Flame retardant resin composition, and insulating electric wire, tube, heat-shrinkable tube, flat cable and DC high-tension electric wire all made of the composition

MYPI1999002051A0Inactive Publication Date: 1999-11-29SUMITOMO ELECTRIC INDUSTRIES LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1999002051
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Filing Date
1999-05-25
Publication Date
1999-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional flame retardant resin compositions used in insulated wires, tubes, and high-voltage DC electric wires generate harmful gases like hydrogen chloride when burned and often contain heavy metals, posing environmental concerns and safety risks, while existing non-halogen alternatives lack sufficient flame retardance and mechanical strength.

Method used

A flame retardant resin composition comprising 100 to 250 parts by weight of metal hydroxide and 5 to 50 parts by weight of acetate or 5 to 80 parts by weight of calcium carbonate, combined with ethylene-olefin copolymers, provides excellent mechanical strength and flame retardance without producing harmful gases, meeting or exceeding the flame retardance of PVC in UL Standards.

Benefits of technology

The composition achieves high mechanical strength and flame retardance, preventing harmful gas emission when burned, and is suitable for various electrical applications, including insulated wires, tubes, and high-voltage DC electric wires, while being environmentally safer than traditional halogen-based materials.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

(1) A FLAME RETARDANT RESIN COMPOSITION COMPRISING 100 PARTS BY WEIGHT OF THERMOPLASTIC RESIN, 100 TO 250 PARTS BY WEIGHT OF METAL HYDROXIDE, AND THEIR 5 TO 50 PARTS BY WEIGHT OF ACETATE OR 5 TO 80 PARTS WEIGHT OF CALCIUM CARBONATE. (2)AN INSULATED WIRE PROVIDED WITH AN INSULATING LAYER MADE OF THE FLAME RETARDANT RESIN COMPOSITION. (3) A THIN-WALL HIGH-STRENGTH INSULATED WIRE OBTAINED BY HAVING A CONDUCTOR WITH AN OUTER DIAMETER NOT GREATER THAN 1.0MM COVERED WITH THE FLAME RETARDANT RESIN COMPOSITION WITH A THICKNESS FROM 0.1MM TO NOT GREATER THAN 1.0MM. (4) AN INSULATING TUBE AND A HEAT-SHRINKABLE TUBE OBTAINED BY MOLDING THE FRAME RETARDANT RESIN COMPOSITION INTO A TUBULAR FORM. (5) A FLAT CABLE OBTAINED BY ENCLOSING A PLURALITY OF CONDUCTORS ARRANGED IN PARALLEL IN AN INSULATING COVER AND THE FLAT CABLE OBTAINED BY FURTHER LAMINATING AT LEAST ONE FACE OF THE INSULATING COVER WITH A FILM MADE OF POLYMERIC MATERIAL. (6) A HIGH-VOLTAGE DC ELECTRIC WIR PROVIDED WITH AN INSULATING COVER MADE OF THE FLAME RETARDANT RESIN COMPOSITION. (7)ARTICLES AS MENTIONED ABOVE HAVING THE FLAME RETARDANT RESIN COMPOSITION CROSS-LINKED, ESPECIALLY IRRADIATED WITH AN IONIZING RADIATION. INSULATED WIRE, TUBE, HEAT-SHRINKABLE TUBE AN FLAT CABLE HAVING EXCELLENT MECHANICAL STRENGTH AND FLAME RETARDANCE WITHOUT GENERATING ANY HARMFUL GAS, WHEN BURNING, ARE PROVIDED. THE INSULATED WIRE AND THE FLAT CABLE ARE SUITABLY USED FOR INNER WIRING OF CONSUMER''S ELECTRONIC DEVICES, AUTOMOBILES AND SHIPS AND SO ON. FIGURE 3.
Need to check novelty before this filing date? Find Prior Art

