Sealed compressor having pipe connectors and method of joining pipe connectors to sealed casing
Patent Information
- Application Number
- MYPI1998002947
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1997-06-30
- Filing Date
- 1998-06-29
- Publication Date
- 1998-12-30
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional sealed compressors require flux and flames for silver-brazing, which can lead to flux residue, annealing of copper pipes, and compromised sealing due to thermal expansion, making it difficult to manage HFC refrigerants and ester-based lubricants, and increasing manufacturing costs.
The use of copper-plated steel sleeves that are resistance-welded and copper-brazed to the sealed casing, eliminating the need for flux and flames, and allowing for hermetic welding without compromising the compressor's reliability or structural integrity.
This method enables reliable hermetic sealing without flux residue or thermal expansion issues, ensuring the integrity of HFC refrigerants and ester-based lubricants, while reducing manufacturing costs and simplifying the welding process.
Abstract
Description
Sealed Compressor Having Pipe Connectors AndMethod Of Joining Pipe Connectors To Sealed CasingBACKGROUND OF THE INVENTION(Field of the Invention)The present invention relates generally to a sealed compressorfor use in a refrigerator, an air conditioner or the like and, in particular butnot exclusively, to pipe connectors for connecting suction and dischargepipes to a sealed casing of the sealed compressor. The present inventionalso relates to a method of joining the pipe connectors to the sealed casing.(Description of Related Art)Fig. 1 depicts a conventional sealed compressor having a sealedcasing 101 in which a motor section 102 and a compression section 103 areboth accommodated. The sealed casing 101 is provided with a suction pipeconnector 104 secured thereto through which a refrigerant is introducedthereinto and a discharge pipe connector 105 secured thereto throughwhich a compressed refrigerant is discharged therefrom. The suction pipeconnector 104 and the discharge pipe connector 105 lead to an evaporator(not shown) and a condenser (not shown), respectively, to form arefrigeration cycle. Because both the evaporator and the condenser areconnected to copper pipes, a material which can be readily connected to thecopper pipes, for example, by copper-brazing is selected for the suction pipeconnector 104 and the discharge pipe connector 105. For this reason, boththe suction pipe connector 104 and the discharge pipe connector 105 aregenerally made of copper pipes. When each of the suction pipe connector104 and the discharge pipe connector 105 is secured to the sealed casing 101,which is generally made of steel, it is the general practice that a portion ofthe pipe connector 104 or 105 is first inserted into a hole defined in thesealed casing 101 and is then rigidly secured thereto by silver-brazing withthe use of flux.More specifically, as shown in Fig. 1, the sealed casing 101 hasa hole defined therein in alignment with a suction hole 106 defined in thecompression section 103. An external suction sleeve 107 is inserted intothe hole of the sealed casing 101 and is secured thereto. The compressionsection 103 also has a suction sleeve insertion hole 108 defined therein so asto be continuous to the suction hole 106. The suction sleeve insertion hole108 is positioned radially outwardly of the suction hole 106 and has adiameter slightly larger than that of the suction hole 106. The suctionpipe connector 104 includes the external suction sleeve 107 referred toabove and an internal suction sleeve 109 pressed into the suction sleeveinsertion hole 108 so that a low-pressure refrigerant to be introduced intothe sealed casing 101 may be separated from a high-pressure refrigerantinside the sealed casing 101. The length of the internal suction sleeve 109is determined so that an outer end thereof may be positioned radiallyoutwardly of an outer end of the external suction sleeve 107. After asuction pipe 110 has been inserted into the internal suction sleeve 109pressed into the suction sleeve insertion hole 108, the suction pipe 110, theinternal suction sleeve 109 and the external suction sleeve 107 aresimultaneously hermetically secured together by brazing, therebyseparating the external atmosphere, the low-pressure refrigerantintroduced into the sealed casing 101, and the high-pressure refrigerantinside the sealed casing 101 from one another.In the above-described construction, the internal