Phosphine compound
Patent Information
- Application Number
- MYPI1999000973
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1998-03-16
- Filing Date
- 1999-03-16
- Publication Date
- 1999-09-16
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing methods for manufacturing phosphine compounds used in catalyst systems for olefin carbonylation are hindered by the use of toxic, highly reactive, and flammable secondary phosphines, resulting in low yields and significant waste production.
A method involving the reaction of a compound with an organometallic compound to form an intermediate, which is then reacted with a halophosphine to produce a phosphine compound of the formula (R3-C)2P-L1-X-L2-P-(C-R3)2, using more benign materials and reducing waste, preferably in the presence of a complexing agent like tetramethylenediamine.
This method achieves high yields and minimizes waste production, using more benign materials and improving the efficiency of phosphine compound synthesis for catalyst systems in olefin carbonylation.
Abstract
Description
A method of manufacturing a compound of general formula (R3-C)2P-L1-X-|_2-P-(C-R3)2, in which each R is independently a pendant, optionally substituted, organic group through which the group is linked to tertiary carbon atom C; L1, L2are independently a linking group selected from an optionally substituted lower alkylene chain connecting the respective phosphorus atom to the group X and X is a bridging group comprising an optionally substituted aryl moiety to which the phosphorus atoms are linked on available adjacent carbon atoms comprisesi) reacting together a compound of formula H-L1-X-|_2-H with an organometallic compound to form an intermediate compound of formula M-L1-X-|_2-M, where M is an alkali metal atom, ii) reacting said intermediate compound with a compound of formula (R3-C)2P-A, where A is a halogen atom, to form said compound of general formula (R3-C)2P~L1-X-|_2-P-(C-R3)2M is preferably lithium, potassium or sodium and the intermediate compound may be isolated or not. The reaction (i) may advantageously be carried out in the presence of a complexing agent such as tetramethyethylenediamine.Phosphine CompoundThe present invention relates to a phosphine compound which is useful as a component of a catalyst system which may be used in the carbonylation of olefins, and in particular to a method of manufacturing such phosphine compounds.WO 96 / 19434 discloses a process for the carbonylation of ethylene and a catalyst system for use therein. The catalyst system described in that document comprises a bidentate phosphine of general formula (R3-C)tP-L’-X-L2-P-(C-R3)2, in which each R is independently a pendant, optionally substituted, organic group through which the group is linked to tertiary carbon atom C. I'. L / are independently a linking group selected from an optionally substituted lower alkylene chain connecting the respective phosphorus atom to the group X and X is a cndqmg group comprising an optionally substituted aryl moiety to which the phosphorus atoms are linked on available adjacent carbon atoms. One example of such a bidentate pnosphine is bis (di-'butyl phosphino)-o-xylene (also known as 1,2,bis(di-t-butylphcsohmomethyl)benzene).Such catalysts may be made by mixing the phosphine ligand with a suitable source of palladium such as palladium acetate. WO 96 / 19434 describes the preparation of one form of the ligand via the phosphonium salt produced from the reaction of the appropriate secondary phosphine with the corresponding aromatic dihalide. In the preferred form of the phosphine ligand in WO 96 / 19434, R is a lower alkyl group, in particular methyl. A problem with manufacturing this ligand by the route described is that the secondary phosphine which is used (e.g. di-'butyl phosphine) is toxic, highly reactive, smelly and flammable. We have also found that the reaction is low yielding and converts some of the di-'butyl phosphine to a non-reclaimable waste product which must be disposed of.Al-Salem et al in Journal of the Chemical Society (Dalton) 1979 page 1980 describes making 1,5 bis(di-t-butylphosphino)pentane by reacting lithium metal with1,5-dibromopentane and then phosphorylating the resulting lithiated intermediate with t-butylchlorophosphine. This method, for forming a phosphine of an alkyl compound, starts from the halogenated alkyl compound. Alkyl halides typically require considerable care during storage and use and may be very unpleasant to use. Therefore using this method of making the phosphine using the non-halogenated alkyl compound as a