Method for producing nonslip floor coverings

MYPI1998001686A0Inactive Publication Date: 1998-10-16THOMAS SIEVERS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1998001686
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1997-04-16
Filing Date
1998-04-16
Publication Date
1998-10-16
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods for increasing slip resistance on polished stone and ceramic floors, such as laser bombardment, often compromise aesthetic qualities and reduce process speed, while chemical etching poses safety risks and is labor-intensive.

Method used

A method involving laser treatment followed by continuous hydromechanical post-treatment with acidic sprays and brushes to enhance micro-crater volume without affecting the polished surface, allowing for increased slip resistance without reducing process speed or aesthetic quality.

Benefits of technology

This method effectively enhances slip resistance while maintaining the polished appearance and process efficiency, leveraging the advantages of laser structuring while minimizing the drawbacks of other methods.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

THE INVENTION RELATES TO A METHOD OF MANUFACTURING NON-SLIP FLOOR COVERINGS (1) MADE OF MINERAL MATERIALS, SUCH AS, FOR EXAMPLE, NATURAL STONE, FINE STONEWARE, ARTIFICIAL STONE OR CERAMICS. THIS METHOD IS CARRIED OUT IN A TWO-STAGE PROCESS, THERE BEING PRODUCED ON THE SURFACE OF THE FLOOR COVERINGS (1) OR SLABS, IN A FIRST PROCESS STAGE BY MEANS OF PULSED LASER BOMBARDMENT, STATISTICALLY DISTRIBUTED MICROCRATERS (6) INVISIBLE TO THE HUMAN EYE. THE SURFACE OF THE FLOOR COVERINGS (1) OR SLABS OBTAINED IN THIS WAY IS THEN, ACCORDING TO THE INVENTION, SUBJECTED TO HYDROMECHANICAL AFTERTREATMENT.(FIG 1)
Need to check novelty before this filing date? Find Prior Art

