Pulverulent rubber powders comprising modified fillers, processes for their preparation and their use
Patent Information
- Application Number
- MYPI1999004090
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 1998-09-22
- Filing Date
- 1999-09-21
- Publication Date
- 2000-03-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Current rubber processing techniques require high energy expenditure and damage filler structures due to grinding operations, and prior methods result in filler particles sticking together during storage, making handling difficult.
A process involving the precipitation of rubber powders from aqueous mixtures containing water-soluble metal salts and organosilicon compounds, which are mixed with oxidic or silicatic fillers, allowing for the integration of fillers into the rubber surface without external absorption, enhancing flowability and preventing agglutination.
The process reduces energy consumption, preserves filler structure, and prevents particle sticking, resulting in high flowability and easy handling of rubber powders without loss of properties under mechanical stress.
Abstract
Description
Pulverulent rubber powders comprising modified fillers,processes for their preparation and their use.The invention relates to a process for the preparation otrubber powders comprising fillers modified withorganosilicon compounds, and che powders thus prepared.A. large number of: publications have appeared relating tothe aim and purpose of the use of powdered rubbers andpossible processes for their preparation.The explanation of the interest in pulverulent rubbers canreadily be found from the processing techniques of therubber industry. There, rubber mixtures are prepared with ahigh expenditure on time, energy and personnel. The mainreason for this is that the raw material rubber is presentin the form of balls, and the other constituents of thevulcanizable mixture must be incorporated.Comminution of the balls and intimate mixing with fillers,mineral oil plasticizers and vulcanization auxiliariestakes place on mills in internal mixers in several processstages. Between the stages, the mixture is in generalcooled on a batch-off line, deposited on pallets as rolledsheet and intermediately stored. The internal mixers ormills are followed by appropriate extruders or calenderingprocesses.Only a completely new processing technology can lead awayfrom this very involved technique of rubber processing.The use of free-f1 owing rubber powders has therefore beendiscussed for a relatively long time, because this resultsin Che possibility of being able to process rubber mixtureseasily and quickly in the same way as thermoplasticpowders.DE-PS 2822 148 discloses a process for the preparation of apulverulent, filler-containing rubber.According to this patent specification, an aqueous filleremulsion is added to a rubber latex (e. g. natural rubber)a rubber solution (e. g. BR) or an aqueous emulsion of asynthetic rubber (e. g. SBR) and the desired rubber powderis precipitated out.To avoid the particle size-dependent filler contentsobtained by this process, patents have been applied forrelating to variants, which belong to the prior art asDE-PS 3723 213 and DE-PS 3723 214.According to DE-PS 3723213, in a process which proceeds intwo stages, an amount of >50 % of the filler is firstintegrated into the rubber powder particles. In the secondstep, the remainder of the filler is absorbed on to the so-called rubber base particles.This can be regarded as a variant of powdering, since nobond is formed between the filler and rubber.As E.T. Italiaander (Paper 151. Technische Tagung derRubber Div. der ACS [Technical Conference of the RubberDiv. of the ACS], Anaheim, California, 6th - 9th May 1997(GAK 6 / 1997 (50) 456-464) found, however, regardless of thegreat future predicted in the Delphi Report (Delphi Report"Kunftige Herstellverfahren in der Gummiir.dustrie [FutureProduct ion Processes in the Rubber Industry] " RubberJournal, vol. 154, no. 11, 20-34 (1972)) for pulverulentand granulated rubber, and numerous attempts undertaken bywell-known polymer producers from the middle of theseventies into the early eighties to prepare pulverulentNBR, SBR-carbon black masterbatches and granulated NR, thestandard delivery form of polymers has remained rubberballs.A disadvantage of the known processes on the one hand liesin the fact that a grinding operation is required in orderto establish