Printed wiring board and its manufacturing method
Patent Information
- Application Number
- MYPI1999003936
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1999-04-02
- Filing Date
- 1999-09-10
- Publication Date
- 2000-03-14
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional electroplating methods for printed circuit boards result in non-uniform copper layer thickness, low crystallinity, and high residual stress, leading to reliability issues and hindrances in achieving high-density wiring due to regional thickness variations and impurity contamination.
A constant-voltage pulse electroplating process is employed, using an electroless plated metal layer as the cathode and a plating metal as the anode, with intermittent voltage application and interruption to achieve uniform thickness and high crystallinity of the copper layer, reducing residual stress and improving elongation characteristics.
The process ensures a uniform copper layer thickness with high crystallinity and low residual stress, enhancing connection reliability and enabling fine line-definition patterns without the need for annealing, thus facilitating high-density wiring and improved insulation.
Abstract
Description
PRINTED WIRING BOARD AND ITS MANUFACTURING METHODDESCRIPTIONTECHNICAL FIELDThe present invention relates to a printed circuit board and to a method for production thereof. The invention further relates to plating methods and plating solutions which can be applied to the above production of printed circuit boards.BACKGROUND ARTWith the mounting need for higher functionality and further miniaturization of electronic equipment, advances in integration technology of LSI and in size reduction of components, and changes in the mounting mode, the demand for high-density wiring is getting greater in the field of printed circuit boards and, as a consequence, development of the so-called multilayer circuit boards comprising 3 or more conductor layers has been broadly undertaken.In view of the demand for higher wiring density in multilayer circuit boards, the so-called buildup multilayer circuit board is attracting attention. The buildup multilayer circuit board is manufactured by the technology disclosed in Japanese Kokai Publication Hei-4-55555, for instance. Thus, a core substrate board formed with a lower-layer conductor circuit is coated with an electroless plating adhesive comprising a photosensitive resin and, after the coat is dried, exposure to light and development are carried out to provide an interlayer resin insulating layer having openings for via holes. Then, the surface of this interlayer resin insulating layer is roughened with an oxidizing agent or the like and a thin electroless plated copper layer is formed on said interlayer resin insulating layer. Then, a plating resist is disposed thereon and a thick electroplated copper layer is constructed. The plating resist is then stripped off and the thin electroless plated copper layer is etched off to provide a conductor circuit pattern including via holes. This procedure is repeated a plurality of times to provide a multilayer printed circuit board.When, in the above process for fabricating a printed circuit board, the direct-current plating (DC plating) method, which is one of the conventional electroplating techniques, is used to provide said electroplated copper layer on a substrate surface, the current generally tends to be concentrated in the marginal area of the substrate surface as compared with the central area so that, as illustrated in Fig. 6, the thickness ti2of the copper layer in the marginal area of the substrate surface tends to become greater than the thickness tn in the central area, thus causing a regional variation in thickness of the electroplated copper layer.Since, in actual production runs, said substrate surface is the surface of a substrate board (work size substrate) having a large area corresponding to a large number of printed circuit boards integrated (specifically, the average one has an area of 255 to 510 mm square and there is even one having an area of about 1020 mm square at a maximum), the above tendency is particularly pronounced.In the manufacture of printed circuit boards, when the electroplated copper layer constituting a conductor circuit is not uniform in thickness, the insulation interval ti4between conductor layers in the marginal region of the substrate board is relatively smaller than the insulation interval ti3between conductor layers in the central region of the substrate board as shown in Fig. 7, so that the thickness of the insulating layer 1101b between conductor layers must be increased in order to insure a sufficient insulation in all regions of the printed circuit board but this is a hindrance to the implementation of high-density wiring.In addition, when the copper layer is formed by direct current plating, the crystallinity of the plated copper is low because of the use of an organic additive for improved throwing power.Moreover, the residual stress in the plated copper layer is fairly large so that the layer tends to develop cracks and other flaws and show low elongation and high tensile strength characteristics.Therefore, an annealing step for reducing the residual stress has been essential to the manufacture of printed circuit boards.As a technology for insuring the uniformity of thickness of the plated copper layer, it has been proposed to form a thick plated copper