Process for fabricating a magnetic disk substrate

MYPI1998002075A0Inactive Publication Date: 1998-11-28RESONAC HOLDINGS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1998002075
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1997-05-28
Filing Date
1998-05-08
Publication Date
1998-11-28
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional processes for fabricating magnetic hard disk substrates, such as G-G and T-G processes, face challenges in achieving sufficient surface flatness and reducing substrate-to-substrate thickness variation due to limitations in stock removal and grinding stress, leading to difficulties in meeting severe requirements for high-density recording.

Method used

A process involving precision turning with an NC automatic lathe for stock removal of 20 to 150 μm followed by grinding with a depth of 10 μm or less, using a double-surface grinding machine, to achieve uniform surface flatness and thickness distribution, with specific conditions for rotational speed, feed rate, and grinding pressure.

Benefits of technology

This approach results in a magnetic hard disk substrate with excellent surface flatness and reduced substrate-to-substrate thickness variation, enabling narrower gaps between the head and medium for high-density recording without deteriorating the surface quality.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

IT IS AN OBJECT OF THE PRESENT INVENTION TO PROVIDE A MAGNETIC HARD DISK SUBSTRATE HAVING AN EXCELLENT SURFACE FLATNESS. ACCORDING TO THE PRESENT INVENTION, THERE IS PROVIDED THE MAGNETIC HARD DISK SUBSTRATE AND A PROCESS OF FABRICATING THE SUBSTRATE IN WHICH AN ALUMINUM ALLOY BLANK, BEFORE AN NI-P PLATING TREATMENT, IS SUBJECTED TO PRECISION TURNING, WITH A STOCK REMOVAL ON EACH SURFACE IN THE RANGE OF 20 TO 150 ?M IN DEPTH, FOLLOWED BY GRINDING, WITH A STOCK REMOVAL ON EACH SURFACE OF 10 ?M OR LESS IN DEPTH. FIGURE 1
Need to check novelty before this filing date? Find Prior Art

