Dissolution inhibitor of chemically amplified photoresist and chemically amplified photoresist composition containing the same

MYPI1998004261A0Inactive Publication Date: 1999-11-20SAMSUNG ELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1998004261
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1998-05-20
Filing Date
1998-09-17
Publication Date
1999-11-20
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional chemically amplified photoresists with t-butoxycarbonyl (t-BOC) as a dissolution inhibitor suffer from poor thermal characteristics, leading to thermal decomposition and inferior pattern profiles when pre-baked above the glass transition temperature, while pre-baking at lower temperatures allows airborne contaminants to prevent catalytic reactions.

Method used

A chemically amplified photoresist composition incorporating an acid-labile di-alkylmalonate group as a functional group with C1 to C40 hydrocarbons, such as cyclohexane or xylene, which is thermally stable and increases contrast by hydrolyzing into a malonate group upon acid exposure, combined with a photosensitive polymer and acid generator, allowing high-resolution pattern formation.

Benefits of technology

The di-alkylmalonate group's thermal stability and high contrast properties enable pre-baking above the glass transition temperature without decomposition, preventing pattern defects and allowing the formation of high-resolution patterns with excellent profiles.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A DISSOLUTION INHIBITOR OF A CHEMICALLY AMPLIFIED PHOTORESIST, AND A CHEMICALLY AMPLIFIED PHOTORESIST COMPOSITION CONTAINING THE SAME ARE PROVIDED. THE DISSOLUTION INHIBITOR OF THE CHEMICALLY AMPLIFIED PHOTORESIST IS A COMPOUND IN WHICH AN ACID-LABILE DI-ALKYLMALONATE GROUP IS COMBINED AS A FUNCTIONAL GROUP WITH C1 TO C40 HYDROCARBON. THE CHEMICALLY AMPLIFIED PHOTORESIST COMPOSITION CONTAINING THE DISSOLUTION INHIBITOR HAS A HIGH CONTRAST AND HIGH THERMAL DECOMPOSITION TEMPERATURE, MAKING IT SUITABLE FOR FORMING A PATTERN HAVING EXCELLENT PROFILE.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND OF THE INVENTION 5 1. Field ofthe InventionThe present invention relates to a material for forming a semiconductor device, and more particularly, to a dissolution inhibitor of a chemically amplified photoresist used in photolithography, and a chemically amplified photoresist composition containing the same.io 2. Description of the Related ArtSince current semiconductor chips are highly integrated and complicated to manufacture, fine patterns based on a design rule of 0.25^m are now used. Accordingly, a pattern must be formed using deep ultraviolet (UV) rays of 248nm, which is shorter than conventional g-line (436nm) and I-line (365nm) wavelengths.is However, in the case of using deep-UV rays, a smaller number of protons are transferred when a dose of the same energy as a conventional light source is irradiated, so a dose of much greater energy is required in order to obtain the same result as by the conventional photolithography process.Thus, a new material called chemically amplified photoresist has been2o introduced, capable of being easily sensitized due to its improved photosensitivity, even if the deep-UV is irradiated at a dose similar to the conventional dose.In general, the chemically amplified photoresist includes an acid-labile group which is easily subjected to acidolysis by an acid (H+) catalyst, as a dissolution inhibitor, and a photosensitive acid generator for generating proton H+on exposure to light.When exposing the chemically amplified photoresist, acid is generated by the photosensitive acid generator, and the dissolution inhibitor combined with the backbone of the polymer is hydrolyzed by the catalytic reaction of the generated acid, thereby changing polarity (e.g., solubility) of the polymer. Acidolysis of the-2polymer is amplified rapidly with the diffusion of acid, resulting in a pattern having a higher transparency.Thus, contrast, as an index for representing the difference in solubility of a chemically amplified photoresist before and after the exposure, is determined by an acid-labile group combined with the backbone of the polymer.U.S. Patent No. 4,491,528 discloses a chemically amplified photoresist containing a polymer using t-butoxycarbonyl (t-BOC) as a dissolution inhibitor causing a chemical reaction by acid.However, the thermal decomposition temperature Td of the chemically io amplified photoresist containing t-BOC as a dissolution inhibitor is lower than the glass transition temperature Tg. Thus, baking the photoresist to above the glass transition temperature before exposure, in order to vaporize organic solvent and make the photoresist film hard, decomposes the photoresist. On the other hand, if the pre-baking temperature is low enough to prevent the thermal decomposition, is airborne contaminants can be adsorbed onto the surface of the exposed photoresist film, thereby preventing a catalytic reaction by acid. This results in a pattern having an inferior profile, such as a T-top profile.SUMMARY OF THE INVENTIONTo solve the above problems of the conventional polymer containing a2o dissolution inhibitor having poor thermal characteristics, it is an objective of the present invention to provide a dissolution inhibitor which composes a chemically amplified photoresist composition together with a photosensitive polymer, and can increase the contrast of the chemically amplified photoresist composition as well as providing excellent thermal characteristics.It is another objective of the present invention to provide a chemically amplified photoresist composition which has excellent thermal characteristics as well as the ability to form a high resolution pattern due to having high contrast.To achieve the first objective, there is provided a dissolution inhibitor of a chemically amplified photoresist, in which an acid-labile di-alkylmalonate group is3o combined as a functional group with Ct to hydrocarbon.i-3Preferably, the di-alkylmalonate group is one selected from the group consisting of di-t-butyimalonate, di-tetrahydropyranyl malonate and ditrimethylsilylmalonate, and the C, to C40hydrocarbon is one selected from the group consisting of cyclohexane, dimethylenecyclohexane, xylene and methylnaphthalene.According to an aspect ofthe second objective, there is provided a chemically amplified photoresist composition comprising; a photosensitive polymer; a photosensitive acid generator; and a dissolution inhibitor in which an acid-labile di-alkylmalonate group is combined as a functional group with C1to C40hydrocarbon.Preferably, the dissolution inhibitor is mixed at a ratio of 1 -50% by weight based on the total weight of the photosensitive polymer.Preferably, the photosensitive polymer is polymerized from: one or more monomers selected from the group consisting of di-alkylmalonylmethylstyrene, alkoxystyrene derivative and (meth)acrylate derivative; and one monomer selected is from the group consisting of hydroxystyrene and hydroxystyrene derivative.Preferably, the photosensitive polymer is a polymer combined with an acidlabile dialkylmalonate group at the backborn thereofAccording to another aspect of the second objective, there is provided a chemically amplified photoresist composition containing a photosensitive polymer mixture instead of the photosensitive polymer.Preferably, the photosensitive polymer mixture comprises a copolymer A polymerized from alkoxystyrene or an alkoxystyrene derivative monomer and hydroxystyrene or a hydroxystyrene derivative monomer, and a copolymer B polymerized from a (meth)acrylate derivative monomer and hydroxy styrene or a hydroxystyrene derivative monomerPreferably, the photosensitive polymer mixture comprises a copolymer A polymerized from alkoxystyrene or an alkoxystyrene derivative monomer and hydroxystyrene or a hydroxystyrene derivative monomer, and a copolymer B polymerized from t-butoxycarbonyioxystyrene or a t-butoxycarbonyloxystyrene derivative monomer and hydroxystyrene or a hydroxystyrene derivative monomerPreferably, the mixing ratio of the copolymers A and B is 1:9-9:1.