Fine wire of gold alloy, method for manufacture thereof and use thereof

MYPI1998005384A0Inactive Publication Date: 1999-05-29HERAEUS MATERIALS TECHNOLOGY GMBH & CO KG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1998005384
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1997-11-29
Filing Date
1998-11-27
Publication Date
1999-05-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing gold alloy bonding wires for semiconductor devices face challenges in achieving a high strength-to-elongation ratio while maintaining electrical conductivity similar to pure gold, and existing manufacturing methods are not cost-effective or efficient for producing wires with uniform quality.

Method used

A gold alloy fine wire with 0.5 to 0.9 wt% copper and 0.05 to 0.95 wt% platinum, or 0.0001 to 0.1 wt% of alkaline earth or rare earth metals, with the remainder being gold, is manufactured through continuous casting and annealing, resulting in a wire with a diameter of 10 to 200 micrometers, offering improved mechanical strength and electrical conductivity.

Benefits of technology

The solution provides a fine wire with a superior strength-to-elongation ratio and high electrical conductivity, suitable for wire bonding and flip-chip technology, while the continuous manufacturing method ensures uniform quality and cost-effectiveness.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

FINE WIRES OF A GOLD ALLOY CONTAINING 0.5 TO 0.9 W% OF COPPER AND SMALL PROPORTIONS OF PLATINUM OR AT LEAST ONE ELEMENT FROM THE GROUP OF ALKALINE EARTH METAAL AND RARE EARTH METALS ARE CHARACTERIZED BY A SPECIFIC ELECTRICAL RESISTANCE SIMILAR TO THAT OF GOLD AND A FAVORABLE STRENGTH-TO-ELONGATION RATIO. THEY ARE SUITABLE BOTH FOR WIRE BONDING AND FOR MAKING THE BALL BUMPS OF FLIP CHIPS.
Need to check novelty before this filing date? Find Prior Art