Description

SPECIFICATIONPROCESS FOR FABRICATING A MAGNETICDISK SUBSTRATEBACKGROUND OF THE INVENTIONa) Field of the InventionThe present invention relates to a process of fabricating a magnetic hard disk substrate having an excellent surface flatness .b) Description of the Prior ArtThere has been a general trend toward a higher density and larger capacity of a magnetic hard disk devise as a storage device of a computer and the like and it has, therefore, been important technical aspects to finish a magnetic hard disk substrate used for the device to a desired surface roughness and flatness. Particularly, there has been achieved a conspicuous development in reduction of levitation based on improvement on the head side part for realization of high density recording and thereby, a gap between a head and a medium has been narrowed and in company with this, further improvement on not only a surface flatness of a magnetic hard disk substrate but a surface roughness thereof has strongly been demanded in order to prevent a head crash.It is common that a magnetic hard disk substrate is fabricated by a process comprising the steps of: obtaining a blank by blanking a rolled coil of aluminum or aluminum alloy(hereinafter referred to as aluminum, simply); grinding a surface of the blank so as to have surface damages, wavinessPI 98002075 and the like removed to attain a substrate; effecting Ni-P plating on the surface; performing finish polishing on the plated surface; thereafter performing magnetic sputtering on the polished surface to form a magnetic coating layer ; and applying an overcoat on the layer to obtain a sputtering medium. In order to control a surface roughness and flatness within a predetermined range in the process, in the grinding step applied prior to the Ni-P plating step, the magnetic hard disk substrate (as a blank) is subjected to rough grinding by a grinding stone with a grain size of the order of # 800 in a double-surface grinding machine, which is followed by finish grinding by a grinding stone with a grain size of the order of # 3000 in the grinding machine. This kind of grinding is called a G-G (Grinding-Grinding) process, for this grinding step comprises two sub-steps of grinding.In a conventional G-G process, however, since a first step of rough grinding has been applied on plural Aluminum blanks in one operation by a grinding stone or the like, a removal stock by grinding is limited and a stock removal large enough in grinding off a bow, waviness or the like has been a hard issue to be achieved. Therefore, in a second step of grinding, which is performed following the rough grinding in a similar way thereto, a removal stock is obliged to be larger, even with which it is still difficult to reduce a substrate-to-substrate thickness variation. Instead of G-G process, there has well been known a process, which is a so-called T-G process, in which in a first step, turning is performed and in a second step, grinding is performed. According to the T-G process, as a first step, turning by use of a precision lathe is performed and as ·· ·· ·· ·· ·· ······· • ·· ·· ·· · · · · · • ···· · · · · ···· ···· · · · · · · · • · ·· ·· · ·· · ·· ·· ·· ···· · · · ·· • · · · · · • · · · · · • · · · · · ··· ···· · • · · · • · · · · · · ·· · · 9 9 · · · · • · · · · · · • ··· · ···· ······ · • ·· · · · · · ·· ·· · · · · · · a second step following the first step, grinding is perfonned, so that while a bow, waviness and the like of a magnetic hard disk substrate are eliminated, a magnitude of a grinding stress is dispersed by an uneven stock removal, which is, in turn, caused by a substrate-to-substrate thickness variation, and a deteriorated surface flatness of a substrate is resulted, which have been causes for making severe requirements for a magnetic hard disk substrate difficult to be satisfied.SUMMARY OF THE INVENTIONIt is an object of the present invention to provide a magnetic hard disk substrate having an excellent surface flatness and a process of fabricating the same.The present invention has been made based on findings that a aluminum magnetic hard disk substrate is prevented from deterioration of a surface flatness and can satisfy severe requirements therefor by application of process steps of removing stock of a blank by a depth in the range of 2 0 to 150 μ m by precision turning with an NC automatic lathe to adjust a thickness of a substrate; and further removing stock of the blank by a depth of 10 μ m or less by grinding. That is, according to the present invention, there is provided an aluminum magnetic hard disk substrate and a process of fabricating the aluminum magnetic hard disk substrate in which an aluminum alloy blank before an Ni-P plating treatment is subjected to precision turning with a stock removal on each surface in the range of 20 to 150 μ m in depth, which is followed by grinding with a stock removal on each surface of 10 / zm or less in depth.• ·The precision turning is preferably performed in a way in which both surfaces of a blank are machined in uniform manner, a rotational speed of a main spindle of an NC automatic lathe is set at a value in the range of 500 to 10000 rpm, or preferably in the range of 3000 to 6000 rpm and a feed rate of a diamond tool is set at a value in the range of 0.010 to 0.500 mm / rev., or preferably in the range of 0.05 to 0.20 mm / rev. The grinding is preferably performed on two or more blanks simultaneously and a spread of a thickness distribution of blanks to be ground in one batch is prepared at a value of 10 μ m or less, or preferably 5 μ. m or less.Other objects and features of the present invention will become obvious from the following description or the recitation in the appended claims.DESCRIPTION OF THE DRAWINGSFig. 1 is a graph showing a relation between the change in surface flatness and the stock removal in finish grinding.DESCRIPTION OF THE PREFERRED EMBODIMENTSThe present invention will in a more detailed manner be described below. As mentioned above, the present invention has a feature that for the purpose of improvement on a surface flatness after grinding, a blank is first subjected to precision turning by an NC automatic lathe and the blank is further subjected to grinding by a double-surface grinding machine after a heat treatment following the turning step. Each of the turning and grinding steps will be described.First of all, a doughnut-shaped aluminum blank, which isa starting raw material, is subjected to facing by an NC automatic lathe with a diamond tool and then subjected to chamfering, to finish the blank to a predetermined shape and dimensions. In this case, a double-surface uniform turning method proposed in Japanese Patent Laid-open publication No. 192336 / 1997 already filed by the same applicant as the present application is employed in the facing step in order to not only prevent bowing of a substrate from occurring, which is produced due to a difference in stock removal between first and second turning surfaces, but also suppress a substrate-to-substrate dispersion of thickness to a predetermined value or less. In this double-surface uniform turning method, turning is conducted with a cutting depth in the range of 20 to 150 fl m, preferably in the range of 50 to 150 / z m on each surface. If a cutting depth is less than 20 fl m, the depth is not sufficient to eliminate a bow, waviness and the like and in addition a turning resistance is larger. In order not to deteriorate a surface flatness of a substrate, turning is conducted under the following conditions, which are: a rotational speed of a main spindle of an NC automatic lathe is preferably set in the range of 500 to 10000 rpm, or more preferably in the range of 3000 to 6000 rpm and a feed rate of a diamond tool is set in the range of 0.010 to 0.500 mm / rev., or preferably in the range of 0.05 to 0.20 mm / rev.The substrate after the turning step is subjected to a heat treatment in a heating furnace in order to release a residual stress distributed in the substrate. With this heat treatment, not only can the substrate achieve a surface flatness equal to that of an aluminum blank, but a spread of a thickness• · • · distribution of the substrate can also be confined within ± 5 / zm.The blank after the heat treatment is subjected to grinding in a stock removal as small as a depth of 10 μ. m or less, preferably 5 μ m or less by a double-surface grinding machine. Grinding conditions in this grinding step are that a rotational speed of top and bottom surface plates are set in the range of 10 to 60 rpm, a rotational speed of a sun gear is in the range of 1 to 3 rpm and a grinding pressure is in the range of 30 to 100 g / cm2. If such grinding conditions are applied on blanks each with precisely controlled dimensions and an excellent surface flatness, not only can a stock removal of the blanks be equal to each other but uniform grinding can be realized, even when plural blanks are simultaneously ground. A relation between the change in surface flatness in grinding (a surface flatness after grinding minus an original surface flatness of an aluminum alloy blank) and the stock removal is shown in Fig. 1. As seen from Fig. 1, a change in surface flatness can be 2 / z m or less in the case where a stock removal by grinding is limited to 10 / zm or less.ExampleA doughnut-shaped aluminum alloy blank (A5086) was subjected to turning with a stock removal of 50 to 100 μ m in depth for each surface in a uniform manner on both sides of the blank by an NC automatic lathe by use of a diamond tool according to a method described in the Japanese Patent Laid-open publication No. 192336 / 1997 and as a result, the blank was finished to dimensions of an outer diameter of 95 mm, an inner diameter of 25 mm and a thickness of 0.8 mm. In this example, • · ·· ·· ······· • · · · ·· · ·· • · · · · · · · · • · · ···· · ···· · · · · · • · · · · > · · » · I • « · · • · • · 4 turning conditions were set that a rotational speed of a main spindle of the lathe was 5000 rpm and a feed rate of the diamond tool was 0.3 mm / rev. The blanks thus machined were ground with a batch composed of 15 pieces at one time. A maximum spread of blank-to-blank thickness distribution in a batch of blanks to be ground was prepared within 10pm or less. The blanks which have been subjected to the turning step were heated at 25 0°C in a heating furnace for 60 min to remove a residual stress in the substrates and the substrates were subseguently ]_0 subjected to grinding. Grinding conditions were set in such a manner that a rotational speed of top and bottom surface plates was 30 rpm, a rotational speed of a sun gear was 2 rpm and a grinding pressure was 5 0 g and a grinding operation was conducted so as to remove a stock of 5 pm in depth on each side. A change in surface flatness after the grinding operation was lpm and the surface was further treated by an ordinary process including Ni-P plating, finish polishing, magnetic sputtering, overcoat and the like to obtain a magnetic hard disk substrate. Thus obtained substrates had, in a practical sense, no dispersion in substrate-to-substrate thickness distribution and each an excellent surface flatness on a substrate as well. There is a case where a heat treatment is inserted between the steps of Ni-P plating and polishing in order to eliminate a strain in the substrate caused by the plating treatment.According to the present invention mentioned above, a magnetic hard disk substrate having an extremely excellent flatness can be obtained by a simple process and besides there can be obtained a magnetic hard disk substrate which can sufficiently be adapted for a narrower gap between a magnetic • · · · • · · · · • · · · · ··· · · · • · · · ·· ·· ·· ·· ·······« • · · · · · · • · · · · ··· • · · · · · • · · · · · · ···· ·· · ·· ·· ······ · ·· ·· ·· • · head and a medium in the case of reduced levitation of the head accompanying the recent progress in high-density recording.