layer by electroless plating alone without electroplating. However, the thick plated copper layer formed by electroless plating is poor in ductility because of the unavoidable contamination of the layer with many impurities inclusive of the additives used. Therefore, when a thick plated copper layer is formed by electroless plating, the reliability for the wiring and connection is insufficient and in order to attain a sufficient degree of reliability, an annealing step is indispensable in this case, too.To overcome the above problem, a technology for constructing a thick plated copper layer by a constant-current pulse electrolytic technique has been proposed.The constant-current pulse electroplating process is characterized in that the plating current is controlled at a constant level and the representative waveform involved is a square wave.This technology may be further divided into the process {PC plating process; Fig. 8) in which the current is controlled by means of the square pulse wave available by repetition of the alternating supply (ON) and interruption (OFF) of the cathode current and the pulse-reverse electroplating method (PR plating method; Fig. 9) in which the current is controlled with a periodically reversed wave available by repetition of the alternating supply of cathode current and supply of anode current. As compared with the direct current electroplating process, the non-steady diffusion layer can be reduced in thickness in either process, with the result that a smooth plated metal layer can be constructed and further that since plating can be effected at a high pulse current density (high overvoltage}, the evolution of crystal seeds is promoted to yield finer crystal grains, thus enabling formation of a plated metal layer of high crystal Unity. As an example of the PR electroplating method, the process disclosed by Fujinami et al. (SurfaceTechnology, Formation of Via Filling by PR Electrolysis, 48[6], 1997, p.86-87).However, when the plated copper layer is formed by PC process, the uniformity of layer thickness is superior to that obtainable by direct current plating process but is not as good as the objective level (Fig. 4) .On the other hand, the plated copper layer formed by PR process is improved in the uniformity of thickness as compared with the layer obtainable by PC process but is not as high as desired yet and, moreover, plating by PR process requires an expensive current source.The current mainstream of electroless plating in the manufacture of printed circuit boards uses EDTA as a complexing agent, and examples of formation of copper circuits with such electroless plating solutions can be found in the Best Mode sections of Japanese Kokai Publication Sho-63-158156 and Japanese Kokai Publication Hei-2-188992 (corresponding to United States Patent 5055321 and United States Patent 5519177).However, with a plating solution containing EDTA as a complexing agent, a compressive stress (an expanding force) is generated in the plating metal layer to cause peeling of the plated copper film from the resin insulating layer.SUMMARY OF THE INVENTIONDeveloped in the above state of the art, the present invention has for its object to provide an electroplating process which, by utilizing a constant-voltage pulse process is capable of providing with low equipment cost, an electroplated metal of good crystallinity and uniform deposition on substrate.The invention is concerned with a process for manufacturing a printed circuit board which comprises disposing an interlayer resin insulating layer on a substrate formed with a conductor circuit, creating openings for formation of via holes in said interlayer resin insulating layer, formincj an electroless plated metal layer on said interlayer resin insulating layer, disposing a resist thereon, performing electroplating, stripping the resist off and etching the electroless plated metal layer to provide a conductor circuit and via holes, wherein the electroplating is performed intermittently using said electroless plated metal layer as cathode and a plating metal as anode at a constant voltage between said anode and said cathode .The invention is also concerned with a circuit board comprising a substrate and, as built thereon, a circuit comprised of a copper film which has properties that (a) its crystallinity is such that the X-ray diffraction half-width of the (331) plane of copper is less than 0.3 deg and (b) the variation in thickness {(maximum thickness-minimum thickness) / average thickness)) of the electroplated copper layer (electroplated metal layer) as measured over the whole surface of said substrate is not greater than 0.4.As a prior art technology for constructing a conductor circuit by a pulse electroplating method, there is known the PR electrolytic process mentioned hereinbefore but this prior art technology is a plating method using a constant current and not a constant-voltage pulse electroplating-process wherein the voltage is controlled.BRIEF DESCRIPTION OF THE DRAWINGSFig. 