A process of producing molten metals
Patent Information
- Application Number
- MYPI1998004405
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1997-09-26
- Filing Date
- 1998-09-25
- Publication Date
- 1999-03-26
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Current molten bath-based direct smelting processes face challenges in maintaining a strongly reducing condition in the slag layer to effectively reduce FeO levels, which affects metal production efficiency and quality.
The process involves causing upward movement of splashes, droplets, and streams of molten material from the metal layer to promote strong mixing in the slag layer, maintaining it in a reducing condition and forming a transition zone above the molten bath's quiescent surface.
This approach effectively reduces FeO levels below 8 wt% in the slag layer, enhancing metal production efficiency and quality by maintaining a strongly reducing environment.
Abstract
Description
A molten bath-based direct smelting process for producing metals from metal oxides (including partially reduced metal oxides) is disclosed. The process includes causing upward movement of splashes, droplets, and streams of molten material from a metal layer (15) of the molten bath which:(i) promotes strong mixing of metal in a slag layer (16) of the molten bath so that the slag layer (16) is maintained in a strongly reducing condition leading to FeO levels below 8 wt% based on the total weight of the slag in the slag layer (16); and (ii) extends into a space above a nominal quiescent surface of the molten bath to form a transition zone (23).A PROCESS OF PRODUCING MOLTEN METALSABSTRACTA molten bath-based direct smelting process for producing metals from metal oxides (including partially reduced metal oxides) is disclosed. The process includes causing upward movement of splashes, droplets, and streams of molten material from a metal layer (15) of the molten bath which:
Claims
1. A direct smelting process for producing metal from an iron-containing metalliferous feed material which includes the steps of: (a) forming a molten bath having a metal layer (15) and a slag layer (16) on the metal layer in a metallurgical vessel; (b) injecting iron-containing metalliferous feed material into the metal layer (15) via one or more than one lance / tuyere (11) and smelting the metalliferous material to metal at least predominantly in the metal layer (15); (c) injecting solid carbonaceous material into the metal layer (15) via one or more than one lance / tuyere (11); (d) causing upward movement of splashes, droplets, and streams of molten material from the metal layer (15) of the molten bath which: (i) promotes strong mixing of metal in the slag layer (16) of the molten bath; and (ii) extends into a space above a nominal quiescent surface (19) of the molten bath to form a transition zone (23); and (e) injecting an oxygen-containing gas into the vessel via one or more than one lance / tuyere (13) to post-combustion reaction gases released from the molten bath, whereby the ascending and thereafter descending splashes, droplets and streams of molten material in the transition zone (23) facilitate heat transfer to the molten bath; and wherein the amount of solid carbonaceous material supplied in step (c) is selected to be sufficient to maintain: (i) a concentration of at least 3 wt % dissolved carbon in metal in the molten bath based on the total weight of carbon and metal; PI 98004405 (ii) levels of iron oxide (FeO) below 8 wt % based on the total weight of the slag in the slag layer; and (iii) at least 5 wt % carbon in dust, based on the weight of dust, entrained in off-gas leaving the vessel.
52. The process defined in claim 1 wherein the level of dissolved carbon in metal is greater than 4 wt%.
3. The process defined in claim 1 or claim 2 wherein the concentration of FeO in slag in the slag layer is below 6 wt%. 1θ4. The process defined in claim 3 wherein the FeO concentration is below 5 wt%.
5. The process defined in any one of the preceding claims includes selecting the amount of the solid carbonaceous material injected into the metal layer to be 15 such that dust entrained in off-gas leaving the vessel contains at least some carbon.
6. The process defined in claim 5 wherein the concentration of solid carbon in dust in off-gas from the vessel is in the range of 5 to 90 wt% of the weight of dust in the off-gas which corresponds to a rate of dust generation of 10-50g / Nm3 in the off-gas. PI 980044057. The process defined in any one of the preceding claims includes operating the process at primary postcombustion levels greater than 40%8. The process defined in claim 7 includes operating the process at primary post-combustion levels greater than 50%.
9. The process defined in any one of the preceding claims wherein step (d) includes injecting the metalliferous feed material and the carbonaceous material in a carrier gas through one or more than one lance / tuyere that extend downwardly towards the metal layer and thereby upward movement of splashes, droplets, and streams of molten material into the space above the nominal quiescent surface to form the transition zone.
10. The process defined in any one of claims 1 to 8 wherein step (d) includes injecting the metalliferous feed material and the carbonaceous material via one or more than one tuyere in the bottom of the vessel or in side walls of the vessel that contact the metal layer and thereby causing upward movement of splashes, droplets, and streams of molten material into the space above the nominal quiescent surface to form the transition zone.