the particle diameter of the filler particlesof 10 nm regarded as necessary for the quality of the endproduct.However, this not only results in a high expenditure onenergy, but also causes damage to the filler structure,which, in addition to the active surface area, is animportant characteristic parameter for the effectiveness inuse in rubbers.On the other hand, the ease of handling of the productsaccording to the prior art. suffers due to the particlessticking to one another during storageA precipitation process has now been applied for undernumber P 198 16 972.8, in which suspensions of fillersmodified with organosilicon compounds are prepared andthese are stirred into the rubber emulsion.The rubber powder is then precipitated out of this mixture.The object of the invention is to provide a process whichleads with few process stages to a rubber powder which canadvantageously be employed and comprises modified fillers.The invention provides a process for the preparation offinely divided rubbers (rubber powders) by precipitationfrom aqueous mixtures which comprise filler in the form ofsuspensions, water-soluble salts of a metal of groups Ha,lib, Ilia and VIII of the periodic table of the elementsand a rubber latex, an aqueous emulsion of a rubber or arubber solution, which is characterized in thata) one or more organosilicon compound(s) containing atleast one alkoxy group is or are dissolved oremulsified, optionally in the presence of a surface-active substance, in water, or the compounds mentionedare mixed directly, optionally with a surface-activesubstance, with an aqueous suspension of an oxidic orsilicatic finely divided filler or a mixture of thesefillers at a temperature of 10 to 60 ° C, preferably atroom temperature, while stirring, the amount of thismixture envisaged for incoporation in the rubber, basedon the filler content, in general being divided into twobatches, andb) a first batch is mixed with the polymer latex, thepolymer emulsion or the polymer solution, the pH of thismixture is lowered to a pH of 6.0 to 4.5 with an acid,in particular a Lewis acid (first batch, first stage),c) the remaining content (second batch, splitting amount)is added with further lowering of the pH to 4.5 to 2.6,in particular approx. 3.2 (second stage), so that therubber in the mixture precipitates out together with thefiller modified by organosilicon compound(s)d) the solid which has precipitated out is separated off by-measures known per se,e) it is preferably washed, in order to adjust the pH to avalue of approx. 6 to 7 which is more compatible withthe further processing, andf) the filler-containing rubber is dried.Drying is advantageously carried out in a drier at a gasintake temperature of 140 to 160 °C and a gas dischargetemperature of 50 to 70°C. The temperature of the productshould not exceed 40 to 50 °C.The duration, which depends on the pH and the fillercontent, and the extent of the precipitating operation caneasily be determined within a measurement series.In the case of a powdered rubber with a high filler content(>80 parts of filler phr), 1 to 10 parts of this amountwill in general be employed as the remaining content in thesecond stage in the precipitation of the powdered rubber.If the powdered rubber comprises less than 80 parts offiller phr, e. g. only 5 0 parts phr in total, >10 to 20parts of this amount is further introduced into the mixturein the form of a suspension before the conclusion of theprecipi tat ing operation.The fillers are bonded into the outer particle region(margin region) of the rubber powders in this manner.These contents of the filler are therefore not absorbedexternally on to the individual rubber particles (see DE-PS37 23213), but are integrated into the rubber surface.This distribution of the filler and the nature of thebonding of the fillers in the rubber composition cause thehigh flowability of the powders according to the inventionand prevent agglutination during storage of the powders,without these properties being lost due to mechanicalstresses during conveying, silation etc.Further fillers which are optionally employed are thecarbon blacks known from the rubber industry, preferably infinely divided form (fluffy), which in general have anaverage particle diameter of 1 to 9 Jim, preferably 1 to8 nm, without mechanical treatment, before they aresuspended.This facilitates dispersion, so that aqueous suspensionswith filler particles having an