Method for producing a magnetic grain oriented steel sheet with low level loss by magnetic reversal and high polarisation

MYPI1998004670A0Inactive Publication Date: 1999-04-15THYSSEN KRUPP STAHL AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1998004670
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Filing Date
1998-10-13
Publication Date
1999-04-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional production methods for grain oriented electric steel sheets require high energy consumption and complex processes due to the need for high slab-preheating temperatures, leading to inhomogeneous temperature gradients and internal stress, which complicates the formation of a pronounced Goss texture and results in high production costs and reduced magnetic properties.

Method used

The method involves casting and solidifying steel strands into thin slabs, which are then heat-soaked and hot-rolled in a multiple-stand line to achieve a hot strip thickness of 0.5 to 3.0 mm, allowing for single-stage cold-rolling and reducing the need for high-temperature furnaces, with the inhibitor phase formed during hot-rolling to control grain growth and achieve a pronounced Goss texture.

Benefits of technology

This approach significantly reduces energy consumption and production time, achieves thinner hot strip settings, and enhances magnetic properties by optimizing the formation of the inhibitor phase, resulting in improved ductility and magnetic characteristics with reduced defect orientation angles.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

THIS INVENTION CONCERNS A METHOD OF PRODUCING GRAIN-ORIENTED ELECTRIC STEEL SHEET BY MELTING A SILICON STEEL AND CASTING THIS MELT CONTINUOUSLY TO FORM A STRAND WITH A THICKNESS OF 25 MM TO 100 MM. AFTER SOLIDIFYING, THE STRAND IS COOLED TO A TEMPERATURE ABOVE 700?C AND DIVIDED INTO THIN SLABS. THEN THE THIN SLABS PASS THROUGH AN IN-LINE HOLDING FURNACE, WHERE THEY ARE HEATED TO A TEMPERATURE OF < 1170?C AND ROLLED CONTINUOUSLY IN A MULTIPLE-STAGE HOT-ROLLING STAND TO FORM HOT-ROLLED STEEL STRIPWITH A THICKNESS OF < 3.0 MM. THE FIRST FORMING PASS IS PERFORMED AT A TEMPERATURE OF UP TO 1150?C IN THE ROLLING STOCK. AT LEAST A 20% REDUCTION IN THICKNESS IS ACHIEVED. THE HOT-ROLLED STRIP IS COLD ROLLED TO A FINAL THICKNESS IN THE RANGE OF 0.15 TO 0.50 MM IN ONE OR MORE STAGES WITH RECRYSTALLIZING INTERMEDIATE ANNEALING. THEN THE COLD-ROLLED STRIP IS RECYRSTALLIZATION AND DECARBURIZATION ANNEALED, PROVIDED WITH AN ANNEALING SEPARATOR CONTAINING MOSTLY MGO AND THEN SUBJECTED TO THE FINAL ANNEALING TO ACHIEVE A GOSS ORIENTATION. THEN THE STRIP IS COATED WITH ELECTRIC INSULATION AND SUBJECTED TO STRESS-FREE ANNEALING.
