Process for the preparation of polyacetal copolymers.
Patent Information
- Application Number
- MYPI1999002548
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 1999-06-21
- Publication Date
- 2000-03-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Current processes for preparing polyacetal copolymers, such as POM, require complex and costly steps to deactivate initiators and eliminate unstable chain ends, involving multiple intermediate steps like deactivation, filtration, and hydrolysis, which increase production costs and reduce efficiency.
A continuous process using strong protonic acids as initiators added in finely divided form to the monomer mixture, allowing direct transfer of crude polymer to a mixing unit where excess monomers are removed under reduced pressure, and stabilizers and additives are incorporated, eliminating the need for deactivation steps and achieving high stability without additional processing.
This process reduces production costs by eliminating two customary steps, achieving high stability and suitability for commercial use without deactivators, and results in POM copolymers with excellent heat stability, suitable for applications like automotive and electrical industries.
Abstract
Description
Process for the preparation of polyacetal copolymersA continuous process for the preparation of poly acetal copolymers from 1,3,5-trioxane and the comonomsrs known for this purpose using strong protonic acids as an initiator, in which the initiator is added in an amount of 0.01 to 0.6 ppm, based on the total amount of rronomers, in finely divided form to the monomer mixture, after the polymerization step the crude polymer is transferred from the polymerization reactor to a mixirg unit without further intermediate steps, excess monomer is removed from the crude polymer in the mixing unit or between polymerization reactor and mixing unit by applying reduced pressure and, if desired, generally customary slabilizers, assistants, fillers, reinforcing materials and / or colorants are incorporated into the polymer in the mixing unit.FIGURE 1PI 99002548Process for the preparation of polyacetal copolymersThe present invention relates to a process for the continuous preparation of polyacetal copolymers from trioxane with comonomers known for this purpose, in which the initiates used are strong protonic acids which are added in finely divided form to the monomer mixture, and in which, immediately after the polymeiization step, the crude polymer is transferred directly, i.e. without the use of deactivators, to a mixing unit in which further additives are incorporated into the polymer. The material prepared in this manner has excellent ί tabiiity.Polyacetal copolymers have ieen known for many years and have proven useful as material in a variety of applications. Since their market launch about 30 years ago, in particular polyacetal copolymers based on polyoxymethylene (POM) hsve become established as extremely useful industrial materials in many applications. The POM copolymer is widely used, especially as the corstruction material in automotive construction and in the electrical indust y. Examples of this are to be found in the application brochures of the lolyacetal producers.After the polymerization step, polyoxymethylene copolymers in the form of crude polymers have insi fficient stability and are therefore usually subjected to particular wo'king-up steps before they are mixed with stabilizers and assistants in a further step, usually with the use of a granulating extruder, and an thus brought into the commercial state.The process steps for working up the crude polymers are known to include:a) the deactivation of ini iatorsb) the elimination of uns able chain endsc) the removal of uncon ,erted monomersd) the incorporation of s:abilizers and assistantsThere are many known indus:rial processes which combine these steps for the preparation of polyacet: I copolymers (Sabel et al. in Becker / Braun (Editors), Kunststoffhandbuoh [Plastics Manual] Volume 3 / 1, 1992). Common to all known processes is the fact that cationic initiators are used for the preparation of copo ymers of 1,3,5-trioxane. It is also generally known that the cationic polymerization does not involve any true termination reaction in which the active center is irreversibly destroyed (cf. Elias H-G., MakromolekCile [Macromolecules], Huthig and Wepf Verlag, 4th Edition, page 513 et seq. and Penzek et al., Cationic Ring Opening Polymerization in: Advances in Polymer Science No. 68 / 69, page 122).This is important precisely fc r the copolymerization of trioxane since living, i.e. non-deactivated, chain «nds and unconverted radicals of the initiators may decompose the polymer