Menthod of producing an electronic device having a pb free solder connection, pb-free solder-connected structure and electronic device
Patent Information
- Application Number
- MYPI1998005624
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 1998-12-12
- Publication Date
- 1999-06-16
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The use of lead-based solders in electronic devices poses environmental pollution risks due to toxicity and the formation of whiskers, which can lead to electrical failures, and existing lead-free alternatives lack sufficient bonding strength and wettability.
The implementation of a lead-free Sn-Ag-Bi alloy solder with a Bi content of 1 wt% to 5 wt% for bonding electronic devices, which forms a stable interface and provides adequate bonding strength, resistance to whisker formation, and good wettability at soldering temperatures of 220-240°C, using various electrode materials such as Cu or Fe-Ni alloys with or without additional plating layers.
This solution ensures a stable bonding interface with high enough strength to withstand thermal expansion stresses and handling, while preventing whisker formation and maintaining good wettability, thus enabling the production of environmentally friendly electronic devices with reliable solder connections.
Abstract
Description
METHOD OF PRODUCING AN ELECTRONIC DEVICE HAVING A PB FREE SOLDER CONNECTION, PB-FREE SOLDER-CONNECTED STRUCTURE ANDELECTRONIC DEVICEBACKGROUND OF THE INVENTIONThe present invention relates to an electronic device, a method of producing the electronic device, a semiconductor device, a methodof making the semiconductor device and a method of bonding the semiconductor device, in which a lead-free solder of low toxicity is used.In order to produce an electric circuit board by bonding electric devices (e.g. LSIs) to a circuit board made of an organic 'material, for example, conventionally, there has been used a eutectic Sn-Pb alloy solder, another Sn-Pb alloy solder which has a chemical composition and a melting point, each close to that of the eutectic Sn-Pb alloy solder, and other solder alloys which are obtained by adding small amounts of bithmuth (Bi) and / or silver (Ag) to the solders recited above. These solders.comprise about 40 wt% Pb and have a melting point of about 183°C, which permit soldering at 220-240°C.With regard to electrodes of electronic devices, such as QFP (Quad Flat Package)-LSIs, to be soldered, there have been usually used those made of 42 alloy which is an Fe-Ni alloy and on which a layer of 90 wt% Sn-10 wt% Pb alloy (hereinafter referred to Sn-lOPb) is formed. .This is because such electrodes have good wettability, good preservation and no problem of formation of whiskers. / A / / / 2However, the lead (Pb) in the Sn-Pb solders is a heavy metal harmful to humans and pollution of the global environment caused by dumping of lead-containing products and their bad effect on living things have presented problems. The pollution of the global environment by electrical appliances occurs when lead is dissolved by rain, etc. from the dumped lead-containing electrical appliances exposed to. sunlight and rain. The dissolution of Pb tends to be accelerated by the recent acid rain. In order to reduce'environmental pollution, therefore, it is necessary to use a lead-free .soldering material of low toxicity not containing lead as a substitute for the above eutectic Sn-Pb alloy solder which is used in large quantity and to employ a structure of the electrode of a device not containing lead as a substitute, material to. replace the Sn-lOPb layer provided on the electrode of a device. A Sn-Ag-Bi alloy solder is a promising candidate as a’lead-free soldering material in terms of low toxicity, obtainability for raw materials, production cost, wettability, mechanical properties, reliability, etc. Soldering is usually performed at a temperature of about 220-240°C so as to produce compounds among components electrodes of a board and a solder. From this, because the bonding interfaces differs from one another depending upon different kinds of combinations of solder materials and electrode materials of components, an electrode material suitable to the respective ¥solder is requested for obtaining a stable bonding interface .SUMMARY' OF THE INVENTIONAn Object of the present invention is to provide a bonded structure by a lead-free-solder, in which a lead free Sn-Ag-Bi alloy solder having low toxicity 'is used for electrodes of lead formes, etc. and which has a stable bonding interface and an enough bonding strength.Another object of the invention is to provide an electronic article with utilization of a lead-free Sn-Ag-Bi alloy solder having low toxicity, which has a stable bonding interface with respect to a secular change arid a strength high enough to withstand stress generated in bonded portions '15 by soldering due to a difference in thermal expansion coefficient between electric devices and a board, a work of dividing the board after soldering, curving of the board during the probing test, handling and so on.A further object of the invention is to provide an electronic device with utilization of a lead-free Sn-Ag-Bi alloy solder having low toxicity, which has an enough bonding strength while ensuring resistance to formation of whiskers, wettability of the solder and so on.Thus, according to a first aspect of the invention, there are provided the following six types of electronic device. <(1) An electronic device comprising a board and a semiconductor device both of which are connected with each other by means of a Pb-free solder comprising Bi, the semiconductor device having a lead on which a Sn-Bi alloy layer comprising 1 wt% to 5 wt% Bi is formed.(2) An electronic device comprising a board and a .semiconductor device both of which are connected with each other by means of a Pb-free solder comprising Bi, the semiconductor device having a lead made of Cu or a Cu alloy on which a Sn-Bi alloy plating layer comprising 1 wt% to 5 wt% Bi is formed as a surface layer.