starting material would require an extra step of converting first to the alkyl halide.We have now found that phosphine ligands of the type described in WO 96 / 19434 may be prepared by a high yielding route using more benign materials which produce less waste phosphorus product than the route described in WO 96 / 19434.According to the invention, a method of manufacturing a compound of general formula (R3-C)2P-L1-X-L2-P-(C-R ,X . m which each R is independently a pendant, optionally substituted, organic group through which the group is linked to tertiary carbon atom C; L1, L2are independently a linking group selected from an optionally substituted lower alkylene chain connecting the respective phosphorus atom to the group X and X is a bridging group comprising an optionally substituted aryl moiety to which the phosphorus atoms are linked on available adjacent carbon atoms comprises the steps ofi) reacting together a compound of formula H-L1-X-L2-H with an organometallic compound to form an intermediate compound of formula M-l?-X-L2-M, where M is an alkali metal atom, ii) reacting said intermediate compound with a compound of formula (R3-C)2P-A, where A is a halogen atom, to form said compound of general formula (R3-C)2P-L1-X-L2-P-(C-R3)2The compound of general formula (R3-C)2P-L1-X-L2-P-(C-R3)2may be useful as a component of a catalyst compound. In particular WO 96 / 19434 describes the use of such compounds as bidentate ligands which, when used together with a Group VIII metal such as palladium, are effective catalysts for the carbonylation of olefins.The pendant, optionally substituted organic groups, R may be independently selected from a wide range of components. Preferably, the pendant groups are optionally substituted lower alkyl, e.g. C, .a, and may be branched or linear.Particularly preferred is when the organic groups, R, when associated with their respective carbon atom, form composite groups which are at least as sterically hindering as fert-butyl. Steric hindrance in this context is as discussed at page 14 et seq of Homogeneous Transition Metal Catalysis - A Gentle Art, by C Masters, published by Chapman and Hall, 1981. In one preferred embodiment, the organic groups R are all methyl groups, i.e. a preferred form of R3-C group is a tertiary butyl group.The linkinq qrouos, L1and L2, are independently selected from an optionally substituted, particularly lower alkyl, e.g. C, to C„, substituted, lower alkylene, e.g. C, to C4chain. Especially preferred is when both L’ and L2are methylene.The bridging group X is an aryl moiety, e.g. a phenyl group, which may be optionally substituted, provided that the two phosphorus atoms are linked to adjacent carbon atoms, e.g. at the 1 and 2 positions on the phenyl group. Optional substitution of the aryl moiety may be by other organic groups, e.g. alkyl, particularly Ο,.β, aryl, alkoxy, carbalkoxy, halo, nitro, trihalomethyl and cyano. Furthermore, the aryl moiety may be a fused polycyclic group, e.g. naphthalene, biphenylene or indene.Examples of compounds which may advantageously be made by the method according to the invention are bis (di-fert-butyl phosphino) - o - xylene (also known as 1,2 bis (di-tert-butylphosphinomethyl) benzene), bis (di-t-neopentyl phosphino) - o - xylene and bis 1, 2 (di-tert-butyl phosphino) naphthalene.The reaction of a compound of formula H-L1-X-L2-H with a basic organometallic compound of formula RmM to form an intermediate compound of formula M-L1-X-L2-M, where M is an alkali metal atom, may be carried out by various means which are known in the art of organometallic chemistry. For example such metallation methods are described by Wilkinson et al in Comprehensive Organometallic Chemistry at page 54; and by Lambert et al in Preparative Polar Organometallic Chemistry.The organometallic compound may comprise a compound of formula Rm-M, where Rmis an organic group which tends to withdraw electrons from the metal atom M. Suitable organic groups include aromatic or aliphatic groups, especially alkyl groups, which may be substituted. Lower alkyl groups have been found to be particularly suitable, for example preferred Rmcompounds include n-butyl, t-butyl, sec-butyl, methyl or pentyl.M may be any suitable alkali metal which forms a polar organometallic group with Rm. Suitable metals include those of Group IA, e.g. sodium, potassium or lithium. When M comprises K or Na the Rm-M metallating agent is preferably generated in situ by an exchange mechanism, e.g. by the reaction between Rm-Li and potassium or sodium t-butoxide as described by Lochman et al in