Process for preparing ceramic composite material
Patent Information
- Application Number
- MYPI1998003497
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1997-07-31
- Filing Date
- 1998-07-30
- Publication Date
- 1999-01-31
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional methods for coating ceramic powder with a different composition material face challenges with fine particle sizes, leading to increased coagulation forces, poor dispersibility, and segregation issues during drying.
A process involving the adsorption of a low-molecular polymer with a metallic element onto ceramic powder surfaces, using a solvent like water or alcohol, with a hydrophilic functional group, and adjusting the polymer's molecular weight and concentration to ensure uniform coating.
The process achieves uniform and secure adsorption of the metallic element, preventing segregation and improving dispersibility by using a low-molecular polymer with a hydrophilic functional group, ensuring effective coating and molding of ceramic composite materials.
Abstract
Description
PROCESS FOR PREPARING CERAMIC COMPOSITE MATERIALBACKGROUND OF THE INVENTION1. Field ofthe InventionThe present invention relates to a process for preparing a ceramic composite material and, more particularly, to a process for a ceramic composite material which is adapted to uniformly coat surfaces of ceramic powder with a metallic element.2. Description of the Related ArtAs ceramic electronic parts have recently been developed so as to make their sizes smaller and smaller and to make their quality higher and higher, fine pulverization technology and high dispersion technology have also developed. Particularly, powder technology has developed at a very high speed. Under such technical background, the technology of coating surfaces of powder with a different composition material is now being highlighted.For instance, there is known a process for coating surfaces of ceramic powder with a different composition material by admixing the ceramic powder with a liquid additive using a solvent to a sufficient extent while stirring to a sufficient extent and then removing the solvent from the mixture, and drying the mixture.A such conventional coating process, however, suffers from the disadvantages that, when particle sizes of ceramic powder are very fine, a force of coagulation of the ceramic powder is caused to increase leading to poor dispersibility and to difficulties in uniformly coating the ceramic powder with a different composition material. Further, it also has the problem that the different composition material is segregated upon drying the ceramic powder.-2SUMMARY OF THE INVENTIONTherefore, the present invention has the object to provide a process for preparing a ceramic composite material which is so adapted as to uniformly coat surfaces of ceramic powder with a different composition material.In order to achieve the object, the present invention provides a process for preparing a ceramic composite material, which comprises the step of adsorbing a low-molecular polymer having a metallic element in its polymer structure on surfaces of ceramic powder by mixing the lowmolecular polymer with the ceramic powder.Other objects, features and advantages of the present invention will become apparent in the course of the following description with reference to the accompanying drawing.BRIEF DESCRIPTION OF THE DRAWINGFig. 1 is a flow chart showing the steps for preparing the ceramic composite material in accordance with the present invention.DESCRIPTION OF THE PREFERRED EMBODIMENTSThe process in accordance with the present invention comprises admixing a low-molecular polymer having a metallic element in its polymer structure with ceramic powder to adsorb the ceramic powder on the surfaces of the low-molecular polymer, as is briefly illustrated in Fig. 1.The low-molecular polymer may be mixed with the ceramic powder in the presence of a solvent such as, for example, water and / or an alcohol. A solvent other than water and the alcohol may also be used.When water and / or the alcohol are or is used as the solvent, it is 25 preferred to use a low-molecular polymer having a hydrophilic functional group. The hydrophilic functional group may preferably be, for example, a hydroxy group or a carboxyl group although there may also be used any other functional group as long as the group is a hydrophilic one.The low-molecular polymer to be used for the present invention may 30 have a molecular weight in the range of from approximately 5,000 to 15,000. If the low-molecular polymer has a molecular weight of smaller than 5,000,-3on the one hand, the use of such a low-molecular polymer may suffer from the disadvantage that the amount of adsorption of the low-molecular polymer may become too small because the such low-molecular polymer has too small adsorption points. If the low-molecular polymer has a molecular weight having greater than 15,000, on the other