Alloy used for electron gun electrodes

MYPI1998003714A0Inactive Publication Date: 1999-03-30JX NIPPON MINING & METALS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1998003714
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1997-09-30
Filing Date
1998-08-14
Publication Date
1999-03-30
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing nonmagnetic stainless steel alloys used for electron gun electrodes face challenges in meeting the stricter requirements for formability in deep drawing and high burring, particularly with the increased demand for finer and brighter picture tubes, while also needing to reduce material costs, as lowering the Ni content compromises formability and increasing S content complicates management and costs.

Method used

A nonmagnetic alloy with a controlled chemical composition, including 15-20% Cr, 9-15% Ni, 0.12% C or less, 0.005-1.0% Si, 0.005-2.5% Mn, 0.0003-0.0100% S, 2.0% Mo or less, and balanced Fe and impurities, which optimizes formability for deep drawing and high burring by precisely managing elements like P, N, Ti, Nb, V, Zr, and Ca, allowing for a higher S content without excessive desulfurization costs.

Benefits of technology

The alloy achieves superior formability for deep drawing and high burring, maintaining nonmagnetic properties and reducing material costs, with improved punching properties and reduced burr formation, thus addressing the stricter requirements and cost concerns.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

DISCLOSED IS AN ALLOY USED FOR ELECTRON GUN ELECTRODES. THE ALLOY CONSISTS OF: ALL BY WEIGHT, 15 TO 20%OF CR; 9 TO 15%OF NI; 0.12%OR LESS OF C; 0.005 TO 1.0%OF SI; 0.005%TO 2.5%OF MN; 0.03%OR LESS OF P; 0.003 TO 0.0100%OF S; 2.0%OR LESS OF MO; 0.001 TO 0.2%OF AL;0.005%OR LESS OF O; 0.1%OR LESS OF N; 0.1%OR LESS OF TI; 0.1%OR LESS OF NB; 0.1%OR LESS OF V;0.1%OR LESS OF ZR; 0.05%OR LESS OF CA; 0.02%OR LESS OF MG; AND THE BALANCE OF FE AND INEVITABLE IMPURITIES.BY STRICTLY CONTROLLING NOT ONLY THE CONTENTS OF S AND MN BUT ALSO THE CONTENTS OF AL, O AND THE LIKE WHICH WERE NOT CONSIDERED IN THE PAST, THE ALLOY HAS EXCELENT FORMABILITY OF BOTH DEEP DRAWING AND HIGH BURRING, THEREBY BEING OPTIMAL FOR USE IN ELECTRON GUN ELECTRODES.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND OF THE INVENTION This invention relates to a nonmagnetic alloy used for electron gun electrodes, specifically to an alloy with excellent formability for both deep drawing and high burring.For electron gun parts, particularly for the electrodes of electron guns for color picture tubes, nonmagnetic stainless steels have been used and disclosed in Japanese Patent Publication Nos. 32(57)-751 and 4(92)io 43372. Of these proposals, Japanese Patent Publication No. 4(92)-43372 discloses an alloy with improved formability for both deep drawing and high burring, which has adequate properties as a material for electron gun electrodes of conventional picture tubes. The term “high burring” as used herein means a working technique whereby a round hole is made in sheet15metal while forming a burr or flange protruding from the periphery of the hole.More recently, the rapid advent of finer and brighter picture tubes fQr computers has required the improvement of formability for both deep drawing and high burring. That is, the requirement has made it necessary2q to increase the lens aperture diameter of the electrodes while performing high burring with greater precision so as to improve the focusing characteristics of the electron gun. As a result, the requirements for formability for both deep drawing and high burring have become stricter than ever, whereby the prior art alloys have caused a decline in yield due to increase of inferior products. Moreover, there has been a strong demand for reduction in the material cost in recent years. However, if the content of the expensive material Ni is lowered, the formability for both deep drawing and high burring deteriorates, and hence, the prior art alloys can not meet the above requirement.This invention has been achieved considering the aforementioned circumstances and has the objective of providing an alloy for electron gun electrodes that meets the recent stricter requirements for improvement in formability for both deep drawing and high burring.BRIEF SUMMARY OF THE INVENTION The inventors have extensively studied the chemical composition of alloys so as to improve the formability for both deep drawing and high burring. As a result, the inventors found the influences of Ρ, N, Ti, Nb, V, Zr and Ca, which