(3) An electronic device comprising a board and a semiconductor device both of which are connected with each other by means of a Pb-free solder comprising Bi, the semiconductor device having a lead made of Cu or a Cu alloy on which a Sn-Bi alloy layer comprising from about 1 wt% to about 5 wt% Bi is directly formed as a surface layer.(4) An electronic device comprising a board and a . semiconductor device both of which are connected with each other by means of a Pb-free solder comprising Bi,-the semiconductor device having a lead made of Cu or a Cu alloy on which a Sn-Bi alloy plating layer comprising from about 1 wt% to about 5 wt% Bi is formed as' a surface layer without any other plating under-layer.(5) An electronic device comprising a board and a semiconductor device both of which are connected with each other by means of a Pb-free solder comprising Bi, the semiconductor device having a lead made of an Fe-Ni alloy on which a Sn-Bi 'alloy plating layer comprising 1 wt% to 5 wt% Bi is formed as a surface layer.(6) An‘electronic device comprising a board and a semiconductor device both of which are connected with each other by means of a Pb-free solder comprising Bi, the semiconductor device having a lead made of an Fe-Ni alloy on which a Sn-Bi alloy layer comprising from about 1 wt% to about 5 wt% Bi is directly formed as a surface layer.In one embodiment; of the electronic devices,- the Pb-solder comprising Bi is of a Sn-Ag-Bi alloy.In another embodiment of’the electronic devices, the semiconductor device is of the TSOP type.According to a second aspect of the invention, there are provided the following six types of the process.(1) A method of producing an electronic device, which comprises connecting a semiconductor device with a board by means of a Pb-free solder comprising Bi, the semiconductor device having a lead on which a Sn-Bi alloy layer comprising wt% to 5 wt% Bi is formed.(2) A method of producing an electronic device, which comprises connecting a semiconductor device with a board by means of a Pb-free solder comprising Bi', the semiconductor device having a lead made of Cu or a Cu alloy on which a SnBi alloy plating .layer comprising 1 wt% to 5 wt% Bi is formed as a surface layer.(3) A method of producing an electronic device, which comprises connecting a semiconductor device with a board by means of a Pb-free solder comprising Bi, the semiconductor device having a lead made of Cu or a Cu alloy on which a SnBi alloy layer comprising from about 1 wt% to about 5 wt% Bi is directly formed as a surface layer.(4) A method of producing an electronic device, which comprises connecting a semiconductor device with a board by means of a Pb-free solder comprising Bi, the semiconductor device having a lead made of Cu or a Cu alloy on which a SnBi alloy plating layer comprising from about 1 wt% to about 5 wt% Bi is formed as a surface layer without any other plating under-layer.(5) A method of producing an electronic device, which comprises connecting a semiconductor device with a board by means of a Pb-free solder comprising Bi, the semiconductor device having a lead made of an Fe-Ni alloy on which a Sn-Bi alloy plating layer comprising 1 wt% to 5 wt% Bi is formed as a surface layer.(6) A method of producing an electronic device, which' comprises connecting a semiconductor device with a board by means of a Pb-free solder comprising Bi, the semiconductor device having a lead made of an Fe-Ni alloy on which a Sn-Bi alloy layer comprising from about 1 wt% to about 5 wt% Bi is .directly formed as a surface layer.In one embodiment of the methods of producing an electronic device, the Pb-free solder comprising Bi is of a Sn-Ag-Bi alloy.In another embodiment of the methods of producing 5 an electronic device, the semiconductor device is of theTSOP type.According to a third aspect of the invention, there is provided a semiconductor device having an electrode adapted for joining by means of a lead-free solder characterized in that the electrode has a coating layer of a Sn-Bi alloy comprising 1 wt% to 5 wt% B'i.In one embodiment of the semiconductor device, there is provided a copper layer between said electrode and said Sn-Bi alloy coating layer.In another embodiment of the semiconductor·device, the electrode is made of Cu or a Cu alloy.In still another embodiment of the semiconductor device, the electrode is'made of an Fe-Ni alloy.In still another embodiment of the semiconductor device, the semiconductor device is of a TSOP type.In still another embodiment of the semiconductor device, the semiconductor device is of a QFP type.The semiconductor device may be made by the following manners.(1) The Sn-Bi alloy coating layer is formed by plating .(2) The Sn-Bi alloy coating layer is formed by dipping.(3) The Sn-Bi alloy coating layer is formed by any one of deposition by evaporation, -roller coating and metal powder application.According to a fourth aspect of the invention, there is provided a method of bonding a semiconductor device having an electrode, by means of a lead-free solder, characterized in that prior to bonding to the solder the electrode has a coating of a Sn-Bi alloy containing 1 wt% to wt% Bi .In one embodiment of the method Of bonding a semiconductor device, the electrode has a Cu layer under the Sn-Bi alloy coating layer.In another embodiment of the method of. bonding a semiconductor device, the electrode is made of Cu or a Cu layer, or of an Fe-Ni alloy. *In still another embodiment of the method of bonding a semiconductor device, the solder is a.Sn-Ag-Bi alloy. One embodiment of the solder comprises Sn. as a primary component, 5 wt% to 25 wt% Bi, 1.5 wt% to 3 wt% Ag and up to 1 wt% Cu.As can be understood from the above, according to the present invention, it is possible to ensure a stable bonding interface having an enough bonding strength by way of applying the lead-free Sn-Ag-Bi alloy solder of low toxicity to an electrode such as a lead frame. With utilization of the lead-free Sn-Ag-Bi alloy solder of low toxicity, it is also possible to ensure a bonding interface which is stable with respect to a secular change and which has a high enough strength to withstand stress generated in bonded portions by soldering due to a difference in thermal expansion coefficient between electric devices and a board, a work of dividing the board after soldering, curving of the board during the probing test, handling and so on. Further, with utilization of the lead-free Sn-Ag-Bi alloy solder of low toxicity, it is possible to ensure a bonding interface which has an enough strength and good resistance to occurrence of whiskers by way of forming sufficient fillets while keeping good wettability at a soldering temperature of, for example, 220-240°C.BRIEF DESCRIPTION OF THE DRAWINGSFig. 