average particle diameterof significantly less than 10 jim are obtained without ahigh expenditure of energy.Precipitated silica can advantageously be employed in theform of a filter-cake which has been washed free fromsalts.Possible metal salts are those which originate fromelements of groups Ila, lib, Ilia and VIII of the periodictable of the elements. This classification into groupscorresponds to the old IUPAC recommendation (seePeriodisches System der Elemente [Periodic Table of theElements] , Verlag Chemie, Weinheim, 1985) . Typicalrepresentatives are magnesium chloride, zinc sulfate,aluminium chloride, aluminium sulfate, iron chloride, ironsulfate, cobalt nitrate and nickel sulfate, the salts ofaluminium being preferred. Aluminium sulfate and otherLewis acids are particularly preferred.The salts are employed in an amount of 0.1 to 6.5 parts byweight per 100 parts by weight of rubber. The metal saltsprove to be particularly suitable for influencing theparticle size of the precipitated products in the desiredmanner. Mineral acids, such as e. g. sulfuric acid,phosphoric acid and hydrochloric acid, are optionallyadditionally used to establish the desired pH, sulfuricacid being particularly preferred. However, it is alsopossible to employ carboxylic acids, such as e. g. formicand acetic acid.The amount of acid depends on the nature and amount of thewater-soluble metal salt, of the filler, of theorganosilane employed, of the rubber and of the alkalimetal silicate optionally present. It can easily bedetermined by a few orientating experiments.In a preferred embodiment of the process according to theinvention, up to 5 parts by weight, per 100 parts by weightof rubber, of silica (Si02) in the form of an alkali metalsilicate solution, preferably as water-glass with an Na20:Si02 molar ratio of 2 : 1 to 1 : 4, are also additionallyemployed. The alkali metal silicate solution can be addedhere both to the rubber component and to the fillersuspension. Addition to the rubber component is preferred,especially in the continuous procedure.The process according to the invention is in generalcarried out as follows:A filler suspension is first prepared by dispersing aportion, preferably >50 %, of the filler contained in theend product, together with the metal salt, the organosilanecompound and optionally the alkali metal silicate solution,in water, optionally in the presence of an emulsifier. Thetotal amount of water employed depends on the nature of thefiller and the degree of breakdown. In general, the water-insoluble constituents of the suspension are about 4 to 15per cent by weight. This value is not a binding limitation,and the actual value can also be either below or abovethis. The maximum content is limited by the ability of thesuspension to be pumped.The filler suspension thus prepared in then mixedintimately with the rubber latex, which optionally containsalkali metal silicate solution, or the aqueous emulsion,which optionally contains alkali metal silicate solution,of a rubber solution (first batch, first stage). Knownstirrer units, such as e. g. propeller stirrers, aresuitable for this.After the mixing, a pH in the range from 6.0 to 4.5 isfirst established with further stirring, preferably of aLewis acid, in particular Al2(S04)3 with the aid of an acid[sic]. Rubber base particles with a constant filler andorganosilane content are obtained here. The size of thesebase particles is controlled by the amount of metal saltchosen, in the range from 0.1 to 6.5 phr. The control takesplace such that the largest particle size is obtained withthe lowest amount of metal salt.The remaining content of the filler suspension (secondbatch, splitting amount) is added with further lowering ofthe pH to 4.5 to 2.6, in particular approx. 3.2 (secondstage), so that the rubber in the mixture precipitates outtogether with the filler modified by organosiliconcompound{s).The solids content of the latices employed is in general 20to 25 wt.%. The solids content of the rubber solutions isin general 3 to 3 5 wt.%, and that of the rubber emulsionsis in general 5 to 30 wt.