AI Technical Summary
Existing low pill copolyester fibers suffer from poor pilling performance, especially in humid conditions, and undergo significant hydrolysis during processing, affecting their relative viscosity and performance properties.
A basic-dyeable ethylene terephthalate copolyester polymer with 0.5 to 3 mol% sodium sulfonate salt of isophthalic acid, polymerized in the presence of a trifunctional or tetrafunctional silicate ortho ester, is developed, resulting in staple fibers with improved pill resistance and moisture management, even when exposed to moisture, through specific processing techniques that maintain desired viscosities and cross-sectional shapes.
The new copolyester fibers exhibit excellent pill resistance and moisture management, achieving unprecedented RTPT pill ratings of at least 2.5 after 30 minutes, with improved aesthetics and tactile properties, while maintaining desirable performance even after hydrolysis, outperforming previous 100% polyester fabrics.
Abstract
Description
TITLELOW PILL COPOLYESTERFIELD OF THE INVENTIONThis invention concerns improvements in low pill copolyester, as described hereinafter, and is more particularly concerned with a new copolyester composition that provides staple fiber that is capable of forming yarns, fabrics and garments that have a combination of excellent pilling performance, particularly in the presence of humidity / moisture, aesthetics and tactility (hand), especially such staple fiber of non-round cross-sections as multigrooved scalloped-oval cross-sections that retain such cross-section so their fabrics have outstanding qualities of moisture-management, dryness and comfort as well as exhibiting minimal pills (particularly in the presence of moisture), and downstream products thereof, intermediates therefor and processes for obtaining or processing any of these.BACKGROUND OF INVENTIONThis invention is an improvement in, and, largely, a selection from the range of low pill copolyester described and claimed by Anderson et al. in U.S. Patent No. 5,817,740 (DP-6585-A) and corresponding WO 98 / 36027, which are expressly incorporated herein by reference. The extensive background in polyester etacle fibers ar.c previous efforts to ixrcve their pi.lino perfcrnar.ee has been described therein, including trie following prior pubiications , U.S.Patents Nos. 2,071,251 (farotbers) 2,465,319 (Whinfield and Hickson), 4,110,316 (Edging and Lee), 4,113,704 (Maclean and Estes), 4,145,729 (Goodley and Shiffler), 4,945,151 (Goodley and Taylor), 3,104,450 (Christens et al], 3,335,211 (Mead et al), 3,018,272 (Griffwg and Remington), 5,559,205 and 5,507,765 (Hansen et al.),1C 3,576,773 (Vagina / ), and 5,300,626 and 5,478,909 (Jehl et al.), Ludewig in Polyester Fibres, Chemistry and Technology, published m German in 1964 and in English m 1571 by John Wiley and Sons, Ltd., Oxford et al in WO 92 / 13120, and Duncan m U.S. SIR H1275. Also specific non-round cross-sections referred to herein as multi-grooved cross-sections have been disclosed in U.S. Patents Nos. 5,591,523, 5,626,961 and 5,736,243 (Aneja) and in U.S. Application No. 08 / 778,462 (DR6550, Rocpj, now allowed, and earlier cross-sections, referred to as scaiioped-oval, in 3,914,488 (Gorrafai , 4,534,625 (Franklin) and 4,707,407 (Clark et al.).These prior publications are expressly incorporated herein by reference and are discussed in much more detail in U.S. Patent No. 5,817,740 and WC 98 / 36027, referred to hereinabove.Aforesaid U.S. Patent No. 5,617,740 describes and claims a basic-dyeabie, ethylene terephthalate copolyester polymer that contains 0.5 to 3 mol% of a sodium, sulfonate salt of a glycollate of iscphthalic acid, and that has been polymerized in the presence of a trifunctional or tetrafunctional silicate ortho ester m amount 0.05 to 0.5¾ by weight, and that contains titanium dicxioe in amount 0.1 tc 2% by weignt, said copclyester being of relative viscosity about 3 to 12 LRU and about 1 ί: 3 celta RV , as defined, esoeciailv in form of staple fiber that provides fabrics ci acceptable hand and cf improved pill rating as compare· with fabrics cf commercially-available fibers of scalloped-oval cress - sect ion known as Type 702W, as described therein fas Comparison B therein;, and compared also hereinafter. The relative viscosities (LEV, delta RV and NRV) and how they are measured are described in the aforesaid U.S. Patent, and an understanding cf them is important for understanding .0 the present invention, as will be apparent hereinafter The silicate ester acts as a chain-branching agent during polymerization but may be hydrolyzed downstream i.e., later.As m the aforesaid patent, terms such as “filament and “fiber are often used generically.The objective of the present invention is to provide copclvester polymer and fiber cf still further improved pill rating and / or other advantages as compared with what was specifically disclosed in aforesaid U.S. Patent No. 5,617,740 and WO 98 / 36027.We had noted that pilling in 100% polyester garments had been much worse in specific areas of garments, such as the neck, collar, armpits, and upper thigh (groin), and also after undergoing laundering. But we had net understood the effect cf moisture on measurements of pilling, for instance when making RTET pill ratings following ASTM D-3512-82. This will be discussed hereinafter. Another matter that we had not sufficiently understood was the hydrolysis of the polymer in fiber form, especially during downstream precessing, cr its effect upon NRV.