Description

FLAME RETARDANT RESIN COMPOSITION, AND INSULATING ELECTRIC HIRE, TUBE, HEAT-SHRINKABLE TUBE, FLAT CABLE AND DC HIGHTENSION ELECTRIC WIRE ALL MADE OF THE COMPOSITIONBACKGROUND OF THE INVENTIONField of the InventionThe present invention relates to Dame retardant resin compositions that do not produce harmful gases .such as hydrogen halide when burned and having excellent mechanical strength and relates to products made hy using the same, including insulated wire, tube, heat-shrinkable tube, Dat cable, and high voltage DC electric wire.Related Art and ProblemsThe insulation of insulated wires used in the field of electronic appliances and vehicles, insulators for tubes, heat-shrinkable tubes, and Dat cables, and sheath of high voltage DC electric wires for television sets, electromagnetic cooking ranges, copying machines, and the like are generally required to have a mechanical strength of 1.0 kg / mmsor more in terms of tensile strength (ultimate tensile strength at the point of fracture). For example, referring to the UL Standards widely adopted in the field of electronic appliances, in the case of insulated wires, tubes, heat-shrinkable tubes, and Dat cables using such plastics as polyethylene as the insulator, the insulator isFurther, flame retardance is also required ofthe insulated wires, tubes, he at-shrinkable tubes, flat cables, and the high voltage DC electric wires used in the above fields. Generally, horizontal flame retardance of the same is required in the field of vehicles and vertical flame retardance in the field of electronic appliances.As a method for testing the vertical flame retardance, the vertical test (VW-1 test) provided in the Subject 758 of the UL Standards as shown, for example, in FIG. 1 is well known. This is a combustion test performed on a specimen 5 of an insulated wire, a tube, a heat-shrinkable tube, a flat cable, or a high voltage DC electric wire vertically held by a fastener 3. In the test, the flame of a burner 2 is applied to the same specimen five limes , from under the specimen •for a duration o’f 15 seconds each time with 15 seconds intervals between the respective applications thereof. In the test, it is required that the insulation cease to flame within 60 seconds, absorbent cotton 4 placed thereunder should not ignite from burning droppings from the specimen, and kraft paper 1 fixed above the specimen should not burn or scorch.In the case of a tube, an all-tubing flame test is sometimes performed to assess the flame retardance of the specimen, namely, a metallic bar with the same diameter as the inner diameter of the tube is inserted through the tube and the ' 20 specimen is subjected to the same test as the VW-1 test. Sometimes, a heat-shrinkable tube is also subjected to an all-tubing flame test to assess its flame retardance, namely, the heat-shrinkable tube is put on a metallic bar having the same diameter as the inner diameter of the heat-shrinkable tube when it becomes shrunken and the same test as the VW-1 test is performed on the specimen.As materials for the above-described insulators of insulated wires, tubes, heat-shrinkable tubes, and insulators of flat cables satisfying the requirements for both mechanical strength and flame retardance, resin compositions comprising polyvinyl chloride such as flexible polyvinyl chloride compositions have long been known. Since such materials are excellent in both mechanical strength and flame retardance and, economical as well, they are widely used as the materials for forming insulated wires and flat cables applicable to the fields of electronic appliances and vehicles.However, the resin compositions produced by using polyvinyl chloride generate combustion gases harmful to the human body, such as hydrogen chloride, once burned, and also many of the resin compositions are mixed with heavy metal substances such as lead-based compounds for stabilizing their processing. Hence, they have an undesirable aspect against protection of the environment.In view of these problems, there have been known and put to practical use flame retardant resin compositions obtained by mixing ethylene polymer such as polyethylene with a phosphorus-containing flame retardant agent, or by mixing the same with a flame-retardant agent such as aluminum hydroxide or magnesium hydroxide, i.e., the so-called non-halogen flame retardant resin compositions.However, there have been problems with some of the phosphorus-containing flameretardant agents in that they exhibit acute toxicity when taken by mouth and, further, they corrode the conductors when mixed in resin compositions used in insulated wires and flat cables.pt oonnon^iOn the other hand, flame-retardant agents made of metal hydroxide have only a moderate flame-retardant effect on such plastics as ethylene polymer. Therefore, in order to obtain flame retardance equivalent to that of the polyvinyl chloride resin composition, it is required, for example, to have 100 parts or more by weight of metal hydroxide compounded with 100 parts by weight of ethylene polymer such as polyethylene, though this is not always true because it depends on the shape and size of the product. The drawback of compounding such a large quantity of metal hydroxide with the base resin, however, is that it markedly lowers the mechanical strength of the resin composition.Insulated wires based on the UL Standards to be used for wiring work within electronic appliances are normally prescribed to have a minimum thickness of 0.15 mm at 30 V rating, 0.4 mm at 300 V rating, and 0.8 mm at 600 V rating. Further, it is preferred that the insulated wire to be used for wiring work within electronic appliances have as small an outer diameter of as possible to allow easy handling of the wire, and for the conductor, a diameter of about 1.0 mm or less is used except in special cases (refer to page 13 of Handbook of Electronic Wire Products, published by Sumitomo Electric Industries, Ltd.).Halogen-free polyolefin insulated wires having a conductor of 1.0 nun or less in outer diameter and an insulation of 0.1 mm to 1.0 mm thickness which pass theVW-1 test and satisfy the requirements for mechanical strength such as initial tensile strength have been unknown. Recently, however, a thin-wall high-strength nonhalogen insulated wire satisfying the UL Standards was developed (Japanese Patent Nos. 2525982 and 2525968).PI 99002051Although the above-mentioned insulated wire satisfies the requirement to cease to flame within 60 seconds as provided in the Standards for the VW-1 test, it occasionally continues burning over 20 seconds. Therefore, the development of a non-halogen flame retardant insulated wire with greater flame retardance has been desired.On the other hand, in the case of high voltage DC electric wire, ethylene-a-olefin copolymer such as polyethylene is used to cover the conductor to improve the anti-tracking property of the wire.However, to offset the drawback of inflammability of polyethylene, it 10 has been the practice to cover the high voltage DC electric wire with a flame retardant resin composition having, as the main ingredients, a halogencontaining polymer such as polyvinyl chloride, thereby securing the flame retardance of the high voltage DC electric wire. However, since the resin composition using polyvinyl chloride generates combustion gases harmful to the human body such as hydrogen chloride, once burned, and many of the resin compositions contain heavy metal substances such as a lead-base compound for the purpose of stability in the fabrication, it has an undesirable aspect from the viewpoint of environmental preservation. Therefore, the development of a non-halogen high voltage DC electric wire has been desired.SUMMARY OF INVENTIONPI 99002051Through various investigations on the above enumerated problems, the inventors learned that, by having 100 to 250 parts by weight of metal hydroxide and either 5 to 50 parts by weight of acetate or 5 to 80 parts by weight of calcium carbonate compounded with 100 parts by weight of thermoplastic resin, it is possible to provide a flame retardant resin composition that does not produce harmful combustion gases such as hydrogen halide, e.g., hydrogen chloride when burned, exhibiting flame retardance of the same level or higher than that of PVC in the VW-1 test according to the UL Standards. Though this flame retardant resin composition compounded with acetate or calcium carbonate does not show difference in terms of the limiting oxygen index (LOI) when compared with a flame retardant resin composition not compounded with acetate or calcium carbonate, it exhibits excellent mechanical strength and also provides insulated wire, tube, heat shrinkable tube, flat cable, and high-voltage DC electric wire. Thus, this invention has been completed.[1] Flame Retardant Resin Composition (1) Namely, the invention provides a flame retardant resin composition obtained by comprising 100 to 250 parts by weight of metal hydroxide and either 5 to 50 parts by weight of acetate or 5 to 80 parts by weight of calcium carbonate, based upon 100 parts by weight of thermoplastic resin.(2) The flame retardant resin composition is characterized also in that it comprises the calcium carbonate in the amount from 5 to 30 parts by weight.(3) The flame retardant resin composition is characterized in that the thermoplastic resin is one kind or a mixture of two or more kinds of ethylenea -olefin copolymer selected from ethylene-vinyl acetate copolymer, ethyleneethyl acrylate copolymer, ethylene-methyl methacrylate copolymer, ethylenemethacrylic acid copolymer, and ethylene-methyl acrylate copolymer.(4) The flame retardant resin composition is characterized in that the ethylene - a - olefin copolymer is an ethylene-vinylacetate copolymer containing 6 to 50 % by weight of vinyl acetate component and has a melt flow rate of 0.5 to 30(at a temperature of 190X? and under a load of 2.16 kg).(5) The flame retardant resin composition is characterized in that an organosilicon compound coupling agent expressed as general formula Cl) :YlXR - Si - Y2 \Y3 (where R denotes alkyl including acryl, methacryl, or allyl and Y1 , Y 2, andY3 denote atomic groups selected from the groups of alkyl, alkoxyl, and 15 halogen) in the amount of 0.1 to 10 parts by weight is added to 100 parts by weigh of the ethylene-a-olefin copolymer.(6) The flame retardant resin composition is characterized in that the acetate is one kind or a mixture of two or more kinds, having a particle diameter of 0.5 to 5 lim, selected from magnesium acetate, sodium acetate, potassium acetate, zinc acetate, copper acetate, ferrous acetate, calcium acetate, aluminum acetate, nickel acetate, cobalt acetate, gallium acetate, silver acetate, tin acetate, barium acetate, cerium acetate, lead acetate, and beryllium acetate.(7) The flame retardant reein composition is characterized in that the primary particle diameter of the calcium carbonate is not greater than 4 / Im.(8) The flame retardant resin composition is characterized in that the calcium carbonate is one kind or a mixture of two or more kinds selected from calcium carbonate with its surface treated with a surface treatment agent such as that of fatty acid type, oil and fat type, surface-active agent type, or wax type, or calcium carbonate with its surface treated with a coupling agent such as that of silane type, titanate type, aluminum type, zirco-aluminum type, carboxylic acid type, or phosphate type.[II] Insulated Wire (1) The invention provides an insulated wire provided thereon with a covering layer made of the flame retardant resin composition described in [TJ, (1) to (8), above.(2) The insulated wire is characterized in that the covering layer is cross-linked.(3) The invention provides a thin-wall high-strength insulated wire having its conductor, whose outer diameter is 1.0 mm or less, covered with the flame retardant resin composition according to any of [TJ, (1) to (8), above to a thickness of from 0.1 mm to not greater than 1.0 mm and having the covering layer cross-linked.[Ill] Insulated Tube and others (1) The invention provides an insulating tube obtained by molding the flame retardant resin composition according to any of [I], (1) to (8), above into a tubular form.(2) The tube is characterized in that the tube layer is cross-linked.(3) The invention provides a heat shrinkable tube obtained, after a tube-formed molding made of the flame retardant resin composition according to any of [I], (1) to (8), above has been cross-linked, by expanding the tube5 formed molding in its radial direction under a heated condition and, thereupon, cooling the expanded tube to fix its form.[TV] Flat Cable (1) The invention provides a flat cable with a parallel arrangement of a plurality of spaced-apart conductors enclosed in an insulating cover, in which the insulating cover is made of the flame retardant resin composition according to any of [I], (1) to (8), above.(2) The flat cable is characterized in that the insulating cover is crosslinked.(3) The flat cable is characterized in that at least one face of the 15 insulating cover is laminated with a film made of a polymeric material.(4) The flat cable is characterized in that the insulating cover is irradiated with an ionizing radiation.[V] High-voltage DC Electric Wire (1) The invention provides a high-voltage DC electric wire having its 20 conductor provided thereon, as insulating layer, with a coating of an ethyleneα-olefin copolymer resin composition and having the insulating layer provided thereon with a covering layer made of the flame retardant resin composition according to any of [I], (1) to (8), above.