suction sleeve109 is made of a copper pipe or a copper-plated steel pipe, while theexternal suction sleeve 107 and the discharge pipe connector 105 bothsecured to the sealed casing 101 are generally made of copper pipes. Thesuction pipe 110 is also generally made of a copper pipe.The sealed compressor of the above-described construction hasa problem in that in applications where a copper pipe is hermeticallyconnected to the steel-made sealed casing 101 by silver-brazing, flux isinevitably required, which must be removed after the brazing. Removal ofthe flux is generally carried out in hot water in which the flux dissolves.On the other hand, HFC refrigerants listed as candidates foralternative refrigerants that cause no destruction of the ozone layer aregenerally used with an ester-based lubricant compatible therewith. Theester-based lubricant has a tendency to cause hydrolysis, which in turnproduces acids. Accordingly, if a compressor contains an HFC refrigerant,it is necessary to manage the compressor so that water contained thereinmay be as small as possible. Furthermore, even if the amount of chlorinecontained in the flux is extremely small, it acts to promote decomposition ofthe HFC refrigerant and that of the ester-based lubricant. Because of this,complete removal of the flux is required.Conversely, silver-brazing requires a process in which waterand chlorine-containing impurities remain that must be most removedduring the manufacture of a compressor for use with an alternativerefrigerant. In addition, it is difficult to immerse a relatively large bodysuch as the sealed casing in hot water, and if the compressor is of acomplicated structure, it is very difficult and time-consuming to completelyremove water that has been used for removal of the flux.Also, during brazing, members to be joined together must beheated to a temperature at which a brazing material melts. To this end,such members are generally heated with flames of, for example, a torch.By so doing, copper pipes as the connectors are annealed and reduced instrength. The flames produce on the members an oxide layer, whichsometimes promotes deterioration of a lubricant or a refrigerant.Furthermore, because the copper-made pipe connector has arelatively large thermal expansion coefficient, the pipe connector expandsdue to heat generated during brazing and contracts due to subsequentcooling, thus deteriorating the sealing properties between the pipeconnector and the insertion hole thereof. Also, component parts of thecompression section are likely to be deviated from their desired positions byrelatively large forces applied thereto. If a steel pipe is used for the pipeconnector, it must be finished into a desired size and then copper-plated,resulting in an increase in the manufacturing cost.SUMMARY OF THE INVENTIONThe present invention has been developed to overcome the above-describeddisadvantages.It is accordingly an objective of the present invention to providea sealed compressor having a sealed casing to which pipe connectors arehermetically joined without brazing which requires flux and flames.Another objective of the present invention is to provide amethod of joining pipe connectors to the sealed casing without brazing.In accomplishing the above and other objectives, the sealedcompressor according to the present invention includes a sealed casing inwhich a motor section and a compression section are both accommodated,and also includes a first sleeve having a first end and a second end oppositeto each other. The first end is inserted into a sleeve insertion hole definedin the compression section to allow a refrigerant to flow therethrough, whilethe second end is hermetically brazed to a copper pipe disposed outside thesealed casing. The first sleeve is formed by deep-drawing a copper-platedsteel plate into a generally cylindrical shape.The deep-drawing reduces the manufacturing cost of the firstsleeve. Furthermore, the use of the copper-plated steel plate enables thefirst sleeve to be resistance-welded to the sealed casing and to be copper-brazed to the copper pipe.Advantageously, the first sleeve is inserted into a second sleeve,wherein the second end is flared and wherein the second sleeve ishermetically brazed to an external surface of the first sleeve, while thecopper pipe is hermetically brazed to an internal surface of the first sleeve.Because copper deposits formed on internal and externalsurfaces of the first sleeve are exposed outside, the first sleeve can bebrazed to both the second sleeve and the copper pipe simultaneously.In