have not been considered, and S on the above mentioned formability. Heretofore, sulfur has been known as an undesirable element that deteriorates hot rolling properties and corrosion resistance.L5With respect to the formability for both deep drawing and high burring, it has also been considered that the S content should be held as low as possible. The applicant also mentioned in Japanese Publication No. 4(92)43372 that decrease in S content enhances the formability for both deep drawing and high burring. On the other hand, the alloys proposed in •θ Japanese Application No. 336866 improve punching properties by containing a proper amount of S, thereby uniformly dispersed S or S compounds (primarily composed of MnS) along grain boundaries or within grains in the alloy stock.Lately, the inventors have discovered that when S is not properly contained, the punching properties are deteriorated, whereby wear of the die results in formation of large burrs, which may cause burring cracks. Therefore, an appropriate amount of S should be contained for high burring formability. However, if the maximum S content is set at 0.003 % as mentioned in Japanese Application No. 6(92)-336866, the management of raw materials may be complicated and the desulfurization cost may increase.Therefore, the inventors have extensively studied the chemical composition of the alloy; as a result, we have discovered that when the contents of the elements including P, N, Ti, Nb, V, Zr and Ca are precisely controlled, the maximum content of S is not required to be set at 0.003 %.The present invention was completed based on the above mentioned10studies with quantitative analyses of the chemical composition. This invention provides an alloy used for electron gun electrodes consisting of: all by weight, 15 to 20 % of Cr; 9 to 15 % of Ni; 0.12 % or less of C;0.005 to 1.0 % of Si; 0.005 % to 2.5 % of Mn; 0.03 % or less of P; 0.0003 to 0.0100 % of S; 2.0 % or less of Mo; 0.001 to 0.2 % of Al; 0.005 % or less of O; 0.1 % or less of N; 0.1 % or less of Ti; 0.1 % or less of Nb;0.1 % or less of V; 0.1 % or less ofZr; 0.05 % or less of Ca; 0.02 % or less of Mg; and the balance of Fe and inevitable impurities.The reasons for the above quantitative limitations will be explained together with the effects of the present invention. In the following explanation, “%” means “weight %”.(Cr): An alloy for electron gun electrodes is essentially required to be nonmagnetic. In order to meet the requirement, the contents of Cr and Ni must be controlled to within the proper ranges. The Cr content is, therefore, restricted to the range from 15 to 20 % for achieving non25 magnetic property. More preferable range of the Cr content is from 15 to 17 %.(Ni): At least 9 % of Ni is required for achieving non-magnetic character. If the Ni content exceeds 15 %, the material cost increases too much. Hence the Ni content is restricted to within the range of 9 to 15 %. More preferable range of the Ni content is from 13 to 15 %.(C): If the C content exceeds 0.12 %, a large amount of carbide is formed, thereby deteriorating the formability for both deep drawing and high burring, and hence, the C content is restricted to 0.12 % or less.(Si): Si is added for deoxidation. If the Si content is less than0.005 %, the effect as a deoxidizer can not be obtained. On the other hand, if the Si content exceeds 1.0 %, the formability for both deep drawing and high burring deteriorates. Hence the Si content is restricted10to within the range of 0.005 to 1.0 %.(Mn): Mn is added for deoxidation and formation MnS, thereby obtaining the aforementioned effects. If the Mn content is less than 0.005 %, these effects are not expected. If the Mn content exceeds 2.5 %, the hardness of the alloy markedly increases, thereby deteriorating the15formability for both deep drawing and high burring. Hence the Mn content is restricted to within the range of 0.005 to 2.5 %.(P): If the P content exceeds 0.03 %, the formability for both deep drawing and high burring deteriorates. Hence the P content must be 0.03 % or less.2Q. (S): When contained in an appropriate amount, S forms MnS together with Mn, thereby improving the formability for deep drawing and high burring. If the S content is less than 0.0003 %, such an effect is not expected. If the S content exceeds 0.0100 %, coarse MnS is formed, thereby deteriorating the formability for both deep drawing and high burring. Hence the S content is restricted to within the range of 0.0003 to 0.0100%.