Need to check novelty before this filing date? Find Prior Art

Description

DESCRIPTIONMETHOD FOR PRODUCING A MAGNETIC GRAIN ORIENTED STEEL SHEET WITH LOW LEVEL LOSS BY MAGNETIC REVERSAL AND HIGHPOLARISATIONThe invention relates to a method for producing a grain oriented electric sheet with low level loss by magnetic reversal and high polarisationIn the conventional production of grain oriented electric sheet, steels comprising 2.5 to 4.0 % Si, 0.010 to 0.100 %C, up to 0.150 % Mn, up to 0.065 % Al and up to 0.0150 % N, as well as in each case optionally 0.010 to 0.3 % Cu, up to 0.060 % S, up to 0.100 % P, in each case up to 0.2 % As, Sn, Sb, Te, and Bi, with the remainder being iron and unavoidable impurities, are melted and cast. The solidified strands with a thickness of 25 to 100 mm are divided into thin slabs, without cooling to below 700 °C, and are homogenously heat-soaked to a temperature of up to 1170 °C in an in-line compensating furnace, with a dwell time of max. 60 min. These homogenously heat-soaked thin slabs are then continuously rolled in a multiple-stand hot-rolling line to form hot strip with a thickness of 0.5 to 3.0 mm, and are subsequently coiled. Finally, the hot strip is optionally annealed. The hot strip treated in this way is cold-rolled, in one or several roll passes, to a finished strip thickness of 0.15 to 0.50 mm. The cold strip is subjected to recrystallising and decarbonising annealing. Subsequently, after application of an annealing separator which predominantly contains MgO, said cold strip is subjected to secondary-recrystallising high-temperature annealing, which results in a very pronounced Goss texture.PI 98004670Finally, in a final annealing process, said cold strip is insulated and freed of any residual internal stress.Grain oriented electric sheets are used in particular in output transformers, for carrying the magnetic flux. This requires the lowest possible losses by magnetic reversal and at the same time the highest possible polarisation values. For this purpose a very pronounced Goss texture is purposefully generated in grain oriented electric sheets. In this way very good magnetic properties are achieved along the direction of rolling, which is the preferred magnetic direction.For more than 20 years, production of flat steel products has started with the continuous casting of meltings by way of the continuous casting technique. In this process, the melting is poured into a die from which it issues as a solidifying strand, approx. 100 to 300 mm in thickness. Subsequently, the strand is mostly brought in a curve from the vertical to the horizontal plane, while at the same time being cooled. After leaving the continuous casting plant, the strand is divided into individual slabs. Usually, simple soft steel slabs are stored in a slab storage area where they cool down to ambient temperature. However, slabs for grain oriented electric sheet, which are alloyed comprising 2.5 to 4.0 % Si, must be stored at higher temperatures. This is because they are particularly susceptible to cracking or fissuring during reheating prior to hot-strip rolling if they have previously been cooled down to temperatures which are too low. In this respect, the large slab thickness obtained in the conventional continuous casting technique has been shown to be particularly disadvantageous because it causes very considerable and inhomogeneous temperature gradients during reheating of the slabs, which gradientsPI 98004670 cause very considerable internal stress. For this reason, slabs destined for the production of grain oriented electric sheet usually have to be stored in heated holding furnaces at temperatures of, for example, 100 to 500 °C. Such an approach is associated with the disadvantage of increased energy consumption and complex and expensive processing.Subsequently, the slabs produced in the conventional continuous casting process are placed in a pusher-type furnace, a walking-beam annealing furnace or in a unit which has an equivalent effect, where said slab is heated to a temperature which is sufficiently high to achieve good hot plasticity. Thereafter, hot-rolling usually takes place in two partial steps: firstly the slabs, which are 100 to 300 mm in thickness, are rough-rolled to a thickness of approx. 30 to 60 mm. Such rough rolling often takes place in reversing stands. In a multiple-stand finishing roll line, the roughed slabs are then continuously rolled to hot strip, 2.0 to 6.0 mm in thickness.Grain oriented electric sheet produced according to conventional processes has a peculiar characteristic in that heating the slabs to a temperature of up to 1400 °C is absolutely essential in order to dissolve foreign-phase particles in the slab, so that said foreign-phase particles can undergo fine-disperse precipitation during subsequent hot-rolling (US 2 599 340). In a known process for example, these particles are predominantly Mn sulphides or Mn selenides (J.E. May and D. Turnbull: Trans. ΑΙΜΕ, 212 (1958), 769). In another process, Al nitrides are produced in addition (US 3 159 511; US 3 287 183). In a further process, MnSe and MnSb are produced (DE 23 51 141 A). Also known are other nitrides such as VN, (Al, Si)N, ...(DE 19 20 666 A, EP 0 219 611) and sulphides such as Cu2S, TiS,PI 98004670CrS,...