during the further processing. All known preparation processes therefore include a step in which the remaining amount of initiator is reactivated after the polymerization. The considerable complication o' this procedure greatly increases the costs of the preparation.Thus, it is known that the dsactivation of the initiator is carried out in the aqueous phase or in an o ganic solvent, subsequent filtration, washing and drying steps being required. The deactivation of the initiator with the addition of different deacti cators can also be effected in the melt (DE 3703790). The deactivation step is often carried out in combination with the demonomerization and he elimination of unstable chain ends (DE 37 38 632 and EP 0 137 305) EP 0673 955 describes a process in which crude polymer is treated w th a steam stream which also contains small amounts of volatile base. In this way, unconverted residual monomer is removed and the initiator is deactivated. JP 05059255 states that the initiator is deactivated by ac ding alkali metal or alkaline earth metal oxides to the polymer melt.The elimination of unstable terminal groups, which usually remain in the crude polymer after the polymerization and in particular lead to chain degradation when the polymer is heated, is also a usual process step in the preparation of POM copolymers. Hydrolysis, in which the crude polymer is dissolved in a solvent under elevated pressure at elevated temperature is often used for this purpose. After the hydrolysis, theThis shows that all process3S known to date entail considerable effort which serves only to remcve unstable terminal groups and residual monomers, to deactivate initiators or their reaction products and to work up the results of undesired seco idary reactions.The object is therefore to develop a process which makes it possible economically to prepare .table copolymers of 1.3,5-trioxane in a continuous process while avoiding the deficiencies of the known processes.The object is achieved if strong protonic acids are used as initiator and are added in finely divided form to the monomer mixture and if, after the polymerization step, the pol'mer is transferred without intermediate steps from the polymerization rea:tor to a mixing unit in which the material is melted, the conventional additives and assistants are added and the material is thus brought into a form suitable for sale.The invention thus relates O a continuous process for the preparation of polyacetal copolymers from 1,3,5-trioxane and the comonomers known for this purpose using a strong protonic acid as an initiator, in which the initiator is added in an amount of from 0.01 to 0.6 ppm, based on the total amount of monomers, in finely divided form to the liquid monomer mixture, the crude polymer is transferred from the polymerization reactor directly to a mixing unit immediately after the polymerization step without further intermediate steps, excess monomer is removed from the crude polymer in the mixing unit or between the polymerization reactor and mixing unit by applying reduced pressure ind, if desired, generally customary stabilizers, assistants, fillers, reinforcirg materials and / or colorants are incorporated into the polymer in the mixir g unit.The advantages of the process according to the invention are that neither a process step for deactiva ion of initiators nor a separate process step for the elimination of unstable terminal groups is required in the entire process sequence. Thus, two process steps customary to date are saved by the process, with the result tha POM preparation is more economical.That POM copolymers no longer have to be treated with deactivators after .... „ r„. .·.,a.·.,av. „ .,,,., „w-«, .'·ηι=, addition of the stabilizers and assista its customary to date was surprising and overcomes a prejudice which has existed to date. In particular, it is surprising that the POM c ipolymers obtained without the addition of deactivators and without additional hydrolysis nevertheless have a very high stability.According to the invention, strong protonic acids are used as initiators, it being possible in principle to use all strong protonic acids. Heteropoly acids, perchloric acids or perfluoroalkanesulfonic acids are particularly suitable, trifiuoromethanesulfonic acid being preferred. The concentration ofthe initiators is generally i ι the range from 0.01 to 0.6 ppm, preferably in the range from 0,03 to 0.4 apm. and particularly preferably in the range from 0.05 to 0.19 ppm, based in each case on the monomer mixture. It is essential for the process a ccording to the invention that the initiator be added in finely divided torn- to the monomer mixture comprising trioxane and the comonomers.This is