Claims

CLAIMS 1. A process of fabricating a magnetic hard disk substrate comprising the steps of: providing a blank made of aluminum or an aluminum alloy and having two opposing surfaces to be finished; turning said blank with a lathe to effect the 5 removal of from 20-150 pm in depth of stock from each of said surfaces; and grinding said blank to effect a stock removal of not more than 10 pm in depth from each of said surfaces.

2. A process according to claim 1, wherein the precision turning is performed in 10 a way in a which both surfaces of the blank are simultaneously machined in uniform manner.

3. A process according to claim 2, wherein the turning step is performed step by an NC automatic lathe, a rotational speed of a main spindle thereof is set at a 15 value in the range of 500 to 10000 rpm and a feed rate of a diamond tool is set at a value in the range of 0.010 to 0.500 mm / rev.

4. A process according to claim 3, wherein the rotational speed of a main spindle is set at a value in the range of 3000 to 6000 rpm and the feed rate of a 20 diamond tool is set at a value in the range of 0.05 mm to 0.20 mm / rev.

5. A process according to claim 1, wherein the grinding is performed simultaneously on two or more substrates which have already been subjected PI 98002075 to the turning step, and a spread of a substrate-to-substrate thickness distribution of which is prepared at a value of 10 pm or less for one batch.

6. A process according to claim 5, wherein the grinding is performed 5 simultaneously on two or more substrates which have already been subjected to the turning step, and a spread of a substrate-to-substrate thickness distribution of which is controlled at a value of 5pm or less for one batch.

7. A process according to claim 1, wherein the substrate, after the turning step, 10 is subjected to a heat treatment in a heating furnace in order to release a residual stress distributed in the substrate before the grinding step.

8. A process according to claim 6, wherein conditions in the grinding step are such that a rotational speed of top and bottom surface plates are in the range of 15 10 to 60 rpm, a rotational speed of a sun gear is in the range of 1 to 3 rpm and a grinding pressure is in the range of 30 to 100 g / cm2under control.