(EP 0 619 376 Al, DE 23 48 249 A). Generally speaking, these particles are intended to block the movement of grain boundaries during the subsequent productions steps right up to before secondary recrystallisation, thus inhibiting normal grain growth during various annealing treatments. For this reason they are referred to as grain growth inhibitors. From a distribution of particles of various sizes, it is only the particles smaller than approx. 100 nm, which can sufficiently inhibit movement of the grain boundaries, and which can thus act as inhibitors. During high-temperature annealing, the inhibitors control the process of secondary recrystallisation which leads to the formation of the desired, very pronounced Goss texture.After casting and solidification, precipitations are usually so coarse in conventional continuous casting that there are practically no particles of a size below 100 nm. This is why the coarse particles have to be dissolved during slab preheating. In the case of Mn sulphides, this requires annealing temperatures of up to approx. 1400 °C. During subsequent hot-rolling with suitably set parameters (pass sequences and deformation temperatures in the various stands, cooling) the particles are precipitated again in the desired way.Heating of the slabs to the high temperature required for dissolving the particles which act as grain growth inhibitors, can either be carried out directly in one furnace, or in two furnaces in sequence. In the latter case, the slabs are for example heated to 1250 °C in the first furnace, and subsequently to a temperature of up to 1400 °C in the second furnace. Although this makes the process sequence more complicated and more expensive, it has been shown to be advantageous for the magnetic characteristics ofPI 98004670 the finished product, to carry out a first hot forming pass of the slab (pre-rolling) between these two stages, for homogenising and refining their microstructure (EP 0 193 373 Bl) .The high slab-preheating temperature necessary to form the inhibitor phase, makes the production process for hot strip destined for grain oriented electric sheet more difficult and more expensive, as it requires investment in special and expensive high-temperature furnaces. This requirement is due to the fact that the liquid scale which occurs with siliconsteel slabs at temperatures above 1350 °C, damages the bottom of the furnace, which in turn is connected to damage to the bottom of the slabs, leading to loss of yield. The optional intermediate process of pre-rolling also makes production more expensive and displaces capacity which could otherwise be used for the production of other flat steel products .MnS or MnSe particles have only limited effect in relation to grain growth inhibition. For the desired Goss selection process to be able to take place at the right moment during secondary recrystallisation, this effect must only be countered by a correspondingly matching driving force for grain size increase. This means that the degree of deformation during the last cold-rolling stage to final thickness, must not be too high. The most favourable thickness reduction during this cold-rolling stage of the Si steel inhibited by MnS or MnSe, is around 40 to 60 %. Since, with the conventional hot-rolling technique, it is very difficult to reduce the thickness of the hot strip to below 2.0 mm without incurring losses in quality and yield, the optimal degree of deformation during cold-rolling to final thickness must be realised in several stages, with aPI 98004670 recrystallising intermediate annealing step taking place between said stages. The grain oriented electric sheet produced in this expensive way has defect orientation angles of up to approx. 10 ° in relation to the exact Goss position.The so-called Hi-B process (US 3 159 511, US 3 287 183) , in which in addition to MnS, AIN particles are used as a further inhibitor phase, is a further development of the above-mentioned process. This further development results in still lower defect orientation and thus improved magnetic properties. The Hi-B process as well as the first mentioned process are associated with the disadvantage in that high slab-heating temperatures of e.g. 1400 °C are required in order to dissolve the MnS particles. After rolling the hot strip, the AIN is not yet present in suitably finely dispersed particle distribution; it attains this only after precipitation annealing of the hot strip with subsequent quenching. Thus the internal quality of the hot strip, in relation to its chemical composition, the formation of its grain structure and the morphology of its secondary-phase fractions, must be such that it has the ability to precipitate AIN inhibitor phase particles. Overall, grain growth inhibition is enhanced by the AIN particles.This makes it possible in an advantageous way, to carry out a cold-rolling process which is limited to a single-stage, with an increased degree of deformation. The energy which is increased in this way, said energy being stored in the matrix, is now in equilibrium in relation to a stronger inhibition. In this way, the selection during secondary recrystallisation is improved. This results in a more pronounced Goss texture (the defect orientation angle in relation to the precise Goss position is only 3 to 5 °), andPI 98004670 thus in improved magnetic properties.In order to overcome the disadvantages resulting from the high slab-preheating temperature, of the conventional processes described above, in the last few years several new production processes for grain oriented electric sheet have been developed, wherein the required slab temperature was reduced to values below 1330 °C. From these