Preparation processes of an adhesive for lignocellulose and a lignocellulose pressed board

MYPI1998000669A0Inactive Publication Date: 1998-08-21MITSUI CHEM & SKC POLYURETHANES INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1998000669
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1997-02-21
Filing Date
1998-02-18
Publication Date
1998-08-21
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional processes for producing lignocellulose-based boards using organic polyisocyanate adhesives face issues such as adhesive deposition on equipment, clogging of pipes and mixing chambers, and insufficient mixing, leading to production inefficiencies and product damage due to poor releasability from pressing platens.

Method used

A process involving the high-pressure injection of an organic isocyanate compound, a reactive emulsifier, and an emulsifying medium into a mixing chamber, equipped with a mechanical cleaning mechanism, to prepare an adhesive composition that is then applied to lignocellulose materials, ensuring effective mixing and preventing adhesive deposition on equipment.

Benefits of technology

This process enables the production of high-quality lignocellulose pressed boards with improved releasability and efficiency, reducing labor and production costs by preventing adhesive deposition and ensuring continuous operation without line troubles.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

DESCRIBED IN THE PRESENT INVENTION IS A PROCESS FOR THE PREPARATION OF AN ADHESIVE FOR A LIGNOCELLULOSE PRESSED BOARD, WHICH COMPRISES INJECTING A FIRST STREAM FORMED OF (A) AN ORGANIC ISOCYANATE COMPOUND AND A SECOND STREAM FORMED OF (B) A REACTIVE EMULSIFIER AND (C) AN EMULSIFYING MEDIUM AND OPTIONALLY A MOLD RELEASE AGENT INTO A MIXING CHAMBER UNDER A HIGH PRESSURE OF 40 TO 300 KG / CM2 AND THEN MIXING THEM. ACCORDING TO THIS INVENTION, A PREPARATION PROCESS OF AN ADHESIVE OPTIMUM FOR THE CONTINUOUS PROCESS SUITED FOR THE INDUSTRIAL PRODUCTION IS PROVIDED. OWING TO GOOD RELEASABILITY OF THE INVENTION ADHESIVE AT THE TIME OF HOT PRESSING, THIS ADHESIVE IS SUITED FOR THE INDUSTRIAL PRODUCTION OF A HIGH-QUALITY AND INEXPENSIVE LIGNOCELLULOSE PRESSED BOARD WITH GOOD PRODUCTIVITY.(FIG. 1)
Need to check novelty before this filing date? Find Prior Art