Tetrahedron Letters No. 2 pages 257 - 262 (1966). Preferred metallating compounds are butyl lithium, butyl sodium and butyl potassium, the latter compounds preferably being formed in situ by the reaction of butyl lithium with potassium or sodium t-butoxide.Alternative organometallic compounds are also known in the art and may comprise Me3SiCH2K, alkali amides MNH„ preferably used in liquid ammonia, lithium dialkylamides e.g.. lithium diisopropylamide (LDA), lithium, sodium or potassium metals, metal hydrides e.g. KH in the presence of co-ordinating compounds.The reaction between RmM and H-l_'-X-i_z-H may be carried out in the presence of a solvent. Any solvent used must not contain any component which reacts with the intermediate compound, and suitable such solvents will be well known to the skilled chemist. Favoured solvents include dry alkyl ethers e.g. diethyl ether, methyl t-butyl ether, di(n-propyl) ether; tetrahydrofuran (THF), and hydrocarbons such as hexane and heptane.The reaction between FCM and H-L’-X-L2-H may be beneficially carried out in the presence of a basic compound which is capable of forming a complex with the metal. A preferred complexing agent is tetramethylethylenediamine (TMEDA). The presence of TMEDA is greatly preferred when the metallating agent is alkyl lithium or alkyl sodium. When alkyl potassium (or alkyl lithium / potassium t-butoxide mixture) is used, we have found that the reaction proceeds satisfactorily in the absence of TMEDA.The mole ratios of metallating agent :H-L1-X-|_2-H are preferably in the range 1:1 to 10:1, more preferably at least 1.5:1. The preferred ratio depends upon the nature of the metallating agent used, for example when alkyl lithium is used a ratio of R-Li: H-L1-X-L2-H of 3:1 may be preferred. Higher ratios may be preferred to encourage the formation of di-substituted product rather than mono-substituted compounds.A preferred ratio of RmM : complexing agent is in the range 1:1 - 4:1, especially preferred is a ratio of about 1:1 to about 2:1.It is preferred to conduct the metallation reaction between RmM and H-L1-X-|_2-H at a temperature in the range -20 to 150 °C, more preferably at room temperature or above. The optimum temperature and reaction time depends upon the identity of the reactants, in particular upon the alkali metal which is used. For example we have found, using o-xylene as the compound to be metallated that when alkyl lithium is used, the reaction proceeds well at room temperature (i.e. about 20 - 22 °C) whereas reactions using alkyl sodium and potassium are preferably conducted at about 60, (e.g. 50 - 70 °C) and about 80 °C (e.g. 70 - 90 °C) respectively.The intermediate compound. M-L'-X-U-M may be isolated from the reaction mixture prior to conducting the reaction between M-L’-X-L2-M and the compound of formula (R3-C)2P-A. However isolation of the intermediate may not be necessary and the reaction has been found to proceed very satisfactorily when the intermediate is not isolated. When the intermediate product M-L -X-L'-M can be separated relatively easily, for example if it is in a different physical form trom tne starting materials, then it may be advantageous to isolate the intermediate form the reaction mixture to encourage the formation of more intermediate. We have found that the reaction mixture may contain partially reacted compounds of formula M-L -x-L-H which may be reacted to completion by the addition of further quantities of R~M ana complexing agent if used.The phosphorylation reaction between the intermediate product M-L1-X-L2-M and the halophosphine (R3-C).P-A is also earned out in the presence of a solvent and similar solvents to those used for the metallation are suitable, e.g. ethers, C5+ alkanes and petroleum ethers. We have found that, when the metal used is potassium, the reaction is favoured when diethyl ether is used as a solvent for the phosphorylation reaction, although an alkane e.g. heptane, may be preferred for the metallation reaction. Also, even when sodium or lithium is used as the metal species, it may be beneficial to use a different solvent for the phosphorylation from that used for the metallation, e.g. to enable higher temperatures to be used in one reaction yet allow an easy separation of the solvent from the product of the second reaction.The phosphorylation reaction may be conducted at elevated temperatures, e.g. at temperatures of 60°C or greater, but it is preferred to conduct the reaction at room temperature or below, e.g. at -20 to 25 °C.The compound of general formula (R3-C)2P-L1-X-L2-P-(C-R3)2may be isolated from