low-heating processes, two have been selected for description below. These processes have been introduced to industrial practice and form part of the state of the art.The method according to EP 0 219 611 operates entirely without any sulphidic inhibitors. It is thus possible to reduce the S content down to trace-amount level. With values of below 1200 °C, the slab-preheating temperature is particularly low. Formation of a sufficiently effective inhibitor phase, which is already complete in the hot strip, is thus not possible. Nor is such a hot strip, produced in the conventional continuous casting technique, able to form a respective inhibitor phase by way of a precipitation annealing process. The inhibitor AlN is therefore formed by nitriding the strip which has been cold-rolled to finished strip thickness, prior to high-temperature annealing. EP 0 321 695 Bl states several methods by which such a nitriding process can be achieved.In another method (EP 0 619 376 Al) Cu sulphides are used as inhibitors. They have a significantly lower solubility temperature and faster solubility kinetics than AlN and MnS. While the inhibitor formation during hot-rolling does not occur in the correct way, the hot strip produced according to this method nevertheless has the ability of precipitating Cu sulphide inhibitor particles. They are produced during aPI 98004670 precipitation annealing treatment of the hot-rolled strip.The conventional production of hot strip made from continuous cast slabs, as described above, requires considerable effort from the point of view of production technology, and is also very time consuming and costly. For this reason, many steel producers are presently developing casting methods producing near-final dimensions. These methods are aiming to achieve hot strip thicknesses below 6 mm or even finished strip thicknesses right down to 0.01 mm (EP 0 417 318 Bl). Commercial processes have been realised for certain types of special or high-grade steels and for amorphous materials. So far, large-scale production of grain oriented electric sheet comprising 2.5 to 4 % Si, by way of strip casting methods, has not been achieved. One of the main problems is the targeted achievement of suitable microstructures and precipitation structures, during solidification at such low thicknesses and during subsequent cooling, which microstructures and precipitation structures, after further cold-forming and heat treatment, would allow the formation of a pronounced Goss texture in the finished product so that said finished product is competitive, from the point of view of its magnetic properties, with grain oriented electric sheet produced by way of conventional continuous casting techniques (EP 0 390 160 Bl, EP 0 540 405 Bl) .The production of hot strip by way of casting thin slabs and direct hot-rolling of said thin slabs is already known from the state of the art (e.g. EP 0 286 862 Bl).However, the problem of using this technique in the production of grain oriented electric sheet has not yet been solved. This application is associated with the particular difficulty of firstly producing a faultless product, fromPI 98004670 the point of view of its mechanical and technological properties, and secondly of forming the grain growth inhibitor phase in the correct way, so that the finished product will have good magnetic properties.From the Japanese published application no. 56-158816, a method is known for producing grain oriented electric sheet comprising 2.5 to 4 % Si by way of continuous casting of thin slabs with a thickness of 3 to 80 mm with subsequent hot-rolling to 1.5 to 3.5 mm, using MnS and MnSe as the principal inhibitors. In this method, the increased thickness of the hot strip is associated with the disadvantage in that the standard final thicknesses of below 0.35 mm, which are customary in the trade or commerce of grain oriented electric sheet, can only be produced by way of cold-rolling rates above 76 % in the case of single-stage cold-rolling; or by way of conventional multistage coldrolling with intermediate annealing. This process is associated with the disadvantage in that the high degree of cold forming is not matched to the relatively weak inhibition by MnS and MnSe. This leads to unstable and unsatisfactory magnetic properties in the finished product. Alternatively, an elaborate and expensive multi-stage coldrolling process with intermediate annealing steps has to be accepted. Nor is there any decoupling of the casting speed from the throughput speed at which the product passes through the compensating furnace. This results in the disadvantage of reduced flexibility in the utilisation of the compensating furnace for targeted precipitation of sulphidic inhibitors.It is thus the object of the invention to overcome disadvantages in the conventional production approaches while using the economic advantages of casting thin slabsPI 98004670 ίο also in the case of grain oriented electric sheet.This object is met by the method according to claim 1, by optimising the production steps of casting, solidification and hot-rolling. The selection of various mechanisms to form the inhibitor phase and matching subsequent process steps is connected to the above.In a way similar to the procedure applied in the state of the art, in the method according to the invention, a melting is continuously cast into a vertical die, at the end of which the melting solidifies and the strand formed in this way is transferred, in an arc shape, to