another aspect of the present invention, a sleeve is made of acopper-plated steel pipe and has a first end and a second end opposite toeach other. The first end is welded to the sealed casing, while the secondend is copper-brazed to a copper pipe disposed outside the sealed casing.Because the thickness of copper deposits on the sleeve is of theorder of microns, the application of pressure and a subsequent flow ofelectricity as in resistance welding removes the copper deposit on thatsurface of the sleeve which is held in contact with the sealed casing, thusenabling hermetic welding of the internal or base steel pipe to the steelplate of the sealed casing. Flux as required in silver-brazing is not usedand, hence, flux removal with the use of water is not required, making itpossible to reduce water or chlorine-based impurities.Conveniently, the second end is flared to facilitate copper-brazing.Advantageously, the first end is tapered to expand outwardlyand is hermetically resistance-welded to an edge of a hole defined in thesealed casing. By so doing, the sleeve inserted into the hole of the sealedcasing from inside can be rigidly and reliably secured to the sealed casing.The sealed casing may contain an HFC refrigerant and anester-based lubricant. Because no flux is used during welding, impuritiesthat may decompose a refrigerant or a lubricant do not enter the sealedcasing, resulting in a highly reliable compressor.In a further aspect of the present invention, a sleeve is made ofa steel pipe and has a small-diameter portion and a large-diameter portioncontinuous to each other. The large-diameter portion has a tapered endexpanding outwardly and hermetically resistance-welded to an edge of ahole defined in the sealed casing.By this construction, inward expansion of the tapered endcaused by the resistance-welding can be accommodated within the large-diameter portion and, hence, insertion of another sleeve into the abovesleeve can be readily and positively carried out.In a still further aspect of the present invention, the sealedcasing has a generally flat portion in which a hole is defined wherein asleeve made of a steel pipe is hermetically welded directly to the generallyflat portion to communicate with the hole, allowing a refrigerant to flowtherethrough.Because no brazing material nor flux is used, not only can thewelding process be simplified, but also firm joining can be realized.The generally flat portion is formed with a cylindrical body ofthe sealed casing. Because the sleeve does not protrude inside the sealedcasing, incorporation of the motor section and the compression section intothe sealed casing and assemblage of the former inside the latter can bereadily carried out.The method according to the present invention includes thesteps of: forming a generally flat portion with the sealed casing; forming ahole in the generally flat portion; preparing a sleeve made of a copper pipe;tapering one end of the sleeve; and causing electric current to flow throughthe sleeve while the sleeve is being pressed against the generally flatportion with the one end of the sleeve held in contact with the generally flatportion, thereby hermetically welding the sleeve to the generally flatportion to allow a refrigerant to flow through the hole in the generally flatportion.Advantageously, the one end of the sleeve is tapered outwardly.Because the contact portion is heated by the electric current,simultaneously applying a pressure thereto extends the tapered end of thesleeve radially outwardly while removing an oxide layer from the contactportion, making it possible to bring fresh surfaces into close contact witheach other. A continuous flow of electricity heats and fuses the taperedend of the copper pipe and diffuses copper atoms into the steel member,realizing firm joining.Alternatively, the method according to the present inventionincludes the steps of: forming a generally flat portion with the sealedcasing; forming a hole in the generally flat portion; preparing a sleeve madeof a copper pipe; causing electric current to flow through the sleeve whilethe sleeve is being rotated and pressed against the generally flat portionwith one end of the sleeve held in contact with the generally flat portion,thereby hermetically welding the sleeve to the generally flat portion toallow a refrigerant to flow through the hole in the generally flat portion.The method may further include the step of tapering the oneend of the sleeve prior to the step of causing electric current to flow.Rotating the sleeve and pressing