%.For working up of rubber powders with filler contents of>100 phr it is advantageous to lower the pH to 2.5 beforethe phase separation. An acid from the abovementioned groupof acids is expediently used for this.The process according to the invention can be carried outboth discontinuously and continuously.The rubber powder which has precipitated out isadvantageously separated off with the aid of a centrifugeand then dried to a residual water content of in general<1 %, in particular in a fluidized bed drier.The rubber powders according to the invention are preparedusing one or more organosilicon compounds of the generalformula[RLn. (RO)3.n Si - (Alk) m - (Ar) p] g [b] (I) ,RXn (RO) 3_n Si - (Alk) (II) ,orr1h (RO) 3 _ n Si - (alkenyl) (III)in which the symbols denoteB: -SCN, -SH, -Cl, ~NH2 (if q = 1) or -Sx- (if q =2)R and R1: an alkyl group having 1 to 4 carbon atoms,branched or unbranched, the phenyl radical,where all the radical [sic] R and R1 in eachcase can have the same or a different meaning,preferably an alkyl group,R: a Ci-C^-alkyl, -C1-C4-alkoxy group, branched orunbranched,n: 0; 1 or 2,Alk: a divalent straight-chain or branched carbon[sic] radical having 1 to 6 carbon atoms,m: 0 or 1Ar: an arylene radical having 6 to 12 C atomsp: 0 or 1, with the proviso that p and n do notsimultaneously denote 0x: a number from 2 to 8,alkyl: a divalent straight-chain or branchedunsaturated hydrocarbon radical having 1 to 20carbon atoms, preferably 2 to 8 carbon atoms,alkenyl: a divalent straight-chain or branchedunsaturated hydrocarbon radical having 2 to 20carbon atoms, preferably 2 to 8 carbon atoms.These compounds, if they are water-soluble, are in generalemployed in the form of solutions, or otherwise in the formof emulsions, it also being possible for the emulsions tobe formed in the presence of the silica suspension.The emulsion or solution is preferably prepared at roomtemperature. However, temperatures of 10 to 60 ° C are alsosuitable.The concentration of the oreanosilicon compound(s) in thesuspension is 0.5 to 20 wt. ? , preferably 5 to 12 wt.%,based on the total amount oi filler employed.The pH of the emulsion or solution, like the pH of thefiller suspension, after adnixing of the emulsion is in theweakly acid or weakly alkal:.ne range, but preferably at apH of about 7.The term water-insoluble uS'jd is to be understood asfollows:After mixing of the organosilane compound (without surface -active substance) with the suspension of the filler, noclear solution is formed around the filler particles in thedesired pH and concentration range. Rather, the separatephases comprising water, sclid and organosilicon compoundsremain. The oligosulfidic crganosilanes according to thegeneral formula I given abeve are known per se and can beprepared by known processes. Examples of organosilaneswhich are preferably employ ed are the bis(trialkoxysilyl-alkyl) oligosulfides which can be prepared e.g. inaccordance with BE-PS 787 691, such as bis-(trimethoxy-,triethoxy-, -trimethoxy- ethoxy-, -tripropoxy-,-tnbutoxy-, -tri-i-propoxy- and -tri-i-butoxy-silyl-methyl) oligosulfides, and in particular the di-, tri-,tetra-, penta-, hexasulfides etc., furthermore bis-(2-tri-methoxy-, -triathoxy-, -trimethoxyethoxy-, -tripropoxy- and-tri-n-and -i-butoxy-ethyl) oligosulfides and in particularthe di-, tri-, tetra-, penta-, hexasulfides etc., andfurthermore the bis-(3-trimethoxy-, -triethoxy-, -trimethoxyethoxy-, -tripropoxy-, -tri-n-butoxy- and tri-i-butoxysilyl-propyl) oligosulfides and in particular in turnthe di-, tri-, tetrasulfides etc. up to octasulfides, andmoreover the corresponding bis-(3-trialkoxysilylisobutyl)oligosulfides, the corresponding bis-(4-trialkoxysilylbutyl) oligosulfides. Of these selectedorganosilanes of the general formula I which are built uprelatively simply, the bis-(3-trimethoxy-, -triethoxy- andtripropoxysilylpropyl) oligosulfides are in turn preferred,and in particular the di-, tri-, tetra- and pentasulfides,especially the triethoxy compounds with 2, 3 or 4 sulfuratoms, and mixtures thereof. Alk in the general formula Idenotes a divalent, straight-chain or branched hydrocarbonradical, preferably a saturated alkylene radical with astraight carbon chain having 1 to 4 carbon atoms.Compounds which are also specifically suitable are thesilanes with the following structural formulaand methoxy analogues thereof, which can be prepared inaccordance with DE-AS 25 58191. These compounds are notsoluble in water.Surface-active substances which are used in this case are,preferably, nonionic, cationic and anionic surfactants.Their concentration in the emulsion is 1 to 15 wt.%,preferably 2 to 10 wt.