Rolled copper foil and method of manufacturing the same

MYPI1999001200A0Inactive Publication Date: 1999-09-30JX NIPPON MINING & METALS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1999001200
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
1998-03-31
Filing Date
1999-03-30
Publication Date
1999-09-30
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional rolled copper foils lack sufficient flex resistance, especially in applications requiring high-density packaging and miniaturization, where they are subjected to numerous bending cycles without compromising elongation and other properties.

Method used

The manufacturing process involves hot rolling a copper ingot, alternating with cold rolling and annealing, and final cold rolling with a reduction ratio of not less than 90%, while optimizing annealing conditions to achieve a mean grain size of 5-20 μm, resulting in a cube texture with an X-ray diffraction intensity of the 200 plane greater than 20 times that of fine copper powder.

Benefits of technology

The resulting rolled copper foil exhibits stable and outstanding flex resistance, with a flexing fatigue life of over 30,000 cycles and adequate elongation, making it suitable for flexible printed circuits and other flexible applications.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

IMPROVEMENT OF THE FLEX RESISTANCE OF THE EXISTING ROLLED COPPER FOILS WITHOUT SACRIFICING THEIR OTHER PROPERTIES. A ROLLED COPPER FOIL OF EXCELLENT FLEX RESISTANCE HAVING A CUBE TEXTURE SUCH THAT, IN A STATE THERMALLY CONDITIONED AT 200?C FOR 30 MINUTES TO A RECRYSTALLIZED STRUCTURE, THE INTENSITY (I) OF 200 PLANE DETERMINED BY X-RAY DIFFRACTION OF THE ROLLED SURFACE IS I / IO>20 WITH RESPECT TO THE X-RAY DIFFRACTION INTENSITY (IO) OF 200 PLANE OF FINE COPPER POWDER. A METHOD OF MANUFACTURING THE ROLLED COPPER FOIL BY HOT ROLLING A COPPER INGOT, REPEATING COLD ROLLING AND ANNEALING ALTERNATELY, AND FINALLY COLD ROLLING THE WORK TO NOT MORE THAN 50 ?M IN THICKNESS, THE ANNEALING IMMEDIATELY BEFORE THE FINAL COLD ROLLING BEING PERFORMED UNDER CONDITIONS THAT ENABLE THE ANNEALED RECRYSTALLIZED GRAINS TO HAVE A MEAN GRAIN SIZE OF 5-20 ?M AND THE REDUCTION RATIO OF THE ENSUING FINAL COLD ROLLING IS SET TO NOT LESS THAN 90%. FIGURE 1
Need to check novelty before this filing date? Find Prior Art