hand, the such lowmolecular polymer may become too large in viscosity resulting to no uniform adsorption on the surfaces of the ceramic powder.The molecular weight of the low-molecular polymer may be adjusted by changing an amount of a complex relative to an amount of a monomer or by controlling a reaction temperature or a reaction time for esterification of the complex with the monomer.It is preferred to use the low-molecular polymer at the rate of from approximately 0.1% to 20% by weight of the ceramic powder. If the rate of the low-molecular polymer with respect to the amount of the ceramic powder is lower than 0.1% by weight, on the one hand, then the problem may be caused to occur that the viscosity of a resulting slurry may become worse. If the rate of the low-molecular polymer with respect to the amount of the ceramic powder is greater than 20% by weight, on the other hand, the resulting mixture may suffer from the difficulties that the low-molecular polymer may also act as adhesive during drying and it may adversely affect the molding of the resulting powder. Further, it is particularly preferred that the rate of the low-molecular polymer is in the range of from approximately 0.1% to 0.5% by weight with respect to the ceramic powder in terms of uniformly coating the ceramic powder with the metallic element.The low-molecular polymer to be used for the present invention may be prepared by reacting a metallic compound with a chelating agent having, for example, a carboxyl group to yield a complex having the carboxyl group and subjecting a monomer having a hydroxyl group to ester polymerization with the complex. It is to be noted herein that the low-molecular polymer may be prepared by any other process that can provide a polymer having a metallic element in its polymer structure.The chelating agent to be used for the present invention may preferably include, for example, citric acid or L-glutamic acid. It is to be noted herein that any other chelating agent may also be used for the present invention, which has a carboxyl group in its moiety and has a chelating action.-4The chelating agent may preferably be used at the rate of approximately 1 mole to 10 moles per mole ofthe metallic compound. If the rate of the chelating agent is smaller than 1 mole, on the one hand, it may suffer from the difficulty that the total amount of the metallic compound cannot be chelated. If the rate ofthe chelating agent is larger than 10 moles, on the other, the advantages may be cause to occur that the excess amount of the chelating agent does not contribute to the chelating action for the metallic compound and that useless organic components may be increased resulting to the difficulty in eliminating organic materials.The monomer to be used for the present invention may preferably include, for example, ethylene glycol, 1,3-propane diol or 1,3-butane diol. It is to be noted herein that there may be employed any other compound which has a hydroxy group and which can be subjected to ester polymerization with the chelating agent.The monomer may be used at the rate of from 2 moles to 100 moles with respect to mole ofthe metallic compound. The reasons for setting the rate of the monomer to the above range are, on the one hand, because the problem may arise in that the chelating agent cannot be dissolved if the rate of the monomer is below 2 moles and, on the other hand, because useless organic components may be caused to increase resulting to the difficulty in eliminating organic materials if the rate ofthe monomer exceeds 100 moles.Further, the metallic compound to be used herein may preferably include, for example, cobalt acetate trihydrate. It is to be noted herein that the metallic compound is not restricted to this compound and it can optionally be chosen so as to be adapted to the composition of a coating layer of the ceramic composite material sought to be obtained.As the ceramic powder, there may be used, for example, barium titanate powder. It is to be noted herein, however, that the ceramic powder is not restricted to this powder and it can optionally be chosen so as to be adapted to the composition of a core portion of the ceramic composite material sought to be obtained.The resulting ceramic composite material may be employed preferably as a dielectric material for a precision ceramic electronic part including, for example, a laminated ceramic condenser requiring a ceramic material design of e.g. ΙΟμχη ( 10 micron ) or smaller. It is to be noted herein as a matter of course that the ceramic composite material is practically applied by-oburning out the organic materials contained therein by firing.The present invention will he described in more detail by way of examples.Example 1:To 2 grams of ethylene glycol was added 1.9 grams of citric anhydride, and the resulting mixture was heated to 60° C in an oil bath. To the resulting liquid was then added 0.498 gram of cobalt acetate trihydrate while