%, based on the amount oforganosilane compounds.Examples of such surfactants are alkylphenol polyglycolethers, alkyl polyglycol ethers,polyglycols,alkyltrimethylammonium salts, dialkyldimtheylamrnonium [sic]salts, alkylbenzyltrimethylammomium salts,alkylbenzenesulfonates, alkyl hydrogen sulfates, alkylsulfates.The naturally occurring or precipitated fillers to bemodified, also as a mixture of two or more of thesefillers, are fillers which are known per se in rubbertechnology. An essential prerequisite for their suitabilityis the presence on the surface of the filler particles ofOH groups which can react with the alkoxy groups of theorganosilicon compounds. These are oxidic and silicaticfillers which are compatible with rubbers and which havethe fine division necessary and known for this use.Kaolins or clays are particularly suitable as naturallyoccurring silicates. However, kieselguhr or diatomaceousearth can also be employedExamples of oxidic fillers which may be mentioned arealuminium oxide, aluminium hydroxide or trihydrate andtitanium dioxide."Modified fillers" in this connection means that theorganosilane compounds are bonded to the surface either bychemical reaction (OH groups) or adsorptively.The adsorptively bonded groups are converted intochemically bonded groups by the drying step.The emulsion is mixed with the filler suspension in amountssuch that the concentration of the organosilicon compoundis 0.5 to 20 wt.%, preferably 5 to 12 wt.%, based on theamount of filler.The modified fillers comprise 0.5 to20 wt.%, preferably 0.5 to 12 wt.% of the organosiliconcompounds, based on the dry filler.They are particularly suitable for use in rubber mixtureswhich can be vulcanized and shaped.A filter-cake from the silica precipitation which has beenwashed free from salts is advantageously employed for theprocess according to the invention.Suspensions such as are obtained by working up naturallyoccurring fi1lers, such as clays, are also suitable.An energy-intensive drying step is thus saved, comparedwith the prior art.The silicas employed are known from the rubber sector.In general, they have an N2 surface area, determined by theknown BET method, of 35 to 700 m2 / g, a CTAB surface area of30 to 500 m2 / g, and a DBP number of 150 to 400 ml / lOOg.The product according to the invention comprises thesesilicas in an amount of 5 to 250 parts, in particular 20 to100 parts, based on 100 parts of rubber.If the fillers are white naturally occurring fillers, suchas clays or siliceous chalks with an N2 surface area of 2to 35 m2 / g, these are employed in an amount of 5 to 350parts, based on 100 parts of rubber.Filler-containing rubber powders which comprise silicas andcarbon black as a mixture can also be prepared.However, the total amount of filler does not exceed250 phr.Carbon blacks such as are generally employed in rubberprocessing are particularly suitable.These include furnace blacks, gas and flame blacks with aniodine adsorption number of 5 to 1000 m2 / g, a CTAB numberof 15 to 600 m2 / g, a DBP adsorption of 30 to 400 ml / 100 gand a 24 M4 DBP number of 50 to 370 ml / 100 g, in an amountof 5 to 100 parts, in particular 20 to 100 parts per 100parts of rubber.It has been found possible to employ as rubber types andprepare as aqueous emulsions the following species,individually or as a mixture with one another:Natural rubber, emulsion SBR with a styrene content of 10to 50 %, butyl-acrylonitrile rubber.Butyl rubbers, terpolymers of ethylene, propylene (EPM) andnon-conjugated dienes (EPDM), butadiene rubbers, SBR,prepared by the solution polymerization process, withstyrene contents of 10 to 25 %, and contents of 1,2-vinylconstituents of 20 to 55 % and isoprene rubbers, inparticular 3,4-polyisoprene.In the case of polymers prepared by solvent processes,particular safety measures should be taken because of thesolvent content.In addition to the rubbers mentioned, the followingelastomers are possible, individually or as a mixture:carboxyl rubbers, epoxide rubbers, trans-polypentenamer,halogenated butyl rubbers, rubbers of 2-chloro-butadiene,ethylene / vinyl acetate copolymers, epichlorohydrins,optionally also chemically modified natural rubber, such ase. g. epoxidized types.In addition to the fillers already mentioned, the rubberpowders according to the invention optionally compriseknown processing or vulcanization auxiliary substances,such as zinc oxide, zinc stearate, stearic acid,polyalcohols, polyamines, plasticizers, antioxidantsagainst heat, light or oxygen and ozone, reinforcingresins, flameproofing