1 (a) to (g) are diagrams illustrating the conductor circuit-fabricating step in the processes for manufacture of printed circuit boards which belong to a first group of the present invention.Fig. 2 (a) to (e) are diagrams illustrating the printed circuit board-fabricating step in the processes for manufacture of printed circuit boards which belong to the first group of the present invention.Fig. 3 (a) to (b) are diagrams showing exemplary current and voltage waveforms for the constant-voltage pulse plating process.Fig. 4 is a diagram showing the results of evaluation of the deposition uniformity of the electroplated copper layers constructed by four kinds of electroplating techniques, namely the directcurrent plating technique, PC plating technique, PR plating technique and constant-voltage pulse plating technique.Fig. 5 is a diagram showing the result of X-ray diffraction analysis of the electroplated copper layer formed by the constantvoltage pulse plating technique .Fig. 6 is a schematic diagram illustrating the electroplated copper layer formed on an insulating board by the conventional direct-current electrolytic technique .Fig. 7 is a schematic diagram illustrating the disadvantage encountered in laminating the printed circuit board prepared by the technique according to Fig. 6.Fig. 8 (a) to (b) are diagrams showing exemplary current and voltage waveforms for the PC plating technique.Fig. 9 (a) to (b) are diagrams showing exemplary current and voltage waveforms for the PR plating technique.Fig. 10 (a) to (d) are views illustrating the production flow for the manufacture of a CMOS IC.DETAILED DESCRIPTION OF THE INVENTIONThe present invention is now described in detail. Unless otherwise indicated, the thickness of any copper foil, conductor layer or conductor circuit as mentioned in this specif ication is the mean of thicknesses measured on a light or electron microphotograph of its cross-section.As mentioned above, the invention is concerned with a process 5 for producing a printed circuit board which comprises constructing an interlayer resin insulating layer on a conductor circuit-forming substrate board, forming openings for via holes in said interlayer resin insulating layer, forming an electroless plated metal layer over said interlayer resin insulating layer, disposing a resist thereon, performing electroplating, stripping the resist off and etching the electroless plated metal layer to form a conductor circuit pattern and via holes, wherein said electroplating is performed intermittently using said electroless plated metal layer as cathode and a plating metal as anode at a constant voltage between said anode and said cathode.In the above process for producing a printed circuit board, a metal layer may have been formed on the surface of the interlayer resin insulating layer.The intermittent electroplating in the invention comprises application of a voltage between the cathode and anode and interruption thereof in an alternating pattern, and preferably the voltage time / interruption time ratio is 0.1 to 1.0, the voltage time is not longer than 5x10~3seconds and the interruption time is not shorter than lxlO3seconds.Furthermore, the invention is concerned with a circuit board having a copper film circuit on a substrate board, wherein said copper film has properties (a) its crystallinity is such that the half-width of X-ray diffraction of the (331) plane of copper is less than 0.3 deg. and (b) the variation in thickness of said copper film (electroplated copper layer) measured over the whole surface of said substrate, i.e. ((maximum thickness-minimum thickness) / average thickness), is not greater than 0.4.In the circuit board mentioned above, the percent elongation of said copper film as a characteristic parameter is preferably not less than 7%.The invention relates broadly to a technology for fabricating conductor circuits for semiconductor devices and printed circuit boards and an electroplating technology such that intermittent electroplating is performed in a plating metal ion-containing plating solution using the substrate surface as cathode and the plating metal as anode with the voltage between said anode and cathode being kept constant.The intermittent electroplating described above insures a uniform plating thickness. The reason seems to be that while the plating metal deposit is preferentially dissolved by the spike current flowing momentarily toward the anode in the marginal area of the substrate board surface and around the openings for via holes where the amount of deposition of the plating metal tends to be larger, the plating metal is precipitated by the spike current flowing momentarily toward the cathode in the central area of the substrate surface and the interior parts of the via holes where the amount of plating metal deposition tends to be smaller as in the remainder of the region, with the result that a highly uniform thickness of electrodeposition is insured.Furthermore, intermittent electroplating results in an increased crystallinity of the plated metal film. The reason is suspected to be that as the application of a voltage is interrupted, the metal ions in the neighborhood of the interface of the substrate diffuse to maintain a constant concentration at all times so that no defect occurs in the crystal lattice of the precipitated metal layer, thus contributing to a higher degree of crystallinity.By the constant-voltage pulse plating technique in the invention, which insures a uniform plate thickness, the thickness of the conductor circuits for circuit boards such as semiconductor devices and printed circuit boards can be rendered uniform. Therefore, not only is impedance alignment facilitated but, because the thickness of the interlayer resin insulating layer is uniform, an improved interlayer insulation is materialized. Furthermore, because