Description

PREPARATION PROCESSES OF AN ADHESIVE FOR LIGNOCELLULOSE ANDA LIGNOCELLULOSE PRESSED BOARDBACKGROUND OF THE INVENTION1. Field of the InventionThis invention relates to a preparation process of an adhesive used upon the production of a hot-pressed board formed mainly of lignocellulose and a production process of lignocellulose pressed board by using said adhesive.2. Description of the Related ArtA pressed board formed mainly of lignocellulose is called particle board when the lignocellulose is in the form of ligneous chips. In addition to the particle board, there are a wafer board for which large-sized chips are used and an oriented strand board (OSB) in which slender chips (strands) are arranged in a row. In the case of lignified fibers, they are produced as a board such as an insulation board, medium-density fiber board (MDF) or hardboard. These boards are used as floor materials, wall materials, door materials, soundproof materials, adiabatic materials, core materials for tatami, furniture members or automobile members .As an adhesive or binder for the production of a particle board, a wafer board, an OSB, a fiber board such as hard board, MDF or insulation board, a chaff board formed from chaffs or a kaoliang board formed from kaoliang stalks(which will be hereinafter called board, collectively), thermosetting resins such as urea resin, melamine resin, urea melamine resin, phenol melamine resin and phenol resin (which will hereinafter be called formalin-base resin adhesive, collectively) have so far been used widely.The formalin-base resin adhesive features that its exhibits excellent adhesion even at a low cost and hardens in a comparatively short time. Formalin which is emitted from the hot-pressed products adhered by the formalin-base θ resin adhesive is regarded as a problem from the environmental viewpoint. With a view to reducing the emitted amount of formalin, the free formalin amount in the adhesive is reduced (a molar ratio of formalin to phenol, melamine or urea in the resin adhesive is reduced) or formalin catcherL5 or the like is used at the time when the formalin-base resin adhesive is mixed. These countermeasures however have not brought about satisfactory results yet.On the other hand, the use of an isocyanate-base adhesive has been proposed as an adhesive which is a non-formalin base and imparts excellent physical properties to a board in Japanese Patent Laid-Open Nos. 131538 / 1982 and147567 / 1982, U.S. Patent Nos. 35557263, 3636199, 3870665,3919017 and 3930110 and the like.When a lignocellulose-base material is hot pressed 25 using an organic polyisocyanate as an adhesive, the adhesive sticks to a platen owing to its excellent adhesion, whichimpairs the pressed product, thereby causing a marked damage to the commodity value of the product and in addition, requires much labor to remove the deposit from the platen.The use of an additive to the organic polyisocyanate has therefore been studied in order to improve the releasability from the metal of the platen, thereby overcoming the above-described problem. For example, proposed as an additive to the organic polyisocyanate are an alkyl phosphate or pyrophosphate (Japanese Patent Publication No.θ 018068 / 1991), a sulfonated compound (Japanese PatentPublication No. 038309 / 1993), a wax and a liquid ester (Japanese Patent Publication No. 054390 / 1992) , an aliphatic carboxylic acid (Japanese Patent Laid-Open No. 36430 / 1983) , a polysiloxane compound (Japanese Patent Laid-Open No.-5 86225 / 1986), an aliphatic acid polymer (U.S. Patent Nos.4772442 and 4933232) and the like.In addition, proposed is a method of applying a releasing agent directly to a platen prior to hot pressing, which is effected by the formation of a release layer by usingΌ a metal soap (Japanese Patent Laid-Open No. 34026 / 1996), by using a high-boiling-point polyol (German Offenlegungsschrift DE-1653178), by using a polysiloxane film having a functional group (British Patent No. 135992) , by covering with polytetrafluoroethylene (U.S. Patent No. 4374791) or the like. Such a method is not sufficient.In some board plants, an organic polyisocyanate-baseadhesive is used only for the inside layer which is not brought into contact with a platen and a conventional formalin base resin is used for the surface layer which is brought into contact with the platen.As another process for overcoming the above problem, the present inventors have already filed an application for patent (Japanese Patent Laid-Open No. 245622 / 1985) on the invention in which an organic polyisocyanate, polyol, crosslinking agent, catalyst and internal mold release agent are used as raw materials upon preparation of a molded or formed product of a polyurethane resin. It does not, however, satisfy the object of the present invention because it comprises adding at most 5 parts by weight of zinc stearate to 100 parts by weight of a polyol and it is a process for the preparation of expanded polyurethane and elastomer available by pouring into a metal mold. In addition, the present inventors have already filed an application for the use of a mold releasing composition having a zinc salt of an aliphatic carboxylic acid dissolved in a polyol (Japanese Patent Laid-Open No. 137953 / 1988) and also for the use of a mold releasing composition composed of a higher fatty acid metallic salt and N,N,N'-tris(2hydroxypropyl)ethylenediamine (Japanese Patent Laid-Open No. 72757 / 1988). They do not satisfy the object of the present invention, because an amount (parts by weight) of the zinc salt of an aliphatic carboxylic acid or the higher • · · · · ·• · · fatty acid metallic salt used relative to a polyol is different, the polyol has an utterly different composition, non-aqueous system is employed and the mold releasing composition is used for the purpose of the preparation of a polyurethane molded or formed product.In a process which comprises preparing an adhesive composition by adding a diluent to the organic isocyanate compound to increase its amount and then applying the composition to a lignocellulose-base material, the organic isocyanate compound and diluent are generally mixed and emulsified in a mixing pot by the batch method or mixed and emulsified in a static mixer.Owing to high reactivity of the organic isocyanate compound, a polymeric product and the like between the organic isocyanate and diluent is formed in a mixing pot or static mixer and a pipe through which the adhesive composition flows, which causes clogging of the pipe, deposition to the inside wall of the apparatus, termination of the line and / or change in the flow rate in the line, resulting in the difficulty in stable operation of the line. It takes tremendous labor and time for the removal of the deposit and a reduction in the production amount due to the line trouble is not preferred also from the economical point of view.To overcome the above problem, disclosed in Japanese Patent Laid-Open No. 279303 / 1990 are a process for the • ·production of a synthetic board by emulsifying an adhesive composition by a static mixer and immediately after that, mixing it with a stream of cellulose fibers; and an apparatus therefor. In this method, the static mixer is cleaned by installing a baffle at each of input ports for the organic isocyanate compound and the diluent in a static mixer and flushing a fluid at the time of cleaning. This method is however accompanied with the drawback that the static mixer requires periodical cleaning and besides, it takes time to θ clean the mixer by flushing a fluid. Furthermore, the adhesive composition cannot be prepared during cleaning so that the supply of the stream of cellulose fibers must be stopped. The above method is therefore not suited for efficient continuous production.L5 In Japanese Patent Laid-Open No. 276501 / 1988, disclosed is a process for producing a particle board by using an adhesive obtained by carrying out emulsification through a double-liquid injection mixer formed of two nozzles which are arranged so as to cross on an extension line. This process is however accompanied with the drawbacks that owing to a low injection pressure, mixing and emulsification tend to become insufficient; a mixing head requires a special shape permitting the prevention of each of two injected liquids from entering into another's input port and causing solidification in the head; and because the mixer is not equipped with a cleaning means, a polymeric product of the• · · · organic isocyanate compound inevitably adheres and deposits in the mixing chamber after the long-term continuous use of the mixer, which is a cause for a change in the flow rate and line troubles such as clogging.Thus, each of the above-described processes involves various problems and does not withstand the use in the practical production site. At present, there is no technique which is satisfactory from every viewpoint of a step, economy and physical properties .The present inventors have already filed an application for a patent on an adhesive composed of an organic isocyanate, polyether and water (Patent application NOS, 38396 / 97 (AU), 973309 / 97 (ID), 39777 / 97 (TH), 328826 / 97 (NZ), 97.116939 / 97 (CN), / 97 (MY)). The adhesive has excellent performance, but since the organic isocyanate is apt to react with the other adhesive components and a reaction product between the isocyanate and other adhesive components deposits on the inside wall of a mixer or pipes as a scale, there is a demand for the improvement of the adhesive to be suited for a long-term stable use.An object of the present invention is to overcome the above-described problems in the step and physical properties which have not been overcome sufficiently by the conventional process and to provide a process for preparing an organic polyisocyanate adhesive without causing line troubles attributable to the deposition of a polymeric • · · · · · · · ·· • · · · · · · • · · · · *··· · · · · · ·· · · · · ·· • · ·· ·· ·· • · ·· « · ·· ··• · · · · a • · · · · • · · · · ··· ···· · • · · · • · · • · · · · · product of the organic isocyanate compound to the inside wall of the mixer or pipes; and a process for producing a