentadienyl heteroatom. Such a catalyst is disclosed, for example, in EP-04 1681 5 and EP-0420436 Catalysts of Ziegler-Natta type, especially high-activity catalysts and in particular catalysts of metallocene type, are preferably employed on a porous support such as a refractory oxide, for example silica or aluminaThe abovementioned catalysts or catalyst systems can be employed as they are directly in the fluidized-bed reactor, oi converted beforehand to olefin prepolymer, in particular dur ing a prepolymerization bringing the catalyst or catalyst system into contact with one or more olefins such as those mentioned above, in a hydrocarbon liquid medium or in gaseous phase, according, for example, to a noncontinuous or continuous process carried out outside the fluidized-bed polymerization reactor.According to a preferred embodiment it has been found that the present invention is very particularly suitable when the polymer output rate is higher than 50 kg / h / m , preferably higliei than 60 kg / h / nv', more preferably higher than 70 kg / h / m\ this being whutevei the catalyst system employed.The process is very particularly suitable for manufacturing polyolefins in powder form, in particular of high or low linear density polyethylene, with a relative density ranging, for example, from 0.87 to 0.97, or of polypropylene, or of copolymers of propylene with ethylene and / or C'j-Cg olefins, or elastomeric copolymers of propylene with ethylene and optionally at least one unconjugated diene with a relative density ranging, for example, from 0.85 to 0 87.The advantages of the process according to the invention are numerous. In fact, the process is not merely simple, reliable and easy to operate but it also makes it possible to increase considerably the output of polymers.By virtue of the new process it is now possible to debottleneck the existing plants easily and less expensively without changing their designIn addition, unexpectedly, the Applicant Company has discovered that the process according to the present invention reduces the entrainment of polymer particles out of the reactor. This improvement results in a new advantage of the present process, by virtue of which it is now possible to work with upward speeds of the reaction gas mixture which are higher than those which were employed previouslyThe examples which follow illustrate the present invention.ExamplesA gas phase copolymerization of ethylene with I-butene is carried out in an apparatus identical with that shown diagrammatically in Figure 2.The fluidized-bed reactor consists therefore of a cylinder with a vertical side wall having mounted above it a desiuging or disengagement chamber (3) mounted above the said cylinder It has the following characteristics:internal diameter of the cylinder (1) . 5 m- height H of the cylinder : 20 m- volume of the cylinder 393 m'- internal diameter of the disengagement chamber (3) at the height Lp 8 66 in- height Lp 28 61 m height of the disengagement vessel I 2.94 in total volume of the disengagement vessel 403 m'- volume of the disengagement vessel under the height Lp 338 nr' volume of the disengagement vessel above the height Lp (dome) 65 m'Al its base the reactor lias a fluidization grid (4) above which is fluidized a bed of copolymer of ethylene and of I -huiene which has a relative density ofO.950, in the form of a powder consisting of particles which have a mass-average diameter of 750 μιη, 90% by weight of the particles having a diameter ranging from 300 to 1200 μ in. The apparent density of the fluidized powder is 300 kg / m3.The reaction gas mixture passes through the fluidized bed at an absolute pressure of 2 Mpa with an upward speed of 0.6 ιτι / s, at a temperature of92°C. It contains, by volume, 30% of ethylene, 1% of I-butene, 25% of hydrogen and 44% of nitrogenA catalyst of the Ziegler-Natta type comprising titanium, magnesium and halogen atoms is prepared in the form of a prepolymer in a manner identical with example 1 of French Patent No 2 405 961 It is introduced intermittently into the reactor via the entry line (I I)Example ClAfter a starting-up stage in winch the bed is raised progressively, the bed is stabilized at the height of 17 m, which corresponds to a fluidized bed volume of 334 in'In these conditions 2 1 5 lonnes / hour (output i ate: 64 kg / h / in') of copolymer of ethylene and I -butene are manufactuied in the form of a powder which has the characteristics mentioned aboveThe polymer output is next increased piogressively by changing from 21.5 to 33.2 tonnes / hour over a period of S hours while the fluidized bed volume and hence this fluidized bed height of 17 m are kept constant. The appearance of hot spots is then observed, and the production of crusts, which results in stoppage of the reactorThe only means of avoiding the agglomerates is to limit the output of polymer to approximately 23 toiines / lnnii (output rate 69 kg / h / m')Example 2After a starting-up stage in which the bed is raised progressively, the bed is stabilized at a height of 29 m, which corresponds to a fluidized bed volume of 393 m'In these conditions 25 lonnes / hour (output rate 64 kg / h / m*') of copolymer of ethylene and 1-butene are manufactured in the form of a powder which has the characteristics mentioned aboveIn contrast to the legitimate tea is which there may have been in respect of entrainment of the particles out of the ieactor, no fouling problem was thus obtained Not even the leasl inciease in concent ration of fine particles has been observed in the outei circulation amduit (5), when compared with Example CIThe polymer output is next increased progressively changing from 25 to 39 tonnes / hour over a period of 8 hours while the fluidized bed volume and hence this fluidized bed height of 20 m are kept constant The appearance of agglomerates is then observed, which makes it necessary to limit the polymer output to approximately 29 tonnes / hour (output rate : 74 kg / h / trf).Example 3After a starting-up stage in which the bed is raised progressively, the bed is stabilized at a height of 23 m, that is 3 m in the disengagement vessel, which corresponds to a fluidized bed volume of 468 m ’. that is a volume of occupation of the disengagement vessel of 75 m\In these conditions 30 tonnes / hour (output rate : 64 kg / h / ιη3) of copolymer of ethylene and I-butene are manufactured in the form of a powder which has the characteristics mentioned aboveIn contrast to the legitimate fears which there may have been concerning 15 the entrainment ofthe particles out of the reactor, no fouling problem has been found Not even the least increase in concentration of fine particles has been observed in the outer circulation conduit (5) in comparison with example Cl. In addition, a subsequent study ofthe general state of the exchangers (6, 7) situated in the outer circulation line (5) has proved that these exchangers had undergone a lesser degree of fouling in the case of example 3. when compared with the other two examples.The polymer output is next increased progressively by changing from 30 to 46.5 tonnes / hour (output rale 99 kg / h / m') over a period of 8 hours while the fluidized bed volume and hence this fluidized bed height of 23 m are kept constant5 This takes place without the least problem No presence of hot spots nor appearance of crusts was observed, and this has made it possible to continue the polymerization while maintaining these operating conditions