agents, such as e. g. Al(OH)3 andMg(OH)2, pigments, various crosslinking chemicals andoptionally sulfur, in the conventional concentrations ofrubber technology.It is possible according to the invention to prepare afinely divided rubber powder which comprises silicamodified with organosilicon compounds, is free-flowing andalso remains free-flowing after exposure to mechanicalstresses (e. g. conveying, packing).Because of its finely divided nature, no grinding or othercomminution measures are necessary to obtain finely divideddispersions.These then lead to the finely divided rubber powders whichare easy to process, and to vulcanization products withimproved properties.The ease of implementation and the advantages of thepresent invention are explained in the following examples,without the invention being limited to these measuresdemonstrated.Raw materials used in the preparationE - SBR Emulsion styrene-butadiene latex with astyrene content of 23.5 % (BSL)Si 69 Bis(triethoxysilylpropyl)tetrasulfane(Degussa AG)Si 75 Bis(triethoxysilylpropyl)disulfane(Degussa AG)Ultrasil VN3 , Precipitated silica with anUltrasil VN3 N2 surface area (BET) of 175 m2 / gfilter-cake (Degussa AG), dried or as a filter-cake, optionally granulated (gran)Ultrasil 7000, Precipitated silica with anUltrasil 7000 N2 surface area (BET) of 175 m2 / g andfilter-cake improved dispersing properties (DegussaAG), dried or as a filter-cake,optionally granulated (gran)Marlipal 1618 / 25 Emulsifier : fatty alcohol polyethyleneglycol ether (Huls AG)Examp 1 e IPreparation of powdered rubber based onE-SBR, Ultrasil 7000 and Si 69A stable suspension of 14.3 kg Ultrasil 7000, 1.58 kg Si 69( corresponds to 11.3 %, based on the silica ), 142gMarlipal 1618 / 25 (corresponds to 1 %, based on the silica Jin 255 L water is prepared, while stirring, and is thendivided up in the ratio 5:1.The larger portion of the suspension is mixed with 94.3 Lof a 21.0 % E-SBR latex emulsion, with vigorous stirring,and then lowered to a pH of 5.0 by addition of an approx.10% A12(S04)3 solution. This first precipitating step isfollowed by addition of the second portion of thesuspension, prepared as above, with subsequent lowering ofthe pH to an end point of 3.7.After the precipitating process, mechanical removal of mostof the water takes place, followed by a drying step to aresidual moisture content of < 1 % . The pulverulentfinished product (EPB 1} comprises 100 parts E-SBR and 77parts Ultrasil 7000 / Si 69 ( 11.3 % ), determined by meansof thermogravimetric analysis ( TGA ).Example IIPreparation of powdered rubber based onE-SBR, Ultrasil 7000 filter-cake and Si 69A stable suspension of 59.0 kg Ultrasil 7000 filter-cake,1.60 kg Si 69 ( corresponds to 11.3 %, based on thesilica ) , 14Og Marlipal 1618 / 25 (corresponds to 1 %, basedon the silica) in 189 L water is prepared, while stirring,and is then divided up in the ratio 5:1.The larger portion of the suspension is mixed with 95.7 Lof a 20.5 % E-SBR latex emulsion, with vigorous stirring,and then lowered to a pH of 4.9 by addition of an approx.10% A12(S04)3 solution. This first precipitating step isfollowed by addition of the second portion of thesuspension, prepared as above, with subsequent lowering ofthe pH to 3.4.After the precipitating process, mechanical removal of mostof the water takes place, followed by a drying step to aresidual moisture content of < 1 % . The pulverulentfinished product (EPB 2) comprises 100 parts E-SBR and 83parts Ultrasil 7000 (from filter-cake) / Si 69 ( 11.3 % ),(TGA determination).Example IIPreparation of powdered rubber based onE-SBR, Ultrasil 7000 filter-cake and Si 69A stable suspension of 13.9 kg Ultrasil VN3, 1.55 kg Si 69(corresponds to 11.3 %, based on the silica), 137g Marlipal1618 / 15 (corresponds to 1 %, based on the silica) in 267 Lwater is prepared, while stirring, and is then divided upin the ratio 5:1.The larger portion of the suspension is mixed with 94.7 Lof a 20.9 % E-SBR latex emulsion, with vigorous stirring,and then lowered to a pH of 5.2 by addition of an approx.10% A12(S04)3 solution. This first precipitating step isfollowed by addition of the second portion of thesuspension, prepared as above, with subsequent lowering ofthe pH to 3.5.After the precipitating process, mechanical removal of mostof the water takes place, followed by a drying step to aresidual moisture content of < 1 % . The pulverulentfinished product (EPB 3) comprises 100 