- 4 SUMMARY OF THE INVENTIONAccording to one aspect cf the invention, there is provided a basic-dyeable ethylene terephthalate copolvester polymer that contains 0.5 to 3 mol% cf a sodium. sulfonate salt of a glyccllate of isophthalic acid, and that has been polymerized in the presence of a tnfunctior.ai or tetrafunctional silicate ortho ester in amount (TES %' at least 0.05% by weight, said copolyester Ceing of LRV relative viscosity about 8 co about 12 and about 1 to 3 delta RV, as defined, wherein said amount (TES %) corresponds to the Non-AcidRelative Viscosity (NRV) of the polymer as defined by the polygon ASCDEFGA in Figure 1 of the accompanyingDrawings.Preferably said amount (TES %) corresponds to the (NRV) as defined by the triangle JKLJ m Figure 1 of the accompanying Drawings.An important aspect of the invention is the provision of such polymer in the form of fibers. We have found that such new selected copolyester polymer compositions can be spun and drawn and converted into stapje fiber that can provide knit fabrics of 100% polyester that have an excellent pill rating, even when tested in presence of moisture. We have also found chat such fabrics can be made to have a hand that is acceptable for previously unattainable end-uses, hand being rather subjective.According to another aspect cf the invention, therefore, there is provided basic-dyeable ethylene terephchalace copolvester staple fiber of denier perLt atc^t 6 f: Lament: acc_i 1.5 ;o aoo_: 5 (about. c;e:<' anc out length abcut 20 mn :o about 10 ;.τ„ suer, as is capable of providing knitted fabrics of 100% polyester fiber of RTPT pill rating as defined herein 5 of at leasi 2.5, preferably at least 3, after a period of 30 minutes and sometimes mere. Such pill ratings as defined herein have not previously been obtained by a practicable process for knitted fabrics of 100% polyester fiber. As indicated, we have made such 0 fabrics with a good hand.We have found, according to the invention, that some of such new selected copolyester polymers can be formed into staple fiber cf non-round cross-section, especially multi-grooved and scalloped-oval crosssections that have excellent cross-sectional shape retention, for instance an excellent multi-grooved configuration that can provide excellent comfort properties, such as moisture-management and dryness m fabrics, as well as excellent pilling performance anc tactile aesthetics.According to another aspect of the invention, therefore, there is provided basic-dyeable ethylene terephthalate copolyester staple fiber of multi-grooved peripheral cross-section of aspect ratio abcut 1.3:1 to about 3:1 and groove ratio as defined abcut 0.50:1 to about 0.55:1. Groove ratio is described by Aneja m U.S. Patent No. 5,626,961 (DP-6365-A) and by Roop inApplication No. 06 / 773,462 (UP-6550) filed January 3, 1957, and new allowed, and is hereby defined as the ratio of the separation distance (such as d^) between grooves cn either side of the major axis of the cross.such as b^) ci a bulge measured as described therein.chain - Drar.t “,d =5As indicated, the silicate ester ir. trie polymer can be hydrolyzed. This tends to happen over time when the polymer in the form of fiber is exposed to moisture, for instance in the atmosphere, and especially during aqueous treatments at elevated temperatures, such as dyeing of fabrics and garments.As the chain-brancher links are hydrolyzed, the NRV tends to decrease significantly more than the LRV. Consequently, the NRV of polymer and fiber that have been spun having viscosities according to the invention as described already and that oar. be processed io have highly desirable performance properties as have already been described may well decrease below the ranges already described (with reference to polygon ABCDEFGA and triangle JKLJ) although, when spun, that polymer provided the basis for making fibers, fabrics and garments of such highly desirable performance properties because that polymer, as-spun, was within the ranges described (with reference to polygon ABCDEFGA, anc preferably triangle JKLJ). So another aspect of the invention is fiber having a (TES wt %) amount that may not always correspond to the NRV, as described for the amounts (TES %) in relation to such polygon or triangle.According to another aspect of the invention, therefore, there is provided a basic-dyeable ethylene terephthalate copolyester polymer that is in the form of fiber and that contains C.5 to 3 