it against the generally flatportion remove an oxide layer from a contact portion, while a simultaneousflow of electricity fuses copper and diffuses copper atoms into the steelmember, realizing firm joining.BRIEF DESCRIPTION OF THE DRAWINGSThe above and other objectives and features of the presentinvention will become more apparent from the following description of pre-ferred embodiments thereof with reference to the accompanying drawings,throughout which like parts are designated by like reference numerals, andwherein:Fig. 1 is a vertical sectional view of a conventional sealedcompressor;Fig. 2 is a vertical sectional view of a sealed compressoraccording to a first embodiment of the present invention;Fig. 3 is a vertical sectional view of a suction pipe connectorsecured to the sealed compressor of Fig. 2;Fig. 4A is a vertical sectional view of a copper-plated steel plateused to make an internal suction sleeve of the suction pipe connector of Fig.3;Fig. 4B is a vertical sectional view of the copper-plated steelplate after deep draw forming;Fig. 4C is a vertical sectional view of the internal suctionsleeve;Fig. 5 is a vertical sectional view of a discharge pipe connectorsecured to the sealed compressor of Fig. 2;Fig. 6 is a view similar to Fig. 2, but according to a secondembodiment of the present invention;Fig. 7 is a vertical sectional view of a suction pipe connectorsecured to the sealed compressor of Fig. 6;Fig. 8A is a vertical sectional view of a discharge pipe connectorbefore it is secured to the sealed compressor of Fig. 6;Fig. 8B is a view similar to Fig. 8A, illustrating the dischargepipe connector secured to the sealed compressor;Fig. ^A is a vertical sectional view of a modification of thedischarge pipe connector; andFig. 9B is a view similar to Fig. 9A, illustrating anothermodification of the discharge pipe connector.DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTSThis application is based on applications Nos. 9-173427 and 9-173446 both filed June 30, 1997 in Japan, the content of which isincorporated hereinto by reference.Referring now to the drawings, there is shown in Fig. 2 a sealedcompressor according to a first embodiment of the present invention. Thesealed compressor includes a sealed casing 1 having a generally cylindricalbody lb, an upper cover la secured to an upper portion of the cylindricalbody lb, and a bottom cover lc secured to a lower portion of the cylindricalbody lb. They are each formed from a steel plate and hermetically weldedtogether to form the sealed casing 1. A motor section 2 and a compressionsection 3 are both accommodated in the sealed casing 1. The compressionsection 3 includes a rolling-piston type compression mechanism, and thesealed casing 1 is filled with a high-pressure refrigerant dischargedtherefrom when the compressor is in use. A suction pipe connector 4through which a refrigerant is introduced into the sealed casing 1 is securedto the cylindrical body lb, while a discharge pipe connector 5 through whichthe high-pressure refrigerant is discharged from the sealed casing 1 issecured to the upper cover la and is generally copper-brazed to a dischargepipe (not shown) made of copper. The suction pipe connector 4 and thedischarge pipe connector 5 lead to an evaporator (not shown) and acondenser (not shown), respectively, to form a refrigeration cycleAs shown in Fig. 3, the suction pipe connector 4 includes anexternal suction sleeve 7 inserted into a hole Id defined in the cylindricalbody lb of the sealed casing 1. The hole Id of the sealed casing 1 is formedin alignment with a suction hole 6 and a suction sleeve insertion hole 8 bothdefined in the compression section 3. The suction sleeve insertion hole 8 ispositioned radially outwardly of and continuous to the suction hole 6 andhas a diameter slightly greater than that of the suction hole 6. The suctionpipe connector 4 also includes an internal suction sleeve 9 pressed into thesuction sleeve insertion hole 8 so that a low-pressure refrigerant to beintroduced into the sealed casing 1 may be separated from a high-pressurerefrigerant inside the sealed casing 1. The length of the internal suctionsleeve 9 is determined so that an outer end thereof may be positionedradially outwardly of an outer end of the external suction sleeve 7. After asuction pipe 10 has been inserted into the internal suction sleeve 9 pressedinto the suction sleeve insertion hole 8, the suction pipe 10, the internalsuction sleeve 9 and the external suction sleeve 7 are simultaneouslyhermetically copper-brazed together, thereby