the horizontal plane while at the same time being cooled. The thickness of this strand is only 25 to 100 mm, preferably 40 to 70 mm. The strand is not completely cooled; its temperature does not fall below 700 °C. This hot strand is divided into thin slabs which are directly fed through a compensating furnace arranged in line, in which compensating furnace said thin slabs remain for at most 60 minutes, preferably for up to 30 minutes. During this passage through the compensating furnace, the thin slabs are homogenously heat soaked, reaching a relatively low temperature of at most 1170 °C. Immediately thereafter, the thin slabs are conveyed through a multiple-stand hot-rolling line arranged in line, where they are continuously hot-rolled to a hot strip thickness of 0.5 to 3.0 mm. Ideally, the hot-strip thickness is selected such that the subsequent cold-rolling process is carried out only in a single stage. The degree of deformation during this cold-rolling process depends on the respective inhibitor effect which can be set in various ways.One of the advantages of the method according to the invention is that it uses a large part of the heat generatedPI 98004670 during the casting process. Consequently, and contrary to the situation required in the state of the art, there is no need to keep slabs destined for grain oriented electric sheet hot in heated furnaces and to reheat the slabs to high temperatures in a pusher-type furnace or a walking-beam annealing furnace. The annealing treatment which takes place instead, serves to set a defined homogeneous temperature across the entire thickness of the thin slab. Due to their thin shape, thin slabs require significantly less time to achieve this than is the case with conventional slabs, which measure 100 to 300 mm in thickness. Compared to the situation in the state of the art, considerable energy savings and time savings for reheating are achieved.There is a further advantage in that, due to the low thickness of the slabs, pre-rolling, which accompanies the slab heating process, to achieve a homogeneous microstructure, as well as rough rolling at the start of the hot-rolling process, is no longer applies. This results in significant shortening of the production path, in direct cost savings, and in a capacity increase in the hot-strip line, which capacity increase can be used in the production of other flat steel products.The above-mentioned shortening of the production path partly carries over to the subsequent processing stages. For, in the method described, in addition, hot strip settings down to 0.5 mm are possible which are thinner than is the case in the conventional process. This means that multi-stage coldrolling, which has sometimes been undertaken in the conventional method, is no longer absolutely necessary; instead, it is possible to limit cold-rolling to a single stage .PI 98004670So as to utilise the advantages according to the invention, which advantages have been described above, from the casting-rolling process for the production of grain oriented electric sheet, the hot-rolling parameters must be selected such that the material remains sufficiently ductile. Tests have shown that in the case of raw material for grain oriented electric sheet, ductility reaches a maximum if, after solidification, the strand is cooled to approx. 800 °C, subsequently dwells for a relatively short time at compensation temperature, e.g. 1150 °C, in which process it is homogeneously heat soaked. According to an advantageous embodiment of the invention, ideal hot-rollability of such a material is achieved if the first forming pass takes place at a temperature below 1150 °C and at a degree of deformation of at least 20 %, and if the rolling stock, from an intermediate thickness of 40 to 8 mm, is cooled to rolling temperatures below 1000 °C by means of high-pressure cooling devices in the intermediate mill stand within at most two subsequent forming passes. In this way, rolling the rolling stock in the temperature range around 1000 °C, which is critical to ductility, can particularly safely be avoided.Table 1 shows the chemical composition of four steels which were tested from the point of view of their suitability for hot-rolling according to the invention.Table 1Chemical composition in per cent by weight (%w / w)Steel c Si Mn S Al N Cu Sn A 0.076 3.25 0.077 0.025 0.025 0.008 0.07 0.12 B 0.060 3.15 0.077 0.025 0.027 0.008 0.07 0.08 c 0.040 3.15 0.085 0.027 0.022 0.008 0.08 0.07PI 98004670D 0.030 3.15 0.063 0.020 <0.003 <0.005 - -The tests were carried out on 20 mm round test bars whose centre regions were temporarily melted and subsequently cooled such that this corresponds to a 60 mm thin slab at a casting speed (vg) of 2.8 m / min. or of 4.5 m / min. Cooling ceased at 800 °C. Subsequently, after a cycle in the continuous furnace, the specimens were heated to temperatures (Tw) and held at said temperatures for various periods (tw). Finally, the specimens were subjected to a tensile test at a temperature Tw.Table 2 shows the results of the tests.Table 2Hot tensile tests for determining the ductility of the steels in the 'as-cast' conditionSteel A Steel B Steel C Steel D V3 Tw tw Z Z Z Z (m / min) (°C) (min) (%) (%) (%) (%) 2.8 1130 0 49 73 72 >95 2.8 1130 50 33 45 60 >95 2.8 1050 12 45 52 67 >95 2.8 1000 17 24 47 59 >95 >95 4.5 1130 0 40 58 71 4.5 1130 50 32 48 56 >95 4.5 1050 12 40 50 47 >95 4.5 1000 17 23 50 45 >95Vg= Casting speed; t„ = Holding time at Tw;Tw= Heating temperature;Z = Reduction of area when breakingPI 98004670The reduction of area when breaking is the significant parameter relating to ductility. The data shows that, depending on their chemical composition, the steels react with different sensitivity to the respective load cycles. Steel D shows the smallest, steel A shows the largest loss of reduction of area when breaking, or of ductility.The effectiveness of the measures according to the invention are most impressive in steel A. At both casting speeds the heating temperatures of 1130 °C and 1050 °C result in comparatively good reductions of area when breaking, while a heating temperature of 1000 °C results in reduced ductility. The latter also applies in the case of prolonging the holding time to heating temperature.The heating temperature range around 1000 °C has been tested for steel B in the way described above. Table 3 shows the result.Table 3Reduction of area when breaking(Z) of steel B as a function of the heating temperature (Tw)Tw (°C) 1100 1050 1000 950 900 850 Z (%) 65 50 45 55 60 65(vg= 2.8 m / min; tw= 20 min)The values relating to the reduction of area when breaking, as shown in Table 3, show that the ductility of the steel decreases at temperatures ranging between 1100 °C and 1000 °C, while it increases again at temperatures below 1000 °C.Advantageous application of the casting-rolling method,PI 98004670 described above, for producing grain oriented electric sheet, further requires that the inhibitor phase is formed in a suitable way. To this effect, three principal options are shown here, namely in claims 3, 4 and 5.The option described in claim 3 is based on the recognition that solidification after casting can be carried out quite quickly when compared to the continuous casting technique known from the state of the art. For example in a strand with a thickness of only 65 mm, the heat can be carried off significantly more quickly than is the case in a strand with a thickness of 250 mm. While a conventional thick slab therefore comprises only very coarse sulphides, in particular MnS particles, which cannot act as inhibitors, the fast cooling of a significantly thinner strand provides the option of having inhibitors present directly after hotrolling, provided the casting speed is selected properly.During homogeneous heat soaking in the compensating furnace, complete precipitation of the sulphidic particles can take place. The fastest possible passage through this furnace must be aimed for, to prevent excessive growth in particle size. Excessive growth would weaken the inhibitor function. Accordingly, a hot strip produced in this way already comprises the completed inhibitor phase.To achieve the highest possible fine-disperse precipitation of the sulphidic inhibitor phase particles, the Mn content must range from 0.050 to 0.100 % and the S content from 0.015 to 0.035 %. Too low a content of either of these elements prevents the formation of sufficient substance quantity for the inhibitors. Too high a content results in the precipitation of particles which are too coarse. For this reason, the contents of Mn and S should be within thePI 98004670 range of 0.05 to 0.10 % Mn, and 0.015 to 0.035 % S.With this method it is not necessary to carry out multistage cold-rolling with intermediate annealing. Instead, the thickness of the hot strip can be set sufficiently low to allow further processing with only one cold forming stage.To achieve this, the degree of deformation during coldrolling should be within the range of 45 to 75 %.The fact that there is no longer a need to carry out multistage cold-rolling, constitutes a significant advantage of the method. Nevertheless, in certain situations it may be advantageous, from the point of view of logistics, to produce only hot strip of a particular pre-specified thickness, and to match the degree of deformation during cold-rolling to the particular application by multi-stage cold-rolling.The method described in claim 3 thus also permits multistage cold-rolling with intermediate annealing.Claim 4 discloses an advantageous annealing process to be carried out at 800 to 1100 °C. As an alternative to this, the coiling temperature can be set to less than 900 °C. Such annealing enhances the grain structure in the hot strip. In particular, this leads to enlargement of the regions of the microstructure which are close to the surface, and which are important for the subsequent processing steps. No additional inhibitors are formed in the heat treatments described above .Claim 5 describes a method in which the hot strip does not yet contain the grain growth inhibitors in their final shape. But rather, the structure of the hot strip is suchPI 98004670 that during a process of compensation annealing, corresponding inhibitor particles are formed in said hot strip. In particular, Cu sulphide and Al nitride can be considered as inhibitors. This approach provides the advantage that the production of hot strip (casting, solidification, compensation annealing, hot-rolling) does not in addition also have to be optimised for optimal formation of the inhibitor phase. This opens up new degrees of freedom. However, the cooling rate of the cast strand must be selected to be large enough for the grain structure of the thin slab not to become too coarse. To this purpose it has also been shown that it is sensible to select as brief a dwell time in the compensating furnace as possible. Precipitation of the inhibitor particles takes place during precipitation