mcl? of a sodium sulfonate salt of a glycollate of isophthalic acid, and that has been polymerized m the oresence oftri function: =. or tetrafunotional si_icate ortho estcn in amcunt r ΓΪ3 at least 0.05¾ by weight, said finer being of IF.' / relative viscosity about 8 to about 12, as defined, an: i having a (TES wt amount that 5 corresponds to the Non-Acid Relative Viscosity (NEV) cfthe fiber as defined by the pentagon MNCPCtf in Figure 2 of the accompanying Drawings.Pre: ferably said (TES %) amount corresponds to 10 the NRV as c iefined by the quadrilateral RS7UE in Figure 2 cf the zompanying Drawings .We ise herein the expression. (TES wt %) amount to ; .ndicate such amounts in fiber that are 15 relevant to the pentagon and quadrilateral in Figure 2 m contrast to the expression amount (TES %) (whichis also by weight) that is relevant to the polygon and triangle in Figure 1.Preferably, also provided are staple fiber ofdenier, cut length, and providing RTPT pill ratings as hereinabove and also preferably of cross-section as hereinabove .□ Also provided, according to the invention, are downstream products of such fibers, including yarns,fabrics and garments and intermediate products, such as continuous ί filaments, tows and slivers, (including blends with ether fibers, especially with cotton or 3 0 wool, being natural fibers), and processes for obtaining a: ;d for processing any of them. Preferred= precesses are as fol.ows, i: being understood : he ter?, monomer is used for convenience, as oligomer m.av be formed m a vessel before entering a poi / merization vessel .t.tatAccordingly, there is provided a continuous process for preparing such new basic-dveable ethylene terephthalate copolyester polymer comprising (1) forming a monomer by a transesterification reaction1C between ethylene glycol and dimethyl terephthalate m a mole ratio of about 1.5-2.5:1 while introducing into the reaction a trifunotiona1 or tetrafur.ctional silicate ortho ester and the sodium salt of dimetnyl 5sulfoisophthalate mixed in with at least some of said ethylene glycol, preferably at a temperature of aocut 1CC-15C“C, ;Z'. passing the resulting monomer, preferably at a temperature of about 2CC-240°C, via transfer piping while introducing therein a slurry of finely divided titanium dioxide in some of said2C ethylene glycol to a polymerization vessel, and (2) effecting polymerization of said monomer in a series of polvm.erizat ion vessels while reducing the pressure to remove byproduct ethylene glycol and increasing the temperature, and preferably sequentially reducing tne pressure to about 1 to 7 mm Hg.There is also provided a continuous process for preparing such new basic-dyeable ethylene terephthalate copolyester polymer comprising (1) forming a monomer by3C a transesterification reaction between ethylene glycol and dimethyl terephthalate m a mole ratio of about 1.5-2.5:1 while continuously introducing into the reaction the sodi-m salt of dimethyl preterably at a temperature of about 10C-150oC, (z:passing tne resulting monomer, preferably at a temperature of about 200-240°C, via transfer piping while introducing therein a slurry tf finely divided titanium dioxide in additional ethylene glycol and the ethylene giyccllate form of the silicate ortho ester mixed in with additional ethylene glycol to a effecting polymerization m.er m a series of polymerization vessels ng the pressure to remove byproduct polymerizaticn vessel, and (3 10 of said mo while redo· ethylene glycol and increasing the temperature, and preferably sequentially reducing the pressure to abcu 1 to 7 mm Fin.There is further provided a continuous process for preparing sue?, new basic-dyeable ethylene terephtha cpclyester polymer comprising (1) forming a mcncmer by an esterificat ion reaction between 20 ethylene glycol and terephthalic acid in a mole ratio of about 1.5-2.5:1, (2) passing the resulting monomer, preferably at a temperature of about 200-240°C, while introducing therein ethylene glycollates of the sodium, salt of 5-suifoiscphthalic acid and cf a trifunctional 25 or tetrafunctional silicate ortho ester in additional ethylene glycol and a slurry of finely divided titanium dioxide in additional ethylene glycol to a polymerization vessel, and (3) of said monomer m a series cf3C while reducing the pressure to remove byproduct ethylene glycol and increasing the temperature, and preferably sequentially reducing the pressure tc abc effecting polymerization do!vmerizacion vessels to 7 mm He.-10r-oe:erac^y sjtn new ccpoivester pciymer is melt-epun .r.:s· filaments at a withdrawal speed of abcu 1200 co 1811 ypm (1100-1550 m / min), and drawn preferably about 2X-3.5X, preferably at a temperature cf about o0-100°C, crimped and then relaxed, preferabl at a temperature of about 100-175°C, and, if desired being annealed at a temperature of about 150-230°C before being crimped and relaxed. The resulting filaments including staple fiber) are preferably of 0.5 to 5 dof (about 0.5 to 6 dtex).BRIEF DESCRIPTION OF THE DRAWINGSFigure 1 is a plot of NRV vs. amount (TES %' as described herein in more detail.is a plot of NRV vs rein in more detail.