Claims

CLAIMS 1. Process for gas phase polymerization in a fluidized bed reactor consisting of a first volume which is a cylinder with a vertical axis of height H, above which is mounted a second volume, 5 commonly called a disengagement vessel, adjoining the first volume, the enclosure (wall) of which also consists of at least one surface of revolution generated by the rotation, about the same vertical axis known as axis of revolution, of a rectilinear and / or curved segment, characterized in that the height of the fluidized bed (h) is greater than J .05xH.

102. Process according to claim 1, in which one or more olefmic monomers such as ethylene, propylene, 1-butene, I-pentene, 4-methyl-1-pentene, 1-hexene or 1-octene are polymerized.

3. Process according to any of the preceding claims wherein the height of the fluidized bed (h) is greater than 1.1 *H.

4. Process for continuos gas phase polymerization of olefin(s) in a reactor containing a fluidized and optionally mechanically stirred bed, consisting of a cylinder with a vertical side wall and of a desurging or disengagement chamber (3) mounted above the said cylinder, at an absolute pressure higher than the atmosphere pressure, by continuous or intermittent introduction of a catalyst into 20 the reactor, continuous introduction of olefin(s) into a reaction gas mixture passing through the reactor in an upward stream, removal of the heat of polymerization by cooling the recycled reaction gas mixture, draining the polymer manufactured, a process characterized in that the height of the fluidized bed (h) is greater than 1.05xH. 25 5. Process according to claim 4, in which polymerization takes place with a polymer output rate higher than 50 kg / h / m3, preferably higher than 60 kg / h / m\ more preferably higher than 70 kg / h / m3.