Description

Improvement of the flex resistance of the existing rolled copper foils without sacrificing their other properties. A rolled copper cfoil of excellent flex resistance having a cube texture such that, in a state thermally conditioned at 200°C for 30 minutes to a recrystallized structure, the intensity (I) of 200 plane determined by X-ray diffraction of the rolled surface is I / Io>20 with respect to the X-ray diffraction intensity (Io) of 200 plane of fine copper powder. A method of manufacturing the rolled copper foil by hot rolling a copper ingot, repeating cold rolling and annealing alternately, and finally cold rolling the work to not more than 50 μπι in thickness, the annealing immediately before the final cold rolling being performed under conditions that enable the annealed recrystallized grains to have a mean grain size of 5-20 um and the reduction ratio of the ensuing final cold rolling is set to not less than 90%.Figure 1•·•· ·· 4* · 4 4 4 4 4 4 • 4« 4 4 · 4 4 4 4 4 44 ·44 4« 4 4 44 «4 »4444444 4 4 44 44 4444 4 4 «444444 444ROLLED COPPER FOIL AND METHOD OF MANUFACTURING THE SAME [Background of the invention]This invention relates to a rolled copper foil with excellent flex resistance suitable for applications such as flexible printed wiring members of flexible printed circuits and also to a method of manufacturing the same.Printed circuit boards based on organic matter are roughly divided into two types; rigid type with a rigid, copper-clad laminate consisting of glass-epoxy and paper-phenol substrates and flexible type with a flexible, copper-clad laminate consisting of polyimide and polyester substrates . Copper foil is mainly employed as conductive material for the printed circuit boards. The foil products are classified into electrodeposited and rolled foils depending on the manufacturing process used.I cOf the printed circuit boards, those for flexible printed circuits (hereinafter referred to as FPC) are fabricated by laminating copper foil to a resin substrate and joining the layers with adhesive or with the application of heat and pressure into an integral board. In recent years, multilayer boards known as built-up boards have come into extensive use as effective means for high-density packaging or mounting. The copper foil that is used to form components for FPCs is, for the most part, rolled copper foil.FPCs are largely used in printer heads, drives in hard disks , and other locations where wiring to movable parts is required.They are subjected to more than million of bending in service. This • 4 »4 «4 4 44 4 4 calls for greater flexing resistance of the rolled copper foil that forms the FPC components. With the recent tendencies toward miniaturization and higher performance levels of devices, the requirement for flex resistance has been severer than heretofore.As the material for copper foil in use with FPCs, tough-pitch copper or oxygen-free copper is employed. The foil is manufactured by hot rolling an ingot of such material and then repeating cold rolling and annealing alternately until a predetermined thickness is achieved. The rolled copper foil is then plated for surface roughing for enhanced adhesion to resin substrate. Following the roughing plating, the copper foil is cut into pieces and laminated to resin substrates. For the lamination purpose an adhesive of thermosetting resin, e.g., epoxy, is used. The adhesive is then hardened by heating at 130 to 170°C for 1 to 24 hours. The copper foil is etched to form various wiring patterns. The foil incorporated in the FPC may sometimes be folded or otherwise worked at points of contact with devices.The flex resistance of copper foil is markedly improved by recrystallization annealing over the properties as rolled. For this reason the foil is used in the annealed state as FPC components. This annealing is done either by heat treatment after the roughing plating and cutting into sizes or by utilizing the heating at the time of adhering to the resin substrate.The annealing is effected by heating at 130 to 250°C for 15 minutes to 24 hours, typically at 200°C for 30 minutes, when the copper foil is thermally conditioned to a recrystallized structure.[Object of the invention] ·· ·« «· · ·· ·· ·· ···· ·· ·· ···· · ·· ·· ·· • a a «a a a a a aa a a a a a aa a a aaa aa aa a aaaaaa a aaaaa aaaaa a aaaaaaa a a a a a a a a a a a aa a a a a a a a a aaaaaaaaa a aaaaaaaaa aaaaaaaa a a a aAs stated above, rolled copper foil as an FPC material is required to possess high flexing resistance. The recent trends for smaller size and higher levels of devices have made the flexing requirement even more stringent than ever.The present invention is aimed at improving the flex resistance of conventional rolled copper foils without sacrificing their elongation and other properties.