Description

Fine wire of gold alloy, method for manufacture thereof and use thereofBackground of the InventionThe invention relates to a fine wire of a gold alloy for bonding semiconductor devices, a method for manufacture of the fine wire and the use thereof.q Wires suitable for bonding semiconductor devices, also known as bonding wires, must have good electrical characteristics and good mechanical strength values. The diameter of the wires is selected to match the application and can range from about 10 to 200 micrometers, usually about 20 to 60 micrometers.Bonding wires are often made of high-purity gold or of gold alloys. The latter have the advantage of higher strength and, provided they contain only a small quantity of alloy-forming constituents, electrical conductivity similar to that of gold.For example, DE 16 08 161 C teaches that an alloy of gold andIB o.ooi to 0.1% of one or more rare earth metals, especially in the form of cerium mischmetal or yttrium, can be used to make lead wires in integrated circuits. This gold alloy containing small quantities of rare earth metals or yttrium has much better strength and elongation behavior at temperatures up to 500°C2q without experiencing substantial influence on other characteristics of the gold such as hardness, chemical stability or electrical resistance.Gold-rare earth metal alloys for bonding wires are also described in DE 32 37 385 A (US 4 885 135), DE 39 36 281 A (US 4 938 923),JP 5-179375 A, JP 5-179376 A, JP 6-112258 A, EP 0 743 679 A andEP 0 761 831 A.DE 32 37 385 A relates to a gold-alloy fine wire with high tensile strength comprising a gold alloy containing 0.0003 to 0.01 wt% of rare earth metal, especially cerium, and also germanium, beryllium and / or calcium as required.DE 39 36 281 A describes a gold wire, for connecting to a semiconductor device,of high-purity gold alloyed with small quantities of lanthanum, beryllium, calcium and platinum group elements, especially platinum and / or palladium.JP 5-179375 A and JP 5-179376 A relate to gold-alloy fine wires for bonding which comprise high-purity gold and 0.0003 to 0.005 wt% of aluminum or gallium, 0.0003 to 0.003 wt% of calcium and 0.0003 to 0.003 wt% of yttrium, lanthanum, cerium, neodymium, dysprosium and / or beryllium.The bonding wire known from JP 6-112258 A, cited in Chemical Abstracts Vol. 121, 89287m, comprises a gold alloy containing 1 to 30% of platinum and 0.0001 to 0.05% of scandium, yttrium and / or rare earth metal and also 0.0001 to 0.05% of beryllium,-2' calcium, germanium, nickel, iron, cobalt and / or silver as required.A bonding wire of a platinum-containing gold-rare earth metal alloy is also proposed in EP 0 743 679 A. The alloy comprises gold and small quantities of platinum (0.0001 to 0.005 wt%) , silver, magnesium and europium, and can also contain, for example, cerium in a quantity of 0.0001 to 0.02 wt%.A fine wire of a gold-rare earth metal alloy containing platinum and / or palladium is described in EP 0 761 831 A. The alloy comprises 0.1 to 2.2 wt% of platinum and / or palladium, 0.0001 to 0.005 wt% of beryllium, germanium, calcium, lanthanum, yttrium and / or europium, the remainder being gold. The wire is made by melting the alloy-forming elements in a crucible, progressively cooling the molten alloy contained in the crucible from bottom to top to obtain ingots, and thereafter rolling, drawing and annealing. It has an elongation of 3 to 8% and a Young's modulus of 6800 to 9000 kgf / mm2.EP 0 288 776 A2 relates to the bonding to metal coatings of aluminum which have been doped with copper to improve hardness2q and strength and for which the standard gold bonding wires doped with beryllium to reduce the hardness are less well suited. To make connections to bonding pads comprising copper-doped-3aluminum, there is therefore proposed a bonding wire comprising an alloy of gold and 0.01 to 1 wt% of copper with hardness adapted to the doped aluminum.A copper-containing bonding wire is also known from DE 39 90 432 O C2 (= US 5 491 034 A). The bonding wire is used to connect electrodes of a semiconductor device with external leads, and it comprises a gold alloy with at least 1 and less than 5 wt% of copper. In addition, the bonding wire can contain 0.0003 to 0.01 wt% of calcium, germanium, beryllium, lanthanum and / or indium and at least 1 wt% and at most 5 wt% of platinum. The bonding wire is made by melting the gold alloy in a vacuum melting furnace, wire-drawing and then heat treatment (annealing) at 200 to 600°C. The heat treatment is standard, and has the purpose of improving the deformability or elongation, which becomes poor during the drawing process. Since the improvement of deformability