Description

The invention concerns a method for producing a nonslip floor covering made from mineral materials such as for example natural stone, fine stoneware, artificial stone or ceramics.One special application area of the invention is the increasing, i.e. the creation of a slip inhibiting effect on highly polished floors, especially those of the type that are used in public buildings, i.e. buildings with public access as well as in areas where liquid of whatever kind could be deposited upon the floor.Slipping is one of the main causes of injury in Germany today. The severity of such accidents is often underestimated. In order to increase safety shoe soles and floors must be constructed in a slip inhibiting manner. This is necessary especially in locations where glide enhancing media may be deposited upon the floor. In many areas of public life, but also in private life, polished shiny natural stone and artificial stone slabs are commonly utilised as representative floor coverings in dry as well as in wet areas as well as transition areas. It is important here that the slip inhibiting characteristics are co-ordinated harmonically with architectural aesthetics. The evaluation of slip inhibiting properties is carried out according to DIN 51097 (determination of slip inhibiting characteristics - wetted bare-foot areas - access process - sloped floor area) and DIN 51130 - (determination of slip inhibiting characteristics - work rooms and work areas with increased slip risk - access process - sloped floor area) with the aid of a sloped floor area.Measuring equipment for the non-stationary friction measurement [Fb 701 comparative investigation for non-stationary friction measurement on floors (document series by the Bundesanstalt fur Arbeitsschutz)].Various different methods exist for the production, i.e. the increasing of the slip inhibiting characteristics of floors made of natural and artificial stone. Their use depends mostly on where the floor covering is to be laid or where it has already been laid (internal location, external location, degree of soiling that is to be expected, etc.). The most important methods will be briefly described hereafter.During blasting a suitably rough blasting medium is applied to the surface under high pressure. The more or less hard blasting medium will lead to an uneven roughness and a strong matt finish of the surface (DE 31 39 427).PI 98001686During flame blasting highly energetic gas / oxygen flames are created, with which the surface that is to be treated is briefly heated. The effect of these flames is an explosion of the quartzes contained within the uppermost zone of the stone as well as a melting of stone particles which subsequently cool into a glass-like substance which adheres relatively loosely to the surface (DE 35 45 064).The thickening method utilises a thickening tool (thickening hammer), which is equipped with several, evenly spaced chisel tips. During the continuous movement of the tool the thickening hammer hits the surface with a certain frequency (DE 39 33 843).The methods described here or similar methods that utilise abrasive media or chisel-like tools will lead to an increase of safety, but will also lead to the manufacture of less polished surfaces and therefore a substantial loss of sheen and a reduction of the aesthetic value.The coating of surfaces in order to increase slip resistance has the consequence that the treated surfaces are equipped with nipples (DE 33 42 266). Although this method will not change the optical characteristics it has a limited working life, as continuous friction will destroy the coating.The chemical etching of natural stone surfaces incorporates the application of fluoride acidic substances which have an effect especially on feldspar particles (information sheet by the Bundesverband Trittsicherheit, department Public Works). The destruction involves only very few micrometers and the quartz will be mostly protected. The loss of sheen will depend on the length of the application, and the change of the overall optical quality will have to be tested with a piece of trial surface.The use of this method is however restricted to mineral floor coverings. Chemical compositions and concentrations must be adjusted to suit the relevant types of floor covering. Longer application times as well as exact adherence to the correct concentration means that this method cannot or can be integrated only with a high degree of effort into the production process of floor slabs or tiles. An inappropriate handling or disposing of fluoride acidic substances will also lead to an increased risk with regard to working and environmental safety.PI 98001686DE 195 18 270, i.e. WO 96 / 36469 also offers a nonslip floor covering and a method for the production of the same, whereby the slip inhibiting effect is here achieved through the creation of a tight mesh of micro-craters upon the surface of the floor covering, which preferably consists of polished natural stone or fine stoneware slabs, which will be invisible to the human eye, with the aid of laser bombardment. This solution represents a substantial improvement in comparison with the previous methods of prior art.An increasing of the slip inhibiting effect, which will be desirable in certain wet areas, can however be achieved with the aid of laser bombardment through an increasing of the crater frequency and an enlargement of the lateral expansion and an increasing of the depth of the crater itself. One disadvantage of this is the fact that it will lead to a clear effect on optical characteristics, and especially to a loss of sheen. A further disadvantage is the fact that an increasing of the crater frequency and size will lead to reduced process speeds. If the crater size is increased conventional pulse laser performances are often no longer sufficient.It is therefore the purpose of this invention to offer a method for the production of nonslip floor coverings with which the slip inhibiting characteristics can be increased whilst the representative surface characteristics one the one hand are not negatively affected, and a reduction of the process speed will not occur on the other hand, and with which all of the advantages of laser structuring as opposed to other methods of slip inhibition can be retained.This task is solved in accordance with the invention by a method according to one or more of the Claims 1 to 28.It is of special importance here that the nonslip floor covering is to be produced according to DE 195 18 270, i.e. WO 96 / 36469 and that it is subsequently subjected to a continuous hydromechanical post-treatment. This hydromechanical post-treatment can preferably be carried out within the same production plant immediately following the laser bombardment whilst maintaining the same process speed, so that the total process that results out of the 2 process steps (laser bombardment and hydromechanical post-treatment) can be carried out continuously.However, in certain cases, for example when laser treated floor coverings are to be hydromechanically post-treated only once they have been laid at their intendedPI 98001686 location, it may be advantageous if both process steps are carried out separately, i.e. not continuously.Preferred embodiments of this total process are illustrated in the Patent Claims 2 to 28.According to the method of this invention the laser treated surface of the horizontally conveyed floor coverings, i.e. slabs are sprayed at least once with an acidic, preferably lightly acidic liquid for a brief period during the continuous slab advancing process.Following each one of these spray processes the spray liquid will preferably be evenly spread across the surface of the floor coverings, i.e. the slabs with the aid of brushes or a rake and surplus liquid removed.This even distribution will preferably be carried out in such a way that the spray liquid remains only in the recesses and the micro-craters created by the laser treatment, and not on the polished surface of the floor coverings, i.e. slabs. The quantity and dosing of the liquid should be adjusted in such a way that it is more or less the same as the volume of the recesses and micro-craters.Due to the effects of the laser treatment the surface of the craters is microscopically very rough and is therefore rather large in relation to the crater volume. This results in a very good effectiveness of the diluted acid within the craters that have been created by the laser treatment and in the micro pores that are present depending on the type of slab despite having been polished