[Brief summary of the invention]As a means of improving the flex resistance of rolled copper foil, a manufacturing process whereby the reduction ratio of the final cold rolling is increased has been proposed (Japanese Patent Publication Kokai No. 4-228553).In order to verify the effects of the reference invention, the present inventor and his coworkers made copper foils with final reduction ratios of 90 to 97% and tested them for their flex resistance. They did not always exhibit stable, satisfactory flex resistance.With these in view, the present inventor has intensively studied about the way of obtaining rolled copper foil with excellent flex resistance in stable manner. As a result, it has now been found important to adjust not only the reduction ratio of the final cold rolling but also the annealing conditions before the final cold rolling, i.e., in such manner that the mean grain size of the recrystallized grains that result from the annealing ranges from5 to 20 pm, and then perform the final cold rolling at a reduction ratio of not less than 90%.« « # « 4 «The copper foil thus produced shows stable, outstanding flex resistance, and it has been found possible to define the foil as one which, in the state after thermal conditioning at 200°C for 30 minutes to a recrystallized structure for use with an FPC, possesses a cube texture with the integral intensity (I) of 200 plane determined by X-ray diffraction of the rolled surface being I / Io>20 with respect to the X-ray diffraction integral intensity (Io) of 200 plane of fine copper powder. The rolled copper foil of the present invention has excellent flex resistance, showing a flexing fatigue life of not less than 30,000 flexing cycles in the flexing test to be described later.On the basis of the above findings, the present invention provides :(1) A rolled copper foil having excellent flex resistance characterized by a cube texture such that, in a state thermally conditioned at 200°C for 30 minutes to a recrystallized structure, the intensity (I) of 200 plane determined by X-ray diffraction of the rolled surface is I / Io>20 with respect to the X-ray diffraction intensity (Io) of 200 plane of fine copper powder.( 2 ) A method of manufacturing the rolled copper foil of (I) by hot rolling an ingot of tough-pitch copper or oxygen-free copper, repeating cold rolling and annealing alternately, and finally cold rolling the work to not more than 50 pm in thickness, characterized in that the annealing immediately before the final cold rolling is performed under conditions that enable the annealed recrystallized grains to have a mean grain size between 5 and 20 pm and the reduction ratio of the ensuing final cold rolling is set to not less than 90% .·· ·· ·· · · ·· ·· ···· ·· ·· ···· · ·· ·· ·· ·············· · · · · · · «······· «···>· · · · · · · ···· · ······· • «•••a a · a· a · a aa a a a a a aaaaaaaaa a aaaaaaaaa aaaaaaaa a a a a [Brief description of the drawings]Fig. 1 is a schematic diagram of a flex tester used to determine the flex fatigue life of test foils.Fig. 2 is a graph showing the relation among the reduction ratios of final rolling, the grain size upon annealing before final rolling and the I / Io.Fig. 3 is a graph showing the relation between the I / Ioand the fatigue life (number of flexing cycles).[Explanation of embodiments of the invention] jq The material for rolled copper foil to which the present invention applies is chiefly tough-pitch copper or oxygen-free copper. Rolled copper foil is basically manufactured by hot rolling a tough-pitch or oxygen-free copper ingot, repeatedly cold rolling and annealing the work by turns, and finishing the work to a thickness of 50 μπι or less by final cold rolling. According to the present invention, the annealing immediately before the final cold rolling is performed under conditions such that the annealed recrystallized grains have a mean grain size between 5 and 20 um and the reduction ratio of the ensuing final cold rolling is set to not less than 90%.For example, the conditions under which annealing is done are, in operation with a continuous annealing furnace, a temperature between 500 and 800°C and a period dependent on the temperature, between 5 and 600 seconds or, in batch operation, a temperature between 130 and 500°C for 1 to 24 hours.The reasons for which such annealing conditions have significant influences upon the flex resistance of the product will now be explained.