Cathode ray tube

MYPI1999000649A0Inactive Publication Date: 2000-03-19SAMSUNG ELECTRONICS DEVICES CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1999000649
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1998-09-19
Filing Date
1999-02-24
Publication Date
2000-03-19
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Cathode ray tubes face challenges in reducing deflection power consumption and magnetic field leakage while maintaining image resolution and strength against external stress, as existing designs either compromise image quality or funnel strength.

Method used

A cathode ray tube with a funnel that has a deflection yoke mounting portion with a cross-sectional ratio of 1.0 < rh/rv < 1.3, where rh is the horizontal diameter and rv is the vertical diameter, gradually changing from a circular to a non-circular shape to optimize deflection power usage and strength.

Benefits of technology

The design effectively reduces deflection power consumption and prevents magnetic field leakage while maintaining image quality and strength against external pressure, making it suitable for flat-panel CRTs with wide-angle deflections.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A CATHODE RAY TUBE INCLUDES A RECTANGULAR PANEL (3) ON WHICH A PHOSPHOR SCREEN (1) IS FORMED, A NECK (11) IN WHICH AN ELECTRON GUN ASSEMBLY (9) FOR EMITTING THREE ELECTRON BEAMS IS DISPOSED, AND A FUNNEL (7) FORMED CONTIGUOUS TO BOTH THE NECK (11) AND THE PANEL, AND HAVING A DEFLECTION YOKE MOUNTING PORTION ON WHICH A DEFLECTION YOKE (5) IS MOUNTED. THE CROSS SECTION OF THE DEFLECTION YOKE MOUNTING PORTION FULFILLS THE FOLLOWING CONDITION AT THE PANEL SIDE END OF THE DEFLECTION YOKE MOUNTING PORTION.WHERE RH IS A DIAMETER OF THE FUNNEL (7) DIRECTED TO A DIRECTION OF A LONG AXIS OF THE PANEL, AND RV IS A DIAMETER OF THE FUNNEL (7) DIRECTED TO A DIRECTION OF A SHORT AXIS OF THE PANEL.(FIG 2)
Need to check novelty before this filing date? Find Prior Art