high-quality board with good efficiency at a low cost by using an adhesive which is free from the deposition to a platen at the time of hot pressing of a board and is therefore excellent in releasability.SUMMARY OF THE INVENTIONAs a result of an extensive investigation with a view to overcoming the above-described problems, the present inventors have found an adhesive for a hot-pressed board formed mainly of lignocellulose and a production process of the board, more specifically, an adhesive available - upon mixing an organic isocyanate compound with an emulsifying medium and emulsifying the resulting mixture to prepare an adhesive composition - by injecting a first stream composed of the organic isocyanate compound and a second stream composed of a reactive emulsifier and the emulsifying medium into a mixing chamber under high pressure, and then mixing and emulsifying them; and a production process of a hotpressed board by using said adhesive and completed the present invention.BRIEF DESCRIPTION OF DRAWINGSFurther objects and advantages of the more fully understood from the following invention can be detailed ·· ·· • · · ♦ · • · · · · ··· · · · • · · · ·· ·· ·· ·· • · · • ··· ··· • · · · · • · · · · ·· ·· ··I fl ·· • · ·· ·· ·· • · · · · · • · · · ·· ··· ···· · • · · · ·· ·· ·· • · description taken in conjunction with the accompanying drawings in which:FIGS. 1 and 2 are schematic views each illustrating a preparation apparatus of an adhesive used for the practice of the present invention; FIG. 3 is a schematic view illustrating a preparation step of an adhesive of the present invention; and FIG. 4 is a schematic view illustrating an example of production equipment of a medium density fiberboard (MDF) of the present invention.DESCRIPTION OF THE PREFERRED EMBODIMENTSThe present invention embraces the following inventions and embodiments .(1) A process for the preparation of an adhesive for a lignocellulose pressed board, said adhesive being comprised of (A) an organic isocyanate compound, (B) a reactive emulsifier and (C) an emulsifying medium, which comprises injecting a first stream formed of said organic isocyanate compound (A) and a second stream formed of said reactive emulsifier (B) and said emulsifying medium (C) into a mixing chamber under a high pressure of 4 0 to 300 kg / cm2and then mixing said streams.(2) A process as described in (1), which further comprises adding a mold release agent (D) to said first stream or said second stream.(3) A process as described in (1) or (2) , wherein saidI* mixing chamber is equipped with a mechanical cleaning means.(4) A process as described in (3), wherein said mechanical cleaning means cleans inside of said mixing chamber by putting a rod, which is mechanically actuated and substantially fits the inside of said mixing chamber, in and out of said mixing chamber.(5) A process as described in any one of (1) to (3), wherein said emulsifying medium (C) is water or contains at least water.(6) A process as described in any one of (1) to (5), wherein said reactive emulsifier (B) is a polyether and / or polyester polyol or contains at least a polyether and / or polyester polyol.(7) A process as described in (6) , wherein said reactive emulsifier (B) contains at least a polyether and / or polyester polyol; said polyether and / or polyester polyol has 2 to 8 functional groups and has a structure in which a recurring unit of (CH2CH2-O) amounts to 5 to 70% of the weight of the polyether and / or polyester polyol; and the ratio of said polyether and / or polyester polyol is 0.01 to 70 parts by weight per 100 parts by weight of the organic isocyanate compound (A).(8) A process as described in (6) , wherein said reactive emulsifier (B) contains at least a polyether and / or polyester polyol; said polyether and / or polyester polyol contains in a molecule thereof a nitrogen atom; and a ratioof said nitrogen atom is 0.1 to 12.0 wt.% based on the polyether and / or polyester polyol.(9) A process as described in (6), wherein said polyether polyol has been prepared by adding alkylene oxides to at least one compound selected from triethanolamine, diethanolamine, monoethanolamine, orthotoluenediamine, metatoluenediamine, diphenylmethanediamine and polyphenyl polymethylenepolyamine; and an amount of ethylene oxide, among said alkylene oxides, is 5 to 70 parts by weight per 100 parts by weight of said polyether polyol.(10) A process as described in any one of claims 2 to 9, wherein said mold release agent (D) is at least one substance selected from metallic salts of a saturated and / or unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms and waxes.(11) A process as described in (10), wherein said metallic salt of a saturated and / or unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms is at least one combination of a substance selected from the group consisting of octylic acid, lauric acid, myristic acid, palmitic acid, stearic acid, oleic acid and behenic acid and another substance selected from the group consisting of zinc, iron, aluminum, calcium, zirconium, magnesium, barium, nickel, copper and cobalt.(12) A process as described in any one of (2) to (11) , wherein said mold release agent (D) is added in an amountof 1 to 150 parts by weight per 100 parts by weight of said organic isocyanate compound (A).(13) A process as described in any one of (1) to (12) , wherein said organic isocyanate compound (A) is polymethylene polyphenyl polyisocyanate.(14) A process for the production of a lignocellulose pressed board, which comprises mixing a lignocellulose-base material with an adhesive for a lignocellulose pressed board as described in any one of claims (1) to (12) , forming a mat from the resulting mixture and then hot pressing the mat.(15) A lignocellulose pressed board obtained by the process as described in (14).[Embodiment of the Invention]The present invention will hereinafter be described more specifically.In the present invention, a lignocellulose pressed board is produced as a product by injecting under high pressure an organic isocyanate compound, a reactive emulsifier and an emulsifying medium into a mixing chamber equipped with a mechanical cleaning means and mixing and emulsifying the resulting mixture, thereby obtaining an adhesive; and applying said adhesive to a lignocellulose-base material, followed by mat formation, hot pressing and surface abrasion.Examples of the lignocellulose-base material include strand chips, dust chips and flake chips which are used forthe production of a particle board, wafer board or OSB;fibers used for hard board, MDF or insulation board; and agricultural products such as kaoliang stalk, bagasse and chaff. The above-exemplified materials can be used either singly or in combination.As the organic isocyanate compound (A) , any substance containing therein an isocyanate group can be used in the present invention. Specific examples include tolylene diisocyanate, 4,4'-diphenylmethane diisocyanate, hexamethylene diisocyanate, xylene diisocyanate, isophorone diisocyanate, norbornene diisocyanate and polymethylene polyphenyl polyisocyanate (polymeric MDI), and these isocyanate compounds modified with a compound containing at least one active hydrogen. Among them, polymeric MDI is preferred from the economical viewpoint.As the reactive emulsifier (B) used in the present invention, those reacting with said organic isocyanate compound and functioning as an emulsifier can be used without limitations. As the emulsifier having such a function, a polyether and / or polyester polyol is preferred in consideration of economy, compatibility with the organic isocyanate compound, foaming property and physical properties of a board.As the polyether and / or polyester polyol (which will hereinafter be called polyol collectively) , it is possible to use a polyether polyol or polyester polyol singly or as • · · · · · · · · · ·· · · · ·· · · · · ·· ·· · · ········· · ·· ········ ········ • · ·♦ · · · ········ · · · · · · · · · · · ··· a mixture of a polyether polyol and polyester polyol. Alternatively, a polyether-polyester copolymerized polyol can be used.As the polyol used in the present invention, preferred are those containing 2 to 8 functional groups; having a hydroxyl number (OHv) of 24 to 800 mg KOH / g; and having recurring units of (-CH2-CH2-O-) in an amount of 5 to 70 wt.%, more preferably 10 to 60 wt.% relative to the weight of the polyol.Recurring units not less than 5% bring about good emulsifying property, while recurring units not greater than 70% make it possible to form a board having good physical properties .The polyether polyol usable in the present invention is prepared, in a manner known as a conventional process for the preparation of a polyol, by adding alkylene oxides - each having in its molecule an epoxy group - such as ethylene oxide, propylene oxide, butylene oxide or styrene oxide to, as an initiator, a low-molecular compound having at least two active hydrogen atoms in the absence of a catalyst or presence of a catalyst such as a hydroxide of an alkali metal or a tertiary amine.Examples of the initiator include amine initiators and non-amine initiators. Exemplary amine initiators include ethanolamines such as monoethanolamine, diethanolamine and triethanolamine and amines such as ethylenediamine, ·· ·· ·· ·· ·· ·· ·· · ·· ·· ·· · ·· ·· ·· • ••••••a· · ·· ········ ········ * ···· · · ········ · · ·· · · · ·· · · ··· • · · · ·· · · ·· ·· ···· ·· · · · · · ······· · diethylenetriamine, orthotolylenediamine, metatolylenediamine, 4,4'-diphenylmethanediamine, 2,4'diphenylmethanediamine and polymethylpolyphenylpolyamine. They are used either singly or in combination.Exemplary non-amine initiators include sucrose, alcohols such as glycerin, pentaerythritol, sorbitol, trimethylol propane, diglycerin, propylene glycol, dipropylene glycol, diethylene glycol, ethylene glycol, 1,4butanediol and 1,2-butanediol, and phenols such as hydroquinone, bisphenol A and novolak.In the present invention, the above-exemplified amine initiators are preferred. It is also possible to use the amine initiator in combination with any one of the above-exemplified non-amine initiator.The proportion of a nitrogen atom in the polyol is preferably 0.1 to 12.0 wt.