separating the externalatmosphere, the low-pressure refrigerant introduced into the sealed casing1, and the high-pressure refrigerant inside the sealed casing 1 from oneanother.Figs. 4A, 4B and 4C depict the manner in which the internalsuction sleeve 9 is made.As shown in Fig. 4A, a copper-plated steel plate 12 havingcopper deposits 13 formed on opposite surfaces thereof is first cut into a discshape. The copper deposits 13 preferably have a thickness ranging from 5to 100 microns. The copper-plated and disc-shaped steel plate 12 is thenformed, by deep draw forming or pressing, into a generally cylindrical shapehaving a small-diameter portion 14 and a large-diameter portion 15continuous to each other. To facilitate the pressing and to make the wallthickness uniform, a round-headed punch is used. After the pressing, thegenerally cylindrical member has a closed and rounded front portion 16 anda flanged open rear portion 17 extending radially outwardly from acylindrical body. Subsequently, the rounded front portion 16 and theflanged rear portion 17 are cut in a direction axially of the generallycylindrical member, as shown by double-dotted chain lines in Fig. 4B, thusremoving a central portion from the front portion 16 and a generally flatflange from the rear portion 17, and forming a round outlet opening 18 inthe front portion 16. Because the front portion 16 has a round externalsurface 16a radially outwardly of the outlet opening 18, the internal suctionsleeve 9 can be smoothly pressed into the suction sleeve insertion hole 8without any damages, thus ensuring the sealing properties. Furthermore,because only the generally flat flange is removed from the rear portion 17,the rear portion 17 is still provided with a flared portion having a roundinternal surface 17a on which the copper deposit 13 remains, thusfacilitating copper-brazing of the copper-made suction pipe 10 with theinternal suction sleeve 9.If the rear portion 17 of the generally cylindrical member is cutin a direction radially thereof, the base metal, i.e., the internal steel thatrepels a copper-brazing material is exposed at a location close to the suctionpipe 10, making it difficult to ensure reliable and hermetic copper-brazing.Also, axial cutting can be achieved in a pressing machineimmediately after the pressing, resulting in a reduction in themanufacturing cost of the internal suction sleeve 9. In addition, becausesteel is smaller in thermal expansion than copper, the internal suctionsleeve 9 is not much affected by heat generated during brazing and bysubsequent cooling and, hence, does not expand and contact to such anextent that sealing between the internal suction sleeve 9 and the suctionsleeve insertion hole 8 will be lost or component parts of the compressionsection will be deviated from their desired positions by relatively largeforces applied thereto.The external suction sleeve 7 is made of a copper-plated steelpipe 7a having internal and external surfaces on each of which a copperdeposit 7b is formed. The external suction sleeve 7 has a small-diameterportion 7c, a large-diameter portion 7d continuous to the small-diameterportion 7c, a tapered inner end 7g expanding outwardly towards the insideof the sealed casing 1, and a flared outer end 7f. The small-diameterportion 7c has an internal diameter close to the external diameter of theinternal suction sleeve 7. The external suction sleeve 7 is inserted into thehole Id of the sealed casing 1 from inside, and the tapered inner end 7g isrigidly secured to the sealed casing 1 by resistance welding. At thismoment, the tapered inner end 7g expands inwardly under the influence ofa pressure required for the resistance welding or strains caused by theresistance welding. Such strains are mainly caused by the fact that thehole Id is formed in the cylindrical body lb of the sealed casing 1, and aperipheral edge of the hole Id does not lie on a flat plane. The provision ofthe large-diameter portion 7d facilitates insertion of the internal suctionsleeve 9 into the external suction sleeve 7 in the presence of such strains orthe inward expansion of the tapered inner end 7g. The flared outer end 7fof the external suction sleeve 7 facilitates copper-brazing thereof with theinternal suction sleeve 9 inserted thereinto, because the inner copperdeposit of the external suction sleeve 7 faces the outer copper deposit of theinternal suction sleeve 9. For the same reason, the flared rear portion orouter end 17 of the internal suction sleeve 9 facilitates copper-brazingthereof with the