advantageously dont by dissolving the initiator in a solvent which is selected from the group consisting of aliphatic ethers, such as ethylene glycol dimethyl ether or dietnylene glycol dimethyl ether, aliphatic acetals, such as formaldehyde diulkyl acetals, cyclic acetals, such as 1,3dioxolane, or cycloaliphatic ethers, such as 1,6-dioxane. Surprisingly, cyclic acetals and formaldehyde dialkyl acetals having 3 to 9, preferably 3 to 5 carbon atoms, fo example formaldehyde dimethyl acetal, formaldehyde diethyl acetal, formaldehyde dipropyl acetal and formaldehyde dibutyl aceta , are particularly suitable. The weight ratio of initiator to solvent is usually 1:100 to 1:100,000, preferably 1:500 to 1:10,000. When formaldehy de di alky I acetals are used as a solvent for the initiator, the amount of so vent is preferably 3.4 to 34 mmol per kg of monomer mixture.Suitable comonomers for :he preparation of the POM copolymers are compounds which are copclymerizable with 1,3,5-trioxane. Cyclic acetals, preferably formals, having 5 to 11, preferably 5 to 8, ring members are preferred. Suitable cyclic at etals are in particular cyclic formals of aliphatic or cycloaliphatic α,ω diols having 2 to 8, preferably 2, 3 or 4, carbon atoms, whose carbon chain may ba interrupted by an oxygen atom at intervals of 2 carbon atoms. In additior, cyclic ethers having 3 to 5, preferably 3, ring aliphatic or aromatic radicals. The comonomers may be used, either individually or in combination, in an amount of 0.01 to 20% by weight, preferably 0.1 to 10% by weight, in particular 1 to 7% by weight, based in each case on the monomer mixture, the stated mass fraction in % by weight corresponding to the sum of the amounts of all comonomers used.Substances which are known to act as molar mass regulators may also be added to the monomer mixtu'e. In particular, formaldehyde dialkyl acetals having 3 to 9, preferably 3 to 5, carbon atoms, eg. formaldehyde dimethyl acetal, formaldehyde diethi I acetal, formaldehyde dipropyl acetal and formaldehyde dibutyl acetal, are especially suitable for this purpose. The regulator is used in general in an amount of up to 2% by weight (= 20,000 ppm), preferably 0.1 to 1.5% by weight, particularly preferably 0.3 to 1.2% by weight, based on the moncmer mixture.All continuously conveying a id mixing units can be used as polymerization reactors. The use of twin-sc ew extruders is advantageous. In a preferred embodiment, shown in Figuie 1, the polymerization takes place in such a polymerization reactor (1) £t melt temperatures above 65°C, the initially liquid reaction mixture whicli contains the molten monomers, the initiator and optionally the regulator solidifies during the polymerization to give a hard material which leaves the polymerization reactor (1) in the form of small particles via a drop staff (5) in which reduced pressure prevails. As a result of the reduced prissure, unconverted monomers are removed from the polymer and then (ither fed to separate working-up or completely condensed and are recycled to upstream of the polymerization reactor. The polymer leaving the polymerization reactor falls, without further intermediate steps, directly into another continuously conveying and mixing unit (6), which is preferably likewise a twin-screw extruder. In this unit, the polymer is meltec, mixed with the conventional stabilizers and assistants and brought into :he commercial form.The designations in Figure 1 have the following meanings:1: polymerization reactor : feed of trioxane and comonomers : feed of the initiator dissolved in a solvent and optionally of the regulator- -I-! arc5: drop shaft for the crude polymer : continuously conveyin') and mixing unit : feed of stabilizers and assistants : product in commercial formIt is also possible to carry out ail process steps in a single unit or to use a combination of more than two interconnected units. In each case, however, residual monomer is remo / ed from the crude polymer between the polymerization zone and tt e addition of stabilizers and assistants by applying reduced pressure.Antioxidants, acid acceptor:. lubricants, waxes, UV stabilizers, nitrogencontaining co-stabilizers anc other products known as stabilizers for POM may be used as stabilize_s and assistants, either individually or in combination.All fillers and reinforcing materials customary and known for plastics, in particular polyacetal copolymers, may be used as fillers and reinforcing materials.ExamplesExample 1: A molten moromer mixture comprising 97% by weight of trioxane and 3% by weight of dioxolane was fed at a rate of 3 kg / h to a twin-screw extruder used a: a polymerization reactor. 