%, more preferably from 1.0 to 10 wt.%. Proportions not less than 0.1 wt.% permit effective emulsification . When the proportion is not greater than 12.0 wt.%, on the other hand, the reaction is appropriate and the adhesive can be produced easily.The polyester polyol can be obtained by the addition reaction between an acid anhydride and an alcohol, polycondensation reaction between a polycarboxylic acid and an alcohol or the addition of an alkylene oxide to an acid.Examples of the acid anhydride include maleic anhydride, succinic anhydride, trimellitic anhydride, • ······ ·· · ·· • · · · · ·· · · · · · · · · · • · ·· · *····· • · « · · · ····«·· ····· · · · · pyromellitic anhydride, itaconic anhydride, phthalic anhydride, glutaric anhydride, glutaconic anhydride, diglycolic anhydride, citraconic anhydride, diphenic anhydride and toluylic anhydride. Examples of the polycarboxylic acid include maleic acid, terephthalic acid, dimethylterephthalic acid, isophthalic acid, fumaric acid, oxalic acid, malonic acid, glutaric acid, adipic acid, pimelic acid, suberic acid, azelaic acid, sebacic acid, citric acid and trimellitic acid. Illustrative of the alcohol usable in the present invention include alcohols, phenols and alkylene oxide adducts as initiators, each exemplified above.As one function of the reactive emulsifier in the present invention, it is important to dissolve or emulsify the organic isocyanate compound (A) in the emulsifying medium (C) and the reactive emulsifier which can attain this function is required. As a reactive emulsifier which can satisfy the above object, the reactive emulsifier (B) is employed. The reactive emulsifier exhibiting surface activating capacity, in addition to the above function, can be used suitably. Described specifically, surfactants can be given as an example and anionic surfactants, cationic surfactants, nonionic surfactants and the like can be employed .Specific examples of the surfactant include anionic surfactants such as fatty acid soap, rosin soap, alkyl • · · ·· ·· ·· · · · ···· ·· ·· ·· · · · · · · • · · · · · sulfonate, alkylbenzene sulfonate, dialkylaryl sulfonate, alkylsulfosuccinate, polyoxyethylene alkylsulfate and polyoxyethylene alkylarylsulfonate; and surfactants such as polyoxyethylene alkyl ether, polyoxyethylene alkylaryl ether, polyoxyethylene sorbitan fatty acid ester and oxyethylene oxypropylene block copolymer. The present invention is not limited to these surfactants. These surfactants can be used either singly or in combination.Examples of the emulsifying medium (C) usable in the present invention include, as well as water, alcohols such as ethanol, methanol and propanol; hydrocarbon solvents such as benzene, toluene and hexane; and polar solvents such asN,N-dimethylformamide, Ν,Ν-dimethylacetamide, ethylene carbonate, propylene carbonate and furfural. Alternatively, more than one of the above-exemplified mediums may be used as a mixture. When water is used in the form of a mixture, it is preferred to use water in an amount not smaller than 50 wt.%. Among these mediums, water is preferably used from the viewpoints of economy and safety. Upon use of water, pH (hydrogen ion concentration) may fall within a range of from 1 to 13.According to the process of the present invention, an adhesive for lignocellulose can be prepared using the organic isocyanate (A), the reactive emulsifier (B) and the emulsifying medium (C) . Furthermore, a mold release agent (D) may be added.• · · « · · · · · · · • · · · · · · · · · · ··· · » · · · • · · · · ·When the component (D) is not used as an adhesive component, it is recommended to carry out pressing after applying a mold release agent to a platen so that the adhesive composition and the like do not deposit to the platen at the time of hot pressing of a board. As the mold release agent, a known one can be employed. For example, those usable as the component (D) in the present invention can be given as examples. When the mold release agent (D) is added to the adhesive, it is not necessary to apply it to the platen.In the process of the present invention, any mold release agent which can serve the above purpose can be used suitably. Preferred examples of the mold release agent (D) in the present invention include metallic salts of a saturated and / or unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms and waxes.Concerning the metallic salt of a saturated and / or unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms, aliphatic carboxylic acids having any one of mono-, di- and tri-functional groups can be used. Among them, linear aliphatic monocarboxylic acids having 12 to 22 carbon atoms are preferred. Specific examples include octylic acid, lauric acid, myristic acid, palmitic acid, stearic acid, oleic acid, linoleic acid, linolenic acid, arachic acid, lignoceric acid and behenic acid. Examples of the metal component include zinc, iron, aluminum, calcium, zirconium, magnesium, barium, nickel, copper and cobalt. At ········· · · · • · ·· · · · ···· · · · · · ··· · ·· · · · · ·· · ··« • · · · · · • · · · ·· ··· ··· · * • · · · ·· · · · • « · · · • · · · · least one acid component and at least one metal component, each selected from the above-exemplified groups, can be used in combination. In other words, it is possible to use metallic salts of a carboxylic acid either singly or in combination, said salt being composed of an acid component selected from the group consisting of the above preferred carboxylic acids and a metal component selected from the group consisting of the above preferred metals.The metallic salt of a saturated or unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms as the component (D) may exist as is in the adhesive of the present invention. It may be added in the form of a metallic salt or added in the separate forms as an aliphatic carboxylic acid and a metal compound.Examples of the wax usable as the component (D) include candelilla wax, carnauba wax, rice wax, Japan wax, palm wax, beeswax, lanolin, spermaceti, montan wax, ozokerite, ceresin, paraffin wax, petrolatum, Fisher-Tropsch wax, polyethylene wax, modified wax and hydrogenated wax, and mixtures thereof.The metallic salt of a saturated or unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms, as a mold release agent (D) , may be added to any one of the reactive emulsifier, polyether and / or polyester polyol in the reactive emulsifier (B), the emulsifying medium (C) , water in the emulsifying medium (C) and the mixture of the reactive ········· · · · ·······» ········ • · ·· · ·· ···· ··· ·· ····· · · · ·· · ·· ··· · ·· · · · · · · · ··· ··«»·· · ··· ··· · » • •••••••fl·· · ······ · · ··· emulsifier (B) and the emulsifying medium (C) . The metallic salt of a saturated or unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms may be used in the form emulsified by an emulsifier as needed. Here, any one of emulsifiers commonly used can be used. Specific examples include anionic surfactants such as fatty acid soap, rosin soap, alkyl sulfonate, alkylbenzene sulfonate, dialkylarylsulfonate, alkyl sulfosuccinate, polyoxyethylene alkyl sulfate and polyoxyethylene alkyl aryl sulfonate; and surfactants such as polyoxyethylene alkyl ether, polyoxyethylene alkylaryl ether, polyoxyethylene sorbitan fatty acid ester and oxyethylene oxypropylene block copolymer. The present invention is not limited by the above-exemplified surfactants. These surfactants may be used either singly or in combination.When the mold release agent (D) is soluble in an isocyanate as in the case of a wax or the like, it may be added to the first stream. The wax or the like may be used in the form emulsified by an emulsifier, and may be added to the second scream.A description will next be made of the process of the present invention for preparing an adhesive by using the above-described raw materials for the adhesive.FIGS. 1 and 2 are schematic views each illustrating a preparation apparatus of an adhesive used in the practice of the present invention; FIG. 3 is a schematic view ·· ·· ·· ·· ·♦ ·· ·· ········· · · · • · ·· · ·· · · · · · · · · · ···· ·· ·· ·· · · · ··· • · ·· ·· ·· ·· · · ·· ·· ·· ·· ·· ·· ·· • ·· · · ·· ·· · · · · · · • · · · · · • · · · · · • · · · · · ··· ·· · • ·· ·· ·· ··· · · ·· · • · · · · ·· • ··· ··· · · • · · · · • · · · · ·· · · illustrating a preparation step of the adhesive according to the present invention; and FIG. 4 is a schematic view illustrating an example of MDF production equipment of the present invention.The preparation apparatus (which will hereinafter be called mixing head) of the adhesive of the present invention comprises, as is illustrated in FIG. 1, a supply port 1 for supplying the organic isocyanate compound (A) as the first stream; a supply port 2 for supplying as the second stream a mixture obtained in advance by mixing the reactive emulsifier, for example polyether and / or polyester polyol (B) , and the emulsifying medium (C) and optionally the mold release agent (D) ; a mixing chamber 5; a cleaning rod 4 which has been designed to substantially fit the mixing chamber and is actuated by hydraulics or pneumatics; a check valve 3; and a spray nozzle 6.In addition, illustrated in FIG. 3 are incidental facilities such as high pressure pump 20 for supplying the first stream into the mixing chamber under high pressure; and high pressure pump 19 for supplying the second stream into the same chamber under high pressure. A generator of hydraulics or pneumatics for actuating the cleaning rod and a control panel for the generator are not illustrated but can also be given as the incidental facilities.A preparation process of the adhesive according to the present invention will next be described with reference to ·· ·· ·· ·· ·· ·· ·· · ·· ·· ·· · ·· ·· ·· ········· · ·· ··'······ ········ • · ·· · · · «······· · · ·· · · 0 · 0 «· ··· ···· ·· ·· ·· ·· · ··· ·» · · · · · ······· · ··········· · ·»···· · · ···FIGS. 1, 2 and 3. FIG. 1 is a schematic view illustrating a preparation apparatus of an adhesive used in the practice of the present invention and also a cross-sectional view of the mixing head at the time