copper-made suction pipe 10 inserted thereinto. Theexternal suction sleeve 7, the internal suction sleeve 9, and the suction pipe10 can be copper-brazed simultaneously by regulating the length of theinternal suction sleeve 9 protruding outwardly from the external suctionsleeve 7.Fig. 5 depicts the manner in which the discharge pipe connector5 is made.The discharge pipe connector 5 is made of a copper-plated steelpipe 5a having copper deposits 5b formed on opposite surfaces thereof. Inmaking the discharge pipe connector 5, copper-plating is carried out afterthe steel pipe has been molded. To reduce the manufacturing cost of thedischarge pipe connector 5, a copper-plated steel pipe may be molded intothe shape of the discharge pipe connector 5. Alternatively, a copper-platedsteel plate may be formed into a generally cylindrical shape by pressing, asdiscussed above. Attention must be paid to the fact that no copper-platedportion is present on a cut surface 5c in the latter two cases.The discharge pipe connector 5 has a tapered inner end 5dexpanding outwardly towards the inside of the sealed casing 1 and atapered outer end 5e expanding outwardly towards outside. The taperedinner end 5d is secured to the upper cover la of the sealed casing 1, while adischarge pipe (not shown) is connected to the tapered outer end 5e. Theexternal side of the tapered outer end 5e is cut as shown by 5f so that theexternal diameter of the outer end 5e may be smaller than the diameter of ahole 19 defined in the upper cover la of the sealed casing 1.The discharge pipe connector 5 of the above-described structureis first inserted into the hole 19 of the upper cover la from inside until thetapered inner end 5d having an external diameter greater than thediameter of the hole 19 abuts against an edge 21 of the hole 19. Thereafter,a welding electrode 20 having a protruding portion 20a of substantially thesame angle as the tapered inner end 5d is pressed against the tapered innerend 5d, thereby sandwiching and holding the tapered inner end 5d betweenthe edge 21 of the hole 19 and the protruding portion 20a of the weldingelectrode 20. At this moment, it is important that the edge 21 of the hole19 is sharp and not rounded. A relatively large electric current is thencaused to flow through the welding electrode 20 and the upper cover la ofthe sealed casing 1. Because the tapered inner end 5d of the dischargepipe connector 5 h held in abutment with the sharp edge 21 of the hole 19 ofthe upper cover la, the electric current is concentrated on such a portion.As a result, the copper deposit 5b is removed from the external surface ofthe discharge pipe connector 5, and the base material of the discharge pipeconnector 5, i.e., the steel pipe 5a is hermetically welded to the steel-madeupper cover la of the sealed casing 1.This kind of joining does not use flux and, hence, water washingfor removal of the flux is not required. Furthermore, because the amountof dirt or dust produced during joining is relatively small, the sealed casing1 can be washed easily. Accordingly, even in the case where an HFCrefrigerant listed as a candidate for an alternative refrigerant that causesno destruction of the ozone layer is used with an ester-based lubricantcompatible therewith, the reliability of the compressor can be ensuredbecause chlorine contained in the flux or water which has been hithertoused for removal of the flux does not remain in the sealed casing 1.The tapered outer end 5e of the discharge pipe connector 5 iscopper-brazed to a discharge pipe 22 generally made of copper. When thedischarge pipe 22 is inserted into the tapered outer end 5e of the dischargepipe connector 5, the former faces the inner deposit 5b of the latter,facilitating the copper-brazing.Fig. 6 depicts a sealed compressor according to a secondembodiment of the present invention.The sealed compressor includes a sealed casing 1 having agenerally cylindrical body lb, an upper cover la secured to an upper portionof the cylindrical body lb, and a bottom cover lc secured to a lower portionof the cylindrical body lb. They are each formed from a steel plate andhermetically welded together to form the sealed casing 1. A motor section2 and a compression section 3 are both accommodated in the sealed casing 1.The compression section 3 includes a rolling-piston type compressionmechanism, and i the sealed casing 1 is filled with a high-pressurerefrigerant discharged therefrom when the compressor is in use. A suctionpipe connector 4 through which a refrigerant is introduced into the sealedcasing 