(2) The high-voltage DC electric wire is characterized in that the insulating layer and covering layer are cross-linked.Functions performed by the above described aspects of the invention will be summarized as follows.(i) Flame Retardant Resin CompositionThe flame retardant resin composition obtained by having 100 parts by weight of thermoplastic resin compounded with 100 to 250 parts by weight of metal hydroxide and either 5 to 50 parts by weight of acetate or 5 to 80 parts by weight of calcium carbonate (claim 1) when burned, does not produce harmful gases such as hydrogen halide, e.g., hydrogen chloride, exhibits flame retardance of the same level or higher than that of PVC in the VW-1 test according to the UL Standards, and performs with excellent mechanical strength and, further, it can be used as flame retardant insulated wire, flat cable, and high-voltage DC electric wire.(ii) Insulated WireBy having a conductor coated with the flame retardant resin composition (claim 9), a flame retardant insulated wire excellent in mechanical strength can be obtained.By cross-linking the insulated wire, especially by irradiating it with an ionizing radiation (claim 10), an insulated wire and a flat cable not only excellent in flame retardance and mechanical strength but also excellent in such properties as heat resistance, resistance to heat deformation, and resistance to chemicals can be obtained.Such an insulated wire when cross-linked, even if the wire is of a structure having a thin-wall insulating coating applied on an extra fine conductor, can provide a non-halogen insulated wire exhibiting high strength and high flame retardance (claim 11).[iii] Insulating TubeThe flame retardant resin composition can be molded into a tubular form to provide an insulating tube (claim 12).The insulating tube when its tube layer is cross-linked (claim 13) provides an insulating tube not only excellent in flame retardance and mechanical strength but also excellent in such properties as heat resistance, resistance to heat deformation, and resistance to chemicals.Such a tubular molding when cross-linked, especially radiated with an ionizing radiation, and then processed to expand its diameter and keep its form as expanded (claim 14) can be made into a heat-shrinkable tube excellent in flame retardance and mechanical strength.(iv) Flat CableThe flame retardant resin composition extruded to cover up both faces of parallel conductors formed by conductors arranged in parallel (claim 15) can provide a flame retardant flat cable excellent in mechanical strength.The flat cable when cross-linked, especially radiated with an ionizing radiation (claim 16), can be made into a flat cable not only excellent in flame retardance and mechanical strength but also excellent in such properties as heat resistance, resistance to heat deformation, and resistance to chemicals.When the flame retardant resin composition is extruded by a melt extruding method or the like onto one surface of a biaxiafly stretched polyester film to provide a laminating tape of polyester film, two sheets of such tape are placed on both faces of parallel conductors such that the uncoated sides of the polyester film turn outward, and an insulating cover for the parallel conductors is provided by using a heat laminator (claim 17), and a flame retardant flat cable excellent in mechanical strength can be provided.In this case, when the flat cable is cross-linked, especially irradiated with an ionizing radiation (claim 18), a flat cable not only excellent in flame retardance and mechanical strength hut also excellent in such properties as heat resistance, resistance to heat deformation, and resistance to chemicals can be provided.(v) High-voltage DC Electric WireBy coating an ethylene-a-olefin copolymer resin composition as an insulating layer on a conductor and then extruding, over the outer layer, the flame retardant resin composition (claim 19), a flame retardant high-voltage DC electric wire excellent in mechanical strength and environmentally safe can be provided.The high-voltage DC electric wire, when the insulating layer and the covering layer are cross-linked, especially when they are irradiated by an ionizing radiation (claim 20), can provide a high-voltage DC electric wire not only excellent in flame retardance and mechanical strength but also excellent in such properties as heat resistance, resistance to heat deformation, and resistance to chemicals.The invention is described in more detail below.(A) Flame Retardant Resin CompositionsThe flame retardant resin composition according to the invention is basically obtained by compounding 100 parts by weight of thermoplastic resin with 100 to 250 parts by weight of metal hydroxide and either 5 to 50 parts by weight of acetate or 5 to 80 parts by weight of calcium carbonate, (claim 1).(1) Thermoplastic ResinThe thermoplastic resins used as the base polymer of the flame retardant resin compositions can be cited by way of example and without limitation:polyolefin, such as polyethylene and polypropylene;ethylene- a -olefin copolymer, such as ethylene-vinyl acetate copolymer, ethylene-ethyl acrylate copolymer, ethylene-methyl methacrylate copolymer, ethylene-methacrylic acid copolymer, and ethylene-methyl acrylate copolymer;thermoplastic elastomer such as polyolefin elastomer, including polyurethane elastomer, polyester elastomer, and ethylene-propylene copolymer elastomer, and polyamide elastomer; and polyester such as polyethylene terephthalate and polybutylene terephthalate.One of the thermoplastic resins may be used singly or two or more of them may be used in combination.One kind or two or more kinds of the above ethylene-a-olefin copolymer selected from ethylene-vinyl acetate copolymer, ethylene-ethyl acrylate copolymer, ethylene-methyl methacrylate copolymer, ethylene-methacrylic acid copolymer, and ethylene-methyl acrylate copolymer may be preferably used singly or in combination from the point of view of flame retardance, flexibility, and the like. The ethylene-vinyl acetate copolymer especially gives good results from the viewpoint of flame retardance and the like (Claim 3).When the ethylene-vinyl acetate copolymer is used, that containing 6 to % by weight, or preferably 10 to 48 % by weight, of vinyl acetate component 5 can be used favorably from the point of view of the balance between mechanical strength and flame retardance. As to the melt fluidity, when the melt flow rate (at a temperature of 190*0 and under a load of 2.16 kg) is set within the range between 0.5 and 30, or preferably within the range between 0.5 and 20 (claim 4), favorable results can be obtained in view of extrusion workability and the like.When the vinyl acetate content is under 6 % by weight, the flame retardance is decreased, and when it is over 50 % by weight, the mechanical strength is decreased.Further, as to the melt flow rate of the ethylene-vinyl acetate copolymer, 15 when it is under 0.5, the surface of the extruded moldings tends to become rough and, when it is over 30, the mechanical strength tends to decrease.The conditions of the α-olefin content and the melt flow rate as said of the ethylene-vinyl acetate copolymer above are correspondingly applicable to the other ethylene-a-olefin copolymers.In using the above ethylene-a-olefin copolymer, ethylene unsaturated compound other than the above exemplified α-olefin may be copolymerized according to need.(2) Compounding Ingredients (i) Organosilicon Compound Coupling Agent1) When an organosilicon compound coupling agent expressed as general formula [1]:YIXR — Si — Y2 \Y3 (where R denotes alkyl including acryl, methacryl, or allyl and Y1 , Y 2, andY3 denote atomic groups selected from the groups of alkyl, alkoxy 1, and halogen) in the amount of 0.1 to 10 parts by weight is added to 100 parts by weight of the thermoplastic resin (claim 5), favorable results can be obtained from the viewpoint of physical properties.2) As examples of the silane coupling agent expressed as general formula (l) ,T -methacryloxypropyltrimethoxysilane,T -methacryloxypropyltriethoxysilane,T -acryloxypropyltrimethoxysilane,T -methacryloxypropyldimethoxymethylsilane, andT-methacryloxypropyldimethylchlorosilane may be mentioned, and one or a mixture of two or more of them may be used.(ii) Metal Hydroxide (a)1) As examples of the metal hydroxide (a), magnesium hydroxide, calcium hydroxide, aluminum hydroxide, and the like can be mentioned.From the point of view of extrusion working temperature and the like of the resin composition, magnesium hydroxide and aluminum hydroxide are more preferably used.As to the particle size of the used metal hydroxide (a), if that of 0.3 to 30 / Im, or preferably that of 0.5 to 25 / Im, in diameter and that of approximately3 to 30 m2 / g, or preferably that of 5 to 28 m2 / g, in specific surface area by theBET method, is selected, satisfactory results can be obtained from the viewpoint of flame retardance, kneadability, extrusion workability, mechanical strength, and the like.If the particle diameter of the metal hydroxide (a) is under 0.3 / Im, particles tend to stick together to increase the kneading time and, if it exceeds 30 / Im, the mechanical strength tends to be decreased.When the specific surface area of metal hydroxide (a) is under 3 m2 / g, the flame retardance tends to be lowered and, when it exceeds 30 m2 / g, particles tend to readily stick together to prolong the kneading time.2) Further, when the surface of the metal hydroxide (a) is treated with a surface treatment agent, good results can be obtained from the viewpoint of kneadability of the resin composition and elongation.As examples of the surface treatment agent, anionic surface-active agents including fatty acid such as stearic acid and fatty acid metallic salt such as sodium stearate and sodium oleate can be mentioned.3) Further, also when the surface of the metal hydroxide is treated with an organosilicon compound coupling agent expressed as general formula Cl] , favorable results can be obtained from the viewpoint of physical property.(iii) Acetate (bl)The acetate (bl) used in combination with the metal hydroxide (a) in this invention is basically a compound expressed as general formulaMn[CHgCOO]uwhere Mndenotes a cation whose valence is n.As examples of the same, magnesium acetate, sodium acetate, potassium acetate, zinc acetate, copper acetate, ferrous acetate, calcium acetate, aluminum acetate, nickel acetate, cobalt acetate, gallium acetate, silver acetate, tin acetate, barium acetate, cerium acetate, lead acetate, and beryllium acetate can be mentioned.As types of salt of the acetate (bl), there are normal salt, acid salt, basic salt, and polynuclear metallic complex salt, some of which containing crystal water can also be used.Of those mentioned above, magnesium acetate, sodium acetate, zinc acetate, copper acetate, ferrous acetate, calcium acetate, aluminum acetate, nickel acetate, and barium acetate can be favorably used from the viewpoint of extrusion working temperature of the resin composition and the like.As to the particle diameter of the acetate (bl), when that of 0.5 to 5 Mm, preferably that of 0.5 to 3Mm, is selected (claim 6), favorable results can be obtained from the viewpoint of not only the kneadability with the base polymer but also the melt extrusion workability when it is compounded with the base polymer to provide a resin composition. When the surface is treated with an anionic surface-active agent as with the metal hydroxide, such characteristics as the kneadability with the base polymer and the melt extrusion workability when made into a resin composition can be improved.(iv) Calcium Carbonate (b2)1) As examples of calcium carbonate (b2) to be used in combination with metal hydroxide (a) in this invention, heavy calcium carbonate obtained by pulverizing such ore as calcite, Iceland spar, aragonite, limestone, marble, and whiting, precipitated calcium carbonate as synthetic stone, and light calcium carbonate can be mentioned.The crystal structure of the calcium carbonate (b2) takes on a rhombohedral calcite structure of a hexagonal system or an aragonite type structure of an orthorhombic system.Synthetic calcium carbonate of the same, having uniform particle diameter distribution, is favorably used from the viewpoint of extrusion workability and physical properties.As to the primary particle diameter of the calcium carbonate (b2), if that of not greater than 4 / Zm and preferably that of not greater than 3 / Zm, or more preferably not greater than 1 / Zm, is selected (claim 7), favorable results can be obtained from the viewpoint of flame retardance, kneadability with the base polymer, and the like.2) Further, if one kind or a mixture of two or more kinds selected from the group of calcium carbonate (b2) whose surface is treated with a surface treatment agent of fatty acid type, oil and fat type, surface-active agent type, wax type, and the like, or that whose surface is treated with a coupling agent of silane type, titanate type, aluminum type, zirco-aluminum type, carboxylic acid type, phosphate type, and the like is used (claim 8), such characteristics as kneadahility can be improved with the base polymer and the melt extrusion workability when it is made into a resin composition.