annealing of the hot strip at 950 to 1150 °C which is completed with a particularly fast cooling process. During annealing treatment, the elements forming inhibitor phases are brought to solution so that during the subsequent very rapid cooling, preferably using splash water, finedisperse precipitation of the inhibitor phase occurs at > 20 K / s. This method is possible because Cu sulphides have a significantly lower solubility temperature and faster reaction kinetics than is the case, for example, with MnS. The same applies to AIN in the austenite. For this reason, the application of C-contents which are higher than those in claim 3 is recommended. The C-content must be sufficient for at least some conversion of austenite to take place.However, if the C-content exceeds 0.10 %, problems in connection with the ability to decarburise may occur.At 70 to 90 %, the degree of deformation during cold-rolling can be set to be considerably higher than is the case in the method described in claim 3. The increased energy and thus the driving force for secondary grain growth, introduced inPI 98004670 this way, is balanced in the method described in claim 5 by a correspondingly higher inhibitor effect. Similar to the situation in the HiB process, this results in better texture selection and thus in a more pronounced Goss position in the finished strip, and ultimately in better magnetic properties when compared to a material produced according to claim 3.The method according to claim 6 represents a process in which exclusively AIN is used as an inhibitor. This method is advantageous in that practically it completely avoids Cu and S in the melting, thus facilitating hot-rolling and reducing the brittleness of the material. Similar to the situation according to claim 3, the fast cooling rate of the cast strand results in partial prevention of precipitation of the inhibitor-forming elements (Al and N) present in the melting. Any particles which are nevertheless precipitated, are only small in size. As is the case in claim 3, complete precipitation takes place during homogeneous heat soaking in the compensating furnace.Furthermore, this hot strip may have the ability to precipitate further AlN particles which can act as inhibitors, if an adequate C-content ensures the formation of sufficient austenite during precipitation annealing of the hot strip. The overall inhibitor effect set in such a material thus depends on the cooling rate of the strand, i.e. on the number of effective inhibitors which were able to form spontaneously at the beginning. Furthermore, it depends on the number of inhibitors which were additionally produced during precipitation of the hot strip. This depends to a very significant degree on the C-content. Depending on the extent of this total inhibition effect, different degrees of deformation during cold-rolling need to be set.PI 98004670The addition of up to 0.10 % phosphorus strongly promotes a fine solidification structure, without causing negative effects, for example embrittlement in the material.Restricting the superheating temperature during casting, to at most 25 K above the liquidus temperature, as provided for according to one embodiment of the invention, essentially aims to achieve the same objective as does the previously explained addition of phosphorus, namely, to bring about as homogeneous and fine-grained a solidification structure as possible. If the melting is cast at a temperature which is only just above the liquidus temperature of the respective alloy, then a substantially globular solidification structure results, with dendritic growth being restricted. Generally speaking, it is always important, when producing grain oriented electric sheet, to set as fine a solidification structure as possible so that not only texture development but also microstructure development can take place as homogeneously as possible in the volume of the slab or thin slab. In addition, as fine a microstructure as possible particularly promotes the desired fine-disperse precipitation of the inhibitor phase.One option for reinforcing the total inhibition effect consists of forming, by nitriding treatment, additional AIN particles in the matrix of the strip which is cold-rolled to finished strip thickness, with a sufficiently large content of said AlN particles being below the size of 100 nm. The additional AIN particles formed in this way must, in any case, be formed in the matrix prior to commencement of secondary recrystallisation so that they can still influence secondary recrystallisation in an advantageous way. This nitriding treatment can take place in the heating phase at the beginning of high-temperature annealing, and can forPI 98004670 example be caused by an annealing atmosphere rich in nitrogen. But it can also be brought about by agents added to the annealing separator which predominantly contains MgO, with said additives comprising substances which at the beginning of high-temperature annealing release nitrogen which can then diffuse into the matrix. In this context, a very effective method for nitriding consists of carrying out a respective treatment stage at the end of annealing in a decarburising medium, wherein nitrogen from the annealing gas can diffuse into the strip.Elements, such as As, Sn, Sb, Te and Bi, which segregate at the grain boundaries, at a quantity of 0.2 % each, have a favourable influence on stabilising secondary recrystallisation and on bringing about a more pronounced Goss texture.