-4Preferably, the photosensitive acid generator is mixed at a ratio of 1 -50% by weight based on the total weight of the photosensitive polymer or the photosensitive polymer mixture. Also, the photosensitive acid generator may be selected from the group consisting of triarylsulfonium salts, diaryliodonium salts and sulfonates.Preferably, the photoresist composition further comprises an organic base of0.01 -2.0% by weight based on the total weight of the photosensitive polymer or the photosensitive polymer mixture. Also, the organic base may be selected from the group consisting triethylamine, triisobutylamine, triisooctylamine, diethanolamine and triethanolamine.io Therefore, the chemically amplified photoresist composition containing the dissolution inhibitor is suitable for forming a pattern having an excellent profile due to its high contrast and high thermal decomposition temperature.DESCRIPTION OF THE PREFERRED EMBODIMENTS A dissolution inhibitor of a chemically amplified photoresist, and a chemically is amplified photoresist composition containing the same, according to preferred embodiments ofthe present invention, will now be described more fully. Also, a preferred photolithography process using the chemically amplified photoresist composition will be described. This invention may, however, be embodied in many different forms and should not be construed as being limited to the embodiments set2o forth herein; rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the concepts of the invention to those skilled in the art.Dissolution inhibitor of chemicallv amplified photoresist A dissolution inhibitor of a chemically amplified photoresist according to the present invention is a compound in which an acid-labile dialkylmalonate group is combined as a functional group with to C40hydrocarbon.The Ct to C40 hydrocarbon is cyclohexane, dimethylenecyclohexane, xylene or methylnaphthalene, and the dialkylmalonate group is a di-ti-butylmalonate, ditetrahydropyranyl malonate or di-trimethylsilylmalonate group.-5In detail, the dissolution inhibitor ofthe present invention is expressed by the following chemical formula (1).[RiH4_CH(CO2R2)2]m...(1)In the chemical formula (1), m is 1 or 2, R1 is Ct to C40hydrocarbon, and R2 is t-butyl, tetrahydropyranyl or trimethylsilyl group.s Preferably, R1 is a cyclohexyl, dimethylcyclohexyl, xylenyl or naphthalenylmethyl group.The dissolution inhibitor of the present invention has a very low solubility due to its bulky functional group, a dialkylmalonate group. However, after the exposure process, the dialkylmalonate group is hydrolyzed by acid to form a malonate group, io markedly increasing solubility. Also, because the dialkylmalonate group is stable to heat, the dialkylmalonate group shows stable thermal characteristics at a temperature higher than a glass transition temperature of the polymer which composes a photoresist composition together with the dissolution inhibitor.Photosensitive polymer and Photosensitive polymer mixture for photoresist is Photosensitive polymer for photoresistA photosensitive polymer according to the present invention, which composes a photoresist composition together with the dissolution inhibitor, is a polymer formed of one or more monomers such as di-alkylmalonylmethylstyrene, alkoxystyrene derivative or acrylate derivative, and a hydroxystyrene monomer or hydroxystyrene derivative monomer.That is, the photosensitive polymer may be a copolymer, terpolymer or tetrapolymer, and preferably the photosensitive polymer is expressed by the following chemical formula (2).In the chemical formula (2), R3 is t-butyi, tetrahydropyranyl or trimethylsilyl;R4, R5, R7, R9 and R10 are each independently hydrogen atom or methyl group;R6 is alkoxyl-1 -ethyl, tetrahydropyranyl, t-butyl or t-butoxycarbonyl; R8 is t-butyl or tetrahydropyranyl group; and k / (k+l+m+n) is 0.0-0.5, l / (k+1+m+n) is 0.0-0.5, m / (k+l+m+n) is 0.0-0.5, and n / (k+l+m+n) is 0.5-0.99.-(2)CH / \RjOsC CO2R.3Preferably, a polymer in which an acid-labile dialkylmalonate group, such as di-t-butyl malonate, di-tetrahydropyranyl malonate and di-trimethylsilyl malonate, is combined with the polymer's backbone, is used as the photosensitive polymer according to the present invention.The photosensitive polymer according to the present invention is bulky before the exposure. However, after the exposure, side chain group R3, R6 or R8 combined with the backbone of the polymer leaves malonate, hydroxy or carboxyl group by the acid generated during the exposure. Thus, solubility changes greatly during exposure. Also, because the side chain group is stable to heat, the photosensitive polymer has stable thermal characteristics at a temperature higher than the glass transition temperature.Photosensitive polymer mixtureA photosensitive polymer mixture according to a first embodiment of the present invention, which composes a photoresist composition together with the dissolution inhibitor, is a mixture of a copolymer A polymerized from an alkoxystyrene or alkoxystyrene derivative monomer, and a hydroxystyrene or hydroxystyrene derivative monomer, and a copolymer B polymerized from a (meth)acrylate derivative monomer or a hydroxy styrene or hydroxystyrene derivative monomer.~ΊPreferably, the polymer mixture for a chemically amplified photoresist according to the first embodiment of the present invention is formed of the copolymers expressed by the following chemical formulae (3) and (4).RgReIn the chemical formulae (3) and (4), R4, R5, R7, R9 and R10 are each independently hydrogen atom or methyl group; R6 is alkoxyl-1 -ethyl, tetrahydropyranyl, t-butyl or t-butoxycarbonyl; R8 is t-butyl or tetrahydropyranyl group; I, m and n are integers, n / (n+l) is 0.5-0.9, and n(m+n) is 0.5-0.9.Preferably, in the photosensitive polymer mixture ofthe present invention, R6 is 1-ethoxyethyl group.io Preferably, the mixing ratio of the copolymers expressed by the chemical formulae (3) and (4) is 1:9-9:1 and the weight average molecular weight of each polymer is 5,000-50,000.A photosensitive polymer mixture according to a second embodiment of the present invention is a mixture of a copolymer A polymerized from an alkoxystyrene is or alkoxystyrene derivative monomer, and a hydroxystyrene or hydroxystyrene derivative monomer, and a copolymer B polymerized from a t-8butoxycarbonyloxystyrene or t-butoxycarbonyloxystyrene derivative monomer, and a hydroxystyrene or hydroxystyrene derivative monomer.Preferably, the polymer mixture for a chemically amplified photoresist according to the second embodiment of the present invention is formed of the s polymers expressed by the following chemical formulae (3) and (5).F?4 F?9R 1 3In the chemical formulae (3) and (5), R4, R5, R9, R10, R11 and R12 are each independently hydrogen atom or methyl group; R6 is alkoxyl-1-ethyl, tetrahydropyranyl, t-butyl or t-butoxycarbonyl; R13 is t-butoxycarbonyl group; and j, I and n are integers, n / (l+n) is 0.5-0.9 and n / (j+n) is 0.5-0.9.io Preferably, the mixing ratio of the polymers expressed by the chemical formulae (3) and (5) is 1:9-9:1 and the weight average molecular weight of each polymer is 5,000-50,000.Chemically amplified photoresist compositionA chemically amplified photoresist composition according to the present is invention includes the photosensitive polymer or photosensitive polymer mixture, the dissolution inhibitor and photosensitive acid generator.