1 is secured to the cylindrical body lb, while a discharge pipeconnector 5 through which the high-pressure refrigerant is discharged fromthe sealed casing 1 is secured to the upper cover la. The suction pipeconnector 4 and the discharge pipe connector 5 lead to an evaporator (notshown) and a condenser (not shown), respectively, to form a refrigerationcycle.As shown in Fig. 7, the cylindrical body lb of the sealed casing 1has a radially outwardly protruding portion If formed therewith. Theprotruding portion If has a generally flat top lg and a round hole lhdefined therein at the center thereof in alignment with a suction hole 6 anda suction sleeve insertion hole 8 both defined in the compression section 3.The suction sleeve insertion hole 8 is positioned radially outwardly of thesuction hole 6 and has a diameter slightly larger than that of the suctionhole 6. A copper-made external suction sleeve 7 is directly andhermetically welded to the generally flat top lg of the protruding portion Ifso as to communicate with the hole lh. An internal suction sleeve 9 ispressed into the suction sleeve insertion hole 8 from outside so that a low-pressure refrigerant to be introduced into the sealed casing 1 may beseparated from a high-pressure refrigerant inside the sealed casing 1. Thelength of the internal suction sleeve 9 is determined so that an outer endthereof may be positioned radially outwardly of an outer end of the externalsuction sleeve 7. After a suction pipe 10 has been inserted into theinternal suction sleeve 9 pressed into the suction sleeve insertion hole 8, thesuction pipe 10, the internal suction sleeve 9 and the external suction sleeve7 are simultaneously hermetically secured together by brazing 11, therebyseparating the external atmosphere, the low-pressure refrigerantintroduced into *lie sealed casing 1, and the high-pressure refrigerantinside the sealed casing 1 from one another.The discharge pipe connector 5 is made of a copper pipe and ishermetically welded to a flat portion le of the upper cover la so as tocommunicate with a hole defined therein. The discharge pipe connector 5is generally connected to a copper-made discharge pipe (not shown) bycopper-brazing.In the above-described construction, because the pipeconnectors 4 and 5 to which the suction and discharge copper pipes areconnected are directly welded to a steel plate, no brazing material or no fluxis required, thus simplifying the assembling processes of the compressor.Furthermore, because the copper pipes are not annealed by flames, they arenot deteriorated in strength, realizing firm joining. Also, because theexternal suction sleeve 7 does not protrude inside the sealed casing 1, itdoes not hinder incorporation of the motor section 2 and the compressionsection 3 into the sealed casing 1.Figs. 8A and 8B depict the manner in which the discharge pipeconnector 5 is joined to the sealed casing 1.Because the upper cover la constitutes an end plate of thesealed casing 1, the upper cover la generally has a flat portion le.Accordingly, a hole 11 that is to communicate with the discharge pipeconnector 5 is formed in such a flat portion le of the upper cover la.On the other hand, the discharge pipe connector 5 is a copperpipe having a lower end 5b of which the internal surface 5a is tapered.Accordingly, the lower end 5b of the discharge pipe connector 5 is relativelysharp. Prior to welding, the upper cover la and the copper pipe arewashed for removal of oil and the like. Thereafter, the copper pipe isaxially movably arranged above the upper cover la, which is heldstationary and grounded. The copper pipe is then positioned on andpressed against the upper cover la, while a relatively large DC current iscaused to flow therethrough. Because the lower end of the copper pipe isrelatively sharp, a large amount of heat is generated at this portion by theDC current, resulting in an increase in temperature and softening thecopper pipe. At this moment, the pressure applied to the copper pipe fromabove extends the lower end 5b of the copper pipe radially outwardly whileremoving an oxide layer on the flat portion Id of the upper cover la. Afarther flow of DC current increases the temperature of the lower end 5b ofthe copper pipe to fuse it. Because steel has a thermal conductivitysmaller than that of copper, that portion of the steel plate which is held incontact with the copper pipe is increased in temperature, thus diffusingcopper atoms into such a portion. Continued application of pressurecompletely hermetically welds the copper pipe to the