• ·« · · *··· · · · · · • «« · · · · · · · · · ·««««*· · » · · » > · · · B · » · · »When pure copper is annealed for recrystallization, its cube texture (the (100) plane, the <001> direction, and the (100) plane and 200 plane being equivalent) develops. It is a widely known phenomenon that the development of the cube texture becomes remarkable as the reduction ratio before annealing is raised. The present invention is predicated upon the discovery that the crystal grain size before rolling also substantially influences the formation of the cube texture, the smaller the grain size the more the cube texture develops, and the more the cube texture develops the better the flex resistance. This is presumably attributed to the effect of decreasing the Young’s modulus in the direction of deformation, as explained in Japanese Patent Publication Kokai No. 55-54554 as the ground for the improvement in the fatigue properties of copper with the development of its cube texture.As will be appreciated from the foregoing, a mere increase in the reduction ratio of rolling is not effective enough to achieve excellent flex resistance in stable manner; it is additionally necessary to optimize the conditions of the preceding annealing operation. Thus if a copper foil is made by annealing under conditions such that the mean grain size of the recrystallized grains is not more than 20 pm followed by finally cold rolling the work at a reduction ratio of not less than 90%, high flex resistance will be attained stably. The resulting cube texture is such that the intensity (I) of 200 plane determined by X-ray diffraction of the rolled surface is I / Io>20 with respect to the intensity (Io) of 200 plane found by X-ray diffraction of fine copper powder.The intensity (Io) of 200 plane obtained by X-ray diffraction4 4 4 44 4 4 44 4 4 4 4 44 44444 44 4* 44444 4 4 4 44 4 4 4 44 4 4 4 444 4 4 44 44 4 4 4 4 4444 44 44 44 4 4 4 4 4444 444 4444 4 4 of fine copper powder was chosen as a reference value of the state where crystals are oriented at random (in the state where 200 plane is not developed).The grounds on which the recrystallized structure of the5copper foil and the manufacturing method for obtaining the same are specified in accordance with the invention are summarized as follows:(1) The intensity of 200 plane determined by X-ray diffraction of the rolled surface after heating at 200°C for 30 lg minutes is specified to be I / Io>20, because satisfactory flex resistance is achieved when the degree of development (I / Io) of the cube texture is greater than 20.(2) The mean grain size of recrystallized grains is specified to be in the range of 5 to 20 pm, because when the grainIQ size is not larger than 20 pm, I / Io>20 and hence good flex resistance is obtained. On the other hand, a grain size finer than 5 pm lowers elongation and poses problems such as cracking on bending. It is important, therefore, that the grain size be adjusted to not smaller than 5 pm.(3) The reduction ratio is specified to be no less than 90% because when the reduction ratio is less than 90% the I / Io>20 is not attained despite the adjustment of the conditions for the preceding annealing, and no favorable flex resistance is obtained.The rolled copper foil thus obtained has excellent flex resistance, showing a flexing fatigue life of more than 30,000 flexing cycles in the flexing test to be described later.• 4 4 · · 4 • · · · · · •44 444 · 44 4 44 4 4 44 4 4 44 4 4 44 4 4 44444 44 44 44444 4 4 4 44 4 4 4 44 4 4 4 444 4 4 44 444 44 444 4 4 4 4 44 4 4 4 4 4444 444 4444 4 4 [Examples]The invention will be more fully described below in connection with its examples and comparative examples.Ingots of tough-pitch copper (oxygen content: 250 ppm) and oxygen-free copper (oxygen content: 2 ppm), each measuring 200 mm thick and 600 mm wide, were made. They were hot rolled to 10 mm in thickness. After repetition of annealing and cold rolling, sheets of given thicknesses (t mm) as rolled were obtained. As indicated in Table 1, the sheets were annealed for predetermined periods in heating ovens where varied temperature in the range from 300 to 900°C were maintained. Following the removal of oxide scale, they were cold rolled to 0.035 mm in thickness . The reduction ratio R by the final cold rolling is given by the following formula:R = (t-0.035) / t x 100 (%).After the final annealing the annealed grain size was determined from a section perpendicular to the rolled direction obtained by the cutting method conforming to JIS G0551.ft ft ft ft ft ft ft ft ft ft ft ft ITable 1. Histories of working and properties of specimensKoFinal annealing conditionCopperMaterial laugiiaitoh sumac a tanp.ro8008008QQ τοαTOO aeatiag time (aae )2Q3QGramSize (μα)Final rolling radcctior ratio (2)Liter heating 200 *C 30 min1 / 1« rax i LraΜο.αΐ Clex cycles) ζζεπΓ ¢2)50.737.231.439.1645QQ5L10Q42a 004070013.315.616.415.2Example of th<! Invention33.443TGG16.2TOO6QQ6QQ500Cxygan5Q080070060050025.73320017-664.2323 GO12.015030050060048.839.133.472300433003230013.615.216,337.2 53000 15.325.764.233.44330017.633200 111* 6592QQ (ΐ6:Touglinitch80050.3854006·2Oxygen··80014.11370019.4 &E od κCdΦ >H +J odP adP.ε o70056.5916007.7ToughpitchOxyganfra·Tougtr35080070Q800 ··» · · ·· * ·120050..710.36.273.7727008.4176QQ .20.17300 23-992500 • · « · * · • · · » · • · · » · • · · · » · · · ·7.1With test specimens of copper foils thus produced under varied annealing conditions and at varied final rolling reduction ratios, their properties were evaluated as below.