(v) Compounded Amounts1) As to the amount of metal hydroxide (a) and acetate (bl), or calcium carbonate (b2), to be compounded with the thermoplastic resin, favorable results are obtained from the viewpoint of flame retardance and mechanical strength when 100 to 250 parts by weight, or preferably 100 to 200 parts by weight, of metal hydroxide, in combination with 5 to 50 parts by weight, or preferably 10 to 40 parts by weight, of acetate, or with 5 to 80 parts by weight, or preferably 5 to 30 parts by weight, of calcium carbonate, are compounded with 100 parts by weight of the thermoplastic resin.The flame retardance tends to deteriorate if the compounded amount of the metal hydroxide (a) is smaller than 100 parts by weight, regardless of the compounded amount of the acetate (bl) or that of the calcium carbonate (b2), and mechanical strength tends to decrease if the compounded amount of the metal hydroxide (a) exceeds 250 parts by weight.Further, even if the compounded amount of the metal hydroxide (a) is within the range of 100 to 250 parts by weight, problems such as diminished flame retardance arise if the compounded amount of the acetate (bl) is smaller than 5 parts by weight or the compounded amount of the calcium carbonate (b2) is smaller than 5 parts by weight and that mechanical strength is decreased if the compounded amount of the acetate (bl) exceeds 50 parts by weight or the compounded amount of the calcium carbonate (b2) exceeds 80 parts by weight.2) In the flame retardant resin composition of the invention, the drawback of the conventional thin-wall high-strength non-halogen insulating wires, tubes, heat-shrinkable tubes, or flat cables continuing to bum over 20 seconds has been solved hy mixing the thermoplastic resin with the acetate (bl) or calcium carbonate (b2) in an amount within a specific range, in addition to the metal hydroxide (a).Further, it has also been found that, if the flame retardant resin composition is applied to the jacket for high voltage DC electric wire, the product can satisfy the vertical combustion test.3) Mixing and MoldingIn mixing the thermoplastic resin, the metal hydroxide, and the acetate or the calcium carbonate, a known mixing apparatus such as an open roll mixer, Bunhury mixer, pressure kneader, and biaxial mixer can be used.From the thus obtained resin composition, various types of moldings for insulated wire, tube, heat-shrinkable tube, flat cable, high voltage DC electric wire, and the like can be easily produced by using a known resin molding apparatus such as a melt extruder and injection molder.(vi) Other Resin Components and Additives1) The resin composition of the invention can be mixed, for the purpose of improving its characteristics, with various types of polymers such as EDPM and ethylene acrylic rubber within a range of an amount not impairing such characteristics as flame retardance and mechanical strength.2) Further, various additives such as thermal stabilizer, antioxidant, ultraviolet absorber, lubricant, process stabilization auxiliary, coloring agent, foaming agent, reinforcing agent, organic or inorganic filler, and multifunctional monomer can be added to the resin composition.3) The above multifunctional monomer, in particular, serves as a cross5 linking assistant agent and, especially at the time of irradiation with an ionizing radiation, improves the cross-linking effect. Hence, it may be added to the resin component according to need.As examples of the multifunctional monomer, monomers containing plural portions of unsaturated linkage in the molecule such as trimethylolpropanetrimethacrylate, pentaerythritoltriacrylate, ethyleneglycoldimethacrylate, triallylcyanurate, and triallylisocyanurate can be mentioned.(B) Various Moldings and Methods of Fabricating the Same (i) Fabrication of Insulated Wire and Flat Cable 15 When a flame retardant resin composition of the invention is extruded by the use of a melt extruder or the like onto a conductor to cover the same, the product can be used as it is as a flame retardant insulated wire or a flat cable flee from the problem of generating harmful gases when it is burned (claim 15).Further, if the thus obtained flat cable is sandwiched between two sheets of insulating polymeric film such as polyester film, the product can be used as a flame retardant flat cable flee from the problem of generating harmful gases when burned (claim 17).When the covering layer is cross-linked by the method of subjecting the insulated wire or the flat cable to irradiation of an ionizing radiation or the like, the insulated wire or the flat cable can be made into one that is excellent in such characteristics as mechanical strength, heat resistance, and resistance to heat deformation (claims 16 and 18).(ii) Thin-wall High-strength Insulated Wire 5 1) The conventional resin composition made to be flame retardant by having a thermoplastic resin such as polyolefin compounded with a large amount of magnesium hydroxide as halogen-free flame retardant has good flame retardance. However, since it has poor compatibility with the thermoplastic resin when it is applied to an insulated wire, its initial tensile strength becomes low and, further, the physical property is greatly deteriorated when it is heat aged. This invention can solve such problems more effectively.2) The inventors earlier developed a thin-wall high-strength nonhalogen insulated wire in conformity with the UL Standards. While this insulated wire satisfies the requirement of extinguishing a flame within 60 seconds as provided in the VW-1 test, it sometimes continues to burn 20 seconds or more and, hence, it has not been a satisfactory thin-wall highstrength non-halogen insulated wire. Therefore, the development of a nonhalogen flame retardant electric wire having higher flame retardance has been desired. This invention can also solve this problem.3) The flame retardant resin composition of the invention, by virtue of the characteristic feature of its composition, can provide a non-halogen insulated wire being thin-walled, high strengthened, and highly flame retardant.That is, the invention provides a thin-wall high-strength non-halogen insulated wire with a conductor whose outer diameter is not greater than 1.0 mm, preferably between 0.1 and 1.0 mm, covered with a flame retardant reein composition as set forth in any of claims 1 to 8 with a thickness between 0.1 mm and 1.0 mm and with the covering layer cross-linked, especially irradiated with an ionizing radiation (claim 11).If the thickness of the insulating layer is as small as under 0.1 mm, its normal withstand voltage is rendered unpractical and, if the thickness is as great as over 1.0 mm, there arises a problem related to its flame retardance when the wire is such that it has a small-diametered conductor and is used for wiring work within an appliance.4) This thin-wall high-strength insulated wire is suitable as an insulated wire for wiring work within an appliance, satisfying various safety regulations such as the UL Standards and it has such a merit in that it, while securing safety against fire, produces no environmental pollution.(iii) Fabrication of Insulating Tube, etc.The flame retardant resin composition of the invention can he made into an insulating tube by such a method as melt extrusion (claim 12).The tubular molding of the flame retardant resin composition of the invention can be formed into a heat-shrinkable tube, first, by cross-linking it, especially by irradiating it with an ionizing radiation and, then, by expanding it in its radial direction by such a method as to send compressed air into it at a high temperature and thereupon cooling it so that it keeps its expanded form (claim 14).(iv) Fabrication of High Voltage DC Electric WireA conductor is coated with an ethylene- a -olefin copolymer resin composition by using a melt extruder or the like and then a covering layer (jacket) made of the flame retardant resin composition of the invention is provided on the same. By cross-linking each layer by applying it with an ionizing radiation or the like, or by not cross-linking the insulating layer and the covering layer separately, but by cross-linking both the insulating layer and the covering layer at the same time after the provision of the covering layer, of course then having a chemical cross-linking agent such as organic peroxide previously mixed in the insulating layer and the covering layer, a high voltage DC electric wire excellent in such characteristics as mechanical strength, heat resistance, and resistance to heat deformation can be provided (claims 19 and20).(v) Cross-linking, etc.1) While electron beam, accelerated electron beam, gamma ray, beta ray, X-ray, alpha ray, ultraviolet ray, and the like can be mentioned as examples of the ionizing radiation, the accelerated electron beam can be used most favorably from the viewpoint of its industrial utilization, such as handiness of the beam source, the thickness penetrated by the ionizing radiation, and the speediness in the cross-linking process.As to the exposure dose of the ionizing radiation, it is favorable when 20 the electron beam, for example, is used, to set the exposure dose between 3 andMrad, or preferably between 5 and 25 Mrad.If the exposure dose is under 3 Mrad, the effect of improving the tensile strength is diminished and, if it is over 50 Mrad, the elongation is conversely decreased.2) Instead of radiating with an ionizing radiation, a chemical crosslinking method can also be used in which an organic peroxide or the like is previously mixed in the flame retardant resin composition and, after the molding, the product is heat treated.As examples of the organic peroxide, dicumylperoxide, bis(tbutylperoxyisopropyl)peroxide, and the like can be mentioned.However, irradiation with ionizing radiation is preferable if the initial mechanical strength is reconciled with the flame retardance.BRIEF DESCRIPTION OF THE DRAWINGSFIG. 1 is a schematic diagram showing the interior of a combustion testing apparatus for explaining the vertical combustion test (VW - 1 test) according to the UL Standards.FIG. 2 is a schematic diagram for explaining the high-voltage cutthrough test according to the UL Standards, Subject 758.FIG. 3 is a schematic diagram for explaining the withstand voltage test (Method II) according to the UL Standards.DESCRIPTION OF THE PREFERRED EMBODIMENTSWhile the invention will be described as related to some embodiments below, the scope of the invention may not be limited by any of the details of description.Measurement of Physical Properties (1) On Insulated Wire:1) Flame Retardance TestTo check the flame retardance, the VW-1 test according to the UL Standards was carried out on 10 specimens of each example. If even one of the 10 specimens of each example burned over 60 seconds, absorbent cotton placed thereunder was burned due to burning droppings from the specimen, or a sheet of kraft paper fixed thereabove was burned or scorched, the example was judged to have failed the test.Burning times of the 10 specimens were classified into the ranges of 0 second to under 20 seconds, 20 seconds to under 40 seconds, 40 seconds to under 60 seconds, and 60 seconds and over. When all of the specimens extinguished before 40 seconds elapsed, the example was judged to be good.2) Physical PropertyThe tensile strength and elongation (gage length: 50 mm) were measured on three specimens of each example according to the measuring method specified in JIS C3005 and the average values were obtained.A tensile test (pulling speed: 500 mm / min) was carried out on extruded covering material and the tensile strength and elongation (gage length: 20 mm) were measured on three specimens of each example and the average values were obtained.(2) On Insulating Tube:1) Flame Retardance TestAn iron bar having the diameter 6.4mm equal to the inner diameter of a tube was inserted into a tube and the all tubing combustion test was carried out on 10 specimens of each example. If even one of the 10 specimens failed in the test by causing it to burn over 60 seconds, burn the kraft paper, or burn the absorbent cotton, the example was judged to have failed the test. Burning times of the 10 specimens were classified into the ranges of 0 seconds to under 20 seconds, 20 seconds to under 40 seconds, and 40 seconds to under 60.When all of the specimens extinguished before 40 seconds elapsed, the example was judged to be good.2) Physical PropertyTo check the mechanical strength of the tube, the tensile test conforming to the method specified in JIS C3005 (pulling speed: 500 mm / min) was carried out and the tensile strength and elongation (gage length: 20 mm) were measured on three specimens of each example and the average values were obtained.(3) On Heat-shrinkable Tube:1) Flame Retardance TestAn iron bar of 3.3 mm in diameter was inserted into a heat-shrinkable tube whose inner diameter had been expanded to 7 mm and the specimen was put in a constant-temperature bath at a temperature of 150*C and kept therein for three minutes so that the heat-shrinkable tube was heat-shrunk to fit over the periphery of the iron bar. The all tubing test was carried out on 10 20 specimens of each example. If even one of the 10 specimens failed in the test by causing it to burn over 60 seconds, burn the kraft paper, or burn the absorbent cotton, the example was judged to have failed the test.2) Physical PropertyTo check the mechanical strength of the heat-shrinkable tube, the tensile test (pulling speed: 500 mm / min) conforming to the method specified in JIS C3005 was carried out on the specimens of the heat-shrinkable tube heatshrunk by being kept for three minutes in a constant-temperature bath set at a temperature of 150*0 and the tensile strength and elongation (gage length: 20 mm) were measured on three specimens of each example and the average values were obtained.