0.15 ppm, based on the monomer mixture, of tifluoromethanesulfonic acid dissolved in 1,6dioxane and 1050 ppm, based on the monomer mixture, of formaldehyde dimethyl acetal were added continuously to the monomer mixture. The crude polymer obtained wes conveyed at the outlet of the polymerization reactor via a drop shaft in.o a second twin-screw extruder. Unconverted monomers were removed by means of reduced pressure and were absorbed in a water circula.ion. The amount of monomer separated off per hour was 600g. In the secc nd twin-screw extruder, the crude polymer was melted and was mixed wiih a mixture of 46% by weight of Irganox 245 (produced by Ciba Spezial ;hemie), 31% by weight of amide wax Hostalub FA, 15% by weight of trical ;ium citrate and 8% by weight of dicyandiamide. This mixture was fed to tt e second extruder at a rate of 15.6 g / h. After passing through the discharge zone, the polymer was taken off as a molten-. . -, ,,p I-,-, [ρ,Β- -|-|-|θ granules thus obtained were thoroughly dried and were kept under inert gas at a temperature of 240 'C for several hours to determine the heat stability.The material obtained is sui able for further use in injection molding or extrusion process and has vei y good heat stability.Examples 2-4: The procedi re was as in Example 1, the amount of trifluoromethanesulfonic acid oeing varied (for data, cf. Table 1).Example 5: A molten moncmer mixture comprising 97% by weight of trioxane and 3% by weight c f dioxolane was fed at a rate of 3 kg / h to a twin-screw extruder used as a polymerization reactor. 0.1 ppm. based on the monomer mixture, of tri luoromethanesulfonic acid dissolved in 300 ppm, based on the monomer mixture, of formaldehyde dimethyl acetal and a further 850 ppm, based on the monomer mixture, of formaldehyde dimethyl acetal were addec continuously to the monomer mixture. The crude polymer obtained was conveyed at the outlet of the polymerization reactor via a drop shaft inlo a second twin-screw extruder and further processed as in Examples 1-4.Comparative experiment: A commercial POM copolymer (Hostaform) was also tested as in Example 1 with respect to its heat stability. The result is shown in Table 1.Table 1Example T riflui iromethanesulfonic acid PPm Heat stability * Weight loss % / h 1 0.15 0.25 2 0.08 0.22 3 0.18 0.30 4 0.06 0.20 5 0.10 0.21 Comparison Commercial product 0.42* Heat stability measured as rate of weight loss in % / h at a temperature of 5 240°C under inert gas.
Claims
Claims:
1. A continuous process for the preparation of polyacetal copolymers from 1,3,5-trioxane and the comonomers known for this purpose using strong 5 protonic acids as an initiator in which the initiator is added in an amount of 0.01 to 0.6 ppm, based cn the total amount of monomers, in finely divided form to the monomer Tiixture, after the polymerization step the crude polymer is transferred fron the polymerization reactor to a mixing unit without further intermediate steps excess monomer is removed from the crude 10 polymer in the mixing unil or between polymerization reactor and mixing unit by applying reduced pres; ure and, if desired, generally customary stabilizers, assistants, fillers, reinforcing materials and / or colorants are incorporated into the polymer in the mixing jnit 152. The process as claimed in claim 1, wherein at least one heteropoly acid, perchloric acid or perfluoroalkanesulfonic acid, preferably trifluoromethanesulfonic acid, or a combination thereof is used as the initiator.
203. The process as claimed i i claim 1 or 2, wherein the amount of initiator is in the range from 0.03 to 0 4 ppm, preferably in the range from 0.05 to 0.19 ppm, based in each case 3n the monomer mixture. PI 990025484. The process as claimed in any of claims 1 to 3, wherein the initiator is added in the form of a solution in l solvent to the monomer mixture.5 5. The process as claimed in claim 4, wherein at least one aliphatic or cycloaliphatic ether or one aliphatic or cycloaliphatic acetal is used as the solvent for the initiator.
6. The process as claimed ir claim 4 or 5, wherein 1,3-dioxolane, 1,6-dioxane 10 or a formaldehyde dialkyl acetal, preferably formaldehyde dimethyl acetal, formaldehyde dipropyl acetal or formaldedehyde dibutyl acetal, is used as the solvent for the initiator.
7. The process as claimed ir any of claims 4 to 6, wherein the weight ratio of 15 initiator to solvent is 1:100 co 1:100,000, preferably 1:500 to 1:10,000.
8. The process as claimed in any of claims 4 to 6, wherein formaldehyde dialkyl acetals are used in an amount of 3.4 to 34 mmol per kg of monomer mixture as solvents for the initiator9. The process as claimed in any of claims 1 to 8, wherein a twin-screw extruder is used as the polymerization reactor and / or mixing unit PI 99002548