(TES wt amountFigure 3 gives plots of RTPT pill ratings measured after time intervals as described hereinafter in more detail.DETAILED DESCRIPTION OF THE EMBODIMENTSAs indicated in the Background, the art contains much description relevant to the manufacture cf polyester polymer compositions, their melt-spinning (extrusion) mtc filamenrs, processing of the filaments, including conversion to staple fiber, processing of staple fiber into spun yarn, processing of spun yarn into fabrics, and the treatment of fabrics, such as dyeing and finishing, and the testing cf such fabrics and Garments for their performance and would ce so :: ciecursur filaments ana staple, redundant it- repeat such disclosure that is already available :n the art; the disclosures in the art referred tc herein, and in art cited therein are 5 incorporated herein specifically by reference.Useful staple fiber for conversion into spun yarn and for use m fabrics thereof is generally of dpt about 0.5 to 5 {0.5 to 6 dtex) and of cut length about20 mm to about 10 era. The new copolyester may, however, be used for other applications, which may require different shaped articles and / or other parameters .A copclyester having ethylene terephthalate repeat units and containing also a sodium sulfonate salt of a glycollate of isopnthalic acid has been used to improve dyeability for many years, as indicated w references such as we have mentioned hereinabove.Suitable amounts of such metal salt comonomer are generally 0.5 to 3 mol %, as disclosed in the art. The improved dyeability of the new polyesters according to the present invention is an important advantage, and overcomes one of the complaints'' about homopolyesierPET fiber, but is not by itself a novel feature. Much of the disclosure hereinafter is directed to an ethylene terephthalate copolyester composition that has been found especially useful and advantageous, namely the sodium salt of dimethyl 5-sulfcisophthalate modified with tetraethyl orthosilicate, as these comonomers have been available and have given such excellent and surprising results according to the invention. However, variations may be used, as disclosed w the art .Likewise, the use of cxysiiicon compounds, such as tetraethyl orthosi11cate , to improve pilling performance of polyester fibers was suggested generallv and specifically in the prior art, such as mentioned hereinbefore, so is not by itself a novel feature.No combination, however, features of the present invention taught, ar.d, importantly, pilling serious problem for the polyester despite the many suggestions publ:of all claimed has been speci has remained a fiber industry ished m the ar' allyAs indicated already, the viscosities (LRV, NRV and delta F.V’, are fully defined in the aforesaid U.S. Patent No. 5,517,740 and WO 93 / 35027, and as will be understood, depending on the processing of the fibers and fabrics containing the polymers, hydrolysis is likely tc take place so the NRV will decrease as a result and the delta RV may disappear, but traces of the silicate will remain and we have found that pilling performance of fabrics made from fibers spun from filaments having viscosities as claimed has been excellent and these attributes will reveal use of the present invention upstream.The invention for the polymer that is made and spun into fioers may be represented by a basic-dyeable ethylene terephthalate copclyeeter polymer that ί 1 ' contains a sodium sulfonate salt of a glycollate otC isophtnalic acid, (2) generally contains a delusterant. preferably titanium, dioxide, as described m aforesa-C U.S. Patent No. 5,317,740 and WO 96 / 35027, and (3) thatPOINT NRV (TES WT %) AMOUNT >1 a . 9 0.31 N 11 . J C 'Ί 0 11.3 0.24 P 10 . B 0.05 0 8 . 9 0 . 05 P. 9.2 0.10 s 9.2 0.29 T 10 . 2 0.29 u 9.7 0.10LINE EQUATION QM MP.v = a . 9 MN TES w: %) = 0.31 Mt NRV = 11.2 0? (TES wt %) = 0.4 0 NRV -4.23 PC (TES wt ΐ) = 0.05 RS NRV = 9.2 ST (TES w: %) = 0.29 Tt iTES wt %) = 0.39 NRV -3.57 UK (TES wt %) = 0.10Figure 3 provides plots cf RT?T pill ratings measured as described hereinafter (both without ar.d with added moisture) over a period of time for fabrics made from, fiber and polymer described in Example 1 of the invention herein and, for comparison, from Type _e 702W fiber wrier, has a somewhat similar cross-section. Tne imcroveme.nt obtainable by the invention in this regard is very striking. The RTPT Pill Ratings measured as described hereinafter are shown in Figure 3 as follows :1. Solid shapes indicate measurements without added moisture, whereas open shapes indicate measurements in the presence of added moisture as described;2. Triangles were ratings made on knitted fabrics as described hereinafter in Example I according to the invention;3. Squares were ratings made on knitted fabrics as described hereinafter for Type 702W commerciaily-available fiber;Despite