previously. The pH value and the soaking time in comparison with the substantially diluted acids used for the chemotechnical treatment of floor coverings according to this invention should be chosen in such a way that the polished surface will not be affected thanks to the excellent soaking conditions, but that some surface particles within the crater are loosened and that the volume is therefore increased. Those craters that are located within the area of the feldspar components of the natural stone or fine stoneware slabs should preferably be enlarged.It is important to point out at this time that the soaking time of the acidic spray liquid depends on many factors, and especially on the process speed, the length of the path between the first and the last spray process prior to thePI 98001686 cleaning process the concentration of acidIt is also important that the effectiveness of the acid, which can also be concentrated and will depend on individual applications, is applied as far as possible only to the recesses and micro-craters, and that it will not affect the rest of the polished surface.Following the hydromechanical treatment and a subsequent short soaking time of the acid within the craters, preferably with a duration of between 60 and 150 seconds, the slabs are once more sprayed with a liquid, preferably under high pressure, and are brushed once more. Depending on the pH value of the first liquid the liquid for the complete naturalisation can consist of water or a slightly basic liquid (for example diluted lye).One advantageous embodiment can incorporate the fact that the pH value of the drained-off liquid can be tested continuously and that this value can be used as a control parameter for the pH value of the cleaning liquid.Thanks to the mechanically stronger effect of the brushes in comparison with the effect of the acid grain particles that are no longer attached to the mineral components of the floor covering slabs are removed from the craters, as they would otherwise lead to a reduction of the crater volume.Following the cleaning, i.e. neutralising process the slabs are dried with the aid of hot air.The greatest advantage of the method according to this invention is the fact that the same maintains all of the advantages of the laser structured floor coverings,i.e. slabs, whilst at the same time substantially increasing the slip inhibiting effect.The following description of various examples will now illustrate the invention further.Embodiment Example 1This embodiment of the method according to embodiment example 1 is illustrated in Fig. 1. Conveyed floor covering slabs made of fme stonework that have been treated with laser bombardment to be nonslip, and which are of a size measuring 60 x 60 x 1,5 cm are here post-treated according to the method of thisPI 98001686 invention in a production plant. The slabs (1) are conveyed upon a transport conveyor belt (2) at a relatively high speed of 3 m / min. A diluted liquid (4) containing an acid with an acid concentration of 50% of the possible maximum is applied onto the polished slab surface (5) containing the micro-craters (6) via a plurality of holed nozzles with a width of 58 cm incorporated into a spraying arm (3). A rotating brush (7) with soft bristles is positioned at a distance of 10 cm in the direction of the advance of the slabs and behind the spraying arm. This rotating brush (7) distributes the liquid (4) evenly into the micro-craters (6) and into the natural recesses of the slab (1) and removes surplus acid from the surface (5) at the same time. A second spraying arm (8) is positioned at a distance of 50 cm from the spraying arm (1), and this applies a diluted lye (9) according to the concentration of the acid utilised onto the slab surface (5) for neutralisation purposes. Analogue to the spraying arm (3) and behind the spraying arm (8) a rotating brush (10) is located, which does however run at a higher rotation speed and with a greater application pressure. In this way a removal of the liquids from the recesses and from the slab surface is possible at the same time as the distribution and intensifying of the neutralisation of the spray liquid (4). Immediately after the brush (10) the slabs (1) are advanced at an angle of 30° facing upwards and a compressed air jet (11) is applied against the advancing direction at an angle of 30° from the slab surface from a slotted nozzle (12) onto the said slab surface, whereby any remaining liquid is removed from the surface (5) as well as from the micro-craters (6) and other recesses. After that a post-drying process of the slabs (for example removal of residual dampness from possible porous hollows) is carried out with the aid of one or more hot air showers (13) and the slabs (1) are advanced further, for example to a packaging station.Embodiment Example 2The method according to embodiment example 2 is illustrated in Fig. 2. The laser-treated granite slabs (1) with a dimension of 30 x 30 1 cm are initially continuously conveyed upon a transport belt (20) from a work station (14) in 2 rows next to one another, i.e. with a total width of 60 cm, where the nonslip characteristic is applied through the targeted creation of micro-craters (6) with the aid of laserPI 98001686 bombardment, towards a post-treatment area (21). Technologically the advancing speed of the slabs (1), i.e. 0,6 m / min, will depend on the laser treatment. Within the drying area (16) the slabs (1) will initially be advanced under a spraying arm (3), which is equipped with a rows of holes to a width of 58 cm, whereby the same holes incorporate a jet diameter which is smaller in comparison with example 1 by a factor of 5. Here a liquid (4) containing diluted fluoride acid with an acid concentration of 10% of the possible maximum is sprayed onto the polished slab surface (5) containing the micro-craters and the natural recesses (6). The total sprayed amount of liquid (4) is only approximately 15% greater than the volume of the craters and recesses that are already present. At a distance of approximately 15 cm in the direction of the advance and behind the spraying arm (3) a rotating brush (7) with soft bristles is located. The axis of the brush in this example is positioned at an angle of 80° towards the advancing direction. The rotating brush distributes the liquid (4) evenly across the micro-craters and the natural recesses (6) and removes excess liquid from the surface. At a distance of 1 metre from the spraying arm (3) a further spraying arm (8) is positioned in this example, whereby the same sprays a quantity of diluted lye (9) onto the slab surface (5) which stands in direct relation to the utilised acid concentration and is greater than the sprayed quantity of the same acid by a factor of 10. Immediately behind the spraying arm (8) a further rotating brush (10) is located in an analogue position in comparison with the brush (7). This is equipped with harder bristles, rotates ten times as fast as the brush (7), and is pressed harder against the slab surface. Spraying arm (8) and brush (10) are together fitted upon a mechanism (14) whose distance to the spraying arm (3) is adjustable. This serves for the varying of the necessary soaking time according to the desired degree of effectiveness of the nonslip inhibition and bears in mind the various slab materials at a certain process speed. Following the last spraying and brushing process a final spraying process takes place, whereby water is sprayed from a slotted jet (15) with a volume stream of 10 1 / min onto the slab surface (5). This will ensure that possible residuals of the already neutralised mixture consisting of the liquids (9) and (4) as well as possible remaining residuals of mechanical contaminants and remains are removed from the slab surface (5) and completely removed from the micro-craters and recesses (6). Following this the slabs are conveyed through a drying area (16),PI 98001686 where the same are dried with the aid of warm air which is blown through hot air showers (17) as well as IR irradiation (18). Between the working area of the brush (19) and the slotted jet (15) as well as between the slotted jet (15) and the drying area (16) synthetic rakes (19) are positioned, which act as a scraper for the liquid.It is a matter of course that the liquids are collected separately following the individual wet areas (1. and 2. spraying and brushing process, spraying process) and treated accordingly, and that the same are then either returned to the relevant cycle or routed into the waster water system following the relevant treatment.