1 shows a cross-sectional view of a lead for a QFP-LSI according to the invention;Fig. 2 shows a cross-sectional view of a. lead for a ΤΞΟΡ according to the invention;Fig. 3 schematically shows a testing way of evaluating solder-bonding strength;Fig. 4 shows evaluation results of fillet strength with regard to various kinds of metallized leads according to the invention;Fig. 5 shows evaluation results of necessitate time for wetting with regard to various kinds of metallized leads according to the invention;Fig. 6 shows evaluation results of wetting force with regard to various kinds of metallized leads according to the invention;Fig. 7 shows evaluation results of fillet strength with regard to various kinds of metallized leads optionally provided with a copper layer under a metallized layer according to the invention;Fig. 8 shows evaluation results of flat portion strength with regard to various kinds of metallized leads optionally provided with a copper layer under a metallized layer according to the invention;Fig. 9A is a micro-photograph (Magnification; XXXX times) showing a cross-sectional view of an interface portion of a solder and a lead of an Fe-Ni alloy (i.e. 42 alloy) , on which a Sn-'lOPb alloy plating is provided, according to the prior art;Fig. 9B is a micro-photograph (Magnification: YYYY times) of an enlarged view of Fig. 9A, which shows the lead at a fractured portion;Fig. 9C is a micro-photograph (Magnification: YYYY times) of an enlarged view of Fig. 9A, which shows the solder at a fractured portion;·Fig. 10A is a micro-photograph (Magnification:ZZZZ times) showing a cross-sectional view of an interface portion of a solder and a lead of an Fe-Ni alloy (i.e. 42 alloy), on which a Sn-4Bi alloy plating is provided, according to the invention;Fig. 10B is a micro-photograph (Magnification:MMMM times) of an enlarged view of Fig. 10A, which shows the lead at a fractured portion;Fig. 10C is a micro-photograph (Magnification:MMMM times) of an enlarged view of Fig. 10A, which shows the solder at a fractured portion;Fig. 11A is a micro-photograph (Magnification:NNNN times) showing a cross-sectional view of an interface portion of a solder and. a lead of an Fe-Ni alloy (i.e. 42 alloy), on which an under copper layer and an overlay of a Sn-4Bi alloy plating are provided, according to the invention;Fig.' 11B is a micro-photograph (Magnification:0000 times) of an enlarged view of Fig. 11A, which shows the lead at a fractured portion; andFig. 11C is a micro-photograph (Magnification:0000 times) of an enlarged view of Fig. 11A, which shows the solder at a fractured portion.DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTSHereinafter, embodiments of the invention will be described.Provided is an electronic article as one embodiment of the invention, comprising a first and a second electrodes both of which are bonded with each other by means of a lead-free solder having low toxicity, the first electrode being a QFP lead, a TSOP lead or the like in an electronic device such as a semiconductor device (e.g. LSI), for example, and the second electrode being of a lead-free solder having low toxicity.The lead-free solder having low toxicity can be of a Sn-Ag-Bi alloy. With utilization of the Sn-Ag-Bi alloy, it is required to obtain a bonding interface which is stable with respect to a secular change and has a bonding strength high enough to withstand stress generated in solder-bonded portions due to a difference in thermal expansion coefficient between an electronic device and a circuit board, a work of dividing the board after soldering, curving of the board during the probing test, handling and so on.It is also required to obtain an enough bonding strength with utilization of the lead-free Sn-Ag-Bi alloy solder by forming a sufficient fillet shape while ensuring sufficient wettability at 220-240°C, which are suitable soldering temperatures to heat resistance of circuit boards arid electronic devices. If the solder has inferior wettability, sufficient .fillet shapes can not be formed resulting in that an enough bonding strength is not obtained or a more active flux is required so as to adversely affect on insulation resistance. Furthermore, it is also necessary to ensure resistance to formation of whiskers, etc. because shorts occur between electrodes if whiskers form and grow on the electrode surface formed by plating, etc.As shown in Figs. 1 and 2, an Sn-Bi layer 2 is formed on the surface of an electrode 1, which consists a lead, to obtain sufficient- bonding strength as the above electrode structures related to this invention. Next, a selection of an electrode structure related to 'this invention will be described. This selection was made by evaluating mainly bonding strength, wettability and resistance to formation of whiskers based on the above requirements ,First, the results of an examination of the bonding strength obtained between an Sn-Ag-Bi alloy solder and various kinds of electrode materials are shown. An outline of the measuring method is shown in Fig. 3. A model lead 4 was formed by applying lead-free materials (Sn and Sn-Bi, Sn-Zn and Sn-Ag