the abundance of prior literature, no one previously has disclosed how to provide knit fabrics of 100% polyester staple fiber from an ethylene terephthalate polymer that could give a pill rating after 30 cr 60 minutes as high as 4 or 5, using bothRTPT pilling test procedures as described hereinafter, unlike what we have shown in Figure 3.The invention is further illustrated in the following Examples; all parts, percentages and30' proportions are by weight unless indicated otherwise, polymer weight recipes generally being calculated wict regard to the weight cf the polymer in the filaments.convent; i ona 1 unusThe yarn properties are measurer w denier being a metric unit, and so the tensile troperties are given as measured in gpd, but conversions into SI units are also given in parentheses (g / dtex), and the Crimps per Inch, CPI, have similarly been converted, and are likewise shown in parentheses (CPcm) .The test Drocedures were as described in aforesaid U.S. Patent No. 5,817,740, with some refinement however of the pilling test procedure, more rigorous testing conditions having proved desirable because of commercial needs as the presence of moisture has been found to affect the results. The testing (following ASTM D-3512-82) described in the aforesaid U.S. Patent used dehumidified air at a pressure of 3 psi (about 21 kPa' . The ratings described herein were all carried out with air at 2.5 psi (about 17.5 kPa), which we have found to be more rigorous. In addition2C co ratings that were measured using dehumidified air as for the measurements in the aforesaid U.S. Patent, however, ether measurements were made in the presence of moisture added by squirting water twice (applying a total of abcut 1.04 grams of water) into the tester every 30 minutes. As will be understood, therefore, the RTPT ratings are.only truly comparable when all the fabrics are tested under the same conditions, so the RTPT ratings herein should not be compared with those in the U.S Patent, and the RTPT ratings herein are given both for testing without added water and in the presence of added moisture, as described above. The procedure for preliminary treatment of the knit fabrics was also chanced from that described in aforesaid U.S. Patent No. 5,517,740 and was as follows. The knit fabric is secured by first being put into a 69 gallon (260 liter) Klauder, Weldon, Giles Model 25 PPW Sec,<-20l-.-e Machine w_tr. pado^e agitator rilled tat water.It is then heated ever a period of 5-10 minutes to 120° .- (49°Ci while being stirred. When that temperature is reached, the following reagents are adde<at 2% GW?, Soda Ash at 2% OWF, Lana-Foam at 2% OWF, being by weight calculated on the weight cf fiber, temperature is then raised to 220° F (10411(1 kg / cm2) and held for 20 min. The solution is drained and the fabric is rinsed, dried in a home 10 laundry type dryer (Kenmore) for 10 min at about 150° F (65° Cl and pressed with a dry iron (heated to permanent press setting) to simulate calendering. The resulting “finished fabrics are evaluated for aesthetics, “hand, and cover, as well as for pilling 15 by the procedure that has just been described. The following pilling test procedure should, therefore, be used tc measure a pill rating as defined herein.Stacie fiber of cut length 1.5 inches (38 mm.i is converted into yarn of 30 / 1 cc, which is knit on a 4820 feed single jersey, 22-cut machine. The knit fabric is “finished by the procedure that has just been described. The resulting finished fabric is evaluated fcr pilling following the procedure set out in the Random Tumble Pilling Tester Method ASTM D351225 82 and as described above, using dehumidified air at a pressure cf 2.5 psi (about 17.5 kPa), in the presence of moisture added by squirting water twice (applying a total of about 1.04 grams of water) into the tester every 30 minutes. Such ratings are made cn a scale of 30 1 to 5 by comparison with standard samples, 5 being the best, i.e., showing no pilling, whereas 1 is the worst, and the RTPT Pill Rating is an average cf 10 tests, i.e., cn 10 samcies from the same fabric.Klenzol 201 2 % OWF, GWF fiber . The :) at 15 psi n is . homeThe amounts (tes %) giver, in the following Ixamcles and herein were generallv measured on-21i.laments as spun L.e., seen after spinning and Defers drawing'' . Viscosity measurements herein were also generally measured on as-spun filaments. As indicated, however in more detail hereinabove, and especially mExample 11, the LRV remains relatively constant while the NRV tends to decrease and measurements have sometimes been made (where specifically indicated, as in Example 11) cn the fibers in fabrics that have been made and processed (finished) essentially as has just1C been described.EXAMPLE I of 9.1 LRV and of 12.4 Ethylene glycol (EG),An ethylene terephthalate copolyester polymer was made with approx. 