is accompanied by a reduction of strength, the strength-influencing alloy-forming constituents must be selected with a view to type and quantity as well as the heat-treatment conditions that both deformability and strength meet the respective requirements. The strength of the bonding wire becomes higher as the copper content is increased.From JP 01-87734 A (Patent Abstracts of Japan) there is known a fine wire of gold and 0.05 to 0.3 wt% of at least one of the-4elements chosen from the group of copper, aluminum, yttrium, nickel, cobalt, titanium, tungsten, silicon, zirconium, calcium, palladium, ruthenium, iridium, platinum, silver and osmium. The ultra-fine wire has good ductility and very good mechanical characteristics.JP 08-199261 A (Japanese Patent Office - Patent Abstracts of Japan) describes a bonding wire of high-purity gold, 0.1 to 2 wt% of copper, 0.01 to 0.1 wt% of palladium and if required, 0.0001 to 0.01 wt% of tin and / or 0.0001 to 0.01 wt% of at least one metal chosen from the group of calcium, beryllium, germanium, rare earth metals, strontium, barium, indium and titanium. The strength of the bonding wire is sufficient to prevent contact defects between adjacent bond loops in plastic-embedded semiconductor devices .The requirements for selecting bonding wires include not only special chemical and physical properties but also, in particular, the highest possible strength for any given elongation.The object of the invention is therefore to find a fine wire of the type discussed above, comprising a gold alloy which has the best possible strength-to-elongation ratio and whose electrical conductivity differs as little as possible from that of a puregold fine wire. Another object is to provide a cost-effective,-5continuous method for making such fine wire. The fine wire is intended to be suitable both for wire bonding and also for making ball bumps for flip-chip technology, as is described, for example, in DE 44 42 960 C.β Brief Description of the InventionThe object is achieved by a fine wire of a gold alloy which is characterized according to the invention by the fact that the gold alloy consists essential of 0.5 to 0.9 wt% of copper and a further component which is either (i) 0.05 to 0.95 wt% of platinum, or (ii) 0· 0001 to 0.1 wt% of at least one element from the group of alkaline earth metals and rare earth metals, and 0 to 1 wt% of platinum; with the remainder being gold. The usual diameter of the wire can normally range from about 10 to 200 micrometers and usually about 20 to 60 micrometers.Brief- Description of the Drawing✓The figure shows the tensile strength (N / mm2) versus elongation at fracture (%) for fine wires according to the examples described below.Detailed DescriptionA fine wire of a gold alloy which according to the invention is formed of a gold alloy consisting essential of 0.5 to 0.9 wt% of copper, 0.05 to 0.95 wt% of platinum and the rest being gold; or of a gold-6alloy containing 0.5 to 0.9 wt% of copper, 0.0001 to 0.1 wt% of at least one element from the group of alkaline earth metals and rare earth metals, 0 to 1 wt% of platinum and the rest being gold, is provided especially for use as a bonding wire in semiconductor devices. The wire will typically have a diameter of 10 to 200 micrometers, more usually 20 to 60 micrometers.Within the meaning of the invention, alkaline earth metals include beryllium, magnesium, calcium, barium and strontium; and rare earth metals include lanthanum (atomic number 57) and the elements following lanthanum, from cerium (atomic number 58) to lutetium (atomic number 71), also referred to as lanthanum series elements in the technical literature.Advantageously the content of alkaline earth metal and / or rare earth metal, if present, is 0.001 to 0.01 wt% and that of platinum, if present, is 0.1 to 0.9 wt%.The alkaline earth metal preferably comprises beryllium, magnesium, calcium or a mixture of at least two of these alkaline earth metals. If mixtures of beryllium and calcium are used, mixtures comprising 50 wt% each of beryllium and calcium have proved particularly suitable.-7The rare earth metal preferably comprises cerium or a mixture of cerium and one or more of the rare earth metals with atomic numbers of 57 and 59 to 71. Cerium mischmetal has proved a particularly suitable good commercial source of cerium.According to Rompp Chemie Lexikon, 10thedition (1996), 647, the designation of cerium mischmetal usually refers to a mixture of 50 to 60% of cerium, 25 to 30% of lanthanum, 10 to 15% of neodymium, 4 to 6% of praseodymium and 1% of iron plus low proportions of other rare earth metals.The fine wire according to the invention with a diameter which is standard for bonding wires has all the characteristics necessary for semiconductor bonding use. The usual diameter for bonding wires is in the range of 10 to 200 micrometers, more usually 20 to 60 micrometers, although other diameters as required, are of jg course, possible. The invention bonding wire properties are characterized in particular by high electrical conductivity, measured as the specific electrical resistance (see Table VIII) and very good strength-to-elongation ratio (see figure).