(Mo): Since Mo improves corrosion resistance, Mo can be advantageously added when special corrosion resistance is required.However, if the Mo content exceeds 2.0 %, the formability for both deep drawing and high burring is deteriorated. Hence, the Mo content must be 2.0 % or less.(Al): Al is added for deoxidation, which is effective with an Al 5 content of 0.001 % or more. If the Al content exceeds 0.2 %, the formability for both deep drawing and high burring of the alloys deteriorates. Hence the Al content is restricted to within the range of 0.001 to 0.2 %.(O): When a large amount of O is contained, the amount of oxide10type inclusions increase, thereby deteriorating the formability for both deep drawing and high burring. Hence the O content must be 0.005 % or less.(N): When the N content is too large, the formability for both deep drawing and high burring of the alloy deteriorates. Hence the N content15must be 0.1 % or less.(Ti): Ti forms carbides, sulfides, oxides and nitrides, thereby deteriorating the formability for both deep drawing and high burring. Hence the Ti content must be 0.1 % or less. More preferable range of the Ti content is from 0.02 % or less.20(Nb): Nb forms carbides, sulfides, oxides and nitrides, thereby deteriorating the formability for both deep drawing and high burring. Hence the Nb content must be 0.1 % or less. More preferable range of the Nb content is from 0.02 % or less.(V): V forms carbides and nitrides, thereby deteriorating the formability for both deep drawing and high burring. Hence the V content is restricted to 0.1 % or less. More preferable range of the V content is from 0.02 % or less.(Zr): Zr forms oxides, thereby deteriorating the formability for both deep drawing and high burring. Hence the Zr content is restricted to 0.1 % or less. More preferable range of the Zr content is 0.02 % or less.(Ca): Ca forms sulfides and oxides, thereby deteriorating the 5 formability for both deep drawing and high burring. Hence the Ca content must be 0.05 % or less. More preferable range of the Ca content is 0.01 % or less.(Mg): Mg forms oxides, thereby deteriorating the formability for deep drawing and high burring. Hence the Mg content must be 0.02 % orL0less. More preferable range of the Mg content is 0.005 % or less.Furthermore, if the cleanliness based on JIS G0555 of the alloy exceeds 0.03 %, the formability for both deep drawing and high burring deteriorates. Hence the cleanliness of the alloys should be 0.03 % or less.It should be noted that the analysis of carbides and nitrides is difficult5when using the measuring method based on JIS G0555. Therefore, it is not sufficient only to satisfy the condition of the cleanliness being 0.03 % or less, but the chemical composition of the alloys must be strictly controlled in the range of the invention.DETAILED DESCRIPTION OF THE INVENTION „ The present invention will now be described in further detail in oconnection with its working examples and comparative examples. The chemical compositions of sample materials are shown in Table 1. The 18 ingots were produced by VOD or vacuum melting. The ingots were forged, ground, hot rolled and pickled. The samples were, then, . repeatedly cold rolled and annealed to 0.4 mm thick annealed sheets. The process conditions were controlled to obtain the same grain size, 8.0 in grain size number. A deep drawing test was carried out and the limitingΊ draw ratio (LDR) was measured. Hole expansion test was also conducted to evaluate the burring formability. A flat sheet specimen with a circular mm - diameter hole was deformed by a conical punch with a 60° angled tip, which expands and ultimately cracks the edge of the hole. The burring formability was evaluated as hole expansion, λ, defined by the following equation;λ = (hi-ho)Zho where ho and hi are the initial and final hole diameters, respectively.The LDR and the hole expansion of the samples are shown in Table io 2. The cleanliness of each sample was measured according to JIS G0555, and the results are shown in Table 2.TableRemark o Fe Bal Bal —--4 <2 —--4 <2 Bal Bal Bal Bal Bal Bal Bal —·4 ¢2 Bal —·4 ¢2 Bal —μ ¢2 Bal £ QO co co co co co co co co co CO co co co co CO CO CO <o co CO co co CO co CO CO co CO co CO CO co CO co co CO co co CO CO CO CO co CO CO o <d <d <d <d co <d <=5 <d <d <d cd cd <d <d cd cd 3 001 co co co co co co co co co co co co CO CO <o CO co co CO co co co o o co co co CO CO co co CO co CO CO co co co CO CO lO c— co CO co o <o <o <d <d <d o co <=5 cd <d o o o <o cd cd <=5 , 1_ 1_, co co CN CN co co CO <o co CO 5-4 S3 o o co co co co co co co co CO CO o CO co co 00 CO CO co CO CO CO