2 mol % of sodium dimethyl 515 sulfoisophthalate and 0.27 weight % of tetraethyl erthos;1ioate, amount (TES , and containing 0.3 weight % of titanium dioxide and to have relative viscosities (after spinning)NRV, so 3.3 ARV, as follows.containing transesterification and condensation catalysts and, in approximate amounts by weight with respect to the weight of DMT added at this stage, 3.4 wt. % sodium dimethyl 5-sulfoisophthalate, C.40 wt. % of tetraethyl orthosilicate, and SO ppm of tetraisoprepyi titanate, was preheated to 149°C and metered into a transesterification reactor at a location above where dimethyl terephthalate (DMT) was also metered into the reactor at a temperature of approximately 175°C. The molar ratio of EG:DMT metered into the reactor was about 2.25:1. Temperature was controlled by a Dowtherm-heated oalandria at about 236° C at the base of the reactor. Low boiling materials (mainlv methanol and water) were taken overhead m vapor form and condensed, and part was recycled (refluxed) to the tOD of the reactor.Monomer oreduce-22 ; the case ot toe ca_anona ano was transferline to the first of threeA slurry containing titanium m additional c umcec via a mononet polymerization vessels, dioxide and a recipe of whitening agerEG was injected into the monomer transferline prior to entering the first vessel of these polymerization vessels. Phosphoric acid in additional EG was metered into this first polymerization vessel to deactivate the transesterification catalyst. The pressure in the first polymerization vessel was controlled at 100 mm Hg, and the temperature of the resulting prepolymer was controlled at 232°C. Prepolymer was transferred to the second polymerization vessel. Pressure in this second polymerization vessel was controlled at 35 mm Hg. Prepolymer of higher viscosity was removed from this vessel at a temperature of 261°C, and was transferred to the third polymerization vessel. Pressure ir. this third vessel was controlled to give the goal LRV and NRV (9.1 and 12.4, after spinning, respectively) was usually in the range of 1.5 to 4 mm Hg. The temperature of polymer leaving this third vessel controlled at approximately 269°C.mdFilaments of approximately 3 dpf (3.3 dtex) were melt-spun at 272°C from this ccpolyester by being extruded through a spinneret containing 1,506 capillaries at a rate of 92.4 lbs (41.9 Kg) per hour per position on 13 positions of a conventional spinning machine. The capillary orifice shape was three diamonds joined together as described by Aneja in U.S. Patent No. 5,736,243 (UP-6400) so as to make filaments of 4-grooved scalloped-oval cross-section similar to that described therein. The filaments were spur, at a withdrawal speed of 1500 ypm (about 1370 m / miru , quenched as described by Andersen et al m U.S. Patent No. 5,219,552, and collected in a can as a tow bundle-23of approximately 63,252 denier (about 70,280 dtex).The as-spun properties are given in Table I.cans of this tow were combined to give a tow of 548,184 filaments and 1.65 million denier (1.83 million dtex) , which was drawn at a draw ratio of 2.5X in hot spray water at a temperature of 85°C, then passed through a stuffer box crimper, and was then relaxed at a temperature of 123°C to give a final tow of denier 778,421 (864,912 dtex), i.e., of filaments of about 1.42 dpf (1.6 dtex). The resulting (drawn) properties are also given in Table I.The tows were cut to staple of length 1.5 inches (38 mm) after applying a conventional finish to give a level of about 0.22% finish on fiber, and the staple was converted to yarn (22 / 1 cc) and knit as described on a 48-feed single jersey, 22-cut machine to knit fabric that was finished so its pilling and other fabric characteristics could be evaluated as described. Fabrics had excellent pill performance (triangles in Figure 3) both when tested without added moisture and when tested in the presence of added moisture which was not only surprising but an astonishingly high rating for a 100% polyester knit fabric, especially as the fabric also showed excellent aesthetics, hand (tactility), body and cover.Measurements on fiber from the finished fabric gave an NRVof 9.6 and a (TES wt %) amount of 0.28%.-24TABLE IFilaments Tenacity gpd(g / dtex) Eb % Modulus gpd(g / dtex) DHS % CPI (CPcm) Groove Ratio Aspect Ratio As-spun 0.84(0.76) 289 19(17) Drawn 2.47(2.25) 19 38(35) 0.3 12(5) 0.91:1 1.6:1EXAMPLE IICopolyester was prepared and spun into 5 filaments, collected, combined and drawn, essentially as described in Example I except that the amount (TES %) was about 0.22 weight % and the viscosities were 9.3 LRV and 12.2 NRV, so 2.9 ARV, as spun, and the final tows were of denier 789,384 (877,093 dtex), i.e., the filaments were of about 1.44 dpf (1.6 dtex). The properties are given in Table II.