(4) On High Voltage DC Electric Wire:1) Flame Retardance According to UL StandardsTo check the flame retardance, the VW-1 test according to the ULStandards was carried out on 10 specimens of each example.If even one of the 10 specimens of each example burned over 60 seconds, absorbent cotton placed thereunder was burned due to burning droppings from the specimen, or a sheet of kraft paper fixed thereabove was burned or scorched, the example was judged to have failed the test.2) Physical PropertyA tensile test (pulling speed: 500 mm / min) was carried out on the extruded covering layer and the tensile strength and elongation (gage length: 20 mm) were measured on three specimens of each example and the average values were obtained.3) Heat Aged Physical PropertyWire specimens were heat aged by being kept in a Geer oven at a temperature of 158*C for seven days and thereafter the residual elongation rate of the covering layer was assessed.Here, the residual elongation rate is defined by the formula, residual elongation rate (%) = (elongation of heat aged specimen / initial elongation) x100. Having a residual elongation rate of 65 % or above was set as the passing mark.4) High-voltage Cut-through TestFIG. 2 is a schematic diagram for explaining the high-voltage cutthrough test according to Subject 758 of the UL Standards.As shown in FIG. 2, loads 10 of 0.45 kg each were applied to both ends of a wire 13 which was passed over and hung down from two parallel drill rods 11, o.O79 cm in diameter > inahath set at a constant temperature of 125^3 and a voltage of 1.5 times as high as the rated voltage was applied thereto from the DC power source 12. Then, if a breakdown took place within 7 hours, the specimen was judged to have failed. Assessment was made with n = 3.5) Withstand Voltage Test (Method II)FIG. 3 is a schematic diagram for explaining the withstand voltage test (Method II) according to the UL Standards.After electric wire specimens were heat-aged hy being kept in a Geer oven at a temperature of Ιδδ'Ό for seven days, the wire 21 was wound seven turns around a mandrel, 1.27cm in outer diameter. When a voltage of 1.25 times as high as the rated voltage was applied to the wire in the Geer oven at 125*C, if a breakdown took place within seven hours, the specimen was judged to have failed. Assessment was made with n = 3.<Preparation of Flame Retardant Resin Compositions>The resin compositions shown in Tables 1 to 14 were kneaded by a pressure kneader set at a temperature of 140 and the thus kneaded compounds were formed into pellets by using a feeder-extruder.In the preparation of the resin compositions shown in Tables 1 to 14, 5 0.5 part by weight of amide oleate and 1 part by weight of pentaerythritol-tetrakis C 3-(3,5-t-butyl-hydroxyphenyl)propionate ) were commonly added to 100 parts by weight each of the base polymers shown inTables 1 to 14.(A) Insulated Wire -1:(Embodiments 1 to 14)The pellets shown in Tables 1-3 were extruded by the use of a melt extruder (full flight type, 45 mm in diameter, L / D = 24, compression ratio = 2.5) to encase a conductor (tinned annealed copper wire 0.8 mm in diameter) with a wall thickness of 0.40 mm. The thus obtained article was irradiated by an electron beam of 200 kGy at an accelerating voltage of 2MeV to provide a specimen.Incidentally, the electron beam irradiation process was omitted with Embodiment 7 in Table 1, Embodiment 14 in Table 2, and Comparative Example 5 in Table 3.Embodiments 1 to 7 shown in Table 1 are insulated wires produced by using resin compositions in which 100 parts by weight of ethylene-vinyl acetate copolymer resin are compounded with 150 to 190 parts by weight of magnesium hydroxide as metal hydroxide and 10 to 50 parts by weight of magnesium acetate or calcium acetate as acetate.Further, Embodiments 8 to 14 shown in Table 2 are insulated wires produced by using resin compositions in which 100 parts by weight of ethylene-vinylacetate copolymer resin are compounded with 150 to 190 parts by weight of magnesium hydroxide as metal hydroxide and 10 to 50 parts by weight of calcium carbonate.All of the specimens of the embodiments have passed the VW-1 test, the distribution of the burning times has been mostly within 0 to 20 seconds, and the burning time at the longest has been under 40 seconds.Further, the specimens produced by using the resin compositions ofEmbodiments 3 to 6 and 10 to 13 with T -methacryloxypropyltrimetoxisilane added thereto as a silane coupling agent have been found to exhibit such mechanical strength as to exceed the values provided in the UL Standards, namely, over 1.06 kg / mm2in tensile strength and over 100 % in elongation.(Comparative Examples 1 to 7)Comparative Examples 1 to 6 shown in Table 3 are insulated wires produced by using resin compositions in which 100 parts by weight of ethylene-vinylacetate copolymer are compounded with 180 to 250 parts by weight of magnesium hydroxide as metal hydroxide.When the VW-1 test was carried out on the insulated wires made of the resin composition of Comparative Examples 1 to 5 in Table 3, all of the specimens passed the test but the burning times of many of the specimens were distributed in the ranges of 20 to 40 seconds and 40 to 60 seconds, from which it was found that they were inferior in flame retardance to Embodiments 1 to 7 in Table 7 with acetate added thereto or Embodiments 8 to 14 in Table 2 with calcium carbonate added thereto.Specimens of Comparative Example 6 passed the VW-1 test and many of the burning times were distributed in the range of 0 to 20 seconds to prove excellence in flame retardance, but their tensile strength did not satisfy the UL Standard and their elongation also was under 100 %.Comparative Example 7 in Table 3 is an insulated wire produced by using PVC composition and it is known that all the specimens were extinguished within a burning time of 20 seconds.Table 1100 180 o i-H © 7 / 10 3 / 10 0 / 10 0 / 10 Passed 0.55 650 -ti © © © 80 © (N i-H oo: © i-H / 10 / 10 © i-H φ co co .25 © lO <M co © © cd PH 1-H -ti 1Λ © © © 1Λ © co <N © © © i-H / 10 / 10 © i-H Φ co co © co © CQ rd CN 00 <N © © cd n . rH (N w Φ -ti o 100 190 o i-H <N 200 6 / 10 4 / 10 0 / 10 0 / 10 Φ co oo cd 1.20 140 1 Ph -ti CO © © © 1Λ © CO i-H © © © rH / 10 / 10 © i-H φ co oo IO rH © r-l r-l © rH © o cd Ph rH 'ti <N 100 150 © 1Λ 200 10 / 10 0 / 10 0 / 10 0 / 10 φ oo oo cd Ph 0.74 255 -ti rd 100 180 © <N 200 8 / 10 2 / 10 0 / 10 0 / 10 Passe 08Ό 350 x—s o o a o Φ Φ QQ Φ 00 +> co © © h ti © © h <N h h & ti μι Φ Φ £ Tj< 2 Φ T3 ti h d h Φ fr Λ—\ i-H * § ler (*2) ti cd d co •g Si o to und ti ti O © ti ti O © O O Φ 00 © udgem< Λ—S CS 9 9 ~Sb l—l a ti Φ Φ co o © <N © •“D o o z—\ Λ—S ω i-H Insi I cop co * Tj< * Λ—S IO £ T3 Φ 1 «J t-1 & _ti 1 0.8mm φ, inylacetate dnylacetate n hydroxide n hydroxide n acetate (* cetate (*6) ryloxypropy earn exposu Φ oc a 3 ° ti T ti -ti s- c3 x +> +: sile strengt] agation (%) h »γ cd hac u op 2 a ti o -ti φ s f 1 § § • rH CO • QQ QQ ti a g>.5 ·□ 9 ® ® ►3 3 & h - S Φ ti QQ ti I—l (condu< Ethyle: Ethyle: Magne Magne Magne '3 73 u Φ a Electrc Flame test (L Initial InitialNotes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m / g, surface treated with stearic acid * 4: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m Ig,Surface not treated * 5: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Mm * 6: Made by Wako Jun-yaku K.K., Average particle diameter = 3 MmTable 2rd 100 180 © rd © 5 / 10 5 / 10 0 / 10 0 / 10 Passed 0.40 © co o ’ti CO rH 100 180 20 rd © © CO 7 / 10 3 / 10 0 / 10 0 / 10 Passe 1.11 135 t3 <N rH 100 150 o co CM 200 5 / 10 5 / 10 0 / 10 0 / 10 Φ co co ti n . 1.20 230 -Μ MH w V ’ti o rd 100 190 © rH CM 200 8 / 10 2 / 10 0 / 10 0 / 10 Φ co 00 ti 1.20 200 a w P-S t3 O rH 100 150 o eo 200 6 / 10 4 / 10 0 / 10 0 / 10 Passe 1.15 155 ’ti 05 100 150 o IO 200 6 / 10 4 / 10 0 / 10 0 / 10 asse 0.50 440 Pl, t3 00 00 80 o CM © © © © / 10 / 10 Φ 00 00 CD o rH rH rH co o co © © cd Ph © CO Z**\ u ϋ a ϋ φ Φ 00 Φ 00 -M 00 © © Sh mm © co Sh er 4 er 6 ove ti © Φ ’ti ’ti Sh iii . Layer 0. ymer (*1) ymer (*2) netoxisilan .ose (kGy) TO ti ti 5 © 20 to un 40 to un 60 sec. o Judgemi a a be 3 o o Z**\ z-> ω rH 00 ti HH cop cop eo Z**\ IO § 1 -tJ 1 e 43 5 -8 TJ Φ T3 >» a 3 00 Φ 43 ft agation (%) © a a 00 ό dnylaceta dnylaceta n hydroxi n hydroxi n acetate cetate (*6 ryloxypro earn expo be i s s 42 ti tardance td.) sile stren Sh cd u 43 -> 00 S cc ti o © o -M ei § § M 00 •M 00 •M 00 cd Λ ti -+? 3 © © £ a o o ® S ►3 3 & 5 Φ S CO ti (condut Ethyle: Ethyle: Magne Magne Magne o 73 o 7-met Electrc Flame test (TJ Initial InitialNotes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7Surface treated with stearic acid * 4: Average particle diameter = 0.7Surface not treated * 5: Primary particle diameter = 0.04JLtm, BET specific surface area = 7 m / g,JLtm, BET specific surface area = 7 m / g, / im, Surface treated with stearic acid * 6: Primary particle diameter = 1.5 JLtm, Surface not treatedTable 3t— c s: 1 I ° §· o υ sition 100 10 / 10 0 / 10 0 / 10 0 / 10 Passed 1.79 250 ’ti CO 00 50 © © o rd © rd © rd / 10 Φ co co Ti Ti 80 rd CM CM iO CM CM © cd © φ in 100 180 © 0 / 10 ' 0 / 10 10 / 10 0 / 10 Passed 0.45 800 φ X Η ’ti φ > Ti 00 © © CM © © © rd 4 / 10 © rd © φ oo co .20 .40 • fM rd CM CM rd in © cd rn cd Ph cd & ’ti a o co 00 80 rd © © © rd © rd © © see .28 .50 O rd CM © in in © cd Ph rd n ’ti CM 00 00 00 © rd © ^d © © rd see .74 in in rd CM CM rd in co © cd © OI Pm ’ti rd 00 00 00 © © rd © © sse 00 t— © CM rd CM CM © rd © © cd © Ph x—s o Φ 9 o φ φ oo Φ co -M co © © a a r 20 er 4 er 6 ove S Ti © h X“S rd cm * Jane Si ’ti ti § h O O § Φ Φ £ i-3 Φ a ►> ymer netoxisi o β Φ co o © 20 to 40 to 60 se Judg X“S CM a a ti o o X“S z-> ¢0 **—· rd CO a H-1 cop cop co Ti 'ti § 1 ' -tn> d β _rj tate tate xide xide ropy 3 oo 2 Φ 42 be a Φ mgtl g φ H 8mm tylace tylace hydro hydro J S’ Φ a ’ίβ~ £ A rdanc J e stre ation g © .p .{3 g g fr cd φ 3= a 7 cd τ co 00 £ h 3 3 o _Q 2 ® ω a ti Λ 'ti φ cd 9 OQ ti F-1 O i 'ti ti J, Ethylene Ethylene Magnesii Magnesii r -metha Electron -P § si a bo fi -g § 8 ω ►3 9 ω Flame r Initial te Initial ehNotes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 Mm, BET specific surface area = 7m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m / g,Surface not treated (B) Insulated Wire - 2:(Embodiments 15 to 22)The flame retardant resin compositions shown in Tables 4 and 5 were extruded by the use of a melt extruder (full flight type, 45 mm in diameter, L / D = 24, compression ratio = 2.5) to encase a conductor (tinned annealed copper wire 0.8 mm in diameter) with a wall thickness of 0.80 mm. The obtained article was then irradiated by an electron beam of 200 kGy at an accelerating voltage of 2MeV to provide a specimen.The physical properties of the insulated wires were assessed in the same way as applied to Embodiments 1 to 14.Embodiments 15 to 22 shown in Table 4 include insulated wires produced by using resin compositions in which 100 parts by weight of ethylene-vinylacetate copolymer resin are compounded with 150 to 190 parts by weight of magnesium hydroxide as metal hydroxide and 10 to 50 parts by weight of magnesium acetate or calcium acetate as acetate and insulated wires produced by using resin compositions in which 100 parts by weight of ethylene-vinylacetate copolymer resin are compounded with 150 to 190 parts by weight of magnesium hydroxide as metal hydroxide and 10 to 50 parts by weight of calcium carbonate.All of the specimens of the examples have passed the VW-1 test and 5 many of them have been extinguished within 20 seconds to prove their excellence in flame retardance.Further, the specimens produced by using the resin compositions ofEmbodiments 17 and 18, and 21 and 22 in Table 4 with T methacryloxypropyltrimetoxisilane added thereto as a silane coupling agent have been found to exhibit such mechanical strength as to exceed the values provided in the UL Standards, over 1.06 kg / mm2 in tensile strength and over100 % in elongation.