upper cover la. Theradially outwardly extension and the subsequent fusion of the lower end 5bof the copper pipe increases a contact area and reduces the current density,resulting in a reduction in the amount of heat generated in the contactportion between the copper pipe and the upper cover la. In order tocomplete proper welding, however, it is preferred that the DC current valuebe reduced at a final process. It is also preferred that the application ofpressure be continued to promote diffusion with a somewhat smaller forceeven after the DC current has been cut off.It is to be noted here that although the discharge pipe connector5 is illustrated as having a tapered internal surface at the lower end thereofprior to welding, it may have a tapered external surface at the lower endthereof, as shown in Fig. 9A. In this case, however, attention must be paidto burrs that may protrude inwardly of the discharge pipe connector 5.It is also to be noted that although the above embodiment hasbeen discussed with respect to joining the discharge pipe connector 5 to theupper cover la of the sealed casing 1, the external suction sleeve 7 can bejoined to the cylindrical body lb of the sealed casing 1 in substantially thesame manner.Because the above-described joining method enables directwelding of copper pipes to a steel plate, no brazing material or no flux isrequired. Accordingly, even in the case where an HFC refrigerant is usedwith an ester-based lubricant compatible therewith, the reliability of thecompressor can be ensured because chlorine contained in flux or waterwhich has been hitherto used for removal of the flux does not remain in thesealed casing 1. Furthermore, because water washing for removal of theflux is not required, the manufacturing cost of the compressor can bereduced. Also, because flames of a torch or the like are not used, thecopper pipes are not annealed and, hence, not deteriorated in strength. Inaddition, fusion of copper and diffusion of copper atoms into a steel memberrealize firm joining.It is to be noted that although in the above-describedembodiment the copper pipe constituting the discharge pipe connector 5 hasbeen described as being axially pressed against the sealed casing 1, thecopper pipe may be rotated during axial pressing, thereby removing anoxide layer for subsequent diffusion-joining. In this case, although thelower end of the copper pipe need not be tapered, outward tapering asshown in Fig. 8A or tapering on respective sides of the copper pipe as shownin Fig. 9B concentrates electric current on the lower end of the copper pipe,making it easy to select the welding conditions.It is also to be noted that although a rolling-piston type sealedcompressor is employed in the above-described embodiments, the presentinvention is also applicable to other compressors including low-pressuretype reciprocating compressors, scroll compressors and the like.Although the present invention has been fully described by wayof examples with reference to the accompanying drawings, it is to be notedhere that variou s changes and modifications will be apparent to thoseskilled in the art. Therefore, unless such changes and modificationsotherwise depart from the spirit and scope of the present invention, theyshould be construed as being included therein.
Claims
CLAIMS 1. Ina sealed compressor having a sealed casing (1) in which a motor section (2) and a compression section (3) are both accommodated, the improvement comprising: a first sleeve (9) having a first end (16) and a second end (17) opposite to each other, said first end (16) being inserted into a sleeve insertion hole (8) defined in the compression section (3) to allow a refrigerant to flow therethrough, said second end (17) adapted to be hermitically brazed to a copper pipe (10) disposed outside the sealed casing (1), said first sleeve (9) having a generally cylindrical shape and being formed such that said first end (16) has an axiallyrounded external surface (16a), while said second end (17) has an axiallyrounded internal surface (17a).
2. The sealed compressor according to claim 1, further comprising a second sleeve (7) in which said first sleeve (9) is inserted, wherein said second end (17) is flared and wherein said second sleeve (7) is hermetically brazed to an external surface of said first sleeve (9), while the copper pipe (10) is hermetically brazed to an internal surface of said first sleeve (9).
3. The sealed compressor according to claim 1, wherein said first sleeve (9) is formed of a deep-drawn copper-plated steel plate.