- 8 10By virtue of its favorable characteristics, the fine wire according to the·invention can be used with particular advantage for wire bonding, including the high-frequency bonding technique being developed, and for making the ball bumps for flip chips.B The achievement of the objects of the invention further comprises a method for making a fine wire for bonding semiconductor devices comprising a gold alloy which is characterized according to the invention by the fact that a gold alloy of a) 0.5 to 0.9 wt% of copper, 0.05 to 0.95 wt% of platinum, the remainder being gold, or of b) 0.5 to 0.9 wt% of copper, 0.0001 to 0.1 wt% of at least one element from the group of alkaline earth metals and rare earth metals, 0 to 1 wt% of platinum; with the remainder being gold, is melted, the melted alloy is continuously cast into a strand, the strand is drawn to a bonding wire of standard diameter (e.g. 10 to 200 micrometers), and the wire is annealed.The method according to the invention has proved particularly useful when the molten alloy is continuously cast as a strand of circular tcross section and the wire is annealed at about 300 to 700°C.The annealing step imparts the necessary elongation to the wire, which initially is cold drawn. Melting and continuously casting of the alloy can be performed in air, under shielding gas such as argon, or in vacuum.-1011Melting of a gold alloy including the content of alkaline earth metal and / or rare· earth metal of 0.001 to 0.01 wt% and a content of platinum, if present, of 0.1 to 0.9 wt% is preferred in the method according to the invention.As alkaline earth metal there can be used beryllium, magnesium, calcium, strontium, barium or a mixture of at least two of these elements. Beryllium, magnesium, calcium or a mixture of at least two of these alkaline earth metals has proved particularly useful. If mixtures of beryllium and calcium are used, those comprising 50 wt% each of beryllium and calcium are preferred.As rare earth metal there can be used in particular cerium or a mixture of cerium and one or more rare earth metals with atomic numbers of 57 and 59 to 71, the latter preferably in the form of commercial cerium mischmetal.The method according to the invention is particularly commercially favorable because it can be operated continuously to yield products such as cast strand and drawn wire with extremely uniform and constant quality.The invention will be described in more detail hereinafter by examples of fine wires and manufacture thereof according to the invention (Examples 1 to 6) and, for comparison, of a fine wire-1112 according to the prior art known from DE 16 08 161 C (Example 7). The fine wires are characterized by their elongation (elongation after fracture) [%] and strength (tensile strength) [N / mm2] and their specific electrical resistance [ohm mm2 / m].Example 1Fine wire of a gold alloy with 0.8 wt% of copper and 0.8 wt% of platinum.A melt of an alloy of 0.8 wt% of copper, 0.8 wt% of platinum and gold as the remainder is cast in a continuous-casting system to a strand of circular cross section. A wire with a diameter of 30 micrometers is then drawn from the strand and the wire is annealed at about 300 to 700°C in air depending on the elongation to be achieved. The strength values [N / mm2] measured as a function of elongation [%] are listed in Table I.IS The specific electrical resistance at room temperature, measured on a wire with a diameter of 275 micrometers, is 0.041 ohm mm2 / m.-1213Table IElongation [%] Strength [N / mm2] Cold drawn 600 2.6 301 2.7 281 3.6 263 5.3 245 6.8 232 8.5 219 9.1 209 9.7 197 11.4 194Example 2Fine wire of beryllium, 0 a gold alloy with 0.8 wt% of copper, 0.001 wt% of 001 wt% of calcium and 0.8 wt% of platinum.A melt of an alloy of 0 0.001 wt% of calcium, 0 remainder is cast in a circular cross section.is then drawn from the .8 wt% of copper, 0.001 wt% of beryllium, .8 wt% of platinum and gold as the continuous-casting system to a strand of A wire with a diameter of 30 micrometers strand and the wire is annealed at about-1314300 to 700°C in air depending on the elongation to be achieved. The strength values [N / mm2] measured as a function of elongation [%] are listed in Table II.The specific electrical resistance at room temperature, measured 5 on a wire with a diameter of 275 micrometers, is 0.041 ohm mm2 / mTable IIElongation [%] Strength [N / mm2] Cold drawn 585 3 . 