alloys), which are considered to be usable as substitute materials to replace the conventional Sn-10 Pb alloy layer, to a lead, which is an electrode formed from an Fe-Ni alloy (42 alloy). Besides, an evaluation was also conducted for combinations with the conventional Sn-10.Pb alloy. The model lead 4 is 3 mm wide and 33 mm long. It is bent to form right angles so that the length of the soldered portion is 22 mm. The plating thickness was approximately 10 μτη for each composition.This model lead 4 was soldered to a Cu pad (Cu electrode) 7 on a glass epoxy substrate 6, which is a circuit board, with utilization of a lead-free solder 5 with 82.2 wt% Sn-2.8 wt% Ag-15 wt% Bi (hereinafter referred to as Sn-2.8Ag-15Bi).The size of the Cu pad (Cu electrode) 7 on the glass epoxy substrate 6 is 3.5 mm x 25 mm and a solder 5 was fed in the form of solder foil of 0.1 mm x 25 mm x 3.5 mm. More specifically, the above solder foil 5 was placed on the Cu pad 7 on the glass epoxy substrate 6 and the model lead 4 bent to form right angles was placed on the solder foil 5. Soldering was performed in the air at a peak temperature of 220°C after preheating to 140°C for 60 seconds. The flux used was a rosin flux containing chlorine. After soldering, cleaning was conducted with an organic solvent. The peeling test was conducted in three cases; i.e., immediately after soldering, after the exposure of the model lead to a high temperature of 125°C for 168 hours following soldering in consideration of the deterioration of bonding strength due to secular changes, and after soldering following the exposure of the model lead to 150°C for 168 hours to investigate interface strength in a case where the wettability of lead deteriorates. In the peeling test, with the substrate fixed, the model lead was pulled vertically at a rate of 5 mm / minute by yanking on its leading end. The then maximum strength and tensile strength that becomes constant were evaluated as fillet strength and flat portion strength, respectively, for the model leads of each composition. This test was conducted 10 times for each condition and test values were averaged.The results of the evaluation of the fillet strength of model leads of each composition are shown in Fig. 4. In plastic package devices such as ordinary QFP-LSIs, it is necessary that fillet strength be at least approximately 5 kgf in consideration of a differe'nce in terminal expansion coefficient of printed-circuit board.From this, it became apparent that an adequate bonding interface cannot be obtained in the case of Sn-Zn, Sn-Ag and Sn-Pb alloy layers although fillet strength of 5 kgf and more was obtained with the model leads in which an Sn layer or Sn-Bi layers other than Sn-23Bi layers containing 23 wt% Bi are applied to an Fe-Ni alloy (42 alloy). In addition to these model leads, further three kinds of model leads were made by applying an Ni plating layer of about 2 μηη to 42 alloy and plating this Ni layer with an Au layer, a Pd layer, and a Pd layer plus an Au layer. Soldering was performed in the same manner and interface strength was investigated. However, sufficient fillet strength was incapable of being obtained as shown in Fig. 4.Accordingly, it became apparent that it is necessary to apply an Sn-Bi layer to a lead, which is an'electrode.Wettability to the Sn-2.8Ag-15Bi solder was examined by the meniscograph method in the Sn-Bi.alloy plated leads which showed sufficient interface strength in the above peeling test conducted on model leads of various compositions, A flux of weak activity was used in order to investigate wettability. Test pieces were obtained by cutting the above model leads into lengths of 1 cm. The wettability test was conducted under the test conditions: a solder bath temperature of 220°C, an immersion speed of 1 mm / minute, an immersion depth of 2 mm and an immersion time of 20 seconds. The time which elapses till the load recovers to 0 (zero) was regarded as wetting time and the load after immersion for 20 seconds was regarded as wetting force. Wettability was examined in two cases: a lead immediately after plating'and a lead exposed to 150° for 168 hours after plating. Measurements were made 10 times for each test condition and test values were averaged.The wetting time and wetting force for each composition are shown in Fig. 5 and Fig. 6, respectively.It became apparent from the results of wetting time shown in Fig. 5 that the higher, the Bi content, the better wettability in the .Sn-Bi alloy plated leads tested, immediately after plating, while wettability deteriorates at below 1 wt% Bi and at 23 wt% Bi when the leads are exposed to a high temperature of 150° for 168 hours. It can be said that at Bi contents of below 1 wt%, wettability was low because the wetting time became short though the wetting force was ensured as shown in Fig. 6. Therefore, it became apparent that desirable Bi contents are from 1 to 20 wt% in order to obtain sufficient wettability even with Sn-Bi alloy layers .Stresses generated in the interface is high when '5 materials with a great difference in thermal expansion coefficient are bonded together, when materials are used in an environment of great temperature difference, and the like. The bonding strength in the interface must be higher than approximately 10 kgf in order to. ensure sufficient reliability. Therefore, it became evident, from Fig. 4 that fillet strength of more than 10 kgf cannot be obtained by directly applying an Sn-Bi layer to an Fe-Ni'alloy (42 alloy). It is believed that this is because the compound in the interface are not sufficiently formed. Therefore, a Cu plating layer of about 7 μτη on average was applied to theFe-Ni alloy (42 alloy) and an Sn-Bi alloy plating layer was applied to this Cu layer in order to raise.the reactivity with the solder in’the interface and interface strength was measured. The results of the then fillet strength, along with those in the case of absence of a Cu layer, are shown in Fig. 7. Bonding