of the preparation of an adhesive;FIG. 2 is a schematic view illustrating a preparation apparatus of an adhesive used in the practice of the present invention and is also a cross-sectional view illustrating a mixing head used upon cleaning; FIG. 3 is a schematic view illustrating the production step of the adhesive according to the present invention; and FIG. 4 is a schematic view illustrating an example of MDF production equipment of the present invention.The following is a legend of reference numerals used in the drawings.I. Supply port for organic isocyanate compound . Supply port for reactive emulsifier and emulsifying medium3. Check valve4. Cleaning rod5. Mixing chamber6. Spray nozzleII. Raw material tank for reactive emulsifier12. Raw material rank for emulsifying medium13. Raw material tank for organic isocyanate compound14. Service tank for reactive emulsifier15. Service tank of emulsifying medium ·· ·· ·· ·· ·· ·· ·· · ·· ·· ·· · ·· ·· ·· ········· · · · ····«··· «······· • · ·· · · · « ··· ··· ·· ····· · ······· ··· · ·· · · ·· · · · ··· ···«·· · ··· · ··········· · ·····« « · ···16. Pot for mixing reactive emulsifier and emulsifying medium17. Service tank for mixture of reactive emulsifier and emulsifying medium18. Service tank for organic isocyanate compound19. Pressurizing pump20. Pressurizing pump21. Mixing head30. Feeder31. Digester32. Refiner33. Blow line34. First cyclone35. Air lock36. Bypass37. Blender38. Second cyclone39. Fiber storage tank40. Forming head41. Forming belt42. Prepress43. Hot pressFIG. 1 is a schematic view illustrating the mixing head at the time of the preparation of the adhesive. Said mixing head is formed of the supply port 1 for the organic isocyanate compound, supply port 2 for the reactive emulsifier and• · • · · · • • · • · · • • • • · · · • · • · · • • • ··· ··· · · • · · • · · • • · · · • · • · · • · · • • • • · · · ··· • ··· ··· • · • · · • • · • ·emulsifying medium (also of the component (D) as needed), check valve 3, cleaning rod 4, mixing chamber 5 and spray nozzle 6.The organic isocyanate compound (A) is pressurized by the pressurizing pump and is fed, as the first stream, into the mixing room 5 (which will hereinafter called mixing chamber) equipped with a mechanical cleaning means. A mixture, which has been prepared in advance by mixing the reactive emulsifier (B), for example, polyether and / or polyester polyol, emulsifying medium (C) and mold release agent (D) , is pressurized by another pressurizing pump and is fed as the second stream into the mixing chamber 5 from the supply port 2. The first and second streams introduced into the mixing chamber 5 are mixed at once under high pressure into an emulsified form, whereby the adhesive composition of the present invention is obtained. It is discharged / injected through the spray nozzle 6.Injection pressure into the mixing chamber of the present invention equipped with a mechanical cleaning means is preferred to fall within a range of from 40 to 300 kgf / cm2. When the injection pressure is less than 40 kgf / cm2, sufficient mixing and emulsification do not tend to be attained. On the other hand, the injection pressure exceeding 300 kgf / cm2are not preferred, because the mixing and emulsification can be carried out sufficiently under the injection pressure of 300 kgf / cm2and the pressures ·· ·· ·· ·· ftft ftft ftft ft ·· ftft ·· · ·· ftft ·· ft········ ft ftft ft······· ········ • ft ft · · ftft ft·*····· · · ·· ft · ft · · ·· ··· • ftft ft ftft · · ft ft ftft · ··· ft ft ft ft ft ft ft ftftft ftftft ft · ft·········· ft ft ft ft ft ft ft ft ft ft·· exceeding this value do not bring about better results in mixing and emulsification and are therefore industrially useless .As is illustrated in FIG. 1, in the injection apparatus of the present invention, the cross-sections of the outlets for the first and second streams to the mixing chamber are much narrower than that of the mixing chamber. For example, in No. 4 Chamber produced by ISOTHERM AG / Switzerland, the cross-sections of the outlets for the first and second streams to the mixing chamber are each 0.64 mm3, while the cross-section of the mixing chamber is 3.8m3. The pressure at the nozzle of the outlet of the mixing chamber is normal so that the pressures of the pumps for feeding the first and second streams come into collision without a substantial pressure decrease in the mixing chamber, whereby the first stream and second stream are mixed. Accordingly the pressure injected into the mixing chamber of the present invention means the total pressure of the pumps for feeding the first and second streams.FIG. 2 is a schematic view illustrating a mixing head at the time of cleaning. At the time of cleaning in the mixing chamber, that is, at the time when the preparation of an adhesive is terminated, the cleaning rod 4 which has been designed to substantially fit the mixing chamber blocks the supply ports for the first and second streams, thereby inhibiting the occurrence of mixing and at the same time, ·· ·· ·· ·· ·· ·· ·· · ·· ·· ·· · ·· ·· ·· ········· · · · ········ ········ • · ·· · ·· · ··· ··· ·· ····· · ·· ·· · ·· ··· · ·· · · · · · · · ··· ······ · ··· ··· · · ··········· · ······ · · ··· rubs off the polymeric product of the organic isocyanate deposited to the wall of the mixing chamber, thereby cleaning the inside of the mixing chamber. The rod 4 is inserted or taken out by a mechanical means such as hydraulic or pneumatic pressure. During the cleaning inside of the mixing chamber 5, the pumps for the first and second streams may be stopped or operated under the pressure switched to low one. It is also possible to dispose in the rod 4 circulation ports for the first and second streams and to effect circulation by the pumps during cleaning. Alternatively, it is possible to attach check valves 3 to the first and second streams, respectively just before the mixing chamber to prevent one of the liquids from entering into the pipe arranged for another liquid at the time when some trouble happens in the supply of the raw materials.The adhesive may be applied to a lignocellulose-base material by charging the lignocellulose-base material in a drum-system blender equipped with an agitating element and then spraying the adhesive to the material while turning the blender; or by causing the lignocellulose-base material to flow by a blower or the like and spraying or adding dropwise the adhesive to the resulting lignocellulose stream.In each of the steps, a surfactant and / or stabilizer may be added within an extent not impairing the present invention .Concerning the mixing ratio of the reactive emulsifier ········· · · · • · ·· · · · · ··· ··· · · ··· · · · ·· · · ·· · ··· ·· ·· ·· ·· ·· ·· • · · · · · • · · · ·· ··· ··· · · • · · · ·· · · · • · · · · • · · · · (B, to the organic isocyanate compound (A), the component (B) is preferably added in an amount ranging from 0.01 to 70 parts by weight, more preferably from 1 to 30 parts by weight, per 100 parts by weight of the organic isocyanate compound (A). Amounts not less than 0.01 part by weight permit good dispersion of the organic isocyanate compound, while at amounts not greater than 70 parts by weight, the resulting board is provided with good physical properties.Concerning the mixing ratio of the reactive emulsifier (B) to the emulsifying medium (C) , the reactive emulsifier (B) is preferably added in an amount of 0.002 to 50 parts by weight, more preferably 0.01 to 30 parts by weight, per100 parts by weight of the emulsifying medium (C) . Amounts of the reactive emulsifier (B) not less than 0.002 part by weight are preferred because the adding effects of the reactive emulsifier are recognizable. Amounts exceeding 50 parts by weight are not preferred because the addition of such an amount does not bring about a further improvement and is therefore industrially useless.Concerning the mixing ratio of the reactive emulsifier (B) and the emulsifying medium (C) to the organic isocyanate compound (A) , the components (B) and (C) are preferably added in an amount of 10 to 2000 parts by weight, more preferably 30 to 800 parts by weight in total per 100 parts by weight of the organic isocyanate compound (A). When the total amount of (B, + (C) is not less than 10 parts by weight,dilution effects of the organic isocyanate compound (A) appear. When the total amount is not greater than 2000 parts by weight, on the other hand, a hot-pressed board having good physical properties can be produced.In the present invention, the component (D) may be added. When it is added, the mold release agent (D) is added in an amount of 1 to 100 parts by weight in the case where the component (D) is a metallic salt of a saturated and / or unsaturated aliphatic carboxylic acid, and 1 to 150 parts by weight in the case of a wax, each per 100 parts by weight of the organic isocyanate compound (A). Amounts not less than 1 part by weight bring about an improvement in the mold releasing effects, while amounts exceeding 150 parts by weight are industrially useless because a sufficient releasability can be attained in an amount of 150 parts by weight.Concerning the mixing ratio of the reactive emulsifier composed of the reactive emulsifier (B) and mold release agent (D) and the emulsifying medium (C, to the organic isocyanate compound (A) , the components (B) + (C) + (D) are preferably used in an amount of 10 to 500 parts by weight, more preferably 30 to 300 parts by weight, in total per 100 parts by weight of the organic isocyanate compound (A) . When the total amount of the components (B) , (C) and (D) is not less than 10 parts by weight, effects for diluting the organic isocyanate compound (A) appear. When the totalamount is not greater than 500 parts by weight, a hot pressed board having good physical properties can be produced.In each of the above steps, a surfactant and / or stabilizer may be added within an extent not impairing the present invention.Concerning the mixing ratio of the reactive emulsifier composed of a polyether and / or polyester polyol (B) and the mold release agent (D) to the emulsifying medium (C), the reactive emulsifier is preferably used in an amount of 0.002 to 50 parts by weight, more preferably 0.01 to 30 parts by weight, in total of (B) + (D) per 100 parts by weight of the emulsifying medium (C). When the amount of the reactive emulsifier (B) is not less than 0.002 part by weight, adding effects of the reactive emulsifier appear. Amounts exceeding 50 parts by weight are not preferred, because such amounts do not bring about a further improvement in the effects and are therefore industrially useless.The amounts of the lignocellulose-base material and adhesive differ with the water content of the lignocellulose-base material and target physical properties. They may be used in amounts permitting uniform mixing of the adhesive in the lignocellulose-base material. The amount of the adhesive is preferably 1 to 30 wt.