the reaction mixture by distilling off the excess solvent, preferably under vacuum and then extracting the product compound into a solvent, e.g. methanol, from which it may be precipitated.The invention will be further described, by way of example only, below. In all reactions, the reactants and apparatus used were prepared to allow the reaction to proceed in anhydrous and anaerobic reaction conditions.Example 1Λ / ,Α / ,Α / ',Λ / '-Tetramethylethylenediamine (0.79cm3, 5.25 mmol) was added to a stirred solution of n-butyllithium (2.10cm3, 2.5 / Vf in hexane, 5.25 mmol) in heptane (15cm3) under an atmosphere of nitrogen After five minutes, ortho-xylene (0.26cm3, 2.10mmol) was added slowly. A orange-brown precipitate formed after leaving the solution stirring at room temperature for 96 hours.Di-fert-butylchlorophosphine (1 40cm3, 7.37 mmol) was added, then at room temperature the solution was left to stir until the colour disappeared.A sample of the reaction mixture was analysed by31PfH} NMR and the conversion to bis (di-fert-butyl phosphino)-o-xylene and to the mono-substituted analogue, was determined. The results are shown in Table 1.Examples .2.-.5The experimental procedure of Example 1 was repeated but varying the reactant ratios and reaction conditions as shown in Table 1.Example 9The experimental procedure described above was repeated using a ratio of butyllithium:TMEDA: o-xylene of 4 : 4 : 1 , a temperature of 25°C and a reaction time of 48 hrs, but the product of the reaction between the butyl lithium and o-xylene ITMEDA was filtered to separate the brown solid from the red liquid. Each was then reacted separately with di'butylchlorophosphine and the conversion to bis (di-fert-butyl phosphino) - o - xylene and to the mono-substituted analogue, was determined. The results are shown in Table 2.Examples .1.0.--13 n-Butyllithium (11 mmol) was added dropwise to a well-stirred solution of o-xylene (0.6 ml, 5 mmol) and potassium fert-butoxide (1.2g 11 mmol) in heptane (25 ml). The reactions were stirred (and sometimes heated) for a predetermined length of time (see Table 3).The system was cooled by placing it in an ice bath and di-feri-butylchlorophosphine (1.87 ml, 11 mmol) was then slowly added to the flask. The system was allowed to stir until all of the colour had disappeared. Diethyl ether (50 cm3) was added to the flask to ensure that all of the phosphines produced were dissolved. A sample of the resulting solution was collected in a sealed NMR tube and analysed by31P fH} NMR.Table. 1Example Ratio butyllithium TMEDA: o-xylene TCC time (hrs) % conversion to disubstituted product (re: o-xylene) ratio di: mono product 1 2:21 25 96 32 0.7 2 2.5 . 2 5 . 1 25 96 31 0.77 3 2.5:2.5 t 60 12 32 1.60 4 2.5 . 2.5 1 40 6 39 1.08 5 2.5 : 2.5 . 1 60 6 34 0.85 6 3:2.1 60 6 57 1.50 7 4:4:1 25 96 57 1.86 8 4 :2: 1 25 96 69 2.3Table 2% conversion (mono) % conversion (di) solid 5 38 liquid 30 8Table 3Example Ratio BuLi / BuOK / Xylene Potassiation reaction time and temperature (°C) % Conversion di substituted product 10 2.2 : 2.2 . 1 1 hour, room temp. (RT) 40 11 3:3:1 1 hour at R T + 1 hr @ 60 °C 45 12 2.2 : 2.2 : 1 1 hour @ 80 °C 44 13 3:3:1 1 hour @ 80 °C 49Example. .14O-xylene (3.3 cm3, 270 x 10’2mol) was added by syringe to a suspension of potassium t-butoxide (6.6 g, 5.88 x 10'2mol) in 40 / 60 petroleum ether (150 cm3). 42 cm3of a 1.4 M solution of butyl lithium in hexane was added to the ether mixture, with cooling. The mixture was stirred overnight to complete the reaction which resulted in an orange-red solid which was the dipotassio-o-xylene. The mixture was filtered and the solid washed with further petroleum ether.The dipotassio derivative was then suspended in diethyl ether (150 cm3) at -78 °C and di-t-butylchlorophosphine (10 g, 5.54 x 10'2mol) was added by syringe. The mixture was stirred for an hour, brought slowly to room temperature and then filtered. The filtrate was hydrolysed by addition of 1 cm3of degassed water and dried. The yield (based on o-xylene) was 94%. Analysis by31P {’H} NMR showed that the yield of a,a'bis(dit-butylphosphino)o-xylene was 80%, whilst that of the monophosphine was 10%.Example 15Potassium-tert-butoxide (3.99 g, 35.6 mmol), heptane (150 cm3) and o-xylene (1.47 cm3, mmol) were added to a 500 ml round bottomed flask. To this stirred solution n-butyllithium (14.45 cm3. 