parts E-SBR and 72parts Ultrasil VN3 / Si 69 ( 11.3 % ), (TGA determination).Example IVPreparation of powdered rubber based onE-SBR, Ultrasil 7000 and Si 75A stable suspension of 14.6 kg Ultrasil 7000, 1.59 kg Si 75(corresponds to 11.3 %, based on the silica ), 142gMarlipal 1618 / 15 (corresponds to 1 %, based on the silica )in 258 L water is prepared, while stirring, and is thendivided up in the ratio 5:1.The larger portion of the suspension is mixed with 93.8 Lof a 21.5 % E-SBR latex emulsion, with vigorous stirring,and then lowered to a pH of 5.1 by addition of an approx.10% A12(S04)3 solution. This first precipitating step isfollowed by addition of the second portion of thesuspension (saturation agent)with subsequent lowering ofthe pH to 3.3.After the precipitating process, mechanical removal of mostof the water takes place, followed by a drying step to aresidual moisture content of < 1 % . The pulverulentfinished product (EPB 4) comprises 100 parts E-SBR and 76parts Ultrasil 7000 / Si 75 ( 11.3 % ), (TGAdetermination).Examp1e VPreparation of powdered rubber based onE-SBR, Ultrasil 7000 filter-cake Si 75A stable suspension of 61.0 kg Ultrasil 7000 filter-cake,1.63 kg Si 75 (corresponds to 11.3 %, based on the silica),140 g Marlipal 1618 / 25 (corresponds to 1 %, based on thesilica) in 195 1 water is prepared, while stirring, and isthen divided up in the ratio 5:1.The larger portion of the suspension is mixed with 96.2 Lof a 20.5 % E-SBR latex emulsion, with vigorous stirring,and then lowered to a pH of 4.8 by addition of an approx.10% A12(S04)3 solution. This first precipitating step isfollowed by addition of the second portion of thesuspension (saturation agent) with subsequent lowering ofthe pH to 3.5.After the precipitating process, mechanical removal of mostof the water takes place, followed by a drying step to aresidual moisture content of < 1 %. The pulverulentfinished product (EPB 5) comprises 100 parts E-SBR and 80parts Ultrasil 7000 (from filter-cake) / Si 75 ( 11.3 % ),(TGA determination).The following products were employed in the rubbertechnology use:ChemicalsSBR 1500 Styrene-butadiene rubber with a styrenecontent of 23.5 %Naftolen ZD Arom. mineral oil plasticizerEPB 1 Powdered rubber comprising 100 parts E-SBR1500, 77 parts Ultrasil 7000 / Si69EPB 2 Powdered rubber comprising 100 parts E-SBR1500, 83 parts Ultrasil 7000 (fromfilter-cake) / Si69EPB 3 Powdered rubber comprising 100 parts E-SBR1500, 72 parts Ultrasil VN3 / Si69EPB 4 Powdered rubber comprising 100 parts E-SBR1500, 76 parts Ultrasil 7000 / Si75EPB 5 Powdered rubber comprising 100 parts E-SBR,80 parts Ultrasil 7000 {from filter cake) / Si756 PPD N-(1,3-Dimethylbuthyl)-N-phenyl-p-phenylenediamine [sic]CBS Benzothiazyl-2-cyclohexylsulfenamideDPG DiphenylguanidineThe following test: methods of rubber technology were used:Mooney viscosity DIN 53 523 / 3Tensile test on bar DIN 53 504Shore hardness DIN 53 505Tear propagation resistance ASTM D 624Abrasion DIN 53 516Dispersion (Philips) ISO / DIS 11 345Dispersion (coarseness) DIN 4788Elongation at break DIN 53504Breaking energy DIN 53504Example IVComparison of the rubber technology profile of values ofthe product according to the invention(preparation example1) against a standard mixturea) Recipeb) Mixing process1st stage2nd stagec) Rubber technology dataThe powdered rubber from E-SBR latex, Ultrasil 7000 and Si69 is distinguished by higher strength values, a morefavourable abrasion and a significantly improved dispersioncompared with the conventional mixing procedure.Example BComparison of the rubber technology profile of values ofthe product according to the invention EPB 2 (E-SBR / Ultrasil VN3 / Si69), EPB 3 (E-SBR / Ultrasil VN3 filter-cake / Si69)a) Recipeb) Mixing process1st stage2. stagec) Rubber technology dataThe powdered rubber from E-SBR latex, Ultrasil VN3 filter-cake and Si 69 (EPB 3) is distinguished by higher strengthvalues, a better abrasion and by an excellent dispersion inthe compound compared with Ultrasil VN 3 (EPD 2)Example IVComparison between EPB 4 (E-SBR / Ultrasil VN3 filter-cake / Si69) and EPB 5 (E-SBR / Ultrasil 7000 filter-cake / Si69)a) Recipeb) Mixing process1st stage2nd stagec) Rubber technology dataThe product EPB 5 with Ultrasil 7000 filter-cake / Si 75 isdistinguished by even better strength values, a furtherincrease in the abrasion resistance and a better dispersioncompared with the Ultrasil VN3 filter-cake {EPB 4) .