Claims

CLAIMSProcedure for generating grain-oriented electric sheet, in which a steel with (in % w / w)2.5 to 4.0 % Si 0.01 to 0.10 % c, up to 0.30 % Cu up to 0.15 % Mn up to 0.060 % s, up to 0.065 % Al up to 0.015 % N, up to 0.10 % p,and, if necessary, up to 0.2 % w / w of one or more elements As, Sn, Sb, Te and Si, with Fe and unavoidable contaminants as the residue, is melted, in which this melt is continuously cast into a bar at a thickness of 25 to 100 mm, which is cooled while solidifying to a temperature above 700 °C, and divided into thin slabs immediately thereafter, in which these thin slabs then run through a serial compensating furnace, in which they are heated to a temperature < 1170 °C, wherein they remain at this temperature for at most 60 min., in which the thin slabs are then continuously rolled into hot strip with a thickness of 0.5 - 3.0 mm in a serial, multiple-stand hot-rolling line, wherein the first forming pass takes place at a temperature inPI 98004670 the rolling stock of < 1150 °C, and at a deformation degree of at least 20 %, in which the hot strip is subsequently coiled, in which this hot strip is then cold-rolled in one or more stages via recrystallizing intermediate annealing to a final thickness ranging from 0.15 to 0.50 mm, in which the cold strip is then subjected to recrystallizing and decarbonizing annealing, provided with an annealing separator containing primarily MgO, and then undergoes final annealing to produce a Goss-texture, and- in which the finally annealed cold strip is coated with an electric insulation and is stress-free annealed.Procedure according to claim 1, characterized by the fact that rolling stock is cooled to temperatures of under 1000 °C during hot-rolling at an intermediate thickness of under 40 mm and up to an intermediate thickness exceeding 8 mm via high-pressure cooling devices within at most two consecutive forming passes, and rolled to final thickness.PI 98004670Procedure according to claim 1 or 2, characterized by the fact that a steel melt having the composition in claim 1, but with carbon, manganese and sulfur in the following content ranges:0.01 to 0.050 % C,o. 05 to o.io % Μη,0.015 to 0.035 % S, is cast into thin slabs, and hot-rolled to a final thickness of 0.7 to 1.3 mm after compensation annealing, and that the strip is cold-rolled in the last cold forming stage with a thickness reduction ranging from 45 % to 75 %.Procedure according to claim 3, characterized by the fact that the hot strip is annealed at 800 to 1100 °C, or that it is coiled at a temperature of less than or equal to 900 °C.Procedure according to claim 1 or 2, characterized by the fact that hot strip consisting of a melt with (in % w / w) :5 to 4.0 % Si, 03 to 0.1 % c, 05 to 0.10 % Mn, 015 to 0.035 % s, 05 to 0.03 % Cu, 015 to 0.065 % Al, 005 to 0.015 % N, up to 0.10 % P,and, if necessary, an additional 0.2 % w / w of one or more elements As, Sn, Sb, Te and Bi, with iron and unavoidable impurities as the residue, is cast into thin slabs, and hot-rolled to a thickness of 0.5 - 3.0 mm, and subjected to precipitation annealing at 950 to 1150 °C for 30 to 300 s, followed by accelerated cooling with a cooling rate of more than 20 K / s,PI 98004670 wherein this annealing is performed before the last stage of cold forming with a thickness reduction of 70 % to 90 %.Procedure according to claim 1 or 2, characterized by the fact that a melt consisting of a steel according toclaim 1, but with max. 0.010 % s, max. 0.010 % Cu, at least 0.015 % Al, at least 0.005 % N, is cast into thin slabs and hot-rolled to a of 0.5 - 3.0 mm, and that the hot strip isprecipitation annealed at 1000 °C to 1150 °C for 30 to 300 s, followed by accelerated cooling of more than 20 K / s, after which a thickness reduction of 45 % to 90 % is performed in the last cold forming stage.Procedure according to one of claims 1 to 6, characterized by the fact that the steel melt is cast off at an superheating temperature of at most 25 K above the liquidus temperature.Procedure according to one of claims 5 or 6, characterized by the fact that additional AlN particles with a maximal grain size of 100 nm are formed by nitrating the strip cold-rolled to finished strip thickness.