36.1 mmol, 2.5M in hexane) was added slowly and the flask heated to 80 °C for 1 hour. An orange / red precipitate formed which was separated by filtration and washed with pentane (3 x 100cm3) before being resuspended in diethyl ether (100 cm3) which had been pre-cooled to -20°C. To this solution maintained at -20°C was added di-f-butylchlorophosphine (4.58 cm3, 24.1 mmol) and the reaction allowed to warm to room temperature before being stirred overnight. The in-situ reaction yield of a,a'bis(dit-butylphosphino)o-xylene as determined by31P NMR was 64%.Example i_6The reaction described in Example 15 was repeated except that the orange-red precipitate of dipotassio-o-xylene was resuspended in 100 cm3of diethyl ether which had been pre-cooled to 0 °C and the solution was maintained at 0°C while di-f-butylchlorophosphine (4.58 cm3, 24.1 mmol) was added. The reaction was allowed to warm to room temperature before being stirred overnight. The in-situ reaction yield of a,a'bis(dit-butyiphosphino)o-xylene as determined by31P NMR was 74.9%.Example..1.7.The reaction described in Example 15 was repeated except that the orange-red precipitate of dipotassio-o-xylene was resuspended in 100 cm3of diethyl ether at room temperature and the solution was maintained at room temperature while di-f-butylchlorophosphine (4.58 cm3, 24.1 mmol) was added. The reaction was stirred overnight. The in-situ reaction yield of a,a'bis(dit-butylphosphmoio-xylene as determined by31P NMR was 75.5%.Example 1.8Sodium-ferf-butoxide (17 22 a. 130 mmol), W, / V, / V' / V-Tetramethylethylenediamine (27.1 cm3, 180 mmol), heptane ί1GO emu and o-xylene (7.32 cm3, 60 mmol) were added to a 1 litre round bottomed flasx To this stirred solution n-butyllithium (72.0 cm3, 180 mmol, 2.5M in hexane) was added siowiv ana the flask heated to 60 °C for 2 hours. An orange precipitate formed which was separated by filtration and washed with pentane (100cm3) before being resuspended m pentane (100 cm3). To this was added di-f-butylchlorophosphine <22.75 cnr. 120 mmol) and the reaction stirred at room temperature overnight. T*e reaction was quenched by the addition of degassed / deionised water (50 cm i when two dear layers formed and the pentane layer (upper layer) was isolated. The solvent was removed in-vacuo and the product purified by washing with cold methanol (-10C). Yield (20.0g, 84.6%).-11 8. A catalyst suitable for catalysing the carbonylation of ethylene comprising compound of general formula (R3-C)2P-L’-X-L2-P-(C-R3)2 prepared by a method as claimed in claim 1, and palladium or a compound thereof.9. A method as claimed in any one of claims 1 to 7, substantially as 5 hereindescribed with reference to any one of the Examples.10. A catalyst as claimed in claim 8, substantially as hereindescribed with reference to any one of the Examples.
Claims
1. A method of manufacturing a compound of general formula (R3-C)2PL1-X-L2-P(C-R3)2, in which each R is independently a pendant, optionally substituted, organic group through which the group is linked to tertiary carbon atom C;L1, L2 are independently a linking group selected from an optionally substituted C1-C4 alkylene chain connecting the respective phosphorus atom to the group X and X is a bridging group comprising an optionally substituted aryl moiety to which the phosphorus atoms are linked on available adjacent carbon atoms comprising: i) reacting together a compound of formula H-L1-X-Lz-H with an organometallic compound to form an intermediate compound of formula M-U-X-IAm, where M is an alkali metal atom, ii) reacting said intermediate compound with a compound formula (R3C)2P-, where A is a halogen atom, to form said compound of general formula (R3-C)2P-L1-X-L2-P-(C-R3)2.
2. A method as claimed in claim 1, wherein M is a Group 1A metal selected from sodium, potassium or lithium.
3. A method as claimed in claim 1 or 2, wherein the organometallic compound comprises a compound of formula Rfn-M, where Rm is an organic group which tends to withdraw electrons from the metal atom M.
4. A method as claimed in claim 1, 2 or 3 wherein Rm-M is generated in situ by an exchange reaction between Rm-Li and potassium or sodium alkyl oxide.
5. A method as claimed in any of claims 1 to 4, wherein the reaction between RnnM and H-L1-X-L2-H is carried out in the presence of a basic compound which is capable of forming a complex with the metal.
6. A method as claimed in claim 5, wherein said basic compound comprises tetramethylethylenediamine.
7. A method as claimed in any preceding claim, wherein said compound of general formula (R3-C)2P-L1-X-L2-P-(C-R3)2 is selected from the group consisting of a,a’bis(di-t-butylphosphino)o-xylene (also known as 1,2 bis(dit-butylphosphinomethyl) benzene), bis(di-t-neopentyl phosphino)-o-xylene or bis 1,2(di-t-butyI phosphino)naphthalene.