(Comparative Examples 8 to 12)Comparative Examples 8 to 11 shown in Table 5 are insulated wires produced by using resin compositions in which 100 parts by weight of ethylene-vinylacetate copolymer are compounded with 180 to 200 parts by weight of magnesium hydroxide as metal hydroxide.In the VW-1 test performed on the insulated wires produced by using the resin compositions of Comparative Examples 8 to 11, all of the specimens passed the test but the burning times of many of them were distributed in the ranges of 20 to 40 seconds and 40 to 60 seconds, from which it was found that they were inferior in flame retardance to Embodiments 15 to 18 in Table 4 with acetate added thereto or Embodiments 19 to 22 with calcium carbonate added thereto.Comparative Example 12 is an insulated wire made of PVC composition and it is known that all of the specimens were extinguished within a burning time of 20 seconds in the VW-1 test.Table 4Embodiment 22 100 150 50 co 200 6 / 10 4 / 10 0 / 10 0 / 10 Passed 1.20 310 21 100 160 20 rd 200 7 / 10 3 / 10 0 / 10 0 / 10 Passed 1.35 140 20 100 160 40 200 7 / 10 3 / 10 0 / 10 0 / 10 Passed © 00 ό 360 19 100 190 10 200 8 / 10 2 / 10 0 / 10 0 / 10 Passed 0.65 200 18 100 150 50 co 200 7 / 10 3 / 10 0 / 10 0 / 10 Passed © CO τ-H 240 tH 100 160 20 200 8 / 10 2 / 10 0 / 10 0 / 10 Passed 1.23 165 16 100 160 40 200 9 / 10 1 / 10 0 / 10 0 / 10 Passed 0.85 275 15 100 190 10 200 9 / 10 1 / 10 0 / 10 0 / 10 Passed 0.75 o 00 co . Layer 0.8mm thick) Ethylene-vinylacetate copolymer (*1) Ethylene-vinylacetate copolymer (*2) Magnesium hydroxide (*3) Magnesium hydroxide (*4) Magnesium acetate (*5) Calcium acetate (*6) Calcium carbonate (*7) Calcium carbonate (*8) γ -methacryloxypropyltrimetoxisilane Electron beam exposure dose (kGy) 1 0 to under 20 sec. 20 to under 40 sec. 40 to under 60 sec. 60 sec. or over Judgement Initial tensile strength (kg / mm2) Initial elongation (%) Insulated Wire (conductor 0.8mm φ, Insul. Longest burning time distribution (Number of specimens: 10) Flame retardance VW-1 test (UL StdJ_Notes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 fim, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m / g,Surface not treated * 5: Made by Wako Jun-yaku K.K., Average particle diameter = 3 fim * 6: Made by Wako Jun-yaku K.K., Average particle diameter = 3 / Zm * 7: Primary particle diameter = 0.04 / Zm, Surface treated with stearic acid * 8: Primary particle diameter = 1.5 / Zm, Surface not treatedTable 5parative Example 12 PVC compo- sition © © r-1 10 / 10 © r-1 © 0 / 10 0 / 10 Passed 1.65 270 r-t r-t 100 200 i_ <N 200 1 / 10 4 / 10 5 / 10 0 / 10 Passed 1.35 135 10 100 © 00 r-1 r-t © © <N © r-1 © 5 / 10 5 / 10 © r-1 © Passed 1.31 145 Com] © © © r-1 200 200 1 / 10 4 / 10 6 / 10 0 / 10 Passed 08Ό 230 00 © © r-1 200 200 0 / 10 4 / 10 6 / 10 0 / 10 Passed 00 © © 440 . Layer 0.8mm thick) Ethylene-vinylacetate copolymer (*1) Ethylene-vinylacetate copolymer (*2) Magnesium hydroxide (*3) Magnesium hydroxide (*4) γ -methacryloxypropyltrimetoxisilane Electron beam exposure dose (kGy) 0 to under 20 sec. 1 20 to under 40 sec. 1 40 to under 60 sec. 60 sec. or over Judgement Initial tensile strength (kg / mm2) Initial elongation (%) Insulated Wire (conductor 0.8mm φ, Insul Longest burning time distribution (Number of specimens: 10) Flame retardance VW-1 test fUL StdJ_Notes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 / zm, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 / Zm, BET specific surface area = 7 m / g,Surface not treated (C) Insulating Tube - 1 (Embodiments 23 to 28)Flame retardant resin compositions shown in Tables 6 and 7 were formed into tubular moldings having an inner diameter of 6.4 mm and a wall thickness of 0.5 mm by using a melt extruder (full flight type, 45 mm in diameter, L / D = 24, compression ratio = 2.5) at an extruding temperature of 160*C. The tube-shaped moldings were irradiated by 100 kGy of electron beam at an accelerating voltage of 2 MeV so that the tube layers were crosslinked.The electron beam irradiation was omitted for the tubes ofEmbodiments 25 and 28 in Table 6 and Comparative Example 15 in Table 7.To check the thus obtained tube for its flame retardance, an iron bar of6.4 mm in diameter, the same size as the inner diameter of the tube, was inserted into the tube and the all tubing flame test was carried out on ten specimens of each example. If even one of the 10 specimens of each example caused it to burn 60 seconds or longer, burn the kraft paper, or burn the absorbent cotton, the example was judged to have failed the test.Further, to check the tubes for their mechanical strength, a tensile test (pulling speed: 500 mm / min.) was carried out and the tensile strength and the elongation (gage length: 20 mm) of three specimens of each example were measured and the average values were obtained.Embodiments 23 to 28 in Table 6 are tubes produced by using the resin compositions of Embodiments 1, 3, and 7 with acetate added thereto and tubes produced by using the resin compositions of Embodiments 8, 10, and 14 with calcium carbonate added thereto, respectively.All of the specimens have passed the all tubing flame test and the distribution of the burning times has been in the range of under 20 seconds with a probability over 50 %.With respect to the tubes of Embodiments 24 and 27 in Table 6 with T-methacryloxypropyltrimetoxisilane added thereto as silane coupling agent, it has been found that they not only prove to be flame retardant but also satisfy the requirements provided in the UL Standards, over 1.06 kg / mm2 in tensile strength and over 100 % in elongation (Comparative Examples 13 - 15)Comparative Examples 13 to 15 in Table 7 are tubes using the resin compositions of Comparative Examples 1, 3, and 5, respectively. Although they all passed the all tubing flame test, the combustion times of more than 50 % were distributed in the range exceeding 20 seconds, from which these examples were found to be inferior in flame retardance to Embodiments 23 to 25 in Table 6 containing acetate and Embodiments 26 to 28 in Table 6 containing calcium carbonate.Embodiment00 <N 100 180 © i-H © 7 / 10 3 / 10 0 / 10 0 / 10 Passed 0.38 720 <N 100 150 © co i-H 100 5 / 10 5 / 10 0 / 10 0 / 10 Passe 1.15 175 CO <N 100 180 © <N 100 8 / 10 2 / 10 0 / 10 0 / 10 Passe 0.75 295 _ © © © © Φ in © m <N © © © oo fH © i-H © i-H © i-H 0 / 1 1 / 0 Pass 9Ό © 24 100 150 © co i-H 100 7 / 10 3 / 10 0 / 10 0 / 10 Passe 1.24 188 23 100 180 20 100 7 / 10 3 / 10 0 / 10 0 / 10 Passe 0.95 368 T a . o Φ m o Φ Φ Φ CD CD CD © © CD CD Φ © © © <N h h > s Φ h Φ ti Wall thic] ymer (*1) ymer (*2) metoxisilan Si o β Φ CD o 3 © 20 to un 40 to un 60 sec. o Judgemi z—\ Ol 3 3 So o o z—s. z—\ φ fH diameter 6.4mm φ ne-vinylacetate cop ne-vinylacetate cop sium hydroxide (*3 sium hydroxide (*4 sium acetate (*5) m acetate (*6) m carbonate (*7) m carbonate (*8) hacryloxypropyltrii )n beam exposure d .s ° Φ 43 be g © 43 d 1-1 O ® 3 φ © :9 | be C -g ss « retardance VWrLStd.)_ tensile strength (ki elongation (%) | 3» Ethyle: Ethyle: Magne Magne Magne Calciui '3 13 o '3 13 o Φ 3 1 Electrc 4 Flame test iii Initial InitialNotes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 Um, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Um, BET specific surface area = 7 m / g,Surface not treated * 5: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Um * 6: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Um * 7: Primary particle diameter = 0.04 Um, Surface treated with stearic acid *8: Primary particle diameter = 1.5 Um, Surface not treatedTable 7Tube (Inner diameter 6.4mm φ , Wall thickness 0.5mm) Comparative Example 13 14 15 Ethylene-vinylacetate copolymer (*1) 100 100 100 Ethylene-vinylacetate copolymer (*2) Magnesium hydroxide (*3) 200 180 Magnesium hydroxide (*4) 180 γ -methacryloxypropyltrimetoxisilane 1 Electron beam exposure dose (kGy) 100 100 0 Longest burning time distribution (Number of specimens: 10) 0 to under 20 sec. 0 / 10 1 / 10 0 / 10 20 to under 40 sec. 2 / 10 7 / 10 2 / 10 40 to under 60 sec. 8 / 10 2 / 10 8 / 10 60 sec. or over 0 / 10 0 / 10 0 / 10 Flame retardance VW-1 test (UL Std.) Judgement Passed Passed Passed Initial tensile strength (kg / mm2) 0.82 1.21 0.55 Initial elongation (%) 385 165 850Notes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m / g,Surface not treated (D) Heat-shrinkable Tube - 1 (Embodiments 29 and 30)Flame retardant resin compositions shown in Table 8 were formed into tube-shaped moldings with an inner diameter of 3.2 mm and a wall thickness of 0.5 mm by using a melt extruder (full flight type, 45 mm in diameter, L / D = 24, compression ratio = 2.5) at an extruding temperature of 160*C. The tubeshaped moldings were irradiated by 100 kGy of electron beam at an accelerating voltage of 2 MeV to have the tube layer cross-linked.The cross-linked tubes were left to be preheated in a constanttemperature bath set at a temperature of 160*C for 3 minutes. Then, by the method of sending compressed air into the tube, the tube were expanded to increase the inner diameter to 7 mm and, thereupon, the tubes were taken out of the constant-temperature bath and cooled in water so that the tubes would keep the shape as expanded to provide beat-shrinkable tubes.To check the flame retardance of the obtained heat-shrinkable tube, an iron bar with an outer diameter of 3.3 mm was inserted into the heatshrinkable tube having its diameter expanded to 7 mm and then the tube was left in a constant-temperature bath set at a temperature of 150*C for three minutes so that the beat-shrinkable tube would beat-shrunk to fit over the periphery of the iron bar. Ten specimens of each example were subjected to the all tubing test, in which, if one of the ten specimens caused it to bum 60 seconds or longer, burn the kraft paper, or bum the absorbent cotton, the example was judged to have failed the test.Further, to check the mechanical strength of the tube, specimens of the heat-shrinkable tube, which had been heat-shrunk by being left for three minutes in a constant-temperature bath set at a temperature of 150*C, were subjected to a tensile test (pulling speed 500 mm / min) and the tensile strength and elongation (gage length 20 mm) were measured on three specimens of each example and the average values were obtained.Embodiments 29 and 30 in Table 8 are heat-shrinkable tubes produced by using the resin compositions of Embodiments 1 and 8 in Table 1. All of them have passed the all tubing test and the burning times of many of them have been distributed in the range between 0 and 20 seconds to prove their excellence in flame retardance.(Comparative Example 16)Comparative Example 16 in Table 8 is a heat-shrinkable tube produced by using the resin compositions of Comparative Example 1. Though all of the specimens of this comparative example passed the all tubing test, many of the burning times were distributed in the range between 40 and 60 seconds to indicate that they were inferior in flame retardance to Embodiment 29 in Table with acetate added thereto and Embodiment 30 in Table 8 with calcium carbonate added thereto.Table 8Tube (Heat-shrunk inner diameter 3.2mm φ, Wall thickness 0.5mm) Embodiment Compara tive Example 29 30 16 Ethylene-vinylacetate copolymer (*1) 100 100 100 Ethylene-vinylacetate copolymer (*2) Magnesium hydroxide (*3) 180 180 200 Magnesium hydroxide (*4) Magnesium acetate (*5) 20 Calcium acetate (*6) Calcium carbonate (*7) 20 Calcium carbonate (*8) γ -methacryloxypropyltrimetoxisilane Electron beam exposure dose (kGy) 100 100 100 Longest burning time distribution (Number of specimens: 10) 0 to under 20 sec. 8 / 10 7 / 10 0 / 10 20 to under 40 sec. 2 / 10 3 / 10 3 / 10 40 to under 60 sec. 0 / 10 0 / 10 7 / 10 60 sec. or over 0 / 10 0 / 10 0 / 10 Flame retardance VW-1 test (UL Std.) Judgement Passed Passed Passed Initial tensile strength (kg / mm2) 0.90 0.75 0.78 Initial elongation (%) 385 310 390Notes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 / im, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Um, BET specific surface area = 7 m / g,Surface not treated * 5: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Um * 6: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Um * 7: Primary particle diameter = 0.04 U m, Surface treated with stearic acid * 8: Primary particle diameter = 1.5 Um, Surface not treated (E) Flat Cable - 1 (Embodiments 31 to 36)Flame retardant resin compositions shown in Tables 9 and 10 were mixed and extruded to cover up both faces of parallel conductors, which were formed of seven conductors arranged in parallel at intervals of 2.0 mm (each conductor being a stranded wire of seven tinned annealed-copper wires of a diameter of 0.127 mm) with a covering thickness of 0.30 mm by the use of Mitsuba Seisakusho-made extrusion coating apparatus, 50 mm in diameter) at a temperature of 160*C. The coated example was irradiated by 200 kGy of electron beam at an accelerating voltage of 2 MeV to provide a flat cable. Embodiments 33 and 36 in Table 9 and Comparative Example 19 in Table 10 were not subjected to the process of electron beam irradiation.The flame retardance of the thus obtained flat cable was tested by the VW-1 test such that 10 specimens each of the flat cable examples were tested and the example was judged to have failed in the test when even one of the 10 specimens caused it to burn 60 seconds or longer, burn the kraft paper, or burn the absorbent cotton.Further, to check the flat cables for their mechanical strength, a tensile test (pulling speed: 500 mm / min) was carried out. The tensile strength and elongation (gage length: 20 mm) were measured of three specimens of each example and their average values were obtained.Embodiments 31 to 33 in Table 9 are flat cables produced by using the resin compositions of Embodiments 2, 5, and 7 in Table 1 with acetate added thereto, respectively, and Embodiments 34 to 36 in Table 9 are flat cables produced by using resin compositions of Embodiments 9, 12, and 14 in Table 2 with calcium carbonate added thereto, respectively.All of the specimens have passed the VW-1 test and many of their burning times have been distributed within the range of 0 to 20 seconds to prove their excellence in flame retardance.Further, the flat cables of Embodiments 32 and 35 with 7 methacryloxypropyltrimetoxisilane added thereto as a silane coupling agent have been found to be excellent not only in flame retardance but also in mechanical strength, i.e., they have attained higher values than those provided in the UL Standards, over 1.06 kg / mm2 in tensile strength and over 100 % in elongation.(Comparative Examples 17 to 19)Comparative Examples 17 to 19 in Table 10 are flat cables produced by using the resin compositions of Comparative Examples 2 and 4 in Table 3, respectively.All of the flat cables passed the VW-1 test. However, many of the burning times were distributed within the range of 20 to 40 seconds, whereby these were found to be inferior in flame retardance to Embodiments 31 to 33 inTable 9 mixed with acetate and Embodiments 34 to 36 in Table 9 with calcium carbonate added thereto.Table 9fl Φ 36 100 180 o rH o 6 / 10 4 / 10 0 / 10 0 / 10 Passed 0.50 450 35 100 • 150 30 200 6 / 10 4 / 10 0 / 10 0 / 10 Passed 1.23 165 34 100 150 50 200 8 / 10 2 / 10 0 / 10 © 1-rt © Passed 0.65 260 o Td fl o o o © φ © o w co co Ό o rH 00 rH o rH o rH ω 0 / 1 0 / 1 Pass © © Td 32 100 150 30 <N 200 7 / 10 3 / 10 0 / 10 © © Passe 1.25 210 Td rH CO 100 150 50 200 o rH O rH 0 / 10 0 / 10 0 / 10 Passe © 00 © 243 co fl HH 00 υ υ Φ Q Φ Φ •S Φ CO co co o o h o co 9> <N kl kl > fl μ Φ Ά Φ z—s z—s 04 'fl Td fl Ά fl o Φ fl and kl h a co •a ►* O fl fl o fl o -M fl 3 sec. h φ bo z-s μι Φ Φ β o o © fl a co fl fl t>> o Φ φ CO o <N © •S a HH HH o o z**\ z**\ ϋ o Φ Ά rH bo ·© a a ite cop ite cop co nd 'S ΙΩ z**\ ♦. 