stirring with a magnetic stirrer to dissolve the compound in the liquid. At this stage the cobalt acetate trihydrate was allowed to be dissolved therein gradually to form a complex.Then, the resulting mixture was heated at 120° C while controlling the temperature with care. The heating at this stage caused the carboxyl group of citric acid and the hydroxyl group of ethylene glycol to be subjected to dehydration-ester polymerization yielding an oligomer containing cobalt therein.In five minutes after the occurrence of the dehydration-ester polymerization, the reaction material was then allowed to cool to cease the reaction. This reaction yielded a polymer having a molecular weight of approximately 10,000.Separately, 466.4 grams of barium titanate having an average particle diameter of 0.5pm ( 0.5 micron ) was mixed with 700 ml of ion exchange water and 300 ml of ethanol, and the resulting mixture was stirred with a ball mill for 10 hours yielding a slurry. To the resulting slurry was added the polymer prepared above, and the mixture was stirred for 3 hours to yield ceramic composite particles.The resulting ceramic composite particles were observed with an electronic microscope. The microscopic observation revealed that barium titanate particles were adsorbed uniformly over the entire surfaces with the polymer containing cobalt at the rate of one thousandth mole with respect to barium titanate.Further, the resulting ceramic composite particles were analyzed by fluorescent X-ray spectroscopy (XRF) to determine a macro dispersion ofthe composition. The results are shown in Table below as Sample Nos. 1 to 4 and they reveal that no segregation is caused to occur and the sample has a high dispersibility.Comparative Example 1:-6A mixture was prepared by mixing 466 grams of barium titanate powder, 700 ml of water and 0.498 gram of cobalt acetate trihydrate with one another and the resulting mixture was dried in accordance with the spray dry method. The resulting powder was then analyzed in substantially the same manner as in Example 1 and the results of this analysis are shown in Table as Sample No. 5.TABLESampl e Nos. Measurement Locations (mol%) Average Value (mol%) Standard Deviation A B C D E 1 0.125 0.110 0.085 0.105 0.095 0.099 0.011 2 0.110 0.100 0.080 0.115 0.120 0.104 0.018 3 0.130 0.115 0.110 0.085 0.095 0.101 0.014 4 0.105 0.105 0.080 0.120 0.090 0.100 0.015 5 0.150 0.110 0.075 0.120 0.085 0.108 0.030The results of Table above reveals that no segregation of Co is found in the samples obtained in Example 1 and the powder is covered uniformly with Co. On the other hand, Sample No. 5 obtained in Comparative Example 1 is found that the extent of segregation of Co is large.Example 2:The procedures were followed in substantially the same manner as in Example 1 with the exception that the reaction time for reacting the complex with the monomer and the molecular weight ofthe polymer used were varied. As a result, it was found that the resulting materials caused the problems that, when the molecular weight of the polymer was smaller than 5,000, on the one hand, the amount of adsorption was too small because it had too small adsorption points and, when the molecular weight ofthe polymer was greater than 15,000, on the other, the viscosity of the low-molecular polymer became too great, the surfaces of the ceramic powder were not adsorbed uniformly with the low-molecular polymer.Example 3:The procedures were carried out in substantially the same manner as in Example 1 with the exception that the rate ofthe low-molecular polymer to be admixed with the ceramic powder was varied. The results revealed that, when the rate ofthe low-molecular polymer was lower than 0.1% by weight,-7on the one hand, the resulting slurry became too poor in viscosity to achieve the expected effects and that, when the rate of the low-molecular polymer was greater than 20% by weight, on the other hand, the polymer was found to act as adhesive upon drying and has adversely affected the molding of the powder thereafter. It was further found that the rate of the low-molecular polymer may preferably range from 0.1% to 0.5% by weight in terms of the uniform coating with the metallic element.Example 4:The procedures were conducted in substantially the same manner as in Example 1 with the exception that L-glutamic acid was used for the chelating agent to act upon the metallic compound. The results revealed that substantially the same effects could be performed as those achieved in Example 1.Example 5:The procedures were carried out in substantially the same manner as in Example 1 with the exception that the rate of the chelating agent to act upon the metallic compound was varied. As a result, the problems were caused to arise that, when the rate of the chelating agent was smaller than 1 mole per mole of the metallic compound, on the one hand, the total amount of the metallic compound could not be chelated and, when the rate of