-9Preferably, the dissolution inhibitor is mixed at a ratio of 1 -50% by weight based on the total weight of the photosensitive polymer or photosensitive polymer mixture.Also, preferably, the photosensitive acid generator is mixed at a ratio of1-15% by weight based on the total weight of the photosensitive polymer or photosensitive polymer mixture, and a material having a high thermal stability is used as the photosensitive acid generator. Such a material may be triarylsulfonium salts, diaryliodonium salts and sulfonates. In detail, triphenylsulfonium triflate, triphenylsulfonium antimonate, diphenyliodonium triflate, diphenylidonium io antimonate, methoxydiphenyliodonium triflate, di-t-butyldiphenyliodonium triflate, 2,6,-dinitrobenzylsulfonate, pyrogallol tris(alkylsulfonate) or N-hydroxysuccinimide triflate may be used as the photosensitive acid generator.Preferably, the photoresist composition according to the present invention further includes an organic base of 0.01 -2.0% by weight based on the total weight is of the photosensitive polymer or photosensitive polymer mixture. The organic base may be triethylamine, triisobutylamine, triisooctylamine, diethanolamine or triethanolamine. The organic base prevents the acid generated in an exposed portion from being diffused into a non-exposed portion after the exposure, and also ensures that the overall acid concentration remains uniform, even in the case when2o neutralization occurs at the surface by external contaminants.As described above, the photoresist composition of the present invention includes a dissolution inhibitor with which an acid-labile di-alkylmalonate group, e.g., di-t-butyl malonate, di-tetrahydropyranyl malonate or di-trimethylsilyl malonate, is combined as a functional group. The di-alkylmalonate group is very bulky, and is hydrolyzed into malonate by acid generated by the photosensitive acid generator during the exposure. Thus, contrast, which is an index indicating the solubility difference between before and after the exposure, markedly increases. Also, because the di-alkylmalonate group is thermally stable, the photoresist composition of the present invention has thermal stability at a temperature higher than the glass3o transition temperature (approximately 130°C).Also, the photosensitive polymer (or photosensitive polymer mixture) of the present invention is bulky before the exposure. However, a side chain group-10combined with the backbone of the polymer leaves forming a malonate, hydroxy or carboxyl group by the acid generated by the exposure. Thus, the solubility difference between before and after the exposure is markedly increased. Also, because the side chain group is thermally stable, the photosensitive polymer is thermally stable at a temperature higher than the glass transition temperature.Preparation method of dissolution inhibitor for chemically amplified photoresistPreparation method of hydrocarbon compound having di-alkylamlonate group as a functional group io As shown in the following reaction formula (1), after dissolving dialkylmalonate (II) in a tetrahydrofuran (THF) solution in which sodium hydroxide has been dissolved, a halogen compound (I) is added to this solution to form a dialkylmalonylhydrocarbon compound (III) through a substitution reaction.+[ CH2(CO2R2)2]m- [ R1H4- CH(CO2R2)2]m +xm...(1) ( / ) ( / / ) ( / / / )In the reaction formula (1), m is 1 or 2, R1 is to C40hydrocarbon, R2 is ti5 butyl, tetrahydropyranyl or trimethylsilyl group, and X is halogen.Preferably, the C, to C40hydrocarbon is cyclohexane, dimethylenecyclohexane, xylene or methylnaphthalen.Preparation method of photosensitive polymer or photosensitive polymer compound1. Preparation method of polymer having di-alkylmalonate functional group1-1. Preparation of monomer; preparation of di-alkvlmalonylmethylstyrene (VI)CH2= CHCHzClRjOCHz (IV) (V)-11ORjNaH thFCHz = CHCH?ICH <V[)-(2)As shown in the above reaction formula (2), after dissolving di-alkylmalonate (V) in a THF solution in which sodium hydroxide has been dissolved, a chloromethylstyrene (IV) is added to this solution to form dialkylmalonylmethylstyrene (VI) through a substitution reaction.in the reaction formula (2), R3 is t-butyl, tetrahydropyranyl or trimethylsilyl group.1-2. Preparation of polymer (XI)Here, a polymer (XI) is polymerized from one or more monomers selected from the group consisting of di-alkylmalonyimethylstyrene (VI), alkoxystyrene derivative (VII) and (meth)acrylate derivative (VIII), and hydroxystyrene or hydroxystyrene derivative monomer.1-2-1. PolymerizationA polymer (X) is formed through polymerization as shown in the following reaction formula (3).F?9υCHj (IX)-(3) (VI)-12R<R?AlgSNTOLUENE “( CH2 CH -½ (-CHz C~fi—( CH;'—c -) cn2ICH / \R3O2C CO2R3 c=cIR 0CH j(X) is In the reaction formula (3), R3 is a t-butyl, tetrahydropyranyl or trimethylsilyl group; R4, R5, R7, R9 and R10 are each independently hydrogen atom or methyl group; R6 is alkoxyl-1-ethyl, tetrahydropyranyl, t-butyl or t-butoxycarbonyl; R8 is tbutyl or tetrahydropyranyl group; and k / (k+l+m+n) is 0.0-0.5, l / (k+l+m+n) is 0.0-0.5, m / (k+l+m+n) is 0.0-0.5, and n / (k+l+m+n) is 0.5-0.99.That is, after dissolving one or more monomers selected from the group consisting of di-alkylmalonylmethylstyrene (VI), alkoxystyrene derivative (VII) and (meth)acrylate derivative (VIII), and an acetoxystyrene or acetoxystyrene derivative monomer (IX) in an organic solvent, e.g., toluene, a polymerization initiator, e.g., azobisisobutyronitrile (AIBN), is added to obtain a polymer (X) through polymerization.1-2-2. Deacetylation of polymer (X)As shown in the following reaction formula (4), the polymer (X) is deacetylated using an organic base, resulting in a polymer (XI) having a weight average molecular weight of 5,000-100,000, expressed by the chemical formula (2). Here, ammonium hydroxide or hydrazine is used as the organic base.BASEMETHANCl-13R?Rs-( GHz —CH-k-(-CH2 — C-W CHj — C A—(-CH2—C^~CH:ICHX' \RjOjC CO2R3Rs ex)R4C— 0IIRsR 10I c =0CH jR?Ra-( ch2—CH -tCHj—CV( CH2— C )_ ( CH2—C^7 ch2ICHX' \RjO2C COjRjRsC=CR ioOHReRe (xi)2. Preparation method of photosensitive polymer mixture2-1. Preparation of copolymer expressed by the chemical formula (3)The copolymer expressed by the chemical formula (3) is formed of an 5 alkoxystyrene or alkoxystyrene derivative monomer, and a hydroxystyrene or hydroxystyrene derivative monomer.A copolymer is prepared such that k and m are set to 0 and n / (n+l) is set to 0.5-0.9 in the reaction formula (3), and the deacetylation ofthe reaction formula (4) is performed, resulting in the copolymer expressed by the chemical formula (3) having a weight average molecular weight of 5,000-50,000.2-2. Preparation of copolymer expressed by the chemical formula (4)The copolymer expressed by the chemical formula (4) is formed of hydroxystyrene or hydroxystyrene derivative monomer and (meth)acrylate derivative monomer.A copolymer is prepared such that k and I are set to 0 and n / (m+n) is set to0.5-0.9 in the reaction formula (3), and the deacetylation of the reaction formula (4)-14is performed, resulting in the copolymer expressed by the chemical formula (4) having a weight average molecular weight of 5,000-50,000.2-3 Preparation of copolymer expressed by the chemical formula (5)The copolymer expressed by the chemical formula (5) is formed of a hydroxystyrene or hydroxystyrene derivative monomer and a tbutoxycarbonyloxystyrene or t-butoxycarbonyloxystyrene derivative monomer.The copolymer is formed such that acetoxystyrene or acetoxystyrene derivative monomer and t-butoxycarbonyloxystyrene or t-butoxycarbonyloxystyrene derivative monomer are mixed at a ratio of 0.5-0.9. Here, the mixing ratio is io expressed by n / (j+n), wherein n is the number of acetoxystyrene or acetoxystyrene derivative monomer, and j is the number of the t-butoxycarbonyloxystyrene or tbutoxycarbonyloxystyrene derivative monomer. Then, the deacetylation is performed, resulting in the copolymer expressed by the chemical formula (5) having a weight average molecular weight of 5,000-50,000.is Preparation method of chemically amplified photoresist composition, and photolithography using the sameIn the preparation method of a chemically amplified photoresist composition according to the present invention, the photosensitive polymer expressed by the chemical formula (2), the mixture of the photosensitive polymers expressed by the chemical formulae (3) and (4), or the mixture of the photosensitive polymers expressed by the chemical formulae (3) and (5), are dissolved together with the dissolution inhibitor expressed by the chemical formula (1) and the photosensitive acid generator, in an appropriate solution, to form in a photoresist composition.The dissolution inhibitor expressed by the chemical formula (1) is mixed at a ratio of 1 -50% by weight based on the total weight of the polymer or polymer mixture, and the photosensitive acid generator is mixed at a ratio of 1 -15% by weight based on the total weight of the polymer or polymer mixture. Preferably, the photosensitive acid generator is triarylsulfonium salts, diaryliodonium salts or sulfonates, which are thermally stable.-15Preferably, an organic base of 0.01 -2.0% by weight based on the weight of the polymer or polymer mixture is further dissolved to form the photoresist composition. Preferably, the organic base is triethylamine, triisobutylamine, triisooctylamine, diethanolamine or triethanolamine.The chemically amplified photoresist composition formed by the above method may be applied to a general photolithography process. Particularly, the chemically amplified photoresist composition is suitable for forming a fine pattern having a design rule of 0.25^m or less, using deep ultraviolet rays as a light source for exposure.io First, the above-described photoresist composition is deposited on a substrate having a target to be patterned, to form a photoresist film having a predetermined thickness. Then, pre-baking of the photoresist film is performed before exposure. Because the photoresist composition of the present invention, containing a di-alkylmalonate group causing a chemical reaction by acid, has a is higher thermal decomposition temperature Td (approximately 170°C or more) than its glass transition temperature Tg (approximately 130°C), a thermal process at a high temperature is possible during the pre-baking before the exposure. Thus, damage to the photoresist film by airborne contaminants can be effectively prevented.2o After the pre-baking, the photoresist film is exposed to deep ultraviolet rays, using a mask having a predetermined pattern. Acid is generated by the photosensitive acid generator in the photoresist film by the exposure, and dialkylmalonate of the dissolution inhibitor is acidolyzed into malonate by catalytic reaction with the generated acid as shown in the following reaction formula (5).Then, as shown in the reaction formula (6), the di-alkylmalonate, alkoxy or ester group of the photosensitive polymer is acidolyzed to form a malonate, hydroxy or carboxyl group. As a result, the polarity of the exposed portion of the photoresist film and the polarity of the non-exposed portion become very different. That is, contrast is high.[ R, CH(CO2R2)2]m[ R, +(- CH(CO2H)2]mHEAT..(5)-16R4 Rt Rg-( CH?—CH^-f-cH2-0-^( ch2— c5^(-ch2—CH2CHX \RiO2C CCjRjRsR&c= 0ReR·OH (X)R?Rg...(6)Hf.HEAT-(CH; —CH)k( CHZ—0-),-( CH2 — C (-CHz —C“ o Rs nCH2CH X \HOzC COzHR<OHR ioOH (XI)After the exposure, a thermal treatment is performed on the photoresist film for a short time before development. The post-exposure thermal treatment further activates acidolysis by a catalytic reaction of acid within the exposed portion. In other words, this completely acidolyzes the di-alkylmalonate group of the dissolution inhibitor within the exposed portion into malonate, and the di-alkylmalonate group, alkoxy group or ester group of the photosensitive polymer into a malonate, hydroxy or carboxyl group, to remarkably increase the contrast.Next, a developing process is performed using an appropriate developer liquid which is selected depending on whether the photoresist film is used for a io positive or negative purpose. Then, general processes are performed to complete the photoresist pattern.When forming a photoresist pattern using the photoresist composition of the present invention, a high resolution pattern having a good profile can be formed.The present invention will be described through the following examples, is However, the present invention is not limited to the following examples.-17<Example 1: Preparation of dissolution inhibitor1-1. Preparation of 1,4-bis(di-t-butylmalonyl)cyclohexane2.9g of sodium hydroxide (0.12mo!) was put in a round-bottom flask and dissolved in 250ml of tetrahydrofuran (THF). 25g of di-t-butylmalonate (0.11 mol) was slowly dropped into the solution and reacted for about 1 hour. Then, 2.1 g of1,4-dibromocyclohexane (O.OSmol) was slowly dropped into the mixture at 0°C, and reacted for 12 hours at 45°C. After the reaction was completed, excessive THF was evaporated from the reaction product. Then, the resultant product was dissolved in excessive water, neutralized with hydrochloric acid, and then extracted using diethyl io ether.After drying the obtained precipitant using magnesium sulfate, the reaction product was separated using column chromatography (yield 55%).1-2. Preparation of 1,4-bis(di-t-butylmalonyl)-p-xyleneThe same processes as in the above section (1-1) were performed, except is that 12.1g of dibromo-p-xylene (O.OSmol) was used instead of 1,4dibromocyclohexane.After drying the obtained precipitant using magnesium sulfate, the reaction product was separated using column chromatography (yield 55%).