-25TABLE XXFilaments Tenacity Eb Modulus DHS CPI Groove Aspect gpd(g / dtex) % gpd(g / dtex) % (CPcm) Ratio Ratio As-spun 1.0(0.90) 234 19(17) Drawn 2.1(1.9) 17 40(36) 1.5 16(6) 0.78:1 1.6:1The tows were cut to staple of length 1.5 inches (38 mm) after applying a conventional finish to give a level of about 0.26% finish on fiber, and the staple was converted to yarn (30 / 1 cc) and knit as described on a 48-feed single jersey, 22-cut machine to knit fabric that was finished so its pilling and other fabric characteristics could be evaluated as described. Fabrics had excellent pill resistance both when tested without added moisture and when tested in the presence of added moisture. To indicate how the NRV decreases more than the LRV, the filament viscosities after drawing were NRV = 11.2, LRV = 9.2, whereas viscosities in the finished fabric were NRV = 9.6, LRV = 8.6, and the (TES wt %) amount was 0.24 %.EXAMPLE IIICopolyester was prepared essentially as described in Example .1 except that the amount (TES %) was 0.19% by weight, and the viscosities were 9.9 LRV and 12.8 NRV, and so 2.9 ARV, and filaments of similar dpf and cross-section were spun, drawn and relaxed essentially as described in Example 1, and the properties of the spun and drawn filaments are in Table III. The tows of drawn filaments were processed essentially as described in Example 1, and the fabrics were also evaluated and had excellent aesthetics, as did those of Example 1, and their pilling performance was also far superior to that of prior Type 702W-26polyester fabrics, but slightly worse than that of Example 1. Measurements on fiber from finished fabric gave an NRV of 11.0 and a (TES wt %) amount of 0.2S %.TABLE IIIFilaments Tenacity gpd(gZdtex) eb % Modulus gpd(g / dtex) DHS % CPI (CPcm) Groove Ratio Aspect Ratio As-spun .96(.87) 211 18(16) Drawn 2.1(1.9) 17 41(37) 0.9 13(5) 0.85:1 1.6:1EXAMPLE IVCopolyester was prepared essentially as described in Example 1 except that the amount (TES %) was 0.244% by weight, and the viscosities were 10.3 LRV and 14.0 NRV, and so 3.7 ARV, and filaments of similar dpf and cross-section were spun, drawn and relaxed essentially as described in Example 1, and the properties of the spun and drawn filaments are in Table IV. The tows of drawn filaments were processed essentially as described in Example 1, and the fabrics were also evaluated and had excellent aesthetics as did those of Example 1, and their pilling performance was also far superior toprior polyester fabrics, but inferior to that of Example I. Measurements on fiber from finished fabric gave an NRV of 11.0 and a (TES wt %) amount of 0.29 %.-21table rvFilaments Tenacity Eb Modulus DHS CPI Groove Aspect gpd(g / dtex) I gpd(g / dtex) (CPcm) Ratio Ratio As-spun 1.0(0.90) 200 21 (19) prawn 2.5(2.2) 17 38135) 1.5 16(6) 0.78:1 1.6:1-2910I, b^t w:;.': a nigher amount (TES %) cf 0.322?, which. is above Lice Ξ2 of Figure I herein, as the NRV was 12.3. These values for Comparison X are pierced on Figure 1 as Cx, which is outside polygon ASCEEFGA in Figure 1, and estimazec values are plotted cn Figure 2, and are estimated to be outside pentagon MNOFQM. The fibers obtained from Comparison X showed considerable amounts of fly” waste (fiber and finish particles) during mill precessing steps cf carding, roving and spinning. Such fly” waste is undesirable due to reduced productivity and especially inferior yarn quality (poor uniformity;. The fabric had quite good pilling performance, however.COMPARISON YThe filaments for Comparison Y were spun from ccpclyester made essentially as described for Example 1 but of lower viscosity and amount (TES %), i.e., having10.4 NRV (i.e., outside Figure A3CDEFGA, being below10.5 NRV), and amount (TES %) of 0.086% (from approx.C.16 wt. % cf tetraethyl crthosilicate, with respect to the weight cf the DMT, and the molar ratio of EG-.DMT metered into the reactor was about 2.05:1). The values for Comparison Y are plotted on Figures 1 and 2 as C-, , the NRV having decreased to 10.0 NRV, and the (TES wt %) amount being 0.09, measured on fiber in the finished fabric.The fibers for Comparison Y are less desirable (although the fabric also had quite gcod pilling performance) because they could not be made efficiently owing to high levels of spinning breaks during melt spinning. In addition the fibers had very poor shape definition, as can be seen from the Groove Ratio in Table VI. As indicated, however, when filaments arem.ade and precessed into fabrics, the pilling oerfornance is creatly imoroved over Tvce 702W.COMPARISON ΖThe filaments for Comparison Z were spun from copclyester made essentially as described for Example 1 but of relatively high viscosity, having 13.2 NRV, and relatively low amount (TES %) of 0.157 weight % (using, with respect to the weight of the DMT, approx, 0.22 wt. % of tetraethyl orthosilicate, and approximately 62 ppm of tetraisopropyl titanate (TFT), and a molar ratio of EG: DMT metered into the reactor of about 2.00:1) .These values for Comparison Z are plotted on Figure 1 as ”C2, and are below line EF. Estimated values are plotted for Czon Figure 2 and are estimated to be outside pentagon MNOPQM.The fibers for Comparison Z were spun efficiently and precessed efficiently in the mill, but she resulting fabric showed inferior pill performance efter 30 minutes, as can be seen from Table V.TYPE 702WIn addition, fabrics were made and tested from commercially-available fibers, sold by DuPont as Type 702W. The copoiyester was made with 2 mole % of sodium dimethyl 5-sulfoisophthalate and had an DRV of 13.8.No tetraethyl silicate was used. The filaments were spun essentially as described in Example 1, except as follows. The extrusion was through 1,054 capillaries at a rate of 64.7 lbs (29.4 Kg) per hour per position on 16 positions of a commercial spinning machine. The resulting tow was of 16,864 filaments and of 50,592 denier (56,200 dtex). 