% based on 100 parts by weight of the lignocellulose-base material in terms of the absolute dry weight.When the amount of the adhesive is not less than 1 wt.%,effects as an adhesive can be attained. Since a board having sufficient physical properties can be obtained at an adhesive amount of 30 wt.%, the use of the adhesive in an amount exceeding 30 wt.% is not preferred because it is industrially useless.In the production process of the lignocellulose pressed board according to the present invention, the mixture of the adhesive and the lignocellulose-base material is subjected to hot pressing after forming. The mixture can be formed into a single layer or plural layers. The amount of the adhesive may be changed as needed. If necessary, prepressing may be carried out after lamination; or prepressed mats may be laminated.At this time, it is possible to use the adhesive of the present invention only for the outer layer contiguous with a platen and another adhesive, which is inferior in reusability, for the inner layer, thereby forming a multi-layer structure.In order to allow heat penetrate into the materials to be pressed, either hot pressing between flat platens or curved platens can be employed. From the viewpoint of the continuous productivity and low cost, pressing between flat platens is preferred. The hot pressing may be carried out in a continuous or multi-stage manner.After hot pressing, the surface of the outermost layer of the board may be subjected to abrasion finishing into a desired thickness .The MDF production equipment as illustrated in FIG. 4 is one example to which the process of the present invention has been industrially applied. As illustrated in FIG. 4, wood pieces, for example, wood chips are fed to a digester, where the chips are softened and lignin in the chips are destroyed. Then the resulting chips are sent to a refiner, where the chips are decomposed into fibers between disks turning, for example, in one direction or two directions.Hot wet fibers are carried through a so-called blow line into a blender. During the blow line, a reactive emulsifier other than the adhesive, such as a sizing agent or flame-retardant, is added. The adhesive is added between the blow line and flaming head, for example the position indicated by an arrow in FIG. 4. It is also possible to carry out dropwise addition or spraying of the adhesive of the present invention during the blow line, followed by blending the lignified fiber and adhesive. Such an adhesive composed of an aqueous emulsion as is prepared by the process of the present invention is suited to injection through a blow line because of the following reasons. In the first place, hot wet fibers which have been heated to a certain temperature heighten the temperature of the aqueous emulsion added to the adhesive composition so that the water content of the lignified fibers coated with the adhesive can be adjusted. In the second place, a large turbulent flow of lignified • ·· ·· · · ·· · · · • · ·· · ·· ···· ··· · · • · · · ·· ·· ·· · · · · · ·fibers in the blow line rubs off the adhesive deposited to the wall of the blow line, whereby the cleanness inside of the blow line can be maintained. In the third place, owing to a high flow rate in the blow line, it does not take much time for mixing and besides, uniform coating can be attained.Fibers flowing through the blow line are subjected to partial dehydration. For the separation of the fibers from the air stream after dehydration, a first cyclone and air lock are installed. The fibers are then introduced into a blender. It is possible to charge the adhesive and auxiliary agents such as mold release agent, flame-retardant and sizing agent into a blender and mix with the fibers. In the blender wherein an agitation element permitting the mechanical agitation is rotating, the adhesive and auxiliary agents are sprayed downward or from a proper direction and apparently uniform mixing with the fibers can be attained. When a desired reactive emulsifier has already been added, the fibers are introduced through a bypass chute into a second cyclone equipped with an air lock and then fed to a storage tank for the adhesive-coated fibers.The storage tank for the adhesive-coated fibers supply fibers to at least one forming head apparatus, where the adhesive-coated fibers are formed into a mat. The mat so formed is pressed in advance by at least one pre-pressing apparatus, followed by hot pressing into a final thickness by a hot pressing apparatus. By the heat at this time, the ·· ·· ·· ·· ·· ·· ·· · ·· ·· ·· · ·· ·· ·· ········· · ·· ········ ········ adhesive sets and a desired board is produced. If necessary, the board may be subjected to surface abrasion in order to adjust the thickness and surface conditions.Specific examples of the mixing head having a mixing chamber for the production of an adhesive include the mixing heads produced by ISOTHERM AG / Switzerland, GASMER / U.S.A., GLASS-CLAFT and CLAUS MUFFI, CANON and Toho Machinery Co. ,Ltd. Any one of the above-exemplified ones can be used suitably.In the present invention, it is possible to use in combination an antioxidant, ultraviolet absorber, flame retardant, stabilizer, surfactant, plasticizer, silane coupling agent, POVAL, metal catalyst, external releasing agent, synthetic rubber latex and / or acrylic emulsion within an extent not impairing the intended advantages of the present invention.ExamplesThe present invention will hereinafter be described in further detail by examples. It should however be borne in mind that the present invention is not limited to or by these examples. In the examples, production of a fibrous board from a wooden fiber is shown but it is possible to produce various boards from another lignocellulose-base material easily when the present examples are applied. All designations of part or parts and % mean part or parts by weight and wt.% unless otherwise specifically indicated.• ·· ·· ·· ·· · · · • · ·· · ·· ···· ··· · ·The conditions common to the production of a board employed for the comparison of performances are shown below: Raw material: dust chips or lignified fibers (water content: 7.0%, which will hereinafter be called chips)Composition of the board: single layer (dust chips) or three layers (lignified fibers)Thickness of the board (except the abraded portion): 15 mmWater content of the mat: 16%Hot pressing temperature: 180°CPressing pressure: 35 kg / cm2Pressing time: 2.5 minPreset density: 700 kg / m3Evaluation Test1. Flexural strengthThe pressed sample was cut into a test piece of 50 mm wide and 275 mm long (spun: 225 mm) and a flexural test was conducted in accordance with A Testing Method for Particle board of JIS-A-5908. The results are shown as flexural strength in Table.2. Wet flexural strength (Test A)As in the above method, a test piece was cut out from the pressed sample. The test piece was then immersed in warm water of 70+3°C for 2 hours, and then in water of the normal temperature for one hour. The flexural test was conducted using the test piece not dried. The results are indicated in the table as wet flexural strength (A).·· ·· ·· ·· ·· ·· ·· · ·· ·· ·· · ·· ·· ·· ········· · ·· ········ ········ • ···· ·· ········ · · ·· · · · ·· · · ··· ···· ·· ·· ·· ·· · · · · ·· · · · · · ······· ·3. Evaluation on dispersibilityA portion of the adhesive prepared by the above method was sampled and MDI was observed visually to evaluate its emulsifying property.4. Peeling strengthPeeling strength was measured in accordance with the methods specified under JIS A 5905 and MIS A 5908.5. Evaluation on continuous operationThe board was produced continuously for 50 hours and the deposition of the adhesive to the production line and deposition of the raw materials to the Caul plate were visually observed for evaluation.6. Synthetic judgmentThe productivity and physical properties of the board were evaluated. The board which was judged good in both evaluations was ranked as A and the board which was not satisfactory in at least one of them was ranked as B.Example 1First, polymeric MDI (A) (Cosmonate M-200, trade name; product of Mitsui Chemical, Inc.) as a first stream; and, as a second stream, a mixture of ethylenediamine (EDA) as an initiator, a solution of a propylene oxide / ethylene oxide block copolymer PPG (ethylene oxide content: 40%, hydroxyl number: 252 mgKOH / g) dissolved in water, the dispersion medium (C) , to give a concentration of 20%, and a solution of an aqueous emulsion (nonvolatile matter: 31%) • · · · · · · ·· · · · • · ·· · ·· ···· ··· · · ··· · ·· · · · · ·· · ···of zinc stearate dissolved in water to give a concentration of 8% in terms of a solid content were charged in a chamber of a spray gun (SP-300 Gun, trade name; product of ISOTHERM AG; having a pore size of 0.45 mm for each of the first and second streams to be injected into the mixing chamber; equipped with a mixing chamber No.4 having a diameter of 1.1 mm) under a pressure of 100 kgf / cm2and the resulting mixture was spray-coated to the spilt lignified fibers in a blender while stirring. The liquid ratio of the first stream to the second stream was 8:12 and the total of the polymeric MDI and polyol was 6% of the absolute dry wood. The adhesive-coated fibers were than formed on a steel Caul plate, followed by pre-pressing for 30 seconds so that the board thickness would be 500% of the thickness of the board as a product. Then the pre-pressed board was subjected to hot pressing under the above-described conditions.After hot pressing, the adhesion to the steel Caul plate was observed but no deposition was found. The board after hot pressing was provided for the comparison of physical properties and evaluated in accordance with the evaluation method specified in JIS-A-5905 (fiberboard) . As a result, it exhibited physical properties not less than type 30 (which indicates the board having strength not less than 30 N / mm2in both the lengthwise and crosswise directions in the flexural strength, which is the JIS standard for the evaluation of physical properties) as is shown in Table 1.