<Example 2: Preparation of di-t-butylmalonylmethylstyrene monomer>2o 2.9g of sodium hydroxide (0.12mol) was dissolved in 250ml of THF. 25g of di-t-butylmalonate (0.11 mol) was slowly dropped into the solution and reacted for about 1 hour. Then, 0.1 mol of chloromethylstyrene was slowly dropped into the mixture at 0°C, and reacted for 12 hours at room temperature. After the substitution reaction was completed, the reaction product was dissolved in excessive water, neutralized with hydrochloric acid, and then extracted using diethyl ether.After drying the obtained precipitant using magnesium sulfate, the reaction product was separated using column chromatography (yield 65%).Nuclear magnetic resonance (NMR) and Fourier transform infrared radiation (FT-IR) spectroscopy analyses performed on the obtained reaction product showed ao that the product was di-t-butylmalonylmethylstyrene.-18'H-NMR(CDCl3)(ppmy1.4(s,18H), 3.1(d, 2H), 3.5(t, 1H), 5.2(dd, 1H), 5.7(dd, 1H), 6.6(dd, 1H),7.2(m, 4H)FT-lR(NaCI}(cm')·. 2978(C-H, t-butyl), 1727(0=0), 1369, 1140, 847 «Example 3: Preparation of photosensitive copolymer>3-1. Preparation of copolymer polymerized di-t-butylmalonylmethylstyrene and hydroxystyrene monomers3g of di-t-butylmalonylmethylstyrene (9mmol) and 7.5g of acetoxystyrene (45mmol) were dissolved in 50ml of toluene. Then, 0.44g of AIBN was added, and io purged using nitrogen gas for 1 hour, and polymerization was performed for about 24 hours at 70°C.After the polymerization, the reaction product was precipitated in excessive nhexane (about 10 times), and the precipitate was dried in a vacuum oven maintained at a temperature of 50°C for about 24 hours to separate the reaction product (yield is 70%).The obtained reaction product was a copolymer containing di-tbutylmalonylmethylstyrene and hydroxystyrene monomers, having a weight average molecular weight of 12,157 and a polydispersity of 1.6.10g of the obtained reaction product was added to 10ml of ammonium 2o hydroxide (28%), and refluxed for 4 hours for deacetylation. Then, the reaction product was slowly precipitated in excessive water.The precipitant was dissolved in THF, reprecipitated in excessive n-hexane, and then dried at a vacuum oven maintained at a temperature of 50°C to separate the reaction product (yield 90%).The obtained reaction product was a copolymer containing di-tbutylmalonylmethylstyrene and hydroxystyrene monomers, having a weight average molecular weight of 11,438 and a polydispersity of 1.67.3-2. Preparation of copolymer using poty(hydroxystyrene) and ethylvinylether 12g of poly(hydroxystyrene) was dissolved in 60ml of THF and 3.6g of ao ethylvinylether was added. Sufficient p-toluenesulfonate (p-TSA) to act as a catalyst-19was added and reacted at 40°C for 12 hours. After the reaction was complete, the reaction product was slowly dropped into excessive water and neutralized with potassium carbonate.The precipitant was dissolved in THF, reprecipitated in excessive n-hexane, and then dried in a vacuum oven maintained at a temperature of 50°C to separate the reaction product (yield 85%).The obtained reaction product was a copolymer. A weight average molecular weight was 12,285, a polydispersity was 1.67 and transmittance against ultraviolet rays was 73% / μΠΊ.io 3-3. Preparation of copolymer using poly(hydroxystyrene) and 3,4-dihydro-2pyranA copolymer containing tetrahydropyranoxystyrene and hydroxystyrene monomers was prepared by the same processes as in the above section (3-2) except that 4.2g of 3,4-dihydro-2-pyran was used instead of ethylvinylether (yield is 80%).The obtained copolymer had a weight average molecular weight of 13,587 and a polydispersity of 1.74.3-4. Preparation of copolymer using poly(hydroxystyrene) and tbutoxycarbonateA copolymer containing t-butoxystyrene and hydroxystyrene monomers was prepared by the same processes as in the above section (3-2) except that tbutoxycarbonate was used instead of ethylvinylether (yield 85%).The obtained copolymer had a weight average molecular weight of 13,889 and a polydispersity of 1.8.3-5. Preparation of copolymer polymerized hydroxystyrene and t-butylacrylate monomers20g of acetoxystyrene (120mmol) and 7.8g of t-butylacrylate (60mmol) were dissolved in 140ml of toluene. The reaction product was separated by the same processes as in the above section (3-1) except that 1 48g of AIBN was added.-20The obtained reaction product was a copolymer containing acetoxystyrene and t-butylacrylate monomers, having a weight average molecular weight of 12,017 and a polydispersity of 1.83.The obtained reaction product was deacetylated by the same method as in 5 the above section (3-2), resulting in a copolymer containing t-butylacrylate and hydroxystyrene monomers, having a weight average molecular weight of 11,438 and a polydispersity of 1.82.<Example 4: Preparation of photosensitive terpolymer>4-1. Preparation of terpolymer containing hydroxystyrene, t-butylacrylate and io di-t-butylmalonylmethylstyrene monomers11.11 g of acetoxystyrene (70mmol), 2.6g of t-butylacrylate (20mmol) and 3.4g of di-t-butylmalonylmethylstyrene (10mmol) were dissolved into 75ml of toluene. Then, 0.82g of AIBN was added, and purged using nitrogen gas for 1 hour, and polymerization was performed for about 24 hours at 70°C.is After the polymerization, the reaction product was precipitated in excessive nhexane (about 10 times), and the precipitate was dried in a vacuum oven maintained at a temperature of 50°C for about 24 hours to separate the reaction product (yield 70%).The obtained reaction product had a weight average molecular weight of2o 12,557 and a polydispersity of 1.98.10g of the obtained reaction product was added to a mixture of 10ml of ammonium hydroxide (28%) and 50ml of methanol, and refluxed for 4 hours for deacetylation. Then, the reaction product was slowly precipitated in excessive water.The precipitant was dissolved in THF, reprecipitated in excessive n-hexane, and then dried in a vacuum oven maintained at a temperature of 503C to separate the reaction product (yield 90%).The obtained reaction product was a terpolymer containing hydroxystyrene, butylacrylate and di-t-butylmalonylmethylstyrene monomers at a ratio of 70:25:5,3o having a weight average molecular weight of 11,438 and a polydispersity of 1.97.-214-2. Preparation of terpolymer containing hydroxystyrene, t-butoxystyrene and di-t-butylmalonylmethylstyrene monomers10.5g of acetoxystyrene (63mmol), 3.2g of t-butoxystyrene (18mmol) and 3g of di-t-butylmalonylmethylstyrene (9mmol) were dissolved in 80ml of toluene. A terpolymer was prepared by the same processes and under the same conditions as in the above section (4-1) except that 0.74g of AIBN was added (yield 80%).The obtained reaction product was a terpolymer containing hydroxystyrene, tbutoxystyrene and di-t-butylmalonylmethylstyrene at a ratio of 70:20:10. A weight average molecular weight of the product was 12, 639, a polydispersity was 1.85, io and transmittance against ultraviolet rays was 73% / ^m.4-3. Preparation of terpolymer containing hydroxystyrene, t-butylacrylate and t-butoxystyrene monomers9.7g of acetoxystyrene (60mmol), 4.3g of t-butylacrylate (30mmol) and 1.8g of butoxystyrene (1 Ommol) were dissolved in 80ml of toluene. A terpolymer was is prepared by the same processes and under the same conditions as in the above section (4-1) except that 0.67g of AIBN was added (yield 85%).The obtained reaction product was a terpolymer having a weight average molecular weight of 11,537 and a polydispersity of 1.93.