Claims

CLAIMS :

1. Method for producing nonslip floor covering (1) such as slabs from mineral materials such as for example natural stone, fine stoneware, artificial stone or ceramics with the aid of a two-stage process and targeted pulsed laser bombardment, whereby microcraters which cause a suction effect and which are invisible to the human eye are created and statistically distributed on the surface of the floor covering (1) , characterised in that the surface of the laser-structured floor covering (1), i.e. floor covering slabs that are created during the second process step, are further subjected to a targeted hydromechanical post-treatment, characterised in that the same hydromechanical post-treatment is carried out in such a way that the surface of the laserstructured floor covering, i.e. that of the slab will be sprayed with liquid (3,8) at least twice, whereby at least one of the spray processes serves for the loosening of particles from the surface of the micro-craters and therefore their enlargement, and whereby the last spray process (8) serves to clean and / or neutralise previous spray liquids from the surface of the floor covering (1) or slabs.

2. Method according to claim 1, characterised in that the hydromechanical post-treatment is applied only to the recesses of the floor covering (1), i.e. slabs.

3. Method according to claim 2, characterised in that the hydromechanical post-treatment is applied only to the micro-craters that have previously been created with the aid of pulsed laser bombardment. PI 980016864. Method according to one or more of the preceding claims 1 to 3, characterised in that at least one process during which the spray liquid is distributed evenly on the surface of the floor covering, i.e. slabs follows each spraying process and whereby surplus spray liquid is removed (12) from the said surface and whereby subsequently at least one drying process (13) is carried out.

5. Method according to one or more of the preceding claims 1 to 4, characterised in that the hydromechanical post-treatment is carried out in such a way that the surface of the floor covering (1), i.e. slabs are twice sprayed with (3,8),whereby the second spraying process serves to clean and / or neutralise previous spray liquids from the surface of the floor covering (1) and / or slabs after the first and the second spray process has been completed, during which the spray liquid is evenly distributed on the surface of the floor covering (1), i.e. slabs, and whereby surplus spray liquid is removed (12) from the said surface and where subsequently at least one drying process (13) is carried out.