·· ·· ·· ·· ·· ·· ·· * ·· ·· ·· · ·· ·· ·· ········· · ·· ········ ········ • ···· ·· ·······« · · ·· · · · ·· ·· ··· • · · · ·· ·· ·· ·· · · · ft ·· · · ft · · ft ft ft ft ft ft ft · • •••••••••ft · ft ft ft ft ft ft · · ···The above procedure was repeated using the same Caul plate. Even after the repetition 50 times, no deposition to the steel Caul plate was observed.In addition, operation was continued for 50 hours while cleaning by inserting or taking out the cleaning rod from the mixing head of the spray gun once ten minutes. After hours, deposition of a polymeric product of polymeric MDI and water and the like was observed in neither mixing chamber nor spray nozzle. About one second is required for cleaning. It is not necessary to stop the whole line during the cleaning of the mixing chamber, which brings about good productivi ty.Example 2In a similar manner to Example 1 except that the hydroxyl number of the polyol used was changed to 447 mgKOH / g, a board was produced. As shown in Table 1, both the physical properties and productivity of the board were good.Example 3In a similar manner to Example 1 except that the initiator of the polyol used was changed to orthotoluenediamine (ODT) (ethylene oxide content: 40%, hydroxyl number: 447 mgKOH / g), a board was produced. As is shown in Table 1, both the physical properties and productivity of the board so obtained were good.Example 4 ·· ·· ·· • · · · · · • · · · · · ··· ··· · · • · · · • ·· · · · · ··· · · · · · « • · · · · · I «· ·· ·· · ·In a similar manner to Example 1 except that the initiator of the polyol used was changed to orthotoluenediamine / glycerin (G) (molar ratio: 5:1) (ethylene oxide content: 50%, hydroxyl number: 452 mgKOH / g) , a board was produced. As is shown in Table 1, both the physical properties and productivity of the board so obtained were good.Example 5In a similar manner to Example 1 except that the initiator of the polyol used was changed to metatoluenediamine (MTD) (ethylene oxide content: 40%, hydroxyl number: 255 mgKOH / g), a board was produced. As is shown in Table 1, both the physical properties and productivity of the board so obtained were good.Example 6In a similar manner to Example 1 except that the initiator of the polyol used was changed to 4,4'diphenylmethanediamine (MDA) (ethylene oxide content: 40%, hydroxyl number: 452 mgKOH / g) , a board was produced. As is shown in Table 1, both the physical properties and productivity of the board so obtained were good.Example 7In a similar manner to Example 1 except that glycerin (G) (ethylene oxide content: 40%, hydroxyl number: 56 mgKOH / g) was used as an initiator for the polyol, the concentration of the reactive emulsifier was set at 5%, • ·· · · ·· ·· · · · • · ·· · · · · ··· ··· · · ··· · ·· ·· ·· · · · ··· ·· ·· ·· ·· ·· ·· • · · · ·· ··· ··· · • · · ·· · · · • · · · · • · · · · diazabicyclooctane which was a urethane / urea formation catalyst known in the field of urethane was added as a catalyst in an amount of 0.005% and the liquid ratio of the first stream to the second stream was set at 1:1, a board was formed. As is shown in Table 1, the board so obtained was good in both physical properties and productivity.Example 8In a similar manner to Example 1 except that dust chips were used as the lignocellulose-base material, a board was formed. The board so formed had good physical properties at least equal to Type 18 in JIS-A-5908 (which indicates the type of a board having a flexural strength, which is an evaluation standard of JIS concerning the physical properties, not lower than 18 N / mm2in both lengthwise and crosswise directions); and at the same time, it had good product!vi ty.Example 9In a similar manner to Example 1 except that the adhesive was prepared without using zinc stearate which was the mold release agent of the component (D) and instead, a fluorine-base mold release agent (Mold Spat W-833, trade name; product of Asahi Glass Co., Ltd.) was used as an external mold release agent to be coated onto a Caul plate at the time of pressing, a board was formed. As is shown in Table 1, the board so formed had good physical properties and productivity.• ·Example 10In a similar manner to Example 1 except that Polyethylene wax 220MP (trade name; product of Mitsui Chemical Industry Co. , Ltd.) was used as a mold release agent instead of zinc stearate, a board was formed. As is shown in Table 1, the board so formed had good physical properties and productivity.Comparative Example 1In a similar manner to Example 1 except that the mixing was carried out in a mixing pot equipped with an agitation element by the batch system upon preparation of an adhesive, an adhesive was prepared and a board was produced using it.It took 5 hours to completely use up the adhesive in the mixing pot. For about 15 minutes after the production, a board so obtained had good physical properties, which however lowered thereafter. Five hours after the production, polyurea, that is, the reaction product of MDI with water deposited inside of the mixing pot, which required the termination of the board production and cleaning. Comparative Example 2In a similar manner to Example 1 except that the first and second streams were mixed using a static mixer upon preparation of an adhesive, an adhesive was prepared and a board was produced using it. As a result of sampling and visual observation of a portion of the adhesive so obtained, it has been found that there still remained unemulsified MDI• · and therefore emulsifying property was not sufficient. After the continuous operation for 5 hours, polyurea, that is, the reaction product of MDI with water deposited inside of the static mixer, which required the termination of the board production and cleaning.Comparative Example 3In a similar manner to Example 1 except that the injection pressure into the mixing chamber was set at 30 kgf / cm2upon preparation of an adhesive, an adhesive was prepared and a board was produced using it. As a result of sampling and visual observation of a portion of the adhesive so obtained, it has been found that there still remained unemulsified MDI and therefore emulsifying property was insufficient. Besides, the board so obtained had low physical properties.Comparative Example 4In a similar manner to Example 8 except that the injection pressure into the mixing chamber was set at 30 kgf / cm2upon preparation of an adhesive, an adhesive was prepared and a board was produced using it. As a result of sampling and visual observation of a portion of the adhesive so obtained, it has been found that there still remained unemulsified MDI and therefore emulsifying property was insufficient. Besides, the board so obtained had low physical properties.TableSynthetic evaluation < < < < < < < < < < CO CO CO CO Continuous test Good Good Good Good Good Good Good Good Good Good Inferior Inferior Good Good Physical properties of a board N / mm* Peeling strength CM CO 60 - OO o CM CM CO 0.7 90 0.4 0.4 Wet flexural strength (A) 23.0 22.0 o co CM 20.0 21.0 o 23.0 23.0 21.0 o CM 17.0 14.0 13.0 o Dry flexural strength 42.0 41.0 39.0 j 38.0 41.0 25.0 42.0 42.0 I 43.0 44.0 37.0 31.0 o ΙΛ CM 17.0 Cleaning once / 10 min once / 10 min once / 10 min once / 10 min once / 10 min once / 10 min once / 10 min once / 10 min once / 10 min once / 10 min once / 5 hours once / 5 hours once / 10 min once / 10 min Evaluation on dispersibility Good Good 1 CD Good Good Good Good poog Good Good Good Inferior Inferior Inferior Mixing pressure kgf / cmJ 100 100 o o 100 100 100 100 100 100 100 normal pressure - o co o co Mixing method Collisional mixing Collisional mixing Collisional mixing Collisional mixing Collisional mixing Collisional mixing Collisional mixing Collisional mixing Collisional mixing Collisional mixing Batch mixing Static mixer Collisional mixing Collisional mixing Mold release agent Zinc stearate Zinc stearate Zinc stearate Zinc stearate Zinc stearate Zinc stearate Zinc stearate Zinc stearate * * Polyethylene wax Zinc stearate Zinc stearate Zinc stearate Zinc stearate Dispersion medium Water Water Water Water Water Water Water Water Water Water I t Water Water Water Water Reactive emulsifier EDA base PPG EDA base PPG OTG base PPG OTD / G PPG MTD base PPG MDA base PPG GPPG + catalyst EDA base PPG EDA base PPG EDA base PPG EDA base PPG EDA base PPG EDA base PPG EDA base PPG Organic isocyanate Compound Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Polymeric MDI Ligno- cellulose material Lignified fiber Lignified fiber Lignified fiber Lignified fiber Lignified fiber Lignified fiber Lignified fiber Dust chips ! Lignified fiber Lignified fiber Lignified fiber Lignified fiber Lignified fiber Dust chips i2 Ex. 2 Ex. 3 Ex. 4 Ex. 5 Ex. 6 Ex. 7 Ex. 8 Ex. 9 o X LXJ Comp. Ex.1 Comp. Ex. 2 Comp. Ex. 3 Comp. Ex.4external mold release agent was used • 9 • ·As is apparent from the above description, the process of the present invention makes it possible to prepare an isocyanate adhesive without causing the deposition of the polymer of an organic isocyanate to a mixer and pipes.Accordingly, a process for preparing an adhesive which is free from line troubles due to the blocking of the line and is optimum for the continuous process suitable for the industrial production is provided. The process according to the present invention provides an adhesive having good releasability at the time of hot pressing so that it is suited as an industrial process which can produce a high-quality and inexpensive lignocellulose pressed board with good product!vi ty.