strength of more than 10 kgf was obtained with the exception of the case of 23 ,wt% Bi and the effect of the underplate Cu layer was capable of being verified. By adopting this electrode structure it was possible to obtain interface strength higher than the interface strength of 12.1 kgf, which is obtained immediately after soldering in the conventional case where a lead obtained by applying an Sn-lOPb alloy layer to the'42 alloy lead is soldered with utilization of a eutectic Sn-Pb alloy solder, which is shown as a reference in Fig. 7.Furthermore, as shown in Fig. 8, flat portion strength was also capable of being improved by forming a Cu layer under the Sn-Bi alloy layer. This Cu layer may be applied to 42 alloy as described above when a 42 alloy lead frame, is used. However, when a Cu lead frame is used, this lead frame may be allowed to serve as the Cu layer or a further Cu layer may be formed in order to eliminate the effect of other elements which may sometimes be added to the lead frame material to improve rigidity. The wettability of the model leads to which this Cu layer is applied is also shown inFigs. 5 and 6. There is scarcely any effect of the Cu layer and sufficient wettability was capable of being obtained at 1-20 wt%. Bi, although wettability also deteriorated at Bi contents of not more than 1 wt% when the lead frames were exposed to a.high temperature. Incidentally, anSn-2.8Ag-15Bi was used in the examples shown in Figs. 7 and 8. However, the formation of an underplate Cu layer is effective in improving interface strength even in systems of low Bi content, for example, an Sn-2Ag-7.5Bi-0.5Cu alloy.The method of application of the above Sn-Bi alloy and Cu layers is not limited to plating and these layers can also be formed by dip, evaporation, roller coating and metal powder application.Thus, in order to investigate the reason why the interface differs from one another depending upon different kinds of electrode materials, the cross section of bonding portion was polished and the appearance of the interface was examined. Furthermore, the fractured surfaces of samples subjected to the tensile test were observed under an SEM.The results obtained in the typical combinations are described below.First, Figs . 9A, 9B and 9C show the results-of an observation in a case where a lead obtained by applying an Sn-lOPb alloy plating layer directly to the conventional Fe-Ni alloy (42 alloy) is bonded using an Sn-Ag-Bi alloy solder. In this combination, Pb-Bi alloy compounds gathered in the interface and fracture occurred in the interface between 42 alloy and the solder. A small amount of Sn was detected on the fractured 42 alloy surface of the lead and it is believed that the Sn in the solder formed compounds with the 42 alloy of lead.' It is believed, therefore,, that.agglomaration of the above compounds of Pb and Bi in the interface reduced the area of bond between Sn and 42 alloy, greatly weakening bonding strength.Next, Figs. 10A, 10B and 10C show the results of an observation in a case where the Sn-lOPb alloy plating layer was replaced with an Sn-4Bi alloy plating layer. The compound layer formed in the interface was thin and peeling occurred similarly in the interface between 42 alloy and solder. However, Bi remained granular crystals, which do not cause a decrease in the area of bond between Sn and 42 alloy so much as in the case of an Sn-lOPb. It might be thought that this is the reason why bonding strength of more than 5 kgf was capable of being obtained. An Auger analysis revealed that the then compound layer is an Sn-Fe layer of about 70 nm.Figs. 11A, 11B and 11C show the results of an 10 observation in a case where a Cu layer was formed on under the Sn-4Bi layer. It was found that a thick layer .of compounds of Cu and Sn is formed in the interface. Fracture occurred in the interface between this compound layer and the solder or in the compound layer. The fractured surface was almost flat in the case shown in Figs. 10A, 10B and 10C where the Sn-Bi alloy layer was directly formed on the 42 alloy lead, whereas it was uneven in the case where the Cu layer was present. For this reason, it might be thought that this difference in the fractured surface resulted in the improvement in interface strength. . Incidentally, similar investigation’ results, were obtained also from other Sn-Ag-Bi alloy solder compositions.The formation of .whiskers was investigated for the above model leads of each composition. The formation of whiskers was observed on the surfaces of the model leads to .which a Sn-Zn alloy plating layer was applied. It has hitherto been said that Sn plating presents a problem in resistance to the formation of whiskers. However, the formation of whiskers was not observed in the Sn-Bi alloy layers and there was no problem in resistance to formation of whiskers .Accordingly, with the use of the electrode structures according to the invention bonding portions excellent in bonding strength, wettability and resistance to formation of whiskers can be obtained for Sn-Ag-Bi alloy solders .The reason why Sn-Ag-Bi solders containing Sn as a primary component, 5 to 25 wt% Bi, 1.5 to 3 wt% Ag and 0 to 1 wt% Cu were selected is that solders of the composition in these ranges permit soldering at 220-240°C and that these solders have almost the same .wettability as eutectic Sn-Ag alloy solders, which have hitherto been field proven for Cu, and provide sufficient reliability at high temperatures.More specifically, Sn-Ag-Bi alloy solders have portions (ternary eutectic crystals) which melt at approximately 138°C when the Bi content is more than approximately 10 wt% and it is feared that these portions might have an adverse effect on reliability at high temperatures. However, the precipitation of ternary eutectic crystals is controlled to levels that pose no problem in practical use and high-temperature strength at 125°C is also ensured.Accordingly, practical and highly reliable electronic- articles can