33 cans of such tow were combined to a total of 556,=12 filaments, .7 mill ion denier (1.9 million dtex) filaments were relaxed atAfter drawing, the drawn123° to give a tmae ο o, c c (500,000 dtex) and averace-31(about 1.6 dtex, as for Example 1). The cut fibers were formed into yarns of 22 / 1 cc, and processed then essentially as described for Example I. The pill rating was only 1, the decreases in RTPT ratings when tested over a period of up to 2 hours being shown in Figure 3, but the performance experience in spinning and in mill and yarn processing has been good and the fabric has good hand and cover, demonstrating the need for a fiber with comparable aesthetics and performance in spinning and mill yarn processing, but improved pilling performance.The numerics in Table VI need little or no explanation beyond what is described in the art already referred to. A groove ratio of 1.0:1 would indicate the absence of any real groove in the sense that dy would be less than by, as described by Aneja in U.S. Patent No. 5,626,961, for example, but only a discontinuity in the periphery of the filament. Where '‘NONE” is recorded for Comparison Y, there was not even any such discontinuity, i.e., the drawn filaments were of smooth oval peripheral cross-section.TABLE VProcessing PTPT Pill Rating (30 min) Fiber Spinning Mill / Yarn Processing Without Moisture Added Moisture Examples I and II Good Good >3.5 >3.5 Examples III and IV Good Good >3.0 >2.5 Comparison X Good Poor >3.5 >3 Comparison Y Poor Good >3.5 >2.5 Comparison Z Good Good 1-3 1-2 (Type 702W) Good Good 1 1-32TABLE IIProperties of Filaments UsedFilaments Tenacity gpd(g / dtex) Eb % Modulus gpd(g / dtex) DHS % CPI (CPcm) Groove Ratio Aspect Ratio X-as-spun 1.1(1.0) 22 0 16(14) X-drawn 2.0(1.8) 21 34(31) 1.5 0.84:1 1.4:1 Y-as-spun 1.0(0.9) 27 1 18(16) Y-drawn 2.2(2.0) 20 40(36) 1 13(5) None 1.5:1 Z-as-spun 1.0(0.9) 21 2 11(10) Z-drawn 1.8(1.6) 22 40(36) 12(5) 0.84:1 1.43: 1 702W-as- spun 1.3(1.2) 23 9 18 (16) 702W- drawn 3.4(3.1) 37 34(31) 4.1 12(5) 0.68:1 1.7:1
Claims
1. A basic-dyeable ethylene terephthalate copolyester polymer that contains 0.5 to 3 mol Sofa sodium sulfonate salt of a glycollate of isophthalic acid, and that has been polymerized in the presence of a trifunctional or tetrafunctional silicate ortho ester in amount (TES %) at least 0.05% by weight, said copolyester being of LRV relative viscosity about 8 to about 12 and about 1 to 3 delta RV, as defined, wherein said amount (TES %) corresponds to the Non-Acid Relative Viscosity (NRV) of the polymer as defined by the polygon ABCDEFGA in FIG. 1 of the accompanying Drawings.
2. A polymer as claimed in claim 1, wherein said amount (TES %) corresponds to the (NRV) as defined by the triangle JKLJ in FIG. 1 of the accompanying Drawings.
3. The polymer of claim 1 in the form of staple fiber of denier per filament about 0.5 to about 5 and cut length about 20 mm to about 10 cm, said fiber providing fabrics of pill rating as defined herein after 30 minutes of 2.5 to 5.
4. The polymer of claim 3, wherein said fiber is of multi-grooved scalloped-oval peripheral cross-section of aspect ratio about 1.3:1 to about 3:1 and groove ratio as defined about 0.50:1 to about 0.95:1.
5. A basic-dyeable ethylene terephthalate copolyester polymer that is in the form of fiber and that contains 0.5 to 3 mol % of a sodium sulfonate salt of a glycollate of isophthalic acid, and that has been polymerized in the presence of a trifunctional or tetrafunctional silicate ortho ester in amount (TF5 %' = * -34least 0.05% by weight, said fiber being of LRV relative viscosity about 8 to about 12, as defined, and having a (TES wt %) amount that corresponds to the Non-Acid Relative Viscosity (NRV) of the fiber as defined by the 5 pentagon MNOPQM in FIG. 2 of the accompanying Drawings.
6. A polymer as claimed in claim 5, wherein said (TES wt %) amount corresponds to the (NRV) as defined by the quadrilateral RSTUR in FIG. 2 of the accompanying 10 Drawings.
7. The polymer of claim 5 in the form of staple fiber of denier per filament about 0.5 to about 5 and cut length about 20 mm to about 10 cm, said fiber providing 15 fabrics of pill rating as defined herein after 30 minutes of 2.5 to 5.
8. The polymer of claim 7, wherein said fiber is of multi-grooved scalloped-oval peripheral cross-section 20 of aspect ratio about 1.3:1 to about 3:1 and groove ratio as defined about 0.50:1 to about 0.95:1.