of high crystallinity and high elongation characteristics, the residual stress in the plated metal layer is low so that even fine line-definition patterns can be protected against peeling. Therefore, the connection reliability of circuits is improved.The above intermittent electroplating process comprises application of a voltage between the cathode and anode and interruption thereof in an alternating pattern, and preferably the voltage time / interruption time ratio is 0.1 to 1.0, the voltage time is not longer than 5xl0”3seconds and the interruption time is not shorter than lxl0' seconds. If the voltage time exceeds 10 seconds, the film thickness will become uneven as it is the case with the conventional direct-current electroplating, and when the interruption time is less than lxlO12seconds, the diffusion of metal ions wiil be insufficient to detract from crystallinity. The optimum voltage time / interruption time ratio is 0.1 to 1.0.The electroplating mentioned above is preferably copper plating, nickel plating, cobalt plating, tin plating or gold plating.The copper plating solution is preferably an aqueous solution of sulfuric acid and copper sulfate. The nickel plating solution may for example be an aqueous solution of nickel sulfate, nickel chloride, and boric acid. The cobalt plating solution may be an aqueous solution of cobalt chloride, basic cobalt carbonate and phosphorus acid. The tin plating solution may be an aqueous solution of stannous chloride. For gold plating, an aqueous solution of gold chloride, potassium cyanide and gold metal can be used.Since the electroplating bath need not be supplemented with a brightener and other additives, the crystallinity of the plated metal deposit is remarkably high.As the plating metal which serves as the anode, the metal in the form of a ball or a rod, for instance, can be used.The technology of manufacturing circuit boards in accordance with the invention is now described.The substrate board which can be used includes metal, semiconductor, resin and ceramic substrates, among others.First, the surface of the substrate board is made electrically conductive so that it may be successfully electroplated. The technique for imparting electrical conductivity to a resin substrate or a ceramic substrate comprises forming metal layer by using an electroless plated deposit layer or a sputter-metalized layer. As an alternative, the technique of incorporating a colloidal or powdery metal in the matrix resin can be used.On the substrate rendered electrically conductive on the surface, a resist is disposed where necessary. The plating metal adheres to the conductive surface not covered with resist but exposed.This substrate is immersed in the electroplating solution and subjected to intermittent electroplating using the substrate as cathode and the plating metal as anode.The production process relevant to cases in which the circuit board is a printed circuit board is now described.The substrate which can be used includes insulating substrates such as a resin substrate and a ceramic substrate.The resin substrate mentioned above includes an insulating board prepared by laminating prepregs each comprising a fibrous matrix impregnated with a thermosetting resin, a thermoplastic resin or a thermosetting resin thermoplastic resin complex or a copperclad laminate board prepared by laying up such prepregs and copper foils and hot-pressing them.As the fibrous matrix mentioned above, glass cloth, aramid cloth, etc. can be used.An electroless plating catalyst such as a Pd catalyst is applied to the surface of said insulating substrate board to form an electroless plated layer. When a copper-clad laminate board is used, the copper foil as such can be utilized as cathode.A plating resist is then disposed thereon. The plating resist can be formed by a process which comprises pasting a photosensitive dry film followed by exposure and development or a process which comprises coating the substrate board with a liquid resist followed by exposure and development.The conductor circuit is formed by intermittent electroplating using the conductive layer not covered with resist but exposed, e.g. electroless plated metal layer as cathode and the plating metal as anode .Then, the plating resist is stripped off and the conductive layer, e.g. electroless plated metal layer, is etched off with an etching solution to complete the conductor circuit.As the etching solution mentioned above, an aqueous system of sulfuric acid-hydrogen peroxide, ferric chloride, cupric chloride or ammonium persulfate, for instance, can be used.The following procedure is followed for the production of a multilayer printed circuit board.A conductor circuit-forming substrate board is first provided with an interlayer resin insulating layer, which is then formed with openings for via holes. The openings are provided by exposure, development or irradiation with laser light.For the interlayer resin insulating layer mentioned above, a thermosetting resin, a thermoplastic resin, a partially photosensitized thermosetting resin, or a complex resin comprising thereof can be used.The above interlayer resin insulating layer can be formed by coating with an uncured resin or an uncured resin film by pressure bonding under heating. As an alternative, an uncured resin film carrying a metal layer, e.g. copper foil, on one side can be bonded. When such a resin film is used, the areas of