(1) Cube textureEach specimen was heated at 200°C for 30 minutes, and the integral value of intensity (I) of 200 plane as determined by X-ray diffraction of the rolled surface was found. The value was divided by the predetermined integral value of intensity (Io) of 200 plane of a fine copper powder (325 mesh ) to calculate the I / Io.(2) Flex resistanceEach specimen was heated at 200°C for 30 minutes for recrystallization, and then its flex fatigue life was determined using a flex tester illustrated in FIG. 1. The tester comprised a vibration drive unit 4 and a vibration transmitting part 3 connected to the drive unit. A test foil 1 was fixed in place at a total of four points indicated by arrows; at the ends of screws 2 and at the lower end of the part 3. As the vibrating part 3 was driven up and down, intermediate portions of the foil 1 were bent like hairpins at a given radius of curvature r. In the test under review, the bending was repeated under the following conditions to count the number of flexing cycles until failure.The testing conditions were: width of specimen = 12.7 mm; length of specimen - 200 mm; sampling direction = each specimen was cut off so that its length was parallel to the direction of rolling;radius of curvature r = 2.5 mm; vibration stroke = 25 mm; and vibration speed = 1500 vibrations / min.When the flex fatigue life exceeded 30,000 flexing cycles, · ·· ·· · · · · · · · ······ »····* · · · · · · «a············ aaaaa a aaaaaaaa • •a··· · aaaaa aaaaa a aaaaaaa the specimen was deemed to have excellent flex resistance. This test is an accelerated test where the specimen is flexed under severer conditions than in actual application.(3) Elongation5Each specimen was recrystallized by heating at 200°C for 30 minutes, and then was subjected to a tensile test in which the tensile direction was made parallel to the rolling direction. Elongation was measured with each specimen 12.7 mm wide and 150 mm long and a gage length of 50 mm.IQ Table 1 summarizes the histories of working and properties of the test specimens evaluated. The rolled copper foils according to the invention exhibited I / Iovalues of greater than 20 and excellent flex life of more than 30,000 flexing cycles. They also showed adequate elongation values exceeding 10%.On the other hand. Comparative Examples 1, 3, 4, and 7 gave low elongation values under 10% because the grain size after the final annealing was smaller than 5 pm. Comparative Example 2 had a grain size larger than 20 pm after the annealing and Comparative Examples 5 and 6 had final rolling reduction ratios below 90%, and therefore these specimens showed an underdeveloped (200) texture upon heating at 200°C for 30 minutes, and hence short flex life of less than 20,000 flexing cycles.On the basis of the data given in Table 1, the relations among the reduction ratios of final rolling, the grain size upon annealing before final rolling and the I / Iowere as graphically represented in FIG. 2. The recrystallized structure apparently developed with the increase in reduction ratio and with the decrease in grain size.4 4 « 4« 4 4* 44 44 ··♦·»· 4 4 4 4 · · 4 44 44 44 • 44 44 4444 44 44 4 44 44 4 4 >44 44 44 4 »44 44444 4 44444444 44 44 4 4 4 4444444 4 44 «4 •44 4444 • 4 4FIG. 3 shows the relation between the I / Ioand fatigue life (number of flexing cycles) . The graph sums up varying data concerning the conditions of annealing before final rolling and the reduction ratio, and indicates that the development of the recrystallized structure enhances the flex resistance.A comparison between tough-pitch copper and oxygen-free copper as the starting material, the latter provides a foil with slightly longer flex life. The difference is accounted for by the presence of a rather large amount of Cu2O inclusion in tough-pitch copper which promotes the growth and propagation of cracks , whereas oxygen-free copper contains little Cu2O inclusion.[Advantages of the invention]The present invention provides a rolled copper foil having excellent flex resistance and is best suited as flexible wiring material for flexible printed circuits and the like, and also an effective method of manufacturing the same.

Claims

CLAIMS 1. A rolled copper foil having excellent flex resistance characterized by a cube texture such that, in a state thermally conditioned at 200°C for 30 minutes to a recrystallized structure, 5 the intensity (I) of 200 plane determined by X-ray diffraction of the rolled surface is I / Io>20 with respect to the X-ray diffraction intensity (Io) of 200 plane of fine copper powder.

2. A method of manufacturing the rolled copper foil of claim 1 by hot rolling an ingot of tough-pitch copper or oxygen-free 10 copper, repeating cold rolling and annealing alternately, and finally cold rolling the work to not more than 50 urn in thickness, characterized in that the annealing immediately before the final cold tolling is performed under conditions that enable the annealed recrystallized grains to have a mean grain size between 5 and 20 15 pm and the reduction ratio of the ensuing final cold rolling is set to not less than 90%.