be obtained by soldering the above electrode using the solder of this composition.Example 1The cross-sectional structure of a lead forQFP-LSI .is shown in Fig. 1. This drawing illustrates part of the cross-sectional structure of the lead. An Sn-Bi alloy layer-2 is formed on a lead 1, which is' an Fe-Ni alloy (42 alloy). This Sn-Bi alloy layer 2 was formed by plating and its thickness was about 10 μτη. The Bi content of Sn-Bi alloy plating layer was.8 wt%. The above QFP-LSI having this' electrode structure was soldered to a glass epoxy substrate, which is a circuit board, with utilization of anSn-2.8Ag-15Bi-0.5C alloy solder. Soldering was performed in an N^ reflow furnace at a peak temperature of 220°C.Bonding portions having sufficient bonding strength was capable of being obtained. Similarly, reflow was conducted on a glass epoxy substrate in the air at 240°C with utilization of an Sn-2Ag-7.5Bi-0.5C alloy solder. Bonded portions treated by reflow have high reliability especially at high temperatures.Example 2The cross-sectional structure of a lead for TSOP is shown in Fig. 2. This drawing illustrates part of the cross-sectional structure of the lead. A Cu layer 3 is ' formed on a lead 1, which is an Fe-Ni alloy (42 alloy) and an Sn-Bi alloy layer 2 is formed on this Cu layer. TheSn-Bi alloy layer 3 and Sn-Bi layer 2 were formed by plating. The thickness of the Cu layer 3 was about 8 μιπ and that of the Sn-Bi plating layer was about 10 μπι. The Bi content of Sn-Bi alloy plating layer was 5 wt%. Because the rigidity of a lead is high in the TSOP, heat generation occurs in the device itself, stress generated at the interface greater as compared with the QFP-LSI. In such cases, it is necessary to form an interface with sufficient interface strength high enough to withstand this interface stress and the Cu layer under the Sn-Bi layer' is effective for this purpose.This TSOP was soldered to a printed-circuit board in a vapor reflow furnace with utilization of an Sn-Ag-Bi alloy solder and the thermal cycle test was conducted. The test was conducted under the two test conditions: (1) one hour per cycle of -55°C for 30 minutes and 125°C for 30 minutes, and (2) one hour per cycle of 0°C for 30 minutes and 90°C for 30 minutes. After 500 cycles and 1,000 cycles the cross section was observed and the condition of formation of cracks was investigated. The cycle test result of cracks occurrence was compared with a case where a TSOP of the same size having an 42 alloy on which an Sn-lOPb alloy layer is directly formed, was soldered using a eutectic Sn-Pb alloy solder. Although cracks were formed early in the thermal cycles of -55°C / 125°C, no problems arose with the thermal cycles of 0°C / 90°C and a bonding interface which is adequate for practical use was obtained. Example 3:The electrode structures according to this invention can also be applied in an electrode on a board.For example, solder coating is effective in improving the solderability of boards. Conventionally, there have been used lead-containing solders such as a eutectic Sn-Pb alloy solder. Thus, the Sn-Bi alloy layer according to the invention can be used to make the solder for coating lead-free. Furthermore, because the electrode of a board is made of copper, sufficient bonding strength can be obtained when an Sn-Ag-Bi alloy solder is used. An example in which this structure is applied is shown; an Sn-8Bi.alloy layer of about 5 μηι was formed by roller coating on a Cu pad (Cu electrode) on a glass epoxy substrate, which is a circuit board,The wettability to boards improved and at the same time, bonding strength was capable of being improved, because this solder layer was formed.As will be apparent from the above, according to the present invention, the following advantages can be obtained.An electrode structure can be realized, which is suitable for an Sn-Ag-Bi alloy solder excellent as a leadfree material.A bonded structure by a lead-free solder can be .realized with utilization of a lead-free Sn-Ag-Bi alloy solder, in which an bonding interface which is stable and has sufficient bonding strength can be obtained.An electronic article can be realized with utilization of a lead-free eutectic Sn-Ag-Bi alloy solder of low toxicity, which has a bonded structure by the lead-free solder, which can provide a stable bonding interface with respect to a secular change and a strength high enough to withstand stress generated in bonded portions by soldering due to a difference in thermal expansion coefficient between electric devices and a board, a work of dividing the board after soldering, curving of the board during the probing test, handling and so on.With utilization of a lead-free Sn-Ag-Bi alloy solder of low toxicity, it is possible to obtain sufficient bonding strength by forming adequate fillets while ensuring sufficient, wettability, for example, at 220-240° and to ensure resistance to formation of whiskers, etc.Soldering electronic devices with utilization of an Sn-Ag-Bi solder makes it possible to obtain an interface which has sufficient bonding strength and to ensure wettability which is sufficient for practical use. There is no problem in resistance to formation of whiskers. Thus it is possible to realize lead-free electrical appliances which are environmentally friendly by using the same equipment and process as conventionally.
Claims
1. An electronic device comprising a board (6) and a semiconductor device both of which are connected with each other by means of a Pb-free solder (5) comprising Bi, the 5 semiconductor device having a lead (1) on which a Sn-Bi alloy layer (2) comprising 1 wt% to 5 wt% Bi is formed.
2. An electronic device comprising a board (6) and a semiconductor device both of which are connected with each other by means of a Pb-free solder (5) comprising Bi, the 10 semiconductor device having a lead (1) made of Cu or a Cu alloy on which a Sn-Bi alloy plating layer (2) comprising 1 wt% to 5 wt% Bi is formed as a surface layer.