the metal layer which correspond to via holes are etched off, followed by irradiation with a laser beam to provide necessary openings.The above resin film formed with a metal layer may for example be a copper foil having resin film.As the interlayer resin insulating layer mentioned above, the layer formed of an adhesive for electroless plating use can be used. The optimum adhesive for electroplating use is a dispersion of a cured acid- or oxidizing agent-soluble heat-resistant resin powder in a substantially acid- or oxidizing agent-insoluble uncured heatresistant resin. This is because upon treatment with an acid or an oxidizing agent, the heat-resistant resin particles are dissolved and removed so that a roughened surface comprising narrow-necked bottle-like anchors can be provided.Referring to said adhesive for electroless plating use, the cured heat-resistant resin powder mentioned above, in particular, is preferably <D a heat-resistant resin powder having an average particle diameter of not more than 10 pm, © a block powder available on aggregation of heat-resistant resin particles having an average particle diameter of not more than 2 pm, © a mixture of a heat-resistant resin powder having an average particle diameter of 2 to 10 pm and a heat-resistant resin powder having an average particle diameter of not more than 2 pm @ a pseudo-particle comprising a heat-resistant resin powder having an average particle diameter of 2 to 10 pm and at least one of a heat-resistant resin powder and an Inorganic powder each having an average particle diameter of not more than 2 pm as adhered to the surface of the first-mentioned resin powder, ® a mixture of a heat-resistant resin powder having an average particle diameter of 0.1 to 0.8 pm and a heat-resistant resin powder having an average particle diameter of over 0.8 pm to less than 2 pm or © a heat-resistant resin powder having an average particle diameter of 0.1 to 1.0 pm is preferred. With any of those materials, the more sophisticated anchors can be provided.The depth of the roughened surface structure is preferably Rmax = 0.01 to 20 pm. This is preferred for insuring a sufficient degree of adhesion. Particularly in the semi-additive process, the depth of 0.1 to 5 pm is preferred, for the electroless plated metal layer can then be removed without detracting from adhesion.The substantially acid- or oxidizing agent-insoluble heatresistant resin mentioned above is preferably a complex resin comprising a thermosetting resin and a thermoplastic resin” or a ’’complex resin comprising a photosensitive resin and a thermoplastic resin. This is because while the former is highly heat-resistant, the latter is capable of forming openings for via holes by a photolithographic technique .The thermosetting resin which can be used as above includes epoxy resin, phenolic resin and polyimide resin. For imparting photosensitivity, the thermosetting groups are acrylated with methacrylic acid or acrylic acid. The optimum resin is an acrylated epoxy resin.As the above-mentioned epoxy resin, there can be used novolac epoxy resins such as phenol novolac resin and cresol novolac resin and dicyclopentadiene-modified alicyclic epoxy resin.As the thermoplastic resin, there can be used polyethersulfone (PES), polysulfone (PSF), polyphenylenesulfone (PPS), polyphenylene sulfide (PPES), polyphenyl ether (PPE), polyetherimide (PI) and fluororesin.The blending ratio of the thermosetting resin (photosensitive resin) to the thermoplastic resin, i.e. thermosetting (photosensitive) resin / thermoplastic resin, is preferably 95 / 5 to 50 / 50. This range contributes to a high level of toughness without compromise in heat resistance.The blending weight ratio of said heat-resistant resin powder is preferably 5 to 50 weight % based on the solid matter of the heat-resistant resin matrix. The more preferable ratio is 10 to 40 weight %.The heat-resistant resin powder is preferably an amino resin (melamine resin, urea resin, guanamine resin) or an epoxy resin, for instance .Further, an electroless plated metal layer is formed over said interlayer resin insulating layer (on the copper foil when a resincontaining copper foil is used) inclusive of surface of openings and after placement of a resist, electroplating is performed to provide a conductor circuit and via holes.The electroplating is performed intermittently using said electroless plated metal layer as cathode and the plating metal as anode with the voltage between the anode and cathode being kept constant.Then, the resist is stripped off and the electroless plated metal layer is etched off.The circuit board and printed circuit board formed by the electroplating process according to the present invention, in which the conductor wiring or conductor circuit is made of copper, should satisfy the following conditions (a) and (b) .Thus, (a) as to crystallinity, the half-width of X-diffraction of the (331) plane of copper is not greater than 0.3 deg, and (b) the variation in plating thickness of the copper layer (electrolated copper layer) as measured all over the surface of said substrate board ((maximum thickness-minimum thickness) / average thickness) is not greater than 0.4.When the half-width of X-ray diffraction of the (331) plane of copper is 0.3 deg or Larger, the residual stress will be increased and, in the case of a delicate pattern, there will be a risk for peeling. If the variation ((maximum