Description

The present invention relates to a cathode ray tube (CRT) and more particularly, to a cathode ray tube capable of reducing the deflection power consumption.(b) Description of the Related ArtA CRT is a device for displaying image on a screen by vertically and horizontally deflecting electron beams generated from an electron gun and landing the deflected electron beams onto the phosphor layers formed on the screen. The deflection of the electron beam is controlled by a deflection yoke mounted on an exterior surface of a funnel of the CRT and which forms vertical and horizontal magnetic fields. The CRTs are generally employed for color televisions (TVs), monitors and high definition televisions(HDTV). And with the increasing use of the CRTs, there is a need to reduce the length of the CRT for increasing the brightness of the displayed image and for reducing the size of the final products, such as TVs, monitors and HDTVs.When reducing the length of the CRT, the electron beams should be deflected with wide-angles, and the deflection frequency and current supplied to the deflection yoke should be increased for the wide-angle deflections of the electron beams. As the deflection frequency and current increases, the ί 4>deflection magnetic field tends to leak to the outside of the cathode ray tube and the power consumption increases.In order to decrease the deflection power and the magnetic field leakage at the same time, it is conventionally preferable to decrease the neck diameter of the cathode ray tube and the outer diameter of the funnel near the neck side on which the deflection yoke is mounted, so that the deflection field efficiently acts on the electron beams. However, when the neck diameter simply decreases, there are disadvantages that the resolution of the image deteriorates due to the reduced diameter of the electron gun, and the outer electron beams are likely to be bombard the inner wall of the funnel, thus results in that the bombarded electron beams are not properly landed on the phosphor layer of the screen.In order to solve these problems, U.S. patent No. 3,731,129 discloses a funnel having a wider peripheral portion sealed to the periphery of the panel, and a deflection portion whose cross-sectional configuration gradually varies from a rectangular shape substantially similar to that of the rectangular image produced on the panel to a circular shape. Thereby, the vertical and horizontal coils of the deflection yoke are closely located to the passage of the electron beams, and deflect the electron beams with reduced deflection power and without bombarding the electron beams to the inner wall of the funnel. However, the funnel does not have enough strength to endure against external stress, such as pressure, thus the funnel have to be designed to have a circular or round section.< ' . 3 ί*Meanwhile Japanese Laid Open Patent 9-306388 corresponding to U.S.Patent No. 5,763,995 discloses a funnel, whose cross section of the exterior surface at the neck side is changed from a circular shape to a non-circular shape which has a maximum diameter along a direction (diagonal direction) other than the horizontal direction and the vertical direction. In addition, the funnel is designed to fulfill the following condition.0.3 < AHV / L < 0.6 where L is a length of the maximum diameter, and AHV is a sum of ΔΗ and AV, and ΔΗ is a difference between L and a horizontal diameter of section io of the funnel, and Δν is a difference between L and a vertical diameter of the section of the funnel. However, the funnel is defined or configured by three variables, ΔΗ, Δν and L. Thus, for example, even though AH is set to a fixed value, two variables are not fixed or defined. As a result, it is difficult to design the funnel having the optimum configuration and enough strength against external stress.Meanwhile, Japanese Laid Open Patent 10-149785 discloses a funnel, whose cross section of the exterior surface is a non-circular shape which has a maximum diameter along a direction (diagonal direction) other than the horizontal direction and the vertical direction. In addition, when the aspect ratio of a screen is M:N, the cross section of the funnel is designed to fulfill the following condition.(M+N) / (2(M2+N2)1 / 2) < (SA + LA) / (2DA) < 0.86 where SA is a vertical diameter of the external surface of the funnel,• t and LA is a horizontal diameter of the external surface of the funnel, and DA is the maximum diameter of the external surface of the funnel. However, the funnel is also defined or configured by three variables, SA, LA and DA. Thus, it is also difficult to design the funnel having the optimum configuration and enough strength against external stress.SUMMARY OF THE INVENTIONAccordingly, the present invention is directed to a cathode ray tube which substantially obviates one or more of the problems due to the limitations and disadvantages of the related art.An object of the present invention is to provide a cathode ray tube capable of minimizing the power consumption and preventing deflection magnetic fields from leaking to the outside of the cathode ray tube.Another object of the present invention is to provide a cathode ray tube including a funnel having increased strength against external stress.Further object of the present invention is to provide a cathode ray tube particularly suitable for flat-panel cathode ray tubeTo accomplish these and other advantages, the cathode ray tube includes a rectangular panel on which a phosphor screen is formed, a neck in which an electron gun assembly for emitting three electron beams is disposed, and a funnel formed contiguous to both the neck and the panel, and having a deflection yoke mounting portion on which a deflection yoke is mounted. The cross section of the deflection yoke mounting portion fulfills the following condition at the panel side end of the deflection yoke mounting portion.1.0 < rh / rv < 1.3 where rh is a diameter of the funnel directed to a direction of a long axis of the panel, and rv is a diameter of the funnel directed to a direction of a short axis of the panel.The objectives and other advantages of the invention will be realized and attained by the structure particularly pointed out in the written description and claims as well as the appended drawings. It is also to be understood that both the foregoing general description and the following detailed description are io exemplary and explanatory and are intended to provide further explanation of the invention as claimed.BRIEF DESCRIPTION OF THE DRAWINGSThe accompanying drawings, which are included to provide a further understanding of the invention and are incorporated in and constitute a part of this specification, illustrate a particular embodiment of the invention and, together with the description, serve to explain the principles of the invention.In the drawings:Fig. 1 is a perspective view of a cathode ray tube according to an embodiment of the present invention;Fig. 2 is a sectional view of a cathode ray tube according to an embodiment of the present invention, taken along a diagonal line of a panel of the cathode ray tube;Fig. 3 is a schematic diagram for illustrating the cross section of the funnel at the neck side according to an embodiment ofthe present invention;Fig. 4 is a schematic diagram for illustrating the cross section of the funnel, taken along a position at which a deflection yoke is mounted according to an embodiment of the present invention;Fig. 5 is a graph for illustrating the change of rh / rv value according to the distance from the neck;Fig. 6 is a graph for illustrating the relation of the deflection power and the rh / rv value; and io Fig. 7 is a graph for illustrating the relation ofthe magnetic field leakage and the rh / rv value.DETAILED DESCRIPTION OF THE INVENTIONReference will now be made in detail to the preferred embodiments of the present invention, examples of which are illustrated in the accompanying drawings.As shown in Figs 1 and 2, a cathode ray tube is a vacuumed envelope which is formed with a substantially rectangular panel 3, a funnel 7 formed contiguous to the panel 3, and a cylindrical neck 11 formed contiguous to the small-diameter end portion of the funnel 7. A phosphor screen 1 is formed on the inner surface ofthe panel 3. A deflection yoke 5 is mounted on the funnel 7 near the neck 11, and an electron gun assembly 9 for emitting three electron beams is disposed in the neck 11. The three electron beams emitted from the electron gun assembly 9 are deflected by horizontal and vertical deflection fields generated by the deflection yoke 5. The deflected electron beams reach the phosphor screen 1 through a shadow mask 13 mounted on the inner surface of the panel 3, and display a color image.In order to effectively reduce the deflection power, the exterior surface of the funnel 7, on which the deflection yoke 5 is mounted, is designed to have a circular section at the position near the neck 11, and the circular section is gradually deformed from the neck side to the panel side to have a non-circular section having a maximum diameter along a diagonal direction other than the io horizontal and vertical directions, for example, a rectangular section.In addition, the funnel 7 is designed so that the cross section of the funnel 7 fulfills the following condition at the panel side end of the deflection yoke 5.1.0 < rh / rv <1.3 where rh is a diameter of the funnel to the direction of the long axis (horizontal diameter), and rv is a diameter of the funnel to the direction of the short axis (vertical diameter).More preferably, the rh / rv value gradually decreases from the panel side to the neck side, and sets to 1.0 at the position at which the funnel 7 connects with the neck 11. Fig.3 is a schematic diagram for illustrating the cross section of the funnel 7 at the neck side. As shown in Fig. 3, the diagonal diameter (rd) of the funnel directed to the direction of the diagonal axis (d) equals to the horizontal diameter (rh) of the funnel directed to the direction ofthe long axis (h) and the vertical diameter (rv) of the funnel directed to the direction of the short axis (v). Thus, the cross section has a circular shape.Fig. 4 is a schematic diagram for illustrating the cross section of the funnel 7 at which the deflection yoke 5 is mounted. As shown in Fig. 4, at the5. position on which the deflection yoke 5 is mounted, the horizontal diameter (rh) and the vertical diameter (rv).decrease to be shorter than the diagonal diameter (rd). Thus, the cross section has a rectangular shape.The configuration of the funnel 7 of the present invention is derived by simulation tests to reduce the deflection power and to increase the BSN(beam io strike neck) characteristics of the funnel 7and the strength against the external pressure.More preferably, the funnel 7 is designed so that the cross section of the funnel 7 fulfills the following condition at the position of the deflection reference line (R / L).1.1 < rh / rv <1.2 where rh is a diameter of the funnel to the direction of the long axis, and rv is a diameter of the funnel to the direction of the short axis. As shown inFig. 2, the reference line (R / L) is defined by elongating the trajectories of the outer electron beams which are escaped from the effect of the deflection yoke 5, and by calculating the crossing point of the elongated trajectories. Thus, the reference line formed at the middle and center portion of the deflection yoke 5.Fig. 5 is a graph for illustrating an example of the funnel 7 according to the present invention, and shows the change of rh / rv value of the funnel 7 along-- -9 the tube axis of the funnel 7. In the funnel I shown in Fig. 5, the rh / rv value at the reference line is 1.14, and the exterior surface of the funnel 7 is convexed to the tube axis before the reference line(R / L), and the exterior surface is concaved to the tube axis after the reference line(R / L),Fig.6 is a graph for illustrating the relation of the deflection power and the rh / rv value. As shown in Fig.6, as the rh / rv value is between 1.0 and 1.3, the deflection power of the cathode ray tube gradually decreases. In addition, as shown in Fig.7, when the rh / rv value is less than 1.3, the magnetic field leakage is maintained below a predetermined value (horizontal line in Fig.7).io The present invention is particularly suitable for wide-angle deflection cathode ray tube in which the deflection angle is 90° or 100°. In detail, the rh / rv value is preferably maintained between 1.0 and 1.3 when the deflection angle is 90°, and the rh / rv value is preferably maintained between 1.0 and 1.25 when the deflection angle is 100°.By configuring the shape of the funnel according to the present invention, the cathode ray tube of the present invention has enough strength against the external pressure and consumes less deflection power, and the magnetic field leakage is prevented.It will be apparent to those skilled in the art that various modifications and variations can be made in the present invention without departing from the spirit or scope of the invention. Thus, it is intended that the present invention cover modifications and variations of this invention provided they come within the scope of the appended claims and their equivalents. This application is based on application No. 98-38811 filed in Korean Industrial Property Office on September 19, 1998, the content of which is incorporated herein by reference.