<Example 5: Preparation of a tetrapolymer containing hydroxystyrene, t20 butylacrylate, t-butoxystyrene and di-t-butylmalonylmethylstyrene monomers>9.7g of acetoxystyrene (60mmol), 2.8g of t-butylacrylate (20mmol), 1,8g of butoxystyrene (1 Ommol) and 3.4g of di-t-butylmalonylmethylstyrene (1 Ommol) were dissolved in 90ml of toluene. A terpolymer was prepared by the same processes and under the same conditions as in the above section (4-1) except that 0.67g ofAIBN was added (yield 80%).The obtained reaction product was a terpolymer having a weight average molecular weight of 12,430 and a polydispersity of 1.87.<Example 6: Preparation of photoresist composition and photolithography using the same>-226-1. Preparation of photoresist composition containing 1,4-bis(di-tbutylmalonyljcyciohexane as a dissolution inhibitor, a photosensitive copolymer and a photosensitive acid generator, and photolithography using the same1.0g of the photosensitive copolymer containing hydroxystyrene and di-ts butylmalonylmethylstyrene monomers, prepared as per the above section (3-1),0.02g of triphenylsulfonium triflate (TPSOTf) as a photosensitive acid generator, and 0.2g of 1,4-bis(di-t-butylmalonyl)cyclohexane, prepared as per the above section (11), were completely dissolved in 6g of propylene glycol monomethyl ether acetate (PGMEA), then filtered through a filter having pores of 0.2^m. resulting in a io photoresist composition.The obtained photoresist composition was spin-coated on a wafer having a material layer to be patterned, to a thickness of approximately 0.5^m. The wafer coated with the photoresist composition was soft-baked at approximately 130°C for about 90 seconds, exposed using a mask defining a patten with 0.30μΓΠ line and is space arrays and a stepper using a KrF eximer laser having a numerical aperture (NA) of 0.45, and then post-baked at approximately 140°C for about 90 seconds. Then, the resultant was developed using 2.38% by weight of tetramethylammonium hydroxide for 60 seconds to form a photoresist pattern. Then, the material layer was etched using the resultant photoresist pattern.As a result, a photoresist pattern having an excellent profile with 0.30μπι line and space arrays could be formed with an exposure energy of 18mJ / cm2dose.Also, a material layer pattern having an excellent profile could be obtained using the photoresist pattern.6-2. Preparation of photoresist composition containing bis(di-t-butylmalonyl)25 p-xylene as a dissolution inhibitor, a photosensitive copolymer and a photosensitive acid generator, and photolithography using the sameA photoresist composition was prepared and photolithography was performed, by the same methods as in the above section (6-1) except that 0.2g of bis(di-t-butylmalonyl)-p-xylene was used as the dissolution inhibitor, instead of 1,43o bis(di-t-butylmalonyl)cyclohexane.-23As a result, a photoresist pattern having an excellent profile with 0.30μΓΠ line and space arrays could be formed with an exposure energy of 21 mJ / cm2dose.Also, a material layer pattern having an excellent profile could be obtained using the photoresist pattern.6-3. Preparation of photoresist composition containing bis(di-t-butylmalonyI)p-xylene as a dissolution inhibitor, a photosensitive copolymer, a photosensitive acid generator and an organic base, and photolithography using the sameA photoresist composition was prepared and photolithography was performed, by the same method as in the above section (6-2) except that 2mg of io triethylamine was further added as an organic base.As a result, a photoresist pattern having an excellent profile with 0.30μΓΤΐ line and space arrays could be formed with an exposure energy of 33mJ / cm2dose.Also, a material layer pattern having an excellent profile could be obtained using the photoresist pattern.is 6-4. Preparation of photoresist composition containing bis(di-t-butylmalonyl)p-xylene as a dissolution inhibitor, a photosensitive terpolymer and a photosensitive acid generator, and photolithography using the sameA photoresist composition was prepared and photolithography was performed, by the same method as in the above section (6-2), except that 1.0g of2o terpolymer containing hydroxystyrene, t-butylacrylate and di-tbutylmalonylmethylstyrene monomers, prepared as per the above section (4-1), was used instead of the photosensitive copolymer.As a result, a photoresist pattern having an excellent profile with 0.30μΓτι line and space arrrays could be formed with an exposure energy of 24mJ / cm2dose.Also, a material layer pattern having an excellent profile could be obtained using the photoresist pattern.6.5 Preparation of photoresist composition containing bis(di-t-butylmalonyl)p-xylene as a dissolution inhibitor, a photosensitive terpolymer, a photosensitive acid generator and an organic base, and photolithography using the same-24A photoresist composition was prepared and photolithography was performed by the same methods as in the above section (6-4) except that 2mg of triethylamine was further added as an organic base.As a result, a photoresist pattern having an excellent profile with 0.30μΠΊ line 5 and space arrays could be formed with exposure energy of 36mJ / cm2dose. Also, a material layer pattern having an excellent profile could be obtained using the photoresist pattern.The dissolution inhibitor according to the present invention has an acid-labile di-alkylmalonate group as a functional group, to greatly increase the difference in io solubility ofthe chemically amplified photoresist composition before and after exposure. The di-alkylmalonate group, e.g., the di-t-butylmalonate, ditetrahydropyranylmalonate or di-trimethylsilyl malonate group, is very bulky, and its solubility is very low before exposure. However, the di-alkylmalonate group is actdolyzed into malonate by acid generated by the photosensitive acid generator is during exposure, thereby maximizing solubility of the exposed chemically amplified photoresist composition. Thus, the solubility difference before and after exposure, that is, contrast, is significantly higher than a conventional photoresist composition having a t-butoxycarbonyl (t-BOC) group.Also, the photosensitive polymer forming the photoresist composition together with the dissolution inhibitor has the di-alkylmalonate group, alkoxy group or ester group which is in a very bulky state before exposure. The bulky groups are acidolyzed into a malonate, hydroxy or carboxyl group having a higher polarity, by the acid generated during exposure. Thus, polarity of the photoresist film in the exposed portion and the non-exposed portion becomes very different, increasing contrast.The dissolution inhibitor, photosensitive polymer and photosensitive acid generator according to the present invention have excellent thermal characteristics, so the photoresist composition containing those has a thermal decomposition temperature higher than a glass transition temperature (approximately 130°C) so Thus, before exposing the photoresist film, the photoresist film is pre-baked at a temperature higher than the glass transition temperature, to harden the photoresist-25film. Thus, inhibition of the function of the acid within the exposed portion, by airborne contaminants adsorbed onto the photoresist film, can be effectively prevented. As a result, pattern defects such as a T-top profile are prevented, and a fine pattern having an intended profile can be formed.