thickness-minimum thickness) / average thickness) is greater than 0.4, impedance alignment may hardly be obtained.The reason for selection of the (331) plane of copper is that this is the plane revealing the most striking change in crystallinity in X-ray diffraction analysis.The percent elongation mentioned above for the copper layer is preferably not less than 7%. If the elongation is less than 7%, cracks are liable to develop on cold thermal shock.In the inventions of the first group, the purity of copper deposited is as high as 99.8¾ or more. Therefore, the inherent ductility of copper is fully expressed to provide a high elongation rate.The circuit board mentioned above includes printed circuit boards, 1C chips and semiconductor devices such as LSI.BEST MODE FOR CARRYING OUT THE INVENTIONThe following examples are intended to illustrate the present invention in further detail and should by no means be construed as defining the scope of the invention.Example 1Fig. 1 (a) to (g) show an exemplary process for fabricating the conductor circuit of the printed circuit board according to the invention and Fig. 2 (a) to (e) show an exemplary process for manufacturing a multilayer printed circuit board in accordance with the invention.In constructing the conductor circuit on a printed circuit board, an insulating substrate 1001 of glass cloth-epoxy resin or BT material was used as the insulating sheet as shown in Fig. 1 (a) .Then, 35 weight parts of acrylate (25 wt. %} of cresol novolac epoxy resin (Nippon Kayaku; mol. wt. 2500), 3.15 weight parts of photosensitive monomer (Toa Gosei Co.; trade mark, Aronix M315), 0.5 weight part of antifoam (Sun Nopco, S-65), 3.6 weight parts of Nmethylpyrrolidone (NMP), 12 weight parts of polyethersulfone (PES), and epoxy resin powders (Sanyo Kasei; Polymerpol; 1.0 pm of average particle diameter, 7.2 wt. parts, and 0.5 pm of average particle diameter, 3.09 wt. parts) were mixed together, and after supply of additional 30 weight parts of NMP, the mixture was milled in a bead mill. Then, 2 weight parts of imidazole series curing agent (Shikoku Kasei; product designation 2E4MZ-CN) , 2 weight parts of photopolymeri zation initiator(Ciba-Geigy; Irgacure 1-907), 0.2 weight part of photosensitizer (Nippon Kayaku; DETX-S) and 1.5 weight parts, of NMP were added and the whole mixture was stirred to give an electroless plating adhesive composition.Using a roll coater, this electroless plating adhesive 1013 was coated on the substrate and after 20 minutes of sitting horizontally, dried at 60°C for 30 minutes to provide an electroless plating adhesive layer 1013 in a thickness of 35 pm.Both sides of the wiring substrate thus prepared were irradiated for exposure at 500 mJ / cm2with a ultra-high-pressure mercury arc lamp and heated at 150°C for 5 hours.The substrate was then immersed in chromic acid for 19 minutes to dissolve out epoxy resin particles from the surface of the adhesive layer. By this procedure, the electroless plating adhesive layer 1013 was provided with a roughened surface (Fig. 1 (b)).Under the following conditions, a thin electroless plated copper layer 1002 was constructed in a thickness of about 1 pm (Fig. 1 (c) ) . A photosensitive dry film was then superimposed on the copper layer and a resist 1003 was formed by light exposure and development (Fig. 1 (d) ) .Electroless copper plating solution:EDTA 150g / L Copper sulfate 20 g / L HCHO 30 mL / L NaOH 40 g / L a,a’-Bipyridyl 80 mg / L PEG 0.1 g / LElectroless plating conditions:Solution temperature: at 70°C, for 30 min.After a thick copper electrodeposit layer 1004 was thus formed (Fig. 1 (e)), the resist 1003 was removed by stripping with aqueous sodium hydroxide solution (Fig. 1 (f) ) . Then, using an aqueous sulfuric acid-hydrogen peroxide solution, the thin electroless plated copper layer 1002 was etched off (Fig. 1 (g) ) to provide a conductor circuit 1005.The process shown in Fig. 2 (a) to (e) is a process for establishing an electrical connection between two or more conductor layers 1006a, 1006b (2 layers in the drawing) which partly comprises piercing openings in the conductor layer 1006a by etching, forming openings for via holes 1007 within said opening between 1006a and 1006b by laser or other means (Fig. 2 (c)), forming a thin electroless plated metal layer 1008 within said openings 1007 (Fig. 2 (d) ) and forming a thick electroplated metal layer 1009 {Fig. 2 (e)) to provide via holes 1010.First, a resin-copper foil laminate 1012 comprising copper foil 100 6a, i.e. as a metal layer, and insulating resin 1011 was hot-pressed against the substrate sheet on which the conductor circuit 1006b had been formed (Fig. 2 (a)}.Then, openings for via holes were formed by etching with an aqueous sulfuric acid-hydrogen peroxide solution and the insulating resin 1011 was removed by means of a carbon dioxide gas laser, for instance (Fig. 2 (c) ) .Then, electroless copperplating was carried out under the above-mentioned conditions to deposit an electroless plated copper layer 1008 within said openings for a via holes.Thereafter, a plating resist 1003 was disposed and electroplating was carried out to form via holes 1010 and an electroplated metal layer 1009.The outstanding feature of the process for manufacturing a printed circuit board according to the first group of the present invention is that the electroplated metal layer is formed by a constant-voltage pulse plating technique.Fig. 3 (a) and (b) show the typical voltage and current waveforms used in the constant-voltage pulse plating processes according to the invention. For reference's sake, the voltage and current waveforms of PC plating are shown in Fig. 8 (a) and (b) and the voltage and current waveforms of PR plating are shown in Fig. 9 (a) and (b).Those waveforms were observed with the SS-570S synchroscope manufactured by IWATSU. Sony Techtonix A6303 current probe was used as current probe, Sony Techtonix A503B as current probe amplifier, and Sony Techtonix TM502AWO as power supply.Comparison of the voltage and current waveforms shown in Fig. 3 (a), (b) , Fig. 8 (a), (b) , and Fig. 9 (a), (b) reveals that whereas, despite a difference in the occurrence of dissolution of the anode due to reverse electrolysis, both the PR plating technique and the PC plating technique show generally square current waveforms, the novel constant-voltage pulse plating technique according to the first invention of the first group showed a current waveform such that a spike current flows momentarily toward the cathode on voltage application while a spike current flows momentarily toward the anode on voltage interruption.A direct current source (Sansha Denki; DC AUTO Series) was used as power supply and the voltage application and interruption were controlled by ON-OFF of a relay using a digital timer.Electroplated copper layers were built on 255 mm x 340 mm substrate sheets by depositing substantially uniform amounts of copper by 4 different electroplating techniques, namely directcurrent plating, PC plating, PR plating and constant-voltage pulse plating techniques, using a copper sulfate plating solution containing 180 g / L of sulfuric acid and 80 g / L of copper sulfate under the conditions respectively indicated below in Table 1 to prepare printed circuit boards. The thickness of the electroplated copper layer of each board was measured in the central· and marginal areas of substrate and the variation in thickness of the electroplated copper layer in the central and marginal· areas of each board, i.e. [(maximum thickness-minimum thickness) / average thickness], was calculated to evaluate the electrodeposition uniformity .The results of this evaluation are presented in Fig. 4. The smaller the value is, the higher is the uniformity of electrodeposition.Table 1Plating time Pulse condition Current density (A / dm2) Plating time (sec . ) ON OFF (reverse) DC plating -1.8A - -1.2 52 PC plating -6. OA (1 msec.) OA (4msec.) 6.0{ON) 52 PR plating -1.2A {50msec.) +3.6A [2msec.) 1.2(ON) 57 Constant-voltage pulse plating -0.5V (1msec.) OV (4msec.) 52 Power supply: DC plating: Sansha DC AUTO 1520 PC plating: Kikusui Denshi Kogyo, Bipolar PBX20-20 PR plating: Kikusui Denshi Kogyo, Bipolar PBX2 0-2 0 Cons tant-voltage pulse plating: Sansha DC AUTO 1520 as DC source, OMRON solid-state relay (G3WA-O210R) was connected to the output terminal and switched ON and OFF with OMRON digital timer (H5CL).5 It, can be seen from the data in Fig. 4 that, of the above- mentioned four different electroplating techniques, the constant- voltage pulse plating technique provides the highestelectrodeposition uniformity.Then, the electroplated copper layer formed on a stainless 10 steel sheet by the constant-voltage pulse technique was not annealed but directly subjected to X-ray diffraction analysis to determine its diffraction pattern. The data are plotted in Fig. 5. The halfwidth value was 0.25 deg.As controls, the electroplated copper layers formed by the DC,PC and PR plating techniques, respectively, were also subjected toX-ray diffraction analysis in the same manner as above. The diffraction patterns obtained are shown in Table 2. The respective half-width values were 0.45 deg., 0.40 deg. and 0.30 deg.Table 2Plating process Half-width DC plating 0.45 PC plating 0.40 PR plating 0.30 Constant-voltage 0.25Comparison of the data given in Table 2 reveals that, of the above-mentioned four different electroplating techniques, the constant-voltage pulse plating technique provides the narrowest haIf-width and, hence, highest crystallinity.It is, therefore, clear that a conductor circuit comprising an electroplated metal layer of remarkably high crystallinity and electrodeposition uniformity can be provided by adopting the constant-voltage pulse plating technique in the construction of the electroplated metal layer as an essential requisite in the process of the first group of invention.The plating substrate surface area, the composition of the constant-voltage pulse plating solution and the plating conditions are not particularly restricted but the following can be mentioned as preferred typical ranges.