Claims

1. A cathode ray tube comprising: a rectangular panel (3) on which a phosphor screen (1) is formed; a neck (11) in which an electron gun assembly (9) for emitting three electron beams is disposed; and a funnel (7) formed contiguous to both the neck (11) and the panel, and having a deflection yoke mounting portion on which a deflection yoke (5) is mounted, wherein a cross section of the deflection yoke mounting portion fulfills the following condition at the panel side end of the deflection yoke mounting portion. 1.0 < rh / rv < 1.3 where rh is a diameter of the funnel (7) directed to a direction of a long axis of the panel, and rv is a diameter of the funnel (7) directed to a direction of short axis of the panel.

2. The cathode of ray tube according to claim 1, wherein the rh / rv is value gradually decreases from the panel side to the neck side.

3. The cathode of ray tube according to claim 2, the cross section of the funnel (7) fulfills the following condition at a deflection reference line. 1.1 < rh / rv < 1.2 where rh is a diameter of the funnel (7) directed to the direction of the long axis, and rv is a diameter of the funnel (7) directed to the direction of the short axis.

4. The cathode of ray tube according to claim 1, wherein the cross section of the funnel (7) fulfills the following condition at a deflection reference line. 1.1 < rh / rv < 1.2 where rh is a diameter of the funnel (7) directed to the direction of the long axis, and rv is a diameter of the funnel (7) directed to the direction of the short, axis.