the chelating agent was greater than 10 moles per mole of the metallic compound, on the other, the rate of the chelating agent exceeding 10 moles did not contribute to the chelating action and furthermore the elimination of the resulting organic materials become difficult due to an increase in useless organic materials. It was further found that the rate of the chelating agent of approximately 4 moles is preferred.Example 6:The procedures were followed in substantially the same manner as in Example 1 with the exception that 1,3-propane diol or 1,3-butane diol was used as the monomer for subjecting the complex to ester polymerization. The results revealed that substantially the same effects could be performed as achieved in Example 1.Example 7:The procedures were conducted in substantially the same manner as in Example 1 with the exception that the rate of the monomer to be used for subjecting the complex to ester polymerization was varied. As a result, it was-8found that this process suffered from the disadvantages that, when the rate ofthe monomer was smaller than 2 moles per mole ofthe metallic compound, on the one hand, the dissolution ofthe chelating agent became difficult and that, when the rate ofthe monomer was larger than 100 moles, on the other, the elimination of the resulting organic materials became difficult due to an increase in useless organic materials. It was further found that the rate of the monomer was preferred at the rate of approximately 10 moles.EFFECTS OF THE INVENTIONThe present invention can provide the effects that the surfaces ofthe ceramic powder can be adsorbed uniformly and securely with the lowmolecular polymer containing the metallic element therein, thereby failing to cause the polymer to segregate upon drying and as a consequence enabling the surfaces ofthe ceramic powder to be covered uniformly with the metallic element as the other composition material.Further, the present invention presents the advantage that the dispersibility of the ceramic powder can be improved because the ceramic powder repels from each other due to the steric hindrance of the lowmolecular polymer.
Claims
1. A method for preparing a ceramic composite material comprising the step of adsorbing a low-molecular polymer having a metallic element in a molecular structure thereof onto surfaces of ceramic powder by admixing the ceramic powder with the low-molecular polymer.
52. The method for preparing the ceramic composite material as claimed in claim 1, wherein said low-molecular polymer is admixed with said ceramic powder in the presence of a solvent.
3. The method for preparing the ceramic composite material as claimed in claim 2, wherein said solvent is water and / or an alcohol. ·· ···· -104. The method for preparing the ceramic composite material as claimed in claim 1, wherein said low-molecular polymer has a hydrophilic functional group.
5. The method for preparing the ceramic composite material as claimed in claim 4, wherein said hydrophilic functional group is a hydroxyl group or a carboxyl group or a combination of a hydroxyl group with a carboxyl group.
6. The method for preparing the ceramic composite material as claimed in claim 1, wherein said low-molecular polymer has a molecular weight ranging from 5,000 to 15,000.
7. The method for preparing the ceramic composite material as claimed in claim 1, wherein said low-molecular polymer is admixed with said ceramic powder at the rate of from 0.1% to 20% by weight with respect to the ceramic powder.
8. A method for preparing a ceramic composite material, comprising: the step of reacting a chelating agent having a carboxyl group with a metallic compound to form a complex having a carboxyl group; and the step of subjecting said complex to ester polymerization with a monomer having a hydroxyl group to form a low-molecular polymer having a metallic element in its molecular structure.
9. The method for preparing the ceramic composite material as claimed in claim 8, wherein said chelating agent is citric acid or L-glutamic acid.
10. The method for preparing the ceramic composite material as claimed in claim 8, wherein said chelating agent is admixed with said metallic compound at the rate of from 1 mole to 10 moles with respect to mole of said metallic compound.
11. The method for preparing the ceramic composite material as claimed in claim 8, wherein said monomer is ethylene glycol, 1,3-propane -11diol or 1,3-butane diol.
12. The method for preparing the ceramic composite material as claimed in claim 8, wherein said monomer is admixed with said metallic compound at the rate of from 2 moles to 100 moles with respect to mole of 5 said metallic compound.
13. The method for preparing the ceramic composite material as claimed in claim 8, wherein said metallic compound is cobalt acetate trihydrate.
14. The method for preparing the ceramic composite material as 10 claimed in claim 8, wherein said ceramic powder is barium titanate powder.