• Plating surface size: 255-510 mm L x 255-510 mm W • Plating bath compositionCu sulfate: 50 to 80 g / L, sulfuric acid: 180 to 240 g / L, chloride ion: 40 to 50 ppm, pH<l, bath temperature: room temp.; anode-tocathode distance: 10 to 20 cm • plating conditionsAnode: oxygen-free copper, application voltage: 0.01 to 10 V, voltage application time : 0.5xlO3-5xlO3sec ., interruption time :1x103~ 8x103sec., voltage time / interruption time ratio = 0.1 to1.0.Furthermore, since the electroplated metal layer according to the process of this invention is of high crystallinity and features a low internal residual stress, it can be used as it is to insure highly dependable circuits and connections and the annealing for decreasing stress may be omitted.Example 2The following is an example of application of this invention to the manufacture of a CMOS IC chip.An IC wafer was fabricated by the well-known MOS wafer production technology, for example by the process described in LSI Process Engineering, pp. 22 to 23 [Published by Ohm-sha, K.K., June 20, 1987] [Fig. 10 (a)].The whole surface of a substrate was subj ected to Cu sputtering to provide a Cu layer 1014 in a thickness of 0.6 pm (Fig. 10 (b)). Cu sputtering can be carried out using a vacuum sputtering equipment (Tokuda Seisakusho; CFS-8EP).Then, using a spin coater, a negative photoresist (Tokyo Auka Kogyo; OMR83) was coated on the Cu layer 1014, followed by drying. Thereafter, prebaking, exposure, development and postbaking were performed in succession to provide a plating resist 1015 (4 pm thick, L / S=2 0 / 2 0 pm) . Then, the sheet was immersed in 10% aqueous solution of sulfuric acid for surface activation and constantvoltage pulse copper electroplating was performed under the conditions described above (Fig. 10 (c)).The plating resist 1015 was removed with aqueous sodium hydroxide solution and the exposed copper film 1016 was dissolved and removed with aqueous sulfuric acid-hydrogen peroxide solution to provide a CMOS IC (Fig. 10(d)).INDUSTRIAL APPLICABILITYThus, in accordance with the constant-voltage pulse plating process used in the invention, conductor circuit and via holes of good crystallinity and uniform deposition can be constructed on a substrate and high-density wiring and highly reliable conductor connections can be realized without annealing.Moreover, the constant-voltage pulse plating process used in the first group of inventions can be easily carried out using an inexpensive power supply, e.g. a direct current source, by repeating application and interruption of a voltage alternately through manipulation of an ON-OFF switch. Thus, unlike the PR plating process requiring an expensive power source, this process makes it possible to construct an electroplated metal layer of excellent crystallinity and uniform deposition on the substrate surface as well as in the openings for via holes, thus being of great industrial advantage.
Claims
CLAIMS 1. A process for manufacturing a printed circuit board which comprises disposing an interlayer resin insulating layer (1011) on a substrate formed with a conductor circuit (1006b), creating openings (1007) for formation of via holes in said interlayer resin insulating layer (1011), forming an electroless plated metal layer (1008) on said interlayer resin insulating layer (1011), disposing a plating resist (1003) thereon, performing electroplating on said electroless plated metal layer (1008) not covered with said plating resist (1003), stripping the plating resist (1003) off and etching the electroless plated metal layer (1008) to provide a conductor circuit (1006b, 1009) and via holes (1010), characterised in that the electroplating is performed by using said electroless plated metal layer (1008) as cathode and a plating metal as anode at a constant voltage between said anode and said cathode, repeating application of a voltage and interruption of application alternately, with a voltage application time / interruption time ratio of 0.1 to 1.0, a voltage application time of 0.5 x 10‘3 to 5 χ 10”3 seconds and an interruption time of 1 x 10“3 to 8 x 10“3 seconds.
2. The process for manufacturing a printed circuit board according to claim 1, wherein said interlayer resin insulating layer (1011) has a metal layer (1006a) on its surface.
3. The process for manufacturing a printed circuit board according to claim 1, wherein the plating solution used for said electroplating does not contain a brightener.
4. A circuit board comprising a substrate and, as built thereon, a circuit comprised of an electroplated copper film, which is formed by an electroplating performed by repeating application of a voltage and interruption of application alternately, characterised wherein the voltage between the anode and the cathode being constant, with a voltage application time / interruption time ratio of 0.1 to 1.0, a voltage application time of 0.5 χ 10'3 to 5 χ 103 seconds and an interruption time of 1 x 10~3 to 8 χ 103 seconds, and wherein said copper film has properties that (a) its crystallinity is such that the X-ray diffraction half-width of the (331) plane of copper is less than 0.3 deg and (b) the variation in thickness {(maximum thickness-minimum thickness) / average thickness) of said copper film as measured over the whole surface of said substrate is not greater than 0.4.
5. The circuit board according to claim 4, wherein said copper film has an elongation of not less than 7%.
6. The circuit board according to claim 4 or 5, wherein said circuit board is a printed circuit board and said copper film is a plated copper film.
7. The circuit board according to claim 4 or 5, wherein said circuit board is a printed circuit board having said substrate formed with a conductor circuit (1006b), an interlayer resin insulating layer (1011) built thereon and a conductor circuit (1009) comprised of said copper film as built on said interlayer resin insulating layer (1011), said interlayer resin insulating layer (1011) having via holes (1010) by which said conductor circuits (1006b, 1009) are interconnected.
8. The circuit board according to claim 4, wherein the plating solution used for said electroplating does not contain a brightener.