00 « 44 >> ft sure d 1 Φ 42 VW- 44 & 43 fl o fl (Conductor 0.127i Layer 0.3mm thick) Ethylene -vinylaceta Ethylene-vinylaceta Magnesium hydroxi Magnesium hydroxi Magnesium acetate Calcium acetate (*6 Calcium carbonate ι Calcium carbonate ι γ -methacryloxypro Electron beam expo be a fl ° 43 d H 2 ® 43 fl -fl fl Φ s a i a-S'i o ® s ►3 3 S 1 Flame retardance test (UL Std.)_ Initial tensile stren Initial elongation (9Notes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m / g,Surface not treated * 5: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Mm * 6: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Mm * 7: Primary particle diameter = 0.04 Mm, Surface treated with stearic acid * 8: Primary particle diameter = 1.5 Mm, Surface not treatedTable 10Flat Cable (Conductor 0.127mm φ , stranded 7 wires; Insul. Layer 0.3mm thick) Comparative Example 17 18 19 Ethylene-vinylacetate copolymer (*1) Ethylene-vinylacetate copolymer (*2) 100 100 100 Magnesium hydroxide (*3) 200 Magnesium hydroxide (*4) 200 200 r -methacryloxypropyltrimetoxisilane 2 2 Electron beam exposure dose (kGy) 200 200 0 Longest burning time distribution (Number of specimens: 10) 0 to under 20 sec. 0 / 10 1 / 10 0 / 10 20 to under 40 sec. 6 / 10 6 / 10 5 / 10 40 to under 60 sec. 4 / 10 3 / 10 5 / 10 60 sec. or over 0 / 10 0 / 10 0 / 10 Flame retardance VW-1 test (UL Std.Y Judgement Passed Passed Passed Initial tensile strength (kg / mm2) 0.70 1.18 0.55 Initial elongation (%) 225 150 670Notes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 Um, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Um, BET specific surface area = 7 m / g,Surface not treated.(J) Flat Cable - 2 (Embodiments 37 - 42)The flame retardant resin compositions shown in Tables 11 and 12 were mixed and extruded by the use of Mitsuba Seisakusho-made T-die extruder onto one surface of a biaxially stretched polyester film at a temperature of160*C to a thickness of 0.30 mm to provide a laminating tape of polyester film.Two tapes were placed on both faces of parallel conductors, formed of seven conductors arranged in parallel at intervals of 2.0 mm (each conductor being a stranded wire of seven tinned annealed-copper wires of a diameter of 0.127 mm) such that the uncoated sides of the polyester film turn out. Then, the parallel conductors were encased by the insulating cover with the use of a heat laminator set at a temperature of 160*C. An electron beam of 200 kGy was applied to the insulating cover at an accelerating voltage of 2 MeV to provide a flat cable.Embodiments 39 and 42 in Table 11 and Comparative Example 22 inTable 12 were not subjected to the process of electron beam irradiation.The flame retardance of the thus obtained flat cable was tested by theVW-1 test such that 10 specimens each ofthe flat cable were tested and the flat cable was judged to have failed in the test when even one of the 10 specimens caused it to burn 60 seconds or longer, bum the kraft paper, or burn the absorbent cotton.Embodiments 37 to 39 in Table 11 are flat cables using the resin compositions of Embodiments 2, 5, and 7 in Table 1 with acetate added thereto, respectively, and fabricated by the method of laminating polyester films, whileEmbodiments 40 to 42 are flat cables produced by using the resin compositions of Embodiments 9, 12, and 14 in Table 2 with calcium carbonate added thereto, respectively, and fabricated by the method of laminating polyester Aims.In the VW-1 test, all of the flat cables have passed the test and the 5 burning times have been in the range of under 20 seconds with a probability of over 50%, though the burning times have been slightly longer than those of the flat cables of Embodiments 31 to 36 shown in Table 9 because of the structure laminated with polyester Aims.(Comparative Examples 20 to 22)Comparative Examples 20 to 22 in Table 12 are flat cables respectively using the resin compositions of Comparative Examples 2 and 4 in Table 3 and fabricated hy the method of laminating polyester films. When subjected to the VW-1 test, all of them passed the test but more than 50 % of their burning times were over 20 second.Although the magnesium hydroxide content of Comparative Examples to 22 in Table 12 was greater than that of Embodiments 37 to 39 orEmbodiments 40 to 42 in Table 11, it was found that they were unable to satisfy simultaneously both requirements for the burning times provided in the VW-1 test to be within 20 seconds with a probability of 50 % or above and for the tensile strength and elongation provided in the UL Standards.Table 11Embodiment 42 100 180 o rH © 5 / 10 5 / 10 0 / 10 0 / 10 Passed 41 100 150 30 <N 200 © rd © 4 / 10 0 / 10 0 / 10 Passed 40 100 150 50 200 5 / 10 01 / S 0 / 10 0 / 10 Passed 39 100 180 o © 5 / 10 5 / 10 0 / 10 0 / 10 Passed 38 100 150 30 <N 200 6 / 10 4 / 10 0 / 10 0 / 10 Passed co 100 150 50 200 6 / 10 4 / 10 0 / 10 0 / 10 Passed stranded 7 wires; Insul. Ethylene-vinylacetate copolymer (*1) Ethylene-vinylacetate copolymer (*2) Magnesium hydroxide (*3) Magnesium hydroxide (*4) Magnesium acetate (*5) Calcium acetate (*6) Calcium carbonate (*7) Calcium carbonate (*8) r -methacryloxypropyltrimetoxisilane Electron beam exposure dose (kGy) 0 to under 20 sec. 20 to under 40 sec. 40 to under 60 sec. 60 sec. or over Judgement Flat Cable (Conductor 0.127mm φ , Layer 0.3mm thick) Longest burning time distribution (Number of specimens: 10) Flame retardance VW-1 test (UL Std.)_Notes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 Um, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Um, BET specific surface area = 7 m / g,Surface not treated * 5: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Um * 6: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Um * 7: Primary particle diameter = 0.04 Um, Surface treated with stearic acid *8: Primary particle diameter = 1.5 Um, Surface not treatedTable 12Flat Cable (Conductor 0.127mm φ , Insul. Layer 0.3mm thick) stranded 7 wires; Comparative Example 20 21 22 Ethylene-vinylacetate copolymer (*1) Ethylene-vinylacetate copolymer (*2) 100 100 100 Magnesium hydroxide (*3) 200 Magnesium hydroxide (*4) 200 200 γ -methacryloxypropyltrimetoxisilane 2 2 Electron beam exposure dose (kGy) 200 200 0 Longest burning time distribution (Number of specimens: 10) 0 to under 20 sec. 0 / 10 1 / 10 0 / 10 20 to under 40 sec. 2 / 10 3 / 10 4 / 10 40 to under 60 sec. 8 / 10 7 / 10 6 / 10 60 sec. or over 0 / 10 0 / 10 0 / 10 Flame retardance VW-1 test (UL Std.) Judgement Passed Passed PassedNotes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 jttm, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 JLtm, BET specific surface area = 7 m / g,Surface not treated.(G) High Voltage Wire for Direct Current - 1 (Embodiments 43 to 50)With a tinned annealed-copper wire of an outer diameter of 0.8 mm used as the conductor, a material obtained hy adding 0.3 part hy weight of pentaerythrityltetrakis ( 3-(3,5-t-butyl-4hydroxyphenyl)propionate ) to 100 parts by weight of high density polyethylene (density = 0.954, melt flow rate = 0.8: ASTM D1238) was formed into an insulating layer over the conductor by the use of a melt extruder (full flight type, 45 mm in diameter, L / D = 24, compression ratio = 2.5).To form a covering layer (jacket), pellets shown in Tables 13 and 14 were melt-extruded over the insulating layer by the use of a melt extruder (full flight type, 45 mm in diameter, L / D = 24, compression ratio = 2.5) so that the outer diameter would become 4.2 mm and, thereafter, 150 kGy of electron beam was applied at an accelerating velocity of 5 MeV onto the obtained article to provide a high voltage DC electric wire.A high-voltage cut-through test was carried out on the obtained highvoltage DC electric wire by applying a DC voltage of 60 kV to the wire under a load of one pound each applied to both ends of the wire specimen in a Geer oven at a temperature of 125^ and with n = 3.A withstand voltage test (Method II) was carried out, after having electric wire specimens heat-aged in a Geer oven at a temperature of 158^ for seven days, by turning the wire specimen seven turns around a mandrel, 0.5 inch in outer diameter, and then applying a DC voltage of 50 kV to the wire specimen in a Geer oven at a temperature of 125Ό and with n = 3. Under the heading of High-voltage Cut-through Test and Withstand Voltage Test in Tables 13 and 14, there are shown the times taken for the first one to breakdown in each three specimens.In a heat aging test, residual elongation rates (%) of electric wire specimens were assessed after being heat-aged in a Geer oven at a temperature of 158C for seven days.Here, residual elongation rate (%) = (elongation of heat-aged 15 specimen / initial elongation) x 100 and a residual elongation rate of 65 % or above was set as the passing mark. A burning test was carried out according to the VW-1 test and assessment was made with n = 10.Embodiments 43 to 50 in Table 13 are high-voltage DC electric wire using, as the covering layer, the resin compositions in which 100 parts by weight of ethylene-vinylacetate copolymer resin are compounded with 150 to 190 parts by weight of magnesium hydroxide as metal hydroxide and 10 to 50 parts by weight of magnesium acetate or calcium acetate as acetate.All of the specimens have passed the VW-1 test. Further, they have exhibited a mechanical strength to exceed the values provided in the UL Standards, over 1.06 kg / mm2in initial tensile strength and over 100 % in initial elongation. They have also proved to pass the test for physical property after heat aging, the high-voltage cut-through test, and the withstand voltage test.(Comparative Examples 23 and 24)Comparative Examples 23 and 24 shown in Table 14 are high-voltage DC electric wire using, as the covering layer, the resin composition in which 100 parts by weight of ethylene-vinylacetate copolymer resin are compounded with 200 parts by weight of magnesium hydroxide as metal hydroxide.While the resin compositions of Comparative Examples 23 and 24 in Table 14 passed the tests for the initial mechanical property and the residual elongation rate after heat aging, the high-voltage cut-through test, and the withstand voltage test, the high-voltage DC electric wire using such material, though its magnesium hydroxide content was greater than that in Embodiments 43 to 50 in Table 13, failed the VW-1 test.Table 13Embodiment 50 100 160 40 <N 150 1.33 / 165 89 00 Λ 00 Λ 10 / 10 Passed <35 TP 100 © © r-l o 150 1.14 / 162 TP © 00 Λ 00 Λ 10 / 10 Passed 00 TP 100 160 © TP <N 150 1.28 / 168 CO 00 00 Λ 00 Λ 10 / 10 Passed t- TP 100 190 o 150 1.32 / 175 LO © 00 Λ 00 Λ 10 / 10 Passed © TP 100 150 © LO <N 150 1.25 / 160 00 00 00 Λ 00 Λ 10 / 10 Passed LO TP 100 160 © <N rd 150 1.22 / 160 co © 00 Λ 00 Λ 10 / 10 Passed TP TP 100 160 © TP <N 150 1.26 / 158 IO 00 00 Λ 00 Λ 10 / 10 Passed CO TP 100 190 o 150 1.23 / 160 © © 00 Λ 00 Λ 10 / 10 Passed DC High-volt El. Wire (conductor 0.8mm φ , Insul. Layer 0.4mm thick, Jacket Outer diam. 4.2mm φ ) Ethylene-vinylacetate copolymer (*1) Ethylene-vinylacetate copolymer (*2) Magnesium hydroxide (*3) Magnesium hydroxide (*4) Magnesium acetate (*5) I Calcium acetate (*6) Calcium carbonate (*7) Calcium carbonate (*8) γ -methacryloxypropyltrimetoxisilane Electron beam exposure dose (kGy) Initial Tensile Strength (kg / mm2) / Elongation (%) Residual elongation rate (%) after 7-day aging at 158°C High-voltage cut-through holding time (Hr) Withstand voltage test holding time (Hr) Flame retardance (VW-1 test (UL std.)Notes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 |im, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 Mm, BET specific surface area = 7 m / g,Surface not treated * 5: Made by Wako Jun-yaku K.K., Average particle diameter = 3 Mm * 6: Made by Wako Jun-yaku K.K., Average particle diameter = 3 lim * 7: Primary particle diameter = 0.04 lim, Surface treated with stearic acid *8: Primary particle diameter = 1.5 lim, Surface not treatedTable 14DC High-volt El. Wire (Conductor 0.8mm φ, Insul. Layer 0.4mm thick, Jacket outer diam. 4.2mm φ) Comparative Example 23 24 Ethylene-vinylacetate copolymer (*1) 100 Ethylene-vinylacetate copolymer (*2) 100 Magnesium hydroxide (*3) Magnesium hydroxide (*4) 200 200 γ -methacryloxypropyltrimetoxieilane 1 2 Electron beam exposure dose (kGy) 150 150 Initial Tensile Strength (kg / mm^ / Elongation (%) 1.38 / 140 1.45 / 132 Residual elongation rate (%) after 7-day aging at 158°C 78 70 High-voltage cut-through holding time (Hr) >8 >8 Withstand voltage test holding time (Hr) >8 >8 Flame retardance VW-1 test (UL Std.) 8 / 10 Not Passed 7 / 10 Not PassedNotes:* 1: Vinyl acetate content = 25 %, Melt flow rate = 3 * 2: Vinyl acetate content = 45 %, Melt flow rate = 1 * 3: Average particle diameter = 0.7 / im, BET specific surface area = 7 m / g,Surface treated with stearic acid * 4: Average particle diameter = 0.7 / lm, BET specific surface area = 7 m / g,Surface not treated.According to the invention, as described above, insulated wires and jacketed wires, tubes, heat-shrinkable tubes, flat cables, and high voltage DC electric wire which are free from the problem of producing harmful gas when burned, having high mechanical strength and excellent flame retardance can be obtained. These products can be used for wiring work in electronic computers, OA equipment, consumer electronic appliances such as audio and video apparatuses, vehicles, marine vessels, and so on.