6 375 3 . 8 354 4.2 337 4.4 318 4.6 308 5.9 293 7.3 281 8.7 267 10.1 255-1415Example 3Fine wire of a gold alloy with 0.8 wt% of copper, 0.001 wt% of beryllium, 0.001 wt% of calcium and 0.3 wt% of platinum.A melt of an alloy of 0.8 wt% of copper, 0.001 wt% of beryllium, § 0.001 wt% of calcium, 0.3 wt% wt% of platinum and gold as the remainder is cast in a continuous-casting system to a strand of circular cross section. A wire with a diameter of 30 micrometers is then drawn from the strand and the wire is annealed at about300 to 700°C in air depending on the elongation to be achieved.The strength values [N / mm2] measured as a function of elongation [%] are listed in Table III.The specific electrical resistance at room temperature, measured on a wire with a diameter of 275 micrometers, is 0.036 ohm mm2 / m.-1516Table IIIElongation [%] Strength [N / mm2] Cold drawn 614 3.6 367 3.8 343 4.2 319 5.2 308 6.1 294 7.1 281 8.7 270 10.1 257 10.7 246Example 4Fine wire of a gold alloy with 0.9 wt% of copper, 0.001 wt% of beryllium and 0.001 wt% of calcium.A melt of an alloy of 0.9 wt% of copper, 0.001 wt% of beryllium 0.001 wt% of calcium and gold as the remainder is cast in a continuous-casting system to a strand of circular cross section A wire with a diameter of 30 micrometers is then drawn from the strand and the wire is annealed at about 300 to 700°C in air-1617 depending on the elongation to be achieved. The strength values [N / mm2] measured as a function of elongation [%] are listed in Table IV.The specific electrical resistance at room temperature, measured on a wire with a diameter of 275 micrometers, is 0.034 ohm mm2 / mTable IVElongation [%] Strength [N / mm2] Cold drawn 673 4.4 352 4.6 330 5.3 316 6.2 298 7.9 273 10.8 255Example 5Fine wire of a gold alloy with 0.9 wt% of copper, 0.001 wt% of beryllium, 0.001 wt% of calcium and 0.9 wt% of platinum.A melt of an alloy of 0.9 wt% of copper, 0.001 wt% of beryllium, 10 0.001 wt% of calcium, 0.9 wt% of platinum and gold as the-1719A melt of an alloy of 0.8 wt% of copper, 0.01 wt% of cerium and gold as the remainder is cast in a continuous-casting system to a strand of circular cross section. A wire with a diameter of 30 micrometers is then drawn from the strand and the wire is 5 annealed at about 300 to 700°C in air depending on the elongation to be achieved. The strength values [N / mm2] measured as a function of elongation [%] are listed in Table VI.The specific electrical resistance at room temperature, measured on a wire with a diameter of 275 micrometers, is 0.034 ohm mm2 / m.Table VIElongation [%] Strength [N / mm2] Cold drawn 585 2.7 328 3.5 288 4.9 268 8.7 249Example 7 (comparison)Fine wire of a gold alloy with cerium mischmetal according toDE 16 08 161 C.-1920A melt of an alloy of gold and cerium mischmetal is cast in a continuous-casting system to a strand of circular cross section. A wire with a diameter of 30 micrometers is then drawn from the strand and the wire is annealed at about 300 to 600°C in air 5 depending on the elongation to be achieved. The strength values [N / mm2] measured as a function of elongation [%] are listed inTable VII.The specific electrical resistance at room temperature, measured on a wire with a diameter of 275 micrometers, is 0.023 ohm mm2 / mTable VIIElongation [%] Strength [N / mm2] Cold drawn 375 2.9 263 3.1 253 3.6 243 4.0 230 5.7 220 8.1 209 10.1 198-2021Table VIIISpecific electrical resistance | 0.041 0.041 0.036 0.034 0.043 0.034 0.023 0.023 CO o o 0.043 0.073 0.068 4J CO CO co cn o o o Cd o o o o CN IT) CN CJ co CO co cn cn CO o o o o o o o o o CN CN rd a) O u o ο\° 4J rd rd rd rd 5 (0 u O O O O o O o O ρ 0 •Η o o o o 4J •Η rd rd rd rd ο a 1) CQ O O O O O O o O ε ο O O o O υ P p p P P P P P P P Φ QJ Φ Φ Φ Φ Φ 0) qj QJ Ό TJ TJ Ό Ό Ό TJ TJ TJ TJ P P P P P P o P P P P < -H •H •H •rd •H •H o •H -H -H -H nJ nJ nJ nJ nJ nJ rd nJ nJ nJ nJ ε ε ε ε ε ε ε ε ε ε QJ φ QJ φ <u <u QJ <u qj qj P ρ P P P P P P P P Φ f—( a ε nJ rd CN co LT) <0 * a ε 0 Q comp . ) comp . ) (comp .) (comp .) (comp .) X — — Cd co σ> 10 11 CN rdCO co oωCdQP0)CX r—f nJ4J0) εΛ uω-Η εε •ΗΡ φυ η4J-Η >1 οI—f I—1Π3ΌI—fΟΟ *-21 22β 0 •Η 4J Π5 tn C (Μ 0 ε ε ο s »\° ·— 260 335 330 365 373 280 230 |- Strengtl Cold drawn | 009 585 614 673 648 585 375 XJ CU 0.8 0.8 0.3 0.9 | nD 0.8 0.8 0.8 0.9 0.9 0.8 (1) O o\o 1 1 0.01 J5 r- 113 g U H XJ 0.001 0.001 0.001 0.001 Composi Be | 0.001 0.001 0.001 0.001 0 < remainder remainder remainder remainder remainder remainder Example l—I CN m <5f LD <0 7 (comp .) *u