co CO CO CO co <o lO CO <o co o co <=> <d <d co <o <d <0 co <=5 <d <d <d <o <d <o <d <=5 , 1_, co 1_, co co CN co co CO LO co CO <—5 <o <o <o o <o co ¢=5 <o <o co co CO CO co O s- o co co co co CO o co <=5 CO CO co co CO co <o o co <d <o <d <o <d <o co <=5 <d <d <d <d <d <d <d cd <=5 1_! co co 1_, . co co co co co LO co co co CO ¢-5 o ό <o co co CO co <=5 co CO CO CO OO o <o O <o jz: <o co <o <o co <o <o co <=5 <o <o <O co co <o CO <o <o cd <d <d <o <o <d cd <=5 <d <d cd <d cd <d <d <=5 <=5 CO co 1_, co co co CN co co co co co co CO o o <o co co CO co CO co co CO co CO co o <o <o • -4 e—ι co o> co co co co CO <O <=5 o CO CO co co o o <o <O <o <d <o <o <o <d <d <=5 cd <d <d <d o cd CO <=5 C5 LO co <o oo vo co VO oo r— co LT5 co co oo c— TT LO CN CO co co co co co ’TJ* LO LO co co ’TJ* LO z co <o co co co CO CO co <=5 CO CO CO CO co o o <o <o <o <o <o <o <d <=5 <=5 <d <O o <d o <o <d <=5 <d co oo oo co co oo oo LO co OO 03 oo co <o LO co co co co co co co CO co ^>4 t— co co co co co co co <O <o <o <o co co <o o <=5 CO CO co co co o co <o o? o co <o co co co CO co <=5 <=5 CO CO CO co CO co co co o> o <o <o <o <o <o <d o <=5 o o o <d o co CO co cd co co co co — LO CN CO CO co co ’TJ* co LO co β co <o co co co CO o <=5 CO o CO co co o co o o —4 co co co co co CO CO o <=5 o CO CO CO o co <o o co <o o <0 o <0 cd <=5 <=5 <d <d <d <o <o <d cd C5 <d 1__ co co co co — CN CO ^-4 co co CO o co <o <o co co co CO ¢=5 co <o co co co co co co o ae <o <o <o -4 <o <o co <=5 <o <o> <o <d cd o <d co cd <d oo LO co co CO LO LO co co oo oo co LO oo LO r*- co co co ——4 <=5 CN co co co LO co co <O o o <o co co co CO i—4 co co CO co co <O co o <O co <o <o o> <o co co co o <o <o CO <o <o <o <O co co co <d <o <o <o <o CO co <=5 <d o CO <d o <o <o <=5 <=5 cd co oo co CO co LO co OO co co CO r— OT co LO <=5 —4 co co co co i—4 CN co co ---4 co co CO i—4 cu <o <o co <O CO <o co <=5 <O co CO CO CO CO CO <O CO o <o <o <o <o <o <o <d <=5 O o <O o o <o <o ¢=5 <=5 cd c LO co m co co c— CO OT co CO oo co LO oo CO co ae —: — -4 -4 —< ^-4 —1 4 —> O — — —' —' — -1 —' -1 -1 CO co LO CO LO LO CO co LO co LO LO c— LO co co <o <d <o <o <o <O o <=5 o o <d o o <d <d <=5 <=5 cd LO LO CO LO co co LO ’TJ* ’Ti* LO LO CJ <O co <O co <o CO co o CO CO CO CO CO CO CO O o <d <o <o <d <o <O G5 <=5 o o CO o <d <O co <=5 cd <o LO co c— LO c— co OO CO c— co LO o- LO co <=5 LO — co d cd co co co cd xr -Tt» ^-4 F—4 1-4 ^-4 1-4 ^4 ^-4 r-, oo oo <o CN —< CO o — LO 03 03 — oo oo CN co 5-4 CJ co LO t-*- oo co co CO cd co co io ιό ιό co ιό m cd ιό F—4 ^-4 —4 ^-4 ^4 *“* ' * (O co co Lf5 co r— oo o i—4 co CO LO co Γ— oo ^“4 1—· »—« zrepresents examples of the invention represents comparative examplesTable 2No\ Limiting Draw Ratio (LDR) Hole Expansion (A) Cleanliness (%) 1 2.32 1.70 0.017 2 2.35 1.80 0.008 Examples of the 3 2.25 1.65 0.013 4 2.24 1.65 0.017 Invention 5 2.22 1.60 0.021 6 2.20 1.50 0.038 7 2.10 1.35 0.025 8 2.35 1.45 0.033 9 2.15 1.30 0.029 10 2.15 1.40 0.004 11 2.10 1.25 0.075 12 2.15 1.35 0.021 Comparative Examples 13 2.10 1.30 0.029 14 2.10 1.35 0.025 15 2.10 1.30 0.033 16 2.10 1.30 0.021 17 2.15 1.30 0.033 18 2.15 1.35 0.029As seen in Table 2, in all of Examples Nos. 1 to 6 of the present invention, the limiting draw ratio is 2.20 or more and the hole expansion is 1.50 or more, indicating that formability for both deep drawing and high burring is superior. Cleanliness of Example No. 6 exceeds 0.03 %, whereby the limiting drawing ratio and the hole expansion are relatively low compared to other examples of the invention. Therefore, the preferable cleanliness is 0.03 % or less.On the other hand, the P content (0.07 %) of Comparative Example No. 7 exceeds the upper limit (0.03 %) of the invention, whereby the limiting draw ratio and the hole expansion are low. The S content (0.0001 %) of Comparative Example No. 8 is less than the lower limit (0.0003 %) of the invention, whereby the hole expansion is low although the limiting draw ratio is high. Comparative Examples Nos. 9 to 18 exceed the range of the invention in the contents of S, Al, Ο, N, Ti, Nb, V, Zr, Ca and Mg, whereby the limiting draw ratio and the hole expansion are low.The invention restricts the S and Mn contents to within the aforementioned ranges and strictly controls the contents of Al, O and the like which were not considered in the past. Hence, the invention can meet the requirements for the improvement in the formability for both deep drawing and high burring that have become stricter in recent years. Thus, the invention can provide an alloy optimum for electron gun electrodes.