3. An electronic device comprising a board (6) and a semiconductor device both of which are connected with each 15 other by means of a Pb-free solder (5) comprising Bi, the semiconductor device having a lead (1) made of CU or a Cu alloy on which a Sn-Bi alloy layer (2) comprising from about 1 wt% to about 5. wt% Bi is directly formed as a surface layer.
204. An electronic device comprising a board (6) and a semiconductor device both of which are connected with each other by means of a Pb-free solder {5) comprising Bi, the semiconductor device having a lead (1) made of Cu or, a Cu alloy on which a Sn-Bi alloy plating layer (2) comprising 25; from about 1 wt% to about 5 wt% Bi is formed as a surface layer without any other plating under-layer.
5. An electronic device comprising a board (6) and a semiconductor device both of which are connected with each other by means of a Pb-free solder (5) comprising Bi, the semiconductor device having a lead (1) made of an Fe-Ni alloy on which a Sn-Bi alloy plating layer (2) comprising 1 wt% to 5 wt% Bi is formed as a surface layer.
6. An electronic device comprising a board (6) and a semiconductor device both of which are connected with each other by means of a Pb-free solder (5) comprising Bi, the semiconductor device having a lead (1) made of an Fe-Ni alloy on which a Sn-Bi alloy layer (2) comprising from about 1 wt% to about 5 wt% Bi is directly formed as a surface layer.
7. An electronic device according to any one of claims 1 to 6, wherein the Pb-solder (5) comprising Bi is of a Sn-Ag-Bi alloy.
8. An electronic device according to any one of claims 1 to 7, wherein the semiconductor device is of the TSOP type.
9. A method of producing an electronic device by connecting a lead (1) of a semiconductor device with an electrode (7) of a circuit board (6), the semiconductor device having a lead frame structure consisting of a lead material and a single Sn-Bi alloy layer (2) comprising of 1 to 5 wt% Bi, the lead material being a lead (1) of a lead frame, the method comprising: plating the single Sn-Bi alloy layer (2} comprising of 1 to 5 wt% Bi directly on the lead material of the lead frame, thereby forming said lead frame structure; then, directly contacting a Pb-free solder (5) with the electrode (7) of the circuit board and with the single Sn-Bi alloy layer (2) on the lead material; and soldering the lead (1) of the semiconductor device and the electrode (7) of the circuit board (6) by the Pbfree solder .(5) to form a compound layer between the lead material and the Pb-free solder (5).
10. A method of producing an electronic device according to claim 9, consisting essentially of said plating, said directly contacting and said soldering.,11. A method of producing an electronic device according to claim 9, wherein said Pb-free solder (5) contains Bi .
12. A'method.of producing an electronic device according to claim 9, wherein said Pb-free solder .(5) is an Sn-Bi-Ag solder.
13. A method of producing an electronic device according to claim 9, wherein said Pb-free solder (5) contains Sn and Ag.
14. A method of producing an electronic device according to claim 9, wherein said Pb-free solder (5) contains Sn, Ag and Cu. A method of producing an electronic device15. according to claim 9, wherein said Pb-free solder (5) contains 5 to 25 wt% Bi, 1.5 to 3 wt% Ag and up to 1 wt% Cu.
16. A method of producing an electronic device according to claim 9, wherein, at the time of said soldering, said Pb-free solder (5) directly contacts the electrode {7) of the circuit board <6) and the Sn-Bi alloy layer (2) on the lead (1).
17. A method of producing an electronic device according to claim 9, wherein the lead (1) includes a copper layer (3) on a lead substrate.
18. A method of producing an electronic device according to claim 17, wherein the lead on the lead substrate has been formed by plating.
19. A method of producing an electronic device according to claim 9, wherein in said plating, said single Sn-Bi alloy layer {2) is deposited as a single alloy layer.
20. A method of producing an electronic device according to claim 9, wherein said lead has an Fe-Ni alloy lead substrate.
21. A method of producing an electronic device according to claim 9, consisting of said plating, said directly contacting and said soldering.
22. A method of producing an electronic device according to claim 9, wherein said compound layer includes Sn and said lead material.
23. . A method of producing an electronic device according to claim 22, wherein after forming the compound layer, Bi remains as granular crystals.
24. A method of producing an electronic device according to claim 23, wherein the lead material is an Fe-Ni 5 alloy, and the compound layer is an Sn-Fe layer.
25. A method of producing an electronic device according to claim 22, wherein the lead material is an Fe-Ni alloy, and the compound layer is an Sn-Fe layer.
26. A method of producing an electronic device 10 according to claim 9, including the further step of forming a layer (3) of copper on the lead (1), such that the layer (3) of copper is between the lead (1) and the single Sn-Bi alloy layer {2), and wherein the compound layer includes compounds of Cu and Sn. 1527. A method of producing an electronic device according to claim 9, wherein after forming the compound layer, Bi remains as granular crystals.
28. A semiconductor device with a lead (1) which is made from a lead frame, wherein the lead (1) has a 20 layered structure thereon which consists of a single Sn-Bi alloy layer (2} , comprising 1 wt% to 5 wt% Bi, thereon, the single Sn-Bi alloy layer (2) being provided as’the single Sn-Bi alloy layer (2) prior to forming a soldered connection of the lead (1). 2529. A semiconductor device according to claim 28, wherein the lead <1) is a Cu alloy lead.
30. A semiconductor device according to claim 28, wherein the lead (1) is an Fe-Ni alloy lead.
31. A semiconductor device according to claim 28, wherein a Cu layer (3.) is present between the lead (1) and 5 the Sn-Bi alloy layer (2).