Claims

1. A flame retardant resin composition compounded of thermoplastic resin, metal hydroxide, and acetate comprising: 100 to 250 parts by weight of the metal hydroxide; and 5 to 50 parts by weight of the acetate based upon 100 parts by weight of the thermoplastic resin.

2. A flame retardant resin composition according to claim 1 wherein the thermoplastic resin is at least one ethylene -α-olefin copolymer selected from the group consisting of ethylene-vinyl acetate copolymer, ethylene-ethyl acrylate copolymer, ethylene-methyl methacrylate copolymer, ethylenemethacrylic acid copolymer, and ethylene-methyl acrylate copolymer.

3. A flame retardant resin composition according to claim 2, wherein the ethylene-a-olefin copolymer is an ethylene-vinylacetate copolymer containing 6 to 50% by weight of vinyl acetate component and having a melt flow rate of 0.5 to 30 measured at 190°C and under a load of 2.16 kg.

4. A flame retardant resin composition according to claim 1, further comprising an organosilicon compound coupling agent expressed by the formula (1): Yl X R — Si - Y2 Y3 where R denotes alkyl including acryl, methacryl, or allyl and Yl, Y2, and Y3 denote an atomic group selected from the group consisting of alkyl, alkoxyl, and halogen, in the amount of 0.1 to 10 parts by weight based on 100 parts by weight based on 100 parts by weight of the thermoplastic resin. PI 990020515. The flame retardant resin composition according to claim 1, wherein the acetate has a particle diameter of 0.5 to 5pm and is at least one member selected from the group consisting of magnesium acetate, sodium acetate, potassium acetate, zinc acetate, copper acetate, ferrous acetate, calcium acetate, aluminum acetate, nickel acetate, cobalt acetate, gallium acetate, silver acetate, tin acetate, barium acetate, cerium acetate, lead acetate, and beryllium acetate.

6. An insulated wire provided with an insulation layer made of a flame retardant resin composition compounded of thermoplastic resin, metal hydroxide, and acetate, comprising: 100 to 250 parts by weight of the metal hydroxide; and 5 to 50 parts by weight of the acetate, based upon 100 parts by weight of the thermoplastic resin.

7. An insulated wire according to claim 6, wherein the insulation layer is crosslinked.

8. A thin-wall high-strength insulated wire comprising a conductor, having an outer diameter of up to 1.0 mm, and an insulation layer covering said conductor, said insulation being a flame retardant resin composition compounded of thermoplastic resin, metal hydroxide, and acetate, comprising: 100 to 250 parts by weight of the metal hydroxide; and 5 to 50 parts by weight of the acetate, based upon 100 parts by weight of the thermoplastic resin and having a thickness of 0.1 mm to 1.0 mm and wherein said insulation layer is cross-linked. PI 990020519. An insulating tube made of a flame retardant resin composition compounded of thermoplastic resin, metal hydroxide, and acetate, comprising: 100 to 250 parts by weight of the metal hydroxide; and 5 to 50 parts by weight of the acetate, based upon 100 parts by weight of the thermoplastic resin.

10. An insulating tube according to claim 9, wherein said tube is cross-linked.

11. A heat shrinkable tube obtained, after a tube-formed product made of a flame retardant resin composition compounded of thermoplastic resin, metal hydroxide, and acetate, comprising: 100 to 250 parts by weight of the metal hydroxide; and 5 to 50 parts by weight of the acetate, based upon 100 parts by weight of the thermoplastic resin has been crosslinked, by expanding the tubeformed product in its radial direction under a heated condition and, thereupon, cooling the tube to maintain its expanded form.

12. A flat cable with a parallel arrangement of a plurality of conductors spacedapart and enclosed in an insulation layer, said insulation layer being made of a flame retardant resin composition compounded of thermoplastic resin, metal hydroxide, and acetate, comprising: 100 to 250 parts by weight of the metal hydroxide; and 5 to 50 parts by weight of the acetate, based upon 100 parts by weight of the thermoplastic resin.

13. A flat cable according to claim 12, wherein said insulation layer is crosslinked.

14. A flat cable according to claim 12, wherein at least one face of said insulation layer is laminated with a film made of polymeric material. PI 9900205115. A flat cable according to claim 13, wherein at least one face of said insulation layer is laminated with a film made of polymeric material.

16. A flat cable according to claim 12, wherein said insulation layer is irradiated 5 with ionizing radiation.

17. A high-voltage DC electric wire according to claim 16, wherein said insulating layer and said jacketing are cross-linked. 10 18. A high-voltage DC electric wire provided with a coating of an ethylene-aolefin copolymer resin composition as an insulation layer covering the conductor and provided with a jacketing made of a flame retardant resin composition compounded of thermoplastic resin, metal hydroxide, and acetate, comprising: 100 to 250 parts by weight of the metal hydroxide; and 5 to 50 parts by weight of the acetate, based upon 100 parts by weight of the thermoplastic resin over said insulation layer.