Claims

WHAT IS CLAIMED IS:

1. An alloy used for electron gun electrodes consisting of: all by weight, 15 to 20 % of Cr; 9 to 15 % of Ni; 0.12 % or less of C; 0.005 to 1.0 % of Si; 0.005 % to 2.5 % of Mn; 0.03 % or less of P; 0.0003 to 5 0.0100 % of S; 2.0 % or less of Mo; 0.001 to 0.2 % of Al; 0.005 % or less of O; 0.1 % or less of N; 0.1 % or less of Ti; 0.1 % or less of Nb; 0.1 % or less of V; 0.1 % or less of Zr; 0.05 % or less of Ca; 0.02 % or less of Mg; and the balance of Fe and inevitable impurities.

2. An alloy used for electron gun electrodes according to claim 1, 10 wherein the Cr content is in the range of 15 to 17 % by weight.

3. An alloy used for electron gun electrodes according to claim 1, wherein the Ni content is in the range of 13 to 15 % by weight.

4. An alloy used for electron gun electrodes according to claim 1, wherein the content of at least one of Ti, Nb, V and Zr is restricted to 15 0.02 % or less by weight.

5. An alloy used for electron gun electrodes according to claim 1, wherein the Ca content is restricted to 0.01 % or less by weight.

6. An alloy used for electron gun electrodes according to claim 1, wherein the Mg content is restricted to 0.005 % or less by weight. 20 7. An alloy used for electron gun electrodes according to claim 1, wherein the alloy has a cleanliness of 0.03 % or less based on JIS G0555.