32. A semiconductor device according to claim 28, wherein a Cu layer (3) is present between the Fe-Ni alloy lead (1) and the Sn-Bi alloy layer (2}.
33. A semiconductor device according to claim 28, 10 wherein the single Sn-Bi alloy layer (2) is a deposited single Sn-Bi alloy layer (2), deposited by plating.
34. A semiconductor device according to claim 28, wherein the Sn-Bi alloy layer (2) has a thickness of about 10 / im. 1535. A semiconductor device according to claim 28, which is a thin small outline package.
36. A semiconductor device according to claim 28, wherein the lead (1) is adapted for connection to a Pb-free solder (5). 2037. A semiconductor device according to claim 28, wherein the lead (1) is adapted for connection to a Pb-free solder (5) of an Sn-Ag-Bi alloy.
38. A. semiconductor device according to claim 28, wherein the lead (1) is adapted for connection to a Pb-free 25 solder (5) of an Sn-Ag-Bi-Cu alloy.
39. A semiconductor device with a lead (1) which is made from a lead frame, wherein a layered structure which consists of a single Sn-Bi alloy layer (2), which comprises from 1 to 5 wt% Bi, is formed on the lead (1), the single Sn-Bi alloy layer (2) being provided as the single Sn-Bi alloy layer (2) prior to forming a soldered connection of the lead (1).
40. A semiconductor device according to claim 39, wherein the lead (1) is a Cu alloy lead.
41. A semiconductor device according to claim 39, wherein the lead (1) is an Fe-Ni alloy lead.
42. A semiconductor device according to claim 41, wherein a Cu layer (3) is present between the Fe-Ni alloy lead (1) and the Sn-Bi alloy layer (2).
43. A semiconductor device according to claim 39, wherein a Cu layer (3) is present between the lead {1) and the Sn-Bi alloy layer (2).
44. A semiconductor device with a lead (1) which is made from a lead frame, wherein a layered structure which consists of a single Sn-Bi alloy layer (2), which comprises from 1 to 5 wt% Bi, is formed directly on the lead (1), the single Sn-Bi alloy layer {2) being provided as the single Sn-Bi alloy layer (2) prior to forming a soldered connection of the lead (1).
45. A semiconductor device with a lead (1) which is made from a lead frame, wherein the lead (1) includes an Sn-Bi alloy layer (2) comprising 1 to 5 wt% Bi as a surface layer, said Sn-Bi alloy layer (2) being provided as said SnBi alloy layer (2) prior to forming a soldered connection of the lead (1).
46. A semiconductor device according to claim 45, 5 wherein the lead (1) is an Fe-Ni alloy lead.
47. A semiconductor device according to claim 46, wherein a Cu layer (3) is present between the Fe-Ni alloy lead (1) and the Sn-Bi alloy layer (2).
48. A semiconductor device according to claim 45, 10 wherein a Cu layer (3) is present between the lead (1) and the Sn-Bi alloy layer (2).
49. A semiconductor device according to claim 45, wherein the lead (1) is a Cu alloy lead.
50. A semiconductor device with a lead (1) which 15 is made from a lead frame, wherein an Sn-Bi alloy layer (2), which comprises from 1 to 5 wt% Bi, is formed directly on the lead (1) as a surface layer, said Sn-Bi alloy layer (2) being provided as said Sn-Bi alloy layer (2) prior to forming a soldered connection of the lead {1). 2051. A semiconductor device according to claim 39, wherein the single Sn-Bi alloy layer (2) is a deposited single Sn-Bi alloy layer (2).
52. A semiconductor device according to claim 44, wherein the single Sn-Bi alloy layer (2) is a deposited 25 single Sn-Bi alloy layer (2).
53. A semiconductor device according to claim 45, wherein the single Sn-Bi alloy layer (2) is a deposited SnBi alloy layer (2), deposited by plating.
54. A semiconductor device according to claim 50, wherein the single Sn-Bi alloy layer (2) is a deposited SnBi alloy layer (2), deposited by plating.
55. A method of making a semiconductor device : according to any one of claims 29 to 54, wherein said Sn-Bi alloy coating layer (2) is formed by plating.
56. A method of making a semiconductor device according to any one of claims 29 to 54, wherein said Sn-Bi alloy coating layer (2)’ is formed by dipping.
57. A method of making a semiconductor device according to any one of claims 29 to 54, wherein said Sn-Bi alloy coating layer (2) is formed by any one of deposition by evaporation, roller coating and metal powder application.
58. A method of bonding a semiconductor device having an electrode (1), by means of a lead-free solder (5), characterized in that prior to bonding to the solder (5) the electrode (1) has a coating of a Sn-Bi alloy containing 1 wt% to 5 wt% Bi.
59. A method according to claim 58, wherein the electrode (1) has a Cu layer (3) under the Sn-Bi alloy coating layer (2).
60. A method according to claim 58 or 59, wherein the electrode {1) is made of Cu or a Cu layer, or of an FeNi alloy.
61. A method according to claim 58 or 59, wherein the solder (5) is a Sn-Ag-Bi alloy.
62. A method according to claim 61, wherein the solder (5) comprises Sn as a primary component, 5 wt% to 25 5 wt% Bi, 1.5 wt% to 3 wt% Ag and up to 1 wt% Cu.