Claims

WHAT IS CLAIMED IS:

1. A fine wire of a gold alloy for bonding semiconductor devices, wherein the gold alloy consists essentially of 0.5 to 0.9 wt % of copper, 0.05 to 0.95 wt % of platinum, and the remainder being gold.

2. A fine wire of a gold alloy for bonding to semiconductor devices, wherein the gold alloy 6 consists essentially of 0.5 to 0.9 wt % of copper, 0.0001 to 0.1 wt % of at least one element from the group of alkaline earth metals and rare earth metals, 0 to 1 wt % of platinum, and the remainder being gold.

3. A fine wire according to claim 2, wherein the alkaline earth metal and / or rare earth metal content ofthe gold alloy is 0.0001 to 0.01 wt %. 10 4 A fine wire according to one of claims 1 to 3, wherein the platinum content of the gold alloy is 0.1 to 0.9 wt %.

5. A fine wire according to one of claims 2 to 4, wherein the alkaline earth metal is beryllium, magnesium and / or calcium.

6. A fine wire according to one of claims 2 to 5, wherein the rare earth metal is cerium.

7. A method for making a fine wire from a gold alloy for bonding semiconductor devices according to one of claims 1 to 6 comprising the steps of: (a) melting a gold alloy of i) 0.5 to 0.9 wt % of copper, 0.05 to 0.95 wt % of platinum, the remainder being gold, of of ii) 0.5 to 0.9 wt % of copper, 0.0001 to 0.1 wt % of at least one element from the group of alkaline earth metals and rare earth metals, 0 to 1 wt % of platinum; and the remainder being gold; (b) continuously casting the melted alloy into a strand, (c) drawing the strand to a wire of standard diameter for bonding purposes; and (d) annealing the wire.

88. A method according to claim 7, wherein the continuously casting of the molten alloy is to a strand of circular cross section. • f / 9. A method according to claim 7 or 8, wherein a gold alloy with an alkaline earth metal and / or rare earth metal content of 0.001 to 0.01 wt % is melted.

10. A method according to one of claims 7 to 9, wherein a gold alloy with a platinum content of 0.1 to 0.9 wt % is melted.

511. A method according to one of claims 7 to 10, wherein a gold alloy containing beryllium, magnesium and / or calcium as alkaline earth metal is melted.

12. A method according to one of claims 7 to 11, wherein a gold alloy containing cerium as rare earth metal is melted.

13. A method according to one of claims 7 to 12, wherein the annealing step comprises jq heating the wire to a temperature of about 300°C to about 700°C.

14. Use of a fine wire according to one of claims 1 to 6 for wire bonding.

15. Use according to claim 14 for wire bonding by high frequency.

16. Use of a fine wire according to one of claims 1 to 6 for bonding of semiconductor devices in flip-chip technology.