6. Method according to one or more of the preceding claims 1 to 5, characterised in that, during one or more of the spraying processes that serve for the loosening and therefore the enlarging of the surface of the microcraters an acid is used as the spray liquid.

7. Method according to claim 6, characterised in that the said acid that is used consists of an inorganic acid.

8. Method according to claim 7, characterised in that the said acid that is used consists of a halogen-hydrogen PI 98001686 acid.

9. Method according to claim 8, characterised in that the said acid that is used consists of fluoride acid (HFacid).

10. Method according to one or more of the preceding claims 6 to 9, characterised in that the said acid that is used consists of a dilute acid.

11. Method according to claim 10, characterised in that the said acid that is used is present within a solution with a concentration of a maximum 50% of its maximum concentration in water.

12. Method according to claim 11, characterised in that the said acid that is used is present within an aqueous solution with a concentration of a maximum 10% of its maximum concentration in water.

13. Method according to one or more of the preceding claims 1 to 12, characterised in that the final spraying process (8) is carried out in such a way that the liquid of the previous spraying processes is neutralised.

14. Method according to claim 13, characterised in that the spray liquid of the final spraying process (8) consists of a neutral or base liquid.

15. Method according to claim 14, characterised in that the pH-value of the spray liquid of the final spraying process (8) is a maximum of pH 9.

16. Method according to claim 15, characterised in that PI 98001686 the spray liquid of the final spraying process (8) consists of water (pH-value = 7), whereby the applied quantity of water is larger than the quantity of spray liquid in the spraying process that immediately preceded the same application.

17. Method according to one or more of the preceding claims 1 to 16, characterised in that, a further process is carried out following the final spraying process (8), whereby the said further process removes the spray liquid of the previous process without leaving a residual either on the surface, within the recesses, or in the microcraters of the surface of the floor covering (1), i.e. slabs .

18. Method according to claim 17, characterised in that the spray liquid of the final spraying process (8) is removed from the surface of the floor covering (1) i.e. slabs with the aid of a gas stream that is applied at high pressure and / or high velocity.

19. Method according to one or more of the preceding claims 1 to 18, characterised in that, with the exception of the final spraying process (8) the process for the even distribution of the relevant spray liquids on the surface of the floor covering (1) i.e. slabs is carried out in such a way that the relevant spray liquid remains only in the recesses, i.e. the micro-craters, and not on the rest of the polished surface.

20. Method according to claim 19, characterised in that, with the exception of the final spraying process (8) the distribution of the relevant spray liquid and the removal (12) of the surplus spray liquid is carried out with the PI 98001686 aid of a brushing process and / or a rake.

21. Method according to claim 20, characterised in that, in the case of the brushing process rotating brushes (7) with soft bristles, a low rotation speed and low application pressure are used.22 Method according to one or more of preceding claims 1 to 21, characterised in that, the process for the even distribution of the spray liquid, i.e. the mixture consisting of the same and the previous spray liquid is removed (12) completely from the polished surface of the floor covering (1), i.e. slabs as well as from the recesses and the micro-craters following the final spraying process (8), whereby the process steps according to claim 17 or 18 can be omitted in this case.

23. Method according to claim 22, characterised in that an even distribution is achieved with the aid of a brushing process.

24. Method according to claim 23, characterised in that rotating brushes (10) with high rotational speed and relatively high application pressure are used.

25. Method according to one or more of the preceding claims 4 to 24, characterised in that the final drying process is carried out with the aid of hot air showers.

26. Method according to claim 25, characterised in that the hot air showers are supplied with the heated and filtered exhaust air routed from the exhaust mechanism of the pulsed laser process of the first process step.

27. Method according to one or more of the preceding PI 98001686 claims 1 to 26, characterised in that the entire process is carried out during the first and the second process step continuously within a single system, whereby the speed of the entire process, i.e. the processing speed with which the floor covering (1), i.e. slabs travel through the entire process, i.e. the entire system in this case is determined by the soaking time of the individual spray liquids into the floor covering (1), i.e. slabs during the first process step (laser treatment), and in that with the exception of the final spraying process (8) strong undiluted acids are used as the spray liquid of the final spraying process (8) in this case, and in that the spray liquid of the final spraying process (8) is adjusted accordingly.

28. Method according to one or more of the preceding claims 1 to 27, characterised in that the pH value of the liquid drained from the final spraying process (8) is measured and used as a control value for the base characteristics of the final spray liquid.