Claims

CLAIMS 1. A dissolution inhibitor of a chemically amplified photoresist, comprising an acid-labile dialkylmalonate group bound to aCi to C20 hydrocarbons wherein the Ci to C20 hydrocarbon is selected from the group consisting of 5 cyclohexane, dimethylenecyclohexane, xylene and methylnaphthalene, and wherein the di-alkylmalonate group is selected from the group consisting of di-tbutylmalonate, di-tetrahydropyranyl malonate and di-trimethylsilylmalonate.

2. The dissolution inhibitor of claim ], wherein the dissolution inhibitor of the photoresist is represented by the following chemical formula (CF1): 10 [ r, -H- CH{CO2R2)2 Im (CFD wherein m is 1 or 2; Rl is a Ci to C20 hydrocarbon; and R2 is selected from the group comprising a l-butyl, tetrahydropyranyl group and a trimethylsilyl group, and wherein Rl is selected from the group comprising cyclohexyl, dimethylcyclohexyl. xylenyl and naphthalenylmethyl groups.

153. A chemically amplified photoresist composition comprising: a photosensitive polymer, a photosensitive acid generator, and a dissolution inhibitor in which an acid-labile di-alkylmalonate group is bound to a C( to C20 hydrocarbons 20 wherein the Ci to C20 hydrocarbon is selected from the group consisting of cyclohexane, dimethylenecyclohexane, xylene and methylnaphthalene, and wherein the di-alkylmalonate group is selected from the group consisting of di-tbutylmalonate. di-tetrahydropyranyl malonate and di-trimethylsilylmalonate.

4. The chemically amplified photoresist composition of claim 3, wherein the dissolution inhibitor is represented by the following chemical formula (CF1): ( R, -H-CH(CO2r2)2 ]m (cfi) wherein m is 1 or 2; Rl is a Cj to C20 hydrocarbon; and R2 is selected from the group 5 comprising a t-butyl, tetrahydropyranyl group and a trimethylsilyl group, and wherein the Ci to C20 hydrocarbon is selected from the group comprising cyclohexane, dimethylenecyclohexane, xylene and methylnaphthalene.

5. The chemically amplified photoresist composition of claim 3, wherein the dissolution inhibitor is mixed at a ratio of from about 1% to about 50% by weight based on the total 10 weight of the photosensitive polymer.

6. The chemically amplified photoresist composition of claim 3, wherein the photosensitive polymer is polymerized from: one or more monomers selected from the group comprising dialkylmalonylmethylstyrene, alkoxy styrene derivative and a (meth) acryl ate derivative, and 15 one monomer selected from the group comprising hydroxystyrene and a hydroxy styrene derivative.

7. The chemically amplified photoresist composition of claim 6, further comprising an acidlabile di-alkylmalonate group bound to a backbone of the photosensitive polymer, and the dialkylmalonate group is selected from the group comprising a di-t-butylmalonate group, a di20 tetrahydropyranylmalonate group and a di-trimethylsilyl group.