Claims

What is claimed is:

1. A process for the preparation of an adhesive for a lignocellulose pressed board, said adhesive being comprised of (A) an organic isocyanate compound, (B) a reactive 5 emulsifier and (C) an emulsifying medium, which comprises injecting a first stream formed of said organic isocyanate compound (A) and a second stream formed of said reactive emulsifier (B) and said emulsifying medium (C) into a mixing chamber under a high pressure of 40 to 300 kg / cm2 and then 10 mixing said streams.

2. A process according to claim 1, further comprising adding a mold release agent (D) to said first stream or second stream.

3. A process according to claim 1 or 2 , wherein said 15 mixing chamber is equipped with a mechanical cleaning means.

4. A process according to claim 3, wherein said mechanical cleaning means cleans inside of said mixing chamber by putting a rod, which is mechanically actuated and substantially fits the inside of said mixing chamber, in and 20 out of said mixing chamber.

5. A process according to any one of claims 1 to 3, wherein said emulsifying medium is water or contains at least water.

6. A process according to any one of claims 1 to 5, wherein said reactive emulsifier (B) is a polyether and / or polyester polyol or contains at least a polyether and / or 5 polyester polyol.

7. A process according to claim 6, wherein said reactive emulsifier (B) contains at least a polyether and / or polyester polyol; said polyether and / or polyester polyol has 2 to8 functional groups and has a structure in which a IQ recurring unit of (CH2CH2-O) amounts to 5 to 70% of the weight of the polyester and / or polyester polyol; and the ratio of said polyether and / or polyester polyol is 0.01 to 70 parts by weight per 100 parts by weight of the organic isocyanate compound (A). 15 8. A process according to claim 6, wherein said reactive emulsifier (B) contains at least a polyether and / or polyester polyol, said polyether and / or polyester polyol contains in its molecule a nitrogen atom, and the ratio of a nitrogen atom is 0.1 to 12.0% based on said polyester and / or 20 polyester polyol. *9. A process according to claim 6, wherein said polyether polyol has been prepared by adding alkylene oxides to at least one compound selected from triethanolamine, diethanolamine, monoethanolamine, orthotoluenediamine, metatoluenediamine, diphenylmethanediamine and polyphenylpolymethylenepolyamine and an amount of ethylene 5 oxide, among said alkylene oxides, is 5 to 70 parts by weight per 100 parts by weight of said polyether polyol.

10. A process according to any one of claims 2 to 9, wherein said mold release agent (D) is at least one substance selected from metallic salts of a saturated and / or 10 unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms and waxes .

11. A process according to claim 10, wherein said metallic salt (C) of a saturated and / or unsaturated aliphatic carboxylic acid having 8 to 28 carbon atoms is at least lg one combination of a substance selected from the group consisting of octylic acid, lauric acid, myristic acid, palmitic acid, stearic acid, oleic acid and behenic acid and another substance selected from the group consisting of zinc, iron, aluminum, calcium, zirconium, magnesium, bar20 ium, nickel, copper and cobalt. frl.

12. A process according to any one of claims 2 to 11, wherein said mold release agent (D) is added in an amount of 1 to 150 parts by weight per 100 parts by weight of said organic isocyanate compound (A).

13. A process according to any one of claims 1 to 12, wherein said organic isocyanate compound (A) is polymethylene polyphenyl polyisocyanate.

514. A process for the production of a lignocetlulose pressed board, which comprises mixing a lignocellulose-base material with an adhesive for a lignocellulose pressed board produced by a process defined in any one of claims 1 to 12, forming a mat from the resulting mixture and then hot pressing the mat.

15. A lignocellulose pressed board obtained by the prpcess as claimed in claim 14.