Claims
CLAIMS 1. A process for producing a finely divided rubber (a rubber powder) by precipitation from an aqueous mixture containing a filler in the form of a suspension, a water-soluble salt of a metal of group Ila, lib, Ilia or VIII of 5 the periodic table and a rubber latex (polymer latex), an aqueous emulsion of a rubber or a rubber solution, characterised in that a) one or more organosilicon compounds containing at least one alkoxy group are dissolved in water or if desired emulsified in water in the io presence of a surface-active substance, or the compounds mentioned are mixed directly, if desired with a surface-active substance, with the aqueous suspension of a finely divided oxidic or silicatic filler or a mixture of these fillers having an average particle diameter < 10pm at a temperature in the range from 10 to 60°C and preferably at room 15 temperature with stirring, the amount of this mix envisaged for incorporation in the rubber being subdivided into two lots, based on the filler fraction, and b) a first lot is mixed with polymer latex, emulsion or solution, the pH of this mixture is lowered with an acid, especially with a Lewis acid, to a pH in 20 the range from 6.0 to 4.5 (first lot, first stage), c) the remaining fraction (second lot, splitting fraction) is added with continued lowering of the pH to a value in the range from 4.5 to 2.6 and especially about 3.2 (second stage) so that the rubber present in the mixture precipitates together with the filler modified by one or more 25 organosilicon compounds, d) the precipitated solid is separated off in a conventional manner, -37e) it is preferably washed in order that the pH may be adjusted to a more propitious value for further processing, a value in the range from about 6 to 7, and 5 f) the filler-containing rubber is dried.
2. A process according to claim 1, characterised in that it utilizes one or more organosilicon compounds of the general formula [R1n - (R0)^SHAIk)m4Ar)p]q[B] (I), R’n(RO)^Si-(Alk) (II), or R1„(RO)3-nSi-(Alkenyl) (HI) where is -SCN, -SH ,-CI, -NH2 (when q = 1) or -Sx- (when q = 2) R and R1 are each an alkyl group having 1 to 4 carbon atoms, branched or unbranched, phenyl, all R and R1 radicals may each be the same or different, preferably an alkyl group, is a C1-C4- alkyl, -Cj-C^ alkoxy group, branched or unbranched, is 0, 1 or 2 -38Alk is a bivalent straight or branched hydrocarbyl radical having 1 to 6 carbon atoms, m isOorl, 5 Ar is an arylene radical having 6 to 12 carbon atoms, p is 0 or 1 with the proviso that p and m are not 0 at one and the same time, x is a number from 2 to 8, Alkyl is a univalent straight or branched unsaturated dbydrocarbyl io radical having 1 to 20 carbon atoms and preferably 2 to 8 carbon atoms, Alkenyl is a univalent straight or branched unsaturated hydrocarbyl radical having 2 to 20 carbon atoms and preferably 2 to 8 carbon atoms.
153. A process according to claim 1 or 2, characterised in that a nonionic surfactant, a cationic surfactant or an anionic surfactant is used as surface-active substance.
4. A process according to claim 3, 20 characterised in that the surfactant is used in an amount in the range from 1% to 15% by weight and especially in the range from 2% to 10% by weight, based on the amount of organosilane compound in the emulsion. -395. A process according to one or more of the preceding claims, characterised in that the concentration of organosilicon compound in the suspension is in the 5 range from 0.3% to 15% by weight, based on the filler (bone dry).
6. A process according to claim 1, characterised in that the rubber powder is precipitated in the presence of an acid, preferably a Lewis acid, especially Al2<SO4)3.
7. A process according to claim 3, io characterised in that a surfactant from the class of the fatty alcohol polyethylene glycol ethers or alkylphenol polyethylene glycol ethers is used.
8. A process according to one or more of the preceding claims, characterised in that 15 the filler used in stage a) is in particular the filter cake of a precipitated silica that has been washed salt free.
9. A process according to one or more of the preceding claims, characterised in that the solid material arising in the course of the work-up of natural fillers, 20 especially clays, is used.
10. A process according to claim 1, characterised in that the first lot of step b) utilizes z 50 parts of the filler fraction envisaged in the rubber powder. -4011 .A process according to claim 1, characterised in that the first lot as per b) utilizes from 90% to 99% of the filler fraction5 envisaged in the rubber powder when the envisaged filler fraction is > 80 parts of filler per hundred parts of rubber (phr).
12. A process according to one or more of the preceding claims, characterised in that a rubber grade carbon black is added in the desired amount to the io emulsion / suspension of step a) or to the mixture of step b).
13. A process according to claim 1, characterised in that either the emulsion, suspension or solution as per item a) in claim 1 or the mix generated as per items b) c) of claim 1 is admixed with customary is rubber industry processing aids, antioxidants, activators and / or crosslinking chemicals and sulphur in a customary amount.
14. A finely divided rubber (a rubber powder) produced according to claim 1, comprising rubber, a filler and customary rubber industry processing aids, antioxidants, activators and / or crosslinking chemicals and sulphur in a 20 customary amount.