8. The chemically amplified photoresist composition of claim 7, wherein the photosensitive polymer is represented by the following chemical formula (CF2): (CF2) R7 R9 -f CH2 — CH-)e—(-CH2—C-)|—( CH2 —C ) ~ {-CHz— / R3O2C CH2 CH \ CO2R3 Rs Rs Rb I Rio OH wherein R3 is selected from the group comprising t-butyl, tetrahydropyranyl and trimethylsilyl; 5 R4, R5, R7, R9 and RIO are each independently one selected from the group comprising of a hydrogen atom and a methyl group; R6 is selected from the group comprising alkoxyl-1-ethyl, tetrahydropyranyl, t-butyl and t-butoxycarbonyl; R8 is selected from the group comprising a t-butyl group and atetrahydr0pyranyl 10 group; k / (k+l+m+n) is from about 0.0 to 0.5, l / (k+l+m+n) is from about 0.0 to 0.5,m / (k+l+m+n) is from about 0.0 to 0.5, n / (k+l+m+n) is from about 0.5 to 0.99; and the weight average molecular weight of the polymer is from about 5,000 to 100,000.

9. The chemically amplified photoresist composition of claim 3, wherein the photosensitive 15 acid generator is mixed at a ratio of from about 1 to 15% by weight based on the total weight ofthe photosensitive polymer.

10. The chemically amplified photoresist composition of claim 3, wherein the photosensitive acid generator is selected from the group comprising triaryl sulfonium salts, diaryliodonium salts and sulfonates.

11. The chemically amplified photoresist composition of claim 3, further comprising an 5 organic base of from about 0.01 to 2.0% by weight based on the total weight of the photosensitive polymer.

12. The chemically amplified photoresist composition ofclaim 11, wherein the organic base is selected from the group comprising triethylamine, triisobutylamine, triisooctylamine, diethanolamine, triethanolamine, and N-methyl pyrrolidone. 1013. The chemically amplified photoresist composition of claim 12, wherein the dissolution inhibitor is mixed at a ratio of from about 1 to 50% by weight based on the total weight of the photosensitive polymer.14, A chemically amplified photoresist composition comprising: a photosensitive polymer mixture;15 a photosensitive acid generator; and a dissolution inhibitor in which an acid-labile di-alkylmalonate group is bound to a C] to C20 hydrocarbon, wherein the Ci to C20 hydrocarbon is selected from the group consisting of cyclohexane, dimethylenecyclohexane, xylene and methyinaphthalene, and 20 wherein the di-alkylmalonate group is selected from the group consisting of di-tbutylmalonate, di-tetrahydropyranyl malonate and di-trimethylsilylmalonate.

15. The chemically amplified photoresist composition of claim 14, wherein the dissolution inhibitor is represented by the following chemical formula (CF1): [ C / 7(CO2R2)2 ]m (CF1) wherein m is 1 or 2; Rl is Ci to C20 hydrocarbon; and R2 is selected from the group comprising a t-butyl group, a tetrahydropyranyl group and a trimethylsilyl group16. The chemically amplified photoresist composition of claim 14, wherein the photosensitive polymer mixture comprises a copolymer A polymerized from a monomer of 5 alkoxystyrene or an alkoxystyrene derivative, and a monomer of hydroxystyrene or a hydroxystyrene derivative, and a copolymer B polymerized from a monomer of a (meth) aery late derivative and a monomer of hydroxystyrene or a hydroxy styrene derivative, and wherein the copolymers A and B are mixed at a ratio of from about 1:9 to 9:1, 1017. The chemically amplified photoresist composition of claim 16, wherein the copolymer A is represented by the following chemical formula (CF3), the copolymer B is represented by the following chemical formula (CF4), and each copolymer has a weight average molecular weight of from about 5,000 to 50,000: (CF3) R* Rg (CF4) R? O I Rs wherein R4, R5, R7, R9 and RIO are each independently selected from the group comprising a hydrogen atom and a methyl group; R6 is selected from the group comprising alkoxy 1-1 -ethyl, tetrahydropyranyl, t-butyl and t-butoxycarbonyl; 5 R8 is selected from the group comprising a t-butyl group and a tetrahydropyranyl group; 1, m and n are integers, n / (n+l) is from about 0.5 to 0.9, and n / (m+n) is from about 0.5 to 0.9.

18. The chemically amplified photoresist composition of claim 17, wherein R6 is a 11 0 ethoxyethyl group.

19. The chemically amplified photoresist composition of claim 14, wherein the photosensitive polymer mixture comprises a copolymer A polymerized from a monomer of alkoxystyrene or an alkoxystyrene derivative, and a monomer of hydroxystyrene or a hydroxystyrene derivative, and a copolymer B polymerized from a monomer of t1 5 butoxycarbonyloxystyrene or a t-butoxycarbonyloxystyrene derivative, and a monomer of hydroxystyrene or a hydroxystyrene derivative and wherein the copolymers A and B are mixed at a ratio of from about l :9 to 9:1.

20. The chemically amplified photoresist composition of claim 19, w'herein the polymer A is represented by the following chemical formula (CF3), the polymer B is represented by the 20 following chemical formula (CF5), and each polymer has a weight average molecular weight of from about 5,000 to 50,000: (CF3) R4 CH 2 CH 2 Ra OH R 6 Rq R 1 3 (CF5) wherein R4, R5, R9, RIO, Rl 1 and R12 are each independently one selected from the group comprising a hydrogen atom or a methyl group, R6 is one selected from the group comprising alkoxy 1-1-ethyl, atetrahydropyranyl, tbutyl and t-butoxycarbonyl; R13 is a t-butoxycarbonyl group; j, 1 and n are integers; n / (l+n) is from about 0.5 to 0.9, and n / j+n) is from about 0.5 to 0.

9. 1021. The chemically amplified photoresist composition of claim 20, wherein R6 is a 1ethoxyethyl group.

22. The chemically amplified photoresist composition of claim 14, wherein the photosensitive acid generator is mixed at a ratio of from about 1 to 15% by weight based on the total weight ofthe photosensitive polymer mixture. 1523. The chemically amplified photoresist composition of claim 14, wherein the photosensitive acid generator is selected from the group comprising triarylsulfonium salts, diaryliodonium salts and sulfonates.

24. The chemically amplified photoresist composition of claim 14, further comprising an organic base of from about 0.01 to 2.0% by weight based on the total weight of the photosensitive polymer mixture.

25. The chemically amplified photoresist composition